Optical fiber coating mold, optical fiber coating platform and high-temperature-resistant optical fiber

The optical fiber coating mold with adjustable alignment and a tapered receiving cavity addresses the issues of low roundness and concentricity, improving tensile strength and production efficiency through a two-step polyimide coating process.

CN222093872UActive Publication Date: 2024-12-03YANGTZE OPTICAL FIBRE & CABLE CO LTD
View PDF 0 Cites 2 Cited by

Patent Information

Application Number
CN202323651932.6
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-30
Publication Date
2024-12-03
Estimated Expiration
2033-12-30

AI Technical Summary

Technical Problem

Existing polyimide optical fiber production methods result in low roundness and poor concentricity of the coated optical fiber due to inaccurate cutting and alignment issues during the coating process, leading to low tensile strength and complex multi-coating procedures.

Method used

An optical fiber coating mold with adjustable alignment and a tapered receiving cavity, integrated with fixing mechanisms, ensures precise alignment and concentricity, allowing for a two-step coating process with polyimide materials, and a curing oven system to achieve high-temperature resistance.

Benefits of technology

The solution improves the concentricity and tensile strength of the optical fiber, reduces the number of coating steps, and enhances production efficiency while maintaining high-temperature resistance and mechanical properties.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222093872U_ABST
    Figure CN222093872U_ABST
Patent Text Reader

Abstract

The utility model discloses an optical fiber coating mold, an optical fiber coating platform and a high-temperature-resistant optical fiber. The optical fiber coating mold comprises a first fixing mechanism, a second fixing mechanism and a conical containing cavity, the first fixing mechanism, the second fixing mechanism and the conical containing cavity are integrally formed and form through grooves communicated with one another, and the second fixing mechanism is located between the first fixing mechanism and the conical containing cavity; the area of the first fixing mechanism is larger than that of the second fixing mechanism, a base of the wire drawing tower is clamped at the joint of the first fixing mechanism and the second fixing mechanism, and the base is of a hollow annular structure; the first fixing mechanism is fixed on a base of the wire drawing tower through a screw, and the depth of the screw embedded into the base is positively correlated with the collimation degree of the accommodating cavity relative to the base; a through hole is formed in the tip end of the conical containing cavity and serves as an outlet of the coated optical fiber. By adopting the optical fiber coating mold, the concentricity of the optical fiber coating and the tensile strength of the coated optical fiber can be improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of optical fiber preparation, and more specifically, to an optical fiber coating mold, an optical fiber coating platform and a high-temperature resistant optical fiber. Background Art

[0002] Polyimide optical fiber is designed to improve the heat resistance of optical fiber and is mainly used in high temperature environments such as optical fiber sensing. Polyimide is a polymer material with good high and low temperature resistance, good mechanical strength, and excellent comprehensive performance. It can improve the heat resistance of the optical fiber coating and extend the service life of the optical fiber in high temperature environments. At the same time, it can still maintain good mechanical properties in low temperature environments without brittle cracking.

[0003] However, the existing polyimide optical fiber needs to be coated and cured multiple times during the production process, and the outlet of the coated optical fiber is formed by cutting with a knife at the tip of the rubber nozzle. Since it is formed by cutting with a knife, the roundness of the outlet is difficult to control accurately, which will result in a low roundness of the coated optical fiber passing through the outlet of the rubber nozzle. In addition, since the processing accuracy of the Teflon coating cup is not high, the rubber nozzle can only be randomly inserted into the outlet hole of the Teflon coating cup, so it is impossible to ensure the alignment of the Teflon coating cup relative to the base of the drawing tower, and it is even more impossible to ensure the alignment of the rubber nozzle, which leads to poor concentricity of the coated optical fiber coating and low tensile strength. Utility Model Content

[0004] In response to at least one defect or improvement need in the prior art, the utility model provides an optical fiber coating mold, an optical fiber coating platform and a high-temperature resistant optical fiber. The degree of alignment of the accommodating cavity can be adjusted by adjusting the distance of the screws, thereby improving the concentricity of the optical fiber coating and the tensile strength of the coated optical fiber.

