Curved surface solar module

By using nanocomposite film layers on curved glass solar modules to absorb sunlight from multiple bands, the problem of uneven thickness and color of curved coating layer is solved, the light transmittance and power generation efficiency are improved, production costs are reduced, and production costs are extended. The service life of the component.

CN222126549UActive Publication Date: 2024-12-06SHENZHEN HELLO TECH ENERGY CO LTD
View PDF 0 Cites 2 Cited by

Patent Information

Application Number
CN202323604331.X
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-27
Publication Date
2024-12-06
Estimated Expiration
2033-12-27

AI Technical Summary

Technical Problem

In the prior art, after the curved glass front plate is hot-bending, the thickness and color of the coating layer are uneven, resulting in high reflectivity, low light transmittance and low production efficiency.

Method used

Using nanocomposite film layers including ZnO, SiO2 and TiO2 as the anti-reflection and urination film layer, the glass substrate is plated through magnetron sputtering technology to absorb sunlight from multiple bands, improve light transmittance, and in the front plate layer Add an antifouling film layer to prevent dust from adhering.

Benefits of technology

It significantly improves the light transmittance and power generation efficiency of curved solar modules, reduces the demand for post-coated correction plates, improves production efficiency, and extends the service life of the modules.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222126549U_ABST
    Figure CN222126549U_ABST
Patent Text Reader

Abstract

The utility model relates to the technical field of solar power generation, and discloses a curved surface solar module, which comprises a front plate layer, a first packaging adhesive film layer, a battery layer, a second packaging adhesive film layer and a back plate layer which are sequentially stacked, and the back plate layer is adhered to the back surface of the battery layer through the second packaging adhesive film layer; the front plate layer comprises a glass substrate and an anti-reflection film layer, the glass substrate is bonded to the front face of the battery layer through a first packaging adhesive film layer, and the anti-reflection film layer is plated on the surface, away from the first packaging adhesive film layer, of the glass substrate. The antireflection film layer can absorb sunlight of multiple wave bands, the light transmittance is improved, and the power generation efficiency of the curved surface solar module is improved, so that after film coating, the consistency of the reflection color of the low-curvature glass substrate coating film can be realized without using a correction plate to correct the thickness of the film layer, and the purposes of reducing the reflectivity and improving the light transmittance can be achieved; and the production efficiency is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of solar power generation, in particular to a curved solar energy component. Background Art

[0002] As one of the most commonly used packaging materials for solar cell modules, glass is mainly used for packaging large-size solar cell modules, such as standard modules, building curtain walls, photovoltaic tiles and other products. At present, the glass front panel used in solar modules is usually ultra-white embossed float glass, and the light transmittance is generally greater than 91.5%. The anti-reflection (AR) film is plated on the glass front panel by magnetron sputtering, thermal evaporation, electron beam evaporation, spraying and other processes to ensure the light transmittance of the glass front panel, thereby ensuring the power generation efficiency of the solar module.

[0003] In the prior art, the coating process for flat glass front panels is relatively mature. However, for curved glass front panels, after hot bending, the bent portion cannot form a vertical state with the sputtering target, and there will be uneven temperature control and heating, resulting in uneven thickness and color of the curved coating layer. For the coating layer of a single material, the uneven thickness and color will lead to higher reflectivity and lower transmittance. Therefore, a correction plate is needed to correct the coating thickness to achieve consistency in the reflection color of the coating on the low-curvature glass substrate, thus causing problems such as low production efficiency.

[0004] Therefore, there is an urgent need to provide a curved solar panel to solve the above problems. Utility Model Content

[0005] The utility model aims to provide a curved solar panel, which improves the light transmittance of the solar panel by improving the anti-reflection and anti-transmission effect of the front panel layer, thereby improving the power generation efficiency of the solar panel and improving the production efficiency.

[0006] In order to achieve the above purpose, the utility model is implemented through the following technical solutions:

[0007] A curved solar panel comprises a front panel layer, a first encapsulation film layer, a battery layer, a second encapsulation film layer and a back panel layer stacked in sequence, wherein the back panel layer is bonded to the back of the battery layer through the second encapsulation film layer;

[0008] The front panel layer includes a glass substrate and an anti-reflection and anti-reflection film layer. The glass substrate is bonded to the front side of the battery layer through the first packaging film layer. The anti-reflection and anti-reflection film layer covers the surface of the glass substrate away from the first packaging film layer. The anti-reflection and anti-reflection film layer can absorb sunlight in multiple bands.

[0009] As an optional solution, the anti-reflection and anti-reflection film layer includes a stacked ZnO film layer, a SiO2 film layer and a TiO2 film layer.

