Asphalt road pavement with photo-thermal reaction coating

By spraying silicon acrylic emulsion on asphalt roads with light reflective layer and layered structure design, the problem of oil leakage at high temperatures is solved, the integrity and deformation resistance of the road surface are improved, ruts and cracks are reduced, and ruts and cracks are extended. The road life is reduced and maintenance costs are reduced.

CN222065061UActive Publication Date: 2024-11-26ZHEJIANG UNIV OF TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420467223.8
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-12
Publication Date
2024-11-26
Estimated Expiration
2034-03-12

AI Technical Summary

Technical Problem

Traditional asphalt roads are prone to oil production under high temperature conditions, resulting in ruts and road cracks have not been effectively solved, and their thermal stability is serious.

Method used

The asphalt road pavement design adopts photothermal reaction coating, including soil base, base layer, asphalt surface layer and paving layer arranged in sequence from bottom to top, and the outer surface of the paving layer is sprayed with silicon acrylic emulsion as the base material. , and improve the integrity and deformation resistance of the pavement through the design of layered structures and adhesive layers, and use diagonal joints and flat joint structures to strengthen the pavement stability.

Benefits of technology

Effectively reduces the surface temperature of the road surface, reduces the occurrence of ruts and cracks, improves the integrity, deformation and fatigue resistance of the road surface, extends the service life of asphalt roads, reduces maintenance costs, and ensures driving safety and comfort. .

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222065061U_ABST
    Figure CN222065061U_ABST
Patent Text Reader

Abstract

The utility model discloses an asphalt road pavement with a photo-thermal reaction coating, and belongs to the technical field of asphalt roads. The pavement structure comprises a soil base, a base layer, an asphalt surface layer and a pavement layer which are sequentially arranged from bottom to top, wherein the asphalt surface layer comprises a lower surface layer, a middle surface layer and an upper surface layer; the paving layer is an asphalt layer, and the outer surface of the paving layer is sprayed with a light-coated reflecting layer which takes silicone acrylic emulsion as a base material; and a cushion layer playing a transition role is arranged between the base layer and the roadbed. According to the utility model, the light reflecting layer is sprayed on the pavement layer, so that the absorption of the pavement on the heat of irradiation light is reduced, the temperature of the surface of the road is reduced, the rutting phenomenon of the pavement due to high-temperature oil outlet is reduced, and the occurrence of swelling and cracking of the pavement is reduced; the surface layer is divided into the multi-layer structure with the wear resistance sequentially improved from bottom to top, and the bonding layers are arranged between the layers, so that an integral surface layer structure is formed on the basis of facilitating laying, the integrity of the pavement structure is improved, and the deformation resistance and the fatigue resistance of the whole pavement are improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model belongs to the technical field of asphalt pavement, and in particular relates to an asphalt road pavement with a photothermal reaction coating. Background Art

[0002] In recent years, the social economy has developed rapidly, and the urban transportation network has become increasingly mature, but the occurrence of road diseases has not decreased. Analysis of the causes of road diseases shows that high temperature leads to rutting and cracking of the road surface, which are factors of road damage. The source of these problems is mainly related to the excessively high road surface temperature. Studies have found that high temperature does make asphalt pavement prone to oil. Therefore, finding a suitable method to solve such problems and improve the construction of asphalt pavement is now a top priority.

[0003] The pavement layer of traditional asphalt roads will not be further processed after paving is completed. Therefore, the problem of high-temperature rutting on asphalt pavements has not been fundamentally solved, and the thermal stability of asphalt pavements is still serious. Utility Model Content

[0004] In view of the above-mentioned problems existing in the prior art, the purpose of the utility model is to provide an asphalt road pavement with a photothermal reaction coating, which can reduce the temperature of the road surface, reduce the occurrence of rutting and cracking, and improve the integrity, deformation resistance and fatigue resistance of the road surface.

[0005] The utility model provides the following technical solutions: an asphalt road pavement with a photothermal reaction coating, comprising a soil base, a base layer, an asphalt surface layer and a paving layer arranged in sequence from bottom to top, wherein the asphalt surface layer comprises a lower layer, a middle layer and an upper layer with increasing wear resistance; the paving layer is an asphalt layer, and a light-reflecting layer with a silicone-acrylic emulsion as a base material is sprayed on its outer surface; a cushion layer serving as a transition is provided between the base layer and the roadbed.

