High-temperature-resistant and low-temperature-resistant composite film
By designing a high-temperature and low-temperature composite film in the food packaging film, combining PA, EVOH, PE and bamboo charcoal film layers, the problems of brittleness and lack of antibacterial structure of polyethylene film are solved, and better anti-puncture and antibacterial structure are achieved. and temperature stability extend the shelf life of food.
Patent Information
- Application Number
- CN202420049299.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-01-09
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2034-01-09
AI Technical Summary
The existing polyethylene food packaging film is insufficiently brittle and lacks antibacterial structural layer, which leads to food being easily damaged and bacterial erosion, making it difficult to preserve for a long time.
Design a composite film that is resistant to high and low temperatures, including oxygen insulation layer, antibacterial layer and temperature-resistant protective layer. The PA, EVOH, PE, BOPP and bamboo charcoal film layers are combined through extrusion molding technology to form an integrated structure to enhance puncture resistance , block oxygen and antibacterial ability, and set up a protective layer with high temperature and low temperature resistance to improve the overall performance of the film.
It effectively improves the puncture resistance, antibacterial ability and temperature stability of food packaging, avoids the problems of food being vulnerable to damage and bacterial erosion, and extends the shelf life of food.
Smart Images

Figure CN222022340U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the technical field of composite films, and in particular relates to a composite film that is resistant to high and low temperatures. Background Art
[0002] Composite film is a film composed of two or more materials, which are combined by chemical or physical methods to form a new material. Due to its excellent performance, it has been widely used in many fields such as food packaging and medical packaging.
[0003] Most of the existing food packaging films are polyethylene films. Since polyethylene has a certain degree of brittleness and lacks a structural layer that can inhibit bacteria, the food packaging is easily damaged and the food inside is easily corroded by bacteria, making it difficult to preserve the food for a long time. For this reason, we provide a high-temperature and low-temperature resistant composite film. Utility Model Content
[0004] The purpose of the utility model is to provide a composite film that is resistant to high and low temperatures; to solve the problem in the above-mentioned background technology that polyethylene has a certain brittleness and the polyethylene film lacks a structural layer that can inhibit bacteria, making food packaging easily damaged and the food inside it easily corroded by bacteria, making it difficult to preserve the food for a long time.
[0005] A high-temperature and low-temperature resistant composite film comprises an oxygen-isolating layer, an antibacterial layer, a heat-resistant protective layer and an inner layer; the antibacterial layer is arranged at the bottom of the oxygen-isolating layer, the heat-resistant protective layer is arranged at the bottom of the antibacterial layer, the inner layer is arranged at the bottom of the heat-resistant protective layer, and the layers are bonded to each other.
[0006] Furthermore, the oxygen-isolating layer is an integrated structure formed by extrusion molding, and the oxygen-isolating layer includes a PA surface layer, an EVOH barrier layer, a PA middle layer and a PE layer; the EVOH barrier layer is arranged at the bottom of the PA surface layer, the PA middle layer is arranged at the bottom of the EVOH barrier layer, and the PE layer is arranged at the bottom of the PA middle layer.
[0007] Furthermore, the thickness of the PA surface layer is consistent with that of the PA middle layer.
[0008] Furthermore, the antibacterial layer is an integrated structure formed by extrusion molding, and the antibacterial layer includes a BOPP layer, a first bamboo charcoal film layer and a second bamboo charcoal film layer; the first bamboo charcoal film layer and the second bamboo charcoal film layer are respectively arranged on the top and bottom of the BOPP layer.
[0009] Furthermore, the heat-resistant protective layer is an integrated structure formed by extrusion molding, and the heat-resistant protective layer includes a low-temperature resistant protective layer and a high-temperature resistant protective layer; a high-temperature resistant protective layer is arranged at the bottom of the low-temperature resistant protective layer.
[0010] The utility model has the following advantages:
[0011] 1. The PA surface layer provided in the present invention can provide good puncture resistance and excellent strength performance. By adding a PA middle layer having the same thickness as the PA surface layer, the puncture resistance and strength performance of the film can be improved, further preventing the film from being easily damaged.
[0012] 2. The utility model can effectively block oxygen by setting up the EVOH barrier layer, thereby isolating bacteria in the oxygen, and the two layers of bamboo charcoal film layers can play a good antibacterial role, further improving the preservation ability of food; the low-temperature resistant protective layer and the high-temperature resistant protective layer can improve the high-temperature resistance and low-temperature resistance of the film.
[0013] 3. The utility model effectively avoids the problem that the food packaging is easily damaged and the food inside is easily corroded by bacteria, making it difficult to preserve the food for a long time because polyethylene has a certain brittleness and the polyethylene film lacks a structural layer that can inhibit bacteria.
