Method and measuring setup for checking a conductive body

The described method uses periodic bending and electrical resistance measurement to accurately detect cracks in conductive bodies, offering precise assessment of mechanical condition and lifespan without causing damage, addressing the limitations of conventional methods.

DE102013224394B4Active Publication Date: 2024-10-24FRAUNHOFER GESELLSCHAFT ZUR FORDERUNG DER ANGEWANDTEN FORSCHUNG EV
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
DE102013224394
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Filing Date
2013-11-28
Publication Date
2024-10-24
Estimated Expiration
2033-11-28

AI Technical Summary

Technical Problem

Conventional methods for checking the condition of electrically conductive bodies, such as for detecting cracks, are either inaccurate or too complex for many applications, and there is a need for a more precise yet simple method to assess the condition and potential degradation of these bodies.

Method used

A procedure involving periodic bending of a section of the conductive body with a controlled frequency, combined with electrical resistance measurement, to detect fluctuations in resistance that indicate the presence and extent of cracks, using a measurement arrangement comprising a voltage source, actuator, sensor, and frequency filter to analyze these fluctuations.

Benefits of technology

This method allows for accurate detection of cracks without damaging the body, providing insights into the mechanical condition and potential lifespan of the conductive body, with high sensitivity and minimal interference from noise.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

Method for checking an electrically conductive body (2), - wherein an electrical voltage is applied to the body (2) so that an electric current flows through at least a section (7) of the body (2), - wherein the subsection (7) is repeatedly bent at a bending frequency over time, wherein when the subsection (7) is bent a first side region (13) of the subsection (7) is stretched and simultaneously a second side region (14) of the subsection (7) is compressed or the first side region (13) is compressed and simultaneously the second side region (14) of the subsection (7) is stretched, - wherein a time course of a measured quantity which changes as a function of an instantaneous electrical resistance of the subsection (7) is measured and time fluctuations corresponding to the bending frequency are filtered out of the time course of the measured quantity by means of a narrowband frequency filter (18) and subsequently evaluated.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] The invention relates to a method and a measuring arrangement for checking an electrically conductive body.

[0002] In many areas of technology, it is advantageous or even necessary to test electrically conductive components, for example, for quality assurance during the manufacturing and processing of the component, or before, during, or after use, such as for condition monitoring, measuring progressive degradation, or estimating the remaining service life. The component in question could be, for example, an electrical connector for establishing a conductive connection between two or more electrical or electronic components, or a machine component made of an electrically conductive material, such as a helicopter rotor blade or a turbine blade.Other examples of electrically conductive bodies, whose regular inspection is advantageous or even necessary, but which in some cases cannot be carried out, or can only be carried out rarely, for example for economic reasons, include frames of bicycles, motorcycles, cars and trucks; pipes for conveying gases or liquids, such as those in drinking water or wastewater systems; pipes of heating systems; and pipes and supports of scaffolding structures, such as construction scaffolding. In particular, welds on such bodies represent potential weak points where regular inspection is often advisable.

[0003] A typical example of progressive degradation in such a body, especially when it is exposed to frequent temperature fluctuations (temperature cycles) and / or mechanical stress, is the formation of cracks. These cracks typically propagate from the surface of the body into its interior and can develop into increasingly deeper cracks over time. It is often desirable or even necessary to detect cracks in the body as early as possible in their development, when they still have a relatively small depth. Using conventional measurement methods, such as standard resistance measurements, cracks can usually only be reliably detected relatively late, i.e., only after a relatively large crack depth has developed. On the other hand, well-known high-precision methods, such as X-ray or ultrasound tests, are too costly for many applications.

[0004] For example, various methods and systems for checking bodies are known from publications DE 10 2012 006 155 A1, DE 43 42 685 A1, US 2010 / 0 089 161 A1 and DE 10 2010 041 391 A1.

[0005] It is therefore the object of the present invention to propose a method that is as accurate as possible, yet still simple, for checking the condition of an electrically conductive body. Likewise, a corresponding measuring arrangement is to be proposed that enables the most accurate yet simple possible checking of an electrically conductive body.

[0006] This problem is solved by the method according to the main claim and by the measuring arrangement according to the dependent claim. Further developments and special embodiments are the subject of the dependent claims as well as the following description. In particular, although not explicitly described in detail here, the method proposed here, as well as all further developments and embodiments described in connection with this method, can be carried out with the measuring arrangement proposed here. For this purpose, the measuring arrangement or its respective components can be configured, designed, or programmed accordingly. In particular, the components described in connection with carrying out the method, such as the sensor, the actuator, the control unit, or the filter, can serve as corresponding components of the measuring arrangement.Conversely, the implementation of the procedure proposed here represents a possible use of the measuring setup.

