Gauge for calibrating steel rail sample plate
By designing the calibration gauge of the rail sample, the sample qualified comparison benchmark block, wear calibration template and crown-shaped standard block are integrated, which solves the problem of reduced measurement accuracy caused by wear of the rail sample, and achieves efficient calibration and accurate rail Acceptance prevents unqualified rails from being accidentally collected.
Patent Information
- Application Number
- CN202420892028.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-04-26
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2034-04-26
AI Technical Summary
The rail sample wears after long-term use, resulting in a decrease in measurement accuracy, which may lead to the accidental collection of unqualified rails. The existing technology lacks effective calibration methods to prevent such errors.
A rail sample calibration gauge is designed, including sample qualified comparison benchmark blocks, wear calibration templates and crown-shaped standard standard blocks. Through the connection ring, a variety of calibration functions are provided to simplify operation and improve calibration efficiency.
Effectively prevent unqualified rails from being accidentally collected due to sample wear, ensure the accuracy and efficiency of rail acceptance, simplify the on-site calibration process, and improve the service life of rail samples.
Smart Images

Figure CN222124160U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the field of railway measurement, in particular to a gauge for calibrating a rail sample. Background Art
[0002] Rails carry and guide locomotive wheels during train operation and bear the huge pressure of wheels, which is an important part of rail transportation. Rails must provide a continuous, smooth and least resistant rolling surface for wheels. In order to ensure that the rail type and size meet the requirements of the railway industry standard TB / T2344-2020 acceptance standard, the inspection templates specified in the standard are used for inspection and judgment of finished rails. Rail inspection templates include rail height, rail head width, rail crown fullness and wedge, joint clamp installation surface height, rail waist thickness, rail bottom width, rail bottom edge thickness and other templates.
[0003] During the production of rails, samples are used to inspect them. The measurement process is contact-based. After long-term repeated measurements, the samples will be worn to varying degrees, resulting in a decrease in the accuracy of the sample measurement. According to the principles of rail quality acceptance, rails with unqualified types and sizes cannot be mistakenly accepted during rail acceptance inspection. During daily use of the samples, the accuracy of the samples should be checked regularly. If the samples are damaged, they should be replaced immediately to prevent the mistaken acceptance of unqualified rails due to the wear of the samples exceeding the wear limit. Utility Model Content
[0004] The utility model aims to solve the problem of whether a worn rail sample meets the measurement accuracy requirement, and proposes a gauge for calibrating a rail sample, which is convenient for on-site use and prevents the miscollection of unqualified rails due to the sample being worn beyond the wear limit.
[0005] The utility model discloses a gauge for calibrating a rail sample, comprising a sample qualified comparison block, a wear amount calibration sample and a crown-shaped standard block, which are connected in series through a connecting ring.
[0006] Among them, the qualified sample comparison block has a top plate A, a waist plate A and a bottom plate A; among them, the top and bottom ends of the waist plate A are respectively connected to the center positions of the bottom surface of the top plate A and the top surface of the bottom plate A, and the overall structure is an I-shaped structure; and the front and back sides of the three plates are coplanar; at the same time, a rectangular protrusion A is designed in the middle of the top surface of the top plate A, and the upper right side of the rectangular protrusion A is a concave surface that is concave inward.
[0007] The qualified sample plate is 175.4mm higher than the benchmark block; the left-right length of the bottom plate A103 is 149mm, and the height is 11.5mm; the left-right length of the top plate A is 120mm; the left-right length of the waist plate A is 16mm; the vertical distance between the top surface of the bottom plate A and the bottom surface of the left part of the waist plate A is 122.48mm; the vertical distance between the top surface of the bottom plate A and the bottom surface of the right part of the waist plate A is 121.38mm; the left-right length of the rectangular protrusion A104 is 71.3mm, and the height is 30mm.
[0008] The wear calibration sample has a top plate B, a waist plate B and a bottom plate B; wherein the top and bottom ends of the waist plate B are respectively connected to the bottom surface of the top plate B and the center position of the top surface of the bottom plate B, forming an I-shaped structure as a whole, and the front and back sides of the three plates are coplanar.
[0009] The height of the above-mentioned wear calibration sample is 176.6mm; the length of the bottom plate B in the left and right directions is 151mm, and the height is 15mm; the horizontal distance between the left wall of the top plate B and the left wall of the bottom plate is 40.8mm, and the horizontal distance between the right wall of the top plate B and the right wall of the bottom plate B is 38.4mm; the height of the top plate B is 41.6mm; the length of the waist plate B in the left and right directions is 17.5mm, and the height is 120mm.
