Protective-free waterproof coiled material

Through the combined structure of a high-bonding modified asphalt waterproof coating layer and a modified asphalt waterproof roll layer, the problems of frequent laying of waterproof rolls and cracking caused by stress and strain are solved, and efficient waterproofing and durability are achieved in a single laying.

CN222119128UActive Publication Date: 2024-12-06TIANJIN YUSHEN BUILDING WATERPROOF MATERIAL
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420876898.8
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-04-25
Publication Date
2024-12-06
Estimated Expiration
2034-04-25

AI Technical Summary

Technical Problem

The existing waterproof coil laying requires three covers to achieve first-level waterproof performance, resulting in waste of labor and labor hours, and the stress and strain caused by building settlement causes the coil to crack.

Method used

Using a combined structure of a highly bonded modified asphalt waterproof coating layer, an upper and lower layer modified asphalt waterproof coil layer, the high bonded modified asphalt waterproof coating layer is a glue-like substance with creep properties, and is connected by three waterproof layers to reduce the Number of laying times and resist stress and strain.

Benefits of technology

It can meet the requirements of first-level waterproof performance by single laying, save manpower and labor, and prevent the roll from cracking through creep, improving construction efficiency and waterproofing effect.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222119128U_ABST
    Figure CN222119128U_ABST
Patent Text Reader

Abstract

The utility model relates to the technical field of waterproof coiled materials, in particular to a protection-free waterproof coiled material. The utility model provides a protection-free waterproof roll. The protection-free waterproof roll comprises a high-adhesion modified asphalt waterproof coating layer, an upper modified asphalt waterproof roll layer and a lower modified asphalt waterproof roll layer, the high-adhesion modified asphalt waterproof coating layer is arranged between the upper modified asphalt waterproof roll layer and the lower modified asphalt waterproof roll layer; the high-viscosity modified asphalt waterproof coating layer is jelly and has creep property, and the upper modified asphalt waterproof roll layer and the lower modified asphalt waterproof roll layer are connected through the high-viscosity modified asphalt waterproof coating layer. Three waterproof layers are jointly formed, the requirement can be met only by laying for one time, manpower is saved, laying efficiency is improved, meanwhile, due to the fact that the high-viscosity modified asphalt waterproof coating layer is jelly and has creep property, the high-viscosity modified asphalt waterproof coating layer is not cured, stress strain can be resisted through creep property, and the coiled material is prevented from cracking.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of waterproof coiled materials, in particular to a protection-free waterproof coiled material. Background Art

[0002] Waterproofing membrane is mainly used in roofs, basements, tunnels, roads, etc. It is a flexible building material product that protects against external rainwater and groundwater leakage. As a leak-free connection between the engineering foundation and the building, it is the first barrier to waterproofing the entire project and plays a vital role in the entire project. The main products are asphalt waterproofing membrane and polymer waterproofing membrane.

[0003] At present, according to the requirements of the new national standard 55030, if the first-level waterproof performance requirements are to be achieved, three layers of waterproof membranes need to be laid manually, which wastes manpower and working hours. At the same time, after the waterproof membrane is laid, the main body of the building will usually produce stress and strain on the base due to settlement and other reasons. This strain will cause the force concentration of the membrane and cause the membrane to crack. Utility Model Content

[0004] The utility model aims to provide a protection-free waterproofing membrane to solve the technical problem that the waterproofing membrane is manually laid three times, which wastes manpower and working hours. At the same time, after the waterproofing membrane is laid, the main body of the building usually generates stress and strain on the base layer due to settlement and other reasons. This strain will cause the force concentration of the membrane and cause the membrane to crack.

[0005] The utility model provides a protection-free waterproof roll material, comprising: a high-bonding modified asphalt waterproof coating layer, an upper modified asphalt waterproof roll layer and a lower modified asphalt waterproof roll layer;

[0006] The high-bonding modified asphalt waterproof coating layer is arranged between the upper modified asphalt waterproof roll layer and the lower modified asphalt waterproof roll layer;

[0007] The high-adhesion modified asphalt waterproof coating layer is a colloid and has creep properties, and the upper modified asphalt waterproof roll layer and the lower modified asphalt waterproof roll layer are connected through the high-adhesion modified asphalt waterproof coating layer.

