Manufacturing device for efficiently reducing free phenol content of solid phenolic resin

By using a 180° circular steam pipe and dispersed pore structure design in the solid phenolic resin manufacturing device, the efficient removal of free phenol is achieved, the problems of low efficiency and high wastewater in the existing technology are solved, and the requirements of environmentally friendly production are met .

CN221999832UActive Publication Date: 2024-11-15JIANGMEN KUNYI RESIN MATERIAL TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420231300.X
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-01-30
Publication Date
2024-11-15
Estimated Expiration
2034-01-30

AI Technical Summary

Technical Problem

The existing methods are inefficient and produce a large amount of wastewater when reducing the free phenol content in solid phenolic resins, which cannot meet the requirements of environmentally friendly and clean production.

Method used

An efficient manufacturing device was designed, using a 180° circular steam pipe and a dispersed pore structure. Through the full mixing of steam and resin, steam is introduced into the reactor under vacuum to remove free phenol and reduce energy loss and wastewater generation.

Benefits of technology

It improves the efficiency of free phenol removal, reduces energy loss and wastewater generation, and meets the requirements of clean and environmentally friendly production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221999832U_ABST
    Figure CN221999832U_ABST
Patent Text Reader

Abstract

The utility model discloses a manufacturing device for efficiently reducing the free phenol content of solid phenolic resin. The manufacturing device comprises a steam leading-in reaction kettle control valve, a steam leading-in reaction kettle pipeline, a steam pipeline fixing plate and a lower 180-degree circular-ring-shaped steam pipeline, dispersion holes are formed in the circular-ring-shaped steam pipeline at certain intervals, three dispersion holes are formed in the same sectional area of the pipeline, each dispersion hole is distributed at an angle of 45 degrees, and the lower portion of the circular-ring-shaped steam pipeline is connected with the steam pipeline fixing plate. And the aperture of each dispersion hole needs to be set within a certain range. Compared with the prior art that water washing or direct steam introduction is adopted in the prior art, the prior art has the defects of poor efficiency, energy waste loss, long processing time, high possibility of quality variation of finished products and the like. According to the manufacturing device, the steam and the high-viscosity resin can be uniformly dispersed and fully mixed, the production and removal efficiency is improved, the energy loss is reduced, the processing time is shortened, and the manufacturing device is high in efficiency.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of solid phenolic resin, in particular to a manufacturing device for efficiently reducing the free phenol content of solid phenolic resin. Background Art

[0002] Solid phenolic resin is generally a thermoplastic resin, which is widely used in grinding wheels, abrasives, friction materials, molding materials, electronic materials, etc. With the progress of the times, this solid phenolic resin is gradually moving towards the demand trend of low free phenol content due to environmental protection and safety requirements.

[0003] Early domestic solid phenolic resins generally had a free phenol content of 3-4% or more, which no longer meets the current market demand.

[0004] At present, there is a general demand for phenolic resins with low free phenol content in the solid phenolic resin market, especially for use in electronic materials, which generally require the free phenol content of the resin to be within 1%; some specific types of phenolic resins are even required to have a free phenol content close to 0%.

[0005] There are several methods for reducing the free unreacted phenol content in solid phenolic resin. The most commonly used methods are water washing or direct steam passing through a straight pipe. However, the efficiency is poor and a large amount of wastewater is generated, which cannot meet the requirements of environmentally friendly clean production. Summary of the invention

[0006] In order to overcome the technical defects of the existing commonly used methods, the purpose of the utility model is to provide a manufacturing device for efficiently reducing the free phenol content of solid phenolic resin, ensuring that the free phenol of the solid phenolic resin is reduced with minimal energy loss without affecting the physical properties of the solid phenolic resin material, and meeting the production requirements of cleanness and environmental protection.

[0007] In order to achieve the above purpose, the technical solution of the utility model is:

[0008] A manufacturing device for efficiently reducing the free phenol content of solid phenolic resin, comprising:

[0009] Steam introduction into the reactor control valve is used to control the timing of mixing steam with high-viscosity resin;

[0010] Steam introduction pipeline for reactor: used to send steam into the reactor to directly contact and mix with the reaction resin;

[0011] Steam pipe fixing plate: used to fix the steam pipe to the reactor wall so that the vertical steam pipe will not be damaged by vibration when steam is introduced;

[0012] 180° circular steam pipe: used to introduce steam from the lower part of the reactor;

[0013] Ring-shaped steam pipe fixing column: used to fix the ring-shaped steam pipe so that the ring-shaped steam pipe will not shake when the steam is introduced, which will cause damage to the equipment;

[0014] Annular steam pipe dispersion hole: The annular steam pipe dispersion hole is used to evenly disperse the steam in the reactor to promote full mixing of the resin and steam in the reactor;

[0015] The fixing ring between the annular steam pipe fixing column and the pipe: used to fix the annular steam pipe and the fixing plate. When steam is passed, large vibration will be generated, so this fixing ring needs to be fixed with a double-layer anti-slip nut and spot welded to prevent it from falling off;

[0016] The steam pipe enters the reactor control valve, which is used to control the time of introducing steam into the reactor, because this device is only installed to remove free phenol in the resin and is put into use at the end of the resin reaction.