[0007] The proposed method for testing an electrically conductive body involves applying an electrical voltage to the body, causing an electric current to flow through at least a portion of it. During this process, the section is periodically bent at a specific frequency. As the section is bent, one side is stretched while a second side is compressed. Alternatively, the first side is compressed while the second side is stretched. Typically, the section is bent alternately in these two directions.The section can thus be bent back and forth periodically between a first bending state and a second bending state at a bending frequency. In the first bending state, the first side of the section is stretched and the second side is compressed, while in the second bending state, the first side is compressed and the second side is stretched. In principle, however, it is also possible for the section to be bent only on one side, for example, between the first (or alternatively the second) bending state and an equilibrium or neutral position of the section (see below).

[0008] The bending frequency indicates how often per unit of time, typically one second, the section is periodically bent back and forth between two states. This could be, for example, the bending frequency between the maximum deflection of the section in the first bending state and the maximum deflection of the section in the second bending state (in the case of bending in both directions), or between the maximum deflection of the section in the first bending state and the equilibrium position (in the case of bending in one direction). The periodic bending of the section thus results in a periodic bending oscillation of the section, which is characterized by the aforementioned bending frequency. The precise temporal pattern of this bending oscillation, i.e., the time dependence of the lateral deflection of the section, can, for example, correspond to or closely resemble a sinusoidal oscillation with the specified bending frequency.However, other time courses are also possible in principle, such as triangular or rectangular oscillations. The time course of the bending oscillation of the section depends on the time course of the force or bending moment applied to the section for bending.

[0009] A measured quantity, whose measured value changes depending on the instantaneous electrical resistance of the section, is measured repeatedly and as continuously as possible, typically during current flow, in order to determine the time course of the measured quantity. The measured quantity, or rather the time course of its measured values, is examined for fluctuations. In particular, those time-dependent fluctuations of the measured quantity that correspond to the bending frequency of the section are evaluated. Fluctuations corresponding to the bending frequency are typically those whose frequency coincides with the bending frequency, especially when the section is bent with a time-dependent sinusoidal force or bending moment.In addition to the aforementioned fluctuations, fluctuations whose frequency is an integer multiple of the bending frequency can also be included, particularly when the segment is bent with a time-dependent triangular or rectangular force or bending moment. For this purpose, the aforementioned fluctuations are filtered out of the time course using a narrowband frequency filter and then analyzed. Typically, the measured quantity is measured using a sensor, which generates a measurement signal that changes depending on the instantaneous electrical resistance of the segment.From the measurement signal, a component of the signal caused by bending the section can then be filtered out. This component typically contains oscillations at the frequency of the bending frequency, and in some cases also oscillations at frequencies corresponding to integer multiples of the bending frequency, or is identical to them. This component is then evaluated. Examples of the measured quantity are the instantaneous current, the instantaneous applied voltage, or the electrical resistance of the section or the body, or another measured quantity that depends on at least one of these quantities.

[0010] For example, the voltage applied to the body can be varied over time so that the current through the body remains constant. In this case, the voltage source can be designed as a constant current source. The measured quantity can then be a variable that depends on the applied voltage. In the simplest case, the measured quantity can be proportional to or identical to the applied voltage. In this way, the measured quantity is a measure of the electrical resistance of the body and thus also a measure of the resistance of the section. Of course, it is also possible to measure the electrical resistance of the body or the section itself. The sensor can, for example, be designed as a resistance measuring device. The voltage source or the constant current source can be integrated into the resistance measuring device.

[0011] As described above, the repeated (i.e., periodic) bending of the segment can correspond to or resemble a harmonic, i.e., sinusoidal, bending vibration, or, for example, a triangular or rectangular vibration. The described bending is therefore typically achieved by applying a periodic force to the segment, ideally with a sinusoidal, triangular, or rectangular shape. In this way, it can generally be ensured that the fluctuations in the measured quantity caused by the bending are also predominantly harmonic (sinusoidal) vibrations with the bending frequency, i.e., contained within a very narrow frequency band around the bending frequency. Additionally, particularly in the case of triangular and rectangular vibrations of the segment, fluctuations corresponding to integer multiples of the bending frequency can also occur.The fluctuations caused by bending therefore lie within a frequency range defined by the time course of the periodic (excitation) force. Depending on the time course of the periodic (excitation) force, this frequency range is defined by a relatively narrow frequency band around the bending frequency and may include, for example in the case of a triangular or rectangular force curve, additional narrow frequency bands, each comprising exactly an integer multiple of the bending frequency. This allows these fluctuations to be distinguished particularly well from unwanted interference such as noise, temperature fluctuations, and electromagnetic interference, thus enabling a particularly high sensitivity and accuracy of the measurement.

