Corrosion-resistant die-casting aluminum alloy ingot
By designing smooth rounded corners and upper and lower grooves with matching widths on the aluminum alloy ingot, the fracture problem caused by sharp junction between the aluminum ingot and the steel belt is solved, and the stability and storage safety of the aluminum ingot bundle are improved.
Patent Information
- Application Number
- CN202323655595.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-31
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2033-12-31
AI Technical Summary
After the existing corrosion-resistant die-cast aluminum alloy ingots are packaged, the junction of the aluminum alloy ingots and the steel belt is sharp, which can easily lead to the steel belt breakage, causing the aluminum ingots to be bundled and affecting the storage stability.
Designed to have upper grooves on both sides of the upper end of the aluminum alloy ingot body, and lower grooves on both sides of the lower end. The junction of the groove and the aluminum alloy ingot are smooth rounded corners, and the width of the groove matches the steel strip to increase stability.
Through the design of smooth rounded corners and matching width, the steel strip is avoided, the stability of the aluminum ingot bundle is enhanced, the steel strip is prevented from falling off under impact loads, and the aluminum ingot bundle is avoided.
Smart Images

Figure CN222103374U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of aluminum alloy ingots, in particular to a corrosion-resistant die-casting aluminum alloy ingot. Background Art
[0002] After the existing corrosion-resistant die-cast aluminum alloy ingots are packaged, the intersection between the aluminum alloy ingots and the packaging steel belt is relatively sharp. Therefore, when the aluminum ingot bundle is subjected to an impact load, the steel belt is easily broken, causing the aluminum ingot bundle to fall apart, affecting the storage of the aluminum alloy ingots. Summary of the invention
[0003] In view of the above problems, the utility model provides a corrosion-resistant die-casting aluminum alloy ingot.
[0004] In order to achieve the above purpose, the utility model adopts the following technical solutions:
[0005] A corrosion-resistant die-cast aluminum alloy ingot, comprising an aluminum alloy ingot body, characterized in that: upper grooves are formed on both sides of the upper end of the aluminum alloy ingot body, and lower grooves are formed on both sides of the lower end of the aluminum alloy ingot body;
[0006] The lower groove and the upper groove are arranged in the same vertical plane, the junction between the upper groove and the aluminum alloy ingot body is a smooth rounded corner, and the junction between the lower groove and the aluminum alloy ingot body is a smooth rounded corner.
[0007] Preferably, the upper grooves on both sides are connected through an upper connecting groove, and the lower grooves on both sides are connected through a lower connecting groove.
[0008] Preferably, the width of the grooves in the present invention matches the width of the packing steel strap.
[0009] Preferably, the rounded corners of the surface of the utility model are smoothly transitioned, and the surface of the utility model has no sharp edges.
[0010] Compared with the prior art, the utility model has the following beneficial effects: when the utility model is used, the packing steel belt is engaged with the upper groove and the lower groove, and the intersection of the grooves is smooth, which avoids the packing steel belt from breaking due to the sharp edges of the aluminum alloy ingot, causing the aluminum ingot bundle to fall apart. The upper and lower connecting grooves are engaged with the packing steel belt, and the width of the groove matches the packing steel belt, which increases the stability of the aluminum ingot bundle when packing, and avoids the packing steel belt from falling off when the aluminum ingot bundle is subjected to impact load, causing the aluminum ingot bundle to fall apart. BRIEF DESCRIPTION OF THE DRAWINGS
[0011] Figure 1 It is a side view of a corrosion-resistant die-casting aluminum alloy ingot of the utility model.
[0012] Figure 2 It is a cross-sectional view of a corrosion-resistant die-cast aluminum alloy ingot of the utility model. Implementation
[0013] In order to provide a further understanding of the purpose, structure, features, and functions of the present invention, the present invention is described in detail below with reference to the embodiments.
[0014] Please refer to Figure 1 and Figure 2 A corrosion-resistant die-cast aluminum alloy ingot according to an embodiment of the utility model comprises an aluminum alloy ingot body 100, characterized in that: upper grooves 101 are provided on both sides of the upper end of the aluminum alloy ingot body 100, and lower grooves 102 are provided on both sides of the lower end of the aluminum alloy ingot body 100;
[0015] The lower groove 102 and the upper groove 101 are arranged in the same vertical plane. The junction between the upper groove 101 and the aluminum alloy ingot body 100 is a smooth rounded corner. The junction between the lower groove 102 and the aluminum alloy ingot body 100 is a smooth rounded corner.
[0016] When the utility model is in use, the packing steel belt is engaged with the upper groove 101 and the lower groove 102, and the junction of the grooves is smooth, which avoids the packing steel belt from breaking due to the sharp edges of the aluminum alloy ingot, resulting in the aluminum ingot being loosened.
[0017] Preferably, the upper grooves 101 on both sides are connected through the upper connecting grooves 103, and the lower grooves 102 on both sides are connected through the lower connecting grooves 104. This facilitates the engagement of the aluminum alloy ingots at the top and bottom of the aluminum ingot bundle with the packing steel belt, increases the stability of the aluminum ingot bundle during packing, and prevents the packing steel belt from falling off when the aluminum ingot bundle is subjected to an impact load, causing the aluminum ingot bundle to fall apart.
[0018] Preferably, the width of the grooves in the present invention matches the width of the packing steel belt, so as to facilitate the engagement of the aluminum alloy ingots with the packing steel belt, increase the stability of the aluminum ingot bundles, and prevent the packing steel belts from falling off when the aluminum ingot bundles are subjected to impact loads, causing the aluminum ingot bundles to fall apart.
[0019] Preferably, the rounded corners of the surface of the utility model are smoothly transitioned, and the surface of the utility model has no sharp edges and corners, so as to avoid the sharp edges and corners cutting the packing steel belt and causing the aluminum ingot bundle to fall apart.
[0020] The present invention has been described by the above-mentioned relevant embodiments, however, the above-mentioned embodiments are only examples for implementing the present invention. It must be pointed out that the disclosed embodiments do not limit the scope of the present invention. On the contrary, any changes and modifications made without departing from the spirit and scope of the present invention are within the scope of patent protection of the present invention.
Claims
1. A corrosion-resistant die-casting aluminum alloy ingot, characterized in that: It comprises an aluminum alloy ingot body (100), wherein upper grooves (101) are provided on both sides of the upper end of the aluminum alloy ingot body (100), and lower grooves (102) are provided on both sides of the lower end of the aluminum alloy ingot body (100); The lower groove (102) and the upper groove (101) are arranged in the same vertical plane, the junction between the upper groove (101) and the aluminum alloy ingot body (100) is a smooth rounded corner, and the junction between the lower groove (102) and the aluminum alloy ingot body (100) is a smooth rounded corner.
2. The corrosion-resistant die-casting aluminum alloy ingot according to claim 1, characterized in that: The upper grooves (101) on both sides are connected via an upper connecting groove (103), and the lower grooves (102) on both sides are connected via a lower connecting groove (104).
3. The corrosion-resistant die-casting aluminum alloy ingot according to claim 1, characterized in that: The widths of the upper groove (101), the lower groove (102), the upper connecting groove (103), and the lower connecting groove (104) all match the width of the packing steel belt.
4. The corrosion-resistant die-casting aluminum alloy ingot according to claim 1, characterized in that: The rounded corners of the surfaces of the aluminum alloy ingot body (100), the upper groove (101), and the lower groove (102) are all smoothly transitioned, and the surfaces of the aluminum alloy ingot body (100), the upper groove (101), and the lower groove (102) have no sharp edges or corners.