Tool for improving qualified rate of peripheral welding of square laminated lithium ion battery
By designing welding frames and adjusting nuts and springs, the adaptation and dropping of cover plates and shells in square shell lithium battery assembly is solved, the appearance and quality of welding are improved, and the pass rate of peripheral welding is improved.
Patent Information
- Application Number
- CN202420235353.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-01-31
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2034-01-31
AI Technical Summary
During the assembly of square shell lithium battery, the adaptation requirements of the cover plate and the shell are high and easy to fall during the peripheral welding process, resulting in residual glue pre-spot welding, affecting the appearance and quality of the welding.
A tooling including a welded frame, adjustment nut and spring is designed. The adjustment nut and spring are installed on the top and sides of the welded frame, combining the transverse and longitudinal fixing plates to ensure the tightness and welding stability of the cover plate and the shell. , reduce gaps and improve the fixture of welding fixtures.
It effectively reduces the gap between the cover plate and the shell, improves the appearance flatness and quality of the welding, and improves the pass rate of peripheral welding.
Smart Images

Figure CN222095130U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of square shell lithium battery production, in particular to a tool for improving the peripheral welding pass rate of square laminated lithium ion batteries. Background Art
[0002] In the assembly and production process of square shell lithium batteries, the peripheral welding has high requirements for the fit between the cover and the shell, and there is a risk of falling when it is placed in the welding fixture. Most companies will use the glue sticking method, which can solve the fit problem, but there will be a small amount of residue after the pre-spot welding, which seriously affects the appearance and quality of the peripheral welding, so the glue sticking method needs to be replaced.
[0003] Therefore, the utility model provides a tool for improving the pass rate of peripheral welding of square laminated lithium-ion batteries to solve the above problems. Utility Model Content
[0004] The purpose of the utility model is to provide a tool for improving the pass rate of peripheral welding of square laminated lithium-ion batteries, so as to solve the problems raised in the above-mentioned background technology.
[0005] To achieve the above-mentioned purpose, the utility model provides the following technical solutions: a tool for improving the pass rate of peripheral welding of square laminated lithium-ion batteries, characterized in that it includes a welding frame, the top of the welding frame is threadedly engaged with five No. 1 adjusting nuts at equal intervals, a transverse fixing plate is provided at the top inside the welding frame, the bottom of the No. 1 adjusting nut is fixedly connected to the top of the transverse fixing plate, the left side of the welding frame is threadedly engaged with two No. 2 adjusting nuts, a longitudinal fixing plate is provided on the left side of the welding frame, and the end of the No. 2 adjusting nut is fixedly connected to the left side wall of the longitudinal fixing plate.
[0006] Preferably, the top and bottom ends of the front side of the welding frame are each provided with four welding grooves corresponding to each other in the upper and lower directions.
[0007] Preferably, a No. 1 adjusting spring and a No. 2 adjusting spring are respectively mounted on the outer sides of the No. 1 adjusting nut and the No. 2 adjusting nut.
[0008] Preferably, the welding frame, the transverse fixing plate and the longitudinal fixing plate are made of red copper, and the No. 1 adjusting nut, the No. 1 adjusting spring, the No. 2 adjusting nut and the No. 2 adjusting spring are made of stainless steel.
[0009] Beneficial effects of the utility model:
[0010] The utility model reduces the gap between the cover plate and the shell during pre-spot welding, increases the fixation in the welding fixture, makes the peripheral welding smooth in appearance, and achieves the quality that meets the process requirements. BRIEF DESCRIPTION OF THE DRAWINGS
[0011] In order to more clearly illustrate the technical solutions of the embodiments of the utility model, the drawings required for use in the embodiments will be briefly introduced below. It should be understood that the following drawings only show certain embodiments of the utility model and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other relevant drawings can be obtained based on these drawings without paying creative work.
[0012] Figure 1 It is a schematic diagram of the overall structure of the utility model;
[0013] Figure 2 It is a front view of the utility model.
[0014] In the figure: 1. welding frame; 2. horizontal fixing plate; 3. No. 1 adjusting nut; 4. No. 1 adjusting spring; 5. longitudinal fixing plate; 6. No. 2 adjusting nut; 7. No. 2 adjusting spring; 8. welding groove. DETAILED DESCRIPTION
[0015] In order to make the purpose, technical scheme and advantages of the embodiments of the utility model clearer, the technical scheme in the embodiments of the utility model will be clearly and completely described below in conjunction with the drawings in the embodiments of the utility model. Therefore, the following detailed description of the embodiments of the utility model provided in the drawings is not intended to limit the scope of the utility model claimed for protection, but merely represents the selected embodiments of the utility model. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the utility model.
