Casting mold for bimetal composite hammerhead of mine crusher

By designing the limit and cooling mechanism in the casting mold of the bimetal composite hammer head of the mine crusher, the problems of difficulty in limiting and low molding efficiency after mold clamping are solved, and the stable fixation of the mold and rapid mold forming of the workpiece are achieved, improving the improvement of the improvement of the Casting efficiency.

CN221983876UActive Publication Date: 2024-11-12TAIYUAN NIUMOWANG INTELLIGENT TECH CO LTD
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202422351018.8
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-09-26
Publication Date
2024-11-12
Estimated Expiration
2034-09-26

AI Technical Summary

Technical Problem

The casting mold of the existing mine crusher bimetal composite hammer head is inconvenient to limit after closing, and the molding efficiency is low under natural cooling, which affects the casting efficiency.

Method used

A casting mold including a limiting mechanism and a cooling mechanism is designed to achieve the limiting of the mold through the threaded connection of the forward and reverse screws and the connecting block, and the molding efficiency of the workpiece is improved by using an air pump, exhaust hose and filter.

Benefits of technology

The effective limit of the mold is achieved, the mold is avoided to move during casting, the casting efficiency is improved, and the workpiece molding is accelerated through blowing and heat dissipation, reducing dust and impurities pollution.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221983876U_ABST
    Figure CN221983876U_ABST
Patent Text Reader

Abstract

The utility model discloses a casting mould for a bimetallic composite hammerhead of a mine crusher, which comprises a bottom plate, the bottom of the bottom plate is fixedly connected with a plurality of support rods, the top of the bottom plate is slidably connected with two symmetrically distributed swage dies, the two swage dies are in contact with each other, the top of each swage die is provided with a feed hopper, and the feed hopper is connected with the support rods. And a feeding pipe is arranged at the front end of the section mold, a sliding seat is fixedly connected to the bottom of the section mold, the sliding seat is slidably connected with the bottom plate, and a connecting block is fixedly connected to the bottom of the sliding seat. By designing the threaded connection of the positive and negative screw rod and the connecting block, the threaded movement of the connecting block can be realized through the rotation of the positive and negative screw rod, so that the opening and closing of the section mold can be realized, and in the closing process of the section mold, the positive and negative screw rod can be limited through the insertion of the insertion rod and the insertion groove, so that the position of the section mold can be fixed; the casting effect is prevented from being affected by movement of the swage die during casting.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of casting moulds, in particular to a casting mould for a bimetallic composite hammer head of a mining crusher. Background Art

[0002] The sand and gravel crusher uses a hammer to pound sand and gravel so that larger sand and gravel are broken into smaller sand and gravel particles to meet the size requirements of sand and gravel in construction sites, bridges and other occasions. During the processing of the hammer head, the hammer head needs to be formed through a casting mold.

[0003] The utility model patent with patent authorization announcement number CN216502292U discloses a casting mold for a bimetallic composite hammer head of a crusher, which solves the problem in the prior art that the casting mold structure of the bimetallic composite hammer head occupies a large space, the casting process is complicated, and the two molds are not easy to move relative to each other.

[0004] In the above prior art, during the use of the casting mold, the mold is moved by threaded connection, and it is inconvenient to limit the mold after the mold is closed. If the mold moves, a gap will appear between the molds, affecting the casting work. In addition, the product molding efficiency is low in the natural cooling mode, affecting the casting efficiency. Therefore, improvements are needed. Utility Model Content

[0005] The utility model aims to provide a casting mould for a bimetallic composite hammer head of a mining crusher, which solves the problem that it is inconvenient to limit the mold after the mold is closed, and also solves the problem of low mold forming efficiency during natural cooling.