[0008] As a further technical solution, a high-bonding rubber fireproof layer is provided on the upper surface of the upper modified asphalt waterproof roll layer;

[0009] The thickness of the high-bonding rubber fireproof layer is 2-2.5 mm.

[0010] As a further technical solution, the upper surface of the upper modified asphalt waterproof roll layer is also provided with an overlapping edge, and the overlapping edge is located at at least one end of the high-bonding rubber fireproof layer;

[0011] The width of the overlapping edge is 10-15 cm.

[0012] As a further technical solution, the upper surface of the upper modified asphalt waterproofing roll layer is further provided with a first high-adhesion self-adhesive layer, and the first high-adhesion self-adhesive layer is located at the overlapping edge;

[0013] The thickness of the first high-bonding self-adhesive layer is 1.5-2 mm.

[0014] As a further technical solution, an active particle layer is provided on the upper surface of the high-bonding rubber fireproof layer;

[0015] The thickness of the active particle layer is 1-2 mm.

[0016] As a further technical solution, an upper isolation film is provided on the upper surface of the first high-adhesion self-adhesive layer.

[0017] As a further technical solution, a second high-bonding self-adhesive layer is provided on the lower surface of the lower modified asphalt waterproofing roll layer;

[0018] The thickness of the second high-bonding self-adhesive layer is 1-1.5 mm.

[0019] As a further technical solution, a lower isolation film is provided on the lower surface of the second high-adhesion self-adhesive layer.

[0020] As a further technical solution, the thickness of the high-bonding modified asphalt waterproof coating layer is 1.5-2 mm;

[0021] The thickness of the upper modified asphalt waterproof roll layer is 3-4 mm;

[0022] The thickness of the lower modified asphalt waterproofing roll layer is 3-4 mm.

[0023] As a further technical solution, both the upper modified asphalt waterproofing roll layer and the lower modified asphalt waterproofing roll layer have a reinforcement layer, and the thickness of the reinforcement layer is 0.5-1.5 mm;

[0024] The reinforcing layer is a non-woven fabric, and the non-woven fabric includes a first spun yarn and a second spun yarn that are perpendicularly crossed;

[0025] The nonwoven fabric has a first side, the angle between the first spinning and the first side is 45°, and the angle between the second spinning and the first side is 135°.

[0026] Compared with the prior art, the technical advantages of the protection-free waterproofing coiled material provided by the utility model are:

[0027] The protection-free waterproof roll material provided by the utility model comprises: a high-adhesion modified asphalt waterproof coating layer, an upper modified asphalt waterproof roll layer and a lower modified asphalt waterproof roll layer; the high-adhesion modified asphalt waterproof coating layer is arranged between the upper modified asphalt waterproof roll layer and the lower modified asphalt waterproof roll layer; the high-adhesion modified asphalt waterproof coating layer is a colloid and has creep properties, and the upper modified asphalt waterproof roll layer and the lower modified asphalt waterproof roll layer are connected by the high-adhesion modified asphalt waterproof coating layer.

[0028] The upper modified asphalt waterproof roll layer, high-adhesion modified asphalt waterproof coating and lower modified asphalt waterproof roll layer arranged from top to bottom form three waterproof layers together. Only one laying is needed to meet the requirements, saving manpower and improving laying efficiency. At the same time, because the high-adhesion modified asphalt waterproof coating layer is a colloid and has creep properties, the high-adhesion modified asphalt waterproof coating layer does not solidify, and can resist stress and strain through creep properties to avoid cracking of the roll material.

[0029] Other features and advantages of the present invention will be described in detail in the subsequent specific implementation section. BRIEF DESCRIPTION OF THE DRAWINGS

[0030] In order to more clearly illustrate the specific implementation methods of the utility model or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0031] Figure 1 A cross-sectional view of a protection-free waterproofing membrane provided in an embodiment of the utility model;

[0032] Figure 2 This is a schematic diagram of the non-woven fabric structure provided in an embodiment of the utility model.

[0033] Icon: 1-high adhesion modified asphalt waterproof coating layer; 2-upper modified asphalt waterproof roll layer; 3-lower modified asphalt waterproof roll layer; 4-high adhesion rubber fireproof layer; 5-first high adhesion self-adhesive layer; 6-active particle layer; 7-upper isolation membrane; 8-second high adhesion self-adhesive layer; 9-lower isolation membrane; 10-non-woven fabric; 11-first spinning; 12-second spinning; 13-first edge; 14-active particles. DETAILED DESCRIPTION

[0034] The technical solution of the utility model will be clearly and completely described below in conjunction with the embodiments. Obviously, the described embodiments are part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments of the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0035] In the description of the present invention, it should be noted that the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inner", "outer", etc., indicating the orientation or positional relationship, are based on the orientation or positional relationship shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention. In addition, the terms "first", "second", and "third" are used for descriptive purposes only, and cannot be understood as indicating or implying relative importance.

