Flexible packaging structure and electronic device using same

By arranging organic and inorganic protective layers on the glass substrate, the problem that the flexible packaging structure is easily eroded by oxygen and moisture after long-term use is solved, excellent anti-oxygen and anti-moisture properties are achieved, and the life of the electronic device is extended. service life.

CN221930603UActive Publication Date: 2024-10-29AOHENG TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323454411.1
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-18
Publication Date
2024-10-29
Estimated Expiration
2033-12-18

AI Technical Summary

Technical Problem

Existing flexible packaging structures are easily eroded by moisture and oxygen in the air after being bent or used for a long time, resulting in shortened service life of electronic devices.

Method used

Use a glass substrate as the core material with a thickness of less than 210 μm, and set organic and inorganic protective layers on it, including a first protective layer covering the light-emitting element and a second protective layer covering the side surface of the glass substrate to improve oxygen resistance and moisture resistance. Qi ability.

Benefits of technology

It effectively avoids the degradation of optoelectronic components caused by oxygen and moisture, maintains the flexibility of the packaging structure, and extends the service life of electronic devices.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221930603U_ABST
    Figure CN221930603U_ABST
Patent Text Reader

Abstract

The utility model discloses a flexible packaging structure and an electronic device using the same. The flexible packaging structure comprises a glass substrate, a light-emitting element and a first protection layer. The glass substrate has a thickness of less than 210 [mu] m. The light-emitting element is disposed on the glass substrate. The first protective layer is disposed on the glass substrate and covers the light-emitting element. According to the flexible packaging structure and the electronic device using the flexible packaging structure, the oxygen and moisture resistance of the flexible packaging structure and the electronic device using the flexible packaging structure can be improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to a packaging structure and an electronic device using the same, in particular to a flexible packaging structure and an electronic device using the same. Background Art

[0002] With the diversified development of electronic consumer products, packaging structures often need to be bent to meet the diverse needs of users. In order to achieve a thin and light user experience, existing packaging structures generally use thin film packaging to form a protective layer to block moisture, oxygen and other pollutants. However, after being bent or used for a long time, the existing packaging materials still have the defect of being easily corroded by moisture, oxygen and pollutants in the air.

[0003] Therefore, how to improve the oxygen and moisture resistance of the flexible packaging structure through structural design improvement to overcome the above-mentioned defects and extend the service life of the electronic device has become one of the important issues that this industry wants to solve. Utility Model Content

[0004] The technical problem to be solved by the utility model is to provide a flexible packaging structure and an electronic device using the same, so as to enhance the ability of the flexible packaging structure to resist oxygen and moisture.

[0005] In order to solve the above technical problems, the utility model provides a flexible packaging structure, which includes: a glass substrate, a light-emitting element and a first protective layer, the glass substrate has a thickness less than 210μm, the light-emitting element is arranged on the glass substrate, and the first protective layer is arranged on the glass substrate and covers the light-emitting element.

[0006] Furthermore, the glass substrate is lime glass, boron glass, lead glass, aluminum glass or quartz glass.

[0007] Furthermore, the glass substrate has a thickness of 190 to 210 μm.

[0008] Furthermore, the light emitting element is a light emitting diode, a liquid crystal display, a quantum dot television or a solar cell.

[0009] Furthermore, the flexible packaging structure further includes a second protective layer, and the second protective layer covers the first protective layer and the side surface of the glass substrate.

[0010] Furthermore, the first protective layer is an organic protective layer, and the second protective layer is an inorganic protective layer.

[0011] Furthermore, the second protective layer is aluminum oxide, zinc oxide, zirconium oxide, silicon oxide or hafnium oxide.

[0012] Furthermore, the first protective layer is polyvinyl alcohol, vinyl butyral-vinyl alcohol-vinyl acetate copolymer or hydroxyethyl methacrylate and methyl methacrylate copolymer.

