Wafer adsorption carrying platform and film expanding equipment
By dividing the center and edge adsorption areas on the wafer adsorption stage, and using the vacuum chamber to control the negative pressure, the problem of uneven chip spacing caused by the rebound shrinkage of the wafer film is solved, and the production efficiency and yield rate of semiconductor products are improved.
Patent Information
- Application Number
- CN202420454278.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-08
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2034-03-08
AI Technical Summary
In the wafer processing process, the rebound and shrinkage of the wafer film after the crystal expansion process leads to uneven chip spacing, which affects production efficiency and increases the scrap rate.
Design a wafer adsorption stage that divides the center adsorption area and edge adsorption area on the stage body, and uses independent vacuum chambers to control the negative pressure of the center adsorption part and edge adsorption part to fix the wafer and peripheral film. Avoid retraction.
It effectively keeps the wafer spacing stable, improves production efficiency and reduces the scrap rate to meet subsequent process requirements.
Smart Images

Figure CN221928037U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of semiconductor processing, and in particular to a wafer adsorption carrier and film expansion equipment. Background Art
[0002] In the wafer processing technology, the wafer needs to be expanded at room temperature or above room temperature after the crystal expansion treatment, and the outer wafer film part between the wafer and the wafer ring is heated and shrunk after the film expansion treatment is completed. The purpose is to utilize the characteristics of the wafer film shrinking when heated to allow the deformed outer wafer film to shrink to a tensioned state, which is convenient for continued use and recycling in subsequent process steps, eliminating the film replacement step.
[0003] However, due to the strong elasticity and toughness of the wafer film, it is easy for the wafer film to rebound and shrink after the crystal expansion process, resulting in uneven spacing between chips, making it difficult to meet subsequent process requirements, reducing production efficiency and increasing the scrap rate. Utility Model Content
[0004] The purpose of the embodiments of the utility model is to provide a wafer adsorption carrier and film expansion equipment to solve the problem of uneven chip spacing caused by the rebound and shrinkage of the wafer film after the wafer expansion process.
[0005] In order to achieve the above purpose, the utility model adopts the following technical solutions:
[0006] In a first aspect, a wafer adsorption stage is provided, comprising:
[0007] A carrier body, wherein a central adsorption area and an edge adsorption area surrounding the central adsorption area are formed on the carrier body, a central adsorption portion is arranged on the central adsorption area, and edge adsorption portions connected end to end are arranged on the edge adsorption area;
[0008] A first vacuum chamber and a second vacuum chamber are independently provided in the carrier body. One end of the first vacuum chamber and the second vacuum chamber are used to connect to two independent external vacuum sources respectively, the other end of the first vacuum chamber is connected to the central adsorption part, and the other end of the second vacuum chamber is connected to the edge adsorption part.
[0009] As an optional implementation, the central adsorption portion is a plurality of vacuum micropores uniformly distributed in the central adsorption area.
[0010] As an optional implementation, the carrier body is provided with a microporous ceramic carrier in the central adsorption area, and the central adsorption portion is vacuum micropores uniformly distributed on the microporous ceramic carrier.
[0011] As an optional implementation, the edge adsorption portion is an annular adsorption groove.
[0012] As an optional implementation, in the cross-sectional direction of the adsorption groove, the groove wall shape of the adsorption groove is arc-shaped.
[0013] As an optional implementation, the second vacuum chamber includes:
[0014] A gas-homogenizing chamber, used to be connected to one of the external vacuum sources;
[0015] There are multiple vacuum channels, and the multiple vacuum channels are radially arranged around the uniform air cavity at intervals, and the opposite ends of each vacuum channel are respectively connected to the uniform air cavity and the edge adsorption part.
[0016] As an optional implementation, it also includes:
[0017] The first heating component is arranged at the bottom or inside of the carrier body and is used for heating the carrier body.
[0018] As an optional implementation, it also includes:
[0019] A support base, mounted on the bottom of the platform body and sealingly matched with the platform body;
[0020] In the case where the first heat generating component is disposed at the bottom of the stage body, the first heat generating component is disposed between the stage body and the supporting base.
[0021] As an optional embodiment, the support base is provided with a first vacuum hole and a second vacuum hole, the first heat-generating component is provided with a first connecting hole and a second connecting hole, the first vacuum hole and the first connecting hole are correspondingly connected to the first vacuum chamber, and the second vacuum hole and the second connecting hole are correspondingly connected to the second vacuum chamber;
[0022] The first vacuum hole and the second vacuum hole are respectively installed with pneumatic joints, and the two pneumatic joints are used to connect two independent external vacuum sources respectively;
[0023] The first connecting hole and the second connecting hole are respectively installed with sealing rings, and opposite sides of the sealing rings are respectively pressed against the pneumatic joint and the carrier body.