[0012] By considering the additional frequency bands defined above, it is often possible to increase the sensitivity of the method. The precise relationship between the temporal profile of the (excitation) force and the temporal profile of the measured quantity—that is, the fluctuations caused by the force—can depend on several influencing factors, particularly the number, size, and arrangement of cracks occurring in the section. Therefore, by analyzing the fluctuations, especially their frequency and amplitude, it is possible to draw conclusions about the size, number, and arrangement of cracks in the frequency domain.To carry out the proposed method, the proposed measuring arrangement comprises a voltage source with electrical contact elements for applying the electrical voltage to the body, such that an electric current flows through at least the section of the body, and an actuator configured to bend the section as described in connection with the proposed method. The measuring arrangement also includes a sensor configured to measure the time course of a measurand whose measured value changes depending on the instantaneous electrical resistance of the section, and an evaluation unit configured or programmed to evaluate temporal fluctuations in the time course of the measurand whose frequency corresponds to the bending frequency, i.e., typically to filter out and analyze these fluctuations.

[0013] To filter out fluctuations in the measured quantity or the aforementioned signal component of the measurement signal, a frequency filter, such as a bandpass filter, with a very narrow bandwidth, preferably a lock-in amplifier, is used. This ensures that, for subsequent analysis and evaluation, practically only the fluctuations in the measured quantity or measurement signal caused by the bending process remain, if such fluctuations exist. Preferably, the bending frequency or the time course of the periodic (excitation) force is kept constant over time. If the bending frequency or the time course of the periodic (excitation) force changes during the execution of the method, the frequency filter is adjusted accordingly so that the desired fluctuations, if present, can be filtered out at any given time.Typically, the bandwidth is approximately 0.0001%, but preferably less than 0.001%, of the frequency to be measured; more preferably, the bandwidth lies in a range of approximately 0.00001% to approximately 0.001% of the frequency to be measured. The frequency filter can be configured to filter out integer multiples of the bending frequency (so-called harmonics) from the measurement signal in addition to the bending frequency itself.

[0014] For example, the section can be bent by means of an actuator controlled by control signals from a control unit, with the bending frequency for the periodic bending of the section being specified by the control signals. Furthermore, it is possible to use a signal frequency of the control signal that specifies the bending frequency as the reference frequency for the bandpass filter or the lock-in amplifier in order to filter out the aforementioned signal component of the measurement signal. It is also possible to use a multiple of the signal frequency that specifies the bending frequency as the reference frequency for the lock-in amplifier. In addition, it is also possible for the frequency filter to comprise several lock-in amplifiers, each driven by a different reference frequency.Thus, one of the lock-in amplifiers can be driven with the signal frequency defining the bending frequency, and the other lock-in amplifiers can each be driven with a multiple of this signal frequency. Typically, the magnitude of the instantaneously transmitted force or bending moment can also be controlled via the control signal, for example, via the instantaneous signal strength. This allows, in particular, the preferred sinusoidal, triangular, or rectangular time course of the force or bending moment to be specified via the control signal. For example, the control signal can have a sinusoidal, triangular, or rectangular time course, i.e., it can be defined by exactly one signal frequency corresponding to the bending frequency, or by one signal frequency corresponding to the bending frequency and integer multiples of this signal frequency, as well as by exactly one amplitude.Preferably, the actuator has a (control signal-force) characteristic curve that is as linear as possible. For this purpose, the actuator can, for example, be equipped with a piezoelectric element for force generation.

[0015] Typically, the bending frequency is kept constant throughout the process. The bending frequency can be less than 20 Hz or even less than 10 Hz, and is preferably in the range of approximately 1 Hz to approximately 5 Hz. Surprisingly, particularly accurate measurement results can be achieved using a relatively low bending frequency, while simultaneously largely avoiding damage to the specimen during the process. Furthermore, it has been found that using such a low bending frequency makes it possible, in principle, to observe the temporal development of mechanical degradation, such as the formation and deepening of cracks in the section, during the execution of the process.Due to the relatively low bending frequency, the alternating stresses caused by bending correspond particularly well to the stresses typically caused by thermal expansion and contraction of the body, as often occur during short-term or intermittent use of the body or the device in which it is integrated. This correspondence allows, for example, particularly reliable estimates regarding the future expected changes in the body's condition or degradation. One possible explanation could be that, due to the relatively low bending frequency, minor yielding processes of the material can occur in the section (as with the comparably slow thermal alternating stresses), even though the elastic range of the section is not exceeded during bending.

