Device for long-term corrosion test of high-level radioactive waste geological disposal packaging container material

By designing a long-term corrosion test device for packaging container materials with high-level waste geological disposal, and using materials such as glycerol or liquid paraffin and bentonite, long-term corrosion test of packaging container materials is realized, and the environment of simulated high-level waste geological disposal library in the existing technology is solved. The problem of corrosion behavior provides a simple, environmentally friendly and multifunctional test method.

CN222049963UActive Publication Date: 2024-11-22INST OF METAL RESEARCH - CHINESE ACAD OF SCI +1
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202420442756.0
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-07
Publication Date
2024-11-22
Estimated Expiration
2034-03-07

AI Technical Summary

Technical Problem

The prior art is difficult to effectively simulate and study the long-term corrosion behavior of packaging container materials in the environment of high-level waste geological disposal warehouses, and the existing test devices have problems such as complex structure, high cost and poor operability.

Method used

A long-term corrosion test device for packaging container materials with high-level waste geological disposal is designed, using open containers, temperature-resistant plastic sealing tanks, buffer materials, temperature-controlled components, electrochemical impedance spectroscopy measurement sensors and silicone rubber, through glycerol or liquid Paraffin is used as the sealing material and bentonite is used as the buffer material to achieve long-term corrosion tests on packaging container materials.

Benefits of technology

It realizes long-term corrosion research on the versatile, strong operability, good sealing, strong stability and real-time measurement of packaging container materials for high-level waste geological disposal, and provides a simple, environmentally friendly, pollution-free test method, applicable Long-term corrosion experiment study on packaging container materials for high-level waste geological disposal.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222049963U_ABST
    Figure CN222049963U_ABST
Patent Text Reader

Abstract

The utility model relates to the field of metal corrosion behavior monitoring and characterization, in particular to a long-term corrosion test device for a high-level radioactive waste geological disposal packaging container material. The test device comprises an open container, a sealing material, a temperature-resistant plastic sealing tank, a buffer material, a temperature control component, a packaging container candidate material test sample, a wire and silicone rubber, the sealing material is arranged in the open container, the temperature-resistant plastic sealing tank is embedded in the sealing material, the buffer material is filled in the temperature-resistant plastic sealing tank, and the temperature control component is arranged in the temperature-resistant plastic sealing tank. A sensor for electrochemical impedance spectroscopy measurement, a corrosion weightlessness sample and a corrosion product characterization sample are embedded in the buffer material; the wire penetrates through a sealing tank top cover of the temperature-resistant plastic sealing tank, and the temperature control component is inserted into the sealing tank top cover of the temperature-resistant plastic sealing tank. The device is suitable for long-term corrosion research and evaluation of a packaging container candidate material in a high-level radioactive waste geological disposal buffer material environment, and has the characteristics of multiple functions, strong operability, good sealing performance, strong stability and real-time measurement.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the field of metal corrosion behavior monitoring and characterization, in particular to a device for long-term corrosion testing of packaging container materials for geological disposal of high-level radioactive waste. Background Art

[0002] High-level radioactive waste (HLW) mainly refers to high-level waste liquid and its solidified form produced by spent fuel reprocessing. HLW is a special type of waste that poses a potential threat to the environment. The radionuclides contained in HLW have the characteristics of strong radioactivity, high toxicity, long half-life and heat generation. Once they enter the human living environment, they are extremely harmful and difficult to eliminate. Therefore, the safe disposal of HLW has become a major issue affecting the sustainable development of nuclear energy, environmental protection and the well-being of future generations, and is also a major problem in science, technology and engineering.

[0003] At present, the internationally recognized method for safe disposal of high-level radioactive waste is deep geological disposal, which means burying high-level radioactive waste in a stable geological body about 400 to 1000 meters below the surface to effectively isolate it from the biosphere. The high-level radioactive waste disposal repository adopts a "multiple barrier system" design, that is, high-level radioactive waste is stored in a disposal container, which is wrapped with buffer materials on the outside and the outermost layer is surrounding rock. The disposal container is generally made of metal materials, and its main safety function is to contain high-level radioactive waste and prevent groundwater from infiltrating for no less than 1000 years. Therefore, it is very necessary to study the corrosion evolution behavior of disposal container materials in the geological disposal repository environment.

