Extrusion die for crosslinked polyethylene wire sheath
By setting up a drainage part and an outer mold design hole and a projection at the inner die nozzle end of the crosslinked polyethylene wire sheath ejection mold, the slag accumulation problem during the extrusion pipe ejection process is solved, and the quality of the cable sheath layer is improved and processing efficiency.
Patent Information
- Application Number
- CN202420251280.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-02-01
- Publication Date
- 2024-11-05
- Estimated Expiration
- 2034-02-01
AI Technical Summary
The existing crosslinked polyethylene wire sheath is prone to slag accumulation on the inner die nozzle during the extrusion pipe extrusion process, resulting in the intermittent bulge of the wire and the wire diameter exceeding the tolerance standard, affecting product quality.
A cross-linked polyethylene wire sheathing mold is designed, and a flow channel is formed between the inner mold and the outer mold. A drainage part is arranged at the mouth to reduce the flow stress of the rubber, and a dark hole and an inner protrusion are arranged on the outside of the outer mold to Enhance the flow diversion capacity and prevent slag accumulation.
Through the design of the drainage part and the raised part, the flow stress of the rubber is reduced, the formation of slag accumulation is avoided, the quality of the cable sheath layer is improved, the processing process is simplified, and the debugging and scrapping is reduced.
Smart Images

Figure CN221953849U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of extrusion moulds, in particular to a cross-linked polyethylene wire sheath extrusion mould. Background Art
[0002] Cables are usually rope-like cables twisted together by several or several groups of wires (at least two wires in each group). Each group of wires is insulated from each other and often twisted around a center, and the entire outside is covered with a highly insulating cable sheath. It is often necessary to use rubber to wrap the wires. The common protective layer material is cross-linked polyethylene rubber. The rubber flows out from between the inner and outer molds and wraps around the outside of the semi-finished wires. For example, the Chinese patent publication number "CN216832125U" discloses a special extrusion mold for cross-linked polyethylene and modified polyphenylene ether wires, including coaxial and oppositely arranged inner and outer molds; the outer mold forms a trumpet-shaped opening at one end toward the inner mold.
[0003] At present, when cross-linked polyethylene wire sheaths are extruded by tube extrusion, slag will accumulate on the inner die nozzle. When the slag accumulates seriously, small pieces will be formed and carried between the semi-finished product and the sheath layer, causing intermittent bulging of the wires. The wire diameter is likely to exceed the upper tolerance standard, affecting the customer's processing and use. Utility Model Content
[0004] The utility model aims to solve the problem of slag accumulation on the inner die mouth in the prior art. When the slag accumulation is serious, small pieces will be formed and brought between the semi-finished product and the sheath layer, resulting in intermittent bulging of the wire. A cross-linked polyethylene wire sheath extrusion die is proposed to solve the problem that slag accumulation occurs on the inner die mouth in the prior art. When the slag accumulation is serious, small pieces will be brought between the semi-finished product and the sheath layer, resulting in intermittent bulging of the wire.
[0005] In order to achieve the above purpose, the utility model adopts the following technical solutions:
[0006] A cross-linked polyethylene wire sheath extrusion mold is designed, comprising an outer mold and an inner mold, wherein the inner mold is placed inside the outer mold, and a flow channel is formed between the inner mold and the outer mold;
[0007] The inner mold includes a connecting section, a conical portion and a mouth end, the end face of the outer mold has a conical mouth adapted to the conical portion, and a drainage portion is also provided at the tail end of the mouth end, and the drainage portion is used to reduce the flow stress of the rubber.
[0008] Furthermore, the drainage portion is a chamfered portion arranged on the tail end of the tapered portion.
[0009] Furthermore, the chamfer angle of the chamfered portion is 0.5°.
[0010] Furthermore, the length of the mouth end is 7mm-9mm, the thickness of the mouth end is 0.9mm-1.1mm, wherein the aperture of the tapered mouth tail end is larger than the outer diameter of the mouth end by 1.4mm-1.8mm.
[0011] Furthermore, a hidden hole communicating with the tapered opening is provided on the outer side of the outer mold.
[0012] Furthermore, a protrusion is provided on the inner side of the outer mold, and the protrusion has a guide plane, and the guide plane is vertically arranged with the nozzle end.
[0013] The utility model proposes a cross-linked polyethylene wire sheath extrusion die, which has the beneficial effect that: in the utility model, a drainage portion is added to the inner die mouth end, and the drainage portion is used to reduce the flow stress of the rubber material. When the flow stress of the rubber material is reduced, the flow is smoother, thereby avoiding the formation of slag accumulation on the mouth end, causing the slag accumulation to be converted into small pieces and brought between the wire semi-finished product and the sheath, causing bulging problems, greatly improving the quality of the cable sheath layer, the overall structural design is simple, and processing and production are convenient, while effectively meeting the processing requirements of wire materials and reducing debugging and scrapping. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] Figure 1 It is a structural schematic diagram of the utility model;
[0015] Figure 2 This is a schematic diagram of the drainage structure of the utility model;
[0016] Figure 3 It is a schematic diagram of the structure of the raised portion of the utility model.