[0010] The crown-shaped standard block comprises a rectangular main body and an upper rectangular protrusion and a lower rectangular protrusion respectively designed in the middle of the top surface and the bottom surface of the rectangular main body; the four corners of the rectangular main body are designed to be rounded.
[0011] The height of the above-mentioned crown-shaped standard block is 50mm; the rectangular main body is 60mm long in the left and right direction, the vertical distance between the top surface and the top surface of the upper rectangular protrusion is 13.31mm, and the vertical distance between the bottom surface and the bottom surface of the lower rectangular protrusion is 12.18mm; the left and right lengths of the upper rectangular protrusion and the lower rectangular protrusion are both 11mm; the curvature radius of the left and right rounded corners of the upper part of the rectangular main body is 16mm, and the curvature radius of the left and right rounded corners of the lower part is 13mm; the lateral spacing between the two ends of the left and right rounded corners of the upper part of the rectangular main body is 4.465mm; the lateral spacing between the two ends of the left and right rounded corners of the lower part of the rectangular main body is both 4.65mm.
[0012] The utility model provides a gauge assembly for calibrating a rail sample, and the utility model has the advantages that:
[0013] 1. The utility model provides a gauge assembly for calibrating a rail sample, which integrates calibration functions of various rail samples.
[0014] 2. The gauge assembly for calibrating a rail sample of the utility model has a simple structure, simple operation and high calibration efficiency. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 This is a schematic diagram of the structure of a sample qualified comparison block in a gauge assembly for calibrating a rail sample of the utility model;
[0016] Figure 2 This is a schematic diagram of the structure of the wear calibration sample in the gauge assembly for calibrating the rail sample of the utility model;
[0017] Figure 3 This is a schematic diagram of the structure of the crown-shaped standard block in the gauge assembly for calibrating a rail sample of the utility model;
[0018] Figure 4 a is a schematic diagram of the qualified calibration of the rail height negative sample;
[0019] Figure 4 b is a schematic diagram of the failure of the calibration of the rail height negative sample;
[0020] Figure 5 a is a schematic diagram of the qualified calibration of waist-thick negative sample;
[0021] Figure 5 b is a schematic diagram of the failure of waist thickness negative sample calibration;
[0022] Figure 6 a is a schematic diagram of the qualified calibration of the negative sample of rail bottom width;
[0023] Figure 6 b is a schematic diagram of the failure of the calibration of the negative sample of the rail bottom width;
[0024] Figure 7 a is a schematic diagram of the qualified calibration of the rail head width positive sample;
[0025] Figure 7 b is a schematic diagram of the failure of calibration of the rail head width positive sample;
[0026] Figure 8 a is a schematic diagram of the qualified calibration of the negative sample of rail head width;
[0027] Figure 8 b is a schematic diagram of the failure of the negative sample calibration of the rail head width;
[0028] Fig. 9 a is a schematic diagram of the qualified calibration of the positive sample of the joint clamping plate installation surface height;
[0029] Fig. 9 b is a schematic diagram of the failure of the calibration of the positive sample of the joint clamping plate installation surface height;
[0030] Fig.10 a is a schematic diagram of the qualified calibration of the negative sample plate for the joint clamping plate installation surface height;
[0031] Fig.10 b is a schematic diagram of the failure of the negative sample calibration for the joint clamp installation surface height;
[0032] Fig.11 a is a schematic diagram of the qualified calibration of the track height positive sample;
[0033] Fig.11 b is a schematic diagram of the failure of calibration of the positive rail height sample;
[0034] Fig.12 a is a schematic diagram of the qualified calibration of the waist thickness positive sample;
[0035] Fig.12 b is a schematic diagram of the waist thickness positive sample calibration failure;
[0036] Fig.13 a is a schematic diagram of the qualified calibration of the rail bottom width positive sample;
[0037] Fig.13 b is a schematic diagram of the failure of calibration of the rail bottom width positive sample;
[0038] Fig.14 a is a schematic diagram of the qualified calibration of the positive sample with asymmetric cross section;
[0039] Fig.14 b is a schematic diagram of the failure of calibration of the positive sample with asymmetric cross section;
[0040] Fig.15 a is a schematic diagram of the qualified calibration of the negative sample with asymmetric cross section;
[0041] Fig.15 b is a schematic diagram of the failure of calibration of the negative sample with asymmetric cross section;
[0042] Fig.16 a is a schematic diagram of the qualified calibration of the rail crown fullness sample;
[0043] Fig.16 b is a schematic diagram showing that the rail crown fullness sample calibration failed.