[0016] During the process, the section is bent several times, typically at least 5 or 10 times, i.e., bent from the first bending state to the second bending state and back to the first bending state. The more frequently the section is bent, the better the achievable accuracy, particularly in detecting or filtering out the desired fluctuations. Preferably, however, the section is not bent periodically more than 30 or 20 times to minimize the risk of damage to the body. In most cases, sufficient measurement accuracy can be achieved in this way.

[0017] The periodic force is preferably applied transversely, i.e., across or even perpendicular to the longitudinal extent of the subsection or to the neutral layer of the subsection. The direction of force application is then typically also transverse, i.e., again across or even perpendicular to the direction of the current through the subsection. Typically, the force direction and the current direction form an angle with each other in a range between approximately 30° and approximately 90°, preferably in a range between approximately 60° and 90°, and particularly preferably at as close to 90° as possible, in order to generate a controlled and uniform bending vibration of the subsection and thus achieve highly reproducible measurements.

[0018] The invention is based on the understanding that if the electrical resistance, i.e., the DC resistance, of the body changes as a result of the described bending, this is in many cases an indication of a change in the body's condition, typically mechanical degradation. For example, the cross-sectional area of ​​a section may change due to bending if the body has cracks in that section. If such a crack opens due to bending, for example, by stretching the first (or analogously, the second) side, this reduces the cross-sectional area of ​​the section and thereby increases the electrical resistance of that section of the body.If this crack is closed again by subsequent bending, for example from the first to the second bending state, the cross-sectional area of ​​the section increases again and its electrical resistance decreases accordingly. This periodic opening and closing of cracks in the section, caused by repeated bending, is reflected in the aforementioned fluctuations in the measured quantity. These fluctuations, and their amplitude, can be used as an indicator of mechanical degradation of the body due to crack formation in the section in question.

[0019] Advantageously, existing cracks open and close even at relatively small bending amplitudes or relatively large bending radii, so that relatively slight stretching and compression of the aforementioned side regions of the section is generally sufficient to produce noticeable fluctuations in the measured value. In particular, this makes it possible for the described bending to be carried out almost entirely within the elastic range of the section. Preferably, the elastic limit of the elastic-plastic range or the plastic range of the section is avoided as completely as possible.

[0020] The aforementioned bending amplitude can be defined, for example, as the maximum deflection of the section from its (preferably elastic) equilibrium or neutral position during bending. The equilibrium or neutral position can generally be defined as the arrangement or configuration the section assumes when the force or bending moment applied to it is removed or interrupted. The maximum deflection of the section is therefore located at the point where, during periodic bending, it is bent furthest away from this equilibrium or neutral position. Typically, the maximum deflection can be less than 50% or even less than 20% of the section's width, measured in the direction of the maximum deflection.If the object is, for example, a wire, the maximum deflection can be less than one-fifth or even less than one-sixth of the wire's diameter in the section being tested. The maximum deflection of the section is preferably chosen to be large enough to ensure that any crack present in the section is opened and closed as completely as possible by the bending process, thus generating readily detectable fluctuations in the measured value. In some cases, it may be advantageous to first test the method with different bending amplitudes using a reference object comparable to the object being tested, and in this way to empirically determine an optimal bending amplitude for the given object.

[0021] With the proposed method and measurement setup, it is therefore possible, in particular, to ensure that the mechanical condition of the body is practically unaffected during testing, that, for example, no new cracks form in the body, and that any existing cracks do not deepen. Specifically, the procedure can be performed non-destructively on the body; that is, the body is neither destroyed nor torn apart. Furthermore, the method and measurement setup also make it possible to detect, quantify, and characterize the formation and propagation of cracks during the procedure based on fluctuations in the measured quantity.

[0022] Advantageously, it is possible to evaluate and use the amplitude of the fluctuations in the measured quantity that occur during periodic bending as a characteristic value for the mechanical degradation of the body. In particular, the amplitude can serve as a continuous characteristic value for crack formation in the side regions of the section. For example, it is possible to compare the measured amplitude with previously measured reference values, for example, on a reference body comparable to the one at hand, and to derive a mechanical degradation or crack depth of the body in question from this comparison.

[0023] It is also possible to record and analyze the temporal progression of the amplitude fluctuations of the measured quantity. For this purpose, the section is typically bent multiple times, for example, more than 50, more than 100, or several hundred times. The procedure can also be continued until the body is destroyed, for example, until the section is completely torn or broken. The measurement results obtained in this way can be used, for example, to make statements about or predictions for a comparable body, such as its expected (remaining) service life. In the case of bond wires, typically 500 to 1000 cycles, and in some cases up to 6000 cycles, of periodic bending are required, typically at a bending frequency of about 1 Hz, until the bond wire breaks.