[0004] In order to better study the corrosion behavior and evolution characteristics of packaging container materials in a simulated geological repository environment in the laboratory, it is necessary to develop and design test equipment and methods that can effectively isolate the test system from the surrounding atmospheric environment. Utility Model Content

[0005] Aiming at the needs of high-level radioactive waste geological disposal engineering, the purpose of the utility model is to provide a device for long-term corrosion test of high-level radioactive waste geological disposal packaging container materials. The test device has a simple structure, low cost, and various design methods, and is suitable for long-term corrosion test research of high-level radioactive waste geological disposal packaging container materials.

[0006] The technical solution of the utility model is:

[0007] A device for long-term corrosion test of packaging container materials for geological disposal of high-level radioactive waste, comprising an open container, a sealing material, a temperature-resistant plastic sealed tank, a buffer material, a temperature control component, a test sample of candidate packaging container materials, a wire and silicone rubber. The test sample of candidate packaging container materials comprises a sensor for measuring electrochemical impedance spectroscopy, a corrosion weight loss sample and a sample for characterizing corrosion products. The specific structure is as follows:

[0008] The open container is filled with sealing material, in which a heat-resistant plastic sealed tank is buried, in which a buffer material is filled, in which a sensor for electrochemical impedance spectroscopy measurement, a corrosion weight loss sample, and a sample for corrosion product characterization are buried; a wire is passed through the sealed tank top cover of the heat-resistant plastic sealed tank, the lower end of which is connected to the sensor for electrochemical impedance spectroscopy measurement, and the upper end of which is led out of the open container; a temperature control component is inserted into the sealed tank top cover of the heat-resistant plastic sealed tank, the lower end of which extends into the buffer material, and the upper end of which is led out of the open container; the sealed tank top cover and the heat-resistant plastic sealed tank are sealed by silicone rubber, and the wire, the temperature control component and the sealed tank top cover are sealed by silicone rubber.

[0009] In the device for long-term corrosion testing of packaging container materials for geological disposal of high-level radioactive waste, the test sample of candidate packaging container materials and the temperature control component have no direct contact with each other and are buried in a buffer material and are sealed together in a heat-resistant plastic sealed can; the sealed heat-resistant plastic sealed can is placed in an open container and the heat-resistant plastic sealed can is submerged with a sealing material.

[0010] The device for long-term corrosion test of packaging container materials for geological disposal of high-level radioactive waste, the sensor for electrochemical impedance spectrum measurement is composed of a first electrode and a second electrode of the same material, the first electrode and the second electrode have more than three comb teeth so that the first electrode and the second electrode are interlaced with each other in a comb shape, there is a gap between adjacent comb teeth, and the gap is not greater than 0.3mm, the test surface area of ​​the first electrode and the second electrode is 1cm 2 .

[0011] The device for long-term corrosion test of packaging container materials for geological disposal of high-level radioactive waste is characterized in that the first electrode and the second electrode are fixed between and on the outside by filling with high-temperature resistant insulating resin, the upper end surface of the sensor for electrochemical impedance spectroscopy measurement is the test surface, the upper surfaces of the first electrode and the second electrode are exposed and flush with the test surface, a wire is led out from the non-exposed side of the first electrode and the second electrode respectively through a reserved notch on the top cover of the sealing tank of the heat-resistant plastic sealing tank for electrochemical impedance spectroscopy data collection, and the remaining gap in the reserved notch after the wire is led out is sealed with silicone rubber.

[0012] In the device for long-term corrosion test of packaging container materials for geological disposal of high-level radioactive waste, the temperature control component is located in the buffer material and is led out through a reserved notch on the top cover of the heat-resistant plastic sealed tank and connected to a power supply. After the temperature control component is led out, the remaining gap is sealed with silicone rubber.

[0013] In the device for long-term corrosion test of packaging container materials for geological disposal of high-level radioactive waste, after the heat-resistant plastic sealed tank is sealed, silicone rubber is used to seal the sealing circumference of the heat-resistant plastic sealed tank and the sealing tank top cover.

[0014] The device for long-term corrosion testing of packaging container materials for geological disposal of high-level radioactive waste has at least three parallel corrosion weight loss samples, and the sample size is not less than 20mm×10mm×3mm; the number of samples for corrosion product characterization is at least three, and the sample size is not less than 10mm×10mm×2mm.

[0015] The device for long-term corrosion test of packaging container materials for geological disposal of high-level radioactive waste has a sealing material of glycerin or liquid paraffin and a buffer material of bentonite.

[0016] The design idea of ​​the utility model is:

[0017] (1) The utility model utilizes the fluidity of glycerin or liquid paraffin and the characteristics of not reacting with water and silicone rubber. Using it as a sealing material can effectively isolate the isolated heat-resistant plastic sealed can with a lid from the air environment.

