DEVICE AND MANUFACTURING PROCESS

DE102019131909B4Active Publication Date: 2024-10-02TAIWAN SEMICONDUCTOR MANUFACTURING CO LTD
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
DE102019131909
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-11-25
Filing Date
2019-11-26
Publication Date
2024-10-02
Estimated Expiration
2039-11-26

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

A process comprising the following steps: Deposition of a plurality of layers (102-106, 118-122, 218-222) on a substrate (100, 116, 210); Structuring a first mask (108, 128) over the plurality of layers (102-106, 118-122, 218-222); Performing a first etching process on the plurality of layers (102-106, 118-122, 218-222) using the first mask (108, 128) as an etching mask, wherein, after the first etching process, the plurality of layers (102-106, 118-122, 218-222) extend laterally beyond the first mask (108, 128) and form sidewalls of the plurality of layers (102-106, 118-122, 218-222) are tapered; Deposition of a polymer material (110; 132) along sidewalls of the first mask (108, 128) and along sidewalls of the plurality of layers (102-106, 118-122, 218-222); Removal of the polymer material (110; 132), whereby the removal of the polymer material (110; 132) consumes a portion of the first mask (108, 128),so that a first residual mask is created; and performing a second etching process on the plurality of layers (102-106, 118-122, 218-222) using the first residual mask, wherein, after completion of the second etching process, a common sidewall profile of the plurality of layers (102-106, 118-122, 218-) comprises a first part and a second part, wherein a first angle of the first part and a second angle of the second part are different from each other, further comprising: producing a first layer (230), wherein a first part of the first layer (230) is placed over the plurality of layers (218-222-) and a second part of the first layer (230) is not placed over the plurality of layers (218-222), wherein the first part of the first layer (230) is physically separated from the second part of the first layer (230), further comprising: producing a second layer (232) over the first layer (230),wherein a first part of the second layer (232) is arranged above the plurality of layers (218-222) and a second part of the second layer (232) is not arranged above the plurality of layers (218-222), wherein the first part of the second layer (232) is physically separated from the second part of the second layer (232), further comprising: forming a third layer (234), wherein the third layer (234) is connected between a first part of the third layer (234) arranged above the plurality of layers (218-222) and a second part of the third layer (234) not arranged above the plurality of layers (218-222); and forming a fourth layer (236), wherein the fourth layer (236) is connected between a first part of the fourth layer (236) arranged above the plurality of layers (218-222) and a second part of the fourth layer (236),which is not arranged over the majority of layers (218-222), is continuous.
Need to check novelty before this filing date? Find Prior Art

