Improved cross-cut welding device, film packaging machine and process

The transverse separation welding device in film packaging machines addresses poor weld seams by mechanically separating film webs using a resiliently mounted cutting knife, ensuring high-quality welds and cleanliness across varying film types and thicknesses.

DE102017131026B4Active Publication Date: 2024-12-05BECK PACKAUTOMATEN
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
DE102017131026
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Filing Date
2017-12-21
Publication Date
2024-12-05
Estimated Expiration
2037-12-21

AI Technical Summary

Technical Problem

Existing cross-cutting welding devices in film packaging machines often produce poor weld seams due to excessive temperatures that cause film webs to evaporate or melt, leading to contamination and undesirable welding results, especially with thick, multi-layer, or colored films.

Method used

A transverse separation welding device with an upper punch and lower punch, featuring a groove in the upper punch and resiliently mounted pressure-receiving devices, uses a cutting knife that emerges from a gap to mechanically separate film webs, eliminating the need for high thermal cutting temperatures.

Benefits of technology

The mechanical separation process ensures high-quality weld seams without thermal damage, preventing contamination and maintaining cleanliness, while allowing for adjustable film thickness and type handling.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

Transverse sealing device (22) for a film packaging machine (10), comprising an upper punch (44) and a lower punch (46), wherein the upper punch (44) has a transverse sealing surface (84) facing the lower punch (46), wherein the upper punch (44) has at least one heating device (88) for heating the transverse sealing surface (84), characterized in that a groove (86) is formed in the transverse sealing surface (84) of the upper punch (44), wherein the lower punch (46) has two pressure receiving devices (66, 67) spaced apart from each other by a gap (89), wherein the pressure receiving devices (66, 67) form a support surface (70) facing the upper punch (44), wherein the upper punch (44) and the lower punch (46) are movable relative to each other in a sealing plane (57), wherein the gap (89) is opposite the groove (86) of the upper punch (44) is arranged, wherein the lower punch (46) has a separating knife (90) arranged in the gap (89),and wherein each of the pressure-receiving devices (66, 67) is resiliently mounted in the lower punch (46) parallel to the separation welding plane (57), wherein an elastic element is arranged in the groove (86) of the upper punch (44) at a base of the groove (86), wherein a resilient mounting of each of the pressure-receiving devices (66, 67) is designed such that, at maximum deflection of the pressure-receiving devices (66, 67), the separating blade (90) bears against the elastic element or is immersed in the elastic element.
Need to check novelty before this filing date? Find Prior Art

Description

Improved cross-cut welding device, film packaging machine and process

[0001] The present invention relates to a transverse sealing device for a film packaging machine, comprising an upper punch and a lower punch, wherein the upper punch has a transverse sealing surface facing the lower punch, and wherein the upper punch has at least one heating device for heating the transverse sealing surface.

[0002] Such a substamp is known, for example, from the printed document DE 10 2011 015 111 A1.

[0003] Packaging machines are used in many industrial applications for packaging a variety of goods. These goods can range from consumer items such as data carriers, books, or common supermarket products to specialized items like spare parts or building materials such as clay. Packaging machines are also regularly used for magazines with inserts and in mail order.

[0004] The present invention relates primarily to film packaging machines, which are generally divided into forming shoulder machines, serial packaging machines, and banding machines. While forming shoulder machines and serial packaging machines are designed to completely encase a product in film, a banding machine merely places a band around the product to be packaged.

[0005] Within the scope of the present invention, the term "packaging machine" is to be understood as encompassing all of the aforementioned types of packaging machines. The term "outer packaging" is to be understood as encompassing both film packaging that completely encloses the product, which can be supplied either as semi-tubular sleeves or as separate films, as well as bands.

[0006] All packaging machines have in common that the outer packaging must be sealed and cut on at least one side. For bands, this is usually only the case on one side, for shoulder forming machines on two or three sides, and for serial packaging machines on all four sides of the product. Packaging machines therefore always have a so-called transverse sealing device, which seals and at least partially cuts the outer packaging perpendicular to the transport direction of the product within the machine. Furthermore, packaging machines have longitudinal sealing devices or longitudinal sealing devices, which seal the outer packaging parallel to the transport direction of the product and cut off any excess film. This excess film is then usually collected and recycled by means of a film recycling system.

[0007] Packaging machines are rarely designed for just one specific product. Typically, they are intended to handle products of varying dimensions, differing in both width and height. Therefore, it has been proposed that the longitudinal welding device of the packaging machine be adjustable to accommodate different products.

[0008] Furthermore, film sheets of varying thicknesses, colors, and folds are possible, as the outer packaging can vary from product to product. The film material itself can also differ from product to product.

