Connection structure for lower plastic cement and mylar film of battery cell and battery cell
By designing the middle and side protrusions on the plastic plate under the battery core, and using the semi-circular arc surface to achieve hot melt fixation, the problem of interference between the plastic and the Mail film in the single-coil structure is solved, and the electricity is improved Core production efficiency and safety performance.
Patent Information
- Application Number
- CN202420588090.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-25
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2034-03-25
AI Technical Summary
In the battery cell with a single-core structure, the hot melt connection between the lower plastic and the Mail film is prone to interference, resulting in poor safety and difficulty in stabilizing and fixing, and there is a risk of short circuit.
A connection structure between plastic and mala film of the battery cell is designed. By setting the middle protrusion and side protrusion on the lower plastic plate, and a semi-circular arc surface is designed on the side protrusion, using the semi-circular arc surface The hot melt plane realizes stable hot melt fixation between the Maila film and the lower plastic, ensuring that the Maila film can closely fit the outside of the core, and adapts flush with the core by optimizing the outer contour of the side wall.
It improves the production efficiency of small-capacity battery cells, while ensuring the safety performance of the battery cells, avoiding the risk of short circuits, and ensuring the stable hot melt connection between the plastic and the Mail film.
Smart Images

Figure CN222106801U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the field of new energy batteries, and in particular to a connection structure of plastic and Mylar film under a battery cell and a battery cell. Background Art
[0002] The battery cell of a power battery generally includes a metal shell, a winding core arranged in the metal shell, and a cover assembly arranged on the top of the metal shell and electrically connected to the winding core. Positive and negative pole ears are arranged on the winding core. The cover assembly includes a metal cover body, a positive pole column, a negative pole column, an injection hole, an explosion-proof valve and other structures arranged on the metal cover body. In order to prevent the metal cover body from directly contacting and conducting the winding core, the cover assembly also includes a lower plastic part arranged between the metal cover body and the winding core, and the lower plastic part serves the purpose of insulation between the winding core and the metal cover body. After the winding core and the metal cover are connected in a current-carrying manner, a layer of Mylar film will be coated on the outside of the winding core to protect the winding core from being scratched when entering the metal shell.
[0003] In the related technology, due to the limitations of existing core winding technology and ultrasonic welding technology, in order to ensure the quality of core winding and the welding quality of the tabs and connecting pieces, the number of lithium battery cores currently on the market is basically greater than or equal to 2. This structure will also reduce the R angle on both sides of the overall core, making it easier to wrap with Mylar film and to heat-smash with the lower plastic.
[0004] For some smaller-capacity batteries, only one core is needed, which can reduce the number of cores, reduce the workload of ultrasonic welding of connecting pieces, and remove the core bonding and gluing process, thus improving the overall efficiency of the middle stage of battery production. However, due to the single-core structure, the Mylar film will interfere with the lower plastic after wrapping the core, and it is difficult for the two sides to be stably fixed with the lower plastic by hot melting, which may lead to the risk of short circuit. Utility Model Content
[0005] The embodiment of the utility model provides a connection structure between the lower plastic and the Mylar film of a battery cell and a battery cell, which can solve the technical problem in the prior art that the hot-melt connection between the lower plastic and the Mylar film inside the battery cell with a single-roll core structure is prone to interference and poor safety. The technical solution is as follows:
[0006] In a first aspect, an embodiment of the utility model provides a connection structure between a lower plastic plate and a Mylar film of a battery cell, comprising: a lower plastic plate and a Mylar film,
[0007] A middle protrusion and two side protrusions symmetrically arranged on both sides of the middle protrusion are protruding from one side surface of the lower plastic plate. The top surfaces of the side protrusions and the middle protrusion are flush. A semicircular arc surface for adapting to the winding core is arranged on the side wall of the side protrusion away from the middle protrusion. A hot-melt plane is arranged at the top of the semicircular arc surface. The Mylar film is wound around and attached to the side walls of the two side protrusions and the middle protrusion, and the Mylar film is fixed by hot-melt at the contact point with the hot-melt plane.
