Injection mold convenient for cooling plastic product
By setting an annular boss and grooves on the upper and lower mold edges of the injection mold, and using cooling airflow to blow air and cool down, the problem of easy contamination of the surface of the plastic product after the injection mold is opened is solved, and rapid cooling and clean mold release is achieved.
Patent Information
- Application Number
- CN202420369122.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-02-28
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2034-02-28
AI Technical Summary
Plastic products after injection molds are opened are easily contaminated by workshop impurities during the blowing and cooling process, because the surface of the plastic products is directly exposed to the air, resulting in impurities contamination.
An injection mold is designed, by providing suitable annular bosses and grooves on the edges of the upper mold and the lower mold, and air inlet holes and air outlet grooves on the left and right sides of the boss, using a blower and cooling The fan provides cooling airflow to blow inside the mold to the surface of the plastic product to avoid contact with external impurities.
It achieves rapid cooling and mold removal of plastic products, avoids impurity contamination and ensures surface cleanliness.
Smart Images

Figure CN222096818U_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of injection molds, and in particular to an injection mold that facilitates cooling of plastic products. Background Art
[0002] Injection mold is a key tool for producing plastic products. It is a tool used to inject molten plastic material into the mold cavity and then form the desired shape through cooling and solidification. Injection mold is usually divided into upper mold assembly and lower mold assembly, which can be quickly opened and closed on the injection molding machine. The main components of injection mold include: mold shell, mold cavity, mold core, runner system, cooling system, ejector, bottom plate, etc. Injection mold is usually installed on the injection molding machine for mold opening and mold closing. After the injection mold is opened, the surface of some molded plastic products has not been completely cooled and is not easy to demold, so it is necessary to blow air to cool it down. However, the plastic products after mold opening will be directly exposed to the air. If the surface of the plastic products is directly blown to cool it down, impurities in the workshop air will be blown to the surface of the plastic products. Since the surface of the plastic products after mold opening will still have residual temperature for a short time, impurities will be contaminated on its surface, causing pollution to the surface of the plastic products. Utility Model Content
[0003] In view of the deficiencies in the prior art, the purpose of this application is to provide an injection mold that facilitates cooling of plastic products, so as to solve the problems raised in the above background technology.
[0004] According to one aspect of the present application, an injection mold for facilitating cooling of plastic products comprises an upper mold, an upper mold core, a lower mold and a lower mold core, wherein the upper mold core is embedded in the middle of the bottom surface of the upper mold, the bottom surface of the upper mold is assembled in close contact with the top surface of the lower mold, the lower mold core is embedded in the middle of the top surface of the lower mold, the lower mold core is in close contact with the edge of the upper mold core and a molding cavity is formed in the middle of the two, an annular groove is opened downward at the edge position around the top of the lower mold, and the annular groove is connected to the outer peripheral side of the lower mold, and an annular boss is extended downward at the edge position around the bottom of the upper mold , and the annular boss is flush with the outer peripheral side of the upper mold, and the annular boss and the annular groove correspond to each other up and down and are adapted to each other. When the upper mold and the lower mold are tightly matched, the annular boss and the annular groove are tightly matched. The left and right sides of the annular boss are penetrated with multiple air inlet holes along its width direction, and an air inlet joint is fixedly installed at the outer port of each air inlet hole. The front and rear sides of the annular boss are penetrated with air outlet grooves, and each of the air inlet joints is connected to the blower through a connecting pipe, and the blower is connected to the refrigeration fan.
[0005] Preferably, the length and width of the air outlet groove are smaller than the length and width of the annular groove.
[0006] Preferably, an upper template is fixedly installed on the top surface of the upper mold, supporting side plates are fixedly installed on both sides of the bottom surface of the lower mold, a lower template is fixedly installed on the bottom surface of the supporting side plates, an ejection through hole is penetrated through the center portion of the lower template, a first linkage plate is arranged above the lower template, in an initial state, the first linkage plate is in contact with the lower template, a second linkage plate is fixedly installed on the top surface of the first linkage plate, the middle part of the top surface of the second linkage plate is fixedly connected to the lower ends of a plurality of ejector rods, the upper ends of the plurality of ejector rods slide in sequence from bottom to top through the second linkage plate, the lower mold and the lower mold core and are flush with the top surface of the lower mold core, a plurality of support springs are arranged between the top surface of the second linkage plate and the bottom surface of the lower mold.
[0007] Preferably, limiting grooves are provided on the top surface of the second linkage plate and the bottom surface of the lower mold at both ends of the support spring, both ends of the support spring are arranged in the limiting grooves, and the support spring is in a compressed state.
[0008] Preferably, both sides of the first linking plate and the second linking plate are slidably connected to the opposite side sides of the supporting side plates on both sides.