[0013] In order to solve the above-mentioned technical problems, the utility model also provides an electronic device, which includes: a flexible packaging module, the flexible packaging module includes: a glass substrate, a plurality of light-emitting elements and a first protective layer, the glass substrate has a thickness of less than 210 μm, the plurality of light-emitting elements are arranged on the glass substrate, and the first protective layer is arranged on the glass substrate and covers the plurality of light-emitting elements.

[0014] Furthermore, the electronic device is a display screen or a smart watch.

[0015] One of the beneficial effects of the utility model is that the flexible packaging structure and the electronic device using the same provided by the utility model can avoid the degradation of the optoelectronic elements caused by oxygen and moisture in the air and maintain the flexibility of the packaging structure through the technical solutions of "a first protective layer is arranged on the glass substrate and covers the light-emitting element" and "the thickness of the glass substrate is less than 210μm".

[0016] In addition, the present invention uses a glass substrate instead of a plastic polymer substrate, so that the flexible packaging structure has excellent oxygen and moisture resistance. The flexible packaging module made by the flexible packaging structure of the present invention is advantageously applied to various electronic devices that require flexibility and increases the service life of the electronic devices.

[0017] In order to further understand the features and technical contents of the present invention, please refer to the following detailed description and drawings of the present invention. However, the drawings provided are only for reference and description and are not intended to limit the present invention. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] Figure 1 It is a schematic diagram of a flexible packaging structure according to the first embodiment of the utility model.

[0019] Figure 2 This is a schematic diagram of the flexible packaging module of the second embodiment of the present invention in use without being bent.

[0020] Figure 3 It is a schematic diagram of the flexible packaging module of the third embodiment of the utility model being bent downward.

[0021] Figure 4 It is a schematic diagram of the flexible packaging module of the fourth embodiment of the utility model being bent upward.

[0022] Figure 5 It is a schematic diagram of an electronic device according to a fifth embodiment of the present invention.

[0023] Figure 6 It is a schematic diagram of an electronic device according to a sixth embodiment of the present invention.

[0024] Figure 7 It is a schematic diagram of a flexible packaging structure according to the seventh embodiment of the present utility model.

[0025] Figure numerals: 100A, 100B: flexible packaging structure; 101: substrate; 102: light-emitting element; 103: first protective layer; 104: second protective layer; 200: display screen; 300: smart watch; M1-M3: modules. DETAILED DESCRIPTION

[0026] The following is an explanation of the implementation methods of the "flexible packaging structure and the electronic device using the same" disclosed in the present utility model through specific examples. Those skilled in the art can understand the advantages and effects of the present utility model from the contents disclosed in this specification. The present utility model can be implemented or applied through other different specific embodiments, and the details in this specification can also be modified and changed based on different viewpoints and applications without departing from the concept of the present utility model. In addition, the drawings of the present utility model are only simple schematic illustrations and are not depicted according to actual dimensions. It is stated in advance. The following implementation methods will further explain the relevant technical contents of the present utility model in detail, but the disclosed contents are not intended to limit the scope of protection of the present utility model.

[0027] It should be understood that, although the terms "first", "second", "third", etc. may be used herein to describe various elements, these elements should not be limited by these terms. These terms are mainly used to distinguish one element from another element. In addition, the term "or" used herein may include any one or more combinations of the associated listed items depending on the actual situation.

[0028] First embodiment

[0029] See also Figure 1 , is a schematic diagram of the flexible packaging structure of the first embodiment of the utility model. Figure 1 As shown, the flexible packaging structure 100A includes a glass substrate 101, and the glass substrate can be lime glass, boron glass, lead glass, aluminum glass or quartz glass. However, the present invention is not limited to the above examples. Since the glass substrate 101 has poor flexibility when the thickness is greater than 210 μm, especially when the thickness of the glass substrate 101 is 0.7 to 1 mm, it has no flexibility. Therefore, the glass substrate 101 of the present invention can have a thickness of less than 210 μm. Preferably, the thickness of the glass substrate 101 of the present invention can be 190 to 210 μm.