[0009] The cycle rate at which the goods are fed into the film packaging machine and packaged can also vary. Generally, a higher cycle rate necessitates a higher feed speed for the goods, thus reducing the dwell time of a film section in a stationary cross-sealing device. This results in a shorter time for the upper and lower dies of the cross-sealing device to perform the cut-off sealing action. In addition to the dwell time of the cross-sealing dies on the film, the pressure applied to the film by the cross-sealing device and the temperature of the heated upper die also play a role in determining whether a high-quality cut-off seam can be produced across the entire film thickness.

[0010] In known transverse cutting and welding devices, a thermal cutting process is performed. This means that the film webs are thermally separated and fused or welded together using a heated upper die and / or a heated lower die. However, the temperature required to separate the film web is higher than the temperature required for simply welding it together. This resulted in the film webs typically being subjected to a temperature that was too high for the isolated welding process itself.

[0011] Not only can it lead to poor welding results, as the foil webs may evaporate in places, for example, but it can also lead to undesirable behavior of other materials involved.

[0012] For example, with very thick films, films with adhesive tape, or films with a relatively thick coating or a variety of colors, a high temperature must be selected for thermal cutting. However, adhesive tapes, adhesives, or paints melt at these temperatures and can lead to unclean welds. Contamination of the cutting / welding dies can also occur. This contamination, in turn, can lead to undesirable welding results over the operating period.

[0013] Further cross-cutting welding devices are shown in the publications GB 1 465 944 A, DE 69 507 015 T2, EP 2 502 832 A1, DE 4 206 968 A1 and US 2 999 532 A.

[0014] It is an object of the present invention to eliminate the aforementioned problems and to provide a means for high-quality transverse cutting welding of film webs, in particular thick, multi-layered and colored film webs.

[0015] According to a first aspect, a transverse sealing device for a film packaging machine is therefore provided, comprising an upper punch and a lower punch, wherein the upper punch has a transverse sealing surface facing the lower punch, wherein the upper punch has at least one heating device for heating the transverse sealing surface, wherein a groove is formed in the transverse sealing surface of the upper punch, wherein the lower punch has two pressure receiving devices spaced apart from each other by a gap, wherein the pressure receiving devices form a support surface facing the upper punch, wherein the upper punch and the lower punch are movable relative to each other in a sealing plane, wherein the gap is arranged opposite the groove of the upper punch.wherein the lower punch has a separating blade arranged in the gap and wherein each of the pressure-receiving devices is movably and resiliently mounted in the lower punch parallel to the separation weld plane, wherein an elastic element is arranged in the groove of the upper punch at a bottom of the groove, wherein a resilient mounting of each of the pressure-receiving devices is designed such that, at maximum deflection of the pressure-receiving devices, the separating blade rests against the elastic element or is immersed in the elastic element.

[0016] In this way, a transverse cutting and welding device is created in which the film webs are still thermally welded, but are mechanically cut. Due to the spring-loaded mounting of the pressure-absorbing devices, the upper punch can press the pressure-absorbing devices in against their spring force. The cutting blade is fixed in the lower punch. The cutting blade is not movable within the lower punch. Thus, when force is applied, the pressure-absorbing devices move relative to the cutting blade against the spring force of their spring-loaded mounting in the cutting and welding plane. The cutting blade therefore emerges from the gap and enters the opposite groove of the upper punch. The film webs, held between the transverse welding surface and the support surface formed by the pressure-absorbing device, are thereby pressed onto the cutting blade and cut by it.The cutting can take place across the entire width of the film webs, or a continuous strip can remain on the outside on at least one side, which is used for conveying through the longitudinal welding device and is only cut off in the longitudinal welding device.

[0017] Furthermore, the separating blade located in the lower punch provides increased safety for both the packaged goods and the operator of the packaging machine. The separating blade is positioned in the gap between the pressure-absorbing elements of the lower punch and is only released when force is applied by the upper punch, at which point it engages directly in the groove of the upper punch opposite the gap. Access to the cutting surface of the exposed separating blade is therefore impossible for both the packaged goods and the operator while the machine is in operation.

[0018] Since the groove faces downwards, its base is oriented upwards in the operating position of the film packaging machine and the cross-sealing device, so that the elastic element is essentially positioned at the top of the groove. The cutting blade then comes to rest against the elastic element, or something enters it. This prevents the cutting blade from striking the bottom of the groove and any potential damage.

[0019] In this way, the gaps are designed such that when the pressure-absorbing devices are fully depressed and the separating blade is fully immersed in the groove of the upper punch, the cutting edge or teeth of the separating blade rest against, or are slightly embedded in, the elastic or silicone element. This results in a particularly effective cleaning action of the blade, as described above.

[0020] Furthermore, according to another aspect of the invention, a film packaging machine can be provided with such a transverse cutting and welding device.

