Notebook computer surface treatment structure
By setting oxide film, printing, UV and sealing layers on the surface of aluminum alloy notebooks, the problem of single appearance of aluminum surface is solved, diversified appearance and wear resistance are improved, and the competitiveness of the product is improved.
Patent Information
- Application Number
- CN202323311893.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-06
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2033-12-06
Smart Images

Figure CN222024488U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of surface treatment, in particular to a notebook surface treatment structure. Background Art
[0002] Metal materials are used more and more in various existing products because they can better reflect product quality and highlight brand value. Among the many metal materials, aluminum is the first to be adopted by various manufacturers because of its easy processing, good visual effects and rich surface treatment methods. As consumers' aesthetic ability gradually improves, differentiated products are more attractive and can gain an advantage in the competition.
[0003] In the prior art, the aluminum surface is mostly anodized and colored as the final product appearance, which has a single appearance and cannot present a colorful appearance effect.
[0004] In order to solve the above problems, the present utility model is provided. Utility Model Content
[0005] The utility model aims to provide a notebook surface treatment structure to optimize the appearance of aluminum alloy products and improve product competitiveness.
[0006] Based on the above problems, the technical solution provided by the utility model is:
[0007] A notebook surface treatment structure comprises a substrate layer, an oxide film layer arranged on the surface of the substrate layer, a printing layer arranged on the surface of the oxide film layer, a UV layer arranged on the surface of the printing layer and a sealing layer arranged on the surface of the UV layer.
[0008] In some embodiments, the substrate layer is an aluminum alloy plate.
[0009] In some embodiments, the thickness of the substrate layer is 0.8 to 2 mm.
[0010] In some embodiments, the oxide film has a thickness of 20 to 40 μm.
[0011] In some embodiments, the printed layer has a thickness of 0 to 10 μm.
[0012] In some embodiments, the UV layer has a thickness of 20 to 40 μm.
[0013] In some embodiments, the sealing layer has a thickness of 5 to 20 μm.
[0014] Compared with the prior art, the advantages of the utility model are:
[0015] An oxide film layer and a printing layer are arranged on the surface of the substrate layer. The printing layer can present colorful pattern textures, making the appearance of notebook products diversified and improving the competitiveness of products. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] In order to more clearly illustrate the technical solutions of the embodiments of the utility model, the drawings required for use in the description of the embodiments will be briefly introduced below. The drawings described below are only some embodiments of the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0017] Figure 1 This is a schematic structural diagram of an embodiment of a notebook surface treatment structure of the utility model;
[0018] in:
[0019] 1. Base material layer;
[0020] 2. Oxide film layer;
[0021] 3. Printing layer;
[0022] 4. UV layer;
[0023] 5. Sealing layer. DETAILED DESCRIPTION
[0024] The above scheme is further described below in conjunction with specific examples. It should be understood that these examples are used to illustrate the utility model and are not limited to the scope of the utility model. The implementation conditions used in the examples can be further adjusted according to the conditions of the specific manufacturer, and the implementation conditions not specified are usually the conditions in conventional experiments.
[0025] like Figure 1 As shown, it is a structural schematic diagram of an embodiment of the utility model, which provides a notebook surface treatment structure, including a substrate layer 1, an oxide film layer 2 arranged on the surface of the substrate layer 1, a printing layer 3 arranged on the surface of the oxide film layer 2, a UV layer 4 arranged on the surface of the printing layer 3, and a sealing layer 5 arranged on the surface of the UV layer 4.
[0026] The substrate layer 1 is an aluminum alloy plate with a thickness of 0.8 to 5 mm. In actual implementation, a conventional thickness can be selected, such as 0.8 mm, 1.0 mm, 2.0 mm or thicker.
[0027] The thickness of the oxide film layer 2 is 20 to 40 μm. The product is immersed in the anode tank and energized to generate an oxide film layer 2 on the surface of the substrate layer 1. The surface of the oxide film layer 2 has a microscopically visible uneven structure, which can make the printed layer 3 better adhere to the surface of the substrate layer 1.
[0028] The thickness of the printed layer 3 is 0 to 10 μm. Since the printing ink will be embedded in the uneven structure of the oxide film layer 2, the actual thickness is relatively small. The film layer is generated by a 3D printing device to generate a customized colorful pattern on the surface of the oxide film layer 2, which can make the product surface present rich and colorful colors and pattern effects.
[0029] The thickness of the UV layer 3 is 20-40 μm. During implementation, UV varnish is printed on the surface of the printing layer 3 by screen printing equipment to enhance the glossiness of the overall pattern and further enhance the appearance and texture of the product.
[0030] The thickness of the sealing layer 5 is 5 to 20 μm. The printed product is placed in a prepared sealing water tank to seal the product so that a hardened film layer is formed on the outer surface of the printed layer 3 to provide protection, thereby improving the overall wear resistance of the product.
[0031] In summary, the surface treatment structure enables the product surface to present a rich and colorful color pattern effect, optimizes the product appearance, and improves the product's competitiveness.
[0032] The above examples are only for illustrating the technical concept and features of the utility model, and their purpose is to enable people familiar with the technology to understand the content of the utility model and implement it accordingly, and they cannot be used to limit the protection scope of the utility model. Any equivalent changes or modifications made according to the spirit of the utility model should be included in the protection scope of the utility model.
Claims
1. A notebook surface treatment structure, characterized in that: The invention comprises a substrate layer, an oxide film layer arranged on the surface of the substrate layer, a printing layer arranged on the surface of the oxide film layer, a UV layer arranged on the surface of the printing layer and a sealing layer arranged on the surface of the UV layer.
2. The notebook surface treatment structure according to claim 1, characterized in that: The substrate layer is an aluminum alloy plate.
3. The notebook surface treatment structure according to claim 2, characterized in that: The thickness of the substrate layer is 0.8-2 mm.
4. The notebook surface treatment structure according to claim 1, characterized in that: The thickness of the oxide film is 20-40 μm.
5. The notebook surface treatment structure according to claim 1, characterized in that: The thickness of the printing layer is 0-10 μm.
6. The notebook surface treatment structure according to claim 1, characterized in that: The thickness of the UV layer is 20-40 μm.
7. The notebook surface treatment structure according to claim 1, characterized in that: The sealing layer has a thickness of 5 to 20 μm.