Manufacturing process for optoelectronic devices
The method of growing semiconductor layers on a first layer, separating stacks by selective etching, and transferring them onto a second support addresses the high cost issue in III-V compound layer manufacturing, achieving cost-effective optoelectronic device production.
Patent Information
- Application Number
- FR2022004145
- Authority / Receiving Office
- FR · FR
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2022-05-02
- Publication Date
- 2024-10-11
- Estimated Expiration
- 2042-05-02
AI Technical Summary
Current methods for manufacturing optoelectronic devices using III-V compound layers are costly due to the limited number of layers that can be transferred and the high cost associated with the process.
A method involving the growth of semiconductor layers on a first layer of a first semiconductor material, separation of stacks by selective etching, and transfer of these stacks onto a second support, allowing for the reuse of the first support for further growth, using a second material that can be selectively etched, and incorporating a third layer in physical contact with the second layer.
Reduces manufacturing costs by enabling the reuse of the first support and allowing for efficient transfer and growth of semiconductor layers, thereby lowering the overall production expenses.
Smart Images

Figure 00000013_0000 
Figure 00000013_0001 
Figure 00000013_0002
Abstract
Description
Title of the invention: Method for manufacturing optoelectronic devices Technical field
[0001] The present description relates generally to methods of manufacturing optoelectronic devices. Prior art
[0002] Semiconductor materials suitable for producing optoelectronic components capable of capturing or emitting infrared radiation include III-V compounds. No processes are currently known for growing III-V compound layers by epitaxy directly on a silicon substrate.
[0003] An example of a method for manufacturing an optoelectronic device comprising optoelectronic components made of III-V compounds comprises the formation of a block made of a III-V compound, the transfer of a layer of the III-V compound from the block onto a support and the epitaxial growth, from the layer of the III-V compound, of a stack of semiconductor layers made of III-V compounds, in which the optoelectronic components will be formed. Such a method has a high cost, in particular due to the fact that the number of layers of the III-V compound that can be transferred from the same block is reduced. Summary of the invention
[0004] An object of an embodiment is to provide a method of manufacturing optoelectronic devices overcoming all or part of the drawbacks of existing methods.
[0005] Another object of an embodiment is that the manufacturing method has a reduced cost.
[0006] One embodiment provides a method for manufacturing optoelectronic devices comprising epitaxial growth, on each first layer of first layers of a first semiconductor material covering a first support and spaced apart from each other, of a second layer of a second material, and epitaxial growth, on each second layer, of a stack of semiconductor layers comprising a third layer in physical contact with the second layer, separation of each stack from the first layer by etching the second layer by selective etching with respect to both the first and third materials, and transfer of the stacks to a second support, each of the first and third materials being a III-V or II-VI compound.
[0007] According to one embodiment, the method comprises, after the step of separating each stack from the first layer, the reuse of the first support covered with the first layers for the growth by epitaxy, on each first layer, of a new second layer of the second semiconductor material, and the growth by epitaxy on each new second layer, of a new stack of semiconductor layers.
[0008] According to one embodiment, the second material is a ternary or quaternary compound.
[0009] According to one embodiment, the etching used in the step of separating each stack by etching the second layer is a wet etching selective with respect to the first and third materials.
[0010] According to one embodiment, the mesh parameters of the first, second, and third materials are equal to within 0.1%.
[0011] According to one embodiment, each stack further comprises at least a fourth layer of a fourth material, and the etching used in the step of separating each stack by etching the second layer is selective with respect to the first, third and fourth materials.
[0012] According to one embodiment, the second support comprises a plate comprising several copies of an electronic circuit, each electronic circuit being covered with a stack among the stacks after the step of transferring the stacks onto the second support.
[0013] According to one embodiment, the method further comprises cutting the plate to separate the electronic circuits each covered with a stack from among the stacks.
[0014] An embodiment also provides an intermediate product comprising a first support covered with first layers of a first semiconductor material spaced from each other and comprising, on each first layer, a second layer of a second material connected to the first layer by an epitaxial relationship, and, on each second layer, a stack of semiconductor layers comprising a third layer in physical contact with the second layer and connected to the second layer by an epitaxial relationship, each of the first and third materials being a III-V or II-VI compound, the second material being adapted to be etched selectively with respect to the first and third materials.