[0017] Furthermore, in the manufacturing device of the utility model, the lower steam introduction pipe is distributed in a 180° circular ring shape.

[0018] Furthermore, in the manufacturing device of the utility model, three dispersed holes are set on the same cross section at intervals of 60-90 mm on a 180° circular pipe.

[0019] Furthermore, in the manufacturing device of the utility model, the aperture of the dispersion holes is 2-4 mm.

[0020] Furthermore, the manufacturing device of the utility model has three dispersion holes spaced 45 degrees apart on the same cross section, so that the steam can be evenly dispersed and introduced into the reaction kettle, so that the steam can be fully and evenly mixed with the high-viscosity resin.

[0021] Furthermore, in the manufacturing device of the utility model, the annular steam introduction pipe is fixed with a double-layer anti-skid nut, and the lower part is spot welded to prevent it from falling off due to vibration.

[0022] Compared with the prior art, the utility model has the following effective effects:

[0023] The utility model discloses a manufacturing device for efficiently reducing the free phenol content of solid phenolic resin. Different from the direct steam passing method of the old device, the cleaning steam pipeline is introduced by using a dispersion hole to introduce the steam so that the steam and the resin in the reaction kettle are fully and evenly mixed, thereby improving the phenol removal efficiency, reducing the loss of steam energy and greatly reducing the generation of waste water. BRIEF DESCRIPTION OF THE DRAWINGS

[0024] Figure 1: is a plan view of a manufacturing device for efficiently reducing the free phenol content of solid phenolic resin in an embodiment;

[0025] Figure 2 This is a plan view of the circular steam pipeline structure of the manufacturing device in the embodiment;

[0026] Figure 3 The distribution diagram of the positions and opening diameters of the dispersed holes of the annular steam pipe of the manufacturing device in the embodiment;

[0027] Figure 4 This is a structural diagram of a fixing ring between a circular steam pipe fixing column and a pipe of the manufacturing device in the embodiment;

[0028] In the figure, 100, a control valve for introducing steam into the reactor, 110, a pipeline for introducing steam into the reactor;

[0029] 120. Steam inlet pipe fixing plate; 130. Reactor baffle (Baiffle);

[0030] 140, a steam pipe fixing plate; 150 (1-4), a circular steam pipe fixing column;

[0031] 160. Annular steam pipe fixing column fixing bolt; 170. Annular steam pipe;

[0032] 180. View A of the circular steam pipe dispersion hole;

[0033] 190. View B of the circular steam pipe dispersion hole;

[0034] 200. View C of the circular steam pipe dispersion hole. DETAILED DESCRIPTION

[0035] The technical solutions in the embodiments of the present invention will be described clearly and completely below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all of the embodiments.

[0036] The utility model discloses a manufacturing device for efficiently reducing the free phenol content of solid phenolic resin. The manufacturing device comprises: a steam introduction reactor control valve, a steam introduction reactor pipeline, a steam pipeline fixing plate, a lower 180° annular steam pipeline, a circular annular steam pipeline having dispersion holes at certain intervals, and three dispersion holes are set on the same cross-sectional area of ​​the pipeline, each dispersion hole is distributed at a 45° angle, and the aperture of each dispersion hole needs to be set within a certain range.

[0037] The manufacturing device of the utility model can make steam and high-viscosity resin evenly dispersed and fully mixed, thereby improving production and removal efficiency and is a high-efficiency manufacturing device.

[0038] Example 1

[0039] A manufacturing device for efficiently reducing the free phenol content of solid phenolic resin, such as Figure 1-4 As shown, it includes: a steam introduction reactor control valve 100, a steam introduction reactor pipe 110, an introduction steam pipe fixing plate 120, and another steam pipe fixing plate 140 is fixed on the baffle (Baiffle) 130 of the reactor, and is connected to the reactor through the baffle, so as to enhance the anti-vibration ability of the fixing plate.

[0040] At the same time, the lower part of the pipeline is configured with the annular steam pipeline 170, and four annular steam pipeline fixing columns 150 (1-4) are extended from the reactor wall to fix the annular steam pipeline. The fixing method is: fixed by annular steam pipeline fixing column fixing bolts 160, and the fixing bolts are composed of anti-falling nuts spot-welded to prevent falling off due to vibration during the steam introduction process.

[0041] On the annular steam pipe 170, a 3.5mm dispersion hole 180, 190, 200 should be opened in the three directions A, B and C at intervals of 90mm respectively, so that when the steam is introduced into the reactor, the steam and the resin in the reactor can be fully mixed, and the unreacted free phenol in the resin can be discharged under vacuum.