[0005] To achieve the above-mentioned purpose, according to the first aspect of the utility model, there is provided an optical fiber coating mold, which includes a first fixing mechanism, a second fixing mechanism and a tapered receiving cavity, wherein the first fixing mechanism, the second fixing mechanism and the tapered receiving cavity are integrally formed and the three form mutually connected through grooves, the second fixing mechanism is located between the first fixing mechanism and the tapered receiving cavity, and the first fixing mechanism is connected to the coating cup through the through groove; the area of ​​the first fixing mechanism is larger than that of the second fixing mechanism, the base of the drawing tower is engaged at the junction of the first fixing mechanism and the second fixing mechanism, and the base is a hollow annular structure; the first fixing mechanism is fixed to the base of the drawing tower by screws, and the depth of the screws embedded in the base is positively correlated with the degree of alignment of the tapered receiving cavity relative to the base; a through hole is provided at the tip of the tapered receiving cavity, and the through hole serves as an outlet for the coated optical fiber; the large-diameter end of the tapered receiving cavity is connected to the second fixing mechanism; the tapered receiving cavity is used to accommodate coating materials and bare optical fiber / single-layer coated optical fiber.

[0006] Furthermore, the through hole at the tip of the tapered cavity is a circular through hole, and the non-circularity of the through hole at the tip of the tapered cavity is not greater than 0.3%.

[0007] Furthermore, the inner diameter of the through hole at the tip of the conical cavity is 210um~290um.

[0008] Furthermore, the height of the conical receiving cavity is 20 mm to 30 mm.

[0009] Furthermore, the first fixing mechanism is a flat hollow cylinder, and a first through groove is provided in the axial direction of the cylinder; the first fixing mechanism is coaxial with the second fixing mechanism; the second fixing mechanism is a flat hollow cylinder, and a second through groove is provided in the axial direction of the cylinder; the first through groove, the second through groove and the inner cavity of the conical receiving cavity are connected to each other.

[0010] According to a second aspect of the utility model, there is also provided an optical fiber coating platform, comprising a first coating mold, a first curing oven, a second coating mold, a second curing oven and a third curing oven arranged in sequence;

[0011] The first coating die and the second coating die both use the above-mentioned optical fiber coating die, and the inner diameter of the through hole of the tapered receiving cavity of the first coating die is smaller than the inner diameter of the through hole of the tapered receiving cavity of the second coating die;

[0012] The conical receiving cavity of the first coating mold is used to accommodate the bare optical fiber and the coating material, and the conical receiving cavity of the second coating mold is used to accommodate the optical fiber and the coating material after the first layer of coating.

[0013] Furthermore, the non-roundness of the through hole at the tip of the conical cavity of the first coating mold is no more than 0.3%, and the inner diameter is 210um~240um; and / or, the non-roundness of the through hole at the tip of the conical cavity of the second coating mold is no more than 0.3%, and the inner diameter is 270um~290um.

[0014] Furthermore, the coating materials in the first coating mold and the second coating mold are both polyimide.

[0015] Furthermore, the curing temperature of the first curing oven is 80°C to 250°C, the curing temperature of the second curing oven is 80°C to 250°C, and the curing temperature of the third curing oven is 350°C to 600°C.

[0016] According to the third aspect of the utility model, a high temperature resistant optical fiber is provided. The optical fiber is obtained according to the above optical fiber coating platform. The out-of-roundness of the high temperature resistant optical fiber is not greater than 0.5%, and the concentricity error is not greater than 1um.

[0017] In general, the above technical solutions conceived by the utility model can achieve the following beneficial effects compared with the prior art:

[0018] (1) The utility model provides an optical fiber coating mold, comprising an integrally formed first fixing mechanism, a second fixing mechanism and a conical receiving cavity. The degree of alignment of the first fixing mechanism relative to the base of the drawing tower can be adjusted by adjusting the distance of the screws, that is, the degree of alignment of the conical receiving cavity can be adjusted, so that the concentricity of the optical fiber coating after the coated optical fiber passes through the outlet of the conical receiving cavity is better, and accordingly, the tensile strength of the optical fiber is also higher.

