Aluminium oxide sintered bodies and methods for their production

DE102015001547B4Active Publication Date: 2024-10-17ATECT CORP
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
DE102015001547
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2014-02-14
Filing Date
2015-02-06
Publication Date
2024-10-17
Estimated Expiration
2035-02-06
Patent Text Reader

Abstract

Aluminium oxide sintered bodies containing 0.3 to 3.0 volume% cubic aluminium nitride, wherein the thermal conductivity is 35 W / m·k or more and the infrared emissivity is 0.60 or more.
Need to check novelty before this filing date? Find Prior Art

Description

BACKGROUND OF THE INVENTION(1) Technical Field of the InventionThe present invention relates to an alumina sintered body and a method for producing the alumina sintered body.(2) Description of the Prior ArtA computer or an automatic control unit of an automobile or the like is equipped with a heat dissipation part to suppress the deterioration of performance due to an increase in the heat generation amount associated with a large current. In recent years, a heat dissipation sintered substrate made of ceramic material has attracted attention as a heat dissipation member in terms of improved heat dissipation performance, productivity, manufacturing cost, and the like.From the viewpoint of heat dissipation, such a heat dissipation sintered substrate made of ceramic material needs to have not only basic characteristics such as an electrical insulation property but also high thermal conductivity and high infrared ray emissivity. As a material for the heat dissipation sintered substrate, aluminum nitride (AlN), for example, has been used heretofore. However, the AlN heat dissipation substrate exhibits considerably poor water resistance, particularly chemical resistance to an alkaline aqueous solution, and thus has a problem that mounting a circuit on the substrate is technically difficult. For example, the AIN heat dissipation substrate is required to be subjected to surface treatment to provide high chemical resistance by intentionally oxidizing the surface layer to a depth of about several hundred μm, so that the manufacturing cost is increased.Accordingly, a ceramic material replacing aluminum nitride, which has high chemical resistance as well as high electrical insulation property, high thermal conductivity, and high infrared ray emissivity, is desirable. Many of the ceramic materials are produced by a so-called "sintering" method in which a raw material powder is fired to solidify, and an alumina sintered body is one of the typical sintered bodies. The alumina sintered body has a high insulating property and exhibits excellent chemical resistance.It is known that properties which an alumina sintered body alone cannot exhibit can be imparted to the alumina sintered body by selecting an additive used during sintering. For example, Ando et al., "Material No. 52", pages 1464-1470, published in 2003, disclose that when silicon carbide is used as a sintering additive with alumina (Al 2 O 3), which is used as a base material, a sintered body having a mechanical strength three times as high as that of a conventional alumina alone is obtained. In addition, JP H03-112 846 A describes a method for producing a sintered ceramic body excellent in degreasing performance and sinterability, which is applicable to ceramic substrates. Furthermore, JP 2006-327 933 A describes a transparent PCA ceramic, ceramic discharge vessels and methods for producing the same.An alumina sintered body known heretofore exhibits excellent electrical insulating property and chemical resistance, but has low thermal conductivity and low infrared ray emissivity. It is difficult to apply an alumina sintered body having low thermal conductivity and low infrared ray emissivity to a substrate of a heat dissipation member.As mentioned above, a ceramic material which has high thermal conductivity and high infrared ray emissivity and which exhibits excellent electrical insulation property and chemical resistance is desirable, but one which satisfies all these properties and can be suitably used as a substrate of a heat dissipation member has not been found yet.In view of the above circumstances, the main object of the present invention is to provide an alumina sintered body which has high thermal conductivity and high infrared ray emissivity and exhibits excellent electrical insulation property and chemical resistance.SUMMARY OF THE INVENTIONThe present inventor has made extensive studies to achieve the above-mentioned objects. As a result, the present inventor found that an alumina sintered body containing cubic aluminum nitride has high thermal conductivity and high infrared ray emissivity and exhibits excellent electrical insulation property and chemical resistance. Moreover, the present inventor found that the alumina sintered body having the above excellent properties can be produced by a suitable method in which an alumina powder having a specific particle size is fired in a reducing nitrogen