[0044] In the figure:
[0045] 101-Top plate A 102-Waist plate A 103-Bottom plate A
[0046] 104- rectangular protrusion A 105- concave surface 201- top plate B
[0047] 202- waist plate B 203- bottom plate B 301- rectangular body 302-upper rectangular protrusion 303-lower rectangular protrusion DETAILED DESCRIPTION
[0048] The present invention will be further described in detail below in conjunction with the accompanying drawings.
[0049] The utility model provides a gauge for calibrating a rail sample, which is composed of three rail sample calibration parts connected by a connecting ring. The three rail sample calibration parts include a sample qualified comparison block, a wear calibration sample and a crown standard block. Figure 1 , Figure 2 , Figure 3 As shown, it is strictly designed according to the size of the rail sample designed according to the national standard to achieve the measurement of various types of rail samples.
[0050] The specific structure of each gauge in the present invention is:
[0051] A. The qualified sample comparison block has a top plate A101, a waist plate A102 and a bottom plate A103. Among them, the top and bottom ends of the waist plate A102 are connected to the bottom surface of the top plate A101 and the center of the top surface of the bottom plate A103 respectively, and the overall structure is an I-shaped structure; and the front and back of the three plates are coplanar, with an overall thickness of 4mm. At the same time, a rectangular protrusion A104 is designed in the middle of the top surface of the top plate A101, and the upper right side of the rectangular protrusion A104 is an inwardly concave surface 105, which is 1mm lower than the right side of the rectangular protrusion A104 in the horizontal direction.
[0052] Among the qualified comparison blocks of the above structural samples:
[0053] The entire block is 175.4mm high;
[0054] The length of the bottom plate A103 in the left-right direction is 149mm and the height is 11.5mm;
[0055] The length of top plate A101 in left-right direction is 120mm;
[0056] Waist plate A102 left and right length 16mm;
[0057] The vertical distance between the top surface of the bottom plate A103 and the bottom surface of the left part of the top plate A101 located on the waist plate A102 is 122.48 mm;
[0058] The vertical distance between the top surface of the bottom plate A103 and the bottom surface of the top plate A101 located on the right side of the waist plate A102 is 121.38 mm;
[0059] The rectangular protrusion A104 has a length of 71.3 mm in the left-right direction and a height of 30 mm.
[0060] B. The wear calibration sample has a top plate B201, a waist plate B202 and a bottom plate B203. The top and bottom ends of the waist plate B202 are connected to the bottom surface of the top plate B201 and the center of the top surface of the bottom plate B203 respectively, forming an I-shaped structure as a whole, and the front and back of the three plates are coplanar, with an overall thickness of 4 mm.
[0061] In the above structural wear calibration sample:
[0062] The entire sample height is 176.6mm;
[0063] The length of the bottom plate B203 in the left-right direction is 151mm and the height is 15mm;
[0064] The horizontal distance between the left side wall of the top plate B201 and the left side wall of the bottom plate is 40.8 mm, and the horizontal distance between the right side wall of the top plate B201 and the right side wall of the bottom plate B203 is 38.4 mm; the height of the top plate B201 is 41.6 mm;
[0065] The length of the waist plate B202 in the left-right direction is 17.5 mm and the height is 120 mm.
[0066] C. The crown-shaped standard block includes a rectangular body 301 and an upper rectangular protrusion 302 and a lower rectangular protrusion 303 respectively designed in the middle of the top and bottom surfaces of the rectangular body 301, and the overall thickness is 4 mm. The four circumferential corners of the rectangular body 301 are designed to be rounded.
[0067] In the above structural crown standard block:
[0068] The overall height is 50mm;
[0069] The rectangular body 301 is 60 mm long in the left-right direction, the vertical distance between the top surface and the top surface of the upper rectangular protrusion 302 is 13.31 mm, and the vertical distance between the bottom surface and the bottom surface of the lower rectangular protrusion 303 is 12.18 mm; the left-right lengths of the upper rectangular protrusion 302 and the lower rectangular protrusion 303 are both 11 mm.