[0024] In a second aspect, a film expansion device is provided, comprising:
[0025] The wafer adsorption stage as described in the first aspect
[0026] The beneficial effects of the utility model are as follows: the wafer adsorption stage is divided into a central adsorption area and an edge adsorption area arranged sequentially from the inside to the outside on the stage body, so as to carry the wafer and the peripheral wafer film between the wafer and the wafer ring respectively, so that the wafer and the peripheral wafer film can be stably placed on the stage body, the relative movement between the wafer film and the stage body is reduced, and the product stability is improved;
[0027] The first vacuum chamber and the second vacuum chamber are used to independently control the central adsorption part and the edge adsorption part, so that the wafer and the peripheral wafer film can be adsorbed and fixed in the central adsorption area and the edge adsorption area respectively, and the wafer film is kept in a relatively stable state, avoiding the shrinkage of the peripheral wafer film. Even after heating and shrinking the film, the wafer spacing can be kept in the state after expansion, meeting the requirements of subsequent related processes, improving the production efficiency of semiconductor products, and correspondingly reducing the scrap rate. BRIEF DESCRIPTION OF THE DRAWINGS
[0028] The utility model is further described in detail below based on the drawings and embodiments.
[0029] Figure 1 This is an exploded view of the wafer adsorption stage described in the embodiment of the utility model;
[0030] Figure 2 This is a schematic diagram of the structure of the stage body according to an embodiment of the utility model;
[0031] Figure 3 This is a schematic diagram of the internal structure of the stage body according to an embodiment of the utility model;
[0032] Figure 4 This is a cross-sectional view of the stage body described in the embodiment of the utility model;
[0033] Figure 5 for Figure 4 A magnified view of part A;
[0034] Figure 6 It is a schematic diagram of the overall structure of the wafer adsorption carrier described in an embodiment of the utility model.
[0035] In the figure: 10, carrier body; 11, loading table; 111, central adsorption area; 1111, central adsorption part; 112, edge adsorption area; 1121, edge adsorption part; 12, first vacuum chamber; 13, second vacuum chamber; 131, uniform air chamber; 132, vacuum channel; 1321, first channel; 1322, second channel; 14, microporous ceramic carrier; 20, first heating component; 21, first connecting hole; 22, second connecting hole; 23, sealing ring; 30, supporting base; 31, first vacuum hole; 32, second vacuum hole; 33, pneumatic joint. DETAILED DESCRIPTION
[0036] In order to make the technical problems solved by the utility model, the technical solutions adopted and the technical effects achieved clearer, the technical solutions of the embodiments of the utility model are further described in detail below. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of them. Based on the embodiments of the utility model, all other embodiments obtained by those skilled in the art without creative work are within the scope of protection of the utility model.
[0037] In the description of the present invention, unless otherwise clearly specified and limited, the terms "connected", "connected", and "fixed" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0038] In the present utility model, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may include that the first and second features are in direct contact, or may include that the first and second features are not in direct contact but are in contact through another feature between them. Moreover, a first feature being "above", "above" and "above" a second feature includes that the first feature is directly above and obliquely above the second feature, or simply indicates that the first feature is higher in level than the second feature. A first feature being "below", "below" and "below" a second feature includes that the first feature is directly below and obliquely below the second feature, or simply indicates that the first feature is lower in level than the second feature.
[0039] With the rapid development of science and technology, terminal devices such as mobile phones, tablets, and laptops are showing a trend of becoming lighter, thinner, and larger in capacity. The requirements for thinning memory are also getting higher and higher. The thickness of mainstream chips used in related terminal devices is already below 100um (micrometers). Due to the easy generation of chip breakage problems, traditional cutting processes are difficult to cope with wafers with this thickness requirement. SDBG (Stealth Dicing Before Grinding) and DBG (Dicing Before Grinding) processes are currently the mainstream production methods for memories (NAND memory, DRAM dynamic random access memory, etc.).
[0040] Among them, the expansion and shrinkage of wafer products are important parts of the SDBG and DBG processes. After the wafer is expanded at low temperature, it needs to be expanded again at room temperature or above. During the secondary expansion, the distance between chips needs to be maintained by vacuum adsorption and other means. After the secondary expansion, the outer wafer film between the whole wafer and the wafer ring will be heated and shrunk. The purpose is to use the characteristics of the wafer film shrinking when heated to shrink the deformed outer wafer film back to the tensioned state, which is convenient for the continued use and recycling of subsequent process steps, eliminating the film replacement step.
[0041] From the background technology, it can be seen that due to the strong elasticity and toughness of the wafer film, the wafer film is prone to rebound and shrinkage after the crystal expansion process, resulting in uneven spacing between chips, making it difficult to meet subsequent process requirements, reducing production efficiency and increasing the scrap rate.
[0042] In view of this, the present embodiment provides a wafer adsorption platform, which adsorbs and fixes the above-mentioned peripheral wafer film through an edge adsorption area 112 set on the outer edge of the platform, so as to adsorb and fix the wafer film after crystal expansion and secondary film expansion processing, thereby solving the problem of uneven chip spacing caused by rebound shrinkage of the wafer film.
[0043] It should be explained in advance that the wafer adsorption platform provided in this embodiment is a device in semiconductor manufacturing equipment, which is used to fix and support the wafer during the manufacturing process. It is usually located in the processing area of the equipment to ensure the stability and reliability of the wafer during high-speed rotation, high-precision positioning and other processing steps.
[0044] The definitions and functions of the wafer, wafer film, and wafer ring mentioned in this embodiment are briefly described as follows:
[0045] Wafer Ring:
[0046] The wafer ring is usually a circular frame. In the wafer manufacturing process, the wafer ring mainly supports and fixes the position of the wafer. It can also be used for wafer transmission, storage and positioning to ensure that the wafer does not move or deform during processing. It is generally made of materials compatible with the wafer material, such as quartz, ceramic or metal.