[0024] It has been shown that cracks can be characterized based on the temporal change in amplitude. Specifically, a linearly increasing amplitude over time can be attributed to crack formation that develops in exactly one of the two side regions of the subsection. Conversely, a linearly decreasing amplitude, a hyperbolically increasing amplitude, and a amplitude that initially decreases linearly and then increases hyperbolically can all be attributed to crack formation that develops simultaneously in both side regions of the subsection.

[0025] In addition to the previously mentioned example of the electrical contact element or bond wire of an electrical or electronic device, the body can also be a component of a machine (a machine part), such as a rotor blade, for example, of a helicopter or an airplane, or a turbine blade of a turbine, for example, of an airplane or a power plant. Furthermore, as described at the beginning, the body can also include, for example, frames of bicycles, motorcycles, cars, or trucks, as well as pipes for conveying gases or liquids, such as those in drinking water or wastewater systems, or pipes of heating systems or pipes of scaffolding structures, for example, of construction scaffolding. In particular, the aforementioned section must include or exhibit a weld on the body in question. The proposed method can be applied before, during, or after manufacturing or...Further processing can be carried out before, during, or after use of the body. Furthermore, it is possible to perform the procedure before, during, or after use (i.e., operation) of the electronic component or before, during, or after use (i.e., operation) of the machine component or machine, for example, for so-called online monitoring of the body, device, or machine.

[0026] As a rule, direct physical contact between the actuator, sensor, and contact element of the measuring arrangement on the one hand, and the body or part of the body on the other, is not required to carry out the procedure. For example, if the body is an electrical connecting element for electrically connecting two electrical or electronic components, it is sufficient if there is electrical contact between the contact elements of the measuring arrangement and the electrical terminals or contacts of the components to which the connecting element is connected. Furthermore, the actuator can be mechanically coupled to one of the components or be in (contact) contact with it, and transmit a force or bending moment to the connecting element via this component.The components can be semiconductor chips, integrated circuits, or discrete components such as transistors, LEDs, or photodiodes, or even wiring carriers or terminal carriers, such as those found in chip packages. The body can be, for example, a bond wire, which is typically connected to the two components using a wire bonding process, such as thermosonic ball-wedge bonding or ultrasonic wedge-wedge bonding.

[0027] Typically, the current flows from a first end of the subsection to a second end of the subsection opposite the first end, with the subsection extending along a longitudinal extent from its first to its second end. The lateral regions of the subsection, which also typically extend from the first to the second end, border a lateral outer surface of the subsection. This outer surface is typically identical to, or a portion of, a lateral outer surface of the body. Each lateral region of the subsection typically extends in its respective longitudinal extent from the first to the second end of the subsection.

[0028] A neutral layer typically separates the first and second sides of the section, extending along the longitudinal axis of the section from its first end to its second end. This neutral layer, often referred to as the neutral fiber or neutral line in engineering mechanics, is defined by the fact that its length, measured from the first to the second end of the section, remains constant when the section is bent, whereas the corresponding lengths of the two side regions of the section do change when the section is bent, as described above.

[0029] The body can be identical to the subsection. However, the body can also consist of two or more such subsections, whereby the subsections (as well as their first and second side regions) typically adjoin each other in pairs at their ends and thus extend one behind the other along a longitudinal dimension of the body.

[0030] The body can be elongated. For example, the length of the body, measured along its longitudinal axis, can be more than 5, 10, or 50 times its diameter (measured perpendicular to its longitudinal axis). In particular, the body can be a wire, such as a bonding wire. The diameter can range from approximately 10 µm to approximately 800 µm, as is the case with a bonding wire. Typically, the bonding wire has a length between 1 mm and 20 mm. This section is typically identical to the so-called heel of the bonding wire, i.e., the end of the bonding wire that rests on and is firmly connected to a contact surface of a component, and typically has a length between approximately 50 µm and 2 mm.

[0031] The body can also be flat. For example, the body can have the shape of a (possibly curved) sheet of metal, or be a (possibly curved) sheet of metal. The body can then have a width and thickness that are perpendicular to its (already described) longitudinal extent or length, with the thickness of the body typically being at least 10, 50, or 50 times smaller than the longitudinal extent or length of the body. The width can be approximately the same order of magnitude as the length of the body or be smaller than the length by a factor of between approximately 2 and approximately 20.

[0032] The body can be made of a metal, such as aluminum, copper or gold, or an alloy, or of an electrically conductive composite material, in particular a composite material reinforced with carbon fibers.