[0021] According to yet another aspect of the invention, a method for transverse welding of film web sections is provided, comprising the steps of moving a heated transverse welding surface of an upper punch of a transverse welding device relative to a support surface of a lower punch of the transverse welding device, so that the transverse welding surface rests against the support surface and welding of the film web sections takes place between the transverse welding surface and the support surface;and of pressing down the support surface by means of the upper punch, so that a cutting blade emerges from a gap in the support surface and enters a groove formed in a transverse weld surface, so that the film web sections are cut by the cutting blade, in particular wherein the pressing down takes place against a spring force, wherein an elastic element is arranged in the groove of the upper punch at a bottom of the groove, wherein a resilient bearing of each of the pressure-bearing devices is designed such that, at maximum deflection of the pressure-bearing devices, the cutting blade rests against the elastic element or plunges into the elastic element.

[0022] The proposed method also involves initially clamping or holding the film web sections. These film web sections can be sections of a separate top film and a separate bottom film in a serial packaging machine, or two overlapping film web sections of a C-shaped folded film in a forming shoulder machine. While the transverse sealing surface of the upper punch rests on the support surface of the lower punch, the lower punch is pressed down by the upper punch, and the cutting blade emerges from the support surface and enters the groove of the transverse sealing surface of the upper punch, thus mechanically cutting the film web sections.

[0023] The task posed at the beginning is therefore completely solved.

[0024] In one configuration, the first stamp can be the upper stamp and the second stamp the lower stamp. When further configurations are described using the terms "upper stamp" and "lower stamp," these configurations can also be provided without a specific assignment to upper and lower stamps, in which case the term "upper stamp" is replaced by the term "first stamp" and the term "lower stamp" is replaced by the term "second stamp."

[0025] In one embodiment, it can be provided that the upper punch and the lower punch are movable relative to each other in the separation welding plane in such a way that the transverse welding surface of the upper punch and the support surface formed by the pressure receiving devices are in contact with each other.

[0026] The separation welding plane thus refers to a plane that is formed by the longitudinal extension of the upper punch and lower punch in a horizontal direction and by the vertical movement of at least one of the upper punch and the lower punch relative to each other.

[0027] In a further embodiment, the pressure-absorbing devices can be spring-mounted in the lower die in the weld plane such that the separating blade is retracted into the support surface when the support surface and the transverse weld surface are spaced apart, and that the separating blade projects out of the support surface and into the groove when the transverse weld surface exerts a sealing force on the support surface. Instead of "sealing force," the term "force" can also be used. This refers to a force that is large enough to counteract the spring force of the mounting of the pressure-absorbing devices and push the pressure-absorbing devices downwards so that the separating blade can project outwards.

[0028] This ensures that, without force being applied (i.e., when the support surface and the transverse welding surface are spaced apart), the cutting blade is positioned in the gap between the pressure-absorbing devices. This prevents an operator from, for example, reaching into the cutting blade with their hand. Packaged goods also cannot be damaged by the cutting blade. Only when the support surfaces and the transverse welding surface are in contact, and the transverse welding surface then applies further force to the support surface, pressing the pressure-absorbing device downwards, does the cutting blade emerge from the support surface and engage directly in the groove formed in the transverse welding surface of the upper die. The mechanical cutting of the film web thus occurs only when the film web is already clamped between the transverse welding surface and the support surface. In this state, neither a person nor an object can reach the cutting blade from the outside.

[0029] In a further embodiment of the transverse welding device, it can be provided that the upper punch has two hold-down elements which are arranged on opposite sides of the welding plane or the transverse welding surface and are mounted in the upper punch so as to be movable parallel to the welding plane relative to the transverse welding surface, wherein the hold-down elements are arranged opposite each other to one of the pressure receiving devices.

[0030] These hold-down elements allow for initial fixation of the film web sections between the hold-down elements and the pressure-absorbing devices before the transverse welding surface moves towards the pressure-absorbing devices and the support surface. This ensures that the welding process itself is shielded before the transverse welding surface and the support surface come into contact. Furthermore, the film web sections are tensioned and fixed before the transverse welding surface contacts the support surface.

[0031] In a further embodiment, it can be provided that the hold-down elements are resiliently mounted in the upper punch parallel to the separation welding plane in such a way that an end of each hold-down element facing the lower punch is less far from the support surface than the transverse welding surface, if the support surface and the transverse welding surface are spaced apart from each other.

[0032] The hold-down elements are spring-mounted in such a way that they project downwards beyond the transverse welding surface and thus are the first to contact the pressure-absorbing devices. One hold-down element is arranged on each side of the welding plane, so that each pressure-absorbing device is assigned a hold-down element. In the transport direction, one hold-down element is therefore positioned in front of the welding plane and one hold-down element is positioned behind the welding plane.

[0033] In a further embodiment, it can be provided that a spring constant of a resilient bearing of the hold-down elements is lower than a spring constant of each resilient bearing of one of the pressure-receiving devices.

[0034] In other words, the force required to compress the pressure-absorbing devices is greater than the force required to raise or compress the hold-down elements. Thus, when the hold-down elements strike the pressure-absorbing devices, they are initially compressed, or the transverse weld surface moves downwards relative to the hold-down elements resting on the pressure-absorbing device, until the transverse weld surface comes into contact with the support surface. Only then is a force applied to the pressure-absorbing devices by means of the upper punch, which compresses them downwards against the spring force of their resilient bearing.