[0036] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installation", "connection" and "connection" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0037] In addition, the technical solutions between the various embodiments can be combined with each other, but it must be based on the fact that ordinary technicians in the field can implement it. When the combination of technical solutions is contradictory or cannot be implemented, it should be deemed that such combination of technical solutions does not exist and is not within the scope of protection required by the present utility model.

[0038] The present invention will be further described in detail below through specific implementation examples in conjunction with the accompanying drawings.

[0039] Specific structure such as Figure 1 to Figure 2 shown.

[0040] The present embodiment provides a protection-free waterproof roll material, comprising: a high-adhesion modified asphalt waterproof coating layer 1, an upper modified asphalt waterproof roll layer 2 and a lower modified asphalt waterproof roll layer 3; the high-adhesion modified asphalt waterproof coating layer 1 is arranged between the upper modified asphalt waterproof roll layer 2 and the lower modified asphalt waterproof roll layer 3; the high-adhesion modified asphalt waterproof coating layer 1 is a colloid and has creep properties, and the upper modified asphalt waterproof roll layer 2 and the lower modified asphalt waterproof roll layer 3 are connected through the high-adhesion modified asphalt waterproof coating layer 1.

[0041] In this embodiment, the upper modified asphalt waterproof roll layer 2, the high-adhesion modified asphalt waterproof coating and the lower modified asphalt waterproof roll layer 3 arranged in sequence from top to bottom together form three waterproof layers, which only need to be laid once to meet the requirements, saving manpower and improving laying efficiency. At the same time, since the high-adhesion modified asphalt waterproof coating layer 1 is a colloid and has creep properties, the high-adhesion modified asphalt waterproof coating layer 1 does not solidify, and can resist stress and strain through creep properties to avoid cracking of the roll material, so that the waterproof roll material proposed in this embodiment is protection-free.

[0042] In the optional technical solution of this embodiment, a high-bonding rubber fireproof layer 4 is provided on the upper surface of the upper modified asphalt waterproof roll layer 2; the thickness of the high-bonding rubber fireproof layer 4 is 2-2.5 mm.

[0043] In this embodiment, the high-bonding rubber fireproof layer 4 has a fireproof effect and has a thickness of 2-2.5 mm. Since construction often requires hot work, if the construction workers carelessly bring open flames or heat sources close to the non-protective waterproofing membrane, the non-protective waterproofing membrane is easily melted or perforated. Adding this layer of fireproof coating can prevent the non-protective waterproofing membrane from being damaged by hot-melt construction.

[0044] In the optional technical solution of this embodiment, the upper surface of the upper modified asphalt waterproof roll layer 2 is also provided with an overlapping edge, and the overlapping edge is located at at least one end of the high-bonding rubber fireproof layer 4; the width of the overlapping edge is 10-15cm.

[0045] In this embodiment, if multiple rolls of protection-free waterproof membrane are laid in parallel, there will be a gap at the junction of two adjacent rolls of protection-free waterproof membrane, causing water seepage. A 10-15 cm overlapping edge is set on each roll of protection-free waterproof membrane, and the adjacent protection-free waterproof membrane can be staggered and connected through the overlapping edge to improve the waterproof effect.

[0046] In this embodiment, the overlapping edge is located on the upper surface of the upper modified asphalt waterproof roll layer 2, and is located at one end or multiple ends of the high-bonding rubber fireproof layer 4, depending on the specific needs.

[0047] In the optional technical solution of this embodiment, a first high-adhesion self-adhesive layer 5 is further provided on the upper surface of the upper modified asphalt waterproof roll layer 2, and the first high-adhesion self-adhesive layer 5 is located at the overlapping edge; the thickness of the first high-adhesion self-adhesive layer 5 is 1.5-2 mm.