[0009] Preferably, a communicating injection channel is formed through the upper template, the upper mold and the upper mold core, the injection channel on the upper mold core is a conical structure, and a gate sleeve is installed at the top of the upper template at the position of the injection channel.
[0010] The advantages of the present application over the prior art are as follows: an injection mold of the present application that facilitates cooling of plastic products, through the matching annular bosses and annular grooves respectively arranged on the edges of the upper mold and the lower mold, and the air inlet holes arranged on the left and right sides of the annular bosses and the air outlet grooves arranged on the front and rear sides thereof, so that after the plastic product is formed in the molding cavity and cooled by the cooling system of the mold itself, the injection molding machine first pulls the lower mold plate of the injection mold mounted thereon by a certain distance, so that the annular groove on the lower mold and the annular boss on the upper mold move relative to each other, and the annular boss is not completely separated from the annular groove, and the air inlet holes and the air outlet grooves on the annular boss are separated and exposed from the annular groove, at this time, the blower is started to transport the cooling airflow of the refrigeration fan through the connecting pipe to the cavity formed between the upper mold and the lower mold, so that the cooling airflow is blown to the surface of the plastic product and blown out from the air outlet groove, thereby cooling the surface of the plastic product, so that the plastic product is quickly formed and easier to demold, and the blowing and cooling process does not contact the outside world, thereby avoiding impurities from being contaminated on the surface of the plastic product. BRIEF DESCRIPTION OF THE DRAWINGS
[0011] Figure 1It is a stereoscopic diagram of an injection mold that facilitates cooling of plastic products according to an embodiment of the present application.
[0012] Figure 2 It is a three-dimensional cross-sectional view of an injection mold that facilitates cooling of plastic products according to an embodiment of the present application.
[0013] Figure 3 It is a main cross-sectional view of a blowing cooling process of an injection mold that facilitates cooling of plastic products according to an embodiment of the present application.
[0014] Figure 4 It is a side sectional view of an air blowing cooling process of an injection mold for facilitating cooling of a plastic product according to an embodiment of the present application.
[0015] Figure numerals: 1. upper mold; 2. upper mold core; 3. lower mold; 4. lower mold core; 5. molding cavity; 6. annular groove; 7. annular boss; 8. air inlet; 9. air inlet joint; 10. air outlet groove; 11. connecting pipe; 12. blower; 13. refrigeration fan; 14. upper template; 15. supporting side plate; 16. lower template; 17. ejector hole; 18. first linkage plate; 19. second linkage plate; 20. ejector rod; 21. supporting spring; 22. limiting groove; 23. injection channel; 24. gate sleeve. DETAILED DESCRIPTION
[0016] In order to make the content of this application easier to understand, the technical solutions in the embodiments of this application will be described clearly and completely in conjunction with the drawings in the embodiments of this application. It should be noted that the words "front", "rear", "left", "right", "upper" and "lower" used in the following description refer to the attached drawings. Figure 3 In the context of the present invention, the words "inside" and "outside" refer to directions toward or away from the geometric center of a particular component, respectively. In addition, the terms "first", "second", etc. are used only for descriptive purposes and cannot be understood as indicating or implying relative importance.
[0017] like Figure 1 to Figure 4As shown, an injection mold for cooling a plastic product comprises an upper mold 1, an upper mold core 2, a lower mold 3 and a lower mold core 4. An upper mold plate 14 is fixedly mounted on the top surface of the upper mold 1, and an upper mold core 2 is embedded in the middle of the bottom surface of the upper mold 1. A connected injection channel 23 is provided through the upper mold plate 14, the upper mold 1 and the upper mold core 2. The injection channel 23 on the upper mold core 2 is a conical structure for easy demoulding. A gate sleeve 24 is installed at the top of the upper mold plate 14 at the position of the injection channel 23. The bottom surface of the upper mold 1 is closely contacted and assembled with the top surface of the lower mold 3. The lower mold core 4 is embedded in the middle of the top surface of the lower mold 3. The lower mold core 4 is closely contacted with the edge of the upper mold core 2 and a molding cavity 5 is formed in the middle of the two. An annular groove 6 is provided downward at the edge of the top of the lower mold 3. , and the annular groove 6 is connected to the outer peripheral side of the lower mold 3, and an annular boss 7 is extended downward at the edges of the bottom of the upper mold 1, and the annular boss 7 is flush with the outer peripheral side of the upper mold 1, and the annular boss 7 corresponds to the annular groove 6 up and down and the two are adapted. When the upper mold 1 and the lower mold 3 are tightly matched, the annular boss 7 and the annular groove 6 are tightly matched. The left and right sides of the annular boss 7 are penetrated along the width direction thereof. A plurality of air inlet holes 8 are opened, and an air inlet joint 9 is fixedly installed at the outer port of each air inlet hole 8. An air outlet groove 10 is penetrated on both the front and rear sides of the annular boss 7, and the length and width of the air outlet groove 10 are smaller than the length and width of the annular groove 6. This design can ensure that the annular boss 7 and the annular groove 6 are tightly matched. No gap is generated, each