[0019] (2) The utility model provides an optical fiber coating platform which uses two coating steps to simplify the operation steps in the production process of high-temperature resistant optical fiber, and overcomes the problem that the existing polyimide optical fiber needs multiple coatings and curing during the production process, which results in complicated operation, thereby achieving the purpose of improving the production efficiency of polyimide optical fiber. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.

[0021] Figure 1 A schematic diagram of the structure of an optical fiber coating platform provided by an embodiment of the utility model;

[0022] Figure 2 A schematic structural diagram of a first coating die provided in an embodiment of the utility model;

[0023] Figure 3 A schematic diagram of the structure of a high temperature resistant optical fiber provided in an embodiment of the utility model;

[0024] Figure 4 A front view of a first coating die provided in an embodiment of the utility model;

[0025] Figure 5 A cross-sectional view of a first coating die provided in an embodiment of the utility model;

[0026] Figure 6 A top view of a first coating die provided in an embodiment of the utility model;

[0027] Figure 7 A schematic diagram of a coating device provided in an embodiment of the utility model;

[0028] The accompanying drawings are marked as follows:

[0029] 1: first coating mold, 2: first curing oven, 3: second coating mold, 4: second curing oven, 5: third curing oven, 6: coating cup, 7: junction of first fixing mechanism and second fixing mechanism, 11: first fixing mechanism, 12: second fixing mechanism, 13: conical placement cavity, 10: bare optical fiber, 20: inner coating, 30: outer coating. DETAILED DESCRIPTION

[0030] In order to make the purpose, technical solution and advantages of the utility model more clear, the utility model is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described herein are only used to explain the utility model and are not used to limit the utility model. In addition, the technical features involved in each embodiment of the utility model described below can be combined with each other as long as they do not conflict with each other.

[0031] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art in the technical field of the present invention. The terms used herein in the specification of the present invention are only for the purpose of describing specific embodiments and are not intended to limit the present invention. The term "and / or" used herein includes any and all combinations of one or more of the related listed items.

[0032] In the description of the present invention, it should be understood that the terms "upper", "lower", "vertical", "horizontal", "inside", "outside", etc., indicating orientations or positional relationships, are based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention.

[0033] It should be understood that the terms "first", "second" and similar terms used in the description of the present invention do not indicate any order, quantity or importance, but are only used to distinguish different components. Unless the context clearly indicates otherwise, the singular form of "a", "an" or "the" and similar terms do not indicate a quantity limitation, but indicate the presence of at least one. In addition, the terms "including" and "having" and any of their variations are intended to cover non-exclusive inclusions.

[0034] Figure 1 It is a schematic diagram of the structure of the optical fiber coating platform. Figure 1 As shown, the optical fiber coating platform includes a first coating mold 1 , a first curing oven 2 , a second coating mold 3 , a second curing oven 4 and a third curing oven 5 .

[0035] The first coating mold 1 and the second coating mold 3 have substantially the same structure, both comprising a first fixing mechanism, a second fixing mechanism and a tapered placement cavity. The first coating mold 1 is taken as an example for description. Figure 2 Schematic diagram of the structure of the first coating die 1. Figure 2 As shown, the first coating mold 1 includes a first fixing mechanism 11, a second fixing mechanism 12 and a tapered receiving cavity 13, wherein the first fixing mechanism 11, the second fixing mechanism 12 and the tapered receiving cavity 13 are integrally formed and are all made of metal materials; and the first fixing mechanism 11, the second fixing mechanism 12 and the tapered receiving cavity 13 are sequentially connected to form a through groove (or called an optical fiber coating channel) that is interconnected, and the first fixing mechanism 11 is connected to the coating cup 6 through the through groove. The second fixing mechanism is located between the first fixing mechanism and the tapered receiving cavity.

[0036] The area of ​​the first fixing mechanism 11 is larger than the area of ​​the second fixing mechanism 12, and the first fixing mechanism 11 is coaxial with the second fixing mechanism 12. The base of the drawing tower is engaged with the joint 7 of the first fixing mechanism 11 and the second fixing mechanism 12. The base of the drawing tower is a hollow annular structure, which is composed of a frame of the base and a through hole of the base. The first fixing mechanism 11 is threadedly connected to the frame of the base of the drawing tower, and one end of the first fixing mechanism is located at the through hole of the base, and the other end is connected to the coating cup 6 through a through groove. The diameter end of the second fixing mechanism is arranged at the through hole of the base and protrudes out of the through hole, and the protruding end of the second fixing mechanism is connected to the conical receiving cavity. Through such a structural design, the one-piece coating mold can be firmly fixed on the base of the drawing tower, and the coating in the coating cup 6 can reach the inner cavity of the conical receiving cavity through the through groove of the first fixing mechanism and the through groove of the second fixing mechanism in turn.

