A Compressed Air Purging Device Based on SCR Catalyst Protection
By designing a compressed air purging device for the filter and heating components, the problems of ash accumulation, blockage, and activity decay of low-temperature SCR catalysts in high-humidity environments were solved, achieving effective protection and efficient operation of the catalyst.
Patent Information
- Application Number
- CN202522429755.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2025-11-17
- Publication Date
- 2026-11-10
- Estimated Expiration
- 2035-11-17
AI Technical Summary
Low-temperature SCR catalysts are susceptible to ash accumulation, blockage, activity decay, and chemical poisoning in low-temperature and high-humidity environments. Existing purging techniques can easily lead to a sudden drop in temperature or moisture-induced caking, making it difficult to effectively protect the catalyst's activity.
A compressed air purging device comprising a filtration component, a heating component, and a purging component was designed. It removes moisture through filtration, controls the temperature of the airflow, and combines a servo motor and an electric heating wire to achieve online desiccant regeneration, thereby preventing a sudden drop in catalyst temperature and moisture absorption and protecting catalyst activity.
It effectively prevents catalyst ash accumulation and blockage, as well as ammonium bisulfate condensation, maintains catalyst activity, improves unit operating efficiency, simplifies maintenance processes, and reduces downtime.
Smart Images

Figure CN224949907U_ABST
Abstract
Description
Technical Field
[0001] This utility model relates to the field of SCR denitrification technology, specifically a compressed air purging device based on SCR catalyst protection. Background Technology
[0002] SCR (Selective Catalytic Reduction) technology is currently the mainstream technology for controlling nitrogen oxide emissions. Low-temperature SCR technology (reaction temperature 160-220℃) is increasingly widely used due to its suitability for low-grade heat source scenarios (such as waste incineration flue gas and gas turbine exhaust). Its core component is the low-temperature SCR catalyst. However, in actual operation, the performance degradation of low-temperature SCR catalysts is more pronounced due to the influence of operating conditions. Accumulated ash blockage worsens: At a reaction temperature of 180℃, the humidity of flue gas is prone to increase (especially the humidity of waste incineration flue gas can reach 15%-25%). Dust easily combines with water vapor to form sticky ash, which adheres to the catalyst surface and pores. This not only blocks the active sites, but also causes the ash to harden due to the low temperature environment, making it significantly more difficult to clean than high temperature SCR systems. Low-temperature activity decay: The optimal activity temperature range of low-temperature SCR catalysts is narrow (180-200℃). When the flue gas temperature fluctuates below 160℃, the catalyst activity drops sharply. Moreover, at low temperatures, SO2 in the flue gas is easily converted into ammonium bisulfate (NH4HSO4), which adheres to the catalyst surface and forms "ammonium sulfate blockage", irreversibly destroying the active sites. Chemical poisoning risk: Under low-temperature conditions, alkali metals (Na, K) and heavy metals (Hg, P) in the flue gas are more likely to condense and adsorb on the catalyst surface, reacting with active components (such as MnO). X The reaction between CeO2 and CeO2 leads to catalyst poisoning and failure.
[0003] Existing catalyst protection methods have the following obvious shortcomings: 1. Traditional compressed air purging in low temperature and high humidity environments can easily cause a sudden drop in catalyst surface temperature (temperature difference > 20℃), leading to ammonium sulfate condensation; 2. Some technologies use steam purging, but this can easily cause the catalyst to become damp and caking.
[0004] Based on the above, a compressed air purging device based on SCR catalyst protection is invented. Utility Model Content
[0005] To solve the above-mentioned technical problems, this utility model provides the following technical solution: A compressed air purging device based on SCR catalyst protection includes a base plate, with side plates fixedly installed at both ends of the top of the base plate. A cylinder is provided between the two sets of side plates via a connecting assembly. The cylinder has several filter chambers, and filter assemblies are provided in the filter chambers to filter moisture in the steam. A first pipe is connected to one set of the connecting assembly. One end of the first pipe is fixedly connected to a second pipe via a multi-port connector. One end of the second pipe is connected to a purging assembly via a heating assembly.