[0047] Wafer Membrane:
[0048] The wafer film is usually a transparent film made of flexible materials, such as polyester film or polyimide film. The wafer film has sufficient strength and chemical corrosion resistance to support the wafer on the wafer ring. The outer periphery of the wafer film is fixed to the wafer ring, and the wafer can be attached to the wafer film inside the wafer ring to protect the wafer from mechanical damage and chemical contamination.
[0049] Wafer:
[0050] Wafers are the core materials used in semiconductor manufacturing. They are thin slices made of single crystal silicon or other semiconductor materials. They serve as the basis for manufacturing integrated circuits and chips. Their quality and performance directly affect the performance and reliability of the final product.
[0051] The peripheral wafer film described in this embodiment mainly refers to the portion of the wafer film located between the wafer and the wafer ring, specifically located on the outside of the wafer and the inside of the wafer ring, and used to connect the wafer and the wafer ring.
[0052] Please refer to the attached Figure 1-Figure 4 The wafer adsorption platform includes a platform body 10, which serves as a supporting base for the wafer in the relevant process. The platform body 10 plays a role in supporting and fixing the wafer in the wafer adsorption platform and providing a corresponding installation position for relevant functional module components.
[0053] In order to facilitate the understanding of the scheme, the present embodiment defines one side surface of the carrier body 10 as a loading table 11. Theoretically, the loading table 11 can be formed on the surface of any side of the carrier body 10, such as the surface on the upper side, the bottom surface or the surface on other sides of the carrier body 10. The loading table 11 is used to provide the function of loading wafers. In the present embodiment, in order to ensure that the wafer can have a high support stability in the relevant process flow, the loading table 11 is formed on the upper side of the carrier body 10, and the loading table 11 is in a horizontal or nearly horizontal setting state when the wafer adsorption carrier is stably placed on the support structure (such as the workshop floor, etc.), so that the wafer product can also be in a horizontal or nearly horizontal state when it is loaded. In addition, using the upper side of the carrier body 10 as the surface of the loading table 11 is not only conducive to the stable loading of the wafer, but also convenient for the conveying mechanism outside the wafer adsorption carrier to place the wafer on the loading table 11, and convenient for the conveying mechanism to remove the wafer located on the loading table 11, which is beneficial to improving the operation accuracy and efficiency.
[0054] The carrier body 10 is located on the mounting table 11 and is formed with a central adsorption area 111 and an edge adsorption area 112 surrounding the outer periphery of the central adsorption area 111. In the relevant process flow of chip manufacturing, the position of the central adsorption area 111 corresponds to the wafer and is used to carry the wafer, while the position of the edge adsorption area 112 corresponds to the part of the outer wafer film, and the wafer ring is fixed by a fixing mechanism arranged outside the wafer adsorption carrier.
[0055] From the above, it can be seen that since the wafer is attached and fixed to the wafer film to provide corresponding support through the wafer film, when the wafer is carried in the central adsorption area 111 through the wafer film, the wafer is actually also carried on the mounting table 11 through the wafer film. That is to say, the parts corresponding to the central adsorption area 111 and the edge adsorption area 112 are both wafer films, but the areas of the wafer film corresponding to the central adsorption area 111 and the edge adsorption area 112 are different. The central adsorption area 111 is used to carry the part of the wafer film to which the wafer is attached, and the edge adsorption area 112 corresponds to the peripheral wafer film part located outside the wafer.
[0056] Please continue to refer to the attached Figure 1-Figure 4 After the mounting table 11 is divided into areas, in order to achieve effective adsorption and fixation of the wafer and the peripheral wafer film, the central adsorption area 111 is provided with a central adsorption portion 1111, and the edge adsorption area 112 is provided with edge adsorption portions 1121 connected end to end.
[0057] Continuing with the example of the implementation in which the loading table 11 is located above the loading table body 10, both the central adsorption portion 1111 and the edge adsorption portion 1121 can generate negative pressure above the area corresponding to the loading table 11, so that when the wafer is loaded on the central adsorption area 111 through the wafer film corresponding to its position, the central adsorption area 111 adsorbs and fixes the wafer film under the wafer through the central adsorption portion 1111, so that the wafer can be stably adsorbed and fixed in the central adsorption area 111. At the same time, the peripheral wafer film in this state is located on the edge adsorption area 112, and the edge adsorption area 112 adsorbs and fixes the peripheral wafer film through the edge adsorption portion 1121, so that the peripheral wafer film can be adsorbed and fixed in the edge adsorption area 112.
[0058] It is worth mentioning that in order to ensure that the wafer with a relatively large area on the wafer film can be stably fixed on the central adsorption area 111, a plurality of evenly distributed central adsorption parts 1111 can be set on the central adsorption area 111, and the wafer film under the chip at the corresponding position is adsorbed by the plurality of central adsorption parts 1111, thereby ensuring that each chip can be kept in the current position. Of course, this embodiment is not limited to this. In other embodiments except for setting a plurality of central adsorption parts 1111, the central adsorption part 1111 can also be set to only one, and the negative pressure generated by the central adsorption part 1111 on the mounting table 11 can stably adsorb the wafer film corresponding to the position of the wafer and the wafer itself on the central adsorption area 111.