air inlet joint 9 is connected to the blower 12 through a connecting pipe 11, the blower 12 is connected to the refrigeration fan 13, the refrigeration fan 13 can provide cooling airflow, and the blower 12 can accelerate the cooling airflow to the cavity formed between the upper mold 1 and the lower mold 3; an upper mold plate 14 is fixedly installed on the top surface of the upper mold 1, and supporting side plates 15 are fixedly installed on both sides of the bottom surface of the lower mold 3, and a lower mold plate 16 is fixedly installed on the bottom surface of the supporting side plate 15. An ejection through hole 17 is opened through the center of the lower mold plate 16, and a first linkage plate 18 is arranged above the lower mold plate 16. A second linkage plate 19 is fixedly installed on the top surface of the first linkage plate 18, and both sides of the first linkage plate 18 and the second linkage plate 19 are connected to the two sides. The supporting side plates 15 are slidably connected to the opposite sides, and the middle part of the top surface of the second linkage plate 19 is fixedly connected to the lower ends of the plurality of ejector rods 20. The upper ends of the plurality of ejector rods 20 slide through the second linkage plate 19, the lower mold 3 and the lower mold core 4 from bottom to top in sequence and are flush with the top surface of the lower mold core 4. A plurality of support springs 21 are arranged between the top surface of the second linkage plate 19 and the bottom surface of the lower mold 3. Specifically, limiting grooves 22 are provided on the top surface of the second linkage plate 19 and the bottom surface of the lower mold 3 at the positions of the two ends of the support springs 21. The two ends of the support springs 21 are arranged in the limiting grooves 22. After the injection mold is assembled, the support springs 21 are in a compressed state, and the first linkage plate 18 is in contact with the lower mold plate 16 under the elastic force of the support springs 21.In a specific implementation, the assembled injection mold is installed on the injection molding machine, and the lower mold plate 16 is fixedly installed on the moving part (hydraulic cylinder or screw) of the injection molding machine as a movable mold, and the ejector rod of the ejector part (hydraulic cylinder) of the injection molding machine passes through the ejector through hole 17 of the lower mold plate 16 and contacts the first linkage plate 18, and the upper mold plate 14 is fixedly installed on the injection molding part of the injection molding machine as a fixed mold, and the injection nozzle of the injection molding machine is aligned with the gate sleeve 24. ;
[0018] In the above design, by respectively setting matching annular bosses and annular grooves on the edges of the upper mold 1 and the lower mold 3, and the air inlet holes 8 set on the left and right sides of the annular bosses and the air outlet grooves 10 set on the front and rear sides thereof, after the plastic product is formed in the molding cavity 5 and cooled by the cooling system of the mold itself, the moving parts of the injection molding machine first pull the lower mold plate 16 of the injection mold for a certain distance, so that the annular groove 6 on the lower mold 3 and the annular boss 7 on the upper mold 1 move relative to each other, and the annular boss 7 and the annular groove 6 are not completely The air inlet 8 and the air outlet groove 10 on the annular boss 7 are separated and exposed from the annular groove 6. At this time, the blower 12 is started to convey the cooling airflow of the refrigeration fan 13 to the cavity formed between the upper mold 1 and the lower mold 3 through the connecting pipe 11, so that the cooling airflow is blown to the surface of the plastic product and blown out from the air outlet groove 10, thereby cooling the surface of the plastic product, making the plastic product quickly formed and easier to demould. In addition, the blowing and cooling process does not contact the outside world, thereby preventing impurities from being contaminated on the surface of the plastic product.
[0019] Working principle: During installation, the assembled injection mold is installed on the injection molding machine, and the lower template 16 is fixedly installed on the moving part (hydraulic cylinder or screw) of the injection molding machine as the movable mold, and on the ejector rod 2 of the ejector part (hydraulic cylinder) of the injection molding machine, and the injection nozzle of the injection molding machine is aligned with the gate sleeve 24; during operation, after the plastic product is molded in the molding cavity 5 and cooled by the cooling system of the mold itself, the moving part of the injection molding machine first pulls the lower template 16 of the injection mold for a certain distance, so that the annular groove 6 on the lower mold 3 and the annular boss 7 on the upper mold 1 move relative to each other, and the annular boss 7 is not completely separated from the annular groove 6, and the air inlet 8 on the annular boss 7 The air outlet groove 10 is separated from the annular groove 6 and exposed. At this time, the blower 12 is started to transport the cooling airflow of the refrigeration fan 13 through the connecting pipe 11 to the cavity formed between the upper mold 1 and the lower mold 3, so that the cooling airflow is blown to the surface of the plastic product and blown out from the air outlet groove 10, thereby cooling the surface of the plastic product, so that the plastic product can be quickly formed and easier to demold. Then the moving parts of the injection molding machine continue to pull the lower template 16 of the injection mold to separate the lower mold 3 from the upper mold 1, and then the ejection part of the injection molding machine pushes the first linkage plate 18 and then drives the second linkage plate 19 to push the ejector 20 to eject, and then the plastic product formed on the lower mold core 4 is ejected and demolded.