[0030] The flexible packaging structure 100A further includes a light emitting element 102 that can convert light energy into electrical energy. For example, the light emitting element 102 can be a light emitting diode (LED), a liquid crystal display (LCD), a quantum dot television (OLED) or a solar cell. In the flexible packaging structure 100A, the light emitting element 102 is disposed on the glass substrate 101.

[0031] Furthermore, when manufacturing the flexible packaging structure 100A of the present invention, in order to make the glass substrate 101 flexible, a backside thinning process may be performed after the light emitting element 102 is disposed on the glass substrate 101 to adjust the thickness of the glass substrate 101 to less than 210 μm.

[0032] In this embodiment, the flexible packaging structure 100A further includes a first protective layer 103. The first protective layer 103 is also disposed on the glass substrate 101 and covers the light emitting element 102 to prevent the light emitting element 102 from being corroded by moisture, oxygen and dirt. In other words, the first protective layer 103 can be in contact with the light emitting element 102 and the supporting surface of the glass substrate 101. For example, the first protective layer 103 can encapsulate the light emitting element 102 by a coating method.

[0033] Furthermore, the first protective layer 103 may be an organic protective layer formed by polymerizing an organic polymer containing a hydrophilic group, so that the surface of the first protective layer 103 has a hydrophilic functional group such as a hydroxyl group or a carboxylic acid group. For example, the first protective layer 103 may be polyvinyl alcohol (PVA), polyacrylic acid (Polyacrylate), polyvinyl butyral (PVB), polyhydroxyethylmethacrylate (pHEMA). However, the present invention is not limited to the above examples.

[0034] In addition, a monomer without a hydrophilic group may be copolymerized with the above-mentioned monomer with a hydrophilic group to form the first protective layer 103. Preferably, the molar ratio of the monomer with a hydrophilic group to the monomer without a hydrophilic group may be 50:50. If the molar ratio of the monomer with a hydrophilic group is less than the molar ratio of the monomer without a hydrophilic group, it will not help the atomic layer deposition film nucleation growth.

[0035] For example, monomers that still have a hydrophilic group after forming a polymer may be vinyl alcohol, vinyl butyral, or hydroxyethyl methacrylate (HEMA). Monomers that do not have a hydrophilic group after forming a polymer may be ethylene, propylene, butene, vinyl chloride, isoprene, styrene, imide, methyl methacrylate (MMA), and vinyl acetate. However, the present invention is not limited to the above examples.

[0036] In this embodiment, the first protective layer 103 may be polyvinyl alcohol (PVA), vinyl butyral-vinyl alcohol-vinyl acetate copolymer, or hydroxyethyl methacrylate (HEMA) and methyl methacrylate (MMA) copolymer. Preferably, the first protective layer 103 may be a copolymer of HEMA and MMA, wherein the molar ratio of the monomer containing a hydrophilic group (HEMA) to the monomer containing no hydrophilic group (MMA) is greater than 50:50.

[0037] It should be noted that if the thickness of the first protective layer 103 is less than 1 μm, the first protective layer 103 will not be able to effectively cover the glass substrate 101 and affect the quality of the subsequent growth of the organic encapsulation layer film. If the thickness of the first protective layer 103 is greater than 20 μm, the light transmittance will decrease. Therefore, the thickness of the first protective layer 103 of the present invention is preferably between 1 μm and 20 μm.

[0038] Second embodiment

[0039] See also Figure 2 , which is a schematic diagram of the flexible packaging module M1 of the second embodiment of the utility model in an unbent state. The flexible packaging structure 100A of the first embodiment of the utility model can also form a flexible packaging module M1. Different from the flexible packaging structure 100A, the flexible packaging module M1 is to set a plurality of light-emitting elements 102 on the same glass substrate 101, and then encapsulate the plurality of light-emitting elements 102 with a first protective layer 103. In this embodiment, the flexible packaging module M1 can be used in an unbent state.