[0059] Furthermore, the present embodiment does not specifically limit the specific structural form of the central adsorption portion 1111 , and it can be arranged on the central adsorption area 111 in any structural form as long as it can play a role in forming negative pressure on the loading table 11 .
[0060] The edge adsorption portion 1121 is located on the loading table 11 to form a structural form connected end to end. It can be understood that, from a two-dimensional perspective, the edge adsorption portion 1121 is located on the loading table 11 to form a closed figure, which can also be understood as a continuous figure. Exemplarily, the figure formed by the edge adsorption portion 1121 on the edge adsorption area 112 can be a circle or a polygon (such as a triangle, a quadrilateral, etc.). Such a configuration can form a closed vacuum belt surrounding the outer periphery of the central adsorption area 111 on the edge adsorption area 112 through the edge adsorption portion 1121, so that the peripheral wafer film can be adsorbed and fixed on the edge adsorption area 112 by the edge adsorption portion 1121 along the circumferential direction, thereby avoiding the situation where the chip spacing is unevenly narrowed due to wafer film shrinkage. In addition, the peripheral wafer film is adsorbed on the edge adsorption area 112 in the circumferential direction, so that a relatively closed vacuum space can be formed between the wafer film part corresponding to the wafer and the central adsorption area 111, thereby improving the sealing between the wafer film and the central adsorption area 111, and further ensuring the firmness between the wafer film part corresponding to the wafer and the central adsorption area 111 in the adsorption state.
[0061] Continuing with the above embodiment, a first vacuum chamber 12 and a second vacuum chamber 13 are provided in the carrier body 10, which are independent of each other. That is, the first vacuum chamber 12 and the second vacuum chamber 13 are located in the carrier body 10 and do not have any connection relationship in any sense. The two are at least two independently spaced vacuum chambers. One end of the first vacuum chamber 12 and the second vacuum chamber 13 are used to connect two independent external vacuum sources respectively, the other end of the first vacuum chamber 12 is connected to the central adsorption part 1111, and the other end of the second vacuum chamber 13 is connected to the edge adsorption part 1121, wherein one external vacuum source is configured to generate a negative pressure at the corresponding central adsorption part 1111 through the first vacuum chamber 12, and the other external vacuum source is configured to generate a negative pressure at the corresponding edge adsorption part 1121 through the second vacuum chamber 13, and the central adsorption part 1111 and the edge adsorption part 1121 are respectively controlled by two sets of independent vacuum sources, so that the wafer adsorption carrier can meet the requirements of the film expansion equipment during the relevant process of performing relevant processes on the wafer.
[0062] It should be understood from the above embodiment that the external vacuum source described in this embodiment may be a vacuum pump.
[0063] The first vacuum chamber 12 and the second vacuum chamber 13 described in the above embodiment are located in the stage body 10 and can be respectively set to one or more. Taking the embodiment in which there are multiple first vacuum chambers 12 as an example, the second vacuum chamber 13 is similar, and the first end of each first vacuum chamber 12 is used to connect with an external vacuum source, and the first ends of each first vacuum chamber 12 are interconnected. By utilizing the first vacuum chamber 12 with stronger integration to connect with the external vacuum source, it is possible to achieve the effect of generating negative pressure on each first vacuum chamber 12 only by using one external vacuum source, while reducing the number of external vacuum sources used, and making the negative pressure generated between each first vacuum chamber 12 and the corresponding central adsorption portion 1111 more balanced, so that the adsorption force between each part of the wafer film and the central adsorption area 111 is more uniform, and the stability of the wafer on the central adsorption area 111 is effectively improved.
[0064] In addition, through the above setting method, the cumbersome operation of connecting the central adsorption part 1111 and the edge adsorption part 1121 with the external vacuum source can also be reduced. For example, in an embodiment in which the first vacuum chamber 12 and the second vacuum chamber 13 are both set to multiple, and each first vacuum chamber 12 and each second vacuum chamber 13 only uses one set of external vacuum source, each external vacuum source needs to be configured with multiple vacuum pipelines and connected to each first vacuum chamber 12 or each second vacuum chamber 13 through the vacuum pipeline. This not only increases the difficulty of connecting the external vacuum source with the adsorption part on the corresponding area, but also makes there is a greater risk of air leakage between the adsorption part and the external vacuum source. Therefore, setting multiple first vacuum chambers 12 and / or multiple second vacuum chambers 13 to be interconnected at one end can effectively solve the above-mentioned corresponding problems.
[0065] Please continue to refer to the attached Figure 1-Figure 4 This embodiment briefly describes the operation process of the wafer adsorption stage in a specific usage scenario according to the technical solution provided above:
[0066] On the premise that the wafer ring is relatively fixed with the carrier body 10 through the fixing mechanism outside the carrier body 10, and the wafer expansion and the wafer film have completed the secondary expansion, the wafer is carried on the central adsorption area 111 through the wafer film, and the peripheral wafer film is correspondingly carried on the edge adsorption area 112, wherein an external vacuum source generates negative pressure on the first vacuum chamber 11, so that the central adsorption part 1111 located in the central adsorption area 111 adsorbs and fixes the wafer film corresponding to the position of the wafer, so that each chip can be stably placed on the central adsorption area 111 and ensure that the relative position of each chip will not be offset, ensuring that the spacing between chips is uniform, and another external vacuum source generates negative pressure on the second vacuum chamber 12, so that the edge adsorption part 1121 located in the edge adsorption area 112 adsorbs and fixes the peripheral wafer film, so that the peripheral wafer film on the periphery of the wafer can be fixed, to avoid the overall shrinkage of the wafer film and affect the chip spacing, and the wafer film can be released only after the peripheral wafer film is heated and shrunk to a tensioned state.