[0070] The curvature radius of the left and right rounded corners of the upper part of the rectangular body 301 is 16mm, and the curvature radius of the left and right rounded corners of the lower part is 13mm; and the lateral spacing between the two rounded corners of the upper part of the rectangular body 301 (i.e., the lateral distance between the left and right ends of the top plane part of the rectangular body 301 and the left and right side walls of the rectangular body) is 4.465mm; the lateral spacing between the two rounded corners of the lower part of the rectangular body 301 is 4.65mm. In the present utility model, the calibration of each measurement template of the rail is realized by three templates, wherein:
[0071] The qualified sample comparison block is used to calibrate the rail height negative sample, waist thickness negative sample, rail bottom width negative sample, rail head width positive sample, rail head width negative sample, joint clamp installation surface height positive sample, and joint clamp installation surface height negative sample.
[0072] The wear calibration sample is used to calibrate the rail height positive sample, waist thickness positive sample, rail bottom width positive sample, section asymmetry positive sample, and section asymmetry negative sample.
[0073] Crown standard blocks are used to calibrate rail crown fullness samples.
[0074] The above-mentioned qualified sample comparison block, wear calibration sample and crown standard block are provided with through holes, and the three through holes are passed through by connecting rings to realize the series connection between the three, so as to prevent the loss of a sample by storing them separately during use. Among them, the through hole on the qualified sample comparison block is opened at the center of the top plate A101, passing through the front and back sides; the through hole on the wear calibration sample is opened at the center of the top plate B201, passing through the front and back sides; the through hole on the crown standard block is opened at the center of the rectangular body 301, passing through the front and back sides. During calibration, the calibration environment temperature is 20℃±5℃, and the humidity is ≤80%RH. Before calibration, the calibrated sample needs to be inspected, and the working surface of the calibrated special measuring tool should not have appearance defects, bumps and bending deformations that affect the use, and observe whether there are burrs or dirt on the measuring surface, and grind the burrs with oilstone, clean it with gasoline and then wipe it clean with silk cloth.
[0075] The specific calibration method of each rail measurement template by the utility model is as follows:
[0076] (1) Track height negative sample calibration.
[0077] The bottom surface of the qualified sample comparison block is aligned with the rail bottom fitting surface of the rail height negative sample, and then translated toward the rail height negative sample; if the rectangular protrusion A104 of the qualified sample comparison block can pass through the rail top fitting surface of the rail height negative gauge, such as Figure 4 As shown in a, the rail height negative sample is judged to be qualified; otherwise, it is unqualified, such as Figure 4 As shown in b.
[0078] (2) Calibration of waist thickness negative sample.
[0079] The non-measurement surface of the waist thickness negative sample to be calibrated is fitted with the front / rear side of the waist plate A102 of the qualified sample comparison block, and then pushed toward the qualified sample comparison block; if the waist thickness negative sample can pass through the rear / front side of the waist of the comparison block, Figure 5 As shown in a, the rail waist negative sample is judged to be qualified; otherwise, it is unqualified, such as Figure 5 As shown in b.
[0080] (3) Rail bottom width negative sample calibration.
[0081] The non-measuring surface of the calibrated rail bottom width gauge is fitted with the left / right end surface of the base plate A103 of the qualified sample comparison standard block, and then the rail bottom width negative sample is pushed from bottom to top toward the comparison standard block; if the measuring surface of the rail bottom width negative sample can pass through the base plate A103 of the qualified sample comparison standard block, such as Figure 6 As shown in a, the negative sample of rail bottom width is qualified; otherwise, it is unqualified, such as Figure 6 As shown in b.
[0082] (4) Rail head width calibration.
[0083] The left contact point of the calibrated rail head width positive sample is fitted with the left side of the rectangular protrusion A104 on the top of the sample qualified comparison standard block, and then pushed from top to bottom toward the sample qualified comparison standard block; if the right contact point of the rail head width positive sample cannot pass through the non-concave surface 105 of the right side of the rectangular protrusion A104 on the top of the sample qualified comparison standard block, such as Figure 7 As shown in a, the calibration rail head width positive sample is qualified; otherwise, it is unqualified, such as Figure 7 As shown in b.
[0084] (5) Rail head width negative sample calibration.
[0085] The left contact point of the negative sample of the calibrated rail head width is fitted with the left side of the rectangular protrusion A104 on the top of the qualified sample comparison block, and then pushed from top to bottom toward the qualified sample comparison block; if the right contact point of the negative sample of the rail head width can pass through the concave surface 105 on the right side of the rectangular protrusion A104 on the top of the qualified sample comparison block, as shown in the figure, Figure 8 As shown in a, the calibration rail head width positive gauge is qualified; otherwise, it is unqualified, such as Figure 8 As shown in b.
