Polycrystalline silicon deposition carrier silicon core bridging device and reduction furnace
By increasing the cross-sectional area of the silicon core cross-beam in polysilicon production to reduce resistance and magnetic flux density, the problem of deep crack cauliflower coral material in the radiation area of the silicon core is solved, and product quality and production efficiency are improved.
Patent Information
- Application Number
- CN202322925865.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-10-31
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2033-10-31
AI Technical Summary
In the existing polycrystalline silicon production process, the deep crack cauliflower coral material in the silicon core cross beam and the silicon core radiation area is serious, affecting product quality and production efficiency.
Design a polycrystalline silicon deposition carrier silicon core bridge device. By setting electrodes on the chassis of the reduction furnace and installing a silicon core vertically, the cross-sectional area of the silicon core beam is increased to reduce resistance and magnetic flux density, thereby controlling the temperature field and heat of the reduction furnace radiation.
It effectively reduces the chemical vapor deposition temperature of polycrystalline silicon rods, increases the deposition area and speed, reduces deep cracks, and improves product quality and inventory management.
Smart Images

Figure CN221940149U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the field of polysilicon production, in particular to a polysilicon deposition carrier silicon core bridging device. Background Art
[0002] Polysilicon is the basic material for the photovoltaic and microelectronics industries. The main application areas of single crystal silicon produced using polysilicon as raw material include contemporary artificial intelligence, automatic control, information processing, photoelectric conversion and other semiconductor devices.
[0003] Polysilicon is produced by using the mainstream process of modified Siemens chemical vapor deposition. Trichlorosilane and hydrogen are used to obtain energy on the surface of the heat carrier to produce a hydrogen reduction reaction. As the hydrogen reduction reaction runs for 80-120 hours, the diameter of the silicon core gradually grows to 100-200mm. The energy supply is the silicon core that is self-heated to a temperature of 950-1150℃ as the deposition carrier. The product grade of polysilicon after it comes out of the furnace is based on the technical indicators of solar-grade polysilicon GB / T 25074-2017, and the requirements of users on the surface quality of polysilicon are becoming more and more stringent.
[0004] In the existing technology, the silicon core beam and the silicon core radiation area within 0.5m below the silicon core beam have a serious phenomenon of deep cracks. If the proportion of cauliflower coral material exceeds 70%, it will directly drag down the inventory and cash flow of the production enterprise. Summary of the invention
[0005] In order to solve the above technical problems, the purpose of the utility model is to provide a polysilicon deposition carrier silicon core bridging device that can obtain a dense deposition morphology and increase the proportion of high-dense materials.
[0006] In order to achieve the above-mentioned purpose, the technical solution of the utility model is: a polysilicon deposition carrier silicon core bridging device, comprising a group of two electrodes arranged on the bottom plate of the reduction furnace, on which silicon cores are vertically mounted, and a silicon core cross beam is arranged on the top of the two silicon cores. When the unit length is the same, the surface area of the silicon core cross beam is 10%-100% more than the surface area of the silicon core.
[0007] In the above technical solution, according to R (resistance) = ρ (resistivity) L (length) / S (cross-sectional area), increasing the cross-sectional area can reduce the resistance. According to Joule quantitative Q = I2Rt, when the silicon core and the silicon core beam are supplied with the same current, the larger the cross-sectional area, the lower the magnetic flux density per unit cross-sectional area, and the lower the surface temperature.
[0008] According to a preferred technical solution, a mounting hole is provided at each end of the silicon core cross beam, and the top end of the silicon core is mounted in the mounting hole.
[0009] According to a preferred technical solution, the distance between the two silicon cores is 250-300 mm.
[0010] According to a preferred technical solution, the cross section of the silicon core is circular or square, and the diameter of the cross section of the silicon core or the diameter of the inscribed circle is 10-30 mm.
[0011] According to a preferred technical solution, the cross section of the silicon core beam is circular or rectangular, and the diameter of the cross section of the silicon core or the diameter of the inscribed circle is 10-50 mm.
[0012] According to a preferred technical solution, the length of the silicon core is 2500-3000 mm.