[0018] (2) Glycerin or liquid paraffin has a high ignition point and is non-toxic. It can provide long-term and stable isolation for the heat-resistant plastic sealed cans with lids that are isolated at temperatures below 130°C.

[0019] (3) While measuring the electrochemical impedance spectrum of the electrode made of the candidate material for the geological disposal of high-level radioactive waste packaging container, the corrosion weight loss sample and the corrosion product characterization sample are placed in the buffer material system, so that the corrosion rate of the candidate material for the packaging container can be monitored while the corrosion parameters such as the morphology, phase composition, and corrosion type of the corrosion product can be detected. Therefore, the utility model is suitable for the long-term corrosion research and evaluation of the candidate material for the packaging container in the buffer material environment of the geological disposal of high-level radioactive waste, and has the characteristics of multi-function, strong operability, good sealing, strong stability, and real-time measurement.

[0020] Compared with the prior art, the advantages and beneficial effects of the utility model are:

[0021] (1) The sealing material used in the present invention is a viscous liquid with good fluidity. The material is easily available, non-toxic, and not easily volatile. It can effectively isolate the air environment of the temperature-resistant plastic sealed can with a lid, and effectively avoids the disadvantages of other sealing methods such as poor reliability and durability.

[0022] (2) The long-term corrosion test method for packaging container materials for geological disposal of high-level radioactive waste provided by the utility model has simple process, is environmentally friendly and pollution-free, has stable isolation effect, and has a simple device structure, diverse design methods, and strong operability. It is suitable for long-term corrosion test research on packaging container materials for geological disposal of high-level radioactive waste. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Figure 1This is a schematic diagram of a device for long-term corrosion testing of packaging container materials for geological disposal of high-level radioactive waste according to an embodiment of the utility model;

[0024] Figure 2 for Figure 1 Side view of the structure of the sensor used for electrochemical impedance spectroscopy measurement.

[0025] Description of reference numerals:

[0026] 10. Equipment for long-term corrosion test of packaging container materials for geological disposal of high-level radioactive waste; 100. Open container; 200. Sealing material; 300. Heat-resistant plastic sealed can; 310. Sealed can top cover; 400. Buffer material; 500. Temperature control component; 610. Sensor for electrochemical impedance spectroscopy measurement; 611. First electrode; 612. Second electrode; 613. Wire; 614. High-temperature resistant insulating resin; 620. Corrosion weight loss sample; 630. Sample for characterization of corrosion products; 700. Silicone rubber. DETAILED DESCRIPTION

[0027] In order to facilitate the understanding of the present invention, the present invention will be described more fully below with reference to the relevant drawings. The preferred embodiments of the present invention are given in the drawings. However, the present invention can be implemented in many different forms and is not limited to the embodiments described herein. On the contrary, the purpose of providing these embodiments is to make the understanding of the disclosure of the present invention more thorough and comprehensive.

[0028] It should be noted that when an element is referred to as being "fixed to" another element, it may be directly on the other element or there may be an intermediate element. When an element is considered to be "connected to" another element, it may be directly connected to the other element or there may be an intermediate element at the same time.

[0029] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art in the technical field of the present invention. The terms used herein in the specification of the present invention are only for the purpose of describing specific embodiments and are not intended to limit the present invention. The term "and / or" used herein includes any and all combinations of one or more related listed items.

[0030] See also Figure 1As shown, this embodiment relates to a device 10 for long-term corrosion test of packaging container materials for geological disposal of high-level radioactive waste. The device 10 for long-term corrosion test of packaging container materials for geological disposal of high-level radioactive waste includes an open container 100, a sealing material 200, a temperature-resistant plastic sealed tank 300, a buffer material 400, a temperature control component 500, a packaging container candidate material test sample, a wire 613 and a silicone rubber 700; wherein: the packaging container candidate material test sample includes a sensor 610 for measuring electrochemical impedance spectroscopy, a corrosion weight loss sample 620, and a sample 630 for characterizing corrosion products. The specific structure is as follows:

