Detection device for detecting damaged position of aluminum plastic package by using copper sulfate

Through the copper sulfate detection device, the performance degradation of lithium-ion battery aluminum-plastic packaging caused by damage during equipment packaging is solved, and the accurate detection of the damaged position of aluminum-plastic shell is achieved, and the packaging quality and battery safety are improved. in various battery types.

CN222070516UActive Publication Date: 2024-11-26TIANJIN JUYUAN NEW ENERGY TECH CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420201719.0
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-01-29
Publication Date
2024-11-26
Estimated Expiration
2034-01-29

AI Technical Summary

Technical Problem

During the equipment packaging process, existing lithium-ion battery aluminum-plastic packaging is prone to damage due to equipment transfer vibration, friction and wear of the seal head, thermal expansion and other factors, resulting in degradation of battery performance, liquid leakage, moisture and air infiltration, poor shell voltage, and aluminum-plastic corrosion. and other issues affect packaging quality and safety.

Method used

A test container containing copper sulfate solution is used to detect the broken position of the aluminum-plastic shell by using copper sulfate detection device, using copper sulfate solution and copper sulfate solution to form a closed circuit, using copper sulfate solution and conduction Body contact is used to check for damage to the PP layer.

Benefits of technology

Accurately determine the damaged position of aluminum-plastics, improve packaging quality and safety of finished batteries, simple structure, standardized operating procedures, low testing costs, fast judgment speed, suitable for consumption, power and energy storage batteries in aluminum-plastic and aluminum shell packaging.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222070516U_ABST
    Figure CN222070516U_ABST
Patent Text Reader

Abstract

The utility model discloses a detection device for detecting a damaged position of an aluminum plastic package by using copper sulfate. The detection device comprises an output power supply, an electric conductor, a shell alligator clip contact terminal and a test container containing a copper sulfate solution, the positive electrode of the output power supply is connected with the electric conductor, the negative electrode of the output power supply is connected with the shell alligator clip contact terminal, the shell alligator clip contact terminal clamps a to-be-tested aluminum plastic shell, the outer side of the shell alligator clip contact terminal is insulated, and a sawtooth part of the shell alligator clip contact terminal is meshed and penetrates through the to-be-tested aluminum plastic shell to be conducted with the to-be-tested aluminum plastic shell; the electric conductor and the to-be-tested aluminum plastic shell are immersed in the copper sulfate solution, the copper sulfate solution is in infiltration contact with the electric conductor, and the output power supply, the electric conductor and the to-be-tested aluminum plastic shell form a closed loop; according to the method, the aluminum plastic damage position in the battery with the abnormal shell voltage can be accurately confirmed, and the battery with the abnormal shell voltage can be accurately judged.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of lithium ion battery aluminum-plastic packaging detection, in particular to a detection device for detecting the damaged position of the aluminum-plastic packaging by using copper sulfate. Background Art

[0002] As an important product, soft-pack polymer lithium-ion batteries are widely used in consumer electronic products such as mobile phones, tablet computers, laptops, wearables, smart homes, etc. due to their high voltage, high energy density, long cycle life, memory-free charging, light weight, and strong plasticity of appearance and size. They are also widely used in electric vehicles, electric bicycles, power tools, as well as medium and large electric equipment such as drones and AGVs. Therefore, the safety requirements for the use of lithium-ion batteries are becoming increasingly higher.

[0003] The terminal products in the current market have put forward new requirements for service life, high-rate fast charging, and use in different geographical environments. As a result, the size, weight, and materials of lithium-ion batteries are constantly changing, and higher requirements are placed on the reliability of the battery's external shell.

[0004] Existing soft-pack polymer lithium-ion batteries are packaged with aluminum-plastic materials. Through the effective packaging of aluminum-plastic, a sealed space mainly composed of the top seal of the pole ear, the side seal, and the air bag seal is formed. The main function of battery packaging is to isolate external foreign matter, dust, moisture, etc., and to carry the gas generated by the formation process. The use of aluminum-plastic materials for packaging is to use the inner layer of PP glue of the three-layer aluminum-plastic packaging film under the action of the metal head, and use the packaging machine to perform composite packaging on the gas chamber side through time, pressure, and temperature parameters. This packaging method must ensure the sealing of the packaging on the one hand, and on the other hand, it must consider the hidden dangers of the internal reaction of the battery to the aluminum-plastic shell. During the equipment packaging process, due to the influence of factors such as equipment transfer vibration, head friction and wear, thermal expansion, operating parameters, and environment, the battery aluminum-plastic seal is often damaged and fails. It has a serious impact on the subsequent performance of the battery. Utility Model Content

[0005] The utility model aims to provide a detection device for detecting the damaged position of aluminum-plastic package by using copper sulfate, so as to detect the effectiveness of aluminum-plastic package and package damage, and to make targeted improvements to prevent backward leakage, water and air infiltration and bulging, poor shell voltage, aluminum-plastic corrosion, etc., so as to improve the final packaging quality and the safety of finished battery.