[0020] The above embodiments are only used to illustrate the technical solutions of the embodiments of the present application, rather than to limit them. Although the embodiments of the present application are described in detail with reference to the above embodiments, it should be understood by those skilled in the art that the technical solutions described in the above embodiments can still be modified, or some of the technical features can be replaced by equivalents, without departing from the spirit and scope defined by the claims of the present application.
Claims
1. An injection mold for facilitating cooling of plastic products, comprising an upper mold (1), an upper mold core (2), a lower mold (3) and a lower mold core (4), characterized in that: An upper mold core (2) is embedded in the middle of the bottom surface of the upper mold (1), and the bottom surface of the upper mold (1) is assembled in close contact with the top surface of the lower mold (3). A lower mold core (4) is embedded in the middle of the top surface of the lower mold (3). The lower mold core (4) is in close contact with the edge of the upper mold core (2) and a molding cavity (5) is formed in the middle of the two. An annular groove (6) is opened downward at the four edges of the top of the lower mold (3), and the annular groove (6) is connected to the outer peripheral side of the lower mold (3). An annular boss (7) is extended downward at the four edges of the bottom of the upper mold (1), and the annular boss (7) is flush with the outer peripheral side of the upper mold (1). The annular boss (7) and the annular groove (6) correspond to each other in the upper and lower parts and are adapted to each other. When the upper mold (1) and the lower mold (3) are tightly matched, the annular boss (7) and the annular groove (6) are tightly matched. The left and right sides of the annular boss (7) are penetrated with a plurality of air inlet holes (8) along the width direction thereof, and an air inlet connector (9) is fixedly installed at the outer end of each air inlet hole (8). The front and rear sides of the annular boss (7) are penetrated with air outlet grooves (10), and each of the air inlet connectors (9) is connected to a blower (12) through a connecting pipe (11), and the blower (12) is connected to a refrigeration fan (13).
2. The injection mold for facilitating cooling of plastic products according to claim 1, characterized in that: The length and width of the air outlet groove (10) are both smaller than the length and width of the annular groove (6).
3. The injection mold for facilitating cooling of plastic products according to claim 1, characterized in that: An upper mold plate (14) is fixedly mounted on the top surface of the upper mold (1), supporting side plates (15) are fixedly mounted on both sides of the bottom surface of the lower mold (3), a lower mold plate (16) is fixedly mounted on the bottom surface of the supporting side plates (15), an ejection through hole (17) is penetrated through the center of the lower mold plate (16), a first linkage plate (18) is arranged above the lower mold plate (16), in an initial state, the first linkage plate (18) is in contact with the lower mold plate (16), and the first linkage plate (18) is in contact with the lower mold plate (16). A second linkage plate (19) is fixedly mounted on the top surface of the movable plate (18); the middle portion of the top surface of the second linkage plate (19) is fixedly connected to the lower ends of a plurality of push rods (20); the upper ends of the plurality of push rods (20) slide sequentially from bottom to top through the second linkage plate (19), the lower mold (3) and the lower mold core (4) and are flush with the top surface of the lower mold core (4); and a plurality of supporting springs (21) are arranged between the top surface of the second linkage plate (19) and the bottom surface of the lower mold (3).
4. The injection mold for facilitating cooling of plastic products according to claim 3, characterized in that: Limiting grooves (22) are provided on the top surface of the second linkage plate (19) and the bottom surface of the lower mold (3) at the two ends of the supporting spring (21); the two ends of the supporting spring (21) are arranged in the limiting grooves (22), and the supporting spring (21) is in a compressed state.
5. The injection mold for facilitating cooling of plastic products according to claim 3, characterized in that: Both sides of the first linkage plate (18) and the second linkage plate (19) are slidably connected to the opposite sides of the supporting side plates (15) on both sides.
6. The injection mold for facilitating cooling of plastic products according to claim 3, characterized in that: The upper mold plate (14), the upper mold (1) and the upper mold core (2) are provided with a communicating injection channel (23); the injection channel (23) on the upper mold core (2) is a conical structure; a gate sleeve (24) is installed at the top of the upper mold plate (14) at the position of the injection channel (23).