Release film easy to peel

By adopting a multi-layer structure in the release film and bonding the heat-insulating patch on the outside of each adhesive layer, the problem of unstable structure of the existing release film after heating is solved, and a higher service life is achieved. stability.

CN222524440UActive Publication Date: 2025-02-25KUNSHAN ZHONGDATIANBAO AUXILIARY MATERIAL CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420283096.6
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-02-06
Publication Date
2025-02-25
Estimated Expiration
2034-02-06

AI Technical Summary

Technical Problem

The existing release film is prone to overflow after being heated, resulting in unstable structure and low service life.

Method used

An ultra-easy peeling release film is designed, adopting a multi-layer structure, in which an insulating patch is bonded to the outside of each adhesive layer to prevent the overflow of the adhesive layer and improve structural stability.

Benefits of technology

It effectively reduces the probability of product deformation, prevents gaps between levels, and improves the stability and service life of the overall structure.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

The utility model discloses a release film easy to peel off. The release film comprises a diaphragm module, the membrane module comprises an anti-static layer, a first adhesive layer smeared at the bottom of the anti-static layer, a buffer layer bonded to the bottom of the first adhesive layer, a second adhesive layer smeared at the bottom of the buffer layer, a release layer bonded to the bottom of the second adhesive layer and a third adhesive layer smeared at the bottom of the release layer. The temperature-resistant layer is adhered to the bottom of the third adhesive layer, the fourth adhesive layer is applied to the bottom of the temperature-resistant layer, and the scratch-resistant layer is adhered to the bottom of the fourth adhesive layer. According to the utility model, once a heating phenomenon occurs, the first adhesive layer, the second adhesive layer, the third adhesive layer and the fourth adhesive layer in a molten state can be blocked by the heat insulation paste, so that the deformation probability of the product is effectively reduced, gaps are prevented from being formed among the layers, the stability of the whole structure is improved, and the service life is ensured.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of release films, in particular to a super easy to peel release film. Background Art

[0002] A release film refers to a film with a distinguishable surface. The release film has no stickiness or is slightly sticky when in contact with specific materials under limited conditions.

[0003] Release films are mostly made of multi-layer structures. The viscose, which is the key component, is easy to overflow from the release film once heated, resulting in an unstable structure of the release film and a short service life. Utility Model Content

[0004] The utility model aims to solve one of the technical problems existing in the prior art or related technology.

[0005] To this end, the technical solution adopted in this utility model is:

[0006] A super easy-to-peel release film comprises a diaphragm module, wherein the diaphragm module comprises an antistatic layer, a first adhesive layer applied to the bottom of the antistatic layer, a buffer layer bonded to the bottom of the first adhesive layer, a second adhesive layer applied to the bottom of the buffer layer, a release layer bonded to the bottom of the second adhesive layer, a third adhesive layer applied to the bottom of the release layer, a heat-resistant layer bonded to the bottom of the third adhesive layer, a fourth adhesive layer applied to the bottom of the heat-resistant layer, and a scratch-resistant layer bonded to the bottom of the fourth adhesive layer, and thermal insulation stickers are bonded to the outer sides of the first adhesive layer, the second adhesive layer, the third adhesive layer, and the fourth adhesive layer.

[0007] By adopting the above technical solution, once heat occurs, the melted first adhesive layer, second adhesive layer, third adhesive layer and fourth adhesive layer will be blocked by the thermal insulation tape, which effectively reduces the deformation probability of the product and prevents gaps between the layers, thereby improving the stability of the overall structure and ensuring the service life.

[0008] In a preferred example, the utility model can be further configured as follows: the antistatic layer is a composite of resin and antistatic agent.

[0009] In a preferred example, the present invention can be further configured as follows: the first adhesive layer, the second adhesive layer, the third adhesive layer, and the fourth adhesive layer have equal thickness and are made of the same material.

[0010] In a preferred example, the present invention can be further configured as follows: the buffer layer is made of rubber material.

