BONDING PROCESS
The bonding process addresses the complexity and cost issues of hybrid bonding by arranging metal pads to form metal/dielectric interfaces, enabling easy access to electrical contacts and reducing the need for TSVs and RDLs, thus simplifying the manufacturing process.
Patent Information
- Application Number
- FR2023002624
- Authority / Receiving Office
- FR · FR
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-21
- Publication Date
- 2024-09-27
AI Technical Summary
Conventional hybrid bonding processes for creating integrated circuits require the use of through-Silicon vias (TSVs), which increase manufacturing costs and process steps due to inaccessible electrical contacts.
A bonding process where metal pads of two substrates are arranged to form zones with metal/dielectric interfaces, allowing easy access to electrical contacts by selectively removing one substrate after hybrid bonding, eliminating the need for TSVs and RDLs.
Facilitates easy access to electrical contacts while reducing manufacturing complexity and costs by simplifying the removal of one substrate, maintaining strong bonding forces in other zones.
Smart Images

Figure 00000014_0000 
Figure 00000014_0001 
Figure 00000014_0002
Abstract
Description
Title of the invention: BONDING METHOD Technical field
[0001] The present invention relates to the general field of bonding methods, and in particular to hybrid bonding methods.
[0002] The invention relates to a bonding method.
[0003] The invention also relates to a structure obtained by a bonding process.
[0004] The invention finds applications in numerous industrial fields, and in particular for the manufacture of micro- and nano-electronic components.
[0005] The invention is particularly interesting since it makes it possible to facilitate contact resumptions on assemblies obtained with a hybrid bonding process. STATE OF THE PRIOR ART
[0006] Currently, to create stacked and vertically connected integrated circuits, hybrid bonding is implemented.
[0007] As shown in Figures 1A and 