[0008] Optionally, the edge of the lower plastic plate has a limiting ear, and the orthographic projection of the semicircular arc surface on the lower plastic plate is located inside the limiting ear.
[0009] Optionally, hot melt ear plates are provided on both sides of the side protrusion, and the two hot melt ear plates are flush with the two side edges of the lower plastic plate and are symmetrically arranged relative to the hot melt plane.
[0010] Optionally, the two opposite side walls of the central protrusion are flush with the outer side walls of the hot melt ear plate.
[0011] Optionally, weight-reducing holes are provided on the side protrusions.
[0012] Optionally, a vent hole communicating with the other side surface of the lower plastic plate is provided on the top surface of the middle protrusion.
[0013] In the second aspect, an embodiment of the utility model further provides a battery cell, comprising the plastic and Mylar film connection structure at the bottom of the battery cell described in the first aspect, and also comprising a winding core, the top surface of the winding core abuts against the top surfaces of the side protrusions and the middle protrusions, and the side walls at both ends of the winding core are flush with the semicircular arc surface.
[0014] Optionally, a cover plate is further included, and a side surface of the lower plastic plate away from the middle protrusion and the side protrusion is fixedly connected to the cover plate.
[0015] The beneficial effects brought by the technical solution provided by the embodiment of the utility model include at least:
[0016] The connection structure between the lower plastic and the Mylar film of the battery cell provided by the embodiment of the utility model is adopted, by optimizing the outer contour of the side walls of the side protrusions on both sides of the middle protrusion on the lower plastic plate, and making a flush fit with the winding core through the semi-circular arc surface design. When winding and wrapping the Mylar film, it is ensured that it can tightly fit the middle protrusion, the side protrusions and the outer side of the lower winding core at the same time, and at the same time, the hot melt plane in the middle section of the semi-circular arc surface is used to achieve stable hot-melt fixation of the lower plastic plate and the Mylar film, so that the small-capacity battery cell can improve the production efficiency in the middle stage of production while also ensuring the overall safety performance of the battery cell. It can solve the technical problem in the prior art that the hot-melt connection between the lower plastic and the Mylar film inside the battery cell with a single winding core structure is prone to interference, resulting in poor safety. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.
[0018] Figure 1 This is a schematic diagram of the structure of a top cover and a connecting piece structure cooperating with a cover plate provided by an embodiment of the utility model;
[0019] Figure 2 This is a schematic diagram of the structure of the cover plate, the lower plastic plate and the winding core provided by the embodiment of the utility model;
[0020] Figure 3 It is a partial structural schematic diagram of the lower plastic plate provided in an embodiment of the utility model.
[0021] In the figure: 1-lower plastic plate; 2-Mylar film; 3-winding core; 4-cover plate; 11-middle protrusion; 12-side protrusion; 13-limiting ear; 14-hot-melt ear plate; 41-explosion-proof valve; 111-vent; 121-semicircular arc surface; 122-hot-melt plane; 123-weight reduction hole. DETAILED DESCRIPTION
[0022] In order to make the purpose, technical solution and advantages of the present invention more clear, the implementation mode of the present invention will be further described in detail below with reference to the accompanying drawings.
[0023] In the related technology, due to the limitations of existing core winding technology and ultrasonic welding technology, in order to ensure the quality of core winding and the welding quality of the tabs and connecting pieces, the number of lithium battery cores currently on the market is basically greater than or equal to 2. This structure will also reduce the R angle on both sides of the overall core, making it easier to wrap with Mylar film and to heat-smash with the lower plastic.
[0024] For some smaller-capacity batteries, only one core is needed, which can reduce the number of cores, reduce the workload of ultrasonic welding of connecting pieces, and remove the core bonding and gluing process, thus improving the overall efficiency of the middle stage of battery production. However, due to the single-core structure, the Mylar film will interfere with the lower plastic after wrapping the core, and it is difficult for the two sides to be stably fixed with the lower plastic by hot melting, which may lead to the risk of short circuit.