[0035] In a further embodiment, it may be provided that the transverse welding surface and / or the support surface has at least one recess running perpendicular to the separation welding plane.

[0036] The corresponding cutout thus runs parallel to the transport direction. This prevents a complete weld across the entire width, instead creating a number of holes in the weld seam corresponding to the number of cutouts. This allows the sealed film bags to be vented, minimizing their volume. Providing such vent holes in the cut-off weld seam is possible because a thermal separation process is no longer required; instead, the separation is mechanical, allowing cutouts to be created within the weld seam. This eliminates the need to perforate the film bags during the film packaging machine process.

[0037] In one embodiment, the elastic element may be made of silicone.

[0038] This has proven particularly advantageous, as the separating blade can penetrate the silicone slightly. In particular, paint residue from the separating blade can be pressed into the silicone and wiped off there. For system maintenance, it is then only necessary to replace the silicone element at certain intervals, if required. In this way, the separating blade remains relatively free of paint particles and contaminants.

[0039] In one embodiment, it can be provided that the lower punch is fixed, while the upper punch is movable in the welding plane.

[0040] In this way, a simple setup with good welding results can be provided.

[0041] Alternatively, in a further embodiment, it can also be provided that the upper punch and the lower punch are designed to be movable in the separation welding plane.

[0042] In this way, the point of contact between the upper and lower punches can be varied while still achieving a good welding result.

[0043] In one embodiment, the separating blade may be arranged in a fixed position in the lower die.

[0044] In this way, the design can be simplified even further. The cutting blade is thus stationary, specifically arranged in a stationary lower punch. Only the pressing down of the pressure-receiving device by means of the upper punch releases the cutting blade and causes the mechanical cutting of the film webs, which are pressed over the stationary cutting blade.

[0045] In one embodiment of the method, it may be provided that, prior to the step of relative movement, two hold-down elements movable on the upper punch relative to the transverse welding surface are brought into contact with the pressure receiving devices of the lower punch, which form the support surface and are spaced apart by the gap, so that the film web section is held between the hold-down elements and the pressure receiving devices, wherein subsequently, during the step of relative movement, the transverse welding surface is moved onto the support surface relative to the hold-down elements already in contact with the pressure receiving devices.

[0046] In this way, as described above, the overlapping film webs can first be held down, which fixes and tensions them. Only then does the transverse welding surface of the upper punch, moving relative to the already engaged hold-down elements, contact the support surface. Once the transverse welding surface is in contact with the support surface, the support surface or the pressure-bearing devices are pressed down against the spring force of their bearings, so that the cutting blade emerges through the support surface and cuts the overlapping film webs.

[0047] It is understood that the features mentioned above and those to be explained below can be used not only in the combinations specified, but also in other combinations or on their own, without leaving the scope of the present invention.

[0048] Exemplary embodiments of the invention are shown in the drawing and are explained in more detail in the following description. They show: Fig. 1 a schematic view of a film packaging machine, Fig. 2. A merely exemplary presentation of Section II in the Fig. 1, Fig. 3 a cross-section along a line III-III in Fig. 2, which schematically shows a lower die according to the invention, Fig. 4a a cross-sectional view along a line IV-IV in Fig. 3, Fig. 4b to 4d different stages of the transverse welding process; Fig. 5 a schematic view of a cutting knife; and Fig. 6. A schematic flowchart of a procedure.

[0049] Fig. Figure 1 shows a film packaging machine 10 in a schematic view. The packaging machine 10 serves to provide a product 12 with outer packaging. For this purpose, the product 12 is moved through the film packaging machine 10 in a transport direction T.

[0050] The product 12 is wrapped by the film wrapping machine 10 with a film web 14, which is unwound from a film feeder 15. If it is a serial packaging machine, a further film web 16, which is unwound from a further film feeder 17, can be provided. This type of wrapping then corresponds to the principle of a so-called serial packaging machine, so that the present invention is accordingly explained using the example of a film wrapping machine 10 designed as a serial packaging machine.

[0051] The upper film web 14 and the lower film web 16 converge in a film plane 18. The packaged goods 12 thus enter the converging upper film web 14 and lower film web 16, whereby the film webs 14 and 16 are initially subjected to transverse tension.

[0052] A transverse tightening device 20 is provided for this purpose. The wrapped goods 12 with the transversely tightened film webs 14, 16 reach a transverse cutting and welding device 22. The transverse cutting and welding device 22 welds the film webs 14, 16 together transversely to the transport direction T and at least partially cuts through the film webs 14, 16, so that the goods 12 no longer have contact with the preceding goods 12 along the weld seam.