[0006] As a preferred embodiment of the compressed air purging device based on SCR catalyst protection described in this utility model, the connecting assembly includes: The first rigid pipe is rotatably connected to the side plate via a bearing, and the first rigid pipe on the right side is fixedly connected to the first pipe via a rotary joint. The two sets of first rigid tubes are fixedly connected to each other by a multi-port connector, and one end of the L-shaped rigid tube is fixedly installed on the side of the cylinder and connected to the filter chamber.
[0007] As a preferred embodiment of the compressed air purging device based on SCR catalyst protection described in this utility model, the connecting assembly further includes: A servo motor, which is fixedly mounted on a set of side plates; The first gear is fixedly mounted on the output shaft of the servo motor via a connecting shaft; The second gear is fixedly mounted on a set of first rigid tubes, and the first gear and the second gear are meshed together.
[0008] As a preferred embodiment of the compressed air purging device based on SCR catalyst protection described in this utility model, the filter assembly includes: Arc-shaped plates are fixedly installed on the side of the cylinder by screws to seal the filter chamber. The box has several filter holes on its side wall. The box is fixedly installed on the inner side of the arc plate and inserted into the filter chamber.
[0009] As a preferred embodiment of the compressed air purging device based on SCR catalyst protection described in this utility model, the filter assembly further includes: Silica gel desiccant, which is filled in the box; A handle is fixedly mounted on the outer side of the arc-shaped plate.
[0010] As a preferred embodiment of the compressed air purging device based on SCR catalyst protection described in this utility model, the purging assembly includes: A purge pipe, wherein there are several purge pipes and the purge pipes are located above the catalyst layer; The nozzles are a plurality of nozzles arranged at an angle and fixedly installed at the bottom end of the purge pipe.
[0011] As a preferred embodiment of the compressed air purging device based on SCR catalyst protection described in this utility model, the heating component includes: The third rigid tube is fixedly installed on the top end of the purge tube, and the top end of the third rigid tube is fixedly connected to the second pipe. The electric heating wire is fixedly installed in a spiral arrangement within the inner cavity of the third rigid tube.
[0012] As a preferred embodiment of the compressed air purging device based on SCR catalyst protection described in this utility model, wherein: a second rigid pipe with a valve is fixedly installed on the side wall of the cylinder located on both sides of the filter chamber; a fan is fixedly installed in the inner cavity of one set of the second rigid pipes; and an electric heating wire is fixedly installed in the inner cavity of the other set of the second rigid pipes in a spiral arrangement.
[0013] Compared with existing technologies: By combining a filtration and heating assembly, the compressed air is dehydrated and its temperature controlled, preventing a sudden drop in catalyst temperature and caking caused by the purge airflow. This also prevents ammonium bisulfate from condensing and clogging, protecting the catalyst's active sites. Furthermore, the inclusion of a second rigid tube with a fan and electric heating wire on both sides of the cylinder enables online regeneration of the silica gel desiccant, eliminating the need for frequent disassembly and replacement and improving operational efficiency. Finally, the modular design of the arc-shaped plate and housing, along with the combination of handles and servo motors, allows for rapid desiccant replacement, facilitating maintenance and eliminating the need for downtime. Attached Figure Description
[0014] Figure 1 This is a front view schematic diagram of the structure of this utility model; Figure 2 This utility model Figure 1 Enlarged schematic diagram of the structure at point A in the middle; Figure 3 This is a side view of the cylinder and filter assembly of this utility model; Figure 4 This is a side view of the cylindrical body of this utility model; Figure 5 This is a front view schematic diagram of the heating component of this utility model; Figure 6 This is a top view of a plurality of purge tubes arranged according to the present invention; Figure 7 This is a cross-sectional schematic diagram of the second rigid tube of this utility model.
[0015] In the figure: base plate 10, side plate 11, first rigid tube 20, L-shaped rigid tube 21, servo motor 22, connecting shaft 23, first gear 24, second gear 25, cylinder 30, filter chamber 31, second rigid tube 32, arc plate 40, box 41, silica gel desiccant 42, handle 43, first pipe 50, second pipe 51, purge pipe 60, nozzle 61, third rigid tube 70, electric heating wire 71. Detailed Implementation
[0016] To make the objectives, technical solutions, and advantages of this utility model clearer, the embodiments of this utility model will be described in further detail below with reference to the accompanying drawings.