Description

backgroundSemiconductor devices are used in a variety of electronic applications, such as personal computers, mobile phones, digital cameras, and other electronic devices. Semiconductor devices are typically manufactured by depositing insulating or dielectric layers, conductive layers, and semiconductor layers one after the other over a semiconductor substrate and patterning the various material layers by lithography to produce circuit components and elements on the substrate.The semiconductor industry continues to improve the integration density of various electronic components (e.g. transistors, diodes, resistors, capacitors, etc.) by continually reducing the minimum feature size so that more components can be integrated in a given area. However, reducing the minimum feature size creates additional problems that should be addressed.For the prior art, reference is made to US 2009 / 0 191 711 A1, US 2018 / 0 239 244 A1, US 8 071 485 B2, US 2009 / 0 007 416 A1, US 2018 / 0 233 466 A1, US 5 840 625 A and DE 689 26 440 T2. US 2009 / 0 191 711 A1 discloses a method for forming an ultra-thin structure. The method comprises a polymer deposition and etching process. In one embodiment, the process gently etches the substrate while reducing the critical dimension of the structures formed in the substrate. The dimensions of the structures can be reduced by applying a photoresist-like polymer to the sidewalls of the formed structure, but there is essentially no polymer accumulation on the bottom of the formed structure on the substrate.The invention is defined in the claims.Short description of the drawingsAspects of the present invention can best be understood by reference to the following detailed description when taken in conjunction with the accompanying drawings. It should be noted that, in accordance with standard practice in the industry, various elements are not drawn to scale. Rather, for the sake of clarity of discussion, the dimensions of the various elements may be increased or decreased as desired.Figures 1 to 25 are sectional views of intermediate stages in the fabrication of various devices according to some embodiments.Detailed descriptionThe following description provides many different embodiments or examples for implementing various features of the invention. Specific examples of components and arrangements are described below to facilitate the present invention. For example, the fabrication of a first element over or on a second element in the description below may include embodiments in which the first and second elements are fabricated in direct contact, and may also include embodiments in which additional elements may be fabricated between the first and second elements such that the first and second elements are not in direct contact. Moreover, in the present invention, reference numbers and / or letters may be repeated in the various examples. This repetition is for simplicity and clarity and does not in itself dictate any relationship between the various embodiments and / or configurations discussed.In addition, spatially relative terms such as "below," "under," "lower," "above," "upper," and the like may be used herein to conveniently describe the relationship of an element or structure to one or more other elements or structures illustrated in the figures. The spatially relative terms are intended to encompass other orientations of the device in use or operation in addition to the orientation illustrated in the figures. The device may be oriented differently (rotated 90 degrees or in another orientation), and the spatially relative descriptors used herein may be interpreted accordingly.According to some embodiments, multilayer structures and methods of manufacturing the same are provided. The multilayer structures may have sidewalls with profiles that may be tailored to a specific design. For example, in a multilayer structure, one layer of the multilayer structure may have a sidewall that extends at a first angle and a second layer of the multilayer structure may have a sidewall that extends at a second angle, where the first and second angles may be different from each other. In addition, the multilayer structure may also include further layers, and sidewalls of the further layers may extend at angles that are equal to the first or the second angle or that are different from the first or the second angle. In this way, a desired sidewall profile of the multilayer structure may be achieved.According to some embodiments, a desired sidewall profile of a multilayer structure may be achieved with only one deposition / lithography / etch process rather than multiple deposition / lithography / etch processes. Accordingly, a multilayer structure having a desired sidewall profile may be manufactured at a lower cost and in less time. This may improve manufacturing cycle times and / or yields.In some embodiments, a multilayer structure having a sidewall profile described herein may be used in the fabrication of integrated silicon (Si) nanosystem devices that include sandwich architectures extending adjacent to and / or across multilayer structures. In some embodiments, the multilayer structures are disposed above a silicon complementary metal oxide semiconductor (CMOS) chip. One or more layers may be disposed above the multilayer structure, which may extend laterally beyond the multilayer structure above the CMOS chip. In some devices, it may be convenient to fabricate a first layer of the one or more layers such that a first portion of the first layer that is not above the multilayer structure is separated from a second portion of the first layer that is above the multilayer structure. Similarly, in some devices, it may be desirable to fabricate a second layer such that a first portion of the second layer contacting the first portion of the first layer is separated from a second portion of the second layer located above the second portion of the first layer. Additional layers may be desired that are continuous between portions of the layers located above the multilayer structure and portions not located above the multilayer structure. The sidewall profile of the multilayer structure may be designed such that at least a portion of the sidewall helps to define and / or separate the first portion of the first layer from the second portion of the first layer and / or separate the first portion of the second layer from the second portion of the second layer, while other layers may be fabricated continuous.In Fig. 1, a substrate 100 is provided. Any suitable substrate may be used. In some embodiments, the substrate 100 may include an integrated circuit having one or more active devices, passive devices, and electrical circuitry, and one or more layers may be fabricated over the integrated circuit. For example, the substrate 100 may be a complementary metal oxide semiconductor (CMOS) chip. The substrate 100 may also include one or more dielectric layers fabricated over the CMOS chip. In some embodiments, the substrate 100 may include any number of silicon layers, metal layers, conductive layers, semiconductor layers, or the like. In some embodiments, the substrate 100 may not include any active devices, only passive devices or electrical interconnects. In other embodiments, the substrate 100 may not include any active devices, passive devices, or electrical interconnects. Any suitable materials may be used to fabricate the substrate 100. In some embodiments, the substrate 100 may have a thickness T2 of about.A first layer 102 is formed over the substrate 100. In some embodiments, the first layer 102 may be a monolithic or heterogeneous thin film. In some embodiments, the first layer 102 may comprise a metal or a metal-containing material. For example, the first layer 102 may comprise titanium (Ti), copper (Cu), nickel (Ni), chromium (Cr), and / or aluminum (Al). In some embodiments, the first layer 102 may comprise a combination of metallic materials, such as aluminum copper (AlCu). In other embodiments, the first layer 102 may comprise a dielectric material. For example, the first layer 102 may comprise a silicon-based dielectric material, such as silicon oxide or silicon nitride.A material composition for the first layer 102 may be selected according to the etch rate for the material composition in an etch process, alone and / or in comparison to the material composition of a second layer 104 and a third layer 106 (discussed later). For example, the material compositions for the individual layers may be selected alone and / or in comparison to other layers according to the etch rate for each layer in a particular etch process and according to a desired sidewall profile for a multilayer structure under manufacture.The first layer 102 may be deposited, for example, by chemical vapor deposition (CVD), atomic layer deposition (ALD), physical vapor deposition (PVD), plasma enhanced chemical vapor deposition (PECVD), or the like. The first layer 102 may have a thickness T3 of about 5 nm to about 500 nm.A second layer 104 is formed over the first layer 102. In some embodiments, the second layer 104 may be a monolithic or heterogeneous thin film. The second layer 104 may be formed from the same material as the first layer 102 or from a different material than the first layer 102. For example, the second layer 104 may comprise Ti, Cu, Ni, Cr, and / or Al. In some embodiments, the second layer 104 may comprise a combination of metallic materials, such as AlCu. In other embodiments, the second layer 104 may comprise a dielectric material. For example, the second layer 104 may comprise a silicon-based dielectric material, such as silicon oxide or silicon nitride. If the first layer 102 is made of a metal or metal-containing material, the second layer 104 may also be made of a metal or metal-containing material. Likewise, if the first layer 102 is made of a dielectric material, the second layer 104 may also be made of a dielectric material.As discussed above in connection with the first layer 102, a material composition for the second layer 104 may be selected according to the etch rate for the material composition in an etch process, alone and / or in comparison to the material composition for the first layer 102 and the third layer 106 (discussed later). For example, the material compositions for the individual layers may be selected alone and / or in comparison to other layers according to the etch rate for each layer in a particular etch process and according to a desired sidewall profile for a multilayer structure under manufacture.The second layer 104 may be deposited using the same or similar methods as those described above in connection with the first layer 102. For example, the second layer 104 may be deposited by CVD, ALD, PVD, PECVD, or the like. The second layer 104 may have a thickness T4 of about 5 nm to about 5 μm.A third layer 106 is formed over the second layer 104. In some embodiments, the third layer 106 may be a monolithic or heterogeneous thin film. The third layer 106 may be formed from the same material as the first layer 102 and / or the second layer 104, or it may be formed from a different material than the first layer 102 and / or the second layer 104. For example, the third layer 106 may comprise Ti, Cu, Ni, Cr, and / or Al. In some embodiments, the third layer 106 may comprise a combination of metallic materials, such as AlCu. In other embodiments, the third layer 106 may comprise a dielectric material. For example, the third layer 106 may comprise a silicon-based dielectric material, such as silicon oxide or silicon nitride. If the first layer 102 is made of a metal or a metal-containing material and the second layer 104 is also made of a metal or a metal-containing material, the third layer 106 may also be made of a metal or a metal-containing material. Likewise, if the first layer 102 and the second layer 104 are made of one or more dielectric materials, the third layer 106 may also be made of a dielectric material.As discussed above in connection with the first layer 102 and the second layer 104, a material composition for the third layer 106 may be selected according to the etch rate for the material composition in an etch process, alone and / or in comparison to the material composition for the first layer 102 and the second layer 104. For example, the material compositions for the individual layers may be selected alone and / or in comparison to other layers according to the etch rate for each layer in a particular etch process and according to a desired sidewall profile for a multilayer structure under manufacture.The third layer 106 may be deposited using the same or similar methods as those described above in connection with the first layer 102 and the second layer 104. For example, the third layer 106 may be deposited by CVD, ALD, PVD, PECVD, or the like. The