[0010] As an optional solution, the thickness of the anti-reflection and anti-reflection film layer is 100nm-200nm.

[0011] As an optional solution, the front plate layer further includes an anti-fouling film layer, and the anti-fouling film layer is arranged on a surface of the anti-reflection and anti-reflection film layer away from the glass substrate.

[0012] As an optional solution, the material of the antifouling film layer is diluted to 3‰ to 8‰ wt by fluorocarbon solvent or silicone oil.

[0013] As an optional solution, the antifouling film layer has a thickness of 80 nm to 150 nm.

[0014] As an optional solution, the first encapsulation film layer is one of high-cutoff EVA film, POE film, EPE film, and PVB film;

[0015] And / or the second encapsulation film layer is one of highly transparent EVA film, POE film, EPE film and PVB film.

[0016] As an optional solution, the backboard layer is made of one of PET, CPC or glass fiber composite materials.

[0017] The beneficial effects of the utility model are:

[0018] In the curved solar panel provided by the utility model, the anti-reflection and anti-reflection film layer can absorb sunlight of multiple different bands, so as to achieve the effect of anti-reflection and anti-reflection, greatly improve the light transmittance of the curved front panel layer, and improve the power generation efficiency of the curved solar panel. Therefore, after coating, there is no need to use a correction plate to correct the film thickness to achieve the consistency of the reflection color of the low-curvature glass substrate coating, so as to achieve the purpose of reducing reflectivity and improving light transmittance, thereby improving production efficiency. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] In order to explain the embodiments of the utility model or the technical solutions in the prior art more clearly and easily, the following is a brief introduction to the drawings required for use in the embodiments or the description of the prior art. The drawings described below are some embodiments of the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0020] Figure 1 It is a schematic diagram of the structure of a solar energy assembly provided by an embodiment of the utility model;

[0021] Figure 2 It is a structural schematic diagram of the front plate layer provided in an embodiment of the utility model.

[0022] In the figure:

[0023] 10. front plate layer; 11. glass substrate; 12. anti-reflection and anti-reflection film layer; 13. anti-fouling film layer;

[0024] 20. First packaging film layer; 30. Battery layer; 40. Second packaging film layer; 50. Backplane layer. DETAILED DESCRIPTION

[0025] The present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It is to be understood that the specific embodiments described herein are only used to explain the present invention, rather than to limit the present invention. It should also be noted that, for ease of description, only the parts related to the present invention, rather than all structures, are shown in the accompanying drawings.

[0026] In the description of the present invention, unless otherwise clearly specified and limited, the terms "connected", "connected", and "fixed" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0027] In the present utility model, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may include that the first and second features are in direct contact, or may include that the first and second features are not in direct contact but are in contact through another feature between them. Moreover, a first feature being "above", "above" and "above" a second feature includes that the first feature is directly above and obliquely above the second feature, or simply indicates that the first feature is higher in level than the second feature. A first feature being "below", "below" and "below" a second feature includes that the first feature is directly below and obliquely below the second feature, or simply indicates that the first feature is lower in level than the second feature.

[0028] In the description of this embodiment, the terms "upper", "lower", "left", "right" and other directions or positional relationships are based on the directions or positional relationships shown in the drawings, and are only for the convenience of description and simplified operation, rather than indicating or implying that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore cannot be understood as a limitation of the present invention. In addition, the terms "first" and "second" are only used to distinguish in the description and have no special meaning.

[0029] like Figure 1As shown, this embodiment provides a curved solar panel, which is a core component of a photovoltaic power generation system and is mainly used to convert light energy into electrical energy. In actual use, the shape of the curved solar panel is usually constructed as a single-peak arc surface or a multi-peak and trough arc surface, and the radius of the curved surface is approximately 30mm to 150mm, so that it can be better combined with the roof of the building, improving the overall aesthetics and breaking the dull and boring design of conventional flat solar panels.

[0030] Specifically, refer to Figure 1 The curved solar panel comprises a front panel layer 10, a first encapsulation film layer 20, a battery layer 30, a second encapsulation film layer 40 and a back panel layer 50 which are stacked in sequence. The front panel layer 10 is bonded to the front surface of the battery layer 30 through the first encapsulation film layer 20, and the back panel layer 50 is bonded to the back surface of the battery layer 30 through the second encapsulation film layer 40. The front surface of the battery layer 30 is the light-receiving surface, and the back surface of the battery layer 30 is the backlight surface. The front panel layer 10 and the back panel layer 50 are the outermost layers of the entire curved solar panel. The light-receiving surface of the battery layer 30 is protected by the front panel layer 10, and the backlight surface is protected by the back panel layer 50.