[0067] In summary, the wafer adsorption stage is divided into a central adsorption area 111 and an edge adsorption area 112 arranged sequentially from the inside to the outside on the stage body 10, so as to carry the wafer and the peripheral wafer film between the wafer and the wafer ring separately, so that the wafer and the peripheral wafer film can be stably placed on the stage body 10, reduce the relative movement between the wafer film and the stage body 10, and improve the product stability. The first vacuum chamber 12 and the second vacuum chamber 13 are used to independently control the central adsorption part 1111 and the edge adsorption part 1121, respectively, so that the wafer and the peripheral wafer film can be adsorbed and fixed in the central adsorption area 111 and the edge adsorption area 112, respectively, and the wafer film is kept in a relatively stable state, avoiding the shrinkage of the peripheral wafer film. Even after heating and shrinking the film, the wafer spacing can be kept in the state after the expansion, meeting the requirements of subsequent related processes, improving the production efficiency of semiconductor products, and correspondingly reducing the scrap rate.
[0068] It can be understood from the above-mentioned solutions that the central adsorption portion 1111 can adopt any structural form that can meet the negative pressure requirement on the central adsorption area 111. Taking the hole groove structure as an example, the central adsorption portion 1111 can be a vacuum groove structure extending in any direction in the central adsorption area 111, or it can be a vacuum hole structure with only one or multiple holes distributed on the central adsorption area 111.
[0069] Since the wafer film to be adsorbed and fixed by the central adsorption area 111 carries a wafer, the spacing between the chips is required to be relatively high. Therefore, in addition to ensuring that the central adsorption area 111 has a high adsorption strength for the wafer film, it is also necessary to ensure that the adsorption force of the central adsorption area 111 on the wafer film is relatively uniform, avoiding the situation where the wafer film is pulled and deformed, so that the wafer film remains flat and stable on the central adsorption area 111, so that each chip can remain stable. Therefore, in this embodiment, the central adsorption part 1111 is configured as a plurality of vacuum micropores uniformly distributed in the central adsorption area 111, one end of each vacuum micropore is connected to the first vacuum chamber 12, and the other end thereof is located on the central adsorption area 111 to form an orifice.
[0070] Continuing with the above embodiment, the vacuum micropores in this embodiment refer to tiny holes existing inside the carrier body 10 and on the surface of the central adsorption area 111. The size of these holes is generally controlled to be less than 2 mm (millimeter). Under the vacuum conditions formed by the external vacuum source, each vacuum micropore located in the vacuum adsorption area can form a negative pressure to adsorb the wafer film at the corresponding position, so that the chip on the wafer film remains stable.
[0071] On the basis of any of the above embodiments, the carrier body 10 located in the central adsorption area 111 can be provided with a microporous ceramic carrier 14 so as to utilize the vacuum micropores distributed on the microporous ceramic carrier 14 as the central adsorption portion 1111 in the above embodiments.
[0072] It can be explained that the main feature of the microporous ceramic carrier 14 is that it uses microporous ceramic as a substrate. Microporous ceramic is a ceramic material with tiny pores. The microporous ceramic carrier 14 utilizes the excellent properties of microporous ceramic to achieve the following advantages:
[0073] High thermal conductivity: Microporous ceramics have good thermal conductivity and can quickly conduct away the heat generated during wafer processing to prevent the wafer from being deformed or damaged due to thermal stress, or can quickly transfer the heat from the carrier body 10 to the wafer to meet the requirements of wafer-related processes.
[0074] High air permeability: The tiny holes of microporous ceramics can provide good air permeability, which helps the microporous ceramic carrier 14 to form a uniform and stable negative pressure through the vacuum micropores when placed on the first vacuum chamber 12, so that the wafer film and the wafer can be stably adsorbed on the corresponding central adsorption area 111.
[0075] High mechanical strength: Microporous ceramics have high mechanical strength and can withstand the mechanical stress and pressure during wafer processing, ensuring the stability and safety of the wafer, allowing the wafer adsorption carrier to maintain the structural stability of the carrier body 10 during the early crystal expansion and film expansion processing.
[0076] Good chemical stability: Microporous ceramics have good stability to many chemicals and can resist corrosion and contamination that may be encountered during wafer processing.
[0077] The carrier body 10 located on the edge adsorption area 112 can be made of metal or other materials. In one embodiment, a groove having a structure compatible with the structure of the microporous ceramic carrier 14 can be opened at the position of the carrier body 10 corresponding to the central adsorption area 111, so that the microporous ceramic carrier 14 can be embedded in the groove to complete the installation with the carrier body 10, and the first vacuum chamber 12 can also be arranged at the lower part of the groove, so that the microporous ceramic carrier 14 is embedded in the groove and relatively fixed with the carrier body 10, while completing the connection between each vacuum micropore and the first vacuum chamber 12.