[0025] Figure 1 This is a schematic diagram of the structure of a top cover and a connecting piece structure cooperating with a cover plate provided by an embodiment of the utility model; Figure 2 This is a schematic diagram of the structure of the cover plate, the lower plastic plate and the winding core provided by the embodiment of the utility model; Figure 3 Schematic diagram of the partial structure of the lower plastic plate provided by the embodiment of the utility model. Figures 1 to 3 The illustrated connection structure between the lower plastic of a battery cell and a Mylar film comprises a lower plastic plate 1 and a Mylar film 2 .
[0026] Among them, a central protrusion 11 and two side protrusions 12 symmetrically arranged on both sides of the central protrusion 11 are protrudingly provided on one side of the lower plastic plate 1, and the top surfaces of the side protrusions 12 and the central protrusion 11 are flush. A semicircular arc surface 121 for adapting to the winding core 3 is provided on the side wall of the side protrusion 12 away from the central protrusion 11, and a hot melt plane 122 is provided at the top of the semicircular arc surface 121. The Mylar film 2 is wound and attached to the side walls of the two side protrusions 12 and the central protrusion 11, and the Mylar film 2 is fixed by hot melt at the contact point with the hot melt plane 122.
[0027] In the embodiment of the present utility model, reference Figure 3, viewed from one side of the lower plastic plate 1, that is, the bottom surface, one side of the lower plastic plate 1 is protruding with a middle protrusion 11 and a side protrusion 12, which are used to abut against the core 3, while the other side is used to connect with the cover plate 4 of the battery cell, so as to achieve insulation isolation between the core 3 and the metal cover plate 4. The top of the core 3 abuts against the top surface of the middle protrusion 11 and the two side protrusions 12, and two gap spaces are isolated between the middle protrusion 11 and the two side protrusions 12, and between the top surface of the core 3, which are used to set the flow sheet to weld the upper pole of the cover plate 4 and the positive and negative ears extending from the core 3. After completing the flow connection between the core 3 and the upper pole of the cover plate 4, the Mylar film 2 can be wound around the side walls of the side protrusions 12 and the middle protrusion 11. The semi-circular arc surface 121 on the side protrusion 12 is adapted to the side wall contours of the two ends of the core 3, and is in a flush state after the core 3 is installed in place. A hot melt plane 122 is provided at the top of the arc of the semi-circular arc surface 121, and the hot melt plane 122 is perpendicular to the length direction of the cover plate 4. The existence of the hot melt plane 122 makes the semi-circular arc surface 121 form a three-section structure of "arc + plane + arc", and the arc sections on both sides of the hot melt plane 122 are arranged symmetrically. In the process of winding and wrapping the Mylar film 2, it fits with the outer wall contours of the side protrusion 12 and the middle protrusion 11 to achieve a tight fit covering of the lower core 3. After the winding is completed, the flat hot melt plane 122 is used as a hot melt point, and the Mylar film 2 and the lower plastic plate 1 are integrally hot-melted and fixed at this position.
[0028] The connection structure between the lower plastic and the Mylar film of the battery cell provided by the embodiment of the utility model is adopted, by optimizing the outer contour of the side wall of the side protrusions 12 on both sides of the middle protrusion 11 on the lower plastic plate 1, and by designing the semi-circular arc surface 121 to be flush with the winding core 3. When the Mylar film 2 is wound and coated, it is ensured that it can simultaneously and tightly fit the middle protrusion 11, the side protrusion 12 and the outer side of the lower winding core 3, and at the same time, the hot melt plane 122 in the middle section of the semi-circular arc surface 121 is used to achieve stable hot-melt fixation of the lower plastic plate 1 and the Mylar film 2, so that the small-capacity battery cell can improve the production efficiency in the middle stage of production while also ensuring the safety performance of the battery cell as a whole. It can solve the technical problem in the prior art that the hot-melt connection between the lower plastic and the Mylar film inside the battery cell with a single winding core structure is prone to interference, resulting in poor safety.
[0029] Exemplarily, in the embodiment of the utility model, the lower plastic plate 1 corresponds to the insulation isolation between the cover plate of the square shell battery cell and the lower winding core structure, and the overall outline of the lower plastic plate 1 is rectangular.