[0006] Furthermore, an adhesive layer is spread between the lower layer and the middle layer, and between the middle layer and the upper layer.

[0007] Furthermore, the adhesive layer between the lower layer and the middle surface layer is an emulsified asphalt adhesive layer, and the adhesive layer between the middle surface layer and the upper layer is a modified asphalt adhesive layer.

[0008] Furthermore, the aggregates of the lower layer, the middle layer and the upper layer all include coarse aggregate and fine aggregate mixed with the coarse aggregate in a designed proportion, the particle size of the coarse aggregate is 4.75-9.50 mm, and the particle size of the fine aggregate is less than 4.75 mm.

[0009] Furthermore, the base layer is a multi-layer structure.

[0010] Furthermore, the longitudinal joints of the road surface are paved with an oblique joint structure, and the transverse joints are paved with a flat joint structure.

[0011] Furthermore, the joints are connected via force transmission rods.

[0012] By adopting the above technology, compared with the prior art, the beneficial effects of the utility model are as follows:

[0013] 1) In the utility model, by spraying a light-reflecting layer with a silicone-acrylic emulsion as a base material on the pavement layer, the absorption of heat from the irradiated light by the road surface is reduced, the temperature of the road surface is lowered, the problem of rutting caused by high-temperature oil discharge on the road surface is reduced, and the occurrence of bulging and cracking of the road surface is reduced;

[0014] 2) In the utility model, the surface layer is divided into a multi-layer structure with successively improved wear resistance from bottom to top, and an adhesive layer is arranged between the layers to form an integral surface layer structure on the basis of easy paving, thereby improving the integrity of the pavement structure and thus improving the overall deformation resistance and fatigue resistance of the pavement;

[0015] 3) In the present invention, the size of fine aggregate and coarse aggregate in each surface layer is limited, and based on the design of its proportion, the compactness of the surface layer can be improved, and the deformation resistance and fatigue resistance of the surface layer can be further improved;

[0016] 4) In the present invention, the longitudinal joints adopt an oblique joint structure, and the transverse joints adopt a flat joint structure, so as to ensure that the parts between the joints are connected into a whole through the structural form of the joints, thereby improving the stability of the pavement structure. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 It is a cross-sectional schematic diagram of the asphalt road of the utility model;

[0018] Figure 2 The utility model is a schematic diagram of the placement structure of the force transmission rod at the pavement joint. DETAILED DESCRIPTION

[0019] In order to make the purpose, technical solution and advantages of the utility model more clear, the utility model is further described in detail below in conjunction with the accompanying drawings and embodiments of the specification. It should be understood that the specific embodiments described here are only used to explain the utility model and are not used to limit the utility model.

[0020] On the contrary, the present invention covers any substitution, modification, equivalent method and scheme made on the essence and scope of the present invention as defined by the claims. Further, in order to make the public have a better understanding of the present invention, some specific details are described in detail in the following detailed description of the present invention. Those skilled in the art can fully understand the present invention without the description of these details.

[0021] See also Figure 1-2 A photothermal reaction coated asphalt road pavement comprises a soil base 1, a base layer 2, an asphalt surface layer 3 and a paving layer 4 arranged in sequence from bottom to top; a cushion layer is arranged between the base layer 2 and the roadbed, and a light reflecting layer 5 is sprayed on the outer surface of the paving layer 4.

[0022] Specifically, the soil base 1 needs to be repaired and potholes filled before starting to ensure the flatness and firmness of the foundation. During this period, a roller needs to be used to compact the soil base to increase the density of the road surface.

[0023] Specifically, the base layer 2 is a layered structure, and each layer of the base layer needs to be constructed in layers and pressed layer by layer to achieve the specified density to ensure that the base layer construction meets the requirements.

[0024] Specifically, the asphalt surface layer 3 includes a lower layer, a middle layer and an upper layer which are arranged in sequence from bottom to top, and the wear resistance thereof is improved in sequence, so as to ensure the integrity thereof during the surface layer paving construction.