[0042] Example 2

[0043] A method for preparing a solid phenolic resin comprises the following steps: firstly, adding phenol, formaldehyde and other raw materials into a reaction kettle of Example 1, heating the reaction kettle to 100° C. and maintaining the temperature to carry out a polymerization reaction; after the polymerization reaction is completed, vacuum dehydration is performed until the temperature returns to 170-200° C.

[0044] Under vacuum condition, open the steam introduction control valve 100 for introducing steam into the reactor, introduce steam into the reactor through the steam introduction pipeline 110, and pass through the dispersion holes 150 (1-4) on the annular steam pipeline 170 at the lower part of the reactor, and send the steam into the reactor through the dispersion holes to fully mix the steam with the high viscosity resin in the reactor. Under vacuum condition, the residual free phenol in the unreacted resin is dehydrated with the steam, and after passing through the condenser, the steam containing free phenol is condensed into liquid water and discharged. The softening point of the finished product is detected to be 105±2°C, and the finished product production and material discharge are completed.

[0045] Example 3

[0046] A method for preparing a solid phenolic resin comprises the following steps: firstly, the same molar ratio as in Example 2, i.e., the same amount of phenol, formaldehyde and other raw materials are put into a reaction kettle, and the temperature is raised to 100° C. and maintained to carry out a polymerization reaction. After the polymerization reaction is completed, vacuum dehydration is performed until the temperature rises back to 170-200° C.

[0047] Under vacuum, the steam is passed directly into the reactor through a pipe. This pipe is directly inserted into the resin and mixed with the high-viscosity resin in the reactor. Then, under vacuum, the steam containing free phenol is condensed into liquid water through a condenser and discharged. The softening point of the finished product is tested to be 105±2℃, completing the production of the finished product and the discharge of the material.

[0048] Comparative Example 1

[0049] Table 1: Comparison of the effects of different methods for removing free phenol from resin:

[0050] Table 1 Comparison of the effects of different methods for removing free phenol from resin

[0051] Example 2 Example 3 Finished product softening point 105℃ 105℃ Resin free phenol 0-0.05% 0.2-0.3% Steam introduction time 1.5hr 3hr Energy loss efficiency Low high Production costs Low high

[0052] From the comparison results of the above embodiments, it is known that the device of the utility model can mix the solid phenolic resin more evenly than the conventional steam introduction device, and can separate the unreacted free phenol remaining in the phenolic resin in a shorter time, with low energy loss, lower production costs, and more in line with the requirements of environmentally friendly production.

[0053] The above description is only a preferred embodiment of the present invention and does not constitute any form of limitation to the present invention. Therefore, any simple modification, equivalent change and modification made to the above embodiment based on the technical essence of the present invention without departing from the technical solution of the present invention shall still fall within the scope of the technical solution of the present invention.

Claims

1. A manufacturing device for efficiently reducing the free phenol content of solid phenolic resin, Features It includes: Steam introduction into the reactor control valve is used to control the timing of mixing steam with high-viscosity resin; Steam introduction pipeline for reactor: used to send steam into the reactor to directly contact and mix with the reaction resin; Steam pipe fixing plate, used to fix the steam pipe so that the equipment will not be damaged due to pipe vibration when steam is introduced; 180° circular steam pipe, used to deliver steam to the bottom of the reactor and contact with high viscosity resin; On the circular steam pipe, multiple dispersion holes are set within a distance of 60-90 mm, and different dispersion holes are set at the same cross-sectional position, so that the steam can be evenly mixed with the high-viscosity resin, and the unreacted free phenol can be removed efficiently.

2. The manufacturing device for efficiently reducing the free phenol content of solid phenolic resin according to claim 1, Features: The steam introduction pipeline into the reactor is distributed in a 180° circular ring shape.

3. The manufacturing device for efficiently reducing the free phenol content of solid phenolic resin according to claim 2, Features: On the 180° circular steam pipe, three scattered holes are set up on the same section at intervals of 60-90 mm.

4. The manufacturing device for efficiently reducing the free phenol content of solid phenolic resin according to claim 3, Features: The pore size of the dispersion holes is 2-4 mm.

5. The manufacturing device for efficiently reducing the free phenol content of solid phenolic resin according to claim 4, Features: Three dispersion holes are set at intervals of 45 degrees on the same section of the 180-degree circular steam pipe, so that the steam can be evenly dispersed and introduced into the reactor, so that it can be fully mixed with the high-viscosity resin.

6. The manufacturing device for efficiently reducing the free phenol content of solid phenolic resin according to claim 5, Features: The annular steam pipe is fixed in a manner that the annular steam pipe is fixed on a fixing column by a double-layer anti-skid nut and spot welding to prevent the annular steam pipe from falling off due to vibration.