Aluminum oxide continuous fiber weaving and preimpregnation integrated device
Through the integrated alumina continuous fiber braiding prepreg device controlled by electrostatic field and pressure during the braiding of alumina continuous fiber, the problems of uneven distribution of fiber tube resin and production complexity are solved, and more efficient fiber impregnation and Automated production processes reduce the risk of fiber damage.
Patent Information
- Application Number
- CN202323599423.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-27
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2033-12-27
AI Technical Summary
The braiding and prepregation processes of existing continuous alumina fibers are carried out separately, resulting in uneven distribution of resins, increasing production complexity and cost, and the fibers are susceptible to contamination and mechanical damage.
An integrated device for continuous fiber braiding of alumina is designed, including a braiding device, coating chamber and melting furnace. Through electrostatic field and pressure control, the resin powder is evenly distributed and impregnated during the fiber braiding process to ensure the fiber tubes. Evenly impregnate and reduce manual operation.
A uniform impregnation of fiber tubes is achieved, reducing production steps and costs, improving production efficiency, and reducing the risk of fiber damage.
Smart Images

Figure CN222100305U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to an alumina continuous fiber braiding prepreg integrated device, belonging to the technical field of alumina spinning equipment. Background Art
[0002] As one of the recognized new high-performance inorganic fibers, continuous Al2O3 fiber has excellent properties such as high strength and high modulus, high temperature insulation, ablation resistance, and corrosion resistance. Its maximum operating temperature is 1600℃, and the maximum long-term operating temperature is 1200℃. In addition, it has the advantages of low raw material cost and simple process. Continuous alumina fiber can be twisted and woven to make fiber ropes, fiber cloths, fiber sleeves and other fiber products, and can be further compounded into various metal-based, polymer-based and ceramic-based composite materials. Therefore, it has very important applications in the fields of civil composite materials, military industry, aerospace, etc.
[0003] At present, the alumina continuous fiber tube forming process mostly uses compression molding, winding molding, vacuum impregnation molding, and resin transfer molding. In these molding processes, fiber weaving and pre-impregnation are carried out as two independent steps. One method is to pre-impregnate the alumina continuous fiber first, and then use the pre-impregnated alumina continuous fiber to weave into a tube. This method will destroy the resin impregnated on the surface of the alumina continuous fiber during the weaving process, resulting in uneven distribution of the resin on the surface of the alumina continuous fiber after the alumina continuous fiber is woven into the tube; the other method is to weave first to obtain an alumina continuous fiber tube, and then impregnate the woven continuous fiber tube as a whole. After weaving, the resin is difficult to enter the space between the fibers to complete the impregnation, which will make the alumina continuous fiber insufficiently impregnated.
[0004] In addition, prepreg not only requires additional production steps, increasing the complexity and cost of manufacturing, but also requires a higher level of production process control to ensure the consistency of resin impregnation and fiber distribution. When fiber weaving and prepreg are carried out separately, there may be a period of time between the two steps. During this period of time, the fibers are exposed to the external environment and are susceptible to contamination, physical damage or chemical changes, resulting in damage to the integrity of the fiber structure. In addition, human factors may increase the risk of damage to fiber materials. For example, during transportation, storage or other processing, due to improper operation or environmental conditions, the fibers may be squeezed, stretched or scratched, resulting in damage or destruction. Therefore, alumina continuous fiber tubes are more susceptible to mechanical damage during the preparation process. Utility Model Content
[0005] In order to solve one or more of the above-mentioned problems, the utility model provides an alumina continuous fiber weaving prepreg integrated device, and the technical solution is as follows.
[0006] The utility model provides an integrated device for weaving and prepreg of alumina continuous fibers, characterized in that the integrated device for weaving and prepreg of alumina continuous fibers comprises a weaving device, a coating chamber, a melting furnace and a winder; the weaving device is used for weaving alumina fiber tubes; resin powder is evenly distributed in the coating chamber and is used for impregnating the alumina fiber tubes in three stages: before weaving, during weaving and after weaving; the melting furnace fully melts the resin powder coated on the formed alumina fiber tubes; the winder is used for winding and storing the alumina fiber tubes.
[0007] In one embodiment, the braiding device includes a guide ring for conveying alumina continuous fibers.