atmosphere. The present invention is an invention which has been completed by further conducting studies based on the above results.That is, the present invention provides an invention according to appended claims 1 to 6.According to the present invention, there can be provided an alumina sintered body which has high thermal conductivity and high infrared ray emissivity and exhibits excellent electrical insulation property and chemical resistance. The alumina sintered body according to the present invention can be suitably used as an insulation substrate, a substrate of a heat dissipation member, a semiconductor packaging material, or the like. According to the present invention, there can be further provided a production method by which an alumina sintered body having the above-mentioned excellent properties is suitably obtained.DETAILED DESCRIPTION OF THE INVENTIONAn alumina sintered body of the present invention contains cubic aluminum nitride. A method for producing an alumina sintered body according to the present invention includes a sintering step of firing an alumina powder having an average particle size of 10 μm or less in a reducing nitrogen atmosphere. The alumina sintered body and the method for producing the alumina sintered body according to the present invention will be described in detail below.1. Alumina sintered bodyThe alumina sintered body of the present invention contains cubic aluminum nitride (cAlN). More specifically, the alumina sintered body of the present invention has a structure in which cubic aluminum nitride is dispersed in a matrix of alumina (Al 2 O 3). The alumina sintered body of the present invention therefore has high thermal conductivity and high infrared ray emissivity, and exhibits excellent electrical insulation property and chemical resistance. That is, since cubic aluminum nitride having high thermal conductivity is dispersed in a matrix of alumina, the thermal conductivity and the infrared ray emissivity are increased compared to conventional alumina sintered bodies. The alumina sintered body includes cubic aluminum nitride generally having a zincblende type structure.The proportion of cubic aluminum nitride in the alumina sintered body of the present invention is 0.3 to 3.0 volume %, preferably about 0.4 to 2.5 volume %, more preferably about 0.5 to 2.0 volume %, in order to ensure that the alumina sintered body exhibits excellent electrical insulation property and chemical resistance, and has enhanced thermal conductivity and infrared ray emissivity.The alumina sintered body of the present invention may contain aluminum oxynitride (AINO). Aluminum oxynitride has a thermal conductivity higher than that of alumina, and thus the thermal conductivity and the infrared ray emissivity can be increased compared to conventional alumina sintered bodies when aluminum oxynitride is contained in a matrix of alumina. The content of aluminum oxynitride in the alumina sintered body of the present invention is not particularly limited, but is preferably about 0.5 to 10.0% by volume, more preferably about 0.5 to 9.0% by volume, further preferably about 0.5 to 8.0% by volume, in order to ensure that the alumina sintered body exhibits excellent electrical insulation property and chemical resistance, and has increased thermal conductivity and an increased infrared ray emissivity.The proportion of a phase formed of a component other than alumina, such as aluminum nitride or aluminum oxynitride, in the alumina sintered body of the present invention is a value measured by X-ray powder diffractometry using an X-ray powder diffractometer "SmartLab" manufactured by Rigaku Corporation. The proportion (volume percent) of a phase formed of a component other than alumina is a value calculated from an intensity ratio of the strongest peak of each phase to the intensity of the (113) diffraction peak of alumina.As described later, in the method for manufacturing an alumina sintered body according to the present invention, an organic binder, a sintering aid, or the like may be mixed in addition to an alumina powder as a raw material provided to firing. Therefore, the alumina sintered body of the present invention may contain components derived from an organic binder, a sintering aid, and so forth, in addition to alumina, aluminum nitride, and aluminum oxynitride.The component derived from an organic binder in the alumina sintered body of the present invention is, for example, carbon. The content of carbon in the alumina sintered body of the present invention is not particularly limited, but is preferably 150 ppm or less, more preferably less than 100 ppm. The content of carbon in the alumina sintered body is a value measured in accordance with JIS-R1675 using an in-solid carbon meter "EMIA-110" manufactured by HORIBA, Ltd.The component derived from a sintering aid in the alumina sintered body of the present invention varies depending on the kind of the sintering aid, and the alumina sintered body contains an inorganic component which is not evaporated by the