[0011] In a preferred example, the present invention can be further configured as follows: the scratch-resistant layer is a polyester film.

[0012] In a preferred example, the utility model can be further configured as follows: a plurality of thermal insulation stickers are arranged in four groups, and the four thermal insulation stickers in each group are arranged in a matrix.

[0013] By adopting the above technical solution, the beneficial effects achieved by the utility model are as follows:

[0014] 1. In the utility model, once heat occurs, the melted first adhesive layer, second adhesive layer, third adhesive layer and fourth adhesive layer will be blocked by the heat insulation sticker, which effectively reduces the deformation probability of the product and prevents gaps between the layers, thereby improving the stability of the overall structure and ensuring the service life. BRIEF DESCRIPTION OF THE DRAWINGS

[0015] Figure 1 It is a three-dimensional diagram of the overall structure of the utility model;

[0016] Figure 2 This is a schematic diagram of the overall structure of the utility model when the antistatic layer is uncovered;

[0017] Figure 3 It is a left sectional view of the overall structure of the utility model.

[0018] Reference numerals:

[0019] 100, diaphragm module; 110, antistatic layer; 120, first adhesive layer; 130, buffer layer; 140, second adhesive layer; 150, release layer; 160, third adhesive layer; 170, temperature-resistant layer; 180, fourth adhesive layer; 190, scratch-resistant layer; 191, thermal insulation film. DETAILED DESCRIPTION

[0020] In order to make the purpose, technical solution and advantages of the utility model clearer, the utility model is further described in detail below in combination with specific implementation methods and with reference to the accompanying drawings. It should be noted that the embodiments of the utility model and the features in the embodiments can be combined with each other without conflict.

[0021] It should be understood that these descriptions are exemplary only and are not intended to limit the scope of the present invention.

[0022] The following describes an ultra-easy-to-peel release film provided by some embodiments of the present invention in conjunction with the accompanying drawings.

[0023] Embodiment 1:

[0024] Combination Figure 1-3As shown, the utility model provides an ultra-easy-to-peel release film, including a diaphragm module 100, wherein the diaphragm module 100 includes an antistatic layer 110, a first adhesive layer 120 applied to the bottom of the antistatic layer 110, a buffer layer 130 bonded to the bottom of the first adhesive layer 120, a second adhesive layer 140 applied to the bottom of the buffer layer 130, a release layer 150 bonded to the bottom of the second adhesive layer 140, a third adhesive layer 160 applied to the bottom of the release layer 150, a heat-resistant layer 170 bonded to the bottom of the third adhesive layer 160, a fourth adhesive layer 180 applied to the bottom of the heat-resistant layer 170, and a scratch-resistant layer 190 bonded to the bottom of the fourth adhesive layer 180, and a heat insulation sticker 191 is bonded to the outer side of the first adhesive layer 120, the outer side of the second adhesive layer 140, the outer side of the third adhesive layer 160, and the outer side of the fourth adhesive layer 180.

[0025] Furthermore, the antistatic layer 110 is a composite of resin and antistatic agent, and the antistatic layer 110 effectively solves the dust contamination problem caused by static electricity.

[0026] Furthermore, the first adhesive layer 120 , the second adhesive layer 140 , the third adhesive layer 160 , and the fourth adhesive layer 180 are of equal thickness and made of the same material. This structural design reduces the difficulty of manufacturing the product.

[0027] Furthermore, the buffer layer 130 is made of rubber material, and the buffer layer 130 can reduce the probability of damage to the product.

[0028] Embodiment 2:

[0029] Combination Figure 1-3 As shown, on the basis of the first embodiment, the scratch-resistant layer 190 is a polyester film, and the scratch-resistant layer 190 can ensure the aesthetics of the surface of the product and also ensure its service life.

