By designing a light steel keel structure and a prefabricated insulation integrated wall panel combining the outer and inner surface layers, the existing wall panels have solved the problems of large self-weight, many joints and large thermal bridges, and achieved efficient heat insulation and airtightness, simplifying The construction process meets the needs of green buildings.
Patent Information
- Application Number
- CN202420246958.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-01-31
- Publication Date
- 2024-11-05
- Estimated Expiration
- 2034-01-31
AI Technical Summary
The existing prefabricated wall panels have problems such as large self-weight, many joints, large thermal bridges, poor airtightness and waterproofness. After installation, the thermal insulation layer is required to be pasted on the facade, which is complicated.
Design a prefabricated insulation integrated wall panel, adopts a light steel keel structure, with an insulation layer inside, and is connected by longitudinal and transverse keels and edge seal keels, combining the outer and inner keels, and using wire mesh and cast layer to enhance the overall strength and waterproof performance to reduce cold bridge problems.
It improves the integrity and thermal insulation performance of the wall, shortens the construction cycle, reduces energy consumption, enhances building quality and indoor comfort, simplifies processes, and meets the requirements of green buildings.
Smart Images

Figure CN221957050U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of wall panels, in particular to an assembled thermal insulation integrated wall panel. Background Art
[0002] With the implementation of the "dual carbon" goals, energy conservation and emission reduction in the construction industry, green buildings are imminent, and prefabricated buildings are also regarded as a key industry for national sustainable development. The existing prefabricated wall panels mainly include ALC panels, light steel keel wall panels, and concrete prefabricated exterior wall panels, but the above wall panels all have problems such as heavy weight, many joints, large thermal bridges, poor air tightness and waterproofness, and poor wall panel integrity. At the same time, after the wall panels are installed, an insulation layer needs to be pasted on the exterior of the wall, and the process is complicated. Therefore, a utility model patent with patent number CN219671840U appeared, which discloses an assembled insulation integrated steel frame wall panel, including cylindrical columns arranged in pairs longitudinally, cylindrical connecting columns arranged horizontally between the columns, connecting pieces are arranged between the columns arranged in pairs, and the connecting pieces, columns and connecting columns are fixed to each other to form a skeleton structure, and filling materials are arranged inside the skeleton structure, and a covering layer is arranged on the outer side of the filling material.
[0003] With the continuous improvement of my country's building energy-saving standards, especially under the requirements of the "dual carbon" goals, in order to solve the above-mentioned technical problems, it is necessary to design more prefabricated thermal insulation walls that can be prefabricated in factories, installed on site, with good thermal insulation and airtightness, high indoor comfort and good integrity. Utility Model Content
[0004] In view of the deficiencies in the prior art, the utility model develops an assembled thermal insulation integrated wall panel, which has a short construction period, high building quality, good indoor comfort and low energy consumption, effectively improves the use effect of the wall panel, and is very consistent with the current development direction of my country's construction industry.
[0005] The technical solution of the utility model to solve the technical problem is: an assembled thermal insulation integrated wall panel, including a light steel keel, an insulation layer is arranged inside the light steel keel, an outer layer is arranged on one side of the light steel keel, and an inner layer is arranged on the other side of the light steel keel, the light steel keel includes a plurality of groups of longitudinal keels, a plurality of groups of transverse keels and edge-sealing keels, the longitudinal keels are connected to each other through a plurality of groups of transverse keels, and the edge-sealing keels are arranged at the top and bottom of the longitudinal keels.
[0006] As an optimization, the longitudinal keel includes two groups of long C-shaped steels arranged opposite to each other and several groups of first thermal break connectors for connecting the two groups of long C-shaped steels, and a gap is provided between the two groups of long C-shaped steels. By providing the long C-shaped steels, it can serve as the basis of the longitudinal keel and reduce the deadweight of the longitudinal keel; by providing the first thermal break connectors and a gap between the long C-shaped steels, it can avoid the two groups of long C-shaped steels from contacting each other, effectively solving the cold bridge problem.
[0007] As an optimization, the transverse keel includes two groups of short C-shaped steels arranged opposite to each other, and the ends of the short C-shaped steels are vertically connected to the side walls of the long C-shaped steels. By arranging the short C-shaped steels, a transverse keel can be formed to enhance the strength of the longitudinal keel, and the main frame of the light steel keel is formed after connecting the longitudinal keels.
[0008] As an optimization, the edge-sealed keel includes two groups of symmetrically arranged equilateral angle steels and several groups of second thermal break connectors for connecting the two groups of equilateral angle steels, and the equilateral angle steels are connected to the ends of the long C-shaped steels. By setting the equilateral angle steels, the ends of the long C-shaped steels can be edge-sealed, and with the second thermal break connectors, the connection strength of the ends of the longitudinal keels can be enhanced.