[0015] According to one embodiment, each stack further comprises at least a fourth layer of a fourth material, the second material being adapted to be selectively etched with respect to the first, third and fourth materials. Brief description of the drawings
[0016] These characteristics and advantages, as well as others, will be explained in detail in the following description of particular embodiments given without limitation in relation to the attached figures among which:
[0017] [Fig.l], [Fig.2], [Fig.3], [Fig.4], [Fig.5], [Fig.6], [Fig.7], [Fig.8], [Fig.9], and [Fig. 10] illustrate steps of an embodiment of a method for manufacturing optoelectronic devices;
[0018] [Fig.l 1] is a phase diagram; and
[0019] [Fig. 12] is a partial and schematic sectional view of an embodiment of an optoelectronic device. Description of the embodiments
[0020] The same elements have been designated by the same references in the different figures. In particular, the structural and / or functional elements common to the different embodiments may have the same references and may have identical structural, dimensional and material properties. For the sake of clarity, only the steps and elements useful for understanding the embodiments described have been shown and are detailed.
[0021] Unless otherwise specified, when referring to two elements connected together, this means directly connected without intermediate elements other than conductors, and when referring to two elements connected (in English "coupled") together, this means that these two elements can be connected or be connected by means of one or more other elements. Furthermore, the terms "insulator" and "conductor" are considered here to mean respectively "electrically insulating" and "electrically conducting".
[0022] Unless otherwise specified, the expressions "about", "approximately", "substantially", and "of the order of" mean within 10%, preferably within 5%. Unless otherwise specified, ordinal numeral adjectives, such as "first", "second", etc., are used only to distinguish elements from one another. In particular, these adjectives do not limit the described embodiments to a particular order of these elements.
[0023] An embodiment of a method for manufacturing optoelectronic devices comprising III-V or II-VI compound optoelectronic components will now be described in relation to Figures 1 to 10, which are partial and schematic sectional views illustrating the structures obtained at steps of the embodiment of the manufacturing method.
[0024] Figures 1 to 5 illustrate steps of the embodiment of the manufacturing method which are implemented at the first implementation of the method and lead to obtaining a support covered with semiconductor layers shown in [Fig.5]. Figures 6 to 9 illustrate steps which are implemented during a manufacturing cycle of optoelectronic devices from the support covered with semiconductor layers of [Fig.5]. [Fig. 10] represents a support covered with semiconductor layers obtained following the manufacturing cycle of optoelectronic devices illustrated in Figures 6 to 9 and which can be used to carry out again the manufacturing cycle of optoelectronic devices illustrated in Figures 6 to 9.
[0025] [Fig.l] represents the structure obtained after the transfer, onto a support 10, of blocks 16 of a first monocrystalline semiconductor material each having an upper face 14, three blocks 16 being represented by way of example in [Fig.l]. The blocks 16 rest on the support 10 in physical contact with the support 10 at a distance from each other. The blocks 16 can be produced by sawing a donor substrate. Each block 16 is then individually glued onto the support 10. According to one embodiment, the maximum lateral dimension of each block 16 is between 1 mm and 10 mm.
[0026] According to one embodiment, the first semiconductor material is an IILV compound or an ILVI compound. Examples of Group III elements include gallium (Ga), indium (In), or aluminum (Al). Examples of Group V elements include nitrogen (N), phosphorus (P), or arsenic (As). Examples of IILV compounds are AsGa, GaN, AIN, InP, InN, InGaN, AlGaN, InGaAs, or AlInGaN. Generally, the elements in the IILV compound may be combined with different mole fractions. Examples of Group II elements include Group IIA elements, including beryllium (Be) and magnesium (Mg), and Group IIB elements, including zinc (Zn) and cadmium (Cd). Examples of Group VI elements include Group VIA elements, including oxygen (O) and tellurium (Te). Examples of ILVI compounds are ZnO, ZnMgO, CdZnO or CdZnMgO.Generally, the elements in the ILVI compound may be combined with different mole fractions. The first material may comprise a dopant. For example, for IILV compounds, the dopant may be selected from the group comprising a Group II P-type dopant, e.g., magnesium (Mg), zinc (Zn), cadmium (Cd) or mercury (Hg), a Group IV P-type dopant, e.g., carbon (C) or a Group IV N-type dopant, e.g., silicon (Si), germanium (Ge), selenium (Se), sulfur (S), terbium (Tb) or tin (Sn).
[0027] [Fig.2] represents the structure obtained after the formation of a weakening plane P in each block 16. The weakening plane P delimits a semiconductor layer 18 in each block 16 between the free face 14 of the block 16 and the weakening plane P.
[0028] According to one embodiment, the depth of the weakening plane P in each block 16 from the free face 14 of the block 16 is between 200 nm and 3 pm. The formation of the embrittlement plane P may comprise an implantation of hydrogen in each block 16 at the level of the embrittlement plane P.