third layer 106 may have a thickness T5 of about 5 nm to about 500 nm.A photoresist 108 is formed over the third layer 106, for example, using a spin coating process. The photoresist 108 may be a positive or a negative photoresist, and it may be single layer or three layer. The photoresist 108 is patterned to produce a patterned photoresist 108 shown in FIG. 1. In some embodiments, the photoresist 108 is patterned using one or more lithographic and / or etching processes. As shown in FIG. 1, after patterning the photoresist 108, the first layer 102, the second layer 104, and the third layer 106 extend laterally beyond sidewalls of the patterned photoresist 108. The patterned photoresist 108 may have a thickness T1 of about 500 nm to about 2 μm and a width W1 of about 200 nm to about 5 μm.Then, a first etching process is performed using the patterned photoresist 108 as an etch mask. The first etching process may be a dry etching process. In some embodiments, for example, when the first layer 102, the second layer 104, and the third layer 106 are made of one or more dielectric materials, carbon and fluorine may be used as etchants for the first etching process, and in some embodiments, oxygen gas or an oxygen gas mixture may also be used. In some embodiments, for example, when the first layer 102, the second layer 104, and the third layer 106 are made of one or more metallic materials, carbon and fluorine may also be used as etchants for the first etching process. For example, when the first layer 102, the second layer 104, and the third layer 106 are made of one or more metallic materials, CF4 and O2 may be used as etchants for the first etching process. In some embodiments, CF4, CHF3, C2F2, BCl3, HBr, CH4, or the like may be used as etchants for the first etch process. The etchants for the first etch process may be selected based on the material compositions for the first layer 102, the second layer 104, and / or the third layer 106 and according to a desired sidewall profile for the first layer 102, the second layer 104, and / or the third layer 106 after the first etch process. Portions of the first layer 102, the second layer 104, and the third layer 106 that are not under the patterned photoresist 108 may be removed during the first etch process. In some embodiments, the first etch process may have an etch duration of about 25 s to 250 s and an etch temperature of about 10°C to about 100°C. In some embodiments, the first etch process may be performed at an etch pressure of about 10 mTorr to 300 mTorr.As shown in FIG. 2, after the first etch process, the multilayer structure formed by the first layer 102, the second layer 104, and the third layer 106 may have sidewalls that taper. For example, sidewalls of the first layer 102, the second layer 104, and / or the third layer 106 may extend at an angle θ1 to a major surface of the substrate 100. In some embodiments, the angle θ1 may be about 30° to about 90°. A sidewall of the first layer 102 may extend at the same angle to the main surface of the substrate 100 as a sidewall of the second layer 104, or the sidewall of the first layer 102 may extend at a different angle than the sidewall of the second layer 104 (for example, due to material compositions for the first layer 102 and the second layer 104 having different etch rates for the first etch process). Similarly, the sidewall of the first layer 102 may extend at the same angle to the main surface of the substrate 100 as a sidewall of the third layer 106, or the sidewall of the first layer 102 may extend at a different angle than the sidewall of the third layer 106 (for example, due to material compositions for the first layer 102 and the third layer 106 having different etch rates for the first etch process). Additionally, the sidewall of the second layer 104 may extend at the same angle to the main surface of the substrate 100 as the sidewall of the third layer 106, or the sidewall of the second layer 104 may extend at a different angle than the sidewall of the third layer 106 (e.g., due to material compositions for the second layer 104 and the third layer 106 having different etch rates for the first etch process). As shown in FIG. 2, after completion of the first etch process, edges of the first layer 102, the second layer 104, and / or the third layer 106 may extend laterally beyond edges of the patterned photoresist 108. For example, the first layer 102 may extend beyond one or more edges of the patterned photoresist 108 by a distance D1. In some embodiments, D1 is about 5 nm to about 150 nm.Then, in Figure 3, a polymer 110 is formed along the edges of the patterned photoresist 108 and along sidewalls of the first layer 102, the second layer 104, and the third layer 106. In some embodiments, the polymer 110 is deposited. For example, in some embodiments, polymer-forming gases may be used during polymer deposition to coat the sidewalls of the multilayer structure and assist in etch profile control. While Figure 3 shows the polymer 110 being deposited exclusively along the sidewalls of the patterned photoresist 108 and along the sidewalls of the first layer 102, the second layer 104, and the third layer 106, in some embodiments the polymer 110 may also extend over the patterned photoresist 108. In some embodiments, the polymer forming gases are CHF3, CH2F2, CF4, C2F6, and C4F8, or the like. During formation of the polymer 110, a plasma source gas is fed into a process chamber, wherein a flow rate of the plasma source gas depends on the configuration of the process chamber. In some embodiments, a feed rate for the plasma source gas and / or the deposition time may be optimized such that the polymer 110 to be deposited along the edges of the patterned photoresist 108 and along the sidewalls of the first layer 102, the second layer 104, and the third layer 106 is selectively deposited according to a desired design. A thickness of the polymer 110 may be smallest at an upper part of the polymer 110 and larger at a lower part, and may vary according to the height. The lower part of the polymer 110 can contact the substrate 100.In Fig. 4, the polymer 110 is removed. In some embodiments, the polymer 110 may be removed with an O2 stripping process. In the O2 stripping process, a portion of the patterned photoresist 108 may be consumed. For example, a thickness of the patterned photoresist 108 may be reduced by the O2 stripping process. In some embodiments, after the O2 stripping process, the patterned photoresist 108 may have a thickness T6. The thickness T6 may be about 150 nm to about 1.5 μm. After the O2 stripping process, the patterned photoresist 108 may have a top surface that is concave. In other embodiments, after the O2 stripping process, the patterned photoresist 108 may have a top surface that is planar. After the O2 stripping process, the patterned photoresist 108 may have tapered sidewalls. For example, a width of the patterned photoresist 108 may change according to the height. A width W2 of the top surface of the patterned photoresist 108 may be about 2000 Å to about 15,000 Å after the O2 stripping process. A width W3 of the bottom surface of the patterned photoresist 108 may be about 300 nm to about 2 µm after the O2 stripping process. A top surface of the third layer 106 may be exposed by consuming the patterned photoresist 108 by the O2 mixture in the stripping process. In some embodiments, the first layer 102, the second layer 104, and / or the third layer 106 may be consuming by the O2 stripping process.In FIG. 5, a second etch process is performed using the photoresist 108 as an etch mask. The second etch process may be a dry etch process in some embodiments. In some embodiments, an etchant may be selected according to a desired sidewall profile of the first layer 102, the second layer 104, and the third layer 106 and according to a material composition of the first layer 102, the second layer 104, and the third layer 106. The etchant may include the same or similar materials as those used in the first etch process described above. For example, in some embodiments, CHF3, CH2F2, CF4, C2F6, and C4F8 may be used together with an O2 mixture as an etchant, for example when the first layer 102, the second layer 104, and the third layer 106 are made of one or more dielectric materials. The etchant may comprise CF4 and O2 in some embodiments, for example when the first layer 102, the second layer 104, and the third layer 106 are made of one or more metallic materials. In some embodiments, the second etch process may have an etch duration of about 25 s to 250 s and an etch temperature of about 10°C to about 100°C. In some embodiments, the second etch process may be performed at an etch pressure of about 10 mTorr to 300 mTorr. The etch parameters for the second etch process may be the same as or different from the etch parameters for the first etch process.The second etch process may continue until desired profiles for the sidewalls of the first layer 102, the second layer 104, and the third layer 106 are achieved. For example, FIG. 5 shows a specific sidewall profile of a multilayer structure 112 formed by the first layer 102, the second layer 104, and the third layer 106. When the desired sidewall profile of the multilayer structure 112 is achieved, the second etch process may be terminated. In some embodiments, the achievement of the desired sidewall profile may be determined according to an elapsed time for the second etch process. In some embodiments, the achievement of the desired sidewall profile may be determined by measurement.Then, the patterned photoresist 108 is removed, for example, with a stripping process. The resulting structure is shown in Fig. 6. The multilayer structure 112 shown in Fig. 6 includes the first layer 102, the second layer 104, and the third layer 106. The first layer 102, the second layer 104, and the third layer 106 have respective sidewalls that form respective angles with the main surface of the substrate 100. For example, sidewalls of the first layer 102 have a base angle θ2to the main surface of the substrate 100. In some embodiments, the base angle θ2is about 55° to about 90°. Sidewalls of the second layer 104 have a re-entrant angle θ3to the main surface of the substrate 100. In some embodiments, the re-entrant angle θ3is about 80° to about 145°. Sidewalls of the third layer 106 have a cone angle θ4to the main surface of the substrate 100. In some embodiments, the cone angle θ4is about 55° to about 100°.Any combination is possible according to the material compositions for the first layer 102, the second layer 104 and the third layer 106 and according to the etchants used in the second etch process described above with reference to FIG. 5. As already stated, the processes described above can be used to produce multilayer structures with sidewall profiles that are tailored to a particular desired design. The etchants (e.g., CF4, O2, or the like), the power of the voltage source (e.g., a power of about 100 W to about 1500 W), the etch time (e.g., an etch time of about 25 s to about 250 s), and other etch parameters can be selected to produce multilayer structures with a specific sidewall profile. In one embodiment, the base angle is about 89°, the re-entry angle is about 88°, and the cone angle is about 83°. In another embodiment, the base angle is about 60°, the re-entry angle is about 130°, and the cone angle is about 67°. In another embodiment, the base angle is about 64°, the re-entry angle is about 105°, and the cone angle is about 61°.In this way, by changing the material compositions of the first layer 102, the second layer 104 and / or the third layer 106 and / or by changing the etchants and etch parameters used in the etching processes described herein, the base angle, the re-entry angle and the cone angle can be changed and a specific sidewall profile for the multilayer structure 112 can be achieved.In some embodiments, the different etch rates for different layers of the multilayer structure 112 may result in discontinuous sidewalls of the multilayer structure 112, particularly at interfaces of different layers of the multilayer structure 112. For example, at an interface of the first layer 102 and the second layer 104, the sidewall of the second layer 104 may be offset from the sidewall of the first layer 102 by a distance D5. In some embodiments, the distance D5 may be about 0 nm to about 100 nm. At an interface of the second layer 104 and the third layer 106, the sidewall of the second layer 104 may be offset from the sidewall of the second layer 104 by a distance D6. In some embodiments, the distance D6 may be about 0 Å to about 300 Å. In the embodiment discussed above, where the base angle is about 64°, the re-entrant angle is about 105°, and the cone angle is about 61°, D5 is about 16 nm and D6 is about 1 nm. In the embodiment discussed above, where