[0009] As an optimization, the first thermal break connector and the second thermal break connector are any one of an "X" shape, a "Z" shape, an "L" shape and a rectangle, which can enhance the overall strength of the light steel keel.
[0010] As an optimization, the outer layer includes an outer steel mesh and an outer pouring layer. The outer steel mesh is connected to one side of the light steel keel, and the outer pouring layer is arranged on the outer steel mesh. By setting the outer steel mesh, the coating effect of the outer pouring layer can be enhanced, so that the outer layer and the light steel keel form a whole to avoid falling off; by setting the outer pouring layer, the light steel keel and the insulation layer can be protected, the waterproof ability can be improved, the service life can be extended, and the wall insulation ability and air tightness can be further improved, and it has an aesthetic effect.
[0011] As an optimization, the inner surface layer includes an inner steel mesh and an inner pouring layer. The inner steel mesh is connected to the other side of the light steel keel, and the inner pouring layer is set on the inner steel mesh. By setting the inner steel mesh, the coating effect of the inner pouring layer can be enhanced, so that the inner surface layer and the light steel keel form a whole to avoid falling off; by setting the inner pouring layer, the light steel keel and the insulation layer can be protected in cooperation with the outer pouring layer, the waterproof ability can be improved, the service life can be extended, and the wall insulation ability and air tightness can be further improved, and the aesthetic effect can be achieved.
[0012] As an optimization, a reinforcement steel belt is also inclined on the light steel keel. By setting the reinforcement steel belt, the strength of the light steel keel can be further enhanced while ensuring that the thickness of the light steel keel meets the standard, and the light steel keel can be reinforced at the window and door opening position.
[0013] Compared with the prior art, the utility model has the following beneficial effects:
[0014] By setting up a light steel keel, the integrity of the wall can be greatly improved. It not only has a small self-weight but also has high-strength supporting capacity. It can carry the outer layer and the inner layer, which is conducive to factory prefabrication, shortens the construction period and is simple to construct. In addition, there is enough space inside the light steel keel to accommodate the insulation layer, which can improve the overall sound insulation and sound absorption and insulation capacity of the wall panel, integrate the wall and insulation, and solve the risk of falling off of the wall's external insulation; by setting up the insulation layer, the wall's thermal insulation performance and air tightness can be enhanced; by setting up the outer layer and the inner layer, the light steel keel and the insulation layer can be protected, and the waterproof performance can be improved. strength, prolong service life, and further improve the thermal insulation capacity and air tightness of the wall; by arranging longitudinal keels, transverse keels and edge-sealed keels, it can be beneficial to factory prefabrication, shorten the construction period, simplify the construction, and reduce the cost of construction, transportation and later structural seismic design; the utility model has a short construction period and high building quality, is convenient for mass production and on-site installation, has flexible layout and fast construction, can greatly improve construction efficiency, has good indoor comfort and low energy consumption, effectively improves the use effect of wall panels, meets the requirements of green assembly and is in line with the current development direction of my country's construction industry. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 This is a cross-sectional view of the internal structure of the first embodiment of the utility model.
[0016] Figure 2 It is a structural schematic diagram of the light steel keel in the first embodiment of the utility model.
[0017] Figure 3 It is a schematic structural diagram of a light steel keel and a reinforcing steel belt in the second embodiment of the utility model.
[0018] In the figure, 1, light steel keel; 2, insulation layer; 3, outer layer; 4, inner layer; 5, reinforcing steel belt;
[0019] 11. Long C-shaped steel; 12. First thermal break connector; 13. Short C-shaped steel; 14. Equilateral angle steel; 15. Second thermal break connector;
[0020] 31. External steel wire mesh; 32. External casting layer;
[0021] 41. Inner steel wire mesh; 42. Inner casting layer. DETAILED DESCRIPTION
[0022] In order to clearly illustrate the technical features of the present invention, the present invention is described in detail below through specific implementation methods and in conjunction with the accompanying drawings.
[0023] Example 1
[0024] Figure 1 to Figure 2 An embodiment of the present utility model is as follows: Figure 1 to Figure 2As shown, an assembled thermal insulation integrated wall panel includes a light steel keel 1, an insulation layer 2 is arranged inside the light steel keel 1, the insulation layer 2 adopts a lightweight thermal insulation material, the thickness of the insulation layer 2 is the same as the thickness of the light steel keel 1, an outer layer 3 is arranged on one side of the light steel keel 1, and an inner layer 4 is arranged on the other side of the light steel keel 1. The light steel keel 1 includes a plurality of groups of longitudinal keels, a plurality of groups of transverse keels and edge-sealing keels. The longitudinal keels are connected to each other through a plurality of groups of transverse keels, and the edge-sealing keels are arranged at the top and bottom of the longitudinal keels.