[0030] Optionally, the edge of the lower plastic plate 1 has a limiting ear 13, and the orthographic projection of the semicircular surface 121 on the lower plastic plate 1 is located inside the limiting ear 13. For example, in the embodiment of the utility model, the overall contour of the side of the lower plastic plate 1 is larger than the outer contour of the side protrusion 12, and the two ends of the lower plastic plate 1 in the length direction are relative to the semicircular surface 121 on the side protrusion 12, and the limiting ear 13 structure is formed outside the arc segment on both sides of the hot melt plane 122. After the Mylar film 2 is wound and coated, it can limit the position of the Mylar film 2 in the vertical direction through the limiting ear 13 structure to ensure the accuracy of the winding position, avoid shaking, improve processing accuracy, and further reduce the risk of short circuit of the core 3.
[0031] Optionally, hot melt ear plates 14 are provided on both sides of the side protrusion 12, and the two hot melt ear plates 14 are flush with the two side edges of the lower plastic plate 1 and are symmetrically arranged relative to the hot melt plane 122. For example, in the embodiment of the utility model, by extending two hot melt ear plates 14 along the outer contour of the side protrusion 12 to the middle protrusion 11, after the Mylar film 2 is rolled and covered, the contact points between the two hot melt ear plates 14 and the Mylar film 2 can be used as additional hot melt fixing points, so as to achieve multi-point hot melt fixing of the Mylar film 2 and the side protrusion 12, and improve the stability of hot melt fixing.
[0032] Optionally, the two opposite side walls of the middle protrusion 11 are flush with the outer side walls of the hot melt ear plate 14. For example, in the embodiment of the utility model, on the basis of hot-melt fixing of the side protrusions 12 and the Mylar film 2, by adapting the two side surfaces of the middle protrusion 11 in the length direction of the lower plastic plate 1, the Mylar film 2 can also fit with the two opposite side surfaces of the middle protrusion 11 after winding and covering, and the contact position can be further used as an additional hot-melt fixing point to perform hot-melt fixing of the Mylar film 2 and the middle protrusion 11, further improving the hot-melt fixing stability of the Mylar film 2.
[0033] Optionally, a weight-reducing hole 123 is provided on the side protrusion 12. For example, in the embodiment of the utility model, on the basis of ensuring insulation isolation, by opening a plurality of weight-reducing holes on the side protrusion 12, the weight of the connection structure and the entire cell cover can be reduced, thereby improving practicality.
[0034] Optionally, a vent hole 111 is provided on the top surface of the middle protrusion 11 and is connected to the other side of the lower plastic plate 1. For example, in the embodiment of the utility model, the covering position of the middle protrusion 11 corresponds to the installation position of the explosion-proof valve 41 on the cover plate 4. By providing a plurality of vent holes 111 connected to both sides, it can play a role in exhausting in the event of a thermal runaway accident, and at the same time, it can also filter the bursting disc of the explosion-proof valve 41 when the explosion-proof valve 41 explodes to prevent it from falling into the winding core 3 structure on the bottom side of the lower plastic plate 1.
[0035] The utility model also provides a battery cell, including: Figures 1 to 3 The illustrated structure for connecting the lower plastic of the battery cell with the Mylar film also includes a winding core 3, the top surface of the winding core 3 abuts against the top surfaces of the side protrusions 12 and the middle protrusions 11, and the side walls of the two ends of the winding core 3 are flush with the semicircular arc surface 121. The battery cell is prepared by using the structure for connecting the lower plastic of the battery cell with the Mylar film provided by the embodiment of the utility model, which optimizes the outer contour of the side walls of the side protrusions 12 located on both sides of the middle protrusion 11 on the lower plastic plate 1, and is designed to be flush with the winding core 3 by means of the semicircular arc surface 121. When the Mylar film 2 is wound and coated, it is ensured that it can simultaneously closely fit the middle protrusion 11, the side protrusions 12 and the outer side of the lower winding core 3, and at the same time, the hot melt plane 122 in the middle section of the semicircular arc surface 121 is used to achieve stable hot melt fixation of the lower plastic plate 1 and the Mylar film 2, so that the small-capacity battery cell improves the production efficiency in the middle section of production while also ensuring the overall safety performance of the battery cell. The present invention can solve the technical problem in the prior art that the hot-melt connection between the lower plastic and the Mylar film inside the battery cell with a single-wound core structure is prone to interference, resulting in poor safety.