[0078] It is worth mentioning that the surface of the microporous ceramic carrier 14 and the surface of the carrier body 10 located in the edge adsorption area 112 can be set to be parallel to each other or to form a height difference between the two according to the manufacturing requirements of the wafer product.
[0079] Please continue to refer to the attached Figure 1-Figure 5 In this embodiment, the edge adsorption portion 1121 is set as an annular adsorption groove according to the outer edge structure of the wafer, and the outer wafer film is adsorbed and fixed by the adsorption groove opened on the edge adsorption area 112, so that the relative distances between the edge adsorption portion 1121 and the edge of the wafer can be kept equal, further improving the air tightness between the wafer film and the central adsorption area 111, and making the shrinkage amount of the outer wafer film at various locations on the periphery consistent during the heating and shrinking process, so that when the outer wafer film is restored to a tensioned state and is separated from negative pressure adsorption, the force between the wafer film and the wafer ring, as well as between the wafer film and each chip is uniform, so that the distance between each chip on the wafer film can still be maintained within the range required by the corresponding process.
[0080] Continuing with the above-mentioned implementation method of using an annular adsorption groove as the edge adsorption portion 1121, please refer to the attached Figure 4-Figure 5 , located in the cross-sectional direction of the adsorption groove, the groove wall shape of the adsorption groove is arc-shaped. Such a setting can increase the contact area between the peripheral wafer film and the edge adsorption part 1121. Under the action of the external vacuum source, the peripheral wafer film can be evenly adsorbed on the groove wall surface of the adsorption groove under the influence of negative pressure, thereby improving the sealing performance between the peripheral wafer film and the edge adsorption part 1121, and reducing the risk of vacuum leakage between the central adsorption area 111 and the wafer film. The arc-shaped groove wall structure can avoid damage to the surface of the wafer film, so that after the wafer film is released, the wafer film can still meet the requirements of the subsequent wafer manufacturing process.
[0081] In a specific implementation, the cross-sectional shape of the adsorption groove is semicircular, the bottom of the adsorption groove is connected to the second vacuum chamber 13 , and the groove opening of the adsorption groove is opened on the mounting table 11 .
[0082] As an example that can be based on any of the above implementations, Figure 3-Figure 5 As shown, the second vacuum chamber 13 includes an air-uniform chamber 131 and a vacuum channel 132. The air-uniform chamber 131 is used to connect to one of the external vacuum sources, and the vacuum channel 132 is provided in plurality. The plurality of vacuum channels 132 are radially arranged around the air-uniform chamber 131 at intervals, and the opposite ends of each vacuum channel 132 are respectively connected to the air-uniform chamber 131 and the edge adsorption portion 1121, so that the negative pressure generated by the external vacuum source can be evenly distributed to each vacuum channel 132 in the air-uniform chamber 131. In this way, the negative pressure generated by each vacuum channel 132 at each location of the closed edge adsorption portion 1121 is consistent, so that the peripheral wafer film can be stably adsorbed by the edge adsorption portion 1121 along the circumferential direction.
[0083] It should be noted that the uniform air chamber 131 located in the carrier body 10 may be a closed structure connected end to end, or a chamber with an integral structure having a certain space volume directly opened inside the carrier body 10. In the embodiment where the edge adsorption portion 1121 is an annular adsorption groove opened on the carrier body 10, in order to balance the negative pressure in the uniform air chamber 131, the uniform air chamber 131 may be provided with an annular chamber structure or a circular chamber structure, so that when the vacuum channels 132 are arranged at intervals around the periphery of the uniform air chamber 131, the negative pressure acting in the vacuum channels 132 can be in a relatively balanced state, ensuring that the adsorption force of the peripheral wafer film is consistent at various locations.
[0084] In one embodiment, if Figure 3-Figure 5 As shown, in order to form two independent vacuum spaces with the first vacuum chamber 11 , the uniform air chamber 131 is configured as an annular structure, and the first vacuum chamber 11 is configured as a tubular structure in the center of the annular uniform air chamber 131 , passing through the upper and lower sides of the carrier body 10 .
[0085] In order to facilitate the processing and forming of the vacuum channel 132 in the stage body 10, the vacuum channel 132 includes a first channel 1321 and a second channel 1322, both of which extend in a straight line. Among them, the first channel 1321 extends in the horizontal direction of the stage body 10 and is arranged in a scattered distribution around the periphery of the uniform gas cavity 131 at intervals. The first channel 1321 can be processed by tools such as a drill to open it on the outer peripheral surface of the stage body 10 toward its center. In the actual application scenario of the wafer adsorption stage, the first channel 1321 formed by this processing method needs to be provided with a sealing plug at the opening formed on the outer periphery of the stage body 10 to ensure the airtightness of the second vacuum cavity 13. The second channel 1322 is arranged along the vertical direction of the carrier body 10 and is arranged one by one between each first channel 1321 and the adsorption groove, and is used to connect the first channel 1321 and the adsorption groove. The second channel 1322 can be processed by drilling tools such as a drill bit on the side of the carrier body 10 located on the mounting table 11 from top to bottom until the second channel 1322 is connected with the first channel 1321. In this way, the vacuum channel 132 can be formed by only two straight line processing methods, and the processing difficulty is relatively low, and the connection between each vacuum channel 132 and the uniform air chamber 131 is ensured, and the negative pressure balance requirement of each vacuum channel 132 is met.