[0031] Among them, Figure 2 As shown, the front plate layer 10 includes a glass substrate 11 and an anti-reflection and anti-reflection film layer 12. The glass substrate 11 is bonded to the front surface of the battery layer 30 through the first packaging film layer 20. The anti-reflection and anti-reflection film layer 12 is plated on the surface of the glass substrate 11 away from the first packaging film layer 20 by magnetron sputtering technology. The glass substrate 11 is made of high-transmittance tempered glass or semi-tempered glass, which has good light transmission and impact resistance, and also provides fire retardant protection for the front of the battery layer 30.

[0032] In the prior art, the coating process for flat glass substrates is relatively mature. However, for the curved glass substrate 11, after hot bending, the bent portion cannot form a vertical state with the sputtering target, and there will be uneven temperature control and heating, resulting in uneven thickness and color of the curved coating layer. For the coating layer of a single material, the uneven thickness and color will lead to higher reflectivity and lower transmittance. Therefore, it is necessary to use a correction plate to correct the coating thickness to achieve consistency in the reflection color of the coating on the low-curvature glass substrate 11, thus causing problems such as low production efficiency.

[0033] In order to solve the above problems, in this embodiment, the anti-reflection and anti-reflection film layer 12 is configured to absorb sunlight of multiple bands. Specifically, the anti-reflection and anti-reflection film layer 12 includes multiple metal oxides, and different metal oxides can absorb sunlight of different bands. Therefore, by utilizing the different crystal structures of different metal oxides to absorb sunlight of different bands, the effect of anti-reflection and anti-reflection can be achieved, which greatly improves the light transmittance of the curved front plate layer 10 and improves the power generation efficiency of the curved solar module. Therefore, after coating, there is no need to use a correction plate to correct the film thickness to achieve the consistency of the reflection color of the low-curvature glass substrate 11 coating, so that the purpose of reducing reflectivity and improving light transmittance can be achieved, thereby improving production efficiency.

[0034] In one embodiment, the anti-reflection and anti-reflection film layer 12 is a nano-composite film layer, including nano ZnO particles, nano SiO2 particles and nano TiO2 particles. The nano ZnO particles, nano SiO2 particles and nano TiO2 particles are doped to form the anti-reflection and anti-reflection film layer 12. Different metal oxides have different crystal structures and can absorb sunlight of different wavelengths. In actual operation, these three oxides are mixed in a certain ratio and then plated on the glass substrate 11 by magnetron sputtering technology, so that particles of each metal oxide can be formed on the surface of the glass substrate 11.

[0035] In the anti-reflection and anti-reflection film layer 12 formed in this way, the uniformity of various metal oxides is good. It has been verified that the transmittance of the anti-reflection and anti-reflection film layer 12 can reach 97% to 98%, and the power generation efficiency of the curved solar module can be increased by 3% to 6%. Therefore, after coating, there is no need to use a correction plate to correct the film thickness to achieve the consistency of the coating reflection color of the low-curvature glass substrate 11, which can achieve the purpose of reducing reflectivity and increasing transmittance, thereby improving production efficiency. In addition, this anti-reflection and anti-reflection film layer 12 has good adhesion and high friction resistance, which can play a certain protective role on the glass substrate 11 and the entire curved solar module, and can also absorb part of the solar heat energy, and conduct heat and dissipate heat through molecular vibration to reduce the thermal attenuation of the curved solar module, reduce the generation of hot spots, and extend the service life of the module by 5 to 8 years. In other embodiments, the anti-reflection and anti-reflection film layer 12 can also be formed by doping with a variety of other different nano metal oxide particles, as long as the effect of anti-reflection and anti-reflection can be achieved, and no specific limitation is made here.