the base angle is about 60°, the re-entrant angle is about 130°, and the cone angle is about 67°, D5 is about 55 nm and D6 is about 14 nm.For some components, it may be expedient to produce several multilayer structures next to each other. Figs. 7 to 12 show the production of several multilayer structures next to each other on a substrate 116.In Figure 7, a first multilayer structure may be formed in a first region 124 and a second multilayer structure may be formed in a second region 126. A first layer 118, a second layer 120, and a third layer 122 are formed over the substrate 116. The first layer 118, the second layer 120, and the third layer 122 may be the same or similar to the first layer 102, the second layer 104, and the third layer 106, respectively, and the above discussion of the first layer 102, the second layer 104, and the third layer 106 is fully considered herein. As discussed above in connection with the first layer 102, the second layer 104, and the third layer 106, the material compositions for the first layer 118, the second layer 120, and / or the third layer 122 may be selected according to an etch rate for the material compositions in a particular etch process, either for each individual layer alone and / or relative to the material compositions for the other layers. For example, the material compositions for each layer, alone and relative to other layers, may be selected according to the etch rate for each layer in a particular etch process and desired sidewall profiles for a plurality of multilayer structures under manufacture.In some embodiments, the first layer 118 may be made from the same material in each of the first region 124 and the second region 126. In other embodiments, the first layer 118 may have different material compositions in the first region 124 and the second region 126, for example, to produce a multi-layer structure in the first region 124 that has a sidewall profile that is different from that of the multi-layer structure in the second region 126. In some embodiments, the second layer 120 may be made from the same material in each of the first region 124 and the second region 126. In other embodiments, the second layer 120 may have different material compositions in the first region 124 and the second region 126, for example, to produce a multi-layer structure in the first region 124 that has a sidewall profile that is different from that of the multi-layer structure in the second region 126. In some embodiments, the third layer 122 may be made of the same material in each of the first region 124 and the second region 126. In other embodiments, the third layer 122 may have different material compositions in the first region 124 and the second region 126, for example, to produce a multilayer structure in the first region 124 that has a sidewall profile that is different from that of the multilayer structure in the second region 126.A first patterned photoresist 128 is formed over the third layer 122 in the first region 124, and a second photoresist 130 is formed over the third layer 122 in the second region 126. For example, a photoresist material may be deposited over the third layer 122 using a spin coating process. The photoresist material may be a positive or a negative photoresist material, and may be single layer or three layer. The photoresist material is then patterned to form a first patterned photoresist 128 in the first region 124 and a second patterned photoresist 130 in the second region 126. In some embodiments, the photoresist material may be patterned using one or more lithographic and / or etching processes. As shown in FIG. 7, after patterning the photoresist, the first layer 118, the second layer 120, and the third layer 122 extend laterally beyond sidewalls of the first patterned photoresist 128 and the second photoresist 130. The thicknesses and widths of the first patterned photoresist 128 and the second patterned photoresist 130 may be the same or similar to the thickness and width of the patterned photoresist 108 discussed above with reference to FIG. 1. The thickness and / or width of the first patterned photoresist 128 may be the same as the thickness and / or width of the second patterned photoresist 130. In other embodiments, the thickness and / or width of the first patterned photoresist 128 may be different than the thickness and / or width of the second patterned photoresist 130. In some embodiments, the first patterned photoresist 128 is spaced from the second patterned photoresist 130 by a minimum distance D2, where D2 is about 500 nm to about 5 μm.A first etch process is then performed using the first patterned photoresist 128 and the second patterned photoresist 130 as etch masks. The first etch process may be the same or similar to the first etch process described above with reference to FIG. 2, and the above discussion is fully considered here. Portions of the first layer 118, the second layer 120, and the third layer 122 that are not beneath the first patterned photoresist 128 or the second patterned photoresist 130 may be removed during the first etch process.As shown in FIG. 8, after the first etch process, the multilayer structures formed by the first layer 118, the second layer 120, and the third layer 122 in the first region 124 may have sidewalls that taper. For example, sidewalls of the first layer 118, the second layer 120, and / or the third layer 122 in the first region 124 may extend to a major surface of the substrate 116 at an angle θ5in the first region 124. In some embodiments, the angle θ5may be about 60° to about 90°. A sidewall of the first layer 118 in the first region 124 may extend at the same angle to the major surface of the substrate 116 as a sidewall of the second layer 120 in the first region 124, or the sidewall of the first layer 118 in the first region 124 may extend at a different angle than the sidewall of the second layer 120. Similarly, the sidewall of the first layer 118 in the first region 124 may extend at the same angle to the major surface of the substrate 116 as a sidewall of the third layer 122 in the first region 124, or the sidewall of the first layer 118 in the first region 124 may extend at a different angle than the sidewall of the third layer 122 in the first region 124. Additionally, the sidewall of the second layer 120 in the first region 124 may extend at the same angle to the major surface of the substrate 116 as the sidewall of the third layer 122 in the first region 124, or the sidewall of the second layer 120 in the first region 124 may extend at a different angle than the sidewall of the third layer 122 in the first region 124.After the first etch process, the multilayer structures formed by the first layer 118, the second layer 120 and the third layer 122 in the second region 126 may have sidewalls that taper. For example, sidewalls of the first layer 118, the second layer 120 and / or the third layer 122 in the second region 126 may extend at an angle θ6in the second region 126 to the main surface of the substrate 116. In some embodiments, the angle θ6may be about 60° to about 90°. A sidewall of the first layer 118 in the second region 126 may extend at the same angle to the major surface of the substrate 116 as a sidewall of the second layer 120 in the second region 126, or the sidewall of the first layer 118 in the second region 126 may extend at a different angle than the sidewall of the second layer 120 in the second region 126. Similarly, the sidewall of the first layer 118 in the second region 126 may extend at the same angle to the major surface of the substrate 116 as the sidewall of the third layer 122 in the second region 126, or the sidewall of the first layer 118 in the second region 126 may extend at a different angle than the sidewall of the third layer 122 in the second region 126. Additionally, the sidewall of the second layer 120 in the second region 126 may extend at the same angle to the major surface of the substrate 116 as the sidewall of the third layer 122 in the second region 126, or the sidewall of the second layer 120 in the second region 126 may extend at a different angle than the sidewall of the third layer 122 in the second region 126.For the first layer 118, the second layer 120 and the third layer 122, if the respective layer has the same material composition in the first region 124 and the second region 126, respectively, the angles formed by the side walls of the respective layer in the first region 124 and the second region 126 may be the same. If the respective layer has a different material composition in the first region 124 than in the second region 126, the angles formed by the side walls of the respective layer in the first region 124 and the second region 126 may be different from each other.As shown in Figure 8, after completion of the first etch process, edges of the first layer 118, the second layer 120, and / or the third layer 122 may extend laterally beyond edges of the first patterned photoresist 128. For example, the third layer 122 may extend beyond one or more edges of the first patterned photoresist 128 by a distance D3. In some embodiments, D3 is about 200 Å to about 5000 Å. Additionally, after completion of the first etch process, edges of the first layer 118, the second layer 120, and / or the third layer 122 may extend laterally beyond edges of the second patterned photoresist 130. For example, the third layer 122 may extend beyond one or more edges of the second patterned photoresist 130 by a distance D4. In some embodiments, D4 is about about 20 nm to about 500 nm. The distance D3 may be equal to or different from the distance D4, depending, for example, on the material composition of the third layer 122 in the first region 124 and the second region 126 and / or on the one or more etchants used in the first etch process.Then, in FIG. 9, a polymer 132 is formed along edges of the first patterned photoresist 128 and the second patterned photoresist 130 and along sidewalls of the first layer 118, the second layer 120, and the third layer 122. In some embodiments, the polymer 132 is deposited by, for example, CVD, ALD, PVD, PECVD, or the like. In each of the first region 124 and the second region 126, a thickness of the polymer 132 may be smallest at an upper part of the polymer 132 and larger at a lower part, and may vary according to the height. The lower part of the polymer 132 may contact the substrate 116.In Fig. 10, the polymer 132 is removed. In some embodiments, the polymer 132 may be removed with an O2 stripping process. In the O2 stripping process, a portion of the first patterned photoresist 128 and / or the second patterned photoresist 130 may be consumed. For example, a thickness of the first patterned photoresist 128 and / or the second patterned photoresist 130 may be reduced by the O2 stripping process. In some embodiments, after the O2 stripping process, the first patterned photoresist 128 may have a thickness T7. The thickness T7 may be about 150 nm to about 1 μm. In some embodiments, after the O2 stripping process, the second patterned photoresist 130 may have a thickness T8, which may be about 150 nm to about 1 μm.After the O2 stripping process, the first patterned photoresist 128 and / or the second patterned photoresist 130 may have top surfaces that are concave or otherwise non-planar. In other embodiments, the first patterned photoresist 128 and / or the second patterned photoresist 130 may have top surfaces that are planar after the O2 stripping process.After the O2 stripping process, the first patterned photoresist 128 and / or the second patterned photoresist 130 may have tapered sidewalls. For example, a width of the first patterned photoresist 128 and / or the second patterned photoresist 130 may change according to the height. A width W4 of the top surface of the first patterned photoresist 128 may be about 200 nm to about 1 μm after the O2 stripping process. An approximately width W5 of the bottom surface of the first patterned photoresist 128 may be about 400 nm to about 1.6 μm after the O2 stripping process. A width W6 of the top surface of the second patterned photoresist 130 may be about 1 μm after the O2 stripping process. A width W7 of the bottom surface of the second patterned photoresist 130 may be about 400 nm to about 1.6 μm after the O2 stripping process. A top surface of the third layer 122 may be exposed by consuming the first patterned photoresist 128 and / or the second patterned photoresist 130 by the O2 stripping process. In some embodiments, a portion of the first layer 118, the second layer 120, and / or the third layer 122 may be consuming by the O2 stripping process.In Figure 11, a second etch process is then performed using the first patterned photoresist 128 and the second patterned photoresist 130 as etch masks. The second etch process may be the same