[0033] The proposed method and measurement setup are described below using examples from [reference to be added]. Fig. The specific embodiments shown in schematic representations 1 and 2a to 2c are explained in more detail below. It shows: Fig. 1 a schematic representation of a measuring arrangement of the type proposed here, which is set up to measure a mechanical degradation of a bond wire using the method proposed here, and Fig. Figures 2a to 2c show a side view of an electrically conductive body in a first bending state, in an equilibrium position and in a second bending state.

[0034] Recurring reference symbols in the figures denote identical or corresponding features.

[0035] In Fig. Figure 1 is a schematic (and not to scale) representation of a specific embodiment of a measuring arrangement 1 of the type proposed here, with which the proposed method for testing an electrically conductive body 2 can be carried out. In this example, the body 2 is an electrical contact element designed as a gold bond wire with a length of approximately 5 mm and a diameter of approximately 300 µm. The bond wire connects the electrical terminals 3 of two electronic components 4, each of which in this example is a semiconductor chip. For example, the bond wire could have been connected to the terminals 3 by thermosonic ball-wedge bonding or ultrasonic wedge-wedge bonding.

[0036] The measuring arrangement 1 comprises a voltage source 5, which is connected to the terminals 3 via two electrical contact elements 6. An electrical voltage is applied to the body 2 by means of the voltage source, causing an electric current to flow through the body 2, and in particular through a section 2 of the body. The voltage source 5 is designed as a constant current source, i.e., it is configured to change the voltage over time so that the current intensity remains as constant as possible. This section 7 is a "heel" region of the bond wire. The section 7 extends longitudinally from a first end 8 of the section 7, where it abuts the terminal 3 and is metallurgically connected to it, to a second end 9 of the section 7, which is located in Fig. 1 is represented as a dashed line. The current flows in one direction along this longitudinal orientation of subsection 7, with this direction in Fig. 1 is represented by an arrow marked I and encloses an angle α of approximately 70° with an upper surface 10 of the component 4 on which the connection 3 is arranged.

[0037] The measuring arrangement 1 comprises an actuator 11 with a piezoelectric element 12, which is connected via a piezoelectric slide (not shown here) to one of the two components 4, here to the left component, and is configured to exert a force on this component 4 that is aligned parallel to the surface 10 of this component 4, wherein the direction of the force is in Fig. 1 is represented by the double arrows labeled F. This periodic force causes component 4 to move periodically back and forth, so that a periodic bending moment is transferred to section 4 and the section is periodically bent. Here, section 7 is periodically bent back and forth between a first bending state and a second bending state. In the first bending state, a first side region 13 of section 7 is elastically stretched and a second side region 14 of section 7 is elastically compressed. In the second bending state, the first side region 13 of section 7 is elastically compressed and the second side region 14 of section 7 is elastically stretched. The two side regions 13 and 14 each extend from the first end 8 to the second end 9 and are separated by a neutral layer 15, which is located in the Fig. 1 is represented by a dot-dash line, separated from each other, with this neutral layer of subsection 7 being defined by the fact that its length does not change when subsection 7 is bent.

[0038] The measuring arrangement 4 comprises a sensor 16, which is configured to measure the time course of a measurand whose measured value changes depending on the instantaneous electrical resistance of the subsection. In the present example, the sensor 16 is configured as a voltmeter; the measurand is therefore the electrical voltage instantaneously applied to the body 2 by the voltage source 5, which, due to the constant current, represents a measure of the resistance of the body 2 and thus also of the subsection 7. The voltage source 5 and the voltmeter 16 therefore form a resistance measuring device 17 of the measuring arrangement 1. The sensor 16 generates a measurement signal that represents the time course of the instantaneous voltage, the signal strength of which is, for example, proportional to the instantaneously measured voltage.

[0039] A frequency filter 18 of the measuring arrangement filters out a signal component from the measurement signal whose frequency corresponds to a predetermined bending frequency of the subsection and forwards it to an evaluation unit 19 of the measuring arrangement 1 for further evaluation. In this embodiment, the frequency filter 18 is designed as a lock-in amplifier connected to a control unit 20 of the measuring arrangement 1. The control unit 20 is configured to generate a sinusoidal control signal and transmit it to the actuator 11 and to the lock-in amplifier 18. (However, a triangular or rectangular control signal would also be possible, as described above.) This periodic control signal determines the temporal profile of the force transmitted by means of the piezoelectric element 13.The signal frequency of this control signal thus defines the aforementioned bending frequency of section 7, at which the section is periodically bent between the first and second bending states, and simultaneously serves as the reference frequency of the frequency filter 18 (i.e., the lock-in amplifier). This ensures that the signal component of the measurement signal filtered out by the frequency filter 17 and evaluated by the evaluation unit 19 corresponds with very high accuracy to the bending frequency, meaning it is caused exclusively by the bending of section 7. (In the case of a temporally triangular or rectangular force, signal components of the measurement signal corresponding to integer multiples of the bending frequency would preferably also be filtered out and analyzed, for example, by means of additional lock-in amplifiers driven with corresponding reference frequencies.)In this way, interference from the measurement signal is largely eliminated, and particularly high sensitivity and measurement accuracy are achieved.