[0036] It should be noted that the anti-reflection and anti-reflection film layer 12 formed by mixing multiple metal oxides is a prior art. For example, in the prior art with publication number CN204066058U, it is disclosed that the materials of the first anti-reflection layer and the second anti-reflection layer are both a mixture of silicon oxide and niobium oxide, so that the transmittance of the sapphire touch screen is higher; for example, in the prior art with publication number CN201000491Y, it is disclosed that one side of the glass substrate is covered with a multi-layer anti-reflection film, and the multi-layer anti-reflection film sequentially includes a medium refractive index film layer, a high refractive index film layer and a low refractive index film layer, the medium refractive index film material is a medium refractive index mixed oxide material, and the high refractive index film material is a high refractive index mixed oxide material, so as to increase the transmittance of the lens; for example, in the prior art with publication number CN110655331B, it is disclosed that the glass coating liquid includes a nano-dispersion liquid A and a nano-dispersion liquid B, and the one-dimensional nano-inorganic nano-dispersion liquid A in the nano-dispersion liquid The particles include at least one of needle-shaped nano-SiO2, needle-shaped nano-TiO2, nano-ZnO whiskers, nano-hydroxyapatite, nano-needle-shaped silicon carbide and nano-silver wires. The spherical or quasi-spherical nano-particles in the nano-dispersion liquid B are at least one of nano-SiO2, anatase-type nano-TiO2, nano-ZrO2, nano-MgO, nano-aluminum-doped zinc oxide AZO and nano-γAl2O3. The nano-dispersion liquid A and the nano-dispersion liquid B are respectively coated on the surface of the quartz glass to form a new anti-reflection functional film on the glass surface to increase the light transmittance of the glass. For example, the prior art with the publication number CN101308878A1 discloses a solar cell encapsulation glass, including a glass substrate and a light anti-reflection film layer, the light anti-reflection film layer contains one or two components of oxide SiO2 and TiO2, thereby increasing the light transmittance of the glass substrate and the power of the solar cell encapsulation component.

[0037] It can be seen that the anti-reflection and anti-reflection film layer 12 and its components are all known materials. The present application does not improve the material of the anti-reflection and anti-reflection film layer 12 itself, but only applies the existing anti-reflection and anti-reflection film layer 12 formed by mixing multiple metal oxides to the curved glass substrate 11, so as to achieve the consistency of the coating reflection color of the low-curvature glass substrate 11 without using a correction plate to correct the film thickness after coating, thereby improving the purpose of production efficiency.

[0038] Preferably, the particle sizes of the nano ZnO particles, nano SiO2 particles and nano TiO2 particles are all 10nm to 30nm. It is understandable that if the particle size of each nano metal oxide is too small, the magnetron sputtering technology is not easy to implement, and if the particle size of each nano metal oxide is too large, the light transmission effect is not good. Therefore, by setting the particle size of each nano metal oxide within the above reasonable range, the light transmission effect of the anti-reflection and anti-reflection film layer 12 can be guaranteed while ensuring that the magnetron sputtering technology can be implemented.

[0039] Preferably, the thickness of the anti-reflection and anti-reflection film layer 12 is 100 nm to 200 nm. Therefore, setting the thickness of the anti-reflection and anti-reflection film layer 12 within the above reasonable range can ensure a good light transmission effect of the anti-reflection and anti-reflection film layer 12.

[0040] In another embodiment, the anti-reflection and anti-reflection film layer 12 includes a stacked ZnO film layer, a SiO2 film layer and a TiO2 film layer. In actual operation, the corresponding metal oxides are sequentially plated on the glass substrate 11 by magnetron sputtering technology to form each metal oxide film layer, and each metal oxide film layer is composed of corresponding metal oxide particles, so different metal oxide layers can absorb sunlight of different bands. This form of anti-reflection and anti-reflection film layer 12 can also improve the transmittance, thereby improving the power generation efficiency of the curved solar module. Therefore, after coating, there is no need to use a correction plate to correct the film thickness to achieve the consistency of the reflection color of the low-curvature glass substrate 11, so as to achieve the purpose of reducing reflectivity and improving transmittance, thereby improving production efficiency. Among them, the order of each metal oxide film layer is not specifically limited here, and can be flexibly set according to actual needs. In other embodiments, the anti-reflection and anti-reflection film layer 12 can also be formed by stacking a variety of other different metal oxide film layers, as long as the effect of anti-reflection and anti-reflection can be achieved, and no specific limitation is made here.

[0041] Furthermore, the front plate layer 10 further includes an anti-fouling film layer 13, which covers the surface of the anti-reflection and anti-reflection film layer 12 away from the glass substrate 11. The anti-fouling film layer 13 has a hydrophobic and dustproof effect, so that dust on the surface of the front plate layer 10 cannot adhere, thereby making the surface of the front plate layer 10 have a hydrophobic, anti-fouling and self-cleaning function.

[0042] Optionally, the material of the antifouling film layer 13 is diluted to 3‰ to 8‰ wt by a fluorocarbon solvent or silicone oil to ensure a good hydrophobic and dustproof effect, and is sprayed onto the surface of the anti-reflection and anti-reflection film layer 12 by a spray gun, and baked at a temperature of 100°C to 150°C for 30min to 60min to obtain the antifouling film layer 13. Exemplarily, the material of the antifouling film layer 13 can be a fluorine-containing silane polymer, or other materials can be used, as long as the formed film layer has a hydrophobic and dustproof effect, and no specific limitation is made here.

