A novel conjoined specimen for ester-hardened molding of high-manganese steel fork

By designing a novel integrated specimen and employing integrated casting and a trapezoidal slag collection structure, the problems of material waste and performance feedback distortion in traditional split specimens have been solved, achieving efficient production and low-cost casting.

CN224950947UActive Publication Date: 2026-11-10CHINA RAILWAY SHANQIAO GRP CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202522326780.5
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2025-11-03
Publication Date
2026-11-10
Estimated Expiration
2035-11-03

AI Technical Summary

Technical Problem

In traditional high-manganese steel frog casting, the use of molding sand for split specimens is large, resulting in low production efficiency, an inability to directly reflect the performance of the castings, and serious waste of gating system and molten metal materials.

Method used

A novel integrated specimen was designed, consisting of a first connecting part, a second connecting part, and a third connecting part integrally cast using a specific mold. The second connecting part is an isosceles trapezoid with an inclination angle of 15°-18°. The slag collection part is designed as a trapezoidal structure. The structure was optimized through digital simulation and finite element analysis to achieve material utilization and performance consistency.

Benefits of technology

Simplify the production process, increase production efficiency by 20%, reduce molding sand usage by 25%, improve casting quality by 15%, reduce production costs, improve performance consistency, make demolding easier, and allow slag collection to be recycled, thus reducing costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN224950947U_ABST
    Figure CN224950947U_ABST
Patent Text Reader

Abstract

This utility model discloses a novel integrated specimen for ester-hardening molding of high-manganese steel frogs, belonging to the field of high-manganese steel frog casting technology. It includes a first connecting part, a second connecting part, and a third connecting part integrally cast by a specific mold. The first and third connecting parts constitute the main body of the entire specimen, while the second connecting part serves as a slag-collecting part to reduce casting defects in the main body of the specimen. The cross-section of the second connecting part is an isosceles trapezoid, with its top edge being the short side and integrally connected to the first connecting part, and its bottom edge being the long side and integrally connected to the third connecting part. The integrated specimen designed by this utility model is not only simple in structure and easy to manufacture, but also greatly simplifies the production process and assembly flow, improves production efficiency, reduces production costs, and enhances the performance consistency between the specimen and the casting, thereby effectively improving the quality of the casting.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This utility model belongs to the field of high manganese steel fork casting technology, and in particular relates to a novel one-piece specimen for ester-hardened molding of high manganese steel forks. Background Technology

[0002] In the casting of high-manganese steel turnouts, ester-hardening molding technology is widely used due to its advantages such as fast molding speed and high sand mold strength. However, traditional specimens are mostly designed in a split configuration, which presents the following problems: 1. Split-type specimen molding sand requires a large amount of molding sand, resulting in low production efficiency; 2. Split-type test specimens cannot directly reflect the properties of the casting itself; 3. Split-type specimens need to be cast separately, and there is a serious waste of materials such as the casting system and molten metal.

[0003] Therefore, we propose a novel integral specimen for ester-hardened molding of high-manganese steel forks to address the aforementioned problems. Utility Model Content

[0004] In view of this, in order to solve the problems of traditional split specimens which not only consume a large amount of molding sand and have low production efficiency, but also cannot intuitively reflect the performance of the casting itself, and require separate pouring, resulting in serious waste of materials such as the pouring system and molten metal, this utility model provides a new type of integrated specimen for ester hardening molding of high manganese steel forks.

[0005] To achieve the above objectives, this utility model provides the following technical solution: A novel integral specimen for ester-hardening molding of high-manganese steel frogs, comprising a first connecting part, a second connecting part, and a third connecting part integrally cast by a specific mold. The first connecting part is located at the uppermost part of the entire specimen, and the third connecting part is located at the lowermost part of the entire specimen. The first connecting part and the third connecting part constitute the main body of the entire specimen and match the end of the high-manganese steel frog casting. The second connecting part is a slag-collecting part of the entire specimen, used to reduce casting defects in the main body of the specimen. The cross-section of the second connecting part is an isosceles trapezoid, with the top edge of the second connecting part being the short side and integrally connected to the first connecting part, and the bottom edge of the second connecting part being the long side and integrally connected to the third connecting part. The slope angle of the waist edge of the second connecting part is 15°-18°.

[0006] Furthermore, the overall length of the first connecting part, the second connecting part, and the third connecting part is 280mm.

[0007] Furthermore, the width of the first connecting part is 79mm and the height is 45.5mm.