[0036] Optionally, a cover plate 4 is further included, and a side of the lower plastic plate 1 away from the middle protrusion 11 and the side protrusion 12 is fixedly connected to the cover plate 4. For example, in the embodiment of the utility model, the lower plastic plate 1 is arranged as a whole separately from the cover plate 4, and can be prepared separately and then combined, which has high preparation flexibility and further improves practicality.
[0037] Unless otherwise defined, the technical terms or scientific terms used herein shall have the usual meanings understood by persons with ordinary skills in the field to which the utility model belongs. The words "first", "second" and similar words used in the specification and claims of the utility model patent application do not indicate any order, quantity or importance, but are only used to distinguish different components. Similarly, words such as "one" or "one" do not indicate a quantity limitation, but indicate the existence of at least one. Words such as "include" or "comprise" mean that the elements or objects appearing before "include" or "comprise" include the elements or objects listed after "include" or "comprise" and their equivalents, and do not exclude other elements or objects. Words such as "connect" or "connected" are not limited to physical or mechanical connections, but may include electrical connections, whether direct or indirect. "Up", "down", "left", "right" and the like are only used to indicate relative positional relationships. When the absolute position of the described object changes, the relative positional relationship may also change accordingly.
[0038] The above description is only an optional embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention shall be included in the protection scope of the present invention.
Claims
1. A connection structure between plastic and Mylar film under a battery cell, characterized in that: include: The lower plastic sheet (1) and the Mylar film (2) A central protrusion (11) and two side protrusions (12) symmetrically arranged on both sides of the central protrusion (11) are protrudingly provided on one side surface of the lower plastic plate (1), the top surfaces of the side protrusions (12) and the central protrusion (11) are flush, a semicircular arc surface (121) for matching with the winding core (3) is provided on the side wall of the side protrusion (12) away from the central protrusion (11), a hot melt plane (122) is provided at the top of the arc of the semicircular arc surface (121), the Mylar film (2) is wound and adhered to the side walls of the two side protrusions (12) and the central protrusion (11), and the Mylar film (2) is fixed by hot melt at the contact point with the hot melt plane (122).
2. A connection structure between plastic and Mylar film under a battery cell according to claim 1, characterized in that: The edge of the lower plastic plate (1) is provided with a limiting ear (13), and the orthographic projection of the semicircular arc surface (121) on the lower plastic plate (1) is located inside the limiting ear (13).
3. The connection structure of plastic and Mylar film under the battery cell according to claim 1, characterized in that: Hot melt ear plates (14) are provided on both sides of the side protrusion (12), and the two hot melt ear plates (14) are flush with the two side edges of the lower plastic plate (1) and are symmetrically arranged relative to the hot melt plane (122).
4. The connection structure of plastic and Mylar film under the battery cell according to claim 3, characterized in that: The opposite side walls of the middle protrusion (11) are flush with the outer side walls of the hot melt ear plate (14).
5. The connection structure of plastic and Mylar film under the battery cell according to claim 1, characterized in that: The side protrusion (12) is provided with a weight-reducing hole (123).
6. The connection structure of plastic and Mylar film under the battery cell according to claim 1, characterized in that: A vent hole (111) is provided on the top surface of the middle protrusion (11) and is communicated with the other side surface of the lower plastic plate (1).
7. A battery cell, characterized in that: It comprises the plastic and Mylar film connection structure under the battery cell as described in any one of claims 1 to 6, and also comprises a winding core (3), the top surface of the winding core (3) is in contact with the top surfaces of the side protrusions (12) and the middle protrusions (11), and the side walls at both ends of the winding core (3) are flush with the semicircular arc surface (121).