[0006] In order to achieve the purpose of the utility model, the technical solution provided by the utility model is as follows:

[0007] The utility model provides a detection device for detecting the damaged position of aluminum-plastic package by using copper sulfate, comprising an output power supply, a conductor, a shell alligator clip contact terminal, and a test container containing copper sulfate solution;

[0008] The positive electrode of the output power supply is connected to the conductor, and the negative electrode is connected to the alligator clip contact terminal of the shell. The alligator clip contact terminal of the shell clamps the aluminum-plastic shell to be tested. The outer side of the alligator clip contact terminal of the shell is insulated, and the sawtooth part bites through the aluminum-plastic shell to be tested and conducts with it.

[0009] The conductor and the aluminum-plastic housing to be tested are immersed in a copper sulfate solution, the copper sulfate solution is in contact with the conductor, and the output power supply, the conductor and the aluminum-plastic housing to be tested form a closed loop;

[0010] The output voltage of the output power supply satisfies or is greater than or equal to 3.7V.

[0011] Compared with the prior art, the beneficial effects of the utility model are as follows:

[0012] The present application can accurately confirm the location of aluminum-plastic damage in batteries with abnormal shell voltage, and make accurate judgments on batteries with abnormal shell voltage. The device provided by the present application has a simple structure, simple overall operation, and a standardized process. The power supply does not need to be adjusted, and the voltage is small and there is no safety risk in use. The power supply uses the original battery to restore the voltage environment placement and use status. The device is reusable, has low testing costs, fast judgment speed, and reduces the time cost caused by multiple judgments. For the shell voltage test judgment of 0.1~3.0V, it can effectively correspond to the location of the aluminum-plastic damage area, the copper plating area and the cumulative amount. After testing, the judgment correspondence rate is above 90%.

[0013] In addition, the conclusions obtained through the above methods and devices provide an accurate position for subsequent improvements in packaging, which can improve related processes in a targeted manner, making the improvements more accurate and saving the cost of trial and error and judgment.

[0014] In addition, the device is applicable to consumer, power, and energy storage batteries encapsulated in aluminum-plastic and aluminum shells, and can produce the same effect in related tests. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] Figure 1 A schematic diagram of the structure of a detection device for detecting the damaged position of an aluminum-plastic package using copper sulfate provided in an embodiment of the present application;

[0016] Figure 2 This is a schematic diagram of the connection structure of the detection circuit components using a voltmeter;

[0017] Figure 3 This is a schematic diagram of the connection structure of the output battery using a voltmeter to test;

[0018] Figure 4 This is a schematic diagram of the shear position of the aluminum-plastic shell;

[0019] Figure 5 This is a schematic diagram of the structure of the cutting part of the aluminum-plastic shell top seal;

[0020] Figure 6 This is a schematic diagram of the structure of the cutting part of the aluminum-plastic shell side seal;

[0021] Figure 7 This is a schematic diagram of the connection between the alligator clip contact terminal of the housing and the aluminum-plastic housing to be tested in the embodiment of the present application;

[0022] In the figure: 1. Output power supply, 1-1. Output battery, 1-2. Positive ear alligator clip contact terminal, 1-3. Negative ear alligator clip contact terminal, 1-4. Power connection wire, 2. Aluminum-plastic shell to be tested, 2-1. Aluminum-plastic shell top seal cutout part, 2-2. Aluminum-plastic shell side seal cutout part, 3. Conductor, 4. Shell alligator clip contact terminal, 5. Copper sulfate solution, 6. Test container, 6-1. Test tool V-shaped load-bearing bracket, 7. Voltmeter. DETAILED DESCRIPTION

[0023] The following is a clear and complete description of the technical solutions in the embodiments of the present invention in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0024] It should be noted that the basic concept of the present invention is to design a set of devices that can be repeatedly verified based on the basic principle of copper electroplating. Figure 4-6 As shown, after the aluminum-plastic shell of the outer layer of the battery is packaged, the aluminum-plastic shell is cut into the required size after the standardized battery disassembly, and the packaged shell of the aluminum-plastic shell top seal cut part and the aluminum-plastic shell side seal cut part is retained for testing. The aluminum-plastic shell is connected to the power supply body, and the test position and the conductor are immersed in the copper sulfate solution, and the power supply is connected for testing. If the PP layer is damaged, the copper sulfate solution will directly contact the aluminum layer of the aluminum-plastic shell and reduce to metallic copper on the surface of the aluminum layer, so as to detect the damaged position of the PP layer.