[0029] [Fig. 3] represents a support 20 covered with an insulating layer 22. According to one embodiment, the support 20 corresponds to a silicon wafer used conventionally in microelectronics. For example, the maximum lateral dimension of the support 20 is between 200 mm and 300 mm and the thickness of the support 20 is between 600 μm and 800 μm. As a variant, the insulating layer 22 may not be present.
[0030] [Fig.4] represents the structure obtained after the realization of a mo collage lecular between the blocks 16 and the insulating layer 22. For this purpose, the structure shown in [Fig.2] is applied against the structure shown in [Fig.3] so that the free face 14 of each block 16 is brought into contact with the insulating layer 22.
[0031] [Fig. 5] represents the structure obtained after the separation, for each block 16, of the semiconductor layer 18 from the rest of the block 16 by breaking the block 16 at the weakening plane P. Monocrystalline semiconductor layers 18 of the first material are thus obtained which rest on the support 20 in physical contact with the insulating layer 22 at a distance from each other. The number of adjacent semiconductor layers 18 depends in particular on the dimensions of the support 20. The maximum lateral dimension of each semiconductor layer 18 corresponds to the lateral dimension of the block 16 described previously, and is for example between 1 mm and 10 mm. According to one embodiment, the number of semiconductor layers 18 on the support 20 is between 1 and 4. According to one embodiment, the thickness of each semiconductor layer 18 is between 10 nm and 4 pm.
[0032] The method may comprise a treatment of the semiconductor layers 18 present on the support 20 to promote subsequent epitaxial growth steps on the semiconductor layers 18. The treatment may comprise trimming the periphery of the semiconductor layers 18 and / or etching on the side of the upper faces of the semiconductor layers 18 to remove parts of the semiconductor layers 18 whose crystalline quality would not be sufficient for subsequent epitaxial growth steps. The treatment may comprise a chemical-mechanical planarization step, also called chemical-mechanical etching or CMP (English acronym for Chemical-Mechanical Planarization), which generally combines chemical and mechanical etching.
[0033] [Fig. 6] represents the structure obtained after the growth by epitaxy of a monocrystalline sacrificial layer 24 in a second material on each semiconductor layer 18, and after the formation, on each sacrificial layer 24, of a stack 26 of monocrystalline semiconductor layers in IILV or ILVI compounds, in which at least one optoelectronic component, preferably a plurality of optoelectronic components, are subsequently formed.
[0034] According to one embodiment, the optoelectronic components that are subsequently formed in each stack 26 correspond to photodiodes. According to another embodiment, the optoelectronic components that are subsequently formed in each stack 26 correspond to light-emitting diodes. For example, each stack 26 comprises first and second semiconductor layers 28 and 30, and an active layer 32 interposed between the two semiconductor layers 28 and 30. The first semiconductor layer 28 is located on the side of the sacrificial layer 24, in physical contact with the sacrificial layer 24, and the second semiconductor layer 30 comprises a free face 34. The semiconductor layers 28 and 30 are layers of a third semiconductor material, which may be identical to the first material.
[0035] According to one embodiment, the total thickness of each stack 26 is between 50 nm and 3 pm.
[0036] The active layer 32 is the region from which the majority of the electromagnetic radiation received by the optoelectronic components formed in the stack 26 is captured or the majority of the electromagnetic radiation provided by the optoelectronic components formed in the stack 26 is emitted. According to one embodiment, the active layer 32 may comprise confinement means, such as a single quantum well or multiple quantum wells. According to one embodiment, the active layer 32 forms a single quantum well. The active layer 32 is then composed of a monocrystalline monolayer of a fourth semiconductor material, for example an alloy of the compound IILV or ILVI and of a third element, in particular InGaAs, the band gap of which is different from the first doped semiconductor material.A multiple quantum well structure comprises a stack of semiconductor layers forming alternating quantum wells and barrier layers.
[0037] The third semiconductor material composing the semiconductor layers 28 and 30 is an IILV compound or an ILVI compound as defined previously for the first material. Preferably, the third material is identical to the first material. According to one embodiment, the thickness of the semiconductor layer 28 is between 50 nm and 500 nm.
[0038] According to one embodiment, the second material composing the sacrificial layer 24 is a ternary compound or a quaternary compound. The second material is different from the first material, the third material, and the fourth material. The second material is chosen so as to have a lattice parameter, also called lattice constant, close to the lattice parameter of the first material for allow the epitaxial growth of a crystal of the second material from a crystal of the first material. Preferably, the lattice parameters of the first and second materials are equal to within 0.1%. The second material is chosen so as to have a lattice parameter close to the lattice parameter of the third material to allow the epitaxial growth of a crystal of the third material from a crystal of the second material. Preferably, the lattice parameters of the third and second materials are equal to within 0.1%.