firing. For example, when yttrium oxide is used as a sintering aid, YAG (Y 3 Al 5 O 12) or the like may be contained. The proportion of a component derived from a sintering aid in the alumina sintered body of the present invention varies depending on the kind of the sintering aid, etc., but is usually about 0.5 to 10.0 volume %, preferably about 0.5 to 8.0 volume %, more preferably about 0.5 to 7.5 volume %. The method for determining the proportion of a component derived from a sintering aid in the alumina sintered body is similar to the method for determining the proportion of a phase formed from a component other than alumina.The thermal conductivity of the alumina sintered body of the present invention is 35 W / m·k or more, preferably 41 W / m·k or more. Accordingly, the alumina sintered body of the present invention has very high thermal conductivity as an alumina sintered body. The thermal conductivity of the alumina sintered body of the present invention is usually 100 W / m·k or less. In the present invention, the thermal conductivity of the alumina sintered body is a value measured at room temperature (25° C.) by a laser flash method using "TC-7000" manufactured by ULVAC-RIKO, Inc.The infrared ray emissivity of the alumina sintered body of the present invention is 0.60 or more. The infrared ray emissivity of the alumina sintered body of the present invention is usually 0.95 or less. In the present invention, the infrared ray emissivity of the alumina sintered body is a value measured at room temperature (25° C.) in accordance with JIS-R16932 using a Fourier transform infrared spectrometer "FT-IR System 2000" manufactured by PerkinEl Co., Ltd.The volume resistivity of the alumina sintered body of the present invention is usually more than 10 14 Ωcm. If the volume resistivity is more than 10 14 Ωcm, the alumina sintered body can be suitably used as a heat dissipation member of a computer or an automatic control unit of an automobile or the like because the electrical insulation property is sufficiently high. The volume resistivity of the alumina sintered body is a value measured at room temperature (25° C.) in accordance with JIS-K6911 using "HIGHRESER" manufactured by Mitsubishi Chemical Corporation.The bending strength of the alumina sintered body of the present invention is preferably 300 MPa or more. If the bending strength is 300 MPa or more, the alumina sintered body can be suitably used as a heat dissipation member of a computer or an automatic control unit of an automobile or the like because the alumina sintered body has sufficient strength. The bending strength of the alumina sintered body of the present invention is usually 440 MPa or less. The bending strength of the alumina sintered body is a value determined by measuring a three-point bending strength at room temperature (25° C.) in accordance with JIS-R1601 using "AUTOGRAPH AG-20kNG" manufactured by Shimadzu Corporation.The alumina sintered body of the present invention has excellent chemical acid and caustic resistance. For example, the alumina sintered body of the present invention has a mass loss rate of less than 0.1 mass % when, for example, an alumina sintered body test piece (surface area: 5.3 cm 2) is immersed in a 6N NaOH aqueous solution at 100° C. for 16 hours. For example, the alumina sintered body has a mass decrease rate of less than 0.01 mass % when an alumina sintered body test piece (surface area: 5.3 cm 2) is immersed in a 1N H 2 SO 4 aqueous solution at 100° C. for 16 hours. Since the alumina sintered body of the present invention has excellent chemical acid and caustic resistance, a circuit is more easily mounted as compared with aluminum nitride.The density of the alumina sintered body of the present invention is not particularly limited, but is usually about 3.80 to 4.00 g / cm 2, preferably about 3.85 to 3.98 g / cm 2.The alumina sintered body of the present invention can be suitably used as an insulation substrate, a substrate of a heat dissipation member, a semiconductor packaging material, or the like, because the alumina sintered body has high thermal conductivity and high infrared ray emissivity and exhibits excellent electrical insulation property and chemical resistance.2. Method for Producing Alumina Sintered BodyThe method for producing an alumina sintered body according to the present invention includes a sintering step of firing an alumina powder having an average particle size of 10 μm or less in a reducing nitrogen atmosphere.The average particle size of an alumina powder to be used as a starting material of the alumina sintered body of the present invention needs to be 10 μm or less. By firing such a fine alumina powder in a reducing nitrogen atmosphere, it can be ensured that the alumina sintered body exhibits excellent electrical insulation property and chemical resistance, and has enhanced thermal conductivity and infrared ray emissivity. The average particle size of the alumina powder is preferably about 0.6 to 5 μm in order to further improve these properties of the