[0013] A reduction furnace uses the polysilicon deposition carrier silicon core bridging device.
[0014] The working principle of this utility model:
[0015] After the polysilicon deposition carrier silicon core bridge device is built, when the electrode starts to be energized, since the cross-sectional area of the silicon core beam is larger than the cross-sectional area of the silicon core, the resistance of the silicon core beam of the same length unit is less than the resistance of the silicon core. The current passing through is the same, the magnetic flux density of the silicon core beam is lower than the magnetic flux density of the silicon core, and the surface temperature of the silicon core beam is lower than the surface temperature of the silicon core, which can effectively control the temperature field at the top of the reduction furnace and the thermal radiation within 0.5m under the silicon core beam. Thereby increasing the proportion of dense materials after the polysilicon rods are taken out of the furnace, and reducing the phenomenon of deep cracks in the silicon core radiation area within 0.5m under the silicon core beam and the silicon core beam.
[0016] The advantages of the utility model are:
[0017] 1. The utility model can reduce the chemical vapor deposition temperature of the polysilicon rod silicon core bridge part, increase the deposition area, optimize the deposition speed, and reduce the unit consumption;
[0018] 2. The utility model can alleviate the problem of deep cracks in the cauliflower coral material in the crossbeam and the silicon core radiation area within 0.5m below the crossbeam that has troubled the industry;
[0019] 3. The utility model can obtain a relatively easy-to-control temperature field at the top of the reduction furnace and the heat radiation within a range of 0.5m under the beam between the two silicon cores, thereby increasing the proportion of dense materials after the polysilicon rods are taken out of the furnace, improving the product quality grade, and optimizing inventory. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] In order to more clearly illustrate the technical solutions of the embodiments of the utility model, the drawings required for use in the description of the embodiments will be briefly introduced below. The drawings described below are only some embodiments of the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0021] The utility model is further described below in conjunction with the accompanying drawings and embodiments:
[0022] Figure 1 It is a schematic diagram of the structure of the utility model;
[0023] Figure 2 This is a top view of the silicon core beam of Example 1;
[0024] Figure 3 This is a cross-sectional view of the silicon core beam of Example 1;
[0025] Figure 4 Schematic diagram of silicon core and silicon core beam assembly.
[0026] Wherein: 1. reduction furnace; 100. electrode; 110. silicon core; 120. silicon core beam; 130. chassis. DETAILED DESCRIPTION
[0027] Embodiment 1:
[0028] like Figure 1 As shown, a polysilicon deposition carrier silicon core bridging device includes a group of two electrodes 100 arranged on the bottom plate 130 of the reduction furnace 1, and silicon cores 110 are vertically installed on the electrodes 100. A silicon core cross beam 120 is arranged on the top of the two silicon cores 110. When the unit length is the same, the surface area of the silicon core cross beam 120 is 33% more than the surface area of the silicon core 110.
[0029] like Figure 4 As shown, a mounting hole is provided at each end of the silicon core beam 120, and the top end of the silicon core 110 is mounted in the mounting hole.
[0030] The distance between the two silicon cores 110 is 255 mm.
[0031] The cross section of the silicon core 110 is a square, and the side length of the cross section of the silicon core 110 is 15 mm.
[0032] like Figure 2 , 3 As shown, the cross section of the silicon core beam 120 is rectangular, and the length of the cross section of the silicon core is 20 mm and the width is 15 mm.
[0033] Embodiment 2:
[0034] A polysilicon deposition carrier silicon core bridging device includes a group of two electrodes 100 arranged on a bottom plate 130 of a reduction furnace 1, silicon cores 110 are vertically mounted on the electrodes 100, and a silicon core cross beam 120 is arranged on the top of the two silicon cores 110. When the unit length is the same, the surface area of the silicon core cross beam 120 is 44% greater than the surface area of the silicon core 110.
[0035] A mounting hole is provided at each end of the silicon core beam 120, and the top end of the silicon core 110 is mounted in the mounting hole.
[0036] The distance between the two silicon cores 110 is 255 mm.