[0037] Exemplarily, the first fixing mechanism 11 is fixed to the base by screws, and the depth of the screws embedded in the base is positively correlated with the degree of alignment of the conical receiving cavity 13 relative to the base. In other words, the alignment of the first fixing mechanism relative to the base of the drawing tower can be adjusted by adjusting the distance of the screws (i.e., the depth of the screws embedded in the base). The alignment of the conical receiving cavity depends on the alignment of the first fixing mechanism of the one-piece coating mold relative to the base of the drawing tower. Therefore, the alignment of the conical receiving cavity can be adjusted by controlling the distance of the screws, so that the concentricity of the optical fiber coating after the coating is better after passing through the outlet of the conical receiving cavity, and accordingly, the tensile strength of the coated optical fiber is also higher.

[0038] The conical receiving cavity 13 is a conical cavity for accommodating the bare optical fiber and the coating material. One end (large diameter end) is connected to the second fixing mechanism, and the other end (tip) is provided with a through hole. The through hole serves as the outlet of the coated optical fiber, and the coated optical fiber passes through the through hole. The conical receiving cavity forms a stable coating pressure at the through hole.

[0039] Specifically, the conical receiving cavity of the first coating mold 1 is used to accommodate the bare optical fiber and the coating material, wherein the bare optical fiber includes a quartz core layer and an optical fiber cladding from the inside to the outside, and the coating material is a polyimide material.

[0040] The accommodating cavity of the second coating mold 3 is used to accommodate the first layer of coated optical fiber and the coating material, wherein the first layer of coated optical fiber is composed of a bare optical fiber and an inner coating coated on the surface of the bare optical fiber. After the first layer of coated optical fiber passes through the second coating mold 3, a second layer of coated optical fiber is obtained, wherein the second layer of coated optical fiber is composed of a bare optical fiber, an inner coating coated on the surface of the bare optical fiber, and an outer coating coated on the surface of the inner coating. After curing the second layer of coated optical fiber, the following is obtained: Figure 3 High temperature resistant optical fiber shown.

[0041] Figure 3 It is a schematic diagram of the structure of high temperature resistant optical fiber. Figure 3 As shown, the high temperature resistant optical fiber is composed of a bare optical fiber 10, an inner coating 20 coated on the surface of the bare optical fiber, and an outer coating 30 coated on the surface of the inner coating.

[0042] In one embodiment, the inner diameter of the tapered receiving cavity gradually decreases toward the tip, and the tip of the tapered receiving cavity is processed along the direction in which the inner diameter of the tapered receiving cavity gradually decreases, thereby forming an outlet for the coated optical fiber. The roundness of this outlet can be precisely controlled, so that the coated optical fiber has a smaller non-roundness after passing through the outlet of the tapered receiving cavity.

[0043] In one embodiment, the through hole at the tip of the conical cavity is a circular through hole. The non-circularity of the through hole at the tip of the conical cavity is no more than 0.3%. The inner diameter of the through hole at the tip of the conical cavity is 210um to 290um. The height of the conical cavity is 20mm to 30mm.

[0044] The inner diameters of the through holes of the first coating die 1 and the second coating die 3 are different. The inner diameter of the through hole of the first coating die 1 is larger than the inner coating diameter, and the inner diameter of the through hole of the second coating die 3 is larger than the outer coating diameter.

[0045] Among them, the inner coating diameter is the diameter of the optical fiber cladding and the double-sided coating thickness of the first coating mold 1, and the outer coating diameter is the sum of the diameter of the optical fiber cladding, the double-sided coating thickness of the first coating mold 1 and the double-sided coating thickness of the second coating mold 3.