[0025] By setting the light steel keel 1, the integrity of the wall can be greatly improved. It not only has a small self-weight but also has high-strength supporting capacity. It can carry the outer layer 3 and the inner layer 4, which is conducive to factory prefabrication, shortening the construction period and simplifying the construction. The light steel keel 1 has enough space inside to accommodate the insulation layer 2, which can improve the overall sound insulation and sound absorption and insulation capabilities of the wall panel, integrate the wall and insulation, and solve the risk of falling off of the wall's external insulation; by setting the insulation layer 2, the thermal insulation and air tightness of the wall can be enhanced; by setting the outer layer 3 and the inner layer 4, the light steel keel 1 and the insulation layer 2 can be protected, the waterproof ability can be improved, the service life can be extended, and the thermal insulation and air tightness of the wall can be further improved; by setting the longitudinal keel, the transverse keel and the edge sealing keel, it can be conducive to factory prefabrication, shorten the construction period, simplify the construction, and reduce the cost of construction, transportation and later structural seismic design.
[0026] The longitudinal keel includes two groups of long C-shaped steels 11 arranged mouth to mouth and several groups of first thermal break connectors 12 for connecting the two groups of long C-shaped steels 11. A gap is provided between the two groups of long C-shaped steels 11, and the interval between two adjacent groups of longitudinal keels is 500mm to 1000mm. By providing the long C-shaped steel 11, it can serve as the basis of the longitudinal keel and reduce the deadweight of the longitudinal keel; by providing the first thermal break connector 12 and a gap between the long C-shaped steels 11, it can avoid the two groups of long C-shaped steels 11 from contacting each other, effectively solving the cold bridge problem.
[0027] The transverse keel includes two groups of short C-shaped steels 13 arranged mouth to mouth, the short C-shaped steels 13 are arranged opposite to the long C-shaped steels 11, the ends of the short C-shaped steels 13 are vertically connected to the side walls of the long C-shaped steels 11 by welding or self-tapping screws, the interval between two adjacent groups of transverse keels is 600mm to 1000mm, and the thickness of the short C-shaped steels 13 and the long C-shaped steels 11 are both 1.5mm to 3.0mm. By arranging the short C-shaped steels 13, a transverse keel can be formed, the strength of the longitudinal keel can be enhanced, and the main skeleton of the light steel keel 1 can be formed after connecting the longitudinal keels.
[0028] The edge-sealed keel includes two groups of symmetrically arranged equilateral angle steels 14 and several groups of second thermal break connectors 15 for connecting the two groups of equilateral angle steels 14. The equilateral angle steels 14 are connected to the ends of the long C-shaped steels 11. The thickness of the equilateral angle steels 14 is 1.5 mm to 3.0 mm. By arranging the equilateral angle steels 14, the ends of the long C-shaped steels 11 can be edge-sealed, and the second thermal break connectors 15 can be used to enhance the connection strength of the ends of the longitudinal keel.
[0029] The first thermal break connector 12 and the second thermal break connector 15 are any one of "X" shape, "Z" shape, "L" shape and rectangular shape. The first thermal break connector 12 and the second thermal break connector 15 are both made of high-density polyethylene, which can enhance the overall strength of the light steel keel 1.
[0030] The outer layer 3 includes an outer steel mesh 31 and an outer pouring layer 32. The outer steel mesh 31 is welded to one side of the light steel keel 1. The outer pouring layer 32 is arranged on the outer steel mesh 31. The thickness of the outer pouring layer 32 is 20 mm to 30 mm. The outer pouring layer 32 is any one of anti-cracking mortar and fiber concrete. By setting the outer steel mesh 31, the coating effect of the outer pouring layer 32 can be enhanced, so that the outer layer 3 and the light steel keel 1 form a whole to avoid falling off; by setting the outer pouring layer 32, the light steel keel 1 and the insulation layer 2 can be protected, the waterproof ability can be improved, the service life can be extended, and the wall insulation ability and air tightness can be further improved, and the aesthetic effect can be achieved.
[0031] The inner surface layer 4 includes an inner steel mesh 41 and an inner pouring layer 42. The inner steel mesh 41 is welded to the other side of the light steel keel 1. The inner pouring layer 42 is arranged on the inner steel mesh 41. The thickness of the inner pouring layer 42 is 10 mm to 20 mm. The inner pouring layer 42 is anti-cracking mortar. By setting the inner steel mesh 41, the coating effect of the inner pouring layer 42 can be enhanced, so that the inner surface layer 4 and the light steel keel 1 form a whole to avoid falling off; by setting the inner pouring layer 42, the outer pouring layer 32 can be used to protect the light steel keel 1 and the insulation layer 2, improve the waterproof ability, extend the service life, and further improve the wall insulation and air tightness, and have an aesthetic effect.
