Continuous annealing device for molybdenum wire

By designing a molybdenum wire annealing device including annealing box, through-hole, winding mechanism and continuous annealing mechanism, the problem of uneven heat received by the molybdenum wire during the annealing process is solved, and better annealing effect and reduced oxidation effect are achieved. .

CN222499239UActive Publication Date: 2025-02-18JIANG SU DONG PU WU MU ZHI PIN YOU XIAN ZE REN GONG SI
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202421111908.5
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-05-21
Publication Date
2025-02-18
Estimated Expiration
2034-05-21

Smart Images

  • Figure CN222499239U_ABST
    Figure CN222499239U_ABST
Patent Text Reader

Abstract

The utility model discloses a continuous annealing device for molybdenum wires, which relates to the technical field of molybdenum wire annealing and comprises an annealing box, two sides of the annealing box are provided with through holes, the top of the annealing box is fixedly provided with an air inlet, two sides of the annealing box are provided with winding mechanisms, and a continuous annealing mechanism is arranged in the annealing box. The continuous annealing mechanism comprises a fixed cylinder, a heating wire, a conveying cylinder and a pressing cylinder; according to the technical scheme provided by the utility model, the continuous annealing mechanism is adopted, and the first notch and the second notch are arranged, so that the molybdenum wire can be temporarily cooled at the positions of the first notch and the second notch, and then the next annealing is carried out, so that the molybdenum wire is more uniform during continuous annealing; by arranging the conveying cylinder and the pressing cylinder, the molybdenum wire can be always located at the center of the fixing cylinder in the annealing process, so that the molybdenum wire can be heated more uniformly during annealing, and the annealing effect of the molybdenum wire is better.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of molybdenum wire annealing, in particular to a continuous annealing device for molybdenum wire. Background Art

[0002] In the existing technology, after multiple stretching processes, the deformation resistance of molybdenum wire increases and the plasticity decreases due to work hardening, so it must be annealed to eliminate internal stress and improve its processing performance. There are three annealing methods currently used: one is intermittent annealing under hydrogen protection, using a box-type muffle electric furnace, and the coiled molybdenum wire is placed in the furnace for a certain period of time and then taken out; the other is continuous annealing under hydrogen protection, using a corundum tube electric furnace for indirect heating; and the other is continuous oxidation annealing using natural gas or liquefied gas for direct heating.

[0003] The conventional continuous annealing device for molybdenum wire cannot ensure that the molybdenum wire is heated evenly during the annealing process and cannot perform continuous annealing evenly, resulting in poor annealing effect of the molybdenum wire. Utility Model Content

[0004] The technical problem to be solved by the utility model is to overcome the shortcomings of the prior art and provide a continuous annealing device for molybdenum wire, so as to solve the problem that the prior art cannot better ensure that the molybdenum wire is heated evenly during the annealing process and the continuous annealing is performed evenly, resulting in poor annealing effect of the molybdenum wire.

[0005] In view of this, the utility model provides a continuous annealing device for molybdenum wire, comprising an annealing box, through holes are opened on both sides of the annealing box, an air inlet is fixedly installed on the top of the annealing box, winding mechanisms are arranged on both sides of the annealing box, and a continuous annealing mechanism is arranged inside the annealing box;

[0006] The continuous annealing mechanism includes a fixed cylinder, a heating wire, a conveying cylinder and a pressing cylinder. The fixed cylinder is fixedly installed on the inner wall of the annealing box, the fixed cylinder is connected to the through hole, a plurality of first notches are opened on the top of the fixed cylinder, a plurality of second notches corresponding to the first notches are opened on the bottom of the fixed cylinder, a heating wire is fixedly installed on the inner wall of the fixed cylinder, the conveying cylinder is rotatably connected to the inside of the annealing box, the conveying cylinder is located in the second notch, the pressing cylinder is located in the first notch, and a groove is opened on the side wall of the conveying cylinder.

[0007] Optionally, the heating wire is located between a plurality of the first notches and a plurality of the second notches.

[0008] Optionally, a transmission device is fixedly mounted on the side wall of the annealing box, and the conveying cylinder is fixedly mounted on the connecting end of the transmission device.

[0009] Optionally, a mounting frame is fixedly mounted on the top of the inner wall of the annealing box, a movable frame is slidably connected to the inside of the mounting frame via a spring, and the pressing cylinder is rotatably connected to the bottom end of the movable frame.

[0010] Optionally, a plurality of anti-slip parts are fixedly installed inside the groove.

[0011] Optionally, the winding mechanism includes a fixed frame and a winding disk, the fixed frame is fixedly installed at one end of the annealing box, a slot is opened at one end of the fixed frame, and the winding disk is rotatably connected to the inside of the slot through a torsion spring.

[0012] Optionally, a plurality of sealing members are fixedly installed inside the through hole.