as the second etch process described above with reference to Figure 5, and the above discussion is fully reflected here.The second etching process may continue until desired profiles for the sidewalls of the first layer 118, the second layer 120, and the third layer 122 in the first region 124 and the second region 126 are achieved. For example, FIG. 11 shows a particular sidewall profile of a first multilayer structure 134 formed by the first layer 118, the second layer 120, and the third layer 122 in the first region 124, and a particular sidewall profile of a second multilayer structure 136 formed by the first layer 118, the second layer 120, and the third layer 122 in the second region 126. When the desired sidewall profiles of the multilayer structures 124 and 126 are achieved, the second etching process may be terminated. In some embodiments, the achievement of the desired sidewall profiles may be determined according to an elapsed time for the second etching process. In some embodiments, the achievement of the desired sidewall profiles may be determined by measurement. The desired sidewall profiles of the multilayer structures produced in the first region 124 and the second region 126 may be the same or different.Then, the first patterned photoresist 128 and the second patterned photoresist 130 are removed, for example, using a stripping process. The resulting structure is shown in Fig. 12. Fig. 12 shows an enlarged view of the multilayer structures of Fig. 11. The first multilayer structure 134 shown in Fig. 12 includes the first layer 118, the second layer 120, and the third layer 122. The first layer 118, the second layer 120, and the third layer 122 that are part of the first multilayer structure 134 of Fig. 12 have respective sidewalls that form respective angles with the main surface of the substrate 116. For example, sidewalls of the first layer 118 of the first multilayer structure 134 have a base angle θ7to the major surface of the substrate 116. In some embodiments, the base angle θ7is about 55° to about 90°. Sidewalls of the second layer 120 of the first multilayer structure 134 have a re-entrant angle θ8to the major surface of the substrate 116. In some embodiments, the re-entrant angle θ8is about 80° to about 145°. Sidewalls of the third layer 122 of the first multilayer structure 134 have a cone angle θ9to the major surface of the substrate 116. In some embodiments, the cone angle θ9is about 55° to about 116°.Any combination is possible according to the material compositions for the first layer 118, the second layer 120, and the third layer 122 and according to the etchants used in the second etching process described above with reference to FIG. 11. For example, as set forth above with reference to FIG. 6, in one embodiment, the base angle of the first multilayer structure 134 is about 89°, the re-entrant angle of the first multilayer structure 134 is about 88°, and the cone angle of the first multilayer structure 134 is about 83°. In another embodiment, the base angle of the first multilayer structure 134 is about 60°, the re-entrant angle of the first multilayer structure 134 is about 130°, and the cone angle of the first multilayer structure 134 is about 67°. In another embodiment, the base angle of the first multilayer structure 134 is about 64°, the re-entry angle of the first multilayer structure 134 is about 105°, and the cone angle of the first multilayer structure 134 is about 61°. In this way, by changing the materials used and the parameters and etchants for the etch processes described herein, a specific base angle, re-entry angle, and cone angle can be created and a specific sidewall profile for the first multilayer structure 134 can be achieved.A second multilayer structure 136, shown in FIG. 12, includes the first layer 118, the second layer 120, and the third layer 122. The first layer 118, the second layer 120, and the third layer 122, which are components of the second multilayer structure 136, have respective sidewalls that form respective angles with the major surface of the substrate 116. For example, sidewalls of the first layer 118 of the second multilayer structure 136 have a base angle θ10 to the major surface of the substrate 116. In some embodiments, the base angle θ10 is about 55° to about 90°. The base angle θ10 may be equal to or different from the base angle θ7 depending, for example, on the material compositions of the first layer 118 in the first region 124 and the second region 126. Sidewalls of the second layer 120 of the second multilayer structure 136 have a re-entry angle θ11to the main surface of the substrate 116. In some embodiments, the re-entry angle θ11is about 80° to about 145°. The re-entry angle θ11may be equal to or different from the re-entry angle θ8, depending, for example, on the material compositions of the second layer 120 in the first region 124 and the second region 126. Sidewalls of the third layer 122 of the second multilayer structure 136 have a cone angle θ12to the main surface of the substrate 116. In some embodiments, the cone angle θ12is about 55° to about 116°. The cone angle θ12may be equal to or different from the cone angle θ9, which depends, for example, on the material compositions of the third layer 122 in the first region 124 and the second region 126.According to the material compositions for the first layer 118, the second layer 120, and the third layer 122 and according to the etchants used in the second etch process described above with reference to FIG. 11, any desired sidewall profile for the second multilayer structure 136 is possible. In one embodiment, the base angle of the second multilayer structure 136 is about 83°, the re-entrant angle of the second multilayer structure 136 is about 88°, and the cone angle of the second multilayer structure 136 is about 89°. In another embodiment, the base angle of the second multilayer structure 136 is about 67°, the re-entrant angle of the second multilayer structure 136 is about 130°, and the cone angle of the first multilayer structure 134 is about 60°. In another embodiment, the base angle of the second multilayer structure 136 is about 61°, the re-entry angle of the second multilayer structure 136 is about 105°, and the cone angle of the second multilayer structure 136 is about 64°. In this way, by changing the base angle, the re-entry angle, and the cone angle, a specific sidewall profile for the second multilayer structure 136 can be achieved.1-12 illustrate the fabrication of multilayer structures having three layers. In some embodiments, the processes described above may be used to fabricate multilayer structures having more than three layers. FIG. 13 illustrates a multilayer structure 138 having four layers. A first layer 140 may be the same or similar to the first layer 102 discussed above with reference to FIG. 1, and the above discussion is incorporated herein. A second layer 142 and a third layer 144 may each be the same or similar to the second layer 104 discussed above with reference to FIG. 1, and the above discussion is incorporated herein. In some embodiments, material compositions of the second layer 142 and the third layer 144 are different. In other embodiments, material compositions of the second layer 142 and the third layer 144 are the same. A fourth layer 146 may be the same or similar to the layer 106 discussed above with reference to FIG. 1, and the above discussion of the third layer 106 is considered here. The multilayer structure 138 may be formed using the processes described above with reference to FIGS. 1-12.As shown in Fig. 13, a sidewall of the first layer 140 may form a base angle θ13 with a major surface of a substrate 148. In some embodiments, the base angle θ13 may be the same or similar to the base angle θ2 described above with reference to Fig. 6, and the above discussion of the base angle θ2 is considered here. A sidewall of the second layer 142 may form a re-entrant angle θ14 with the major surface of the substrate 148. In some embodiments, the re-entrant angle θ14 may be the same or similar to the re-entrant angle θ3 described above with reference to Fig. 6, and the above discussion of the re-entrant angle θ3 is considered here. A sidewall of the third layer 144 may form a reentrant angle θ13 with the major surface of the substrate 148. In some embodiments, the reentrant angle θ13 may be the same or similar to the reentrant angle θ3 described above with reference to FIG. 6, and the above discussion of the reentrant angle θ3 is considered here. The reentrant angles θ14 and θ13 may be equal to or different from each other. A sidewall of the fourth layer 146 may form a cone angle θ16 with the major surface of the substrate 148. In some embodiments, the cone angle θ16may be the same or similar to the cone angle θ4 described above with reference to Figure 6, and the above discussion of the cone angle θ4 is considered here.Various embodiments may be fabricated using the processes discussed above. In Fig. 14, a structure is shown that includes a first multilayer structure 150 and a second multilayer structure 152 fabricated side by side on a substrate 154. The first multilayer structure 150 and the second multilayer structure 152 each have four layers, for example, as described above with reference to Fig. 13. The first multilayer structure 150 and the second multilayer structure 152 may be fabricated simultaneously, for example, as set forth with reference to Figs. 7-12. The first multilayer structure 150 may be substantially the same as the second multilayer structure 152, or it may be different from the second multilayer structure 152. For example, the material compositions of the layers of the first multilayer structure 150 may be the same as those of the layers of the second multilayer structure 152. In this case, the sidewall profiles of the first multilayer structure 150 may be substantially the same as the sidewall profiles of the second multilayer structure 152. In other embodiments, the material compositions of one or more layers of the first multilayer structure 150 may be different from those of one or more layers of the second multilayer structure 152. In this case, the sidewall profiles of the first multilayer structure 150 may be different from those of the second multilayer structure 152.Fig. 15 shows a structure comprising a first multilayer structure 156 and a second multilayer structure 158 fabricated side by side on a substrate 160. For example, the first multilayer structure 156 has four layers and the second multilayer structure 158 has three layers, as set forth above with reference to Figs. 6-13. The first multilayer structure 156 and the second multilayer structure 158 may be fabricated simultaneously, as set forth, for example, with reference to Figs. 7-12.16 shows a multilayer structure 176 that may be manufactured, for example, using the processes discussed above with reference to FIGS. 1-6. The multilayer structure 176 may include a bottom layer 164. The bottom layer 164 may be the same or similar to the first layer 102 discussed above with reference to FIG. 1, and the discussion of the first layer 102 is considered here. The multilayer structure 176 also includes middle layers 166, 168, 170, and 172. The middle layers 166, 168, 170, and 172 may each be the same or similar to the second layer 104 discussed above with reference to FIG. 1, and the discussion of the second layer 104 above is considered here. Although four middle layers 166, 168, 170, and 172 are shown in FIG. 16, other embodiments may use more or fewer middle layers. In some embodiments, material compositions of middle layers 166, 168, 170, and 172 may be different from one another. In other embodiments, material compositions of middle layers 166, 168, 170, and 172 may be the same. Multilayer structure 176 also includes a top layer 174. Top layer 174 may be the same or similar to third layer 106 discussed above with reference to FIG. 1, and the above discussion of third layer 106 is incorporated herein. Multilayer structure 176 may be formed using the processes described above with reference to FIGS. 1-12.As shown in Figure 16, a sidewall of the bottom layer 164 may form a base angle θ17 with a major surface of a substrate 162. In some embodiments, the base angle θ17 may be the same or similar to the base angle θ2 described above with reference to Figure 6, and the above discussion of the base angle θ2 is considered here. A sidewall of each of the middle layers 166, 168, 170, and 172 may each form a reentrant angle θ18 with the major surface of the substrate 162. In some embodiments, the re-entry angle θ18 of a respective middle layer may be the same or similar to the re-entry angle θ3 described above with reference to FIG. 6, and the above discussion of the re-entry angle θ3 is considered here. The re-entry angles θ3 of the individual