[0008] Furthermore, the height of the second connecting part is 126.2 mm.

[0009] Furthermore, the width of the third connecting part is 162mm and the height is 18.3mm.

[0010] Furthermore, the specimen is integrally formed and connected to the main body of the casting.

[0011] Furthermore, the specimen was made of the same high-manganese steel as the main body of the casting.

[0012] The embodiments of this utility model have the following beneficial effects: 1. By integrating the test piece with the high-manganese steel frog casting, the production process and assembly flow can be simplified, production efficiency can be improved, the performance consistency between the test piece and the casting can be improved, the problem of performance feedback distortion of separate test pieces can be avoided, and the amount of material used can be reduced, thus reducing production costs.

[0013] 2. By designing the slag collection section with a trapezoidal structure, not only can casting defects in the main body of the specimen be reduced and casting quality improved, but stress relief can also be achieved by using the inclined transition, so that the maximum stress value of the specimen is lower than the yield strength of the material, avoiding cracking of the slag collection section. At the same time, it can also make the specimen easier to demold, thus solving the problem of difficult demolding of traditional structures.

[0014] 3. After separating the casting from the integral test piece, the slag-collecting part of the integral test piece can be reused, further reducing production costs.

[0015] The integrated specimen designed in this utility model is not only simple in structure and easy to manufacture, but also greatly simplifies the production process and assembly flow, improves production efficiency, reduces production costs, and improves the performance consistency between the specimen and the casting, thereby effectively improving the quality of the casting.

[0016] Other advantages, objectives, and features of this invention will be set forth in part in the description which follows, and in part will be apparent to those skilled in the art from the following examination and study, or may be learned from practice of this invention. The objectives and other advantages of this invention can be realized and obtained through the following description. Attached Figure Description

[0017] To make the objectives, technical solutions, and advantages of this utility model clearer, the preferred embodiments of this utility model will be described in detail below with reference to the accompanying drawings, wherein: Figure 1 This is a three-dimensional structural view of a novel integral specimen for ester-hardening molding of high-manganese steel forklifts according to this utility model. Figure 2 This is a left-side structural dimension drawing of a novel integral specimen for high-manganese steel pitchfork ester hardening molding according to this utility model. Figure 3 This is a front view structural dimension drawing of a novel integral specimen for ester-hardened molding of high-manganese steel forklifts according to this utility model.

[0018] In the diagram: 100, first connecting part; 200, second connecting part; 300, third connecting part. Detailed Implementation

[0019] The following specific examples illustrate the implementation of this utility model. Those skilled in the art can easily understand other advantages and effects of this utility model from the content disclosed in this specification. This utility model can also be implemented or applied through other different specific embodiments, and various details in this specification can also be modified or changed based on different viewpoints and applications without departing from the spirit of this utility model. It should be noted that the illustrations provided in the following embodiments are only schematic representations of the basic concept of this utility model. Unless otherwise specified, the following embodiments and features can be combined with each other.

[0020] Please see Figures 1-3 This embodiment provides a novel integral specimen for ester-hardening molding of high-manganese steel frogs, comprising a first connecting portion 100, a second connecting portion 200, and a third connecting portion 300 integrally cast using a specific mold. The first connecting portion 100 is located at the top of the entire specimen, with a width of 79 mm and a height of 45.5 mm. The third connecting portion 300 is located at the bottom of the entire specimen, with a width of 162 mm and a height of 18.3 mm. The first connecting portion 100 and the third connecting portion 300 constitute the main body of the entire specimen and match the end of the high-manganese steel frog casting. The entire specimen and the main casting body are integrally cast using a mold, and the specimen is cast from the same high-manganese steel material as the main casting body. By integrating the test specimen with the high-manganese steel frog casting, the production process and assembly flow can be simplified, increasing production efficiency by more than 20%. It also improves the performance consistency between the test specimen and the casting, avoiding the problem of performance feedback distortion in separate test specimens. At the same time, it can reduce the amount of material used, thereby reducing production costs.

[0021] The structural design of this integrated specimen is not based on simple adaptation using traditional empiricism, but rather on a modern design system that relies on multi-physics coupling simulation, digital verification, and deep synergy of material properties. Through cutting-edge technologies such as numerical simulation of the casting process, finite element structural optimization, and fluid dynamics analysis, it achieves a precise match between structural function and manufacturing efficiency.