[0086] With reference to any of the above embodiments, Figure 1As shown, the wafer adsorption platform also includes a first heating component 20, which is arranged at the bottom or inside of the platform body 10, and is used to heat the platform body 10, so that the temperature of the platform body 10 on the side of the mounting table 11 can be increased and the wafer film can be softened, thereby reducing the force generated by the shrinkage of the wafer film, thereby reducing the adsorption pressure of the central adsorption area 111 and the edge adsorption area 112, and can also reduce the risk of wafer film damage to a certain extent, so that the chip can be more stably adsorbed and fixed on the platform body 10, ensuring uniform chip spacing.
[0087] It is understandable that the first heating component 20 can be set to one or more according to the structural design of the stage body 10 and the requirements of the wafer manufacturing process, and any heating component with heating function available in the prior art can be used, and can be set at the bottom or inside of the stage body 10 to achieve the purpose of heating the stage body 10. Exemplarily, the first heating component 20 can be a thin film heating plate, a heating tube, etc.
[0088] Continuing from the above embodiment, the wafer adsorption stage further includes a support base 30, which serves as a connection structure between the stage body 10 and the relevant support structure, and is installed at the bottom of the stage body 10 and is sealed with the stage body 10. In the case where the first heat generating component 20 is disposed at the bottom of the stage body 10, the first heat generating component 20 is disposed between the stage body 10 and the support base 30, so as to press the first heat generating component 20 tightly between the stage body 10 and the support base 30.
[0089] Specifically, the first heating component 20 of the present embodiment is a thin film heating plate. The thin film heating plate is arranged in a form in which its outer circumferential dimension is smaller than the carrier body 10 according to the structural dimension of the carrier body 10, and is installed at the bottom of the carrier body 10, and is pressed against the carrier body 10 by the supporting base 30. The use of the thin film heating plate can make the various parts of the carrier body 10 heated more evenly, so that when the heat is transferred to the wafer film through the carrier body 10 and the microporous ceramic carrier 14, the various parts of the wafer film are heated uniformly and the overall softening degree is the same, so that the wafer film can be fixed on the carrier body 10 under uniform negative pressure suction, further reducing the risk of deformation and damage of the wafer film.
[0090] Please continue to refer to the attached Figure 1 , Figure 4-Figure 6, in order to ensure that the first vacuum chamber 12 and the second vacuum chamber 13 can still be connected to the external vacuum source when the first heating component 20 and the support base 30 are arranged at the bottom of the stage body 10. Under the condition of ensuring that the support base 30 is sealed and connected to the stage body 10, the support base 30 is provided with a first vacuum hole 31 and a second vacuum hole 32. The first vacuum hole 31 and the second vacuum hole 32 are located in the support base 30 and are also two independent hole structures to avoid the vacuum leakage between the two when they are respectively connected to the first vacuum chamber 12 and the second vacuum chamber 13. The first vacuum hole 31 and the second vacuum hole 32 respectively penetrate any two sides of the support base 30. One end of the first vacuum hole 31 and the second vacuum hole 32 are respectively arranged close to the first vacuum chamber 12 and the second vacuum chamber 13, so as to facilitate the communication with the first vacuum chamber 12 and the second vacuum chamber 13, and the other end of the first vacuum hole 31 and the second vacuum hole 32 are used to be connected to two independent external vacuum sources respectively. Correspondingly, the first heating component 20 is provided with a first connecting hole 21 and a second connecting hole 22, the first vacuum hole 31 and the first connecting hole 21 are correspondingly connected to the first vacuum chamber 12, the second vacuum hole 32 and the second connecting hole 22 are correspondingly connected to the second vacuum chamber 13, wherein an external vacuum source is connected to the first vacuum chamber 12 via the first vacuum hole 31 and the first connecting hole 21 in sequence, and another external vacuum source is connected to the second vacuum chamber 13 via the second vacuum hole 32 and the second connecting hole 22 in sequence.
[0091] In order to realize the independent control of the first vacuum chamber 12 and the second vacuum chamber 13 and avoid the vacuum leakage caused by the installation gap between the support base 30, the first heating component 20 and the stage body 10 during the control of the two, the first vacuum hole 31 and the second vacuum hole 32 are respectively installed with pneumatic joints 33, and the two pneumatic joints 33 are used to connect two independent external vacuum sources respectively. The pneumatic joints 33 can be opened when the external vacuum source is turned on, so that the two external vacuum sources are connected to the first vacuum chamber 12 and the second vacuum chamber 13 respectively, and closed when the external vacuum source stops running, so as to avoid vacuum leakage of the first vacuum chamber 12 and the second vacuum chamber 13. At the same time, the first connection hole 21 and the second connection hole 22 are respectively installed with sealing rings 23, and the opposite sides of the sealing rings 23 are pressed against the pneumatic joints 33 and the stage body 10 respectively, to ensure good air tightness between the pneumatic joints 33 and the first sealed chamber or the second sealed chamber.
[0092] In one embodiment, the sealing ring 23 can be installed by opening a sealing groove corresponding to its structure at the bottom of the carrier, so that the sealing ring 23 can be stably set in the sealing groove. Under further squeezing by the pneumatic joint 33, the pneumatic joint 33 and the corresponding vacuum chamber form a good sealing fit.