middle layers 166, 168, 170, and 172 may be the same or different from each other. A sidewall of a top layer 174 may form a cone angle θ19 with the major surface of the substrate 162. In some embodiments, the cone angle θ19 may be the same or similar to the cone angle θ4 described above with reference to FIG. 6, and the above discussion of the cone angle θ4 is considered here.Fig. 17 shows a structure in which a first multilayer structure 178 and a second multilayer structure 180 are fabricated side by side on a substrate 182. The first multilayer structure 178 and the second multilayer structure 180 may each be the same or similar to the multilayer structure 176 shown in Fig. 16, and the discussion of the multilayer structure 176 is considered here. The first multilayer structure 178 and the second multilayer structure 180 may be fabricated simultaneously using the processes described above with reference to Figs. 7-12.18 shows a structure in which a first multilayer structure 184 and a second multilayer structure 186 are fabricated side by side on a substrate 188. The first multilayer structure 184 may be the same or similar to the multilayer structure 176 shown in FIG. 16, and the discussion of the multilayer structure 176 is considered here. The second multilayer structure 186 may be the same or similar to the multilayer structure 138 shown in FIG. 13, and the discussion of the multilayer structure 138 is considered here. The first multilayer structure 184 and the second multilayer structure 186 may be fabricated simultaneously using the processes described above with reference to FIGS. 7-12.19 shows a structure in which a first multilayer structure 190 and a second multilayer structure 192 are fabricated side by side on a substrate 194. The first multilayer structure 190 may be the same or similar to the multilayer structure 176 shown in FIG. 16, and the discussion of the multilayer structure 176 is considered here. The second multilayer structure 192 may be the same or similar to the multilayer structure 112 shown in FIG. 6, and the discussion of the multilayer structure 112 is considered here. The first multilayer structure 190 and the second multilayer structure 192 may be fabricated simultaneously using the processes described above with reference to FIGS. 7-12.20 shows a structure in which a first multilayer structure 196, a second multilayer structure 198, and a third multilayer structure 200 are fabricated side by side on a substrate 197. The first multilayer structure 196 may be the same or similar to the multilayer structure 176 shown in FIG. 16, and the discussion of the multilayer structure 176 is considered here. The second multilayer structure 198 may be the same or similar to the multilayer structure 112 shown in FIG. 6, and the discussion of the multilayer structure 112 is considered here. The third multilayer structure 200 may be the same or similar to the multilayer structure 138 shown in FIG. 13, and the discussion of the multilayer structure 138 is considered here. The first multilayer structure 196, the second multilayer structure 198, and the third multilayer structure 200 may be simultaneously fabricated using the processes described above with reference to FIGS. 7-12.The above embodiments may be used for many different purposes. In some embodiments, the multilayer structures described herein may be used in the fabrication of a sandwich architecture for an integrated Si nanosystem device, for example, for sensing, display, and MEMS (micro-electromechanical system) applications, and the like.21 to 25 show intermediate stages in the fabrication of a sandwich architecture for an integrated Si nanosystem device having the multilayer structures described herein. In FIG. 21, a substrate 210 is shown. Any suitable substrate 210 may be used. In some embodiments, the substrate 210 may include an integrated circuit having one or more active devices, passive devices, and electrical circuits. For example, the substrate 210 may include a complementary metal oxide semiconductor (CMOS) chip. In other embodiments, the substrate 210 may not include any active devices, but only passive devices or electrical interconnects. In further embodiments, the substrate 210 may not include any active devices, passive devices, or electrical interconnects. Any suitable materials may be used to fabricate the substrate 210.Electrical interconnects 212 are fabricated on the substrate 210. In some embodiments, the electrical interconnects 212 are fabricated from a conductive material, such as a metal. For example, the electrical interconnects 212 may be fabricated from aluminum, copper, a combination thereof, or the like. The electrical interconnects 212 may establish electrical connections to devices and / or circuits in the substrate 210.A dielectric material 214 may be deposited over the electrical interconnects 212 and along sidewalls of the electrical interconnects 212. The dielectric material 214 may extend along a surface of the substrate 210. The dielectric material 214 may electrically isolate an electrical interconnect 212 from an adjacent electrical interconnect 212. Any suitable dielectric material may be used. The dielectric material 214 may be made from a polymer such as polybenzoxazole (PBO), polyimide, benzocyclobutene (BCB), or the like; a nitride such as silicon nitride or the like; an oxide such as silicon oxide, phosphosilicate glass (PSG), borosilicate glass (BSG), borophosphosilicate glass (BPSG), or a combination thereof or the like; or the like, for example, by spin coating, lamination, chemical vapor deposition (CVD), or the like.A lower conductive layer 216 is formed over the dielectric material 214. The lower conductive layer 216 extends through the dielectric material 214 to contact the electrical interconnects 212. In this way, the lower conductive layer 216 may be electrically connected to an electrical circuit of the substrate 210. The lower conductive layer 216 may be formed from a metal, for example, Al, AlCu, Ti, TiN, or the like. In other embodiments, the lower conductive layer 216 may be formed from a metal oxide, for example, ITO, ZnO, RuO, or the like. The lower conductive layer 216 may be formed using a suitable deposition process, such as ALD, CVD, PVD, or the like.Multilayer structures 224, 226, and 228 are formed over the lower conductive layer 216. In some embodiments, the multilayer structures 224, 226, and 228 are formed using the processes described above with reference to FIGS. 1-20. Although the cross-section shown in FIG. 21 illustrates the multilayer structures 224, 226, and 228 as separate from one another, in plan view two or more of the multilayer structures 224, 226, and 228 may be contiguous. And although three layers are shown in each of the multilayer structures 224, 226, and 228, in some embodiments one or more of the multilayer structures 224, 226, and 228 may be formed from additional layers described above with reference to FIGS. 1-20.In some devices, a first layer, a second layer, a third layer, and a fourth layer are formed over the structure shown in Fig. 21 (see Figs. 22-25). The first through fourth layers each have portions that are located over the multilayer structures 224, 226, and 228 and portions that are not located over the multilayer structures 224, 226, and 228. In some devices, it may be desirable for the portions of one or more of these layers (e.g., the second layer and the first layer) that are not located over the multilayer structures 224, 226, and 228 to be separated from portions of the second and first layers that are located over the multilayer structures 224, 226, and 228. In these devices, it may be desirable for other layers, such as the third layer and the fourth layer, to be contiguous between the portions of the third and fourth layers that are above the multilayer structures 224, 226, and 228 and the portions of the third and fourth layers that are not above the multilayer structures 224, 226, and 228. In some embodiments, the multilayer structures 224, 226, and 228 may enable the first through fourth layers to be fabricated to be contiguous or separate as desired.In Figure 22, a first layer 230 is formed over the lower conductive layer 216 along sidewalls of the multilayer structures 224, 226, and 228 and along top surfaces of the multilayer structures 224, 226, and 228. The first layer 230 may be formed from a metal, for example, Al, AlCu, Ti, TiN, or the like. In other embodiments, the first layer 230 may be formed from a metal oxide, for example, ITO, ZnO, RuO, or the like. In some embodiments, the first layer 230 is deposited by, for example, CVD, ALD, PVD, plasma enhanced chemical vapor deposition (PECVD), or the like.As shown in Fig. 22, the sidewall profiles of the multilayer structures 224, 226, and 228 allow the first layer 230 to be fabricated such that portions of the first layer 230 that are not located above any of the multilayer structures 224, 226, and 228 are separated from portions of the first layer 230 that are located above any of the multilayer structures 224, 226, and 228. For example, a top surface of the first layer 230 may intersect second layers 220 of the multilayer structures 224, 226, and 228, and the re-entrant angles of the sidewalls of the second layers 220 may assist in separating the portions of the first layer 230 that are not located above any of the multilayer structures 224, 226, and 228 from the portions of the first layer 230 that are located above any of the multilayer structures 224, 226, and 228.In Fig. 23, a second layer 232 is formed over the first layer 230. Some portions of the second layer 232 are located over the multilayer structures 224, 226, and 228, and other portions of the second layer 232 are not located over the multilayer structures 224, 226, and 228. In some embodiments, the second layer 232 is deposited by, for example, CVD, ALD, PVD, PECVD, or the like. In some embodiments, the second layer 232 is a conductive layer. The second layer 232 may be made of a metal, for example, Al, AlCu, Ti, TiN, or the like. In other embodiments, the second layer 232 may be made of a metal oxide, for example, ITO, ZnO, RuO, or the like.As shown in Fig. 23, the sidewall profiles of the multilayer structures 224, 226, and 228 may fabricate the second layer 232 such that portions of the second layer 232 that are not located over one of the multilayer structures 224, 226, and 228 are separated from portions of the second layer 232 that are located over one of the multilayer structures 224, 226, and 228. For example, a top surface of the second layer 232 may intersect the second layers 220 of the multilayer structures 224, 226, and 228, and the re-entrant angles of the sidewalls of the second layers 220 may assist in separating the portions of the second layer 232 that are not located above any of the multilayer structures 224, 226, and 228 from the portions of the second layer 232 that are located above any of the multilayer structures 224, 226, and 228.In Fig. 24, a third layer 234 is formed over the second layer 232. Some portions of the third layer 234 are located over the multilayer structures 224, 226, and 228, and other portions of the third layer 234 are not located over the multilayer structures 224, 226, and 228. In some embodiments, the third layer 234 is deposited, for example, by CVD, ALD, PVD, PECVD, or the like. In some embodiments, the third layer 234 is a conductive layer. The third layer 234 may be formed from a metal, for example, Al, AlCu, Ti, TiN, or the like. In other embodiments, the third layer 234 may be formed from a metal oxide, for example, ITO, ZnO, RuO, or the like.As shown in Figure 24, the sidewall profiles of the multilayer structures 224, 226, and 228 allow the third layer 234 to be fabricated such that portions of the third layer 234 that are not located above one of the multilayer structures 224, 226, and 228 are continuous with portions of the third layer 234 that are located above one of the multilayer structures 224, 226, and 228. For example, a top surface of the third layer 234 may intersect third layers 222 of the multilayer structures 224, 226, and 228, and the taper angles of the sidewalls of the third layers 222 may assist in bonding the portions of the third layer 234 that are not located above any of the multilayer structures 224, 226, and 228 to the portions of the third layer 234 that are located above any of the multilayer structures 224, 226, and 228.In Fig. 25, a fourth layer 236 is formed over the third layer 234. Some portions of the fourth layer 236 are located over the multilayer structures 224, 226, and 228, and other portions of the fourth layer 236 are not located over the multilayer structures 224, 226, and 228. In some embodiments, the fourth layer 236 is deposited by, for example, CVD, ALD, PVD, PECVD, or the like. In some