[0025] like Figure 1 and Figure 7 As shown, the detection device for detecting the damaged position of aluminum-plastic package using copper sulfate provided in this embodiment includes an output power supply 1, a conductor 3, a shell alligator clip contact terminal 4, and a test container 6 containing a copper sulfate solution 5;

[0026] The positive electrode of the output power supply 1 is connected to the conductor 3, and the negative electrode is connected to the shell alligator clip contact terminal 4. The shell alligator clip contact terminal 4 clamps the aluminum-plastic shell 2 to be tested. The outer side of the shell alligator clip contact terminal 4 is insulated, and the sawtooth part bites through the aluminum-plastic shell 2 to be tested and conducts with it.

[0027] During the detection, the conductor 3 and the aluminum-plastic housing 2 to be tested need to be immersed in the copper sulfate solution 5, the copper sulfate solution 5 is in contact with the conductor 3, and the output power supply 1, the conductor 3 and the aluminum-plastic housing to be tested form a closed loop;

[0028] The output voltage of the output power supply 1 satisfies or exceeds 3.7V.

[0029] Preferably, the output power supply 1 includes an output battery 1-1, a positive ear crocodile clip contact terminal 1-2, a negative ear crocodile clip contact terminal 1-3 and a power connection wire 1-4. The positive and negative ears of the output battery 1-1 are respectively clamped and contacted with the positive ear crocodile clip contact terminal 1-2 and the negative ear crocodile clip contact terminal 1-3. The positive ear crocodile clip contact terminal 1-2 is connected to the conductor 3 through the power connection wire 1-4, and the negative ear crocodile clip contact terminal 1-3 is connected to the shell crocodile clip contact terminal 4 through the power connection wire 1-4.

[0030] Preferably, the aluminum-plastic shell 2 to be tested comprises an aluminum-plastic shell top seal cutting portion 2-1 and an aluminum-plastic shell side seal cutting portion 2-2.

[0031] Preferably, it also includes a voltmeter 7 for testing the output battery voltage and testing whether the output power supply 1, the conductor 3, and the aluminum-plastic housing 2 to be tested form a circuit.

[0032] Preferably, the concentration of copper sulfate in the copper sulfate solution is greater than or equal to 10%.

[0033] Preferably, a test tool V-shaped load-bearing bracket 6-1 is placed in the copper sulfate solution. The test tool V-shaped load-bearing bracket 6-1 is composed of multiple V-shaped structures connected in sequence. The aluminum-plastic shell 2 to be tested is placed in the V-shaped structure, which is convenient for the upright test of the aluminum-plastic shell to be tested, and multiple samples can be tested at the same time.

[0034] Preferably, there are multiple alligator clip contact terminals 4, each of which clamps an aluminum-plastic housing 2 to be tested, and multiple aluminum-plastic housings 2 to be tested are tested simultaneously. The surface of the alligator clip contact terminal 4 is wrapped with insulating rubber to avoid short circuit. The material is generally pure copper, nickel-plated iron, zinc-plated iron, copper-plated iron or stainless steel, which is conducive to electrical conduction.

[0035] Preferably, the conductor 3 is made of copper material to facilitate current conduction and electroplating reaction.

[0036] Preferably, the output battery 1-1 can be made of soft-pack, cylindrical, or power batteries.

[0037] Preferably, the test container 6 is made of insulating and corrosion-resistant plastic material and can be integrally die-cast.

[0038] It should be noted that the output battery 1-1 can use soft-pack batteries or cylindrical batteries as output, and the voltage must be above 3.7 V. In addition, the output battery 1-1 can be replaced and the actual voltage can be measured.

[0039] It should be noted that during the test, the conductive conductor and the aluminum-plastic housing to be tested are placed in a test container, and a copper sulfate solution is poured into the test container to immerse the aluminum-plastic housing to be tested, and the copper sulfate solution is infiltrated and contacted with the conductor.

