Crescent pouring gate capable of overcoming gas marks
By adopting a crescent gate structure in injection molding technology, the gate gas mark problem in injection molding technology of automobile parts is solved, the stability of product appearance quality and dimensional control is improved, the gate trimming process is simplified, and the cost is reduced.
Patent Information
- Application Number
- CN202323419633.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-14
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2033-12-14
AI Technical Summary
In the existing injection molding technology of automobile parts, the gate marks are serious, resulting in difficulty in controlling the size of the product, difficulty in pruning, unstable quality, and increasing the cost of molds and products.
Using a crescent gate structure, including the main channel, cold material well and split channel, the crescent gate gradually transitions from the middle thick section to the thinning section at both ends, forming a thick section that is easy to flow rapidly and is relatively hindered. Slowly thinning area to avoid air wrapping and prevent air mark defects.
Through the crescent-shaped gate structure, prevent air mark defects in the product appearance, improve the quality and dimensional stability of injection molding, simplify gate trimming, and improve work efficiency.
Smart Images

Figure CN222004284U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the technical field of injection molding of automobile parts production, and particularly relates to a crescent-shaped gate for overcoming air marks. Background Art
[0002] Auto parts such as anti-scratch strips, grilles, grille trims, spoilers, fog lamp trims and other parts are all visible injection molded parts with high appearance requirements. The products do not allow appearance defects such as streaks, shrinkage, punch marks, and air marks. The gate is one of the factors strongly related to air marks. Usually the shape and structure of the gate will determine the appearance quality of the gate area. The products in the prior art have obvious problems with gate air marks, and the product size is difficult to control, the product gate area is difficult to trim, and the quality is unstable. The problems caused by air marks, such as multiple process trials, structural changes, paint bites, electroplating defects, etc., greatly increase the cost of molds and products. Utility Model Content
[0003] The technical problem to be solved by the utility model is to provide a crescent-shaped gate which has more stable injection molding filling, high gate trimming rate and solves the appearance gas mark defects in the gate area of the injection molded part, in view of the current status of the prior art.
[0004] The technical solution adopted by the utility model to solve the above-mentioned technical problems is: a crescent-shaped gate for overcoming air marks, including a main channel, a cold material well and a branch channel, the injection melt flows to the cold material well through the main channel, and then is branched to the branch channel, and is characterized in that the branch channel is provided with a crescent-shaped gate, and a thick area that is easy for the melt to flow quickly is formed in the middle of the crescent-shaped gate, and thinning areas that are easy for the melt to flow relatively slowly and are relatively obstructed are formed on both ends, and the injection melt is injected into the mold cavity through the crescent-shaped gate.
[0005] In the above-mentioned crescent-shaped gate for overcoming air marks, the crescent-shaped gate gradually transitions and becomes thinner from the thick area in the middle to the thinning areas at both ends.
[0006] In the above-mentioned crescent-shaped gate for overcoming air marks, the height H of the crescent-shaped gate is equal to the product wall thickness*1-2.
[0007] In the above-mentioned crescent-shaped gate for overcoming air marks, the height W in the middle of the crescent-shaped gate = product wall thickness * 3 / 4.
[0008] In the above-mentioned crescent-shaped gate for overcoming air marks, the length L of the crescent-shaped gate = product wall thickness * 5-10.
[0009] In the above-mentioned crescent-shaped gate for overcoming air marks, the width V of both ends of the crescent-shaped gate is W*1 / 2.
[0010] Compared with the prior art, the advantage of the utility model lies in the crescent-shaped gate structure style that is thick in the middle and gradually becomes thinner at both ends. The crescent-shaped gate structure is thick in the middle and thin at both ends, and the reasonable shape and size ratio relationship is used to prevent the plastic melt from being trapped in the air, thereby achieving the effect of preventing the product appearance gas mark defects. The overall injection molding filling behavior is more conducive to injection molding, and the product size and appearance quality are more stable than the traditional method. The appearance gas mark defects in the gate area of the injection molded part are solved, which is more conducive to gate trimming and improves work efficiency. BRIEF DESCRIPTION OF THE DRAWINGS
[0011] Figure 1 This is a schematic diagram of the overall structure of the crescent-shaped gate that overcomes the gas mark;
[0012] Figure 2 It is a schematic diagram of the Z-direction structure of a crescent-shaped gate. DETAILED DESCRIPTION
[0013] The following are specific embodiments of the present invention and the accompanying drawings to further describe the technical solution of the present invention, but the present invention is not limited to these embodiments.