[0016] The utility model provides Figure 1-2 A tooling for improving the peripheral welding pass rate of square laminated lithium-ion batteries is shown, including a welding frame 1, five No. 1 adjusting nuts 3 are installed on the top of the welding frame 1 by threaded engagement at equal intervals, a transverse fixing plate 2 is provided on the top of the inside of the welding frame 1, the bottom of the No. 1 adjusting nut 3 is fixedly connected to the top of the transverse fixing plate 2, two No. 2 adjusting nuts 6 are installed on the left side of the welding frame 1 by threaded engagement, a longitudinal fixing plate 5 is provided on the left side of the welding frame 1, the end of the No. 2 adjusting nut 6 is fixedly connected to the left side wall of the longitudinal fixing plate 5), wherein the lengths of the transverse fixing plate 2 and the longitudinal fixing plate 5 are slightly smaller than the length and width of the shell to be welded, and are controlled at 3-5mm, thereby ensuring that there is no interference between the No. 1 adjusting spring 4 and the No. 2 adjusting spring 7 when subjected to force.
[0017] Furthermore, four upper and lower corresponding welding grooves 8 are respectively provided at the top and bottom of the front side of the welding frame 1. The size of the welding grooves 8 is larger than the pre-spot welding points by more than 3 mm to ensure that the laser has sufficient welding margin.
[0018] Furthermore, the outer sides of the No. 1 adjusting nut 3 and the No. 2 adjusting nut 6 are respectively provided with a No. 1 adjusting spring 4 and a No. 2 adjusting spring 7 .
[0019] Furthermore, the welding frame 1, the transverse fixing plate 2 and the longitudinal fixing plate 5 are made of red copper, and the No. 1 adjusting nut 3, the No. 1 adjusting spring 4, the No. 2 adjusting nut 6 and the No. 2 adjusting spring 7 are made of stainless steel, whose high temperature resistance can well prevent the high temperature during the welding process from damaging the device.
[0020] Working principle:
[0021] During the actual operation, the entire battery is placed flat on the table, leaving the installation position of the device, and the No. 1 adjusting nut 3, No. 1 adjusting spring 4, No. 2 adjusting nut 6, No. 2 adjusting spring 7, transverse fixing plate 2, and longitudinal fixing plate 5 are installed in place. First, let the short side of the positive electrode of the battery contact the longitudinal fixing plate 5, and then press the longitudinal fixing plate 5 to allow the No. 2 adjusting spring 7 to be stressed, slowly lift the transverse fixing plate 2 and press it into the long side of the battery, and then put the entire positive electrode of the battery into the welding frame 1. Similarly, the negative electrode is installed in the same way. After installation, put the entire battery into the welding station for pre-spot welding. At this time, the gap between the cover plate and the shell is reduced, and the fixation in the welding fixture is increased, so that the appearance is smooth after the surrounding welding, the quality meets the process requirements, and the yield is improved.
[0022] The above are only preferred embodiments of the present invention and are not intended to limit the present invention. For those skilled in the art, the present invention may be subject to various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.
Claims
1. A tool for improving the pass rate of peripheral welding of square laminated lithium-ion batteries, characterized in that: The invention comprises a welding frame (1), wherein five No. 1 adjusting nuts (3) are installed at equal intervals on the top of the welding frame (1) by thread engagement, a transverse fixing plate (2) is provided on the top of the inside of the welding frame (1), the bottom of the No. 1 adjusting nut (3) is fixedly connected to the top of the transverse fixing plate (2), two No. 2 adjusting nuts (6) are installed on the left side of the welding frame (1) by thread engagement, a longitudinal fixing plate (5) is provided on the left side of the welding frame (1), and the end of the No. 2 adjusting nut (6) is fixedly connected to the left side wall of the longitudinal fixing plate (5).
2. A tool for improving the peripheral welding pass rate of square laminated lithium-ion batteries according to claim 1, characterized in that: The top and bottom ends of the front side of the welding frame (1) are each provided with four welding grooves (8) corresponding to each other in the upper and lower directions.
3. A tool for improving the peripheral welding pass rate of square laminated lithium-ion batteries according to claim 1, characterized in that: The outer sides of the No. 1 adjusting nut (3) and the No. 2 adjusting nut (6) are respectively provided with a No. 1 adjusting spring (4) and a No. 2 adjusting spring (7).
4. A tool for improving the peripheral welding pass rate of square laminated lithium-ion batteries according to claim 1, characterized in that: The welding frame (1), the transverse fixing plate (2) and the longitudinal fixing plate (5) are made of red copper, and the No. 1 adjusting nut (3), the No. 1 adjusting spring (4), the No. 2 adjusting nut (6) and the No. 2 adjusting spring (7) are made of stainless steel.