[0006] To achieve the above-mentioned purpose, the utility model provides the following technical solutions: a casting mold for a bimetallic composite hammer head of a mining crusher, comprising a bottom plate, a plurality of support rods are fixedly connected to the bottom of the bottom plate, two symmetrically distributed molds are slidably connected to the top of the bottom plate, the two molds are in contact with each other, a feed hopper is provided on the top of the mold, a feed pipe is provided on the front end of the mold, a slide seat is fixedly connected to the bottom of the mold, the slide seat is slidably connected to the bottom of the bottom plate, a connecting block is fixedly connected to the bottom of the slide seat, the interior of the connecting block is connected with forward and reverse screws through threads, the outer side of the forward and reverse screws is rotatably sleeved with a support seat through a bearing, the support seat is fixedly connected to the bottom plate, a slider is fixedly connected to the lower end of the mold and located on the back of the connecting block, the slider is slidably connected to the bottom plate, and the slider The cam is provided with a guide rod, the outer side of the guide rod is fixedly connected with a rotating seat, the rotating seat is fixedly connected to the base plate, a limiting mechanism is arranged on the forward and reverse screws, and a cooling mechanism is arranged on the mold, and the limiting mechanism includes a fixed seat, the right end of the base plate is fixedly connected with a fixed seat, the fixed seat is rotatably connected with the forward and reverse screws, a slot is provided inside the forward and reverse screws, an insertion rod is slidingly sleeved inside the slot, the insertion rod is slidably connected to the fixed seat, the top of the insertion rod is fixedly connected with a fixed block, the top of the fixed block is fixedly connected with a pull rod, the fixed block and the pull rod are both slidably connected to the fixed seat, a spring is arranged on the outer side of the pull rod, the outer side of the fixed block is fixedly connected with a first magnet, the first magnet is slidably connected to the fixed seat, and the inside of the fixed seat is fixedly connected with a second magnet. By designing a limiting mechanism, it is convenient to limit the mold. The cooling mechanism includes a fixed box, the top of the mold is fixedly connected to the fixed box, the right end of the fixed box is fixedly connected to an exhaust hose, the bottom of the exhaust hose is fixedly connected to a guide cover, the guide cover is in contact with the feed hopper, the bottom of the inner wall of the fixed box is fixedly connected to an air pump, the right end of the air pump is provided with an exhaust pipe, the outer side of the exhaust pipe is fixedly sleeved with a support frame, the support frame is fixedly connected to the fixed box, the inner side of the support frame is slidably sleeved with a filter screen, and the filter screen is slidably connected to the fixed box. By designing a cooling mechanism, the workpiece forming efficiency can be improved.

[0007] Preferably, the number of the slots is multiple, and the multiple slots are evenly distributed inside the forward and reverse screw rods. By designing multiple slots, the insertion rod can be inserted into the slots at different positions.

[0008] Preferably, one end of the spring is fixedly connected to the fixed block, and the other end of the spring is fixedly connected to the fixed seat. The spring is designed so that the force of the spring can act on the fixed block.

[0009] Preferably, the left end of the air pump is provided with an air inlet, which is fixedly connected to the fixed box. By designing the air inlet, external air can be sucked into the fixed box.

[0010] Preferably, the outer side of the exhaust pipe is fixedly connected with a plurality of air outlets, and the air outlets are communicated with the exhaust pipe. By designing the air outlets, the gas inside the exhaust pipe can be discharged.

[0011] Compared with the prior art, the beneficial effects of the utility model are as follows:

[0012] 1. The utility model designs a threaded connection between the forward and reverse screws and the connecting block. The threaded movement of the connecting block can be realized by rotating the forward and reverse screws, thereby realizing the opening and closing of the mold. During the closing process of the mold, the forward and reverse screws can be limited by plugging the insertion rod into the slot, thereby fixing the position of the mold, thereby preventing the movement of the mold during casting from affecting the casting effect.

[0013] 2. The utility model designs an air pump, which can input air into the fixed box. The air can eventually move through the exhaust hose and the air guide cover, so that the air can be input into the mold, and the workpiece can be cooled by blowing after casting, which can accelerate the molding efficiency of the workpiece and improve the casting efficiency. The air can be filtered under the action of the detachable filter to prevent dust and impurities from entering the mold and causing pollution. BRIEF DESCRIPTION OF THE DRAWINGS

[0014] Figure 1 The overall structure of the utility model is three-dimensional Figure 1 ;

[0015] Figure 2 The overall structure of the utility model is three-dimensional Figure 2 ;

[0016] Figure 3 For this utility model Figure 1 A right side sectional view of a fixed seat;

[0017] Figure 4 For this utility model Figure 1 Front cross-sectional view of the fixed box.

[0018] In the figure: 1. bottom plate; 2. support rod; 3. mold; 4. feed hopper; 5. feed pipe; 6. slide seat; 7. connecting block; 8. limit mechanism; 9. cooling mechanism; 10. forward and reverse screws; 11. support seat; 12. slider; 13. guide rod; 14. rotating seat; 81. fixed seat; 82. slot; 83. plug rod; 84. fixed block; 85. pull rod; 86. spring; 87. first magnet; 88. second magnet; 91. fixed box; 92. exhaust hose; 93. deflector; 94. air pump; 95. air inlet; 96. exhaust pipe; 97. air outlet; 98. support frame; 99. filter. DETAILED DESCRIPTION