[0022] Integrated structural topology optimization based on numerical simulation of the casting process. To address the pain points of sand waste and performance feedback distortion in traditional split-type specimens, the design team used ProCAST / AnyCasting casting simulation software to conduct full-process numerical simulation of the integrated casting process of high-manganese steel turnouts and specimens. By establishing a multi-physics coupled model that includes molten metal filling, solidification heat transfer, and stress field evolution, the flow trajectory of molten metal, temperature field gradient, and formation law of shrinkage cavities / porosity defects under different structural topologies were accurately simulated.

[0023] Simulation results show that traditional split structures, due to the difference in pouring timing between the specimen and the casting body, result in a solidification rate deviation of 18%-22% between the specimen and the casting body, failing to accurately reflect the mechanical properties of the casting. In contrast, the integrated topology structure designed in this paper, by geometrically integrating the specimen body and the frog end, allows both to share the same gating system and temperature field environment. Simulations show that the integrated structure reduces the molten metal filling time by 12%, improves solidification uniformity by 30%, and controls the performance consistency error between the specimen and the casting body within 5%, fundamentally solving the technical bottleneck of performance feedback distortion in split specimens. Furthermore, by optimizing the topology of the sand-encased area of ​​the integrated structure, the amount of sand used is reduced by 25% while maintaining the strength of the sand mold, further verifying the superiority of the integrated structure in terms of material utilization and production efficiency.

[0024] Digital Verification of Geometric Compatibility between Specimen and Casting Based on Dimensional Chain Accuracy Analysis. To ensure accurate matching between the integrated specimen and the ends of different types of frogs, the design team introduced digital dimensional chain analysis technology. Taking the 60kg / m frog as an example, this invention establishes a three-dimensional dimensional chain model that includes frog end tolerances, specimen body size tolerances, and casting shrinkage rate. The Monte Carlo simulation method is used to analyze the accuracy of 1000 dimensional combinations.

[0025] Simulation results show that in traditional designs, the fit clearance between the specimen and the frog fluctuates between 0.5 and 1.2 mm, which can easily lead to molten metal leakage during casting. This design, however, optimizes the specimen length (280 mm) by setting the main body width to 79 mm (allowing a 6 mm compensation margin compared to the standard rail width of 73 mm) and combining this with the solidification shrinkage rate of high-manganese steel (1.8%-2.2%) obtained from finite element simulation. This results in a final assembly clearance fluctuation range controlled within 0.1-0.3 mm, meeting the high-precision assembly requirements of ester-hardened molding. Furthermore, digital dimensional chain analysis proactively mitigates the risk of fit failure due to material shrinkage and processing errors, ensuring the engineering feasibility of the structural design.

[0026] In addition, the second connecting part 200 is designed as a slag-collecting section for the entire specimen. The cross-section of the second connecting part 200 is an isosceles trapezoid, extending longitudinally along the entire specimen body. This reduces casting defects in the specimen body, increasing the casting pass rate by 15%, thereby effectively improving casting quality. The top edge of the second connecting part 200 is the short side and is integrally connected to the first connecting part 100, while the bottom edge is the long side and is integrally connected to the third connecting part 300. The height of the second connecting part 200 is 126.2 mm, and the overall length of the first connecting part 100, the second connecting part 200, and the third connecting part 300 is 280 mm.

[0027] In one aspect of this embodiment, the angle between the waist edge of the second connecting portion 200 and the vertical edge of the first connecting portion 100, i.e., the slope angle of the second connecting portion 200, is set to 15°-18°, which ensures maximum slag separation efficiency. Through the trapezoidal structure design, stress relief can be achieved using the slope transition. This not only ensures that the maximum stress value of the specimen is lower than the yield strength of the material, preventing cracking of the slag-collecting part, but also, by forming an appropriate draft angle through the slope, makes the specimen easier to demold, thus solving the problem of difficult demolding in traditional structures.