embodiments, the fourth layer 236 is a conductive layer. The fourth layer 236 may be formed from a metal, for example, Al, AlCu, Ti, TiN, or the like. In other embodiments, the fourth layer 236 may be formed from a metal oxide, for example, ITO, ZnO, RuO, or the like.As shown in Figure 25, the sidewall profiles of the multilayer structures 224, 226, and 228 allow the fourth layer 236 to be fabricated such that portions of the fourth layer 236 that are not located above one of the multilayer structures 224, 226, and 228 are continuous with portions of the fourth layer 236 that are located above one of the multilayer structures 224, 226, and 228. For example, a top surface of the fourth layer 236 may intersect the third layers 222 of the multilayer structures 224, 226, and 228, and the taper angles of the sidewalls of the third layers 222 may assist in bonding the portions of the fourth layer 236 that are not located above any of the multilayer structures 224, 226, and 228 to the portions of the fourth layer 236 that are located above any of the multilayer structures 224, 226, and 228.As set forth herein, multilayer structures and methods of making the same are provided in accordance with some embodiments. The multilayer structures may have sidewalls with profiles that may be tailored to a specific design. For example, in a multilayer structure, one layer of the multilayer structure may have a sidewall that extends at a first angle and a second layer of the multilayer structure may have a sidewall that extends at a second angle, where the first and second angles may be different from each other. In addition, the multilayer structure may also include additional layers, and sidewalls of the additional layers may extend at angles that are equal to or different from the first or second angle. In this way, a desired sidewall profile of the multilayer structure may be achieved.According to some embodiments, a desired sidewall profile of a multilayer structure may be achieved with only one deposition / lithography / etch process rather than multiple deposition / lithography / etch processes. Accordingly, a multilayer structure having a desired sidewall profile may be manufactured at a lower cost and in less time. This may improve manufacturing cycle times and / or yields.In some embodiments, a multilayer structure having a sidewall profile described herein may be used in the fabrication of integrated Si nanosystem devices that include sandwich architectures extending adjacent to and / or across multilayer structures. In some embodiments, the multilayer structures are disposed over a substrate, for example, a silicon complementary metal oxide semiconductor (CMOS) chip. Some Si nanosystem devices may include a multilayer structure over the CMOS chip. One or more layers may be disposed over the multilayer structure, which may extend laterally beyond the multilayer structure above the CMOS chip. In some devices, it may be convenient to fabricate a first layer of the one or more layers such that a first portion of the first layer not located above the multilayer structure is separated from a second portion of the first layer located above the multilayer structure. Similarly, in some devices, it may be desirable to fabricate a second layer such that a first portion of the second layer that contacts the first portion of the first layer is separated from a second portion of the second layer that is above the second portion of the first layer. Additional layers that are continuous between portions of the layers that are above the multilayer structure and portions that are not above the multilayer structure may be desired. The sidewall profile of the multilayer structure may be designed such that at least a portion of the sidewall helps to define and / or separate the first portion of the first layer from the second portion of the first layer and / or separate the first portion of the second layer from the second portion of the second layer, while other layers may be fabricated continuous.According to some embodiments, a method is provided. The method comprises the steps of: depositing a plurality of layers on a substrate; patterning a first mask over the plurality of layers; performing a first etching process on the plurality of layers using the first mask as an etching mask, wherein after the first etching process the plurality of layers extend laterally beyond the first mask and sidewalls of the plurality of layers are tapered; depositing a polymer material along sidewalls of the first mask and sidewalls of the plurality of layers; removing the polymer material, wherein the removal of the polymer material consumes a portion of the first mask to form a first residual mask; and performing a second etching process on the plurality of layers using the first residual mask as an etching mask, wherein after completion of the second etching process a common sidewall profile of the plurality of layers comprises a first portion and a second portion and a first angle of the first portion and a second angle of the second portion are different from each other. In one embodiment, removing the polymer material results in sidewalls of the first mask being tapered. In one embodiment, the first angle is formed by the first part with respect to a major surface of the substrate and the second angle is formed by the second part with respect to the major surface of the substrate, the first angle is acute and the second angle is obtuse. In one embodiment, the plurality of layers comprises a first layer, a second layer, and a third layer, the first part comprising a sidewall of the first layer, the second part comprising a sidewall of the second layer, and a third part of the common sidewall profile comprising a sidewall of the third layer, and the first angle, the second angle, and the third angle of the third part are different from each other. In one embodiment, the first angle is 55° to 90°. In one embodiment, the second angle is 80° to 145°. In one embodiment, the third angle is 55° to 100°. In an embodiment, the method further comprises forming a first layer, wherein a first portion of the first layer is disposed over the plurality of layers and a second portion of the first layer is not disposed over the plurality of layers, wherein the first portion of the first layer is physically separated from the second portion of the first layer. In an embodiment, the method further comprises forming a second layer over the first layer, wherein a first portion of the second layer is disposed over the plurality of layers and a second portion of the second layer is not disposed over the plurality of layers, wherein the first portion of the second layer is physically separated from the second portion of the second layer. In an embodiment, the method further comprises: forming a third layer, wherein the third layer is contiguous between a first portion of the third layer disposed over the plurality of layers and a second portion of the third layer not disposed over the plurality of layers; and forming a fourth layer, wherein the fourth layer is contiguous between a first portion of the fourth layer disposed over the plurality of layers and a second portion of the fourth layer not disposed over the plurality of layers.According to some embodiments, a method is provided. The method includes the steps of: forming a first plurality of layers on a substrate, wherein a material composition of a first layer of the first plurality of layers is different from a material composition of a second layer of the first plurality of layers; depositing a photoresist material over the first plurality of layers; patterning the photoresist material to form a first mask and a second mask; performing a first etching process using the first mask and the second mask as etching masks, wherein the first etching process removes portions of the first plurality of layers extending between the first mask and the second mask to form a second plurality of layers beneath the first mask and a third plurality of layers beneath the second mask; depositing a polymer along sidewalls of the first mask and the second mask, wherein sidewalls of the polymer are tapered; Removing the polymer with a stripping process, the stripping process consuming a portion of the first mask and a portion of the second mask to form a first residual mask and a second residual mask, wherein a shape of the first residual mask is different from a shape of the first mask and a shape of the second residual mask is different from a shape of the second mask; performing a second etching process on the second plurality of layers and the third plurality of layers using the first residual mask and the second residual mask as etching masks, the second etching process ending when a sidewall profile of the second plurality of layers is a desired sidewall profile, the desired sidewall profile having different portions of the desired sidewall profile extending at different angles; and removing the first residual mask and the second residual mask. In one embodiment, after the stripping process, sidewalls of the first residual mask and the second residual mask are tapered. In one embodiment, the second etching process is performed using a first etchant and oxygen gas as an etchant, the first etchant comprising carbon and fluorine. In one embodiment, the second plurality of layers comprises a first layer, a second layer, a third layer, and a fourth layer, wherein a first angle is formed by a sidewall of the first layer and a major surface of the substrate, a second angle is formed by a sidewall of the second layer and the major surface of the substrate, a third angle is formed by a sidewall of the third layer and the major surface of the substrate, and a fourth angle is formed by a sidewall of the fourth layer and the major surface of the substrate, wherein the second angle and the third angle are equal and the first angle and the fourth angle are different from the second angle and the third angle. In one embodiment, the method comprises forming a first layer, a second layer, a third layer, and a fourth layer along sidewalls of the second plurality of layers, wherein the desired sidewall profile results in the first layer and the second layer being separated along the sidewalls of the first plurality of layers and the third layer and the fourth layer being contiguous along the sidewalls of the first plurality of layers. In one embodiment, the first plurality of layers comprises at least six layers.According to some embodiments, a device is provided. The device comprises: a substrate; a lower conductive layer over the substrate; a multilayer structure over the lower conductive layer, wherein a first portion of the lower conductive layer is not covered by the multilayer structure and a second portion of the lower conductive layer is covered by the multilayer structure; a first layer, wherein a first portion of the first layer is disposed over the first portion of the lower conductive layer and a second portion of the first layer is disposed over the multilayer structure, wherein the first portion of the first layer is separated from the second portion of the first layer and a portion of the multilayer structure extends between the first portion of the first layer and the second portion of the first layer; a second layer, wherein a first portion of the second layer is disposed over the first portion of the first layer and a second portion of the second layer is disposed over the multilayer structure, wherein the first portion of the second layer is separated from the second portion of the second layer, wherein the portion of the multilayer structure extends between the first portion of the second layer and the second portion of the second layer; a third layer, wherein a first portion of the third layer is disposed over the first portion of the second layer and a second portion of the third layer is disposed over the second portion of the second layer, the first portion of the third layer being continuous with the second portion of the third layer; and a fourth layer disposed over the third layer, wherein a first portion of the fourth layer is disposed over the first portion of the third layer and a second portion of the fourth layer is disposed over the second portion of the third layer, the first portion of the fourth layer being continuous with the second portion of the fourth layer. In one embodiment, the multilayer structure includes a fifth layer, a sixth layer, and a second layer, wherein a portion of the sixth layer extends between the first portion of the first layer and the second portion of the first layer. In one embodiment, the portion of the sixth layer extends between the first portion of the second layer and the second portion of the second layer. In one embodiment, the first layer covers a sidewall of the fifth layer.