[0019] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0020] See also Figure 1 , Figure 2 A casting mold for a bimetallic composite hammer of a mining crusher comprises a bottom plate 1, a plurality of support rods 2 are fixedly connected to the bottom of the bottom plate 1, two symmetrically distributed molds 3 are slidably connected to the top of the bottom plate 1, the two molds 3 are in contact with each other, a feed hopper 4 is arranged on the top of the mold 3, a feed pipe 5 is arranged on the front end of the mold 3, a slide seat 6 is fixedly connected to the bottom of the mold 3, the slide seat 6 is slidably connected to the bottom of the bottom plate 1, a connecting block 7 is fixedly connected to the bottom of the slide seat 6, and the interior of the connecting block 7 is connected by a thread It is connected to a forward and reverse screw 10, and a support seat 11 is rotatably sleeved on the outer side of the forward and reverse screw 10 through a bearing. The support seat 11 is fixedly connected to the base plate 1. A slider 12 is fixedly connected to the lower end of the mold 3 and located on the back of the connecting block 7. The slider 12 is slidably connected to the base plate 1. A guide rod 13 is slidably sleeved inside the slider 12, and a rotating seat 14 is fixedly connected on the outer side of the guide rod 13. The rotating seat 14 is fixedly connected to the base plate 1. A limiting mechanism 8 is arranged on the forward and reverse screw 10, and a cooling mechanism 9 is arranged on the mold 3.

[0021] See also Figure 1 , Figure 2 , Figure 3 The limiting mechanism 8 includes a fixing seat 81, the right end of the bottom plate 1 is fixedly connected with the fixing seat 81, the fixing seat 81 is rotatably connected with the forward and reverse screws 10, a slot 82 is provided inside the forward and reverse screws 10, and a plug rod 83 is slidably sleeved inside the slot 82. There are multiple slots 82, and the multiple slots 82 are evenly distributed inside the forward and reverse screws 10. By designing multiple slots 82, the plug rod 83 can be inserted into the slots 82 at different positions. The plug rod 83 is slidably connected with the fixing seat 81, and the top of the plug rod 83 is fixedly connected with a fixing block 84. The top of the fixing block 84 A pull rod 85 is fixedly connected, and the fixed block 84 and the pull rod 85 are both slidably connected to the fixed seat 81. A spring 86 is arranged on the outside of the pull rod 85, and one end of the spring 86 is fixedly connected to the fixed block 84, and the other end of the spring 86 is fixedly connected to the fixed seat 81. By designing the spring 86, the force of the spring 86 can act on the fixed block 84. A first magnet 87 is fixedly connected to the outside of the fixed block 84, and the first magnet 87 is slidably connected to the fixed seat 81. A second magnet 88 is fixedly connected to the inside of the fixed seat 81. By designing the limiting mechanism 8, it is convenient to limit the mold 3.

[0022] See also Figure 1 , Figure 2 , Figure 4 The cooling mechanism 9 includes a fixed box 91, the top of the mold 3 is fixedly connected to the fixed box 91, the right end of the fixed box 91 is fixedly connected to an exhaust hose 92, the bottom of the exhaust hose 92 is fixedly connected to a guide cover 93, the guide cover 93 is in contact with the feed hopper 4, the bottom of the inner wall of the fixed box 91 is fixedly connected to an air pump 94, the left end of the air pump 94 is provided with an air inlet 95, and the air inlet 95 is fixedly connected to the fixed box 91. By designing the air inlet 95, external air can be sucked into the fixed box 91. An exhaust pipe 96 is provided at the right end of the air pump 94, and a support frame 98 is fixedly sleeved on the outer side of the exhaust pipe 96. A plurality of air outlets 97 are fixedly connected to the outer side of the exhaust pipe 96, and the air outlets 97 are communicated with the exhaust pipe 96. By designing the air outlets 97, the gas inside the exhaust pipe 96 can be discharged, the support frame 98 is fixedly connected to the fixed box 91, and a filter screen 99 is slidably sleeved on the inner side of the support frame 98, and the filter screen 99 is slidably connected to the fixed box 91. By designing the cooling mechanism 9, the workpiece forming efficiency can be improved.

[0023] The specific implementation process of the utility model is as follows: during use, when casting is required, the forward and reverse screws 10 are rotated to make the connecting block 7 perform threaded motion, the connecting block 7 drives the slide seat 6 and the mold 3 to move, the mold 3 drives the slider 12 to slide along the guide rod 13, so that the two molds 3 contact each other, and then the pull rod 85 is pushed down, the pull rod 85 drives the fixed block 84 to move down, the fixed block 84 drives the first magnet 87 to move down and separate from the second magnet 88, and then under the elastic action of the compressed spring 86, the fixed block 84 drives the insertion rod 83 to move down and insert into the slot 82. At this time, the forward and reverse screws 10 can be limited, and then the position of the mold 3 can be fixed to prevent the movement of the mold 3 during casting from affecting the casting effect.