[0039] The second semiconductor material is a material capable of being etched selectively relative to the first material, the third material, and the fourth material. The etching of the second material is said to be selective relative to the first material, third, and fourth materials when, under the same etching conditions, the etching speed, also called etching rate, for example expressed in nm / min, of the second material is greater by at least a factor of 200 than the etching speeds of the first, third, and fourth materials. Preferably, the second semiconductor material is a material capable of being etched by humic chemical etching selectively relative to the first, third, and fourth materials. According to one embodiment, the thickness of the sacrificial layer 24 is between 200 nm and 800 nm.
[0040] [Fig. 7] represents a plate 40 comprising several non-separated copies of an electronic circuit and covered with a bonding layer 42. The number of copies of the electronic circuit of the plate 40 corresponds to the number of stacks 26 intended to be fixed to the plate 40. The plate 40 can in particular be produced according to conventional technologies for manufacturing a plate of integrated circuits with MOS transistors. The plate 40 can comprise a semiconductor substrate 44 covered with an interconnection structure 46. The interconnection structure 46 makes it possible in particular to connect electronic components of the plate 40, for example MOS transistors, to each other and to conductive pads on the surface of the interconnection structure 46. The interconnection structure 46 comprises a stack of insulating layers in which conductive elements are arranged, for example conductive tracks and conductive vias (not shown in [Fig.7]), located between and through the insulating layers of the stack. The bonding layer 42 may be a layer of silicon oxide (SiO2).
[0041] [Fig. 8] represents the structure obtained after the separation of the stacks 26 of the semiconductor layers 18 for their transfer onto the plate 40. The separation of each stack 26 from the underlying semiconductor layer 18 is obtained by eliminating the sacrificial layer 24 interposed between the stack 26 and the semiconductor layer 18. According to one embodiment, the elimination of the sacrificial layer 24 is carried out by selective etching of the sacrificial layer 24, by example wet chemical etching. The separate stacks 26 of the semiconductor layers 18 can be moved by means of a handle, not shown in [Fig.8].
[0042] [Fig.9] represents the structure obtained after fixing the stacks 26 to the plate 40. Stacks 26 are thus obtained which rest on the plate 40 in physical contact with the bonding layer 42 at a distance from each other. According to one embodiment, the fixing of the stacks 26 to the bonding layer 42 may comprise a step of collective transfer by picking and transferring (Micro transfer printing in English).
[0043] The manufacturing method may comprise subsequent steps for producing several copies of the optoelectronic devices, each optoelectronic device comprising a stack 26 and the underlying electronic circuit of the plate 40 and the separation of the optoelectronic devices from each other. The manufacturing method may in particular comprise a step of forming optoelectronic components in the stacks comprising in particular the formation of the doping zones, the etching zones and the zones containing the metal electrodes of the optoelectronic components.
[0044] [Fig. 10] is a partial and schematic sectional view of the structure obtained after the separation of each stack 26 from the support 20 illustrated in [Fig. 8]. [Fig. 10] is identical to [Fig. 5]. Therefore, the structure shown in [Fig. 10] can be used for the production of new optoelectronic devices, in particular by implementing the steps described previously in relation to Figures 6 to 9. According to one embodiment, the same structure shown in [Fig. 10] can be used at least ten times, preferably at least fifty times, more preferably at least one hundred times, for the implementation of the method described in relation to steps 6 to 9.
[0045] [Fig. 11] represents a phase diagram illustrating a method for selecting the second material composing the sacrificial layer 24. The phase diagram illustrates, for different semiconductor materials, the bandgap B of the material as a function of the lattice constant L of the material expressed in nanometers (nm). The bandgap B is expressed in electron volts (eV) on the left-hand ordinate axis and in micrometers (pm) on the right-hand ordinate axis.
[0046] In [Fig. 11], each square corresponds to an element or a binary compound whose chemical formula is indicated next to the square. Some squares corresponding to two binary compounds having an element in common are connected by a curve which then corresponds to a ternary compound comprising the three elements of the two binary compounds. For example, the curve, which connects the square corresponding to the binary compound GaAs and the square corresponding to the binary compound InAs, corresponds to the ternary compound InxGaixAs, where x is a real number varying from 0 to 1 depending on the point considered on the curve.
[0047] According to one embodiment, when the first material composing the semiconductor layer 18 and the third material composing the semiconductor layers 28 and 30 is InP and the fourth material composing the active layer 32 is InGaAs, in order to be able to grow the sacrificial layer 24 by epitaxy on the InP layer 18, as described previously in relation to [Fig. 6], it is necessary for the lattice parameter L of the second material to be close to the lattice parameter L of the binary InP compound.