alumina sintered body. If the particle size of the alumina raw material powder is more than 10 μm, the crystal particle size after sintering increases, so that the density and thermal conductivity of the sintered body are easily decreased. If the particle size of the alumina powder is less than 0.5 μm, it is difficult to produce an alumina sintered body, and therefore, the average particle size of the alumina powder is preferably 0.5 μm or more.According to the present invention, the average particle size of the alumina powder to be used as a starting material is a volume-based D50 particle size measured using a laser diffraction particle size distribution meter (FPIA-3000 manufactured by Sysmex Corporation).According to the present invention, it is necessary to carry out sintering of the alumina powder in a reducing nitrogen atmosphere. Here, the reducing nitrogen atmosphere means an atmosphere including a gas containing nitrogen components other than an air atmosphere including oxygen gas (O 2) etc. Specific examples of gases constituting the reducing nitrogen atmosphere include nitrogen (N 2) and ammonia (NH 3). According to the present invention, cubic aluminum nitride can be efficiently produced by sintering the alumina powder in a reducing nitrogen atmosphere. The gases constituting the reducing nitrogen atmosphere may be used alone or in combination of two or more thereof. As long as the reductive nitration reaction of the alumina powder is not impaired, a gas other than the gas containing nitrogen components may be enclosed in the reducing nitrogen atmosphere.According to the present invention, it is preferable to burn a sintering aid together with the alumina powder. Thereby, the sintering of the alumina sintered body of the present invention can be promoted. The sintering aid is not particularly limited, and a known sintering aid used in an alumina sintered body may be used. Examples of the preferable sintering aid include boron compounds, alkaline earth metal compounds and rare earth compounds. The sintering assistants may be used alone or in combination of two or more thereof.Specific examples of the boron compound include oxides such as boric acid, boron trioxide (boric anhydride), and aluminum borate. Among them, boric acid and boron trioxide (boric anhydride) are more preferred in order to further improve the thermal conductivity of the alumina sintered body.Concrete examples of the alkaline earth metal compound include oxides of metals such as magnesium, calcium, strontium and barium, carbonates of these metals and stearates of these metals. Among them, oxides and carbonates of calcium such as calcium oxide, calcium aluminate and calcium carbonate, calcium stearate and the like are more preferred in order to further improve the thermal conductivity of the alumina sintered body.Concrete examples of the rare earth compound include oxides of metals such as yttrium and lanthanum, and carbonates of these metals. Among them, yttrium oxide and the like are more preferred in order to further improve the thermal conductivity of the alumina sintered body.Among these sintering aids, boron compounds and alkaline earth metal compound are preferred, with boron trioxide and calcium stearate being particularly preferred.The particle size of the sintering aid is not particularly limited, but is preferably 10 μm or less, more preferably 5 μm or less, because the sintering aid becomes more active as its particle size decreases. A sintering aid soluble in water or alcohol, such as boron trioxide and calcium stearate, may be added to an alumina raw material powder, the sintering aid being dissolved in water or alcohol, followed by mixing the mixture using a method such as granulation.The amount of the sintering aid added is not particularly limited, but is preferably about 0 to 10 parts by mass, more preferably about 0.1 to 5 parts by mass, based on 100 parts by mass of the alumina powder. If the added amount of the sintering aid is set to fall within the above range, the density and thermal conductivity of the obtained alumina sintered body can be further increased. If the added amount of the sintering aid is 5 parts by mass or more, highly thermally conductive components such as cubic aluminum nitride and aluminum oxynitride formed by the reductive nitration reaction of the alumina powder easily make it difficult to compact an alumina sintered body base material. Therefore, the density of the alumina sintered body decreases, so that the thermal conductivity is easily lowered.According to the present invention, the mixed powder of the alumina powder and the sintering aid is obtained by known mixing methods. The mixing method is, for example, a method in which the mixing is performed in a dry method or a wet method using a mixer such as a ball mill. If mixing is carried out in a wet process, a dispersant such as water, an alcohol or the like is used, and from the standpoint of dispersibility, use of an alcohol is desirable.According to the present invention, it is preferable to