[0053] The packaged item 12 then passes through a longitudinal sealing device 24, which is designed to seal the film webs 14, 16 together laterally of the packaged item 12 and to trim off any lateral film overhang. Finally, the side of the packaged item 12 facing away from the direction of transport T is again sealed and trimmed by the transverse sealing device 22. The packaged item 12 is now sealed and trimmed on all four sides, so that it is completely enclosed in a film covering.

[0054] The sequence of the transverse cutting welding device 22, the longitudinal cutting welding device 24, and the transverse tightening device 20 is shown only as an example of a frequently occurring configuration. The sequence of these devices can also be different; for example, the transverse cutting welding device 22 can be arranged after the longitudinal cutting welding device 24. Elements of the transverse tightening device 20 can also be provided between or within the transverse cutting welding device 22 or the longitudinal cutting welding device 24.

[0055] It may be provided that at least one further module is then added, for example, a shrink tunnel 26, which is heated to a specific temperature and shrinks the film webs 14, 16 onto the packaged goods 12, so that the film webs 14, 16 tightly enclose the packaged goods 12 without any play. Furthermore, a sealing station may be provided, for example, which cuts off any remaining film overhang in the longitudinal direction after the product has passed through the longitudinal sealing device 24, closely adhering to the packaged goods. This may be particularly useful for packaged goods 12 with varying widths. The packaging process is then complete.

[0056] The presence of a shrink tunnel 26 depends fundamentally on the packaging requirements. A shrink tunnel 26 is not necessarily required, particularly in high-volume packaging machines.

[0057] Furthermore, the film packaging machine 10 typically has adjustment devices 28 to adapt it to products of varying widths, lengths, and heights. The speed of the packaging process can also be adjusted using these devices 28. Additionally, the machine provides options for adjusting it to different types of film, which may differ, for example, in thickness, tear resistance, and surface texture.

[0058] Ultimately, a film return system 30 is usually provided, which collects excess film material separated by the longitudinal cutting welding device 24 in order to feed it, for example, into a recycling process.

[0059] The number II designates a section of the film packaging machine 10, which is located in Fig. 2 is shown in a detailed view.

[0060] The one in Fig. Figure 2 shows the transverse clamping device 20, the transverse cutting welding device 22 and the longitudinal cutting welding device 24.

[0061] The transverse tensioning device 20 typically has an upper transverse tensioning wheel 32 and a lower transverse tensioning wheel 34, which draw the upper film web 14 and the lower film web 16 between them and tension them in a transverse direction, i.e., perpendicular to the transport direction T. The transverse tensioning wheels 32, 34 are typically inclined slightly outwards with their axis of rotation.

[0062] A first transport device 36 conveys the goods to be packaged on the film level 18 to the transverse sealing device 22. There, the first transport device 36 terminates in a first deflection roller 38. A second transport device 40 follows the first transport device 36 and conveys the goods 12 from the transverse sealing device 22 to the longitudinal sealing device 24. The longitudinal sealing device 24 and the transition from the second transport device 40 to the longitudinal sealing device 24 are shown only schematically and can be designed as desired.

[0063] The second transport device 40 begins with a second deflection roller 42, which is moved very close to the first deflection roller 38 in a first position. This first position is in the Fig. 2 is shown and is intended to indicate the position in which a punch gap existing between the first deflection roller 38 and the second deflection roller 42 is minimized.

[0064] The transverse cutting and welding device 22 has a first punch, in the illustrated embodiment the upper punch 44, and a second punch, in the illustrated embodiment the lower punch 46. Therefore, in the following, we will refer directly to the upper punch and the lower punch. The upper punch 44 and the lower punch 46 are movable towards each other in order to at least partially cut and weld the upper film web 14 and the lower film web 16.

[0065] In the Fig. However, in the first position shown in Figure 2, this is not possible because the punch gap is closed. The upper punch 44 and the lower punch 46 cannot meet because the second deflection roller 42 is located between them.

[0066] Therefore, the second transport device 40 is movable in the horizontal direction, i.e., parallel to the film plane 18. This movement is indicated by an arrow 48.

[0067] The lower die 46, in turn, moves along a direction indicated by an arrow 49. In an operating state of the film packaging machine 10, direction 48 is horizontal and direction 49 is vertical. According to the terminology used in this description, direction 48 extends in the direction of a "length" of the film packaging machine 10 or one of its elements. Direction 49 accordingly denotes a "height". Perpendicular to direction 48 and direction 49, a "width" of the film packaging machine 10 or of the lower die 46 therefore extends.

[0068] To effect the movements, a drive unit 50 is provided. The drive unit 50 is in Fig. Figure 2 is shown schematically only. It can be any device; preferably, a servo motor or another suitable electric motor is provided to effect the movements.

[0069] For this purpose, the drive unit 50 actuates a double-sided lever 52, which has a first lever 54 articulated to the lower punch 46 and a second lever 56 articulated to the upper punch 44. In this way, a rotation of the double lever 52 effected by the drive unit 50 can cause both an upward movement of the lower punch in a direction 49 and a downward movement of the upper punch 44 in a direction 49.