[0025] in:

[0026] The lower layer has 20% aggregate of ordinary asphalt; or 40% aggregate of modified asphalt;

[0027] The middle surface layer has 40% aggregate of ordinary asphalt; or 50% aggregate of modified asphalt;

[0028] The upper layer has 20% aggregate of ordinary asphalt;

[0029] A layer of adhesive layer is spread between each connecting layer, wherein the lower layer and the middle layer are connected with 0.5kg / m2 of emulsified asphalt, and the middle layer and the upper layer are connected with 0.6kg / m2 of modified asphalt adhesive layer.

[0030] Specifically, the light reflective layer 5 has a silicone-acrylic emulsion as a base material with a material ratio of: 38.5% silicone-acrylic emulsion, 9.6% glass beads, 12.5% ​​titanium dioxide, 4.8% dispersant, 3.8% film-forming aid, and 15.4% pure water.

[0031] The construction process of the pavement in this embodiment is as follows:

[0032] An asphalt road pavement with a photothermal reaction coating comprises the following steps:

[0033] S1. Making a light-reflecting coating layer 5 with silicone-acrylic emulsion as the base material:

[0034] S2. Grind the base material particles required for the roadbed surface layer and select the required aggregate type to ensure the quality and safety of the asphalt pavement;

[0035] S3, recycled aggregate and screening particle size, the aggregate ground into powder is screened to separate the powder into coarse aggregate and fine aggregate, and the coarse aggregate with a particle size range of 4.75-9.50 mm and the fine aggregate with a particle size range of less than 4.75 mm are screened out;

[0036] S4. Mixing the asphalt mixture, and mixing the coarse aggregate and fine aggregate in order according to the proportion;

[0037] S5, layered paving. The content of ceramic particles in each surface layer is different, so it needs to be paved in layers, and each layer needs to be compacted separately to ensure the density of the road surface;

[0038] S6. For construction joint treatment, use inclined joints for longitudinal construction and flat joints for transverse joints;

[0039] In this embodiment, the aggregate collection process is as follows:

[0040] The milling method used is a mechanical form. In the process of recycling old materials, milling is a common way to recycle waste. In the recycling step of old materials, milling is carried out at a speed of 20m / min.

[0041] In this embodiment, the asphalt road pavement recycled aggregate and the screening particle size process are as follows:

[0042] After verification by the Marshall test, the particle size range of aggregate particles is determined, and the ground aggregate is screened to separate the powder into coarse and fine aggregates. Aggregates with a particle size range of 4.75-9.50 mm are screened out, of which aggregates smaller than 4.75 mm are considered fine aggregates, and those in the particle size range of 4.75-9.5 mm are considered coarse aggregates. The coarse and fine aggregates are then stored separately so that the ratio of coarse and fine aggregates is appropriate during the grading design process.

[0043] In this embodiment, the asphalt mixture mixing process of the asphalt road pavement is as follows:

[0044] First, ordinary asphalt is mixed and stirred for 5 to 10 seconds, and then 4.75-9.5mm coarse aggregate and fine aggregate are added in sequence according to the proportion, and the stirring time is 10-15 seconds; a more specific form of the step of heating and stirring the mixture is that the mixture is first heated separately at a high position, and the heating temperature is 80-130 degrees Celsius. The temperature used in this article is 115 degrees Celsius. Then, according to the bonding curve of asphalt, the adding temperature of the bonding material particles is determined to be between 190-220 degrees Celsius, and the temperature is determined to be 200 degrees Celsius in the example.

[0045] In the layered paving step of this embodiment, after the mixture is mixed, it is necessary to use a grader to carry out paving operations. The paving operation should be carried out continuously. According to the paving operation volume of the mixture, two unloading vehicles are equipped at the construction site to avoid the phenomenon of untimely supply of the mixture. At the same time, the specific paving area is determined in combination with the paving thickness and the compacted dry density, and the post-unloading distance is controlled. For the graded crushed stone subbase operation, the paving thickness is 18cm each time, and the cross-sectional length should be controlled within 15cm. During the paving process, when encountering larger gravel, it should be cleaned out of the mixture in time. When segregation problems are found in the mixture, manual methods should be adopted in time to deal with it; during the paving process, the initial pressure, repeated pressure, and final pressure must be considered; the flatness of the three compactions, and it should be noted that the roller cannot be parked at will.