[0013] It can be seen from the above technical solutions that the embodiments of the utility model have the following advantages:

[0014] 1. The utility model is a continuous annealing device for molybdenum wire, which adopts a continuous annealing mechanism. By setting a first notch and a second notch, the molybdenum wire can be briefly cooled at the position of the first notch and the second notch, and then the next annealing is performed, so that the molybdenum wire is more uniform during continuous annealing. By setting a conveying cylinder and a pressing cylinder, the molybdenum wire can always be located at the center of the fixed cylinder during the annealing process, thereby ensuring that the molybdenum wire is heated more evenly during annealing, and the annealing effect of the molybdenum wire is better.

[0015] 2. The utility model is a continuous annealing device for molybdenum wire, which adopts a sealing design. Such a design can ensure the sealing effect inside the annealing box and reduce the oxidation of the molybdenum wire during the annealing process.

[0016] These features and advantages of the present invention will be disclosed in detail in the following specific implementation manners and drawings. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] The utility model is further described below in conjunction with the accompanying drawings:

[0018] Figure 1 It is a schematic diagram of the structure of the utility model;

[0019] Figure 2 For this utility model Figure 1 The enlarged structural diagram at A in the middle;

[0020] Figure 3 This is a schematic diagram of the local structure of the fixed cylinder of the utility model;

[0021] Figure 4 It is a partial cross-sectional structural schematic diagram of the annealing box of the utility model;

[0022] Figure 5 This is a schematic diagram of the structure of the conveying tube of the utility model.

[0023] Explanation of the reference numerals: 1, annealing box; 2, through hole; 3, transmission device; 4, air inlet; 5, fixed frame; 6, slot; 7, winding disk; 8, sealing member; 9, fixed cylinder; 10, first notch; 11, second notch; 12, heating wire; 13, conveying cylinder; 14, groove; 15, anti-slip member; 16, mounting frame; 17, movable frame; 18, pressing cylinder. DETAILED DESCRIPTION

[0024] The following is an explanation and description of the technical scheme of the embodiment of the utility model in conjunction with the drawings of the embodiment of the utility model, but the following embodiment is only a preferred embodiment of the utility model, not all. Based on the embodiment in the implementation mode, other embodiments obtained by those skilled in the art without creative work are all within the protection scope of the utility model.

[0025] A continuous annealing device for molybdenum wire according to an embodiment of the utility model will be described in detail below with reference to the accompanying drawings.

[0026] Example 1

[0027] For easier understanding, see Figures 1 to 5 The utility model provides an embodiment of a continuous annealing device for molybdenum wire, comprising an annealing box 1, through holes 2 are opened on both sides of the annealing box 1, an air inlet 4 is fixedly installed on the top of the annealing box 1, winding mechanisms are arranged on both sides of the annealing box 1, and a continuous annealing mechanism is arranged inside the annealing box 1;

[0028] The continuous annealing mechanism includes a fixed cylinder 9, a heating wire 12, a conveying cylinder 13 and a pressing cylinder 18. The fixed cylinder 9 is fixedly installed on the inner wall of the annealing box 1, the fixed cylinder 9 is connected to the through hole 2, a plurality of first notches 10 are opened on the top of the fixed cylinder 9, a plurality of second notches 11 corresponding to the first notches 10 are opened on the bottom of the fixed cylinder 9, a heating wire 12 is fixedly installed on the inner wall of the fixed cylinder 9, the conveying cylinder 13 is rotatably connected to the inside of the annealing box 1, the conveying cylinder 13 is located inside the second notch 11, the pressing cylinder 18 is located inside the first notch 10, a groove 14 is opened on the side wall of the conveying cylinder 13, and a plurality of anti-slip parts 15 are fixedly installed inside the groove 14.

[0029] It should be noted that, by providing the anti-slip part 15, it is easier to transport the molybdenum wire. By providing the through hole 2, the molybdenum wire can be delivered to the fixed cylinder 9 inside the annealing box 1 and then transmitted out from the through hole 2 at the other end. By providing the air inlet 4, nitrogen or helium can be delivered to the inside of the annealing box 1 to reduce oxidation of the molybdenum wire during annealing. By providing the first notch 10 and the second notch 11, the molybdenum wire can be briefly cooled at the position of the first notch 10 and the second notch 11, and then the next annealing can be carried out, so that the continuous annealing of the molybdenum wire is more uniform. By providing the conveying cylinder 13 and the pressing cylinder 18, the molybdenum wire can always be located at the center of the fixed cylinder 9 during the annealing process, thereby ensuring that the molybdenum wire is heated more evenly during annealing, so that the annealing effect of the molybdenum wire is better.

[0030] In some embodiments, Figure 3 As shown, the heating wire 12 is located between a plurality of first slots 10 and a plurality of second slots 11 .

[0031] In some embodiments, Figure 1 As shown, a transmission device 3 is fixedly installed on the side wall of the annealing box 1, a conveying cylinder 13 is fixedly installed on the connecting end of the transmission device 3, a mounting frame 16 is fixedly installed on the top of the inner wall of the annealing box 1, a movable frame 17 is slidably connected to the inside of the mounting frame 16 through a spring, and a pressing cylinder 18 is rotatably connected to the bottom end of the movable frame 17.