[0070] Fig. Figure 3 shows a schematic cross-sectional view along line III-III representing a separation welding plane 57 in Fig. 2.

[0071] A lower die 46 is shown. The lower die 46 can be heated, but this is not mandatory. The upper die 44 is heated in the illustrated embodiment. For this purpose, the film packaging machine 10 has a heating control device 58 for the upper die 44. A heating control device 60 can be provided for the lower die 46 if it is also heated. The provision of two separate heating control devices 58 and 60 is not mandatory; if necessary, a single heating control device can be provided for both the upper die 44 and the lower die 46. The heating control device 58 is connected to the upper die 44 via a line 62. The heating control device 60 is connected to the lower die 46 via a line 63. A signal can be transmitted via the lines 62 and 63 to either the upper die 44 or the lower die 46. Fig. 3 (not shown) the current to be introduced can be transmitted as well as a measurement signal from a temperature sensor arranged in the upper die 44 or the lower die 46 (in the Fig. 3 (not shown) can be read out. If two separate heating control devices 58, 60 are provided, these can be connected by means of a line 64 for data exchange in order to jointly control or synchronize the heating of the upper die 44 and the lower die 46.

[0072] The lower punch 46 has a pressure-receiving device 66 made of a suitable material, for example, a heat-resistant plastic material such as silicone, or a rubber material. The pressure-receiving device 66 is supported by a support device 68. Furthermore, the lower punch 46 may have a rib element that laterally supports the pressure-receiving device 66 on the support device 68 in the transport direction. However, the rib element is not mandatory; for example, it may be omitted in the case of a stationary transverse cutting welding device 22.

[0073] The lower punch 46 extends along a longitudinal axis 72. The longitudinal axis 72 of the lower punch 46 thus runs transversely to the transport direction T.

[0074] The upper punch 44 has a heated element 82 which extends transversely to a separation welding plane at least one of the elements in Fig. Figure 3 shows two recesses 61, 61'. In this way, air holes can be formed in the weld.

[0075] The Fig. Figure 4 shows a schematic cross-sectional view along a line IV-IV in Fig. 3.

[0076] Fig. Figure 4a shows a cross-sectional view of the transverse cutting welding device 22 along line IV-IV in the Fig. 3. The upper die 44 and the lower die 66 are shown. The lower die 46 has two pressure-receiving devices 66 and 67. These pressure-receiving devices 66 and 67 can, for example, be made of a hard, heat-resistant plastic material. The surfaces of the pressure-receiving devices 66 and 67 facing the upper die 44 form the support surface 70. Each of the pressure-receiving devices 66 and 67 is arranged in a support element 72 or 73, respectively. The pressure-receiving devices 66 and 67 have a gap 89 between them. On the opposite side, strip sections 74 or 75 can be arranged to prevent the pressure-receiving devices 66 and 67 from slipping. However, these are not strictly necessary. For example, the pressure-receiving devices 66 and 67 can be bonded to the support elements 72 and 73. The support elements 72, 73 are separated from spring mounting elements 78 and 73 respectively.The pressure-absorbing devices 66, 67, the support elements 72, 73, and the spring receptacles 78, 79 are spaced apart and resiliently mounted in them by means of one of the respective springs 80, 81. The separating blade 90 extends between the pressure-absorbing devices 66, 67, the support elements 72, 73, and the spring receptacles 78, 79. In this way, it is resiliently mounted in the lower punch 46 relative to the pressure-absorbing device 66, 67 and is movable parallel to the separation welding plane 57 or in the vertical direction against the spring force of the spring elements 80 and guided in the vertical direction.

[0077] The upper die 44 has a heated element 82, the surfaces of which facing the lower die 46 form a transverse welding surface 84. A groove 86 is formed in the transverse welding surface 84, extending vertically upwards, i.e., away from the lower die 46. An elastic element 87, which may be made of silicone, is arranged at one end of the groove, i.e., at the end of the groove furthest from the lower die 46. A heating element 88, for example a cartridge heater or a heating coil, is arranged in the heated element 82, which heats the heated element 82 to the welding temperature.

[0078] Furthermore, the upper punch 44 has hold-down elements 94 and 96, which are arranged on both sides of the heated element 82 and the transverse welding surface 84, respectively. In the cross-sectional view shown, the hold-down element 94 is thus arranged in front of the heated element 82 in the transport direction, and the hold-down element 96 is arranged behind the heated element 82 in the transport direction. The hold-down elements are slightly bent towards each other at their ends 75 and 97, respectively, which face the lower punch 46. Hold-down elements 94 and 96 are resiliently mounted in the upper punch 94 by means of a spring bearing 88. In this way, the hold-down elements 94 and 96 can move parallel to the separation welding plane 97 relative to the heated element 82 and the transverse welding surface 84.

[0079] The sequence of the transverse welding process is described below successively in the Fig. 4b to 4d explained.

