Structure capable of detecting electroplating thickness in manufacturing process
Patent Information
- Application Number
- CN202323626023.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-28
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2033-12-28
AI Technical Summary
In the prior art, the electroplating thickness detection efficiency of ceramic substrates is low and affects the appearance of the product, and an efficient method of detecting the electroplating thickness during the manufacturing process is needed.
A structure is designed, including a ceramic substrate, a first line layer, a first plating layer and a second plating layer. The test zero surface and a height detection surface are formed by electroplating, and the electroplating thickness is detected by external detection instruments to avoid manual excavation. Dry film.
It improves the efficiency of electroplating thickness detection without affecting the appearance of the product, bringing convenience to production.
Smart Images

Figure CN222016879U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the field of ceramic substrate electroplating technology, in particular to a structure capable of detecting electroplating thickness during a manufacturing process. Background Art
[0002] Based on the thin film circuit process, the ceramic surface is metallized by magnetron sputtering, and the copper layer thickness is greater than 10 microns by electroplating. That is DPC (Direct Plate Copper). The thin film method is the main method for metal film deposition in microelectronics manufacturing, among which direct copper plating is the most representative. Direct copper plating (DPC) mainly uses surface deposition processes such as evaporation and magnetron sputtering to metallize the substrate surface. First, titanium is sputtered under vacuum conditions, then copper particles, and finally electroplating thickening. Then the circuit is completed by ordinary PCB process, and finally the thickness of the circuit is increased by electroplating / chemical plating deposition. The preparation method of DPC includes vacuum coating, wet coating, exposure and development, etching and other process links, so the price of its products is relatively high. The DPC process is suitable for most ceramic substrates.
[0003] In the process of manufacturing DPC ceramic substrates, it is necessary to detect the electroplating thickness on the ceramic substrate to ensure the accuracy of the electroplating thickness. In the prior art, the electroplating thickness is generally detected by manually digging the dry film and then using a detection instrument to detect the electroplating thickness. This method has low detection efficiency and seriously affects the product appearance. Therefore, it is necessary to study a solution to solve the above problems. Utility Model Content
[0004] In view of this, the present invention aims to address the deficiencies in the prior art, and its main purpose is to provide a structure that can detect the thickness of electroplating during the manufacturing process, which can effectively solve the problems of low efficiency and poor product appearance in the existing method of detecting the thickness of electroplating.
[0005] In order to achieve the above purpose, the utility model adopts the following technical solutions:
[0006] A structure capable of detecting electroplating thickness in a manufacturing process comprises a ceramic substrate and a first circuit layer; the first circuit layer is formed on the surface of the ceramic substrate by electroplating; a first resist layer is arranged on the first circuit layer, the surface of the first resist layer is flush with the surface of the first circuit layer, and the surface of the first resist layer has a test zeroing surface; a second resist layer is arranged on the surface of the first circuit layer and the surface of the first resist layer, a first window and a second window are arranged on the second resist layer, the surface of the first circuit layer is partially exposed in the first window, the test zeroing surface is exposed in the second window, and a second circuit layer is formed in the first window by electroplating, the second circuit layer is stacked and formed with the first circuit layer, the surface of the second circuit layer is a height detection surface, and a height misalignment is formed between the height detection surface and the test zeroing surface.
[0007] As a preferred solution, the first plating resist layer is a dry film or a solder resist insulating material.
[0008] As a preferred solution, the second plating resist layer is a dry film or a solder resist insulating material.
[0009] As a preferred solution, both the first circuit layer and the second circuit layer are made of copper-plated material.
[0010] As a preferred solution, there are five first resist layers distributed at the four corners and the middle of the ceramic substrate, and the surface of each first resist layer has a test zeroing surface to accurately detect the electroplating thickness at various locations on the ceramic substrate.
[0011] Compared with the prior art, the utility model has obvious advantages and beneficial effects. Specifically, it can be seen from the above technical solution that:
[0012] A first resist is provided on the first circuit layer, the surface of the first resist is used as a test zeroing surface, and a height detection surface is formed on the surface of the second circuit layer. A height misalignment is formed between the height detection surface and the test zeroing surface, so that the thickness of the electroplating can be detected by an external detection instrument without manually digging out the dry film for detection, thereby effectively improving the detection efficiency, not affecting the appearance of the product, and bringing convenience to production.
[0013] In order to more clearly illustrate the structural features and functions of the present invention, the present invention is described in detail below in conjunction with the accompanying drawings and specific embodiments. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] Figure 1 It is a partial cross-sectional view of a preferred embodiment of the utility model.
[0015] Description of the accompanying drawings:
[0016] 10. Ceramic substrate 20. First circuit layer
[0017] 30. First resist coating 31. Test zeroing surface
[0018] 40. Second resist layer 41. First window
[0019] 42. Second window 50. Second circuit layer
[0020] 51. Height detection surface. DETAILED DESCRIPTION
[0021] Please refer to Figure 1 As shown, it shows the specific structure of a preferred embodiment of the utility model, including a ceramic substrate 10 and a first circuit layer 20.