[0048] In [Fig. 11], this means that the second material that by drawing a straight line D parallel to the ordinate axis and passing through the corresponding square binary compound InP, the coefficient x of the ternary compound InxGaixAs of layer 32 is close to that of the ternary compound located at the intersection of the straight line D and the curve which connects the square corresponding to the binary compound GaAs and the square corresponding to the binary compound InAs.
[0049] A method for selecting the material composing the sacrificial layer 24 comprises searching for a ternary or quaternary compound on the line D parallel to the ordinate axis and passing through the square corresponding to the first material, in the present example InP. The second material must also be able to be etched selectively with respect to the first material (binary compound InP), the third material (binary compound InP), and the fourth material (ternary compound InGaAs). In the present example, it may be a ternary compound InAlAs, InAlP, AlGaS, AlAsSb, ZnSeCd, ZnSeTe, or GaAsSb, or even quaternary InAlGaAs. Indeed, for such compounds, etching based on hydrated iron (III) chloride (FcCUtLO) is selective with respect to the binary compound InP and the ternary compound InGaAs.
[0050] The embodiment of the manufacturing method described previously in relation to FIGS. 1 to 10 can be implemented for the manufacturing of optoelectronic devices corresponding in particular to infrared image sensors or visible light and infrared image sensors.
[0051] [Fig. 12] is a partial and schematic sectional view of an embodiment of an optoelectronic device 50 comprising a stack of a first electronic circuit 52, a second electronic circuit 54, and a third electronic circuit 56. The second electronic circuit 54 is interposed between the first electronic circuit 52 and the third electronic circuit 56. The first electronic circuit 52 comprises optoelectronic components, for example photodiodes, based on silicon. The second electronic circuit 54 comprises optoelectronic components, for example photodiodes made of IILV or ILVI compounds. The third electronic circuit 56 comprises electronic components, in particular MOS transistors, for controlling III-V or II-VI compound optoelectronic components and silicon-based optoelectronic components. According to one embodiment, the second electronic circuit 54 is fixed to the third electronic circuit 56 by hybrid molecular bonding.
[0052] According to one embodiment, the manufacturing of the stack comprising the first electronic circuit 52 and the second electronic circuit 54 can implement the embodiment of the manufacturing method described previously in relation to FIGS. 1 to 10. The first electronic circuit 52 corresponds to the electronic circuit 40 described previously and the second electronic circuit 54 comprises one of the stacks 26 described previously.
[0053] Various embodiments and variations have been described. Those skilled in the art will understand that certain features of these various embodiments and variations could be combined, and other variations will occur to those skilled in the art.
[0054] Finally, the practical implementation of the embodiments and variants described is within the reach of those skilled in the art from the functional indications given above.
Claims
Claims
1. A method of manufacturing optoelectronic devices comprising epitaxial growth, on each first layer (18) of first layers of a first semiconductor material covering a first support (20) and spaced from each other, of a second layer (24) made of a second material, and epitaxial growth, on each second layer, of a stack (26) of semiconductor layers comprising a third layer (28) in physical contact with the second layer, separating each stack from the first layer by etching the second layer by selective etching with respect to both the first and third materials, and transferring the stacks onto a second support (40), each of the first and third materials being a III-V or II-VI compound.
2. Method according to claim 1, comprising, after the step of separating each stack (26) from the first layer (18), reusing the first support (20) covered with the first layers for the epitaxial growth, on each first layer, of a new second layer (24) of the second semiconductor material, and the epitaxial growth on each new second layer, of a new stack (26) of semiconductor layers.
3. The method of claim 1 or 2, wherein the second material is a ternary or quaternary compound.
4. A method according to any one of claims 1 to 3, wherein the etching used in the step of separating each stack (26) by etching the second layer (24) is a wet etching selective with respect to the first and third materials.
5. A method according to any one of claims 1 to 4, wherein the mesh parameters of the first, second, and third materials are equal to within 0.1%.
6. A method according to any one of claims 1 to 5, wherein each stack (26) further comprises at least a fourth layer (32) of a fourth material, and wherein the etching used in the step of separating each stack (26) by etching the second layer (24) is selective with respect to both the first, third and fourth materials.
7. A method according to any one of claims 1 to 6, wherein the second support (40) comprises a plate comprising several
8. copies of an electronic circuit, each electronic circuit being covered with a stack (26) among the stacks after the step of transferring the stacks onto the second support. The method of claim 7, further comprising cutting the plate (40) to separate the electronic circuits each covered by a stack (26) from among the stacks.