[0037] The cross section of the silicon core 110 is circular, and the diameter of the cross section of the silicon core 110 is 15 mm.
[0038] The cross section of the silicon core beam 120 is circular, and the diameter of the cross section of the silicon core is 18 mm.
[0039] Embodiment 3:
[0040] A polysilicon deposition carrier silicon core bridging device includes a group of two electrodes 100 arranged on a bottom plate 130 of a reduction furnace 1, silicon cores 110 are vertically mounted on the electrodes 100, a silicon core 110 cross beam is arranged on the top of the two silicon cores 110, and at the same unit length, the surface area of the silicon core cross beam 120 is 83% more than the surface area of the silicon core 110.
[0041] A mounting hole is provided at each end of the silicon core beam 120, and the top end of the silicon core 110 is mounted in the mounting hole.
[0042] The distance between the two silicon cores 110 is 255 mm.
[0043] The cross section of the silicon core 110 is circular, and the diameter of the cross section of the silicon core 110 is 15 mm.
[0044] The cross section of the silicon core beam 120 is a square, and the side length of the cross section of the silicon core 110 is 18 mm.
[0045] Embodiment 4:
[0046] A polysilicon deposition carrier silicon core bridging device includes a group of two electrodes 100 arranged on a bottom plate 130 of a reduction furnace 1, silicon cores 110 are vertically mounted on the electrodes 100, and a silicon core cross beam 120 is arranged on the top of the two silicon cores 110. When the unit length is the same, the surface area of the silicon core cross beam 120 is 20% more than the surface area of the silicon core 110.
[0047] A mounting hole is provided at each end of the silicon core beam 120, and the top end of the silicon core 110 is mounted in the mounting hole.
[0048] The distance between the two silicon cores 110 is 255 mm.
[0049] The cross section of the silicon core 110 is a square, and the side length of the cross section of the silicon core 110 is 15 mm.
[0050] The cross section of the silicon core beam 120 is rectangular, and the length and width of the cross section of the silicon core are 18 mm and 15 mm respectively.
[0051] This embodiment closely follows the market orientation, increases the proportion of high-purity and dense polysilicon materials, optimizes the deposition speed, and reduces energy consumption. A relatively easy-to-control top temperature field in the reduction furnace 1 can be obtained, the chemical vapor deposition temperature and deposition area of the polysilicon rod silicon core bridging part can be optimized, and the phenomenon of cauliflower coral material with radial deep cracks in the silicon core within the range of 0.5m under the beam and the beam that troubles the industry can be alleviated, and the severe photovoltaic market development situation can be adapted to make steady progress.
Claims
1. A polysilicon deposition carrier silicon core bridging device, comprising a set of two electrodes arranged on the bottom plate of a reduction furnace, silicon cores are vertically mounted on the electrodes, and a silicon core cross beam is arranged on the top of the two silicon cores, characterized in that: At the same unit length, the surface area of the silicon core beam is 10%-100% greater than the surface area of the silicon core.
2. A polysilicon deposition carrier silicon core bridging device according to claim 1, characterized in that: A mounting hole is respectively arranged at both ends of the silicon core cross beam, and the top end of the silicon core is mounted in the mounting hole.
3. The polysilicon deposition carrier silicon core bridging device according to claim 1, characterized in that: The distance between the two silicon cores is 250-300 mm.
4. The polysilicon deposition carrier silicon core bridging device according to claim 1, characterized in that: The cross section of the silicon core is circular or square, and the diameter of the cross section or the diameter of the inscribed circle of the silicon core is 10-30 mm.
5. The polysilicon deposition carrier silicon core bridging device according to claim 1, characterized in that: The cross section of the silicon core beam is circular or rectangular, and the diameter of the cross section of the silicon core or the diameter of the inscribed circle is 10-50 mm.
6. The polysilicon deposition carrier silicon core bridging device according to claim 1, characterized in that: The length of the silicon core is 2500-3500 mm.
7. A reduction furnace, characterized in that: The polysilicon deposition carrier silicon core bridging device described in any one of claims 1 to 6 is used.