[0046] Exemplarily, the diameter of the optical fiber cladding is 125 um, the double-sided coating thickness of the first coating die 1 is 13.5 um to 15 um, and the double-sided coating thickness of the second coating die is 13.5 to 16.5 um.

[0047] Among them, reference Figure 3Since the inner coating 20 and the inner coating 30 are both annular, the double-sided coating thickness of the first coating die is twice the difference between the outer diameter and the inner diameter of the inner coating, and the double-sided coating thickness of the second coating die is twice the difference between the outer diameter and the inner diameter of the outer coating.

[0048] The inner diameter of the through hole at the tip of the conical cavity of the first coating mold 1 is 210um~240um, and the non-roundness of the through hole at the tip of the conical cavity is not greater than 0.3%. The inner diameter of the through hole at the tip of the conical cavity of the second coating mold 3 is 270um~290um, and the non-roundness of the through hole at the tip of the conical cavity is not greater than 0.3%. Figure 5 As shown, the inner diameter of the through hole of the first coating die 1 is 0.210±0.002 mm.

[0049] like Figure 4 As shown, the outer diameter of the through hole at the tip of the tapered cavity of the first coating mold 1 is 2 mm. The outer diameters of the through holes at the tip of the tapered cavity of the second coating mold 2 and the first coating mold 1 can be the same or different.

[0050] In one embodiment, the outer diameter of the first fixing mechanism 11 is greater than the diameter of the through hole of the base, and the outer diameter of the second fixing mechanism 12 is equal to the diameter of the through hole of the base. The first fixing mechanism 11 is a flat hollow cylinder, and a first through groove is provided in the axial direction of the cylinder; the second fixing mechanism 12 is a flat hollow cylinder, and a second through groove is provided in the axial direction of the cylinder; the first through groove, the second through groove and the inner cavity of the tapered receiving cavity form the above-mentioned mutually connected through grooves.

[0051] For example, Figure 4 As shown, the outer diameter of the first fixing mechanism 11 of the first coating die 1 is 84 mm, and the outer diameter of the second fixing mechanism 12 of the first coating die 1 is 62 mm.

[0052] In one embodiment, Figure 2 As shown, the outer diameter of the second fixing mechanism 12 is larger than the outer diameter of the large diameter end of the tapered receiving cavity 13 .

[0053] For example, Figure 4 As shown, the outer diameter of the second fixing mechanism 12 of the first coating die 1 is 62 mm, and the outer diameter of the large diameter end of the tapered receiving cavity 13 of the first coating die 1 is 15 mm.

[0054] In one embodiment, the height of the tapered receiving cavity 13 is greater than the height of the first fixing mechanism 11 , and the height of the first fixing mechanism 11 is greater than the height of the second fixing mechanism 12 .

[0055] For example, Figure 4 As shown, the height of the tapered receiving cavity 13 is 25 mm, the height of the first fixing mechanism 11 is 10 mm, and the height of the second fixing mechanism 12 is 8 mm.

[0056] Figure 6 : is a top view of the first coating mold provided by the embodiment of the utility model. Figure 6 As shown, three screws are installed on the first fixing mechanism 11, and the three screws are threadedly connected to the base of the drawing tower so that the optical fiber coating mold is fixed on the base.

[0057] In one embodiment, the first curing oven 2 and the second curing oven 4 are both low-temperature curing, and the third curing oven 5 is high-temperature curing. The first curing oven 2, the second curing oven 4 and the third curing oven 5 are all equipped with temperature control units, which are commonly used temperature control chips for controlling the heating power to control the temperature of the heating wire. Among them, the curing temperature of the first curing oven 2 is 80°C~250°C, the curing temperature of the second curing oven 4 is 80°C~250°C, and the curing temperature of the third curing oven 5 is 350°C~600°C.

[0058] The following describes the steps for coating an optical fiber using the optical fiber coating platform.