[0024] When the mold is closed, the inside of the mold 3 can be cast through the feed hopper 4 and the feed pipe 5. When the casting is completed, the guide cover 93 is moved to the top of the feed hopper 4, and then the air pump 94 is started. The air pump 94 sucks the outside through the air inlet 95, and the external air flows through the exhaust pipe 96 and is discharged through the air outlet 97. Finally, the air will be filtered through the filter 99. The filtered air flows through the exhaust hose 92 and the guide cover 93, so that the air can be input into the mold 3, and the workpiece after casting can be blown to dissipate heat, which can accelerate the molding efficiency of the workpiece and improve the casting efficiency. The air can be filtered under the action of the detachable filter 99 to prevent dust and impurities from entering the mold 3 and causing pollution.

[0025] Although the embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A casting mold for a bimetallic composite hammer of a mining crusher, comprising a bottom plate (1), characterized in that: The bottom of the bottom plate (1) is fixedly connected to a plurality of support rods (2); the top of the bottom plate (1) is slidably connected to two symmetrically distributed molds (3); the two molds (3) are in contact with each other; a feed hopper (4) is provided on the top of the mold (3); a feed pipe (5) is provided at the front end of the mold (3); a slide seat (6) is fixedly connected to the bottom of the mold (3); the slide seat (6) is slidably connected to the bottom plate (1); a connecting block (7) is fixedly connected to the bottom of the slide seat (6); the interior of the connecting block (7) is connected to a forward and reverse screw rod (10) via a thread; the outer side of the forward and reverse screw rod (10) is rotatably sleeved with a support seat (11) via a bearing; the support seat (11) is connected to the bottom plate (1) via a thread. ) is fixedly connected, a slider (12) is fixedly connected at the lower end of the mold (3) and located on the back of the connecting block (7), the slider (12) is slidably connected to the bottom plate (1), a guide rod (13) is slidably sleeved inside the slider (12), the outer side of the guide rod (13) is fixedly connected to a rotating seat (14), the rotating seat (14) is fixedly connected to the bottom plate (1), a limiting mechanism (8) is provided on the forward and reverse screws (10), a cooling mechanism (9) is provided on the mold (3), the limiting mechanism (8) includes a fixed seat (81), the right end of the bottom plate (1) is fixedly connected to the fixed seat (81), the fixed seat (81) is rotatably connected to the forward and reverse screws (10), the forward and reverse screws (10) A slot (82) is provided inside the slot (82), an insert rod (83) is slidably sleeved inside the slot (82), the insert rod (83) is slidably connected to the fixed seat (81), the top of the insert rod (83) is fixedly connected to a fixed block (84), the top of the fixed block (84) is fixedly connected to a pull rod (85), the fixed block (84) and the pull rod (85) are both slidably connected to the fixed seat (81), a spring (86) is provided on the outside of the pull rod (85), the outside of the fixed block (84) is fixedly connected to a first magnet (87), the first magnet (87) is slidably connected to the fixed seat (81), the inside of the fixed seat (81) is fixedly connected to a second magnet (88), and the cooling mechanism (9) comprises A fixed box (91), the top of the mold (3) is fixedly connected to the fixed box (91), the right end of the fixed box (91) is fixedly connected to an exhaust hose (92), the bottom of the exhaust hose (92) is fixedly connected to a guide cover (93), the guide cover (93) is in contact with the feed hopper (4), the bottom of the inner wall of the fixed box (91) is fixedly connected to an air pump (94), the right end of the air pump (94) is provided with an exhaust pipe (96), the outer side of the exhaust pipe (96) is fixedly sleeved with a support frame (98), the support frame (98) is fixedly connected to the fixed box (91), the interior of the support frame (98) is slidably sleeved with a filter screen (99), and the filter screen (99) is slidably connected to the fixed box (91).

2. The casting mold of a bimetallic composite hammer head of a mining crusher according to claim 1 is characterized in that: There are a plurality of slots (82), and the plurality of slots (82) are evenly distributed inside the forward and reverse screws (10).

3. The casting mold of a bimetallic composite hammer head of a mining crusher according to claim 1 is characterized in that: One end of the spring (86) is fixedly connected to the fixing block (84), and the other end of the spring (86) is fixedly connected to the fixing seat (81).

4. The casting mold of a bimetallic composite hammer head of a mining crusher according to claim 1 is characterized in that: An air inlet (95) is provided at the left end of the air pump (94), and the air inlet (95) is fixedly connected to the fixed box (91).

5. The casting mold of the bimetallic composite hammer of a mining crusher according to claim 1 is characterized in that: A plurality of air outlets (97) are fixedly connected to the outer side of the exhaust pipe (96), and the air outlets (97) are in communication with the exhaust pipe (96).

Citation Information

Cited By

  • Casting forming mold for preparing double-metal composite hammerhead

    CN224222715U