[0031] The open container 100 is filled with a sealing material 200, a heat-resistant plastic sealed tank 300 is buried in the sealing material 200, a buffer material 400 is filled in the heat-resistant plastic sealed tank 300, and a sensor 610 for measuring electrochemical impedance spectroscopy, a corrosion weight loss sample 620, and a sample 630 for characterizing corrosion products are buried in the buffer material 400; a wire 613 is passed through the sealed tank top cover 310 of the heat-resistant plastic sealed tank 300, and its lower end is connected to the electrochemical impedance spectroscopy sensor 610. The measuring sensor 610 is connected, and its upper end is led out of the open container 100; the temperature control component 500 is inserted into the sealed tank top cover 310 of the heat-resistant plastic sealed tank 300, and its lower end extends into the buffer material 400, and its upper end is led out of the open container 100; the sealed tank top cover 310 and the heat-resistant plastic sealed tank 300 are sealed by silicone rubber 700, and the wire 613, the temperature control component 500 and the sealed tank top cover 310 are sealed by silicone rubber 700.

[0032] The packaging container candidate material test sample and the temperature control component 500 have no direct contact with each other and are buried in the buffer material 400 and sealed together in the temperature-resistant plastic sealed can 300 .

[0033] The sealed heat-resistant plastic can 300 is placed in the open container 100 and is submerged with the sealing material 200 to isolate the test unit from the infiltration of ambient air.

[0034] See also Figure 2 As shown, the electrochemical impedance spectroscopy sensor 610 is composed of a first electrode 611 and a second electrode 612 of the same material; the first electrode 611 and the second electrode 612 each have more than three comb teeth so that the first electrode 611 and the second electrode 612 are interlaced with each other in a comb shape, and there is a gap between adjacent comb teeth, and the gap is not greater than 0.3mm. The test surface area of ​​the first electrode 611 and the second electrode 612 is 1cm 2 .

[0035] See also Figure 2As shown, the first electrode 611 and the second electrode 612 are fixed between and on the outside by filling a high temperature resistant insulating resin 614, the upper end surface of the sensor 610 for electrochemical impedance spectroscopy measurement is a test surface, the upper surfaces of the first electrode 611 and the second electrode 612 are exposed and flush with the test surface, and a probe copper wire 613 is led out from the non-exposed side of the first electrode 611 and the second electrode 612 respectively, and is led out through a reserved notch on the sealing tank top cover 310 of the heat-resistant plastic sealing tank 300, for electrochemical impedance spectroscopy data collection; after the copper wire 613 is led out, the remaining gap of the reserved notch is sealed with silicone rubber 700.

[0036] See also Figure 1 As shown, the temperature control component 500 is located in the buffer material 400, and is led out through a reserved notch on the sealing tank top cover 310 of the heat-resistant plastic sealing tank 300, and is connected to a power source; after the temperature control component 500 is led out, the remaining gap is sealed with silicone rubber 700.

[0037] See also Figure 1 As shown, after the heat-resistant plastic sealed can 300 is sealed, the silicone rubber 700 is used to seal the sealing circumference of the heat-resistant plastic sealed can 300 and the sealed can top cover 310 .

[0038] See also Figure 1 As shown, the buffer material 400 is bentonite, which should have a certain compaction degree of 1.2 to 1.85 g / cm according to the test parameter requirements. 3 , and contains a certain proportion of groundwater.

[0039] See also Figure 1 As shown, the number of the corrosion weight loss samples 620 set in parallel is not less than 3, which are used to measure the corrosion rate of the candidate materials for packaging containers, and the sample size is not less than 20mm×10mm×3mm; the number of the corrosion product characterization samples 630 is not less than 3, which are used to characterize the corrosion morphology, corrosion product composition and corrosion type of the candidate materials for packaging containers, and the sample size is not less than 10mm×10mm×2mm.

[0040] See also Figure 1 As shown, the sealing material 200 is glycerin or liquid paraffin, which has good fluidity, is difficult to volatilize, has a flash point of not less than 130° C., and does not react with the silicone rubber 700 and the temperature-resistant plastic sealing can 300 .

[0041] See also Figure 1-2 As shown, in this embodiment, the device for long-term corrosion test of high-level radioactive waste geological disposal packaging container materials, when used for long-term corrosion test research of high-level radioactive waste geological disposal packaging container materials, involves a long-term corrosion test method for high-level radioactive waste geological disposal packaging container materials, including the following steps:

[0042] (1) Prepare 400 ml of bentonite as a buffer material, and mechanically mix groundwater and 400 ml of bentonite as a buffer material according to test requirements for later use, wherein the weight of groundwater accounts for no more than 70%; at the same time, prepare an open container 100 and a sealing material 200 ml of glycerin or liquid paraffin;