[0022] The first circuit layer 20 is formed on the surface of the ceramic substrate 10 by electroplating; a first resist layer 30 is arranged on the first circuit layer 20, and the surface of the first resist layer 30 is flush with the surface of the first circuit layer 20, and the surface of the first resist layer 30 has a test zeroing surface 31. In this embodiment, the first circuit layer 20 is made of copper-plated material with good conductivity. The first resist layer 30 is a dry film or solder resist insulating material, and can also be other insulating materials, without limitation. In addition, there are five first resist layers 30, which are distributed at the four corners and the middle position of the ceramic substrate 10, and the surface of each first resist layer 30 has a test zeroing surface 31, so as to accurately detect the electroplating thickness at various locations on the ceramic substrate 10.
[0023] The surface of the first circuit layer 20 and the surface of the first resist coating 30 are provided with a second resist coating 40, and the second resist coating 40 is provided with a first window 41 and a second window 42, the surface of the first circuit layer 20 is partially exposed in the first window 41, the test zeroing surface 31 is exposed in the second window 42, and a second circuit layer 50 is formed in the first window 41 by electroplating, and the second circuit layer 50 is superimposed and formed with the first circuit layer 20, and the surface of the second circuit layer 50 is a height detection surface 51, and a height misalignment is formed between the height detection surface 51 and the test zeroing surface 31. In the present embodiment, the second resist coating 40 is a dry film or solder resist insulating material, and may also be other insulating materials, without limitation. The second circuit layer 50 is made of copper-plated material and has good conductivity.
[0024] The production process of this embodiment is described in detail as follows:
[0025] First, a ceramic substrate 10 is taken, and a first circuit layer 20 is formed by electroplating on the ceramic substrate 10. Then, a first resist layer 30 is arranged at a suitable position of the first circuit layer 20 so that the surface of the first resist layer 30 is flush with the surface of the first circuit layer 20. Then, when performing a second pattern electroplating, a second resist layer 40 is arranged on the surface of the first circuit layer 20 and the surface of the first resist layer 30. Then, a first window 41 and a second window 42 are arranged on the second resist layer 40 by exposure and development, and then a second electroplating is performed. Since the first circuit layer 20 is exposed in the first window 41, a second circuit layer 50 is formed in the first window 41. Since there is no coating in the second window 42, electroplating cannot be performed, and the test zeroing surface 31 remains exposed in the second window 42. At this time, the height detection surface 51 on the second circuit layer 50 is displaced with the test zeroing surface 31, so that the thickness of the electroplating can be detected using an external detection instrument.
[0026] The design focus of the utility model is that a first resist coating is provided on the first circuit layer, the surface of the first resist coating is used as a test zeroing surface, and a height detection surface is formed on the surface of the second circuit layer. A height misalignment is formed between the height detection surface and the test zeroing surface, so that an external detection instrument can be used to detect the thickness of the electroplating, without the need for manual digging of the dry film for detection, thereby effectively improving the detection efficiency, and will not affect the appearance of the product, bringing convenience to production.
[0027] The above description is only a preferred embodiment of the present invention and does not limit the technical scope of the present invention. Therefore, any slight modifications, equivalent changes and modifications made to the above embodiments based on the technical essence of the present invention are still within the scope of the technical solution of the present invention.
Claims
1. A structure capable of detecting the thickness of electroplating during a manufacturing process, comprising a ceramic substrate and a first circuit layer; the first circuit layer is formed on the surface of the ceramic substrate by electroplating; characterized in that: A first resist coating is arranged on the first circuit layer, the surface of the first resist coating is flush with the surface of the first circuit layer, and the surface of the first resist coating has a test zeroing surface; a second resist coating is arranged on the surface of the first circuit layer and the surface of the first resist coating, and a first window and a second window are arranged on the second resist coating, the surface of the first circuit layer is partially exposed in the first window, the test zeroing surface is exposed in the second window, and a second circuit layer is formed in the first window by electroplating, the second circuit layer is stacked and formed together with the first circuit layer, the surface of the second circuit layer is a height detection surface, and a height misalignment is formed between the height detection surface and the test zeroing surface.
2. The structure capable of detecting the thickness of electroplating during the manufacturing process according to claim 1, characterized in that: The first plating resist layer is a dry film or a solder resist insulating material.
3. The structure capable of detecting the thickness of electroplating during the manufacturing process according to claim 1, characterized in that: The second plating resist layer is a dry film or a solder resist insulating material.
4. The structure capable of detecting the thickness of electroplating during the manufacturing process according to claim 1, characterized in that: The first circuit layer and the second circuit layer are both made of copper-plated materials.
5. The structure capable of detecting the thickness of electroplating during the manufacturing process according to claim 1, characterized in that: There are five first resist layers, which are distributed at four corners and a middle position of the ceramic substrate, and the surface of each first resist layer has a test zeroing surface.