[0008] In one embodiment, the coating chamber includes an electrostatic generator, a porous plate, a booster chamber, a dry air inlet, a de-vacuum pump and a braided tube; wherein the booster chamber is arranged at the bottom of the coating chamber, and is used to control the internal pressure to ensure that the resin powder is evenly and stably distributed in the coating chamber; the dry air inlet is located on the side of the bottom of the coating chamber, connected to the booster chamber, and is used for air intake, and the resin powder enters the coating chamber through the dry air inlet; the porous plate is located above the booster chamber, and is used to ensure that the resin powder enters the coating chamber through the holes in a uniform manner; the electrostatic generator is located above the booster chamber in the coating chamber, and is used to generate an electrostatic field; the de-vacuum pump is arranged at the top of the coating chamber, and is used to evacuate the coating chamber, so that the resin powder enters the coating chamber under the action of atmospheric pressure, and the resin powder in the coating chamber floats in the coating chamber under the action of the electrostatic field, and is used to impregnate the alumina continuous fiber tube before, during and after weaving.
[0009] In one embodiment, the coating chamber further comprises a high voltage generator, which is located outside the coating chamber and electrically connected to the electrostatic generator inside the coating chamber to provide the required voltage for the electrostatic generator to generate an electrostatic field.
[0010] In one embodiment, the braiding device is used to braid alumina continuous fibers onto a braided tube to form an alumina fiber braided tube.
[0011] Advantages of the utility model:
[0012] (1) The utility model provides an integrated alumina continuous fiber weaving pre-impregnation device that can impregnate the alumina continuous fibers before weaving, the alumina continuous fibers during weaving, and the fiber tubes after weaving, so that the fiber tubes after weaving are impregnated more evenly, ensuring the consistency of resin impregnation and fiber distribution.
[0013] (2) Compared with the traditional preparation method of alumina continuous fiber weaving and pre-impregnation, the preparation method of the utility model can realize an automated process, reduce manual operation, and minimize the variability caused by manual operation, which helps to improve production efficiency.
[0014] (3) The utility model provides an integrated alumina continuous fiber braided prepreg device that can accurately control the amount of resin used by adjusting the electric field strength and other parameters, thereby reducing the waste of raw materials and improving the effectiveness. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 It is a schematic structural diagram of the alumina continuous fiber weaving prepreg integrated device of the present invention;
[0016] Among them, 1. weaving device; 2. guide ring; 3. alumina continuous fiber; 4. coating chamber; 5. melting furnace; 6. winder; 7. resin powder; 8. electrostatic generator; 9. porous plate; 10. pressurization chamber; 11. dry air inlet; 12. high voltage generator; 13. de-vacuum pump; 14. braided tube. DETAILED DESCRIPTION
[0017] The following is a specific description of the utility model.
[0018] Example 1
[0019] like Figure 1 As shown, the present embodiment provides an integrated device for weaving and prepregging alumina continuous fibers, comprising a weaving device 1, a coating chamber 4, a melting furnace 5 and a winder 6; the weaving device 1 is used for weaving alumina fiber tubes, and during the weaving process, the weaving device 1 moves regularly under the drive of an external power, so that the alumina continuous fibers are wound around a weaving tube 14 located in the coating chamber to form an alumina fiber tube; the coating chamber 4 is evenly distributed with resin powder 7, and the entire process from the fiber entering the coating chamber 4 to being woven into a tube is impregnated with the resin powder 7, so that the fiber tube can be impregnated in three stages of weaving, before weaving, during weaving and after weaving; the melting furnace 5 fully melts the resin coated on the formed alumina fiber tube; the winder 6 receives the fabric winding after impregnation.