[0030] Embodiment three:

[0031] Combination Figure 1-3 As shown, in the above embodiment, a plurality of thermal insulation stickers 191 are arranged into four groups of four, and the four thermal insulation stickers 191 in each group are arranged in a matrix. This structural design can effectively prevent the first adhesive layer 120, the second adhesive layer 140, the third adhesive layer 160, and the fourth adhesive layer 180 from overflowing, thereby improving the structural stability of the product.

[0032] The working principle and use process of the utility model: when the product is put into actual use, once heat occurs, the melted first adhesive layer 120, the second adhesive layer 140, the third adhesive layer 160, and the fourth adhesive layer 180 will be blocked by the heat insulation sticker 191, which effectively reduces the deformation probability of the product and prevents gaps between the layers, thereby improving the stability of the overall structure and ensuring the service life.

[0033] In the present utility model, the term "plurality" refers to two or more than two, unless otherwise clearly defined. The term "and / or" used in this article includes any and all combinations of one or more related listed items. The terms "install", "connect", "connect", "fix" and the like should be understood in a broad sense. For example, "connection" can be a fixed connection, a detachable connection, or an integral connection; "connection" can be a direct connection or an indirect connection through an intermediate medium. For those of ordinary skill in the art, the specific meanings of the above terms in the present utility model can be understood according to the specific circumstances.

[0034] It should be noted that when an element is referred to as being "assembled on", "installed on", "fixed on" or "disposed on" another element, it may be directly on the other element or there may be a central element. When an element is considered to be "connected to" another element, it may be directly connected to the other element or there may be a central element at the same time. The terms "vertical", "horizontal", "upper", "lower", "left", "right" and similar expressions used herein are for illustrative purposes only and do not represent the only implementation method.

[0035] In the description of this specification, the description of the terms "one embodiment", "some embodiments", "specific embodiments", etc. means that the specific features, structures, materials or characteristics described in conjunction with the embodiment or example are included in at least one embodiment or example of the utility model. In this specification, the schematic representation of the above terms does not necessarily refer to the same embodiment or example. Moreover, the specific features, structures, materials or characteristics described can be combined in any one or more embodiments or examples in a suitable manner.

[0036] Although the embodiments of the present invention have been shown and described, those skilled in the art will appreciate that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the claims and their equivalents.

Claims

1. A super easy to peel release film, characterized in that: include: The diaphragm module (100) comprises an antistatic layer (110), a first adhesive layer (120) applied to the bottom of the antistatic layer (110), a buffer layer (130) bonded to the bottom of the first adhesive layer (120), a second adhesive layer (140) applied to the bottom of the buffer layer (130), a release layer (150) bonded to the bottom of the second adhesive layer (140), and a third adhesive layer (150) applied to the bottom of the release layer (150). 160), a heat-resistant layer (170) bonded to the bottom of the third adhesive layer (160), a fourth adhesive layer (180) applied to the bottom of the heat-resistant layer (170), and a scratch-resistant layer (190) bonded to the bottom of the fourth adhesive layer (180); and a heat-insulating sticker (191) is bonded to the outside of the first adhesive layer (120), the outside of the second adhesive layer (140), the outside of the third adhesive layer (160), and the outside of the fourth adhesive layer (180).

2. The ultra-easy peelable release film according to claim 1, characterized in that: The antistatic layer (110) is a composite of resin and antistatic agent.

3. The ultra-easy peelable release film according to claim 1, characterized in that: The first adhesive layer (120), the second adhesive layer (140), the third adhesive layer (160), and the fourth adhesive layer (180) have the same thickness and are made of the same material.

4. The ultra-easy peelable release film according to claim 1, characterized in that: The buffer layer (130) is made of rubber material.

5. The ultra-easy peelable release film according to claim 1, characterized in that: The scratch-resistant layer (190) is a polyester film.

6. The ultra-easy peelable release film according to claim 1, characterized in that: The plurality of thermal insulation stickers (191) are arranged in four groups, with four of them forming a group, and the four thermal insulation stickers (191) in each group are arranged in a matrix.