Forming die for powder metal
By setting up a recycling groove and piston plate in the powder metal forming mold, the problem of connecting waste between the finished products is solved, and seamless molding and efficient production are achieved.
Patent Information
- Application Number
- CN202323632490.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-29
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2033-12-29
AI Technical Summary
During the powder metal molding process, the connecting grooves between the forming grooves lead to the presence of connecting waste between the finished products, which requires cutting and separation, which is troublesome and inefficient.
Design a mold for powder metal, including fixed mold and moving mold, set up a recycling groove and piston plate, use a check valve and a powder recovery, combine a servo motor and sealing ring to achieve negative pressure absorption and isolation Heat insulation.
It avoids connecting waste between finished products, simplifies subsequent processing steps, improves production efficiency, reduces cutting work, and ensures the independence of finished products.
Smart Images

Figure CN222001857U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of forming dies, in particular to a forming die for powder metal. Background Art
[0002] Powder metal forming dies are tools used to manufacture powder metallurgy parts. Powder metallurgy is a manufacturing technology that mixes metal powder with appropriate additives, puts the mixture into a mold, presses it under high pressure, and then solidifies it into a metal part of the desired shape through sintering or heat treatment.
[0003] Mechanical parts formed by powder metal are often smaller and more delicate parts. On this basis, a single injection molding process often processes multiple parts. At this time, connecting grooves are set between adjacent molding grooves, and the injection liquid is injected into different molding grooves through the connecting grooves. After molding, there will be connecting waste between the processed parts, and the waste needs to be cut to obtain independent parts. The whole operation is relatively troublesome. Therefore, a multi-molding groove mold that can directly mold independent parts is designed. Utility Model Content
[0004] The utility model aims to provide a forming die for powder metal in view of the problems existing in the background technology.
[0005] The technical solution of the utility model is as follows: a forming die for powder metal, comprising a fixed die and a movable die, a group of forming grooves are provided on the sides close to each other of the fixed die and the movable die, and the forming grooves are arranged in a one-to-one correspondence, a connecting groove is arranged between the forming grooves, a one-way valve is installed in the connecting groove and at the connection with the forming groove, an injection hole is provided at the center of the fixed die, the injection hole is communicated with the connecting groove, a recovery groove is provided in the fixed die and at a position corresponding to the injection hole, a piston plate is slidably connected in the recovery groove, a connecting hole is provided between the recovery groove and the middle position of the injection hole, and a check valve is fixed in the injection hole and at the outside of the connecting hole.
[0006] Preferably, a servo motor is fixed on the outer side wall of the fixed mold and at a position corresponding to the recovery groove, and a threaded rod is fixed to the output of the servo motor. The end of the threaded rod is rotatably connected in the recovery groove and is threadedly connected to the piston plate.
[0007] Preferably, a limiting block is fixed on the outer side of the piston plate, a limiting groove is provided on the inner side wall of the recovery groove at a position corresponding to the limiting block, and the limiting block is slidably connected in the limiting groove.
[0008] Preferably, a sealing ring is fixed to one end of the piston plate close to the connecting hole.
[0009] Preferably, a heat insulating lining is fixed to the inner wall of the recovery tank.
[0010] Preferably, positioning holes are formed at the four corners of the fixed mold, and positioning rods matching the positioning holes are fixed at the four corners of the fixed mold.
[0011] Compared with the prior art, the utility model has the following beneficial technical effects: a recovery groove is set in the mold, and the metal powder liquid in the connecting groove can be recovered, so that there is no connection waste between multiple finished products, thereby avoiding the trouble of subsequent cutting and separation, and improving production efficiency. BRIEF DESCRIPTION OF THE DRAWINGS
[0012] Figure 1 This is a schematic diagram of the combined structure of the movable mold and the fixed mold of the utility model;
[0013] Figure 2 This is a schematic diagram of the internal structure of the fixed mold of the utility model;
[0014] Figure 3 For this utility model Figure 2 The enlarged structural diagram at A in the middle;
[0015] Figure 4 This is a schematic diagram of the appearance structure of the piston plate of the utility model.
[0016] Figure numerals: 1, fixed mold; 11, positioning hole; 12, injection hole; 13, check valve; 2, movable mold; 21, positioning rod; 3, molding groove; 31, connecting groove; 32, one-way valve; 4, recovery groove; 41, connecting hole; 5, piston plate; 51, sealing ring; 52, limit block; 6, servo motor; 61, threaded rod. DETAILED DESCRIPTION
[0017] The technical solution of the utility model is further described below in conjunction with the accompanying drawings and specific embodiments.