[0020] The braiding device 1 includes a guide ring 2, which is used to transport alumina continuous fibers 3; the coating chamber 4 includes an electrostatic generator 8, a porous plate 9, a pressurizing chamber 10, a dry air inlet 11, a high-voltage generator 12, a de-vacuum pump 13 and a braiding tube 14; the pressurizing chamber 10 is arranged at the bottom of the coating chamber 4 to control the internal pressure and ensure that the resin powder 7 is evenly and stably distributed in the coating chamber 4 to wet the fibers; the dry air inlet 11 is located on the side of the bottom of the coating chamber and is connected to the pressurizing chamber 10 for air intake; the resin powder 7 enters the prepreg chamber through the dry air inlet 11; the porous plate 9 is located above the pressurizing chamber 10 to prevent large resin powder particles from entering the coating chamber 4 and ensure that the resin powder 7 enters the coating chamber 4 through the holes in a uniform manner and is not easy to accumulate; the electrostatic generator 8 is located above the pressurizing chamber 10 in the coating chamber 4 and is connected to the high-voltage generator 12 outside the coating chamber 4 to generate an electrostatic field; the de-vacuum pump 13 is arranged at the top of the coating chamber 4 to control the pressure of the coating chamber 4. 4 is vacuumed, so that the resin powder can enter the coating chamber 4 under the action of atmospheric pressure, and the resin powder 7 in the coating chamber 4 floats in the coating chamber 4 under the action of the electrostatic field, which is used to simultaneously impregnate the three stages of the alumina continuous fiber tube weaving process; the weaving device 1 weaves the alumina continuous fiber 3 on the braiding tube 14 to form an alumina fiber braided tube, and the alumina continuous fiber 3 enters the coating chamber 4 and is impregnated with the resin powder 7. While being weaved on the braiding tube 14, it is also impregnated with the resin powder 7. After being woven into a tube, the fiber tube is also impregnated with the resin powder 7, so that the fiber itself is impregnated with a part of the resin powder 7, and each position during the weaving process is also impregnated with a part of the resin powder 7. After being woven into a tube, the surface of the tube is impregnated with a part of the resin powder 7, so as to ensure that the final continuous fiber tube is evenly impregnated with the resin powder 7 to the greatest extent, and enters the melting furnace 5 to fully melt the resin. The fabric after impregnation is wound onto the winding machine 6.
[0021] The working principle of this embodiment is as follows: start the vacuum pump 13 to allow the resin powder 7 to enter the boost chamber 10 from the dry air inlet 11, and then enter the coating chamber 4 from the holes in the porous plate 9. When the coating chamber 4 is filled with the resin powder 7, close the vacuum pump 13, and the pressure in the coating chamber 4 reaches equilibrium. Under the action of static electricity, the suspended resin powder 7 is filled. Under the action of the weaving device 1 and the guide ring 2, the alumina continuous fiber 3 enters the coating chamber 4 and is wound on the braided tube 14 to form an alumina fiber tube. While weaving, it is impregnated with the resin powder 7 to complete the weaving and pre-impregnation. The impregnated fabric enters the melting furnace 5 to fully melt the resin, and then is wound and stored by the winder 6 to finally obtain an alumina fiber braided tube.
[0022] Although the present invention has been disclosed as above in terms of preferred embodiments, it is not intended to limit the present invention. Anyone familiar with the technology may make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the scope of protection of the present invention should be based on the definition of the claims.
Claims
1. An alumina continuous fiber braided prepreg integrated device, characterized in that: The alumina continuous fiber braiding prepreg integrated device comprises a braiding device, a coating chamber, a melting furnace and a winder; the braiding device is used to braid the alumina fiber tube; the coating chamber is evenly distributed with resin powder, which is used to impregnate the alumina fiber tube before, during and after braiding; the melting furnace fully melts the resin powder coated on the formed alumina fiber tube; the winder is used to wind and store the alumina fiber tube; The coating chamber comprises an electrostatic generator, a porous plate, a pressurizing chamber, a dry air inlet, a vacuum pump and a braided tube; wherein the pressurizing chamber is arranged at the bottom of the coating chamber, and is used to control the internal pressure to ensure that the resin powder is evenly and stably distributed in the coating chamber; the dry air inlet is located on the side of the bottom of the coating chamber, and is connected to the pressurizing chamber for air intake, and the resin powder enters the coating chamber through the dry air inlet; the porous plate is located above the pressurizing chamber, and is used to ensure that the resin powder enters the coating chamber through the holes in a uniform manner; the electrostatic generator is located above the pressurizing chamber in the coating chamber, and is used to generate an electrostatic field; the vacuum pump is arranged at the top of the coating chamber, and is used to evacuate the coating chamber, so that the resin powder enters the coating chamber under the action of atmospheric pressure, and the resin powder in the coating chamber floats in the coating chamber under the action of the electrostatic field, and is used to impregnate the alumina continuous fiber tube before, during and after braiding; The coating chamber also includes a high voltage generator, which is located outside the coating chamber and is electrically connected to the electrostatic generator inside the coating chamber to provide the required voltage for the electrostatic generator to generate an electrostatic field.
2. The alumina continuous fiber braided prepreg integrated device according to claim 1, characterized in that: The braiding device comprises a guide ring, which is used for conveying alumina continuous fibers.