[0093] In addition to providing the wafer adsorption stage of any one of the above-mentioned embodiments, the utility model also provides a film expansion device, which adopts the wafer adsorption stage mentioned in any one of the above-mentioned embodiments.
[0094] In summary, by adopting the wafer adsorption platform, the film expansion equipment can enable the corresponding product to maintain a high stability during the process of crystal expansion, film expansion and subsequent heating and shrinking, avoiding the problem of wafer film shrinkage after crystal expansion and film expansion, so that the peripheral wafer film can be heated and shrunk stably, meeting subsequent process requirements, and improving the yield rate and product manufacturing efficiency.
[0095] In the description of this article, it should be understood that the terms "upper", "lower", "left", "right", etc., and other directions or positional relationships are only for the convenience of description and simplification of operation, and do not indicate or imply that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore cannot be understood as a limitation of the present invention. In addition, the terms "first" and "second" are only used to distinguish in the description and have no special meaning.
[0096] In the description of this specification, the description with reference to the terms "an embodiment", "example", etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the utility model. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example.
[0097] In addition, it should be understood that although this specification is described according to implementation methods, not every implementation method contains only one independent technical solution. This narrative method of the specification is only for the sake of clarity. Those skilled in the art should regard the specification as a whole. The technical solutions in each embodiment may also be appropriately combined to form other implementation methods that can be understood by those skilled in the art.
[0098] The technical principle of the present invention is described above in combination with specific embodiments. These descriptions are only for explaining the principle of the present invention and cannot be interpreted as limiting the protection scope of the present invention in any way. Based on the explanations here, technicians in this field can think of other specific implementation methods of the present invention without creative work, and these methods will fall within the protection scope of the present invention.
Claims
1. A wafer adsorption carrier, characterized in that: include: A carrier body (10), wherein a central adsorption area (111) and an edge adsorption area (112) surrounding the central adsorption area (111) are formed on the carrier body (10), a central adsorption portion (1111) is provided on the central adsorption area (111), and edge adsorption portions (1121) connected end to end are provided on the edge adsorption area (112); The carrier body (10) is provided with a first vacuum chamber (12) and a second vacuum chamber (13) which are independent of each other. One end of the first vacuum chamber (12) and the second vacuum chamber (13) are used to connect to two independent external vacuum sources respectively. The other end of the first vacuum chamber (12) is connected to the central adsorption part (1111), and the other end of the second vacuum chamber (13) is connected to the edge adsorption part (1121).
2. The wafer adsorption stage according to claim 1, characterized in that: The central adsorption portion (1111) is a plurality of vacuum micropores uniformly distributed in the central adsorption area (111).
3. The wafer adsorption stage according to claim 1, wherein: The carrier body (10) is located in the central adsorption area (111) and is provided with a microporous ceramic carrier (14). The central adsorption portion (1111) is a vacuum micropore evenly distributed on the microporous ceramic carrier (14).
4. The wafer adsorption stage according to claim 1, wherein: The edge adsorption portion (1121) is an annular adsorption groove.
5. The wafer adsorption stage according to claim 4, characterized in that: In the cross-sectional direction of the adsorption tank, the tank wall of the adsorption tank is in an arc shape.
6. The wafer adsorption stage according to claim 1, characterized in that: The second vacuum chamber (13) comprises: A gas-uniform chamber (131) for connecting to one of the external vacuum sources; The vacuum channels (132) are multiple, and the multiple vacuum channels (132) are radially arranged around the uniform air cavity (131) at intervals, and the opposite ends of each vacuum channel (132) are respectively connected to the uniform air cavity (131) and the edge adsorption portion (1121).
7. The wafer adsorption stage according to any one of claims 1 to 6, characterized in that: Also includes: A first heating component (20) is arranged at the bottom or inside of the carrier body (10) and is used to heat the carrier body (10).
8. The wafer adsorption stage according to claim 7, characterized in that: Also includes: A support base (30) is mounted on the bottom of the carrier body (10) and is sealed with the carrier body (10); When the first heating component (20) is arranged at the bottom of the carrier body (10), the first heating component (20) is arranged between the carrier body (10) and the supporting base (30).
9. The wafer adsorption stage according to claim 8, characterized in that: The support base (30) is provided with a first vacuum hole (31) and a second vacuum hole (32); the first heating component (20) is provided with a first connecting hole (21) and a second connecting hole (22); the first vacuum hole (31) and the first connecting hole (21) are correspondingly connected to the first vacuum chamber (12); the second vacuum hole (32) and the second connecting hole (22) are correspondingly connected to the second vacuum chamber (13); The first vacuum hole (31) and the second vacuum hole (32) are respectively installed with a pneumatic connector (33), and the two pneumatic connectors (33) are used to connect to two independent external vacuum sources respectively; The first connecting hole (21) and the second connecting hole (22) are respectively installed with sealing rings (23), and opposite sides of the sealing rings (23) are respectively pressed against the pneumatic joint (33) and the carrier body (10).
10. A film expansion device, characterized in that: include: The wafer adsorption platform according to any one of claims 1 to 9.
Citation Information
Cited By
Crimping platform deck capable of being controlled in partition mode
CN120614799A
Wafer processing operation table and wafer edge crystal grain stripping device
CN122069969A