[0017] In the figure: 1, outer mold; 11, conical mouth; 12, hidden hole; 13, raised part; 14, guide plane; 2, inner mold; 21, connecting section; 22, conical part; 23, mouth end; 24, drainage part. DETAILED DESCRIPTION
[0018] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all of the embodiments.
[0019] Reference Figure 1-3 An embodiment of the utility model discloses a cross-linked polyethylene wire sheath extrusion mold, comprising an outer mold 1 and an inner mold 2, wherein the inner mold 2 is placed inside the outer mold 1, and a flow channel is formed between the inner mold 2 and the outer mold 1. During operation, the semi-finished wire is passed through the inner mold 2, and the rubber is left along the gap between the outer mold 1 and the inner mold 2 to realize the extrusion of the semi-finished circuit sheath;
[0020] Among them, the inner mold 2 includes a connecting section 21, a tapered portion 22 and a mouth end 23. The end face of the outer mold 1 has a tapered mouth 11 adapted to the tapered portion 22. A drainage portion 24 is also provided at the tail end of the mouth end 23. The drainage portion 24 is used to reduce the flow stress of the rubber. When the flow stress of the rubber is reduced, the flow is smoother, thereby avoiding the formation of slag on the mouth end 23, causing the slag to turn into small pieces and be brought between the semi-finished wire and the sheath, resulting in bulging problems, which greatly improves the quality of the cable sheath layer.
[0021] On the basis of the above-mentioned embodiment, the drainage portion 24 in the present invention is a chamfered portion arranged on the rear end of the tapered portion 22 .
[0022] Specifically, the chamfer angle of the chamfered portion is 0.5°. The design of the chamfered portion is used to improve the flow ability of the rubber at the tail end of the mouth end 23, thereby preventing the rubber from being discharged quickly and smoothly and avoiding the problem of slag accumulation.
[0023] In addition, in the utility model, the length of the mouth end 23 is 7mm-9mm, and the thickness of the mouth end 23 is 0.9mm-1.1mm, wherein the aperture of the tail end of the tapered mouth 11 is larger than the outer diameter of the mouth end 23 by 1.4mm-1.8mm. By utilizing the structure of the tube extrusion die, the cross-linked polyethylene is evenly attached to the surface of the semi-finished wire, thereby preventing the occurrence of sheath bulging.
[0024] Furthermore, a hidden hole 12 connected to the tapered mouth 11 is provided on the outer side of the outer mold 1. The hidden hole 12 is used for guiding the rubber material along the hidden hole 12 and realizing elastic expansion after the sheath layer is extruded, and brushing the surface of the rubber material through the side wall of the hidden hole 12, thereby ensuring the surface of the sheath layer is smooth.
[0025] In some embodiments, in the embodiments of the utility model, a protrusion 13 is further provided on the inner side of the outer mold 1, and the protrusion 13 has a guide plane 14, and the guide plane 14 is perpendicular to the mouth end 23. Through the design of the protrusion 13, it is used to change the direction of part of the rubber material so that the rubber material can impact the chamfered part, thereby further improving the anti-slag accumulation ability of the mold and making it more durable.
[0026] The above description is only a preferred specific implementation manner of the present invention, but the protection scope of the present invention is not limited thereto. Any technician familiar with the technical field can make equivalent replacements or changes within the technical scope disclosed by the present invention according to the technical scheme and the utility model concept of the present invention, which should be covered by the protection scope of the present invention.
Claims
1. A cross-linked polyethylene wire sheath extrusion die, comprising an outer die (1) and an inner die (2), characterized in that: The inner mold (2) is placed inside the outer mold (1), and a flow channel is formed between the inner mold (2) and the outer mold (1); The inner mold (2) comprises a connecting section (21), a conical portion (22) and a mouth end (23); the end face of the outer mold (1) has a conical mouth (11) adapted to the conical portion (22); a drainage portion (24) is also provided at the tail end of the mouth end (23); the drainage portion (24) is used to reduce the flow stress of the rubber material.
2. A cross-linked polyethylene wire sheath extrusion die according to claim 1, characterized in that: The drainage portion (24) is a chamfered portion arranged on the tail end of the conical portion (22).
3. A cross-linked polyethylene wire sheath extrusion die according to claim 2, characterized in that: The chamfering angle of the chamfered portion is 0.5°.
4. A cross-linked polyethylene wire sheath extrusion die according to claim 2, characterized in that: The length of the mouth end (23) is 7mm-9mm, and the thickness of the mouth end (23) is 0.9mm-1.1mm, wherein the aperture of the tail end of the conical mouth (11) is larger than the outer diameter of the mouth end (23) by 1.4mm-1.8mm.
5. A cross-linked polyethylene wire sheath extrusion die according to claim 1, characterized in that: A hidden hole (12) communicating with the tapered opening (11) is provided on the outer side of the outer mold (1).
6. A cross-linked polyethylene wire sheath extrusion die according to claim 1, characterized in that: A raised portion (13) is also provided on the inner side of the outer mold (1), and the raised portion (13) has a flow guide plane (14), and the flow guide plane (14) is arranged perpendicular to the mouth end (23).