[0017] This invention provides a compressed air purging device based on SCR catalyst protection. Please refer to [link / reference]. Figures 1-7 The system includes a base plate 10, with side plates 11 fixedly installed at both ends of the top of the base plate 10. A cylinder 30 is provided between the two sets of side plates 11 via a connecting assembly. The cylinder 30 has a plurality of filter chambers 31, and filter assemblies are provided in the filter chambers 31 to filter moisture in the steam. A set of the connecting assembly is connected to a first pipe 50. One end of the first pipe 50 is fixedly connected to a second pipe 51 via a multi-port connector. One end of the second pipe 51 is connected to a purging assembly via a heating assembly.
[0018] The connecting assembly includes: a first rigid tube 20, an L-shaped rigid tube 21, a servo motor 22, a connecting shaft 23, a first gear 24, and a second gear 25; The first rigid pipe 20 is rotatably connected to the pre-set mounting hole in the side plate 11 via a deep groove ball bearing. The outer ring of the bearing is interference-fitted with the mounting hole, and the inner ring is interference-fitted with the first rigid pipe 20. The first rigid pipe 20 on the left is fixedly connected to a pipe connected to an external steam generator via a rotary joint. A compressor is installed between the pipe and the steam generator to compress and transport steam. The first rigid pipe 20 on the right is fixedly connected to the first pipe 50 via a rotary joint. The opposite ends of the two sets of first rigid pipes 20 are fixedly connected to several L-shaped rigid pipes 21 via multi-port joints (made of stainless steel with built-in sealing gaskets). Valves are provided on the L-shaped rigid pipes 21. One end of the L-shaped rigid tube 21 is fixedly installed on a pre-set interface on the side of the cylinder 30 by welding, and is connected to the filter chamber 31 to realize the conduction of airflow between the first rigid tube 20 and the filter chamber 31; the servo motor 22 is fixedly installed on the outside of the left side plate 11 by motor bracket bolts; the output shaft of the servo motor 22 is fixedly connected to the connecting shaft 23 by a coupling, and the other end of the connecting shaft 23 is fixedly installed with the first gear 24 by a flat key; the second gear 25 is fixedly installed on the first rigid tube 20 on the left side by a flat key, and the first gear 24 and the second gear 25 are meshed and connected, and the meshing transmission ratio is set according to the actual purging angle requirements. The servo motor 22 is controlled by an external PLC control system (such as Siemens S7-200 series), which can realize forward and reverse rotation and speed adjustment to control the rotation angle and speed of the cylinder 30; its power supply is industrial 380V AC, which is connected to the workshop power supply circuit through a dedicated cable and equipped with a leakage protection device.
[0019] The filter assembly includes: an arc-shaped plate 40, a box body 41, a silica gel desiccant 42, and a handle 43; Several arc-shaped plates 40 are fixedly installed on the side of the cylindrical body 30 corresponding to each filter chamber 31 using hexagonal screws. High-temperature resistant sealing gaskets are adhered to the inner side of the arc-shaped plates 40 to seal the filter chambers 31 and prevent air leakage. The box body 41 is made of stainless steel and is fixedly installed at the center of the inner side of the arc-shaped plates 40 with screws. The box body 41 fits easily into the filter chambers 31. Furthermore, sealing gaskets can be installed at the connection between the box body 41 and the filter chambers 31 as needed. Several filter holes are provided on the side wall of the box body 41, with the hole diameter set according to requirements. The silica gel desiccant 42 is filled in the box body 41 in spherical granular form. The handle 43 is fixedly installed at the center of the outer side of the arc-shaped plates 40 by welding, facilitating the operator to disassemble the arc-shaped plates 40 to replace the silica gel desiccant 42.
[0020] The purging assembly includes a purging pipe 60 and a nozzle 61; The purge pipes 60 are configured in several quantities (based on the width of the catalyst layer), and the purge pipes 60 are fixedly installed 100-150mm (preferably 125mm) above the catalyst layer by a bracket to ensure that the purge range covers the entire catalyst layer; the bottom end of the purge pipes 60 is fixedly installed with several nozzles 61 arranged in an inclined manner, with an inclination angle of 30°-45° (preferably 37.5°), and the purge range of adjacent nozzles 61 overlaps to avoid purge dead corners. The nozzles 61 adopt a fan-shaped spray structure to increase the purge area.