[0080] From the in the Fig. In the starting position shown in Figure 4a, the upper punch 44 is moved onto the stationary lower punch 46. Initially, the hold-down elements 94 and 96, with their ends 95 and 97 facing the lower punch 46, come into contact with the pressure receiving devices 66, 67. This situation is shown in the Fig. 4b shown.

[0081] Sections of foil web running between the upper die and the lower die are now held and tensioned between the hold-down elements 94, 96 and the pressure receiving devices 66, 67.

[0082] The upper punch is now moved further towards the lower punch. The hold-down elements, already resting on the pressure-absorbing devices 66, 67, are now inserted into the spring-loaded bearing 98 and move relative to the other elements of the upper punch 44. This movement continues until the heated element 82, with its transverse welding surface 84, comes into contact with the pressure-absorbing devices 66, 67 and the support surface 70. The situation is thus... Fig. 4c is shown. The sealing process now begins and the film web sections are welded between the pressure-receiving devices 66, 67 and the heated element 82. The situation is as follows: Fig. 4c shown.

[0083] The upper punch is now moved further downwards, pressing the pressure receiving device 66, 67 further downwards against the force of the springs 80, 81. In doing so, the separating blade 90 emerges from the gap 89 and enters the groove 86. In the fully compressed state, which is in the Fig. As shown in Figure 4d, the support elements 72, 73 rest on the spring retainers 88, 89. The cutting blade 90 dips minimally into the silicone element 87 with its tips. The film web sections are thus mechanically cut by means of the cutting blade 90. The film webs are therefore mechanically cut and simultaneously thermally sealed or welded together. If the recesses 61 or 61' are provided, openings for venting the film bags are also present in the weld seams. Nevertheless, separation can be achieved across the entire width due to the mechanical cutting action of the cutting blade 90.

[0084] The dies are then opened again, i.e., the upper die 44 is moved upwards into the space in the Fig. 4a shown condition.

[0085] The Fig. Figure 5 schematically shows a possible separating blade 90. The cutting edge, designated 91, is, for example, serrated as shown. In particular, two offset rows of serrations can be provided. It is therefore not essential that the cutting edge of the separating blade be straight; rather, the serrated cutting edge 91 shown allows for effective mechanical separation. Furthermore, the tips of the serrations 91 can be inserted into the silicone element 97, thus wiping away dirt or paint from the silicone on the sides of the serrations. In this way, clogging of the stamping elements or the welding blade can be prevented, and only the silicone element needs to be replaced during maintenance.

[0086] The Fig. Figure 6 shows a schematic flowchart of a method according to the invention.

[0087] This procedure follows the one described in the Fig.The sequence is shown in Figures 4a to 4d. After the start of the process, an optional step 106 can be performed, in which, prior to the step of relative movement of the upper punch relative to the lower punch relative to the cross-sectional area, hold-down elements are brought into contact with the pressure-receiving devices of the lower punch, which form the support surface and are spaced apart by the gap, so that the film web sections 14, 16 are held between the hold-down elements and the pressure-receiving devices 66, 67. Subsequently, during the step of relative movement 102, the transverse welding surface is moved relative to the hold-down elements already in contact with the pressure-receiving devices onto the support surface. The step of relative movement 1 or 2 brings the heated transverse welding surface of the upper punch into contact with the support surface 70 of the lower punch 46 of the transverse cutting welding device 22.The transverse welding surface 84 lies close to the support surface 70 and welds the film web sections 14, 16 between the transverse welding surface 84 and the support surface 70 or the pressure receiving devices 66, 67.

[0088] Finally, step 104 involves pressing down the support surface or the pressure-receiving device 66, 67 by means of the upper punch against a spring force, in particular the spring elements 80, 81. The cutting blade 90 thus emerges from the gap 89 between the pressure-receiving devices 66, 67 and enters the groove 86 in the transverse welding surface 84, so that the film web sections 14, 16 are cut by the cutting blade 90. The process then ends.

