Casting sand mold for overcoming position defects of cold core and cold iron
By using sand covering and stopping design in casting sand molds, the problem of misfire and pores of cold core cold iron is solved, the contact between cold iron and liquid steel is avoided, the product quality and yield rate are improved, and the repair is reduced cost.
Patent Information
- Application Number
- CN202322924712.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-10-31
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2033-10-31
AI Technical Summary
During the sand mold casting process, cold core cold iron is prone to inactivity, and direct contact between cold iron and liquid steel leads to chemical reactions and pore problems, resulting in product scrapping.
A cast sand mold is designed, in which a sand coating with a thickness of 1.5mm-2mm is laid on the side of the cold core cold iron near the lower mold of the sand box, and a stop is set between the cold core cold iron and the upper mold of the sand box. Prevent cold iron from contacting liquid steel, and at the same time, the irregular curved surface of the cold core cold iron is the same as the outer surface of the casting, and the cooling speed is controlled.
It effectively solves the problems of cold iron fissure and pores, reduces the number of workers' revisions and product scrap rates, improves product yield and production quality, and has low cost.
Smart Images

Figure CN221966747U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the technical field of sand mold casting, and in particular relates to a casting sand mold which solves the defects of cold core and cold iron positions. Background Art
[0002] Sand casting is a widely used casting form that uses sand to make a mold. In sand casting, first, you need to put a finished part model or a wooden model (pattern) in the sand, then fill the sand around the pattern, and after unpacking and taking out the pattern, the sand forms a mold. After the mold is made, the metal liquid can be cast, and the metal forms a part after solidification. Sand casting can be used for iron casting, bronze casting, brass casting, aluminum casting, and wet casting can also be used. Since the mold needs to be made before casting the metal, sand casting is usually not suitable for producing a large number of identical parts. However, affected by the casting characteristics of the mold, the following technical problems often occur during the casting process: the cold core cold iron is exposed, the cold iron position is prone to shooting failure, and it is difficult for workers to repair and draw; some cold iron surfaces have moisture or rust. When the cold iron is exposed, the cold iron directly contacts the molten steel during the pouring process, and the gas is decomposed by chemical reaction, which easily causes pores in the cold iron position, resulting in product scrapping. Therefore, whether a casting sand mold that can effectively solve the defects of the cold core cold iron position can be designed is a technical problem that needs to be solved in the utility model. Utility Model Content
[0003] In order to solve the above technical problems, the utility model provides a casting sand mold that solves the position defects of the cold core and the cold iron, which can solve the problem of the cold iron not being shot solidly. After the sand is covered, the cold iron does not directly contact with the molten steel, thus avoiding the occurrence of chemical reactions and solving the problem of cold iron pores.
[0004] The utility model discloses a casting sand mold for solving the position defect of a cold core chilling iron. A cold core chilling iron is arranged at a sand box upper mold of the casting sand mold, a covering sand layer is laid on a side of the cold core chilling iron close to a sand box lower mold, and a stopper is arranged between the cold core chilling iron and the sand box upper mold.
[0005] Specifically, the sand coating layer is coated sand with a thickness of 1.5 mm to 2 mm.
[0006] More specifically, one end of the chill near the sand box lower mold is an irregular arc surface, and the irregular arc surface has the same structure as the outer surface of the casting near the chill.
[0007] Specifically, the cross-sectional size of the cold core cold iron is 9-16cm 2 .
[0008] The beneficial effects of the utility model are:
[0009] The exposed chiller is changed to a sand-covered chiller. The problem of incorrect chiller position shooting is solved by pre-embedded sand and adding blocks on the back of the upper mold. After sand covering, the chiller does not come into direct contact with the molten steel, avoiding chemical reactions and solving the problem of chiller porosity. The casting sand mold reduces the amount of workers' repair work and reduces the risk of slag eyes in the product. The sand-covered chiller solves the problem of chiller porosity and greatly improves the product yield. The defect elimination cost is low. Through the cooperation of the chiller, blocks and pre-embedded sand, the product scrap rate due to porosity is reduced by 0.04%, effectively improving the product production quality. BRIEF DESCRIPTION OF THE DRAWINGS
[0010] Figure 1 It is an overall schematic diagram of the utility model.