[0021] The heating assembly includes a third rigid tube 70 and an electric heating wire 71; The third rigid tube 70 is made of stainless steel and is fixedly installed on the top of the purge tube 60 by welding. The top of the third rigid tube 70 is fixedly connected to the second pipe 51 through a flange. The inner cavity of the third rigid tube 70 is spirally arranged and fixedly installed with electric heating wires 71. The electric heating wires 71 are controlled by an external temperature control system and a PLC system. The temperature sensor monitors the temperature of the airflow after heating in real time to achieve closed-loop temperature control. The power supply is industrial 220V AC power, which is connected to the power supply circuit through a dedicated cable and equipped with an overheat protection device.
[0022] The side walls of the cylinder 30 located on both sides of the filter chamber 31 are fixedly installed with second rigid pipes 32 equipped with manual shut-off valves by welding. A fan (model selected according to the cylinder volume) is fixedly installed in the inner cavity of one set of second rigid pipes 32 by a bracket. An electric heating wire 71 is fixedly installed in the inner cavity of the other set of second rigid pipes 32 in a spiral arrangement. The fan and the electric heating wire 71 in the second rigid pipe 32 are both controlled by a PLC system and are linked with the servo motor 22 and the electric heating wire 71 of the heating component. The power supply is industrial 380V AC, connected to the workshop power supply circuit. The fan is equipped with an overload protection device, and the electric heating wire is equipped with an overheat protection device.
[0023] In practical use, the operating steps for those skilled in the art are as follows: The working process of this device is divided into a pretreatment stage, a purging stage, and a desiccant regeneration stage. Each stage is automatically controlled by a PLC system, and can also be operated in manual mode.
[0024] 1. Preprocessing stage After the device is started, the PLC system first controls the manual shut-off valve on the second rigid tube 32 to open (it can be manually opened in advance), starts the fan and the electric heating wire 71 in the second rigid tube 32, and introduces hot air into the cylinder 30 (the temperature is controlled at 80-100℃) to preheat and activate the silica gel desiccant 42 for 10-15 minutes; at the same time, the electric heating wire 71 of the heating component is started to preheat the third rigid tube 70. The airflow temperature is monitored by the temperature sensor. When the temperature reaches 180-200℃ (matching the optimal activity temperature of the catalyst), the pretreatment stage ends and the purging stage begins.
[0025] 2. Purging stage After pretreatment, the PLC system shuts down the fan and electric heating wire 71 of the second rigid tube 32 and turns on the external steam generator so that steam enters the filter chamber 31 through the left first rigid tube 20 and L-shaped rigid tube 21. In the filter chamber 31, the steam comes into full contact with the silica gel desiccant 42 through the filter holes of the box 41, and the moisture is adsorbed by the silica gel desiccant 42 to achieve airflow dehydration. The dehydrated dry airflow enters the third rigid tube 70 through the right L-shaped rigid tube 21, the first pipe 50, and the second pipe 51.
[0026] Inside the third rigid tube 70, the dry airflow is heated to 170-180℃ by the electric heating wire 71. The temperature sensor provides real-time temperature data, and the PLC system maintains temperature stability by adjusting the power supply of the electric heating wire 71. The heated airflow enters the purge pipe 60 and is evenly sprayed onto the catalyst surface and pores through the inclined nozzles 61 to remove accumulated ash and salt blockage.
[0027] 3. Desiccant regeneration stage After the device has been working continuously for 10-12 hours, the adsorption capacity of silica gel desiccant 42 will decrease, and the PLC system will prompt that regeneration is required. The operator will turn off the external steam generator, turn on the fan and electric heating wire 71 of the second hard tube 32, and introduce a hot air flow of 80-100°C into the cylinder 30. The hot air flow will carry the moisture adsorbed by the silica gel desiccant 42 and discharge it through the other side of the second hard tube 32. The regeneration time is 15-20 minutes. After the regeneration is completed, the device can be put back into operation.