[0059] After the optical fiber passes through the first coating mold 1, the optical fiber after the first layer of coating passes through the through hole of the tapered receiving cavity of the first coating mold 1, enters the first curing furnace 2, and is cured at gradually increasing curing temperatures such as 80°C, 150°C, 200°C, and 250°C; then enters the second coating mold 3, passes through the second coating mold 3 to apply the second layer of coating to it, and the optical fiber after the second layer of coating passes through the through hole of the tapered receiving cavity of the second coating mold 3; enters the second curing furnace 4, and is cured at gradually increasing curing temperatures such as 80°C, 150°C, 200°C, and 250°C; then enters the third curing furnace 5, and is baked at a high temperature of 350°C to 600°C until it is completely imidized to obtain a high-temperature resistant optical fiber.

[0060] In one embodiment, the out-of-roundness of the high-temperature resistant optical fiber obtained by using the above optical fiber coating platform is no more than 0.5%, and the concentricity error is no more than 1 um.

[0061] In one embodiment, both the inner coating and the outer coating are made of high-viscosity, high-solid content polyimide coating materials, wherein the viscosity of the coating material of the inner coating ranges from 8500cp to 12000cp, and the solid content ranges from 28% to 32%; the viscosity of the coating material of the outer coating ranges from 10000cp to 12000cp, and the solid content ranges from 28% to 35%.

[0062] In one embodiment, the inner coating layer uses a coating material with low Tg and low modulus, wherein the Tg value range of the coating material of the inner coating layer is 250°C~280°C, and the modulus value range is 500MPa~1000MPa; and low-temperature curing is adopted, the curing temperature is 80°C~200°C, and the curing temperature increases in a step-by-step manner, so that the stress of the coating material is slowly released during the film formation process, so as to improve the flexibility of the inner coating layer and reduce the stress between the inner coating layer and the glass part of the optical fiber.

[0063] In one embodiment, the outer coating layer is made of a high Tg, high modulus polyimide coating material, wherein the Tg value range of the polyimide coating material of the outer coating layer is 350°C~450°C, and the modulus value range is 1800MPa~4000MPa; and it is cured at high temperature, the curing temperature is 350°C~600°C, and the coating material is completely imidized to form a high-strength outer coating, thereby achieving the purpose of improving the high temperature resistance of the optical fiber to resist external stress damage.

[0064] Table 1 is the test results of coating non-circularity and coating / cladding concentricity error of high temperature resistant optical fiber produced by using the optical fiber coating mold provided by this embodiment.

[0065] Table 1

[0066]

[0067] It can be seen from Table 1 that compared with conventional optical fiber (50PI optical fiber coated with a rubber nozzle), the high-temperature resistant optical fiber produced using the optical fiber coating mold provided in this embodiment has a smaller coating non-circularity, better coating / cladding concentricity, and more precise coating diameter / outer diameter.

[0068] Table 2 is the tensile strength test results of the high temperature resistant optical fiber produced by using the optical fiber coating mold provided in this embodiment.

[0069] Table 2

[0070]

[0071] It can be seen from Table 2 that, compared with conventional optical fibers (50PI optical fibers coated with rubber nozzles), the high-temperature resistant optical fibers produced using the optical fiber coating mold provided in this embodiment have greater tensile strength.

[0072] Table 3 shows the coating performance test results of the high temperature resistant optical fiber produced by the optical fiber coating platform provided in this embodiment and the performance test results of the coating after film formation.

[0073] Table 3

[0074]

[0075] Referring to Table 3, after testing, the high-temperature resistant optical fiber produced using the optical fiber coating platform provided in this embodiment has an inner coating material having a tensile strength greater than 100 MPa and an elongation at break greater than 80% after film formation, and an outer coating material having a tensile strength greater than 150 MPa and an elongation at break greater than 30% after film formation.

[0076] The above is only an exemplary embodiment of the present disclosure, and the scope of the present disclosure cannot be limited thereto. That is, any equivalent changes and modifications made according to the teachings of the present disclosure are still within the scope of the present disclosure. After considering the specification and practicing the disclosure here, those skilled in the art will easily think of the implementation scheme of the present disclosure. The utility model is intended to cover any variation, use or adaptive change of the present disclosure, which follows the general principles of the present disclosure and includes common knowledge or customary technical means in the technical field not recorded in the present disclosure. The description and examples are regarded as exemplary only, and the scope and spirit of the present disclosure are defined by the claims.