[0040] The bending frequency is, for example, constant at 2 Hz. However, a different bending frequency could also be selected, preferably within the ranges specified above. During the process, section 7 is, for example, only bent back and forth periodically 20 times between the first and second bending states, so that the bending process is completed after 10 seconds and the mechanical stress on body 2 caused by the process is minimized. The amplitude of the filtered-out (sinusoidal) signal component is evaluated by the evaluation unit 19 as a characteristic parameter for the mechanical condition of body 2, in particular section 7, by comparing it, for example, with reference values ​​previously measured on a reference body corresponding to the bond wire in question, and from this comparison, for example, a crack depth of any cracks present within section 7 is derived.For example, the remaining service life of the body 2 or the connection made by the bond wire can also be derived from this using the evaluation unit 19. The procedure can be carried out before, during, and after commissioning of the components 4. In principle, it is possible for the measuring arrangement 1 to be integrated together with the components 4 in a common housing for regular online monitoring of the components 4.

[0041] In principle, it would also be possible to bend section 7 for checking body 2 more frequently, for example several hundred or several thousand times, for instance to carry out random quality control during the production of components 4. The evaluation unit 19 can be configured to characterize any cracks present based on a temporal change in the amplitude of the filtered signal component, whereby a linearly increasing amplitude over time is assigned to unilateral crack formation in exactly one of the two side regions 13, 14, and whereby an amplitude that initially decreases linearly and then increases hyperbolically over time is assigned to crack formation in both side regions 13, 14 simultaneously.

[0042] In Fig. 2a to 2c is subsection 7 of the in Fig. 1 Body 3 shown in the first bending state described above, see Fig. 2a, in a middle position in which no bending moment is transferred to the subsection by means of actuator 11, see Fig. 2b, and in the second bending state, see Fig. Figure 2b, a highly schematic and not to scale side view, shows that in the first bending state, a crack 21 in the first side region 13 is open, while two cracks 22 in the second side region 14 are closed. In the equilibrium position, however, all cracks 21 and 22 are closed, and in the second bending state, only the cracks in the second side region 14 are open. The opening and closing of cracks 21 and 22 during the bending of the section 7 changes its cross-sectional area and thus also its electrical resistance between the first end 8 and the second end 9. This leads to the described fluctuations in the measured voltage.

[0043] The two bending states are in Fig. 2a and Fig. Figure 2c is exaggerated. Typically, a less pronounced bending, i.e., smaller bending amplitudes, is sufficient to open and close even very small cracks and thus make them detectable by the method. In the present example, exceeding the elastic limit to the elastic-plastic region or the plastic region of subsection 7 is avoided as completely as possible. To this end, the maximum bending amplitude when bending the subsection is less than one-sixth of the diameter of subsection 7. Reference symbol list: 1 Measuring setup 2 bodies 3 connection 4 component 5 Voltage source 6 contact element 7 Subsection 8 first end 9 second end 10 surface 11 Actuator 12 Piezoelectric elements 13 first page area 14 second page area 15 neutral layer 16 Sensor 17 Resistance measuring device 18 frequency filters 19 evaluation units 20 Control unit 21. Crack in the first side area 22. Crack in the second side area