[0048] In this embodiment, self-adhesive rubber is coated on the upper surface of the upper modified asphalt waterproof roll layer 2 to form a first high-adhesion self-adhesive layer 5. The self-adhesive rubber does not need to be hot-melted, and can be used like self-adhesive glue to combine two pieces of protection-free waterproof roll materials at the overlapping edges.

[0049] In an optional technical solution of the present embodiment, an active particle layer 6 is provided on the upper surface of the high-bonding rubber fireproof layer 4; the thickness of the active particle layer 6 is 1-2 mm.

[0050] In this embodiment, the high-bonding rubber fireproofing layer 4 is capable of adhering to the active particles 14 , and a plurality of active particles 14 are bonded to the upper surface of the high-bonding rubber fireproofing layer 4 to form an active particle layer 6 .

[0051] Among them, the active particles 14 can be well combined with concrete and have the function of self-repairing cracks. The active particles 14 are calcium-containing materials that react quickly with concrete and are firmly bonded. Due to their small particle structure, they can fill concrete cracks and repair cracks.

[0052] In this embodiment, the thickness of the active particle layer 6 is preferably 1.5 mm, which can meet the functional requirements while avoiding being too thick and saving costs.

[0053] In an optional technical solution of this embodiment, an upper isolation film 7 is provided on the upper surface of the first high-adhesion self-adhesive layer 5 .

[0054] In this embodiment, the upper isolation film 7 is used to temporarily protect the first high-adhesion self-adhesive layer 5 from being contaminated, and needs to be torn off when in use.

[0055] In the optional technical solution of this embodiment, a second high-adhesion self-adhesive layer 8 is provided on the lower surface of the lower modified asphalt waterproofing roll layer 3; the thickness of the second high-adhesion self-adhesive layer 8 is 1-1.5 mm.

[0056] In this embodiment, the second high-adhesion self-adhesive layer 8 can be bonded to the base concrete layer, eliminating the need for hot-melt construction bonding.

[0057] Specifically, a self-adhesive rubber is coated on the lower surface of the lower modified asphalt waterproofing roll layer 3 to form a second high-adhesive self-adhesive layer 8. The self-adhesive rubber does not need to be hot-melted, but is bonded to the base concrete layer like a self-adhesive glue.

[0058] In an optional technical solution of this embodiment, a lower isolation film 9 is provided on the lower surface of the second high-adhesion self-adhesive layer 8 .

[0059] In this embodiment, the lower isolation film 9 is used to temporarily protect the second high-adhesion self-adhesive layer 8 from being contaminated, and needs to be torn off when in use.

[0060] In the optional technical solution of this embodiment, the thickness of the high-bonding modified asphalt waterproof coating layer 1 is 1.5-2mm; the thickness of the upper modified asphalt waterproof roll layer 2 is 3-4mm; the thickness of the lower modified asphalt waterproof roll layer 3 is 3-4mm. It can meet the waterproof function and ensure that the overall thickness is not too large.

[0061] In the optional technical solution of the present embodiment, both the upper modified asphalt waterproof roll layer 2 and the lower modified asphalt waterproof roll layer 3 are provided with a reinforcement layer, and the thickness of the reinforcement layer is 0.5-1.5 mm; the reinforcement layer is a non-woven fabric 10, and the non-woven fabric 10 includes a first spun yarn 11 and a second spun yarn 12 that are perpendicularly crossed; the non-woven fabric 10 has a first edge 13, and the angle between the first spun yarn 11 and the first edge 13 is 45°, and the angle between the second spun yarn 12 and the first edge 13 is 135°.

[0062] In this embodiment, the reinforcing layer can be a product of a non-woven fabric 10 vertically cross-woven, wherein the first spinning 11 in one direction and the first side 13 of the non-woven fabric 10 have an angle of 45°, and the second spinning 12 in the other direction and the first side 13 of the non-woven fabric 10 have an angle of 135°. This structure can resist the lateral and longitudinal stress of the waterproof coiled material, disperse the tension, and not easily damage the waterproof coiled material.

[0063] Compared with the existing problems of modified asphalt waterproofing membranes, such as the need for hot-melt construction during laying, workers are vulnerable to toxic and harmful gases, which is not conducive to the implementation of carbon emission reduction policies; the membrane needs to be protected by a cement mortar layer in underground and other construction environments to prevent the steel bars from penetrating the waterproofing membrane when tying the steel bars, causing the membrane to fail. After the waterproofing membrane is laid, the main body of the building will usually produce stress and strain on the base due to settlement and other reasons. This strain will cause the force concentration of the membrane, resulting in cracking of the membrane, etc. The protection-free waterproofing membrane provided in this embodiment is a composite functional membrane that is non-hot-melt and resistant to deformation while reducing the number of construction layers. It can not only improve construction efficiency and protect the environment, but also obtain a long-lasting waterproof function.