[0040] Third embodiment

[0041] See also Figure 3, is a schematic diagram of the flexible packaging module M2 of the third embodiment of the utility model being bent downward. The flexible packaging module M2 also has a structure in which multiple light-emitting elements 102 are arranged on the same glass substrate 101, and then the multiple light-emitting elements 102 are encapsulated with a first protective layer 103. Moreover, the flexible packaging module M2 can be used in a state in which it is bent downward.

[0042] Fourth embodiment

[0043] See also Figure 4 , is a schematic diagram of the use of the flexible packaging module M3 of the fourth embodiment of the utility model when it is bent upward. The flexible packaging module M3 also has a structure in which multiple light-emitting elements 102 are arranged on the same glass substrate 101, and then the multiple light-emitting elements 102 are encapsulated with a first protective layer 103. In addition, the flexible packaging module M3 can be used in a state in which it is bent upward.

[0044] Fifth embodiment

[0045] Figure 5 FIG. 5 is a schematic diagram of an electronic device according to a fifth embodiment of the present utility model. Figure 5 As shown, the electronic device may be a display screen 200. The display screen 200 has a plurality of flexible packaging modules M2 described in the aforementioned embodiments. Specifically, the display screen 200 may be any product or component with a display function, such as an OLED display device with a curved surface, a QLED display device, an electronic paper, a tablet computer, a television, a monitor, a notebook computer, a digital photo frame, a navigator, or the like.

[0046] Sixth embodiment

[0047] Figure 6 FIG. 6 is a schematic diagram of an electronic device according to a sixth embodiment of the present invention. Figure 6 As shown, the electronic device may be a portable electronic device. For example, the electronic device may be a smart watch 300. The display surface of the smart watch 300 may have a plurality of flexible packaging modules M3 described in the aforementioned embodiments. Since the flexible packaging module M3 may be used in a bent state, the surface of the smart watch may have a curved arc, so that the user may have a more comfortable experience when wearing it.

[0048] Seventh embodiment

[0049] See also Figure 7 , is a schematic diagram of the flexible packaging structure of the seventh embodiment of the utility model. Figure 7As shown, the flexible packaging structure 100B may further include a second protective layer 104. The second protective layer 104 may be coated on the first protective layer 103 after the first protective layer 103 is formed to cover the first protective layer 103 and the side surface of the glass substrate 101. Accordingly, the side surface of the glass substrate 101 and the light emitting element 102 may be further protected.

[0050] The second protective layer 104 may be an inorganic encapsulation layer. Specifically, the material of the second protective layer 104 may be aluminum oxide, zinc oxide, zirconium oxide, silicon oxide or hafnium oxide. However, the second protective layer 104 may also be formed of multiple layers of materials arranged alternately, such as aluminum oxide / zirconium oxide. The present invention is not limited to the above examples.

[0051] In addition, the thickness of the second protective layer 104 may be between 5 nm and 100 nm. If the thickness of the second protective layer 104 is less than 5 nm, it cannot effectively prevent moisture or other contaminants from damaging the light emitting element 102. If the thickness of the second protective layer 104 is greater than 100 nm, the light transmittance and flexibility of the flexible packaging structure 100B will be reduced.

[0052] In an embodiment, the second protective layer 104 can also be formed on the first encapsulation layer 103 by atomic layer deposition. Further, the atomic layer deposition method uses the pulsation generated by the precursor gas or the heated vapor to grow a thin film layer by layer on the surface of the substrate to be deposited. In the present invention, the process temperature of the atomic layer deposition method can be between 50°C and 120°C. If the temperature of the atomic layer deposition method is lower than 50°C, the time required to form the second protective layer 104 will be prolonged. If the temperature of the atomic layer deposition method is higher than 120°C, it will cause damage to the first protective layer 103 and even the light-emitting element 102.

[0053] Specifically, the atomic layer deposition method may include a first step, a second step, and a third step. In the first step, argon gas is used to send the heated vapor of trimethylaluminum into the reaction chamber, and the trimethylaluminum reacts with the hydroxyl groups on the surface of the first protective layer 103 as follows: -(OH) n +nAl(CH3)3→Surface of organic encapsulation layer -(O-Al(CH3)2*) n +nCH4 (Formula 1).