Claims

[1] Method for testing an electrically conductive body (2), - wherein an electrical voltage is applied to the body (2) so that an electrical current flows through at least a partial section (7) of the body (2), - wherein the partial section (7) is bent repeatedly over time at a bending frequency, wherein during the bending of the partial section (7) a first side region (13) of the partial section (7) is stretched and simultaneously a second side region (14) of the partial section (7) is compressed or the first side region (13) is compressed and simultaneously the second side region (14) of the partial section (7) is stretched, - wherein a temporal profile of a measured variable which changes as a function of a momentary electrical resistance of the subsection (7) is measured and temporal fluctuations which correspond to the bending frequency are filtered out of the temporal profile of the measured variable by means of a narrow-band frequency filter (18) and subsequently evaluated. [2] Method according to claim 1, characterized by that the narrow-band frequency filter (18) has a frequency band, wherein the frequency band comprises the bending frequency or exactly an integer multiple of the bending frequency as the frequency to be measured. [3] Method according to one of the preceding claims, characterized bythat the measured variable is measured by means of a sensor (16), wherein the sensor (16) generates a measuring signal which changes as a function of the instantaneous electrical resistance of the sub-section (7), wherein a signal component whose frequency corresponds to the bending frequency is filtered out of the measuring signal and this signal component is subsequently evaluated. [4] Method according to claim 3, characterized by that the said signal component is filtered out by means of the narrowband frequency filter (18). [5] Method according to claim 4, characterized by that the frequency filter (18) is a lock-in amplifier. [6] Method according to one of the preceding claims, characterized by that the partial section (7) is bent by means of an actuator (11) which can be controlled by control signals, wherein the bending frequency for the temporally repeated bending of the partial section (7) is predetermined by means of the control signals. [7] Method according to claims 5 and 6, characterized by that a signal frequency of the control signal specifying the bending frequency is used as a reference frequency for the frequency filter (18) for filtering out the said signal component of the measuring signal. [8] Method according to one of the preceding claims, characterized by that the bending frequency is less than 20 Hz. [9] Method according to one of the preceding claims, characterized by that by means of a force acting on the partial section (7) and varying sinusoidally, triangularly or rectangularly with the bending frequency, a bending moment is generated which varies periodically with the bending frequency for the temporally repeated bending of the partial section. [10] Method according to claim 9, characterized by that the force acts on the sub-section (7) transversely to a flow direction of the electric current through the sub-section (7). [11] Method according to one of the preceding claims, characterized by that the temporally repeated bending of the partial section (7) is an elastic deformation of the partial section (7). [12] Method according to one of the preceding claims, characterized by that the voltage applied to the body (2) is varied over time such that the current has a temporally constant current intensity, wherein the said measured variable varies as a function of the applied voltage and is preferably proportional to the applied voltage. [13] Method according to one of the preceding claims, characterized by that an amplitude of the temporal fluctuations of the measured quantity is used as a parameter for a mechanical condition, a degradation or a remaining lifetime of the body (2). [14] Method according to claim 13, characterized by that a temporal progression of the amplitude of the fluctuations of the measured variable is recorded and analyzed, whereby - a temporally linearly increasing amplitude is assigned to a crack formation that develops in exactly one of the two side areas of the section (7), and - a temporally linearly decreasing amplitude as well as a hyperbolically increasing amplitude is assigned to a crack formation that develops simultaneously in both side areas of the section (7). [15] Method according to one of the preceding claims, characterized by that the body (2) is a bonding wire or another electrical connecting element of an electronic component (4) or a sheet or a component made of a carbon fiber composite material or a component of a machine, a turbine blade or a rotor blade or a frame of a vehicle, a pipe for conducting a flowable medium or a pipe of a framework structure. [16] Method according to one of the preceding claims, characterized bythat the process is carried out before, during or after production or further processing of the body (2) or before, during or after use of the body (2). [17] Measuring arrangement (1) for checking an electrically conductive body (2), comprising: - a voltage source (5) with electrical contact elements (6) for applying an electrical voltage to the body (2) so that an electrical current flows through at least a partial section (7) of the body (2), - an actuator (11) which is designed to bend the partial section (7) repeatedly over time at a bending frequency, wherein during the bending of the partial section (7) a first side region (13) of the partial section (7) is stretched and simultaneously a second side region (14) of the partial section (7) is compressed or the first side region (13) of the partial section (7) is compressed and simultaneously the second side region (14) of the partial section (7) is stretched, - a sensor (16) which is designed to measure a temporal course of a measured variable which changes as a function of a momentary electrical resistance of the subsection (7), - a narrow-band frequency filter (18) which is designed to filter out fluctuations corresponding to the bending frequency of the section (7) from the temporal course of the measured variable, and - an evaluation unit (19) which is arranged to evaluate the filtered fluctuations which correspond to the bending frequency of the partial section (7). [18] Measuring arrangement (1) according to claim 17, characterized by that the narrow-band frequency filter (18) has a frequency band, wherein the frequency band comprises the bending frequency or exactly an integer multiple of the bending frequency as the frequency to be measured. [19] Measuring arrangement (1) according to one of claims 17 or 18, characterized bythat it is arranged to carry out the method according to one of claims 1 to 16.

Citation Information

Patent Citations

  • Examination of the condition of a connection between components

    DE102010041391A1

  • Sensor device and method for detecting and locating cracks in components

    DE102012006155A1

  • Testing surfaces for inhomogeneities

    DE4342685A1

  • Vibration Based Damage Detection System

    US20100089161A1