[0086] (6) The height of the joint clamp installation surface is calibrated according to the sample.
[0087] The installation surface of the joint clamp to be calibrated is aligned with the lower surface of the sample, and is fitted with the upper surface of the bottom plate A103 on the left side of the waist plate A102 in the qualified comparison block of the sample, and then pushed from left to right toward the qualified comparison block of the sample; if the installation surface of the joint clamp is aligned with the upper surface of the sample and can pass through the lower surface of the top plate A101 on the left side of the waist plate A102 in the qualified comparison block of the sample, as shown in the figure, Fig. 9 As shown in a, the calibration joint clamp installation surface height is judged to be qualified; otherwise, it is unqualified, such as Fig. 9 As shown in b.
[0088] (7) Negative sample calibration of the joint clamp installation surface height.
[0089] The lower surface of the negative sample plate with the installation surface height of the joint clamp to be calibrated is fitted with the upper surface of the bottom plate A103 on the right side of the waist plate A102 in the qualified sample comparison block, and then pushed from right to left toward the qualified sample comparison block; if the upper surface of the negative sample plate with the installation surface height of the joint clamp can pass through the lower surface of the top plate A101 on the right side of the waist plate A102 in the qualified sample comparison block, as shown in the figure below: Fig.10 As shown in a, the negative sample of the calibration joint clamp installation surface height is qualified; otherwise, it is unqualified, such as Fig.10 As shown in b.
[0090] (8) Track height calibration.
[0091] Fit the bottom fitting surface of the rail height positive sample to be calibrated with the bottom surface of the wear calibration block, and then push it from the side toward the wear calibration block; if the rail height positive sample cannot pass through the top plate B201 of the wear calibration block, Fig.11 As shown in a, the calibration rail height positive sample is judged to be qualified; otherwise, it is unqualified, such as Fig.11 As shown in b.
[0092] (9) Calibration of waist thickness sample.
[0093] The non-measurement surface of the calibrated waist thickness positive sample is set flush with the front / rear side of the waist of the wear calibration standard block, and the waist thickness positive sample is pushed toward the wear calibration standard block. If the waist thickness positive sample cannot pass through the waist side of the wear calibration standard block, as shown in 12a, the calibration rail waist positive sample is judged to be qualified; otherwise, it is unqualified, such as Fig.12 As shown in b.
[0094] (10) Calibration of rail bottom width sample.
[0095] The non-measurement surface of the calibrated rail bottom width positive sample is placed against the left / right end surface of the wear calibration block bottom plate B203, and the rail bottom width positive sample is pushed from bottom to top toward the wear calibration block. If the measurement surface of the rail bottom width positive sample cannot pass through the wear calibration block bottom plate B203, as shown in 13a, the calibrated rail bottom width positive sample is qualified; otherwise, it is unqualified, such as Fig.13 As shown in b.
[0096] (11) Calibration of positive sample with asymmetric cross section.
[0097] The rail bottom fitting surface of the calibrated asymmetric positive sample is fitted with the bottom surface of the wear calibration block; then the wear calibration block is pushed from the side from right to left, and the end point of the asymmetric positive sample does not touch the right side of the top plate B201, that is, t2>0; the asymmetric positive sample is judged to be qualified, such as Fig.14 On the contrary, the distance between the right end face of the wear calibration block bottom plate A103 and the asymmetric positive sample is t1>0, t2=0, which is unqualified, as shown in 14b.
[0098] (12) Calibration of negative sample with asymmetric cross section.
[0099] Fit the rail bottom fitting surface of the calibrated asymmetric negative sample with the bottom surface of the wear calibration block; then push the wear calibration block from the side from left to right; if the end point of the asymmetric negative sample contacts the left side of the top plate B201 of the wear calibration block, and the distance t1 between the right end surface of the bottom plate B203 of the wear calibration block and the asymmetric positive sample is > 0, then the asymmetric negative sample is judged to be qualified. Fig.15 a; otherwise, t1=0, t2>0, which is unqualified, such as Fig.15 As shown in b.
[0100] (13) Calibration of 60N and 60kg rail crown fullness samples.