[0018] Example
[0019] like Figure 1-4As shown, the utility model proposes a powder metal forming mold, including a fixed mold 1 and a movable mold 2, a group of forming grooves 3 are opened on the side close to the fixed mold 1 and the movable mold 2, and the forming grooves 3 are arranged one by one, and a connecting groove 31 is arranged between the forming grooves 3, and a one-way valve 32 is installed in the connecting groove 31 and at the connection with the forming groove 3, which can prevent the powder metal liquid in the forming groove 3 from flowing back into the connecting groove 31, an injection hole 12 is opened at the center of the fixed mold 1, and the injection hole 12 is communicated with the connecting groove 31, a recovery groove 4 is opened in the fixed mold 1 and at a position corresponding to the injection hole 12, a piston plate 5 is slidably connected in the recovery groove 4, and a piston plate 5 is opened between the recovery groove 4 and the injection hole 12. There is a connecting hole 41, and a check valve 13 is fixed in the injection hole 12 and on the outside of the connecting hole 41 to prevent the powder metal liquid in the injection hole 12 from flowing back. Positioning holes 11 are opened at the four corners of the fixed mold 1, and positioning rods 21 compatible with the positioning holes 11 are fixed at the four corners of the fixed mold 1. A sealing ring 51 is fixed at one end of the piston plate 5 close to the connecting hole 41. By utilizing the better air tightness of the sealing ring 51, a negative pressure can be formed in the recovery tank 4 when the piston plate 5 slides, thereby absorbing the powder metal liquid. An insulating lining is fixed to the inner wall of the recovery tank 4. By utilizing the heat preservation effect of the insulating lining, the recovered powder metal liquid in the recovery tank 4 is prevented from being cooled and solidified synchronously.
[0020] A servo motor 6 is fixed on the outer wall of the fixed mold 1 and at a position corresponding to the recovery groove 4. A threaded rod 61 is fixed to the output of the servo motor 6. The end of the threaded rod 61 is rotatably connected in the recovery groove 4 and is threadedly connected to the piston plate 5. A limiting block 52 is fixed on the outer side of the piston plate 5. A limiting groove is provided on the inner wall of the recovery groove 4 and at a position corresponding to the limiting block 52. The limiting block 52 is slidably connected in the limiting groove. The output end of the servo motor 6 is used to drive the threaded rod 61 to rotate, and the horizontal limiting of the limiting block 52 is used to realize the telescopic drive of the piston plate 5.
[0021] In this embodiment, the entire device is first connected to an external power supply. After the movable mold 2 and the fixed mold 1 are closed, the powdered metal liquid can be injected into the molding groove 3 through the injection hole 12. During this process, the connecting groove 31 will also be filled with powdered metal liquid. After the molding groove 3 is filled, the sliding of the piston plate 5 can form a negative pressure in the recovery groove 4, thereby absorbing the powdered metal liquid in the injection hole 12 and the connecting groove 31 and allowing it to enter the recovery groove 4. Therefore, there will be no connection waste between the finished products after cooling and molding, so there is no need for subsequent cutting work. During the next injection, the piston plate 5 is pushed outward, and the powdered metal liquid in the recovery groove 4 can be squeezed into the injection hole 12 for supplementary injection. When the piston plate 5 is telescopically controlled, the output end of the servo motor 6 can be used to drive the threaded rod 61 to rotate, and the horizontal limit of the limit block 52 can be used to realize the telescopic drive of the piston plate 5. The thermal insulation effect of the thermal insulation lining is not used to avoid the synchronous cooling and solidification of the recovered powdered metal liquid in the recovery groove 4.
[0022] The above-mentioned specific embodiments are only several preferred embodiments of the present invention. Based on the technical solution of the present invention and the relevant inspiration of the above-mentioned embodiments, those skilled in the art can make various alternative improvements and combinations to the above-mentioned specific embodiments.
Claims
1. A powder metal forming die, comprising a fixed die (1) and a movable die (2), Features: A group of molding grooves (3) are provided on the sides close to the fixed mold (1) and the movable mold (2), and the molding grooves (3) are corresponding to each other. A connecting groove (31) is provided between the molding grooves (3). A check valve (32) is installed in the connecting groove (31) and at the connection with the molding groove (3). An injection hole (12) is provided at the center of the fixed mold (1). The injection hole (12) is communicated with the connecting groove (31). A recovery groove (4) is provided in the fixed mold (1) and at a position corresponding to the injection hole (12). A piston plate (5) is slidably connected in the recovery groove (4). A connecting hole (41) is provided between the recovery groove (4) and the injection hole (12). A check valve (13) is fixed in the injection hole (12) and at the outside of the connecting hole (41).
2. A powder metal forming die according to claim 1, It is characterized in that A servo motor (6) is fixed on the outer wall of the fixed mold (1) and at a position corresponding to the recovery groove (4); a threaded rod (61) is fixed to the output of the servo motor (6); an end of the threaded rod (61) is rotatably connected in the recovery groove (4) and is threadedly connected to the piston plate (5).
3. A powder metal forming die according to claim 1, It is characterized in that A limiting block (52) is fixed on the outer side of the piston plate (5), and a limiting groove is provided on the inner side wall of the recovery groove (4) at a position corresponding to the limiting block (52), and the limiting block (52) is slidably connected in the limiting groove.
4. A powder metal forming die according to claim 1, It is characterized in that A sealing ring (51) is fixed to one end of the piston plate (5) close to the connecting hole (41).
5. A powder metal forming die according to claim 1, It is characterized in that A heat-insulating lining is fixed to the inner wall of the recovery tank (4).