[0032] It should be noted that the transmission device 3 is composed of a servo motor, a plurality of transmission gears and a transmission belt. The connection end is arranged on one side of the transmission gear. The servo motor is operated in conjunction with the transmission belt to drive the transmission gear to rotate, so that the conveying cylinder 13 rotates inside the annealing box 1. By setting a spring, the pressing cylinder 18 can be pressed downward to make the molybdenum wire easier to be conveyed.

[0033] In some embodiments, Figure 1 As shown, the winding mechanism includes a fixed frame 5 and a winding disk 7. The fixed frame 5 is fixedly installed at one end of the annealing box 1. A slot 6 is opened at one end of the fixed frame 5. The winding disk 7 is rotatably connected to the inside of the slot 6 through a torsion spring.

[0034] It should be noted that by arranging winding reels 7 on both sides of the annealing box 1, one of them can be used to wind up the unannealed molybdenum wire, and the other can be used to wind up the annealed molybdenum wire. By arranging a card slot 6 to install the winding reel 7, the installation and disassembly of the winding reel 7 can be more convenient.

[0035] Example 2

[0036] In some embodiments, Figure 5 As shown, a plurality of sealing members 8 are fixedly installed inside the through hole 2 .

[0037] It should be noted that, by arranging a plurality of sealing members 8 inside the through hole 2, the sealing effect inside the annealing box 1 can be ensured, thereby reducing the oxidation of the molybdenum wire during the annealing process.

[0038] The heating wire 12 in the present invention is a well-known component and will not be described in detail here.

[0039] Working principle: When in use, place the winding reel 7 with molybdenum wire in the internal slot 6 of the fixed frame 5 on one side of the annealing box 1, insert the molybdenum wire into the through hole 2 on one side, drive the conveying cylinder 13 to rotate through the transmission device 3 to cooperate with the pressing cylinder 18 to move the molybdenum wire in the center of the fixed cylinder 9, and heat and temper the molybdenum wire through the heating wire 12 inside the fixed cylinder 9. By setting the first notch 10 and the second notch 11, the molybdenum wire can be briefly cooled at the position of the first notch 10 and the second notch 11, and then the next annealing is carried out, so that the molybdenum wire is more uniform during continuous annealing, and then it is transmitted from the through hole 2 on the other side and wound on the side wall of the other winding reel 7 to complete the annealing.

[0040] As described above, the above embodiments are only used to illustrate the technical solutions of the present application, rather than to limit them. Although the present application has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present application.

Claims

1. A continuous annealing device for molybdenum wire, characterized in that: It comprises an annealing box (1), both sides of the annealing box (1) are provided with through holes (2), the top of the annealing box (1) is fixedly provided with an air inlet (4), both sides of the annealing box (1) are provided with a winding mechanism, and a continuous annealing mechanism is provided inside the annealing box (1); The continuous annealing mechanism comprises a fixed cylinder (9), a heating wire (12), a conveying cylinder (13) and a pressing cylinder (18); the fixed cylinder (9) is fixedly mounted on the inner wall of the annealing box (1); the fixed cylinder (9) is in communication with the through hole (2); a plurality of first notches (10) are provided on the top of the fixed cylinder (9); a plurality of second notches (11) corresponding to the first notches (10) are provided on the bottom of the fixed cylinder (9); a heating wire (12) is fixedly mounted on the inner wall of the fixed cylinder (9); the conveying cylinder (13) is rotatably connected to the inside of the annealing box (1); the conveying cylinder (13) is located inside the second notches (11); the pressing cylinder (18) is located inside the first notches (10); and a groove (14) is provided on the side wall of the conveying cylinder (13).

2. A continuous annealing device for molybdenum wire according to claim 1, characterized in that: The heating wire (12) is located between a plurality of the first notches (10) and a plurality of the second notches (11).

3. A continuous annealing device for molybdenum wire according to claim 1, characterized in that: A transmission device (3) is fixedly mounted on the side wall of the annealing box (1), and the conveying cylinder (13) is fixedly mounted on the connecting end of the transmission device (3).

4. A continuous annealing device for molybdenum wire according to claim 1, characterized in that: A mounting frame (16) is fixedly mounted on the top of the inner wall of the annealing box (1), a movable frame (17) is slidably connected to the inside of the mounting frame (16) via a spring, and the pressing cylinder (18) is rotatably connected to the bottom end of the movable frame (17).

5. A continuous annealing device for molybdenum wire according to claim 1, characterized in that: A plurality of anti-slip parts (15) are fixedly installed inside the groove (14).

6. A continuous annealing device for molybdenum wire according to claim 1, characterized in that: The winding mechanism comprises a fixed frame (5) and a winding disk (7); the fixed frame (5) is fixedly mounted on one end of the annealing box (1); a clamping slot (6) is provided at one end of the fixed frame (5); and the winding disk (7) is rotatably connected to the inside of the clamping slot (6) via a torsion spring.

7. A continuous annealing device for molybdenum wire according to claim 1, characterized in that: A plurality of sealing members (8) are fixedly installed inside the through hole (2).