burn an organic binder together with the alumina powder. Thereby, the shape stability of the alumina sintered body of the present invention can be improved.The organic binder is not particularly limited, and a known organic binder may be used. Specific examples of the organic binder include acrylic resins such as polymethacrylic butyl, polyolefin-based resins such as polystyrene and polypropylene, butyral resins such as polyvinyl butyral, and ethylene-vinyl acetate copolymers. The organic binders may be used alone or in combination of two or more thereof.In the case where the organic binder is used, the amount of the organic binder added is not particularly limited, but is preferably about 0.1 to 30 parts by mass, more preferably about 1 to 20 parts by mass, based on 100 parts by mass of the alumina powder. If the amount of the organic binder added is less than 0.1 parts by mass, it is difficult to obtain an alumina sintered body having a desired shape. If the amount of the organic binder added exceeds 30 parts by mass, an alumina sintered body shaped into the desired shape is obtained, but in the degreasing method described below, excessive shrinkage may occur, resulting in deformation.According to the present invention, in addition to the organic binder, a lubricant can be used when an alumina sintered body is molded by a method such as powder injection molding. Specific examples of the lubricant include oils and fats such as paraffin wax, montanic acid ester wax and carnauba wax, and fatty acid amides such as stearic acid amide.If the organic binder is used, the method for mixing the organic binder is not particularly limited. The organic binder may be added and mixed during the production of the mixed powder of the alumina powder and the sintering aid, for example. The alumina powder, the sintering aid, and the organic binder may be simultaneously added and kneaded using a known powder kneader such as LABO PLASTOMILL.In the case where the sintering aid agent, the organic binder, etc. are fired together with the aluminum powder according to the present invention, a composition containing these components may be fired together with the aluminum powder to form an alumina sintered body. Further, such a composition containing an alumina powder is shaped and then fired to obtain an alumina sintered body shaped into a desired shape. The method for forming a composition containing an alumina powder is not particularly limited, and a known method can be used. A known powder melting method such as powder injection molding, compression molding or plate molding using a doctor blade method can be used.The firing temperature (maximum firing temperature) in the sintering step is not particularly limited, but is preferably about 1600 to 1825° C., more preferably about 1700 to 1825° C., in order to ensure that the alumina sintered body exhibits excellent electrical insulation property and chemical resistance, and has increased thermal conductivity and an increased infrared ray emissivity. If the firing temperature is lower than 1600°C, the reductive nitration reaction of alumina will proceed with difficulty, so that an alumina sintered body having a desired high thermal conductivity could not be obtained even if the firing is carried out for a long time. If the firing temperature is higher than 1825° C., alumina having a low thermal conductivity and a spinel structure (γ-Al 2 O 3) is excessively generated, so that the thermal conductivity of the alumina sintered body is easily lowered.The firing time in the sintering step is preferably about 0.5 to 10 hours, more preferably about 1 to 5 hours, in order to ensure that the alumina sintered body exhibits excellent electrical insulation property and chemical resistance, and has enhanced thermal conductivity and infrared ray emissivity. From a similar standpoint, the pressure during sintering is preferably about 0.1 to 2.0 atm. If the firing time is less than 0.5 hour, sintering does not proceed sufficiently and therefore it is difficult to obtain an alumina sintered body having a high thermal conductivity. On the other hand, if the firing time exceeds 10 hours, the generation of a highly thermally conductive component by the reductive nitration reaction of the alumina powder, i.e., improvement in the thermal conductivity of the alumina sintered body, reaches the highest level.According to the present invention, it is preferable that, before the sintering step, a degreasing step of firing a composition containing the alumina powder and the organic binder is performed at a temperature lower than that in the sintering step. The degreasing step is performed in the reducing nitrogen atmosphere. It is considered that, by the degreasing step, the organic binder joined with the alumina powder is carbonized to generate carbon in the sintered body, and the carbon serves as a catalyst in the reductive nitration reaction of the alumina in the firing step, so that a reaction for generating cubic aluminum nitride in an alumina base phase is promoted.The