[0014] In the figure, the main channel 1; the cold material well 2; the branch channel 3; the crescent-shaped gate 4; the thick area 5; and the thinning area 6.
[0015] like Figure 1 and Figure 2As shown, the crescent-shaped gate for overcoming air marks includes a main channel 1, a cold material well 2 and a branch channel 3. The injection melt flows to the cold material well 2 through the main channel 1, and then is branched to the branch channel 3. Here, the branch channel 3 on the patent is provided with a crescent-shaped gate 4, and the injection melt is injected into the mold cavity through the crescent-shaped gate 4. The relevant dimensions of the crescent-shaped gate 4 are determined according to the product thickness, specifically, the height H of the crescent-shaped gate 4 = product wall thickness * 1-2; the height W in the middle of the crescent-shaped gate 4 = product wall thickness * 3 / 4; the length L of the crescent-shaped gate 4 = product wall thickness * 5-10; the width V at both ends of the crescent-shaped gate 4 = W * 1 / 2, a thick area 5 for easy rapid flow of the melt is formed in the middle of the crescent-shaped gate 4, and thinning areas 6 for easy slow flow of the melt are formed at both ends, that is to say, the entire crescent-shaped gate 4 is thick in the middle and thin at both ends. In the state, the crescent-shaped gate 4 gradually transitions from the thick area 5 in the middle to the thinning areas 6 at both ends. When the viscoelastic melt of the traditional rectangular gate flows in the flow channel, there will be tension accumulation at the right angles and acute angles. When the tension reaches a certain critical value, it will collapse. At this time, the gas is easily entrained and brought into the cavity, forming appearance defects such as gas marks and silver streaks on the surface of the product. The structure of the crescent-shaped gate 4 is thick in the middle and thin at both ends. The material flow channel in the middle is spacious, which is easy for the molten material to flow quickly. The walls at both ends of the gate are thin, and the melt flow is relatively obstructed and slow, thereby forming a fountain flow trend that is beneficial to injection molding, in which the material flow in the middle is relatively fast and the material flow at both ends is relatively slow. Moreover, because the two ends of the gate are arc-shaped and gradually thinned, the gas in the molten material is not easy to be entrained, thereby preventing the occurrence of gas mark defects, solving the appearance gas mark defects in the gate area of the injection molded part, and being more conducive to gate trimming and improving work efficiency.
[0016] The specific embodiments described in this article are merely examples of the spirit of the present invention. Technicians in the technical field to which the present invention belongs can make various modifications or additions to the described specific embodiments or replace them in a similar manner, but they will not deviate from the scope defined by the spirit of the present invention.
Claims
1. A crescent-shaped gate for overcoming gas marks, comprising a main channel, a cold well and a diverter channel, wherein the injection molten material flows through the main channel to the cold well and then to the diverter channel, characterized in that: The branch channel is provided with a crescent-shaped gate, a thick area is formed in the middle of the crescent-shaped gate for the molten material to flow quickly, and thinning areas are formed at both ends for the molten material to flow relatively slowly and with relatively obstruction. The injection molding molten material is injected into the mold cavity through the crescent-shaped gate.
2. A crescent-shaped gate for overcoming gas marks according to claim 1, characterized in that: The crescent-shaped gate gradually transitions and becomes thinner from the thick area in the middle to the thinning areas at both ends.
3. A crescent-shaped gate for overcoming gas marks according to claim 2, characterized in that: The height H of the crescent-shaped gate = product wall thickness * 1-2.
4. A crescent-shaped gate for overcoming gas marks according to claim 3, characterized in that: The height W in the middle of the crescent-shaped gate = product wall thickness * 3 / 4.
5. A crescent-shaped gate for overcoming gas marks according to claim 4, characterized in that: The length L of the crescent-shaped gate = product wall thickness * 5-10.
6. A crescent-shaped gate for overcoming gas marks according to claim 5, characterized in that: The width V at both ends of the crescent-shaped gate is W*1 / 2.