[0014] The high-temperature and low-temperature resistant composite film of the utility model is suitable for the packaging industry. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 Schematic diagram of the high-temperature and low-temperature resistant composite film of the utility model; 1 represents the oxygen barrier layer, 2 represents the antibacterial layer, 3 represents the temperature-resistant protective layer, and 4 represents the inner layer;
[0016] Figure 2 for Figure 1 The enlarged structural diagram at A in the middle, wherein 101 represents the PA surface layer, 102 represents the EVOH barrier layer, 103 represents the PA middle layer, 104 represents the PE layer, 201 represents the BOPP layer, 202 represents the first bamboo charcoal film layer, and 202 represents the second bamboo charcoal film layer;
[0017] Figure 3 for Figure 1 The enlarged structural diagram at B in the middle shows that 301 represents a low-temperature resistant protective layer and 302 represents a high-temperature resistant protective layer. DETAILED DESCRIPTION
[0018] The technical solution of the present utility model is not limited to the specific implementation modes listed below, but also includes any combination of the specific implementation modes.
[0019] Specific implementation method 1: Combination Figure 1-Figure 3As shown, the present embodiment is a high temperature and low temperature resistant composite film, characterized in that it includes an oxygen isolation layer 1, an antibacterial layer 2, a heat resistant protective layer 3 and an inner layer 4; the antibacterial layer 2 is arranged at the bottom of the oxygen isolation layer 1, the heat resistant protective layer 3 is arranged at the bottom of the antibacterial layer 2, and the inner layer 4 is arranged at the bottom of the heat resistant protective layer 3, and the layers are bonded to each other.
[0020] In this embodiment, the adhesive used for mutual bonding is made of an adhesive resin material.
[0021] Specific embodiment 2: This embodiment is different from specific embodiment 1 in that the oxygen barrier layer 1 is an integral structure formed by extrusion molding, and the oxygen barrier layer 1 includes a PA surface layer 101, an EVOH barrier layer 102, a PA middle layer 103 and a PE layer 104; the EVOH barrier layer 102 is arranged at the bottom of the PA surface layer 101, the PA middle layer 103 is arranged at the bottom of the EVOH barrier layer 102, and the PE layer 104 is arranged at the bottom of the PA middle layer 103. The rest is the same as specific embodiment 1.
[0022] In this embodiment, the oxygen barrier layer 1 is an integral structure formed by extrusion molding and can play a role in isolating oxygen.
[0023] Specific embodiment 3: This embodiment is different from specific embodiment 1 in that the thickness of the PA surface layer 101 is consistent with that of the PA middle layer 103. Other aspects are the same as those of specific embodiment 1.
[0024] In this embodiment, the thickness of the PA surface layer 101 is consistent with that of the PA middle layer 103 , which can improve the puncture resistance and strength performance of the film.
[0025] Specific embodiment 4: This embodiment is different from the specific embodiment 1 in that the antibacterial layer 2 is an integrated structure formed by extrusion molding, and the antibacterial layer 2 includes a BOPP layer 202, a first bamboo charcoal film layer 201, and a second bamboo charcoal film layer 203; the first bamboo charcoal film layer 201 and the second bamboo charcoal film layer 203 are respectively disposed on the top and bottom of the BOPP layer 202. The rest is the same as the specific embodiment 1.
[0026] In this embodiment, the antibacterial layer 2 is an integrated structure formed by extrusion molding, which can play an antibacterial role.
[0027] Specific embodiment 5: This embodiment is different from specific embodiment 1 in that the heat-resistant protective layer 3 is an integral structure formed by extrusion molding, and the heat-resistant protective layer 3 includes a low-temperature resistant protective layer 301 and a high-temperature resistant protective layer 302; the high-temperature resistant protective layer 302 is disposed at the bottom of the low-temperature resistant protective layer 301. The rest is the same as specific embodiment 1.
[0028] In this embodiment, the heat-resistant protective layer 3 is an integrated structure formed by extrusion molding, which can improve the high temperature resistance and low temperature resistance of the film.
[0029] The beneficial effects of the present invention are verified by the following examples:
[0030] Example:
[0031] Combination Figure 1-Figure 3 As shown, the present embodiment is a high temperature and low temperature resistant composite film, which includes an oxygen insulation layer 1, an antibacterial layer 2, a heat resistant protective layer 3 and an inner layer 4; the antibacterial layer 2 is arranged at the bottom of the oxygen insulation layer 1, the heat resistant protective layer 3 is arranged at the bottom of the antibacterial layer 2, and the inner layer 4 is arranged at the bottom of the heat resistant protective layer 3, and the layers are bonded to each other.