degreasing temperature (maximum temperature) varies depending on the type of the organic binder, but is preferably about 250 to 900° C., more preferably 300 to 800° C., in order to promote the generation of cubic aluminum nitride, aluminum oxynitride, or the like. If the degreasing temperature is lower than 250° C., organic binder components easily remain as impurities in the alumina sintered body. If the degreasing temperature is higher than 900° C., excessive shrinkage occurs in the degreasing step, so that the alumina sintered body is easily deformed.The degreasing time in the degreasing step is not particularly limited as long as degreasing of the organic binder can be caused to sufficiently proceed, but the degreasing time is preferably about 5 to 70 hours, more preferably about 15 to 50 hours.For example, in the case where the organic binder is fired together with the alumina powder according to the present invention, it is considered that the reductive nitration reaction of the alumina powder is promoted by carbon in a nitrogen atmosphere according to the following reaction formula (1): Al 2 O 3+ 3 C+N 2 → 2AlN+3CO (1).It is considered that cubic cAlN is efficiently produced at the grain boundary or in the grain of the Al 2 O 3 base phase due to the above-described reaction. That is, it is considered that an alumina sintered body having high thermal conductivity is synthesized by the reductive nitration reaction between the surface of the alumina base phase and nitride using carbon as a catalyst produced from the organic binder. This alumina sintered body is considered to have a structure in which very fine cubic aluminum nitride particles are dispersed in a matrix of alumina, thereby enhancing the thermal conductivity of the alumina sintered body.According to the present invention, it is considered that the reductive nitration reaction of the alumina powder is promoted by using a sintering aid. For example, in the case where calcium oxide is used as the sintering aid, it is considered that, by sintering the alumina powder in a nitrogen atmosphere, a reaction in which an intermediate CaO-Al 2 O 3 produced to an intermediate point reacts with nitrogen in the presence of carbon to cause cubic aluminum nitride as a highly thermally conductive component in an alumina base phase by successive reactions as shown in the following chemical reaction formulae (2) to (4), To produce: CaO •2Al 2 O 3+ 3 C + N 2 → CaO •Al 2 O 3+ 2 AlN + 3CO (2) 12(CaO •Al 2 O 3) + 15 C + 5N 2 → 12CaO •7Al 2 O 3+ 10 AlN + 15CO (3) 12CaO •7Al2O3 + 21C + 7N2→14AlN + 12CaO + 21CO (4).Further, it is considered that, as shown in the chemical reaction formula (4), removal of an additive-derived compound such as CaO by thermal decomposition, etc. is simultaneously released because the reductive nitration reaction proceeds upon firing the alumina powder, and as a result, an alumina sintered body in which AlN having a high thermal conductivity is uniformly present in an alumina base phase is obtained.According to the present invention, the degreasing step and the sintering step can be performed by, for example, purging the inside of a fixed-seal furnace with nitrogen, an ammonia gas, or the like, placing a firing vessel (setter) formed of a material made of ceramic such as aluminum nitride or boron nitride in the fixed-seal furnace, and firing an alumina powder (a composition containing an alumina powder) in the setter in a reducing nitrogen atmosphere.ExamplesThe present invention will be described in more detail below by way of Examples and Comparative Examples. However, it should be noted that the present invention is not limited to the examples.In the examples and comparative examples, various kinds of physical properties, etc. of the alumina sintered body were measured as follows.<>Measurement was performed at room temperature (25° C.) in accordance with JIS-R1634 using an in-water weighing method.<>Measurement was performed at room temperature (25° C.) by a laser flash method using "TC-7000" manufactured by ULVAC-RIKO, Inc.< Emissivity>Measurement was performed at room temperature (25° C.) in accordance with JIS-R16932 using a Fourier transform infrared spectrometer "FT-IR System 2000" manufactured by PerkinEl Co., Ltd.< Durability Test>Alumina sintered body specimens (surface area: 5.3 cm 2) were immersed in a 6N NaOH aqueous solution (alkaline) at 100° C. and a 1N H 2 SO 4 aqueous solution (acidic) at 100° C. for 16 hours, respectively, and the resulting mass decrease rate was measured from each specimen.<Beurteilung of Electrical Insulation Property by Measurement of Resistivity>Measurement was performed at room temperature (25° C.) in accordance with JIS-K6911 using "HIGHRESER" manufactured by Mitsubishi Chemical Corporation.<Identifiy of Crystal Phase of Component Other than Alumina>X-ray powder diffractometry was carried out using an X-ray powder diffractometer "SmartBac" manufactured by Rigaku Corporation. The proportion (volume percent) of a phase formed of a component other than alumina was calculated from an intensity ratio of the strongest peak of each phase to the intensity of the (113) diffraction peak of alumina.