[0028] When the silica gel desiccant 42 has a severely reduced adsorption capacity after multiple regenerations, the operator can first use the servo motor 22 to turn the arc plate 40 to be disassembled upwards. Then, after removing the screws, the arc plate 40 can be disassembled using the handle 43, the box 41 can be taken out, and the silica gel desiccant 42 can be replaced. The replacement process is simple and convenient, without the need to disassemble the entire device.
[0029] Although the present invention has been described above with reference to embodiments, various modifications can be made and components can be replaced with equivalents without departing from the scope of the present invention. In particular, as long as there is no structural conflict, the features in the embodiments disclosed in this invention can be combined with each other in any way. The lack of an exhaustive description of these combinations in this specification is merely for the sake of brevity and resource conservation. Therefore, the present invention is not limited to the specific embodiments disclosed herein, but includes all technical solutions falling within the scope of the claims.
Claims
1. A compressed air purging device based on SCR catalyst protection, comprising a base plate (10), wherein side plates (11) are fixedly installed at both ends of the top of the base plate (10), characterized in that, A cylinder (30) is provided between the two sets of side plates (11) via a connecting assembly. The cylinder (30) is provided with a plurality of filter chambers (31), and a filter assembly is provided in the filter chambers (31) to filter the moisture in the steam. A first pipe (50) is connected to one set of the connecting assembly. A second pipe (51) is fixedly connected to one end of the first pipe (50) via a multi-port connector. A purging assembly is connected to one end of the second pipe (51) via a heating assembly.
2. The compressed air purging device based on SCR catalyst protection according to claim 1, characterized in that, The connection component includes: The first rigid pipe (20) is rotatably connected to the side plate (11) by a bearing, and the first rigid pipe (20) on the right side is fixedly connected to the first pipe (50) by a rotary joint. L-shaped rigid tubes (21), the opposite ends of the two sets of first rigid tubes (20) are fixedly connected to several L-shaped rigid tubes (21) through multi-port connectors, and one end of the L-shaped rigid tube (21) is fixedly installed on the side of the cylinder (30) and connected to the filter chamber (31).
3. The compressed air purging device based on SCR catalyst protection according to claim 2, characterized in that, The connection component also includes: Servo motor (22), the servo motor (22) is fixedly mounted on a set of side plates (11); The first gear (24) is fixedly mounted on the output shaft of the servo motor (22) via a connecting shaft (23). The second gear (25) is fixedly mounted on a set of first rigid tubes (20), and the first gear (24) and the second gear (25) are meshed together.
4. The compressed air purging device based on SCR catalyst protection according to claim 1, characterized in that, The filtering component includes: Arc-shaped plates (40): Several arc-shaped plates (40) are fixedly installed on the side of the cylinder (30) by screws to seal the filter chamber (31) through the arc-shaped plates (40); The box (41) with several filter holes on its side wall is fixedly installed on the inner side of the arc plate (40) and the box (41) is inserted into the filter cavity (31).
5. A compressed air purging device based on SCR catalyst protection according to claim 4, characterized in that, The filtering component also includes: Silica gel desiccant (42), which is filled in the box body (41); A handle (43) is fixedly mounted on the outside of the arc plate (40).
6. The compressed air purging device based on SCR catalyst protection according to claim 1, characterized in that, The purging assembly includes: A purge pipe (60) is provided, wherein there are several purge pipes (60), and the purge pipes (60) are provided above the catalyst layer; The nozzle (61) is fixedly installed at the bottom end of the purge pipe (60) with several nozzles (61) arranged in an inclined manner.
7. A compressed air purging device based on SCR catalyst protection according to claim 6, characterized in that, The heating component includes: The third rigid tube (70) is fixedly installed on the top end of the purge tube (60), and the top end of the third rigid tube (70) is fixedly connected to the second pipe (51). The electric heating wire (71) is fixedly installed in a spiral arrangement in the inner cavity of the third rigid tube (70).
8. The compressed air purging device based on SCR catalyst protection according to claim 1, characterized in that, The second rigid pipe (32) with valves is fixedly installed on the side wall of the cylinder (30) located on both sides of the filter chamber (31). A fan is fixedly installed in the inner cavity of one set of the second rigid pipes (32), and an electric heating wire (71) is fixedly installed in the inner cavity of the other set of the second rigid pipes (32) in a spiral arrangement.