Claims

A method comprising the steps of: depositing a plurality of layers (102-106, 118-122, 218-222) on a substrate (100, 116, 210); patterning a first mask (108, 128) over the plurality of layers (102-106, 118-122, 218-222); Performing a first etching process on the plurality of layers (102-106, 118-122, 218-222) using the first mask (108, 128) as an etching mask, wherein after the first etching process the plurality of layers (102-106, 118-122, 218-222) extend laterally beyond the first mask (108, 128) and sidewalls of the plurality of layers (102-106, 118-122, 218-222) are tapered; Depositing a polymer material (110; 132) along sidewalls of the first mask (108, 128) and along sidewalls of the plurality of layers (102-106, 118-122, 218-222); Removing the polymer material (110; 132), wherein the removal of the polymer material (110; 132) consumes a portion of the first mask (108, 128) to form a first residual mask; and performing a second etching process on the plurality of layers (102-106, 118-122, 218-222) using the first residual mask, wherein after completion of the second etching process, a common sidewall profile of the plurality of layers (102-106, 118-122, 218-) comprises a first part and a second part, wherein a first angle of the first part and a second angle of the second part are different from each other, further comprising: producing a first layer (230), wherein a first part of the first layer (230) is arranged above the plurality of layers (218-222-) and a second part of the first layer (230) is not arranged above the plurality of layers (218-222), wherein the first part of the first layer (230) is physically separated from the second part of the first layer (230), further comprising: producing a second layer (232) above the first layer (230), wherein a first portion of the second layer (232) is disposed over the plurality of layers (218-222) and a second portion of the second layer (232) is not disposed over the plurality of layers (218-222), wherein the first portion of the second layer (232) is physically separated from the second portion of the second layer (232), further comprising: forming a third layer (234), the third layer (234) being contiguous between a first portion of the third layer (234) disposed over the plurality of layers (218-222) and a second portion of the third layer (234) not disposed over the plurality of layers (218-222); and forming a fourth layer (236), the fourth layer (236) being continuous between a first portion of the fourth layer (236) disposed over the plurality of layers (218-222) and a second portion of the fourth layer (236) not disposed over the plurality of layers (218-222).The method of claim 1, wherein removing the polymer material (110; 132) results in sidewalls of the first mask (108; 128) being tapered.The method of claim 1 or 2, wherein the first angle is formed by the first part with respect to a major surface of the substrate (100, 116, 210) and the second angle is formed by the second part with respect to the major surface of the substrate (100, 116, 210), wherein the first angle is acute and the second angle is obtuse.A method according to any one of the preceding claims, wherein the plurality of layers (102-106, 118-122, 218-222) comprises a first layer (102, 118, 218), a second layer (104, 120, 220) and a third layer (106, 122, 222), the first part comprising a sidewall of the first layer (102, 118, 218), the second part comprising a sidewall of the second layer (104, 120, 220) and a third part of the common sidewall profile comprising a sidewall of the third layer (106, 122, 222), the first angle, the second angle and a third angle of the third part being different from each other.Method according to one of the preceding claims, wherein the first angle is 55° to 90°.Method according to one of the preceding claims, wherein the second angle is 80° to 145°.The method of claim 4, wherein the third angle is 55° to 100°.A method comprising the steps of: forming a first plurality of layers (118-122, 218-222) on a substrate (116, 210), wherein a material composition of a first layer (118, 218) of the first plurality of layers is different from a material composition of a second layer (120, 220) of the first plurality of layers; depositing a photoresist material over the first plurality of layers (118-122, 218-222); patterning the photoresist material to produce a first mask (128) and a second mask (130); Performing a first etching process using the first mask (128) and the second mask (130) as etching masks, wherein the first etching process removes portions of the first plurality of layers (118-122, 218-222) extending between the first mask (128) and the second mask (130) to produce a second plurality of layers beneath the first mask (128) and a third plurality of layers beneath the second mask (130); Depositing a polymer (132) along sidewalls of the first mask (128) and the second mask (130), tapering sidewalls of the polymer (132); Removing the polymer (132) with a stripping process, the stripping process consuming a portion of the first mask (128) and a portion of the second mask (130) to create a first residual mask and a second residual mask, a shape of the first residual mask being different from a shape of the first mask (128) and a shape of the second residual mask being different from a shape of the second mask (130); performing a second etching process on the second plurality of layers and the third plurality of layers using the first residual mask and the second residual mask as etching masks, the second etching process ending when a sidewall profile of the second plurality of layers is a desired sidewall profile, the desired sidewall profile having different portions of the desired sidewall profile extending at different angles; and removing the first residual mask and the second residual mask, further comprising: forming a first layer (230), a second layer (232), a third layer (234), and a fourth layer (236) along sidewalls of the second plurality of layers, wherein the desired sidewall profile results in the first layer (230) and the second layer (232) being separated along the sidewalls of the first plurality of layers and the third layer (234) and the fourth layer (236) being contiguous along the sidewalls of the first plurality of layers.The method of claim 8, wherein after the detachment process, sidewalls of the first residual mask and the second residual mask are tapered.The method of claim 8 or 9, wherein the second etching process is performed using a first etchant and oxygen gas as an etchant, the first etchant comprising carbon and fluorine.Method according to one of claims 8 to 10, wherein the second plurality of layers comprises a further first layer, a further second layer, a further third layer and a further fourth layer, wherein a first angle is formed by a side wall of the further first layer and a main surface of the substrate (116, 210), a second angle is formed by a side wall of the further second layer and the main surface of the substrate (116, 210), a third angle is formed by a side wall of the further third layer and the main surface of the substrate (1116, 210) and a fourth angle is formed by a side wall of the further fourth layer and the main surface of the substrate (116, 210), wherein the second angle and the third angle are equal and the first angle and the fourth angle are different from the second angle and the third angle.A method according to any one of claims 8 to 11, wherein the first plurality of layers comprises at least six layers.A device comprising: a substrate (210); a lower conductive layer (216) over the substrate (210); a multilayer structure (218-222) over the lower conductive layer (216), wherein a first portion of the lower conductive layer (212) is not covered by the multilayer structure (218-222) and a second portion of the lower conductive layer (216) is covered by the multilayer structure (218-222); wherein the multilayer structure (218-222) comprises a plurality of layers having a common sidewall profile with a first portion and a second portion, wherein a first angle of the first portion and a second angle of the second portion are different from each other; the device further comprising: a first layer (230), wherein a first portion of the first layer (230) is disposed over the first portion of the lower conductive layer (216) and a second portion of the first layer (230) is disposed over the multilayer structure (218-222), wherein the first portion of the first layer (230) is separated from the second portion of the first layer (230) and a portion of the multilayer structure (218, 220, 222) extends between the first portion of the first layer (230) and the second portion of the first layer (230); a second layer (232), wherein a first portion of the second layer (232) is disposed over the first portion of the first layer (230) and a second portion of the second layer (232) is disposed over the multilayer structure (218-222), wherein the first portion of the second layer (232) is separate from the second portion of the second layer (232) and the portion of the multilayer structure (218-222) extends between the first portion of the second layer (232) and the second portion of the second layer (232); a third layer (234), wherein a first portion of the third layer (234) is disposed over the first portion of the second layer (232) and a second portion of the third layer (234) is disposed over the second portion of the second layer (232), wherein the first portion of the third layer (234) is continuous with the second portion of the third layer (234); and a fourth layer (236) disposed over the third layer (234), wherein a first portion of the fourth layer (236) is disposed over the first portion of the third layer (234) and a second portion of the fourth layer (236) is disposed over the second portion of the third layer (234), wherein the first portion of the fourth layer (236) is continuous with the second portion of the fourth layer (236).The device of claim 13, wherein the multilayer structure (218-222) comprises a fifth layer, a sixth layer, and a further second layer, wherein a portion of the sixth layer extends between the first portion of the first layer (230) and the second portion of the first layer (230).The device of claim 14, wherein the portion of the sixth layer extends between the first portion of the second layer (232) and the second portion of the second layer (232); and / or wherein the first layer (230) covers a sidewall of the fifth layer.

Citation Information

Patent Citations

  • process for the selective deposition of refractory metals on silicon bodies

    DE68926440T2

  • Method to control mask profile for read sensor definition

    US20090007416A1

  • Hardmask open process with enhanced CD space shrink and reduction

    US20090191711A1

  • Semiconductor device with contact pad and fabrication method therefore

    US20180233466A1

  • Method For Reducing Lithography Defects and Pattern Transfer

    US20180239244A1