Clamp for low-frequency crack propagation fatigue test of annular sample
By designing a fixture containing mounting bracket, pin and semicircular sample cover, the problem of difficulty in clamping aluminum alloy ring samples is solved, and efficient fatigue test and accurate data detection of aluminum alloy ring samples are realized, which improves the Overall test efficiency.
Patent Information
- Application Number
- CN202420094837.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-01-15
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2034-01-15
AI Technical Summary
The existing aluminum alloy fracture toughness test fixtures cannot meet the clamping requirements of annular samples, resulting in low-frequency crack propagation fatigue tests of aluminum alloy ring samples.
A clamp including upper and lower mounting brackets, pins, semicircular sample sleeves and tie rods is designed. The combined structure of pins and tie rods achieves efficient clamping of the annular sample to ensure stable installation of the sample on the fatigue tester and Measurement.
It realizes fast and convenient clamping and efficient fatigue testing of aluminum alloy ring samples, improves the accuracy and overall efficiency of test data, and solves the problem of difficulty clamping ring samples.
Smart Images

Figure CN221976613U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of aluminum alloy production, in particular to a clamp used for low-frequency crack extension fatigue test of an annular sample. Background Art
[0002] During the application of aluminum alloy equipment, fatigue fractures that are difficult to detect and prevent often occur. This sudden fracture failure form often causes catastrophic accidents and seriously threatens human life and property. Therefore, fatigue performance is not only an important basis for material selection, but also an important mechanical parameter for designers to perform fatigue design on components. Therefore, aluminum alloy fracture toughness test is a necessary means for the inspection of high-quality aluminum alloy products. At present, the specimens used in aluminum alloy fracture toughness test are generally strip or rod specimens, that is, the two ends of the specimen are clamped on the upper and lower chucks of the fatigue testing machine and the test is started. After the specimen breaks, the test results are recorded. However, for the relevant important pipes used in special environments, it is required to conduct transverse plane stress fracture toughness tests on the pipes. The specimens need to be made into rings, and the specimens with central through cracks are used. Under unidirectional tensile stress conditions, the plane stress fracture toughness is measured. The original clamps for clamping strip or rod specimens cannot meet the clamping of ring specimens. Therefore, it is necessary to further optimize the clamping fixtures of aluminum alloy ring specimens to meet the test requirements of low-frequency crack extension fatigue tests of ring specimens. Utility Model Content
[0003] The utility model provides a clamp for a low-frequency crack extension fatigue test of an annular sample, so as to solve the problems existing in the above background.
[0004] In order to achieve the above purpose, the utility model adopts the following technical solutions:
[0005] A fixture for low-frequency crack extension fatigue testing of an annular specimen comprises an upper mounting bracket, a pin is horizontally passed through the upper mounting bracket, an upper semicircular specimen sleeve is sleeved on the shaft of the pin located on the inner side of the upper mounting bracket, a lower mounting bracket is symmetrically provided at the bottom of the upper mounting bracket, a pin is also horizontally passed through the lower mounting bracket, and a lower semicircular specimen sleeve symmetrical to the upper semicircular specimen sleeve is sleeved on the shaft of the pin located on the inner side of the lower mounting bracket.
[0006] Furthermore, first mounting holes are provided on both sides of the upper mounting bracket and the lower mounting bracket, and the pin shafts are passed through the first mounting holes.
[0007] Furthermore, second mounting holes are symmetrically provided on the upper semicircular sample sleeve plate and the lower semicircular sample sleeve plate, and the pin shafts are arranged through the second mounting holes.
[0008] Furthermore, a first pull rod is vertically provided at the top of the upper mounting bracket, and a second pull rod symmetrical to the first pull rod is provided at the bottom of the lower mounting bracket.
[0009] The utility model has the following beneficial effects:
[0010] The utility model provides a fixture for low-frequency crack extension fatigue test of annular specimens, which is mainly composed of symmetrical pull rods, mounting brackets, mounting holes, pins, semicircular specimen sleeves and other components. The upper and lower mounting brackets are clamped on both sides of the testing machine, and the upper and lower semicircular specimen sleeves are clamped between the mounting brackets through the pins. Then, the processed annular specimens are sleeved on the outer sides of the semicircular specimen sleeves, thereby realizing fast and convenient clamping and installation of aluminum alloy annular specimens, effectively ensuring the convenience and accuracy of data detection of plane stress fracture toughness test of the annular specimens, thereby improving the overall efficiency of fatigue test of aluminum alloy annular specimens, and solving the problem that in the current low-frequency crack fatigue test of aluminum alloy annular specimens, the annular specimens are usually difficult to clamp due to the lack of special and efficient fixtures, which ultimately leads to low overall test efficiency of aluminum alloy annular specimens. BRIEF DESCRIPTION OF THE DRAWINGS
[0011] Figure 1 It is a schematic diagram of the overall structure of the utility model.
[0012] Figure 2 It is a schematic diagram of the overall structure of the semicircular specimen sleeve of the utility model.