[0028] A collaborative design of the trapezoidal slag collection structure based on finite element analysis and fluid dynamics. As the core functional area of ​​the specimen, the slag collection section's structural design must simultaneously meet the dual requirements of slag-liquid separation efficiency and structural mechanical stability. The ANSYS APDL finite element analysis platform was used to perform multi-objective optimization of the slag collection structure from both fluid dynamics and structural mechanics dimensions. At the fluid dynamics level, a two-phase flow model of high-manganese steel molten slag and molten metal was established to simulate the slag's upward trajectory and retention characteristics under different cross-sectional shapes (rectangular, triangular, and trapezoidal). Simulation results show that the trapezoidal structure, due to the "guide-expansion" effect formed by the inclined surfaces on both sides, enhances the synergistic effect of buoyancy and centrifugal force on the molten slag during flow, resulting in an approximately 40% improvement in slag aggregation efficiency compared to the rectangular structure. Simultaneously, the gradually changing channel design of the trapezoidal cross-section effectively reduces the flow resistance of the molten metal, lowering the standard deviation of the flow field velocity distribution by approximately 15%, thus avoiding slag entrapment defects caused by excessively high local flow velocities. Finally, through simulation iteration, the optimal inclined surface angle of the trapezoidal structure was determined to be 15°-18°, ensuring maximum slag separation efficiency.

[0029] At the structural mechanics level, to address the issue of thermal stress concentration during the cooling process after casting, a thermo-structural coupled finite element analysis was used to calculate the stress distribution cloud map of different slag collection structures during the solidification shrinkage stage. The results show that the traditional rectangular slag collection structure is prone to stress concentration at the corners, with a maximum stress value reaching 320 MPa, far exceeding the yield strength of high-manganese steel (280 MPa), easily leading to cracking in the slag collection section. In contrast, the trapezoidal structure achieves stress relief through a sloped transition; finite element simulation shows that its maximum stress value is reduced to 240 MPa, lower than the material's yield strength. Simultaneously, the integrated design of the draft angle (sharing geometric parameters with the trapezoidal slope) reduces the mold release force by 20%, solving the problem of difficult demolding in traditional structures. Furthermore, fatigue strength simulation of the reusability of the slag collection section verifies its structural integrity within five reuse cycles, further supporting the design goal of low-cost recycling.

[0030] In summary, the structural design of this utility model's integrated specimen is a systematic innovation based on digital simulation and engineering verification. Through casting simulation, finite element analysis, dimensional chain optimization, and other technical means, it achieves deep synergy between structural function, manufacturing efficiency, and material properties, providing scientific and reliable technical support for improving the casting quality and reducing the production cost of high-manganese steel turnouts.

[0031] Finally, it should be noted that the above embodiments are only used to illustrate the technical solution of this utility model and are not intended to limit it. Although this utility model has been described in detail with reference to preferred embodiments, those skilled in the art should understand that modifications or equivalent substitutions can be made to the technical solution of this utility model without departing from the spirit and scope of this technical solution, and all such modifications or substitutions should be covered within the scope of the claims of this utility model.

Claims

1. A novel integral specimen for ester-hardened molding of high-manganese steel forks, comprising a first connecting part (100), a second connecting part (200), and a third connecting part (300) integrally cast, wherein the first connecting part (100) is located at the uppermost part of the entire specimen, and the third connecting part (300) is located at the lowermost part of the entire specimen, characterized in that, The first connecting part (100) and the third connecting part (300) constitute the main body of the entire specimen and match the end of the high manganese steel frog casting; the second connecting part (200) is the slag collection part of the entire specimen, used to reduce casting defects in the main body of the specimen; the cross-section of the second connecting part (200) is an isosceles trapezoid, the top edge of the second connecting part (200) is the short side and is integrally connected with the first connecting part (100), the bottom edge of the second connecting part (200) is the long side and is integrally connected with the third connecting part (300); the slope angle of the waist side of the second connecting part (200) is 15°-18°.

2. The novel integral specimen for ester-hardened molding of high-manganese steel forklifts as described in claim 1, characterized in that, The overall length of the first connecting part (100), the second connecting part (200) and the third connecting part (300) is 280mm.

3. A novel integral specimen for ester-hardening molding of high-manganese steel forks as described in claim 2, characterized in that, The width of the first connecting part (100) is 79 mm and the height is 45.5 mm.

4. A novel integral specimen for ester-hardening molding of high-manganese steel forks as described in claim 2, characterized in that, The height of the second connecting part (200) is 126.2 mm.

5. A novel integral specimen for ester-hardening molding of high-manganese steel forks as described in claim 2, characterized in that, The width of the third connecting part (300) is 162 mm and the height is 18.3 mm.

6. A novel integral specimen for ester-hardening molding of high-manganese steel forklifts as described in any one of claims 1-5, characterized in that, The specimen is integrally formed and connected to the main casting body.

7. A novel integral specimen for ester-hardened molding of high-manganese steel forklifts as described in claim 6, characterized in that, The specimen was made of the same high-manganese steel as the main body of the casting.