[0043] Preferably, the thickness of the antifouling film layer 13 is 80 nm to 150 nm. By setting the thickness of the antifouling film layer 13 within the above range, the antifouling film layer 13 can ensure a good hydrophobic and dustproof effect.

[0044] Furthermore, the first encapsulation film layer 20 and the second encapsulation film layer 40 are both hot melt adhesives, and each film layer can be melted and cross-linked during the lamination process of the curved solar module, so as to bond the above-mentioned layers of materials into one, and each film layer needs to have good light transmittance, weather resistance and bonding properties.

[0045] In order to achieve the above functions, illustratively, the first encapsulation film layer 20 can be selected as one of high-cutoff EVA film, POE film, EPE film, and PVB film, and the thickness is preferably 0.3mm to 0.8mm. In this way, the first encapsulation film layer 20 can also effectively cut off ultraviolet rays to prevent the battery layer 30 from being damaged by ultraviolet rays. The second encapsulation film layer 40 can be selected as one of highly transparent EVA film, POE film, EPE film, and PVB film, and the thickness is preferably 0.3mm to 0.8mm. Of course, in other embodiments, the first encapsulation film layer 20 and the second encapsulation film layer 40 can also use other types of films as long as the above effects can be achieved.

[0046] The battery layer 30 is composed of a plurality of crystalline silicon battery cells. The battery layer 30 preferably uses a battery cell having no grid lines on the light-receiving surface and with positive and negative metal electrodes extending from the backlight surface, such as an XBC battery, an MWT battery, or a shingled battery.

[0047] The backplane layer 50 is used as a protective layer for the backlight surface of the battery layer 30 and is made of a flexible polymer backplane material, preferably PET, CPC or glass fiber composite material, and preferably has a thickness of 0.3 mm to 0.7 mm. The backplane layer 50 made of the above material has waterproof and weather-resistant properties, thereby providing good protection for the backlight surface of the battery layer 30. Of course, in other embodiments, the backplane layer 50 can also be made of other materials as long as the above effects can be achieved.

[0048] Obviously, the above embodiments of the present invention are merely examples for clearly illustrating the present invention, and are not intended to limit the implementation methods of the present invention. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all implementation methods here. Any modifications, equivalent substitutions, and improvements made within the spirit and principles of the present invention shall be included in the protection scope of the claims of the present invention.

Claims

1. A curved solar panel, characterized in that: It comprises a front plate layer, a first packaging film layer, a battery layer, a second packaging film layer and a back plate layer which are stacked in sequence, wherein the back plate layer is bonded to the back of the battery layer through the second packaging film layer; The front panel layer includes a glass substrate and an anti-reflection and anti-reflection film layer. The glass substrate is bonded to the front side of the battery layer through the first packaging film layer. The anti-reflection and anti-reflection film layer is plated on the surface of the glass substrate away from the first packaging film layer. The anti-reflection and anti-reflection film layer can absorb sunlight in multiple bands.

2. The curved solar panel according to claim 1, characterized in that: The anti-reflection and anti-reflection film layer comprises a stacked ZnO film layer, a SiO2 film layer and a TiO2 film layer.

3. The curved solar panel according to any one of claims 1 to 2, characterized in that: The thickness of the anti-reflection and anti-reflection film layer is 100nm-200nm.

4. The curved solar panel according to any one of claims 1 to 2, characterized in that: The front plate layer further comprises an anti-fouling film layer, and the anti-fouling film layer is arranged on a surface of the anti-reflection and anti-reflection film layer away from the glass substrate.

5. The curved solar panel according to claim 4, characterized in that: The material of the antifouling film layer is diluted to 3‰ to 8‰ wt by fluorocarbon solvent or silicone oil.

6. The curved solar panel according to claim 4, characterized in that: The thickness of the antifouling film layer is 80nm-150nm.

7. The curved solar panel according to any one of claims 1 to 2, characterized in that: The first encapsulation film layer is one of high-cutoff EVA film, POE film, EPE film, and PVB film; And / or the second encapsulation film layer is one of highly transparent EVA film, POE film, EPE film and PVB film.

8. The curved solar panel according to any one of claims 1 to 2, characterized in that: The backboard layer is made of PET, CPC or glass fiber composite material.

Citation Information

Cited By

  • Curved surface photovoltaic module and application thereof

    CN121057302A

  • Curved photovoltaic module

    WO2025180080A1