[0013] The meanings of the reference numerals are as follows:
[0014] 1. First tie rod; 2. Upper mounting bracket; 3. First mounting hole; 4. Pin; 5. Upper semicircular specimen sleeve; 6. Lower semicircular specimen sleeve; 7. Second mounting hole; 8. Lower mounting bracket; 9. Second tie rod; 10. Specimen. DETAILED DESCRIPTION
[0015] The utility model is further described below in conjunction with the accompanying drawings and specific embodiments.
[0016] like Figure 1-2As shown, a fixture for low-frequency crack extension fatigue test of an annular specimen comprises an upper mounting bracket 2, first mounting holes 3 are provided on both sides of the upper mounting bracket 2 and the lower mounting bracket 8, pins 4 are installed in the first mounting holes 3, and an upper semicircular specimen sleeve 5 is sleeved on the shaft of the pin 4 located inside the upper mounting bracket 2. The lower mounting bracket 8 is symmetrically fixedly installed at the bottom of the upper mounting bracket 2, and the pin 4 is also horizontally penetrated and installed on the lower mounting bracket 8, and a lower semicircular specimen sleeve 6 symmetrical to the upper semicircular specimen sleeve 5 is fitted on the shaft of the pin 4 located inside the lower mounting bracket 8. Second mounting holes 7 are symmetrically provided on the upper semicircular specimen sleeve 5 and the lower semicircular specimen sleeve 6, and the pins 4 are arranged through the second mounting holes 7. A first tie rod 1 is vertically welded to the top of the upper mounting bracket 2, and a second tie rod 9 symmetrical to the first tie rod 1 is welded to the bottom of the lower mounting bracket 8.
[0017] When the utility model is used in a specific application, the upper mounting bracket 2 and the lower mounting bracket 8 are first clamped on the upper and lower chucks of the fatigue testing machine respectively, and then the upper semicircular specimen sleeve plate 5 and the lower semicircular specimen sleeve plate 6 are tightly pressed together to form a circle, and then the processed annular specimen 10 is sleeved on the circular sleeve formed by the upper semicircular specimen sleeve plate 5 and the lower semicircular specimen sleeve plate 6, so that the prefabricated crack of the specimen 10 is parallel to the surface of the circular sleeve, and then the circular sleeve with the specimen 10 is vertically placed into the lower mounting bracket 8, and the pin shaft 4 is inserted into the first mounting hole 3 and the second mounting hole 7 of the lower mounting bracket 8 in sequence and locked, and then the upper chuck of the fatigue testing machine is lowered to make the upper mounting bracket 2 and the lower mounting bracket 8 fit together. At this time, the upper semicircle of the circular sleeve is completely in the upper mounting bracket 2, and then the pin shaft 4 is inserted into the first mounting hole 3 and the second mounting hole 7 of the upper mounting bracket 2 in sequence and locked, thereby completing the convenient and efficient clamping of the annular specimen 10. Then the fatigue testing machine is started. Under the action of the fatigue testing machine, the lower chuck drives the lower semicircle of the circular sleeve to vibrate continuously up and down. When the prefabricated crack extension length of the annular specimen 10 reaches the requirement, the number of fatigue cycles is recorded and the specimen 10 is broken. Then the pin 4, the upper semicircular specimen sleeve plate 5 and the lower semicircular specimen sleeve plate 6, the upper mounting bracket 2 and the lower mounting bracket 8 and the specimen 10 are removed in turn, thereby completing the fatigue test of the annular specimen 10, effectively ensuring the quick and convenient clamping and installation of the aluminum alloy annular specimen 10, improving the convenience and accuracy of the plane stress fracture toughness test data detection of the annular specimen 10, and thereby improving the overall efficiency of the fatigue test of the aluminum alloy annular specimen 10. Therefore, the fixture has good practicality.
Claims
1. A fixture for low-frequency crack growth fatigue test of annular specimens, characterized by: The invention comprises an upper mounting bracket (2), a pin shaft (4) passing through the upper mounting bracket (2) horizontally, an upper semicircular sample sleeve plate (5) being sleeved on the axis of the pin shaft (4) located inside the upper mounting bracket (2), a lower mounting bracket (8) being symmetrically provided at the bottom of the upper mounting bracket (2), a pin shaft (4) passing through the lower mounting bracket (8) horizontally, and a lower semicircular sample sleeve plate (6) symmetrical to the upper semicircular sample sleeve plate (5) being sleeved on the axis of the pin shaft (4) located inside the lower mounting bracket (8).
2. A fixture for low-frequency crack growth fatigue test of annular specimen according to claim 1, characterized in that: First mounting holes (3) are provided on both sides of the upper mounting bracket (2) and the lower mounting bracket (8), and the pin shafts (4) are inserted into the first mounting holes (3).
3. The fixture for low-frequency crack growth fatigue test of annular specimen according to claim 1, characterized in that: Second mounting holes (7) are symmetrically provided on the upper semicircular sample sleeve plate (5) and the lower semicircular sample sleeve plate (6), and the pin shafts (4) are arranged through the second mounting holes (7).
4. The fixture for low-frequency crack growth fatigue test of annular specimen according to claim 2, characterized in that: A first pull rod (1) is vertically arranged at the top of the upper mounting bracket (2), and a second pull rod (9) symmetrical to the first pull rod (1) is arranged at the bottom of the lower mounting bracket (8).