[0043] (2) using a wire cutting device to precisely process the metal sheet of the candidate material of the packaging container into a first electrode 611 and a second electrode 612 of a sensor 610 for electrochemical impedance spectroscopy measurement, a corrosion weight loss sample 620, and a sample 630 for corrosion product characterization according to the designed size;

[0044] (3) Manufacturing a sensor 610 for measuring electrochemical impedance spectroscopy. A probe copper wire 613 is welded to the non-exposed sides of the first electrode 611 and the second electrode 612 respectively, and the first electrode 611 and the second electrode 612 are interlaced with each other in a comb shape, with gaps between adjacent comb teeth and fixed in a mold, and then a high-temperature resistant insulating resin 614 is filled between the first electrode 611 and the second electrode 612 and on the outside, and then placed in an oven for constant temperature curing and then fixed; the test surface of the prepared sensor 610 for measuring electrochemical impedance spectroscopy is mechanically water-grinded to 2000# silicon carbide sandpaper, blown dry with cold air, and dried in a dryer for 24 hours before use;

[0045] (4) The corrosion weight loss sample 620 was mechanically water-grinded to 2000# silicon carbide sandpaper, dried with cold air, degreased with anhydrous ethanol, and placed in a desiccator for 24 hours. The length, width, and thickness of each sample were then recorded with a vernier caliper, and the surface area S of each sample was calculated, and the initial mass W0 of each sample was recorded;

[0046] (5) The corrosion product characterization sample 630 was mechanically water-grinded to 2000# silicon carbide sandpaper, dried with cold air, degreased with anhydrous ethanol, and placed in a desiccator for 24 hours for use;

[0047] (6) Place the sensor 610 for electrochemical impedance spectroscopy measurement, the corrosion weight loss sample 620, and the corrosion product characterization sample 630 into the heat-resistant plastic sealed can 300, then fill it with the prepared buffer material 400 bentonite, insert the temperature control component 500, and perform a certain degree of compaction according to the test requirements, so that the bentonite fills the entire heat-resistant plastic sealed can 300, and then cover the sealed can top cover 310; seal the remaining gap of the sealed can top cover 310 with silicone rubber 700, and also seal the sealing ring of the heat-resistant plastic sealed can 300 and the sealed can top cover 310 with silicone rubber 700;

[0048] (7) Place the sealed heat-resistant plastic sealed can 300 into the open container 100, and fill it with the sealing material 200 so that the liquid level of the sealing material 200 is at least 15 mm higher than the top of the heat-resistant plastic sealed can 300;

[0049] (8) The electrochemical impedance spectroscopy measurement sensor 610 is connected to the electrochemical workstation via a wire 613, and the temperature control component 500 is connected to a power supply. When the temperature control component 500 indicates that the temperature of the buffer material 400 reaches the test set value, the evolution of the electrochemical impedance spectrum of the electrochemical impedance spectroscopy measurement sensor 610 over time is regularly measured and recorded;

[0050] (9) After the test is completed, the corrosion weight loss sample 620 is taken out, and the mass of each parallel sample is weighed after removing the corrosion products, recorded as W1, and its corrosion rate V is calculated according to the corrosion weight loss ΔW, density ρ, corrosion time T and surface area S of the sample; the corrosion product characterization sample 630 is taken out, and after drying in an oxygen-free environment, the corrosion product morphology, corrosion morphology, corrosion product composition and corrosion type are characterized.

[0051] The results of the embodiments show that the long-term corrosion test method for packaging container materials for geological disposal of high-level radioactive waste can effectively simulate the long-term corrosion behavior of packaging container materials in the environment of geological disposal of high-level radioactive waste; in addition, through the regular measurement of sensors for electrochemical impedance spectroscopy measurement and the characterization of corrosion weight loss samples and corrosion product characterization samples, the corrosion rate, corrosion product morphology, corrosion morphology, corrosion product composition and corrosion type characterization of candidate materials for geological disposal of high-level radioactive waste packaging containers in the environment of geological disposal of high-level radioactive waste can be achieved. It can be seen that the long-term corrosion test method for packaging container materials for geological disposal of high-level radioactive waste of the utility model has the characteristics of multi-function, strong operability, good sealing, strong stability and real-time measurement.

[0052] The technical features of the above-mentioned embodiments can be combined arbitrarily. To make the description concise, not all possible combinations of the technical features in the above-mentioned embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.