Claims

[1] Cross-cutting and welding device (22) for a film packaging machine (10), comprising an upper punch (44) and a lower punch (46), wherein the upper punch (44) has a cross-welding surface (84) facing the lower punch (46), wherein the upper punch (44) has at least one heating device (88) for heating the cross-welding surface (84), characterized bythat a groove (86) is formed in the transverse welding surface (84) of the upper punch (44), wherein the lower punch (46) has two pressure-receiving devices (66, 67) spaced apart from one another by a gap (89), wherein the pressure-receiving devices (66, 67) form a support surface (70) facing the upper punch (44), wherein the upper punch (44) and the lower punch (46) are movable relative to one another in a separating-welding plane (57), wherein the gap (89) is arranged opposite the groove (86) of the upper punch (44), wherein the lower punch (46) has a separating knife (90) arranged in the gap (89), and wherein each of the pressure-receiving devices (66, 67) is resiliently mounted in the lower punch (46) parallel to the separating-welding plane (57), wherein in the groove (86) of the upper punch (44) at a base of the groove (86) an elastic element is arranged, wherein a resilient mounting of each of the pressure receiving devices (66, 67) is designed such thatthat at maximum deflection of the pressure absorbing devices (66, 67) the separating knife (90) rests against the elastic element or dips into the elastic element., [2] Cross-cutting welding device (22) according to claim 1, characterized by that the upper punch (44) and the lower punch (46) are movable relative to one another in the separating welding plane (57) in such a way that the transverse welding surface (84) of the upper punch (44) and the support surface (70) formed by the pressure absorption devices (66, 67) abut one another. [3] Cross-cutting welding device (22) according to claim 1 or 2, characterized bythat the pressure absorption devices (66, 67) are resiliently mounted in the lower punch (46) in the separating and welding plane (57) in such a way that the separating knife (90) is arranged retracted into the support surface (70) when the support surface (70) and the transverse welding surface (84) are spaced apart from one another, and that the separating knife (90) projects out of the support surface (70) and projects into the groove (86) when the transverse welding surface (84) applies a sealing force to the support surface (70). [4] Cross-cutting welding device (22) according to one of claims 1 to 3, characterized by in that the upper punch (44) has two hold-down elements which are arranged on opposite sides of the separating-welding plane (57) and are mounted in the upper punch (44) parallel to the separating-welding plane (57) so as to be movable relative to the transverse welding surface (84), the hold-down elements (94, 96) each being arranged opposite one of the pressure-absorbing devices (66, 67). [5] Cross-cutting welding device (22) according to claim 4, characterized by that the hold-down elements are resiliently mounted in the upper punch (44) parallel to the separating welding plane (57) in such a way that an end of each hold-down element facing the lower punch (46) is spaced less from the support surface (70) than the transverse welding surface (84) when the support surface (70) and the transverse welding surface (84) are spaced from one another. [6] Cross-cutting welding device (22) according to claim 5, characterized by that a spring constant of a resilient mounting of the hold-down elements is less than a spring constant of each resilient mounting of one of the pressure-absorbing devices (66, 67). [7] Cross-cutting welding device (22) according to one of claims 1 to 6, characterized by that the transverse welding surface (84) and / or the support surface (70) has at least one recess running perpendicular to the separating welding plane (57). [8] Cross-cutting welding device (22) according to one of claims 1 to 7, characterized by that the elastic element is made of silicone. [9] Cross-cutting welding device (22) according to one of claims 1 to 8, characterized by that the lower punch (46) is stationary, wherein the upper punch (44) is movable in the separating and welding plane (57). [10] Cross-cutting welding device (22) according to one of claims 1 to 9, characterized by that the separating knife (90) is arranged fixedly in the lower punch (46). [11] Film packaging machine (10) with a cross-cutting welding device (22) according to one of claims 1 to 10. [12] Method (100) for transversely cutting and welding film web sections (14, 16), comprising the following steps: • Relative movement (102) of a heated transverse welding surface (84) of an upper punch (44) of a transverse cutting welding device (22) to a support surface (70) of a lower punch (46) of the transverse cutting welding device (22), so that the transverse welding surface (84) bears against the support surface (70) and welding of the film web sections (14, 16) takes place between the transverse welding surface (84) and the support surface (70); and · Pressing down (104) the support surface (70) by means of the upper punch (44) so ​​that a separating knife (90) emerges from a gap (89) in the support surface (70) and enters a groove (86) formed in the transverse welding surface (84), so that the film web sections (14, 16) are severed by the separating knife (90), wherein the pressing down takes place counter to a spring force, wherein an elastic element is arranged in the groove (86) of the upper punch (44) at a base of the groove (86), wherein a resilient mounting of each of the pressure absorbing devices (66, 67) is designed such that when the pressure absorbing devices (66, 67) are deflected to their maximum, the separating knife (90) rests against the elastic element or dips into the elastic element. [13] Method according to claim 12, characterized bythat before the step of relative movement, two hold-down elements (94, 96) on the upper punch (44) which are movable relative to the transverse welding surface (84) are brought into contact with pressure-absorbing devices (66, 67) of the lower punch (46) which form the support surface (70) and are spaced apart by the gap (89), so that the film web sections (14, 16) are held between the hold-down elements (94, 96) and the pressure-absorbing devices (66, 67), wherein subsequently during the step of relative movement the transverse welding surface (84) is moved onto the support surface (70) relative to the hold-down elements (94, 96) which are already in contact with the pressure-absorbing devices (66, 67).

Citation Information

Patent Citations

  • Improved lower stamp for thick foil webs

    DE102011015111A1

  • Automatic wrapping device for rectangular paper stacks - has welding and cutting device and heat sealable plastics foils

    DE4206968A1

  • DEVICE FOR SEALING BAGS

    DE69507015T2

  • A jaw support for a pouch filler

    EP2502832A1

  • Wrapping machines

    GB1465944A