[0046] In the construction joint step of the present embodiment, in order to ensure the construction quality of the pavement cushion layer, joint and U-turn processing are required. First, after the rolling operation is completed, the flatness of the cushion layer should be inspected, which can be achieved using a 3m long ruler. If it is found that the cushion layer flatness is not up to standard, the structure here needs to be cleaned up. During the rolling operation, when rolling a new section, the roller should be parked on the compacted section and go deep into the working section for about 15cm before rolling, thereby achieving effective treatment of the transverse construction joint. Secondly, when the cushion layer rolling meets the requirements and then turns around, it is necessary to first cover it with tarpaulin or a relatively thick plastic sheet with a length of about 10m, and then 10cm of soil or sand can be directly spread on the position and then turn around. In the highway pavement structure, the cushion layer is located between the base and the roadbed, and plays a transitional role in the entire pavement structure, which has a greater impact on the road traffic situation. If you want to ensure the safe driving of vehicles and reduce the occurrence of pavement disease problems, you must do a good job in the construction of the pavement cushion layer.

[0047] In this embodiment, the asphalt surface layer aggregate can be divided into an upper layer made of a mixture of granite aggregates; a middle layer and a lower layer made of a mixture of marble aggregates. The granite used as aggregate is relatively hard and not easily weathered for road paving; and a crusher is used for crushing because it can strictly control the particle size of the crushed stone to ensure the quality of the coarse aggregate.

[0048] In this embodiment, the upper layer is made of SBS modified asphalt, and the lower layer is road petroleum asphalt.

[0049] In this embodiment, the materials used in the preparation of the silicone-acrylic emulsion are simple and easy to obtain, and the discarded materials are reused in the preparation of the road surface light and heat reflective coating. Based on the heat-resistant effect of the light and heat reflective coating, the heat-insulating and heat-resistant effect of the road surface is improved. The raw materials used reduce the cost of heat resistance, and due to the reduction of road rutting and cracking, the service life of the asphalt road is extended, labor costs and maintenance costs are saved, and it has high economic benefits. It also solves the problem of unfavorable driving and easy rutting in summer due to high temperatures, reduces the problem of rutting caused by high oil levels on the road surface, and at the same time, the road surface temperature is reduced, making it less likely for the asphalt road to bulge and crack. Reduce the road surface temperature in high temperature seasons to achieve active protection against rutting diseases, thereby ensuring driving safety and improving driving comfort.

[0050] The above are only preferred embodiments of the present invention and are not intended to limit the present invention. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. An asphalt road pavement with a photothermal reaction coating, characterized in that: The invention comprises a soil base (1), a base layer (2), an asphalt surface layer (3) and a paving layer (4) which are arranged in sequence from bottom to top, wherein the asphalt surface layer (3) comprises, from bottom to top, a lower layer, a middle layer and an upper layer whose wear resistance increases in sequence; the paving layer (4) is an asphalt layer, and a light-reflecting coating layer (5) with a silicone-acrylic emulsion as a base material is sprayed on its outer surface; and a cushion layer which plays a transitional role is arranged between the base layer (2) and the roadbed.

2. The asphalt road pavement with a photothermal reaction coating according to claim 1, characterized in that: An adhesive layer is spread between the lower layer and the middle layer, and between the middle layer and the upper layer.

3. The asphalt road pavement with a photothermal reaction coating according to claim 2, characterized in that: The adhesive layer between the lower layer and the middle surface layer is an emulsified asphalt adhesive layer, and the adhesive layer between the middle surface layer and the upper layer is a modified asphalt adhesive layer.

4. The asphalt road pavement with a photothermal reaction coating according to claim 1, characterized in that: The base layer (2) is a multi-layer structure.

5. The asphalt road pavement with a photothermal reaction coating according to claim 1, characterized in that: The longitudinal joints of the road surface are paved with an oblique joint structure, and the transverse joints are paved with a flat joint structure.

6. The asphalt road pavement with a photothermal reaction coating according to claim 5, characterized in that: The joints are connected via force transmission rods (6).