[0032] The oxygen-isolating layer 1 described in this embodiment is an integrated structure formed by extrusion molding, and the oxygen-isolating layer 1 includes a PA surface layer 101, an EVOH barrier layer 102, a PA middle layer 103 and a PE layer 104; the EVOH barrier layer 102 is arranged at the bottom of the PA surface layer 101, the PA middle layer 103 is arranged at the bottom of the EVOH barrier layer 102, and the PE layer 104 is arranged at the bottom of the PA middle layer 103.
[0033] In this embodiment, the thickness of the PA surface layer 101 is consistent with that of the PA middle layer 103 .
[0034] The antibacterial layer 2 described in this embodiment is an integrated structure formed by extrusion molding, and the antibacterial layer 2 includes a BOPP layer 202, a first bamboo charcoal film layer 201 and a second bamboo charcoal film layer 203; the first bamboo charcoal film layer 201 and the second bamboo charcoal film layer 203 are respectively arranged on the top and bottom of the BOPP layer 202.
[0035] The heat-resistant protective layer 3 in this embodiment is an integrated structure formed by extrusion molding, and the heat-resistant protective layer 3 includes a low-temperature resistant protective layer 301 and a high-temperature resistant protective layer 302 ; the high-temperature resistant protective layer 302 is arranged at the bottom of the low-temperature resistant protective layer 301 .
[0036] The layers described in this embodiment are bonded to each other, and the adhesive used is made of an adhesive resin material.
[0037] In this embodiment, the oxygen-isolating layer 1 is an integral structure formed by extrusion molding and can play a role in isolating oxygen.
[0038] In this embodiment, the thickness of the PA surface layer 101 is consistent with that of the PA middle layer 103, which can improve the puncture resistance and strength performance of the film.
[0039] In this embodiment, the antibacterial layer 2 is an integrated structure formed by extrusion molding and can play an antibacterial role.
[0040] In this embodiment, the heat-resistant protective layer 3 is an integrated structure formed by extrusion molding, which can improve the high temperature resistance and low temperature resistance of the film.
[0041] The implementation principle of a high-temperature and low-temperature resistant composite film in this embodiment is as follows: the PA surface layer 101 provided can have good puncture resistance and excellent strength performance, the EVOH barrier layer 102 provided can effectively block oxygen, thereby isolating bacteria in oxygen, and the two layers of bamboo charcoal film layers 202 provided can have a good antibacterial effect, further improving the food preservation ability, and the low-temperature resistant protective layer 301 and the high-temperature resistant protective layer 302 provided can improve the high-temperature and low-temperature resistance of the film.
[0042] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Although the present invention has been described in detail with reference to the aforementioned embodiments, it is still possible for those skilled in the art to modify the technical solutions described in the aforementioned embodiments or to replace some of the technical features therein with equivalents. Any modifications, equivalent replacements, improvements, etc. made within the spirit and principles of the present invention shall be included in the protection scope of the present invention.
Claims
1. A high temperature and low temperature resistant composite film, characterized in that It comprises an oxygen-isolating layer (1), an antibacterial layer (2), a heat-resistant protective layer (3) and an inner layer (4); the antibacterial layer (2) is arranged at the bottom of the oxygen-isolating layer (1), the heat-resistant protective layer (3) is arranged at the bottom of the antibacterial layer (2), and the inner layer (4) is arranged at the bottom of the heat-resistant protective layer (3), and the layers are bonded to each other.
2. A high temperature and low temperature resistant composite film according to claim 1, characterized in that The oxygen barrier layer (1) is an integrated structure formed by extrusion molding, and comprises a PA surface layer (101), an EVOH barrier layer (102), a PA middle layer (103) and a PE layer (104); the EVOH barrier layer (102) is arranged at the bottom of the PA surface layer (101), the PA middle layer (103) is arranged at the bottom of the EVOH barrier layer (102), and the PE layer (104) is arranged at the bottom of the PA middle layer (103).
3. A high temperature and low temperature resistant composite film according to claim 2, characterized in that The thickness of the PA surface layer (101) is consistent with that of the PA middle layer (103).
4. The high temperature and low temperature resistant composite film according to claim 1, characterized in that The antibacterial layer (2) is an integrated structure formed by extrusion molding, and comprises a BOPP layer (202), a first bamboo charcoal film layer (201), and a second bamboo charcoal film layer (203); the first bamboo charcoal film layer (201) and the second bamboo charcoal film layer (203) are respectively arranged on the top and bottom of the BOPP layer (202).
5. The high temperature and low temperature resistant composite film according to claim 1, characterized in that The heat-resistant protective layer (3) is an integrated structure formed by extrusion molding, and the heat-resistant protective layer (3) comprises a low-temperature resistant protective layer (301) and a high-temperature resistant protective layer (302); the high-temperature resistant protective layer (302) is arranged at the bottom of the low-temperature resistant protective layer (301).
Citation Information
Cited By
Low-temperature-resistant, high-barrier and puncture-resistant aluminum foil composite film and food packaging bag