[0054] In the second step, the reaction chamber is purged with non-reactive gases such as Ar or N2 to remove excess trimethylaluminum and the byproduct methane of the reaction. Then, H2O as an oxidizing source is introduced into the reaction chamber to perform the following reaction: organic encapsulation layer surface -(O-Al(CH3)2*)n+2nH2O→organic encapsulation layer surface -(O-Al-(OH)2*) n +2nCH4 (Formula 2).

[0055] In the third step, the reaction chamber is purged with a non-reactive gas such as Ar or N2 to remove excess moisture and byproduct methane. The reaction of the above formula 1 and formula 2 and the two cleaning steps are called an ALD cycle, which can be repeated until a second protective layer 104 of sufficient thickness is formed.

[0056] For example, the second protective layer 104 may be a dense nano-scale structure to avoid affecting the flexibility of the flexible packaging structure 100B. Preferably, the glass substrate 101, the light emitting element 102, the first protective layer 103 and the second protective layer 104 of the flexible packaging structure 100B are all flexible.

[0057] Advantageous Effects of Embodiments

[0058] One of the beneficial effects of the present invention is that the flexible packaging structure and the electronic device using the same provided by the present invention can avoid the degradation of the optoelectronic element caused by oxygen and moisture in the air and maintain the flexibility of the packaging structure through the technical solutions of "a first protective layer is arranged on the glass substrate and covers the light-emitting element" and "the thickness of the glass substrate is less than 210μm".

[0059] In addition, the present invention uses a glass substrate instead of a plastic polymer substrate, so that the flexible packaging structure has excellent oxygen and moisture resistance. The flexible packaging module made by the flexible packaging structure of the present invention is advantageously applied to various electronic devices that require flexibility and increases the service life of the electronic devices.

[0060] The contents disclosed above are only preferred feasible embodiments of the present utility model, and are not intended to limit the protection scope of the claims of the present utility model. Therefore, all equivalent technical changes made using the contents of the present utility model specification and drawings are included in the protection scope of the claims of the present utility model.

Claims

1. A flexible packaging structure, characterized in that: The flexible packaging structure comprises: A glass substrate having a thickness of less than 210 μm; a light emitting element, wherein the light emitting element is disposed on the glass substrate; and A first protective layer is disposed on the glass substrate and covers the light emitting element.

2. The flexible packaging structure according to claim 1, characterized in that: The glass substrate is lime glass, boron glass, lead glass, aluminum glass or quartz glass.

3. The flexible packaging structure according to claim 1, characterized in that: The glass substrate has a thickness of 190 to 210 μm.

4. The flexible packaging structure according to claim 1, characterized in that: The light emitting element is a light emitting diode, a liquid crystal display, a quantum dot television or a solar cell.

5. The flexible packaging structure according to claim 1, characterized in that: The flexible packaging structure further includes a second protective layer, and the second protective layer covers the first protective layer and the side surface of the glass substrate.

6. The flexible packaging structure according to claim 5, characterized in that: The first protective layer is an organic protective layer, and the second protective layer is an inorganic protective layer.

7. The flexible packaging structure according to claim 5, characterized in that: The second protective layer is aluminum oxide, zinc oxide, zirconium oxide, silicon oxide or hafnium oxide.

8. The flexible packaging structure according to claim 1, characterized in that: The first protective layer is polyvinyl alcohol, vinyl butyral-vinyl alcohol-vinyl acetate copolymer or hydroxyethyl methacrylate and methyl methacrylate copolymer.

9. An electronic device, characterized in that: The electronic device comprises: A flexible packaging module, the flexible packaging module comprising: A glass substrate having a thickness of less than 210 μm; A plurality of light emitting elements, wherein the plurality of light emitting elements are disposed on the glass substrate; and The first protective layer is disposed on the glass substrate and covers the plurality of light emitting elements.

10. The electronic device according to claim 9, characterized in that: The electronic device is a display screen or a smart watch.