[0040] Preferably, the conductor 3 and the aluminum-plastic housing 2 to be tested are immersed in the copper sulfate solution at the same time and immersed for more than 20 minutes.

[0041] It should be noted that if Figure 2-3 As shown, the method provided in this embodiment also includes the step of using a voltmeter to test whether the circuit component is a loop before the detection, and the step of using a voltmeter to test whether the output voltage of the output battery satisfies or is greater than or equal to 3.7V.

[0042] It should be noted that the copper sulfate solution used needs to be prepared in advance, and the copper sulfate content of the reference sample volume and data preparation solution is higher than 10%.

[0043] Finally, it should be noted that the above embodiments are only used to illustrate and explain the present invention, and are not intended to limit the present invention to the scope of the described embodiments. In addition, those skilled in the art can understand that the present invention is not limited to the above embodiments, and more variations and modifications can be made according to the teachings of the present invention, and these variations and modifications all fall within the scope of protection claimed by the present invention.

Claims

1. A detection device for detecting the damaged position of aluminum-plastic packaging using copper sulfate, characterized in that: It comprises an output power supply (1), a conductor (3), a housing alligator clip contact terminal (4), and a test container (6) containing a copper sulfate solution (5); The positive electrode of the output power supply (1) is connected to the conductor (3), and the negative electrode is connected to the shell alligator clip contact terminal (4); the shell alligator clip contact terminal (4) clamps the aluminum-plastic shell (2) to be tested; the outer side of the shell alligator clip contact terminal (4) is insulated, and the sawtooth portion bites through the aluminum-plastic shell (2) to be tested and conducts with it; The conductor (3) and the aluminum-plastic housing to be tested (2) are immersed in a copper sulfate solution (5), the copper sulfate solution (5) is in contact with the conductor (3), and the output power supply (1), the conductor (3) and the aluminum-plastic housing to be tested form a closed loop; The output voltage of the output power supply (1) satisfies the requirement of being greater than or equal to 3.7V.

2. The detection device for detecting the damaged position of aluminum-plastic package by using copper sulfate according to claim 1, characterized in that: The output power supply (1) comprises an output battery (1-1), a positive ear alligator clip contact terminal (1-2), a negative ear alligator clip contact terminal (1-3) and a power connection wire (1-4); the positive and negative ears of the output battery (1-1) are respectively clamped and contacted with the positive ear alligator clip contact terminal (1-2) and the negative ear alligator clip contact terminal (1-3); the positive ear alligator clip contact terminal (1-2) is connected to the conductor (3) via the power connection wire (1-4); and the negative ear alligator clip contact terminal (1-3) is connected to the shell alligator clip contact terminal (4) via the power connection wire (1-4).

3. The detection device for detecting the damaged position of aluminum-plastic package by using copper sulfate according to claim 2, characterized in that: The output battery (1-1) is a soft-pack battery, a cylindrical battery or a power battery.

4. The detection device for detecting the damaged position of aluminum-plastic package by using copper sulfate according to claim 1, characterized in that: The aluminum-plastic shell (2) to be tested comprises an aluminum-plastic shell top seal cutting portion (2-1) and an aluminum-plastic shell side seal cutting portion (2-2).

5. The detection device for detecting the damaged position of aluminum-plastic package by using copper sulfate according to claim 1, characterized in that: It also includes a voltmeter (7) for testing the output battery voltage and testing whether the output power supply (1), the conductor (3) and the aluminum-plastic housing (2) to be tested form a circuit.

6. The detection device for detecting the damaged position of aluminum-plastic package by using copper sulfate according to claim 1, characterized in that: The copper sulfate concentration in the copper sulfate solution is greater than or equal to 10%.

7. The detection device for detecting the damaged position of aluminum-plastic package by using copper sulfate according to claim 1, characterized in that: A test fixture V-shaped load-bearing bracket (6-1) is placed in the copper sulfate solution. The test fixture V-shaped load-bearing bracket (6-1) is composed of a plurality of V-shaped structures connected in sequence. The aluminum-plastic housing (2) to be tested is placed in the V-shaped structure.

8. The detection device for detecting the damaged position of aluminum-plastic package using copper sulfate according to claim 1, characterized in that: There are a plurality of alligator clip contact terminals for the housing, each of which clamps an aluminum-plastic housing (2) to be tested, and a plurality of aluminum-plastic housings (2) to be tested are tested simultaneously.

9. The detection device for detecting the damaged position of aluminum-plastic package using copper sulfate according to claim 1, characterized in that: The conductor (3) is made of copper.