[0101] Align the groove side of the calibrated 60N rail crown fullness sample with the upper rectangular protrusion 302 side of the crown standard block, and push it from top to bottom toward the crown standard block until the bottom surface of the groove of the rail crown fullness gauge contacts the top surface of the upper rectangular protrusion 302; at this time, if the distance t1 between the two measuring claws in the middle of the calibrated rail crown fullness sample and the left and right rounded corners above the rail crown fullness sample is greater than 0, the rail crown fullness gauge is judged to be qualified. Fig.16 a; on the contrary, if the two measuring claws in the middle of the calibrated rail crown fullness sample fit with the left and right rounded corners above the rail crown fullness sample, the distance t2 between the upper rectangular protrusion 302 and the bottom surface of the groove of the rail crown fullness gauge is greater than 0, which is unqualified, such as Fig.16 As shown in b.
[0102] The calibration of the calibrated 60kg rail crown fullness sample is carried out by cooperating with the lower rectangular protrusion 302 and the left and right inclined surfaces above the rail crown fullness sample, using the same method as above. Fig.16 a and Fig.16 As shown in b.
Claims
1. A gauge for calibrating a rail sample, characterized in that: It includes a sample qualified comparison block, a wear calibration sample and a crown standard block, which are connected in series through a connecting ring; The qualified sample comparison block has a top plate A, a waist plate A and a bottom plate A; the top and bottom ends of the waist plate A are connected to the center of the bottom surface of the top plate A and the top surface of the bottom plate A respectively, and the overall structure is an I-shaped structure; and the front and back of the three plates are coplanar; at the same time, a rectangular protrusion A is designed in the middle of the top surface of the top plate A, and the upper right side of the rectangular protrusion A is a concave surface that is inwardly concave; The qualified sample is 175.4mm higher than the benchmark block; the length of the bottom plate A in the left-right direction is 149mm, and the height is 11.5mm; the length of the top plate A in the left-right direction is 120mm; the length of the waist plate A in the left-right direction is 16mm; the vertical distance between the top surface of the bottom plate A and the bottom surface of the left part of the waist plate A is 122.48mm; the vertical distance between the top surface of the bottom plate A and the bottom surface of the right part of the waist plate A is 121.38mm; the length of the rectangular protrusion A in the left-right direction is 71.3mm, and the height is 30mm; The wear calibration sample has a top plate B, a waist plate B and a bottom plate B; wherein the top and bottom ends of the waist plate B are connected to the bottom surface of the top plate B and the center of the top surface of the bottom plate B respectively, and the whole is an I-shaped structure, and the front and back surfaces of the three plates are coplanar; The height of the wear calibration sample is 176.6mm; the length of the bottom plate B in the left-right direction is 151mm, and the height is 15mm; the horizontal distance between the left wall of the top plate B and the left wall of the bottom plate is 40.8mm, and the horizontal distance between the right wall of the top plate B and the right wall of the bottom plate B is 38.4mm; the height of the top plate B is 41.6mm; the length of the waist plate B in the left-right direction is 17.5mm, and the height is 120mm; The crown-shaped standard block includes a rectangular main body and an upper rectangular protrusion and a lower rectangular protrusion are respectively designed in the middle of the top surface and the bottom surface of the rectangular main body; the four corners of the rectangular main body are designed to be rounded; The height of the above-mentioned crown-shaped standard block is 50mm; the rectangular main body is 60mm long in the left and right direction, the vertical distance between the top surface and the top surface of the upper rectangular protrusion is 13.31mm, and the vertical distance between the bottom surface and the bottom surface of the lower rectangular protrusion is 12.18mm; the left and right lengths of the upper rectangular protrusion and the lower rectangular protrusion are both 11mm; the curvature radius of the left and right rounded corners of the upper part of the rectangular main body is 16mm, and the curvature radius of the left and right rounded corners of the lower part is 13mm; the lateral spacing between the two ends of the left and right rounded corners of the upper part of the rectangular main body is 4.465mm; the lateral spacing between the two ends of the left and right rounded corners of the lower part of the rectangular main body is both 4.65mm.
2. A rail sample calibration gauge as claimed in claim 1, characterized in that: The thickness of the qualified sample comparison block, wear calibration sample and crown standard block are all 4mm.
3. A rail sample calibration gauge as claimed in claim 1, characterized in that: The through hole on the qualified comparison block of the sample is opened at the center position of the top plate A and passes through the front and back sides; the through hole on the wear calibration sample is opened at the center position of the top plate B and passes through the front and back sides; the through hole on the crown standard block is opened at the center position of the rectangular body and passes through the front and back sides.