[0032] Example 2
[0033] Figure 3 This is another embodiment of the utility model, which differs from the embodiment 1 in that a reinforcing steel belt 5 is also obliquely provided on the light steel keel 1, and the width of the reinforcing steel belt 5 is 30 mm to 50 mm. By providing the reinforcing steel belt 5, the strength of the light steel keel 1 can be further enhanced while ensuring that the thickness of the light steel keel 1 meets the standard, and the light steel keel 1 can be reinforced at the window and door opening position.
[0034] During the production and assembly process, the number and spacing of the longitudinal keels are determined according to the size of the wall. The longitudinal keels cooperate with the transverse keels to form a "well"-shaped keel frame. The equilateral angle steel 14 of the edge sealing keel cooperates with the second thermal break connector 15 to form an edge wrapping structure, and finally forms a "field"-shaped light steel keel 1; a gap is provided between the two groups of equilateral angle steels 14 to avoid contact between the two groups of equilateral angle steels 14, and cooperate with the longitudinal keel to effectively solve the cold bridge problem. The width of the inner side of the edge sealing keel is the same as the width of the outer side of the longitudinal keel. The equilateral angle steel 1 4 is the same as the width of the long C-shaped steel 11, so that the edge-sealed keel can cover the end of the longitudinal keel; after the light steel keel 1 is assembled, the outer steel mesh 31 is welded to one side of the light steel keel 1, and then the outer casting layer 32 is poured to form the outer layer 3; then the insulation layer 2 is filled into the light steel keel 1; finally, the inner steel mesh 41 is welded to the other side of the light steel keel 1, and the inner casting layer 42 is poured to form the inner surface layer 4, and then the anti-cracking mortar or fiber concrete is poured on the four side walls of the light steel keel 1 to form a complete wall panel.
[0035] The descriptions of the orientation or relative position relationship of the structure in the present invention, such as the orientation or relative position relationship indicated by "center", "up", "down", "left", "right", "vertical", "horizontal", "inside", "outside", etc., are based on the orientation or position relationship shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the structure referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention.
Claims
1. An assembled thermal insulation integrated wall panel, comprising a light steel keel (1), characterized in that: The light steel keel (1) is provided with an insulation layer (2) inside, an outer layer (3) is provided on one side of the light steel keel (1), and an inner layer (4) is provided on the other side of the light steel keel (1). The light steel keel (1) includes a plurality of groups of longitudinal keels, a plurality of groups of transverse keels and edge-sealing keels. The longitudinal keels are connected to each other through a plurality of groups of transverse keels, and the edge-sealing keels are arranged at the top and bottom of the longitudinal keels.
2. The assembled thermal insulation integrated wall panel according to claim 1 is characterized in that: The longitudinal keel comprises two groups of long C-shaped steels (11) arranged opposite to each other and a plurality of groups of first thermal break connectors (12) for connecting the two groups of long C-shaped steels (11), and a gap is provided between the two groups of long C-shaped steels (11).
3. The assembled thermal insulation integrated wall panel according to claim 2 is characterized in that: The transverse keel comprises two groups of short C-shaped steels (13) arranged opposite to each other, and the ends of the short C-shaped steels (13) are vertically connected to the side walls of the long C-shaped steels (11).
4. The assembled thermal insulation integrated wall panel according to claim 3 is characterized in that: The edge sealing keel comprises two groups of symmetrically arranged equilateral angle steels (14) and a plurality of groups of second thermal break connectors (15) for connecting the two groups of equilateral angle steels (14). The equilateral angle steels (14) are connected to the ends of the long C-shaped steels (11).
5. The assembled thermal insulation integrated wall panel according to claim 4 is characterized in that: The first thermal break bridge connector (12) and the second thermal break bridge connector (15) are in any one of an "X" shape, a "Z" shape, an "L" shape and a rectangle.
6. The assembled thermal insulation integrated wall panel according to any one of claims 1 to 5, characterized in that: The outer layer (3) comprises an outer steel wire mesh (31) and an outer casting layer (32); the outer steel wire mesh (31) is connected to one side of the light steel keel (1); and the outer casting layer (32) is arranged on the outer steel wire mesh (31).
7. The assembled thermal insulation integrated wall panel according to claim 6 is characterized in that: The surface layer (4) comprises an inner steel wire mesh (41) and an inner cast layer (42), wherein the inner steel wire mesh (41) is connected to the other side of the light steel keel (1), and the inner cast layer (42) is arranged on the inner steel wire mesh (41).