<>A three-point bending strength was measured at room temperature (25° C.) in accordance with JIS-R1601 using "AUTOGRAPH AG-20kNG" manufactured by Shimadzu Corporation.<Carbon Content>Measurement was carried out in accordance with JIS-R1675 using an In-Solid Carbon Meter "EMIA-110" manufactured by HORIBA, Ltd.<Mittlere Particle Size of Alumina Powder>The average particle size of the alumina powder used as the starting material means a volume-based D50 particle size measured using a laser diffraction particle size distribution meter (FPIA-3000 manufactured by Sysmex Corporation).< 1 to 12>To 100 parts by mass of an alumina powder (average particle size: 0.9 μm), 7.0 parts by mass of polymethacrylic butyl, 5.0 parts by mass of an ethylene-butadiene copolymer, and 6.0 parts by mass of paraffin wax as an organic binder were added, and the mixture was heated with LABO PLASTOMILL and kneaded at 140° C. to pellet it. In Examples 6 to 12, 1 part by mass of each of the additives described in Table 1 was added to 100 parts by mass of alumina. Subsequently, the pellet was molded into a round shape having a thickness of 2.2 mm and a diameter of 15 mm using a powder injection molding machine. The obtained molded product was placed in a container made of boron nitride, heated and degreased at 800° C. at maximum for 20 hours, and then held at a maximum temperature set to a temperature shown in Table 1 for 3 hours, so that the molded product was sintered. Physical properties of the obtained alumina sintered bodies are shown in Table 1.< Example 1>An alumina sintered body was obtained in the same manner as in Example 3 except that the molded product was sintered in the air under normal pressure. Physical properties of the obtained alumina sintered bodies are shown in Table 1. Table 1 Table 1Comparison 1Air Airnone none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none17803,928>10 140,58Acid < 0,01no no no no no no no no no no no no no no no no no no no no no no no no no no no no no no no no no no no no no370< 100Alkali<0..,1Example 1Nitrogen Nitrogennone none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none17803,951>10 140,82Acid < 0,01cAlN (1.1) AlNO (4.3)370< 100Alkali<0..,1Example 2Nitrogen Nitrogennone none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none18003,949>10 140,81Acid < 0,01cAlN (1.0) AlNO (5.1)380< 100Alkali<0..,1Example 3Nitrogen Nitrogennone none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none none18253,941>10 140,82Acid < 0,01cAlN (2.5) AlNO (7.6)420< 100Alkali<0..,1Example 4Nitrogen NitrogenYttrium oxide (1)1780448>10 140,68Acid < 0,01cAlN (1.6) AlNO (3.2) YAG (5.1)300< 100Alkali<0..,1Example 5Nitrogen NitrogenYttrium oxide (1)1825445>10 140,61Acid < 0,01cAlN (1.6) γAl 2 O 3 (5,2) AlNO (4.8) YAG (7.1)320< 100Alkali<0..,1Example 6Nitrogen NitrogenCalcium stearate (1)17803,972>10 140,77Acid < 0,01cAlN (1.4) AlNO (3.6)340< 100Alkali<0..,1Example 7Nitrogen NitrogenCalcium stearate (1)17003,944>10 140,75Acid < 0,01cAlN (0.5) AlNO (3.3)340< 100Alkali<0..,1Example 8Nitrogen NitrogenCalcium stearate (1)17803,972>10 140,77Acid < 0,01cAlN (1.4) AlNO (3.6)340< 100Alkali<0..,1Example 9Nitrogen NitrogenCalcium stearate (1)18253,959>10 140,78Acid < 0,01cAlN (1.9) γAl 2 O 3 (5,1) AlNO (3.6)350< 100Alkali<0..,1Example 10Nitrogen NitrogenBoron oxide (1)17003,951>10 140,73Acid < 0,01cAlN (0.7) AlNO (1.6)350< 100Alkali<0..,1Example 11Nitrogen NitrogenBoron oxide (1)17803,985>10 140,78Acid < 0,01cAlN (1.2) AlNO (4.1)320< 100Alkali<0..,1Example 12Nitrogen NitrogenBoron oxide (1)18253,963>10 140,76Acid < 0,01cAlN (1.9) γAl 2 O 3 (1,1) AlNO (3.9)350< 100Alkali<0..,1In Table 1, AINO represents aluminum oxynitride. YAG represents Y 3 Al 5 O 12 cAlN represents cubic (zincblende type structure) aluminum nitride. γAl 2 O 3 represents alumina of spinel structure.As shown in Table 1, the alumina sintered bodies of Examples 1 to 12 in which the sintering was performed in a nitrogen atmosphere had a high thermal conductivity of 41 to 85 W / m·k. In each of the alumina sintered bodies of Examples 1 to 12, a cubic (zinc-blende-type structure) aluminum nitride phase (cAlN) believed to contribute to the high thermal conductivity of the alumina sintered body was observed. The alumina sintered bodies of Examples 1 to 12 exhibited a relatively high infrared ray emissivity of 0.61 to 0.82, and it was also confirmed that the alumina sintered bodies of Examples 1 to 12 have a high volume resistivity and bending strength and excellent chemical resistance. On the other hand, the alumina sintered body of Comparative Example 1 in which sintering was carried out in air showed a low thermal conductivity of 28 W / m·k, and showed a much inferior infrared ray emissivity than Example 3 using the same maximum sintering temperature. In the alumina sintered body of Comparative Example 1, a cubic (zincblende type structure) aluminum nitride phase (cAlN) could not be observed.