[0053] The above-mentioned embodiment only expresses one implementation mode of the utility model, and its description is relatively specific and detailed, but it cannot be understood as limiting the scope of the utility model. It should be pointed out that for ordinary technicians in this field, several modifications and improvements can be made without departing from the concept of the utility model. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the utility model belong to the protection scope of the utility model. Therefore, the protection scope of the utility model shall be based on the attached claims.

Claims

1. A device for long-term corrosion testing of packaging container materials for geological disposal of high-level radioactive waste, characterized in that: It includes open containers, sealing materials, temperature-resistant plastic sealed cans, buffer materials, temperature control components, test samples of candidate packaging container materials, wires and silicone rubber. The test samples of candidate packaging container materials include sensors for electrochemical impedance spectroscopy measurement, corrosion weight loss samples, and samples for corrosion product characterization. The specific structure is as follows: The open container is filled with sealing material, in which a heat-resistant plastic sealed tank is buried, in which a buffer material is filled, in which a sensor for electrochemical impedance spectroscopy measurement, a corrosion weight loss sample, and a sample for corrosion product characterization are buried; a wire is passed through the sealed tank top cover of the heat-resistant plastic sealed tank, the lower end of which is connected to the sensor for electrochemical impedance spectroscopy measurement, and the upper end of which is led out of the open container; a temperature control component is inserted into the sealed tank top cover of the heat-resistant plastic sealed tank, the lower end of which extends into the buffer material, and the upper end of which is led out of the open container; the sealed tank top cover and the heat-resistant plastic sealed tank are sealed by silicone rubber, and the wire, the temperature control component and the sealed tank top cover are sealed by silicone rubber.

2. The device for long-term corrosion test of packaging container materials for geological disposal of high-level radioactive waste according to claim 1 is characterized in that: The test sample of the candidate material for the packaging container has no direct contact with the temperature control component and is buried in the buffer material and sealed together in a temperature-resistant plastic sealed can; the sealed temperature-resistant plastic sealed can is placed in an open container and the temperature-resistant plastic sealed can is submerged with sealing material.

3. The device for long-term corrosion test of packaging container materials for geological disposal of high-level radioactive waste according to claim 1 is characterized in that: The sensor for electrochemical impedance spectroscopy measurement consists of a first electrode and a second electrode of the same material. The first electrode and the second electrode each have three or more comb teeth, so that the first electrode and the second electrode are interlaced with each other in a comb shape. There is a gap between adjacent comb teeth, and the gap is no more than 0.3mm. The test surface area of ​​the first electrode and the second electrode is 1cm 2 .

4. The device for long-term corrosion test of packaging container materials for geological disposal of high-level radioactive waste according to claim 3 is characterized in that: The first electrode and the second electrode are fixed between and on the outside by filling with high-temperature resistant insulating resin. The upper end surface of the sensor for measuring electrochemical impedance spectroscopy is a test surface. The upper surfaces of the first electrode and the second electrode are exposed and flush with the test surface. A wire is led out from the non-exposed side of the first electrode and the second electrode respectively, and then led out through a reserved notch on the top cover of the sealing tank of the heat-resistant plastic sealing tank for electrochemical impedance spectroscopy data collection. The remaining gap in the reserved notch after the wire is led out is sealed with silicone rubber.

5. The device for long-term corrosion test of packaging container materials for geological disposal of high-level radioactive waste according to claim 1 is characterized in that: The temperature control component is located in the buffer material and is led out through a reserved notch on the top cover of the sealing tank of the temperature-resistant plastic sealing tank and connected to a power source. After the temperature control component is led out, the remaining gap is sealed with silicone rubber.

6. The device for long-term corrosion test of packaging container materials for geological disposal of high-level radioactive waste according to claim 1 is characterized in that: After the heat-resistant plastic sealed can is sealed, silicone rubber is used to seal the sealing circumference of the heat-resistant plastic sealed can and the top cover of the sealed can.

7. The device for long-term corrosion test of packaging container materials for geological disposal of high-level radioactive waste according to claim 1 is characterized in that: The number of parallel samples for corrosion weight loss samples shall be no less than 3, and the sample size shall be no less than 20mm×10mm×3mm; the number of samples for corrosion product characterization shall be no less than 3, and the sample size shall be no less than 10mm×10mm×2mm.

8. The device for long-term corrosion test of packaging container materials for geological disposal of high-level radioactive waste according to claim 1 is characterized in that: The sealing material is glycerin or liquid paraffin, and the buffer material is bentonite.

Citation Information

Cited By

  • Rapid evaluation method for material corrosion rate and influence factors in high-level radioactive waste geological disposal environment

    CN120294089A