[0011] Figure 2 It is an enlarged schematic diagram of the cold core and cold iron of the utility model.
[0012] Figure 3 It is a schematic diagram of the lower mold of the sand box when the stopper and the cold core cold iron are not installed. DETAILED DESCRIPTION
[0013] In order to further explain the technical means and effects adopted by the present invention to achieve the predetermined purpose, the specific implementation method, structure, characteristics and effects of the present invention are described in detail below in combination with the accompanying drawings and preferred embodiments.
[0014] It should be noted that in the present application, unless otherwise specified, the directional words used, such as "up, down, top, bottom", usually refer to the directions shown in the drawings, or to the components themselves in the vertical, perpendicular or gravity directions; similarly, for ease of understanding and description, "inside and outside" refer to the inside and outside relative to the outline of each component itself, but the above-mentioned directional words are not used to limit the present invention.
[0015] Example
[0016] like Figure 1-3 As shown, a casting sand mold for solving the position defect of the cold core chill iron, a cold core chill iron 2 is arranged at the sand box upper mold of the casting sand mold, a sand covering layer 3 is laid on the side of the cold core chill iron 2 close to the sand box lower mold 1, a stopper 4 is arranged between the cold core chill iron 2 and the sand box upper mold, and the stopper 4 can ensure that the cold core chill iron is pressed while preventing it from being exposed.
[0017] In this embodiment, the coating sand layer 3 is a coated sand with a thickness of 1.5 mm, which separates the cold core cold iron 2 from the pouring molten metal to avoid problems such as inaccurate cold iron position shooting and cold iron porosity caused by uneven cooling rate of the molten metal. The thickness of the coating sand cannot be too large to avoid a decrease in the shrinkage compensation effect of the cold core cold iron 2, thereby causing porosity and reducing the product molding quality.
[0018] One end of the cold core chill 2 close to the sand box lower mold 1 is an irregular arc surface, and the irregular arc surface has the same structure as the outer surface of the molded casting close to the cold core chill 2, so that the curvature of the cooling end of the cold core chill 2 is the same as the outer surface of the casting to be cast, and the cooling speed of the casting at the position of the cold core chill 2 is controlled to be the same.
[0019] The cross-sectional size of the cold core cold iron 2 is 9 cm 2 , control the cooling rate of each part of the casting to avoid uneven cooling rate caused by too large or too small cold core and cold iron, resulting in casting stress, cold cracking and other problems.
[0020] The above description is only a preferred embodiment of the present invention and does not constitute any form of limitation to the present invention. Although the present invention has been disclosed as a preferred embodiment as above, it is not intended to limit the present invention. Any technical personnel in this field can make some changes or modify the technical contents disclosed above into equivalent embodiments without departing from the scope of the technical solution of the present invention. However, any brief modifications, equivalent changes and modifications made to the above embodiments based on the technical essence of the present invention without departing from the content of the technical solution of the present invention are still within the scope of the technical solution of the present invention.
Claims
1. A casting sand mold for solving the cold core cold iron position defect, characterized in that: A cold core chill is arranged at the sand box upper mold of the casting sand mold, a sand covering layer is laid on the cold core chill on one side close to the sand box lower mold, and a stopper is arranged between the cold core chill and the sand box upper mold.
2. A casting sand mold for solving the cold core and cold iron position defect according to claim 1, characterized in that: The sand coating layer is coated sand with a thickness of 1.5 mm to 2 mm.
3. A casting sand mold for solving the cold core and cold iron position defect according to claim 2, characterized in that: One end of the chill core cold iron close to the sand box lower mold is an irregular arc surface, and the irregular arc surface has the same structure as the outer surface of the casting close to the chill core cold iron.
4. A casting sand mold for solving the cold core and cold iron position defect according to claim 3, characterized in that: The cross-sectional size of the cold core cold iron is 9-16cm 2 .