[0064] Finally, it should be noted that the above embodiments are only used to illustrate the technical solution of the utility model, rather than to limit it. Although the utility model has been described in detail with reference to the aforementioned embodiments, ordinary technicians in this field should understand that they can still modify the technical solutions recorded in the aforementioned embodiments, or replace some or all of the technical features therein with equivalents. However, these modifications or replacements do not make the essence of the corresponding technical solution deviate from the scope of the technical solution of the embodiments of the utility model.

Claims

1. A kind of protection-free waterproof membrane, It is characterized in that include: A high-adhesion modified asphalt waterproof coating layer (1), an upper modified asphalt waterproof roll layer (2) and a lower modified asphalt waterproof roll layer (3); The high-adhesion modified asphalt waterproof coating layer (1) is arranged between the upper modified asphalt waterproof roll layer (2) and the lower modified asphalt waterproof roll layer (3); The high-adhesion modified asphalt waterproof coating layer (1) is a colloid and has creep properties, and the upper modified asphalt waterproof roll layer (2) and the lower modified asphalt waterproof roll layer (3) are connected via the high-adhesion modified asphalt waterproof coating layer (1).

2. The protection-free waterproofing coiled material according to claim 1, It is characterized in that The upper surface of the upper modified asphalt waterproof roll layer (2) is provided with a high-bonding rubber fireproof layer (4); The thickness of the high-bonding rubber fireproof layer (4) is 2-2.5 mm.

3. The protection-free waterproofing coiled material according to claim 2, It is characterized in that The upper surface of the upper modified asphalt waterproof roll layer (2) is also provided with an overlapping edge, and the overlapping edge is located at at least one end of the high-bonding rubber fireproof layer (4); The width of the overlapping edge is 10-15 cm.

4. The protection-free waterproofing coiled material according to claim 3, It is characterized in that The upper surface of the upper modified asphalt waterproofing roll layer (2) is also provided with a first high-adhesion self-adhesive layer (5), and the first high-adhesion self-adhesive layer (5) is located at the overlapping edge; The thickness of the first high-bonding self-adhesive layer (5) is 1.5-2 mm.

5. The protection-free waterproofing coiled material according to claim 2, It is characterized in that An active particle layer (6) is provided on the upper surface of the high-bonding rubber fireproof layer (4); The thickness of the active particle layer (6) is 1-2 mm.

6. The protection-free waterproofing coiled material according to claim 4, It is characterized in that An upper isolation film (7) is provided on the upper surface of the first high-adhesion self-adhesive layer (5).

7. The protection-free waterproofing coiled material according to claim 1, It is characterized in that The lower surface of the lower modified asphalt waterproofing roll layer (3) is provided with a second high-adhesion self-adhesive layer (8); The thickness of the second high-adhesion self-adhesive layer (8) is 1-1.5 mm.

8. The protection-free waterproofing coiled material according to claim 7, It is characterized in that A lower isolation film (9) is provided on the lower surface of the second high-adhesion self-adhesive layer (8).

9. The protection-free waterproofing membrane according to any one of claims 1 to 8, It is characterized in that The thickness of the high-adhesion modified asphalt waterproof coating layer (1) is 1.5-2 mm; The thickness of the upper modified asphalt waterproofing roll layer (2) is 3-4 mm; The thickness of the lower modified asphalt waterproofing roll layer (3) is 3-4 mm.

10. The protection-free waterproofing membrane according to any one of claims 1 to 8, It is characterized in that The upper modified asphalt waterproofing roll layer (2) and the lower modified asphalt waterproofing roll layer (3) both have a reinforcement layer, and the thickness of the reinforcement layer is 0.5-1.5 mm; The reinforcing layer is a non-woven fabric (10), and the non-woven fabric (10) comprises a first spun yarn (11) and a second spun yarn (12) that are perpendicularly crossed; The nonwoven fabric (10) has a first edge (13), the angle between the first spun yarn (11) and the first edge (13) is 45°, and the angle between the second spun yarn (12) and the first edge (13) is 135°.