Claims

An alumina sintered body containing 0.3 to 3.0 volume % of cubic aluminum nitride, wherein the thermal conductivity is 35 W / m·k or more and the infrared ray emissivity is 0.60 or more.The method for producing an alumina sintered body according to claim 1, wherein the method comprises a sintering step of firing an alumina powder having an average particle size of 10 μm or less in a reducing nitrogen atmosphere.The method for producing an alumina sintered body according to claim 2, wherein the alumina powder having an average particle size of 10 μm or less is fired together with an organic binder.The method for producing an alumina sintered body according to claim 2 or 3, wherein the alumina powder having an average particle size of 10 μm or less is fired together with a sintering aid.The method for producing an alumina sintered body according to any one of claims 2 to 4, wherein the firing temperature in the sintering step is in a range of 1600 to 1825°C.The method for producing an alumina sintered body according to any one of claims 2 to 5, wherein the alumina powder having an average particle size of 10 μm or less is fired in the sintering step in an atmosphere of at least one of nitrogen and ammonia.

Citation Information

Patent Citations

  • Production of sintered ceramic

    JP1991112846A

  • Translucent polycrystalline alumina ceramic, ceramic discharge vessel and method of making ceramic discharge vessel

    JP2006327933A

  • JP000H03112846A

  • JP002006327933A