[0077] The technical features of the above embodiments may be combined arbitrarily. To make the description concise, not all possible combinations of the technical features in the above embodiments are described. However, as long as there is no contradiction in the combination of these technical features, they should be considered to be within the scope of this specification.

[0078] It is easy for those skilled in the art to understand that the above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. An optical fiber coating mold, characterized in that: It includes a first fixing mechanism, a second fixing mechanism and a conical placement cavity, wherein: The first fixing mechanism, the second fixing mechanism and the conical receiving cavity are integrally formed and a through groove is formed between the three of them, the second fixing mechanism is located between the first fixing mechanism and the conical receiving cavity, and the first fixing mechanism is connected to the coating cup through the through groove; The area of ​​the first fixing mechanism is larger than that of the second fixing mechanism, the base of the drawing tower is engaged with the junction of the first fixing mechanism and the second fixing mechanism, and the base is a hollow annular structure; The first fixing mechanism is fixed to the base of the drawing tower by screws, and the depth of the screws embedded in the base is positively correlated with the degree of alignment of the conical receiving cavity relative to the base; The tip of the conical cavity is provided with a through hole, which serves as an outlet for the coated optical fiber; the large diameter end of the conical cavity is connected to the second fixing mechanism; The tapered receiving cavity is used to accommodate coating materials and bare optical fibers / optical fibers after single-layer coating.

2. The optical fiber coating mold according to claim 1, characterized in that: The through hole at the tip of the tapered cavity is a circular through hole, and the out-of-roundness of the through hole at the tip of the tapered cavity is no more than 0.3%.

3. The optical fiber coating mold according to claim 1 or 2, characterized in that: The inner diameter of the through hole at the tip of the conical cavity is 210um-290um.

4. The optical fiber coating mold according to claim 3, characterized in that: The height of the conical receiving cavity is 20 mm to 30 mm.

5. The optical fiber coating mold according to claim 4, characterized in that: The first fixing mechanism is a flat hollow cylinder, and a first through groove is provided in the axial direction of the cylinder; The second fixing mechanism is a flat hollow cylinder, and a second through groove is provided in the axial direction of the cylinder; The first fixing mechanism is coaxial with the second fixing mechanism; the first through groove, the second through groove and the inner cavity of the tapered accommodating cavity are interconnected.

6. An optical fiber coating platform, characterized in that: It includes a first coating mold, a first curing oven, a second coating mold, a second curing oven and a third curing oven which are arranged in sequence; The first coating die and the second coating die are both optical fiber coating dies as described in any one of claims 1 to 5, and the inner diameter of the through hole of the tapered receiving cavity of the first coating die is smaller than the inner diameter of the through hole of the tapered receiving cavity of the second coating die; The conical receiving cavity of the first coating mold is used to accommodate the bare optical fiber and the coating material, and the conical receiving cavity of the second coating mold is used to accommodate the optical fiber and the coating material after the first layer of coating.

7. The optical fiber coating platform according to claim 6, characterized in that: The out-of-roundness of the through hole at the tip of the tapered cavity of the first coating die is no more than 0.3%, and the inner diameter is 210um-240um; and / or, The out-of-roundness of the through hole at the tip of the tapered cavity of the second coating die is no more than 0.3%, and the inner diameter is 270um-290um.

8. The optical fiber coating platform according to claim 7, characterized in that: The coating materials in the first coating mold and the second coating mold are both polyimide.

9. The optical fiber coating platform according to claim 7, characterized in that: The curing temperature of the first curing oven is 80°C to 250°C, the curing temperature of the second curing oven is 80°C to 250°C, and the curing temperature of the third curing oven is 350°C to 600°C.

10. A high temperature resistant optical fiber, characterized in that: The optical fiber is obtained according to the optical fiber coating platform described in any one of claims 6 to 9, the high temperature resistant optical fiber comprises a bare optical fiber, an inner coating and an outer coating from the inside to the outside, the out-of-roundness of the high temperature resistant optical fiber is not greater than 0.5%, and the concentricity error is not greater than 1um.

Citation Information

Cited By

  • Photoelectric composite cable suitable for unmanned aerial vehicle platform

    CN120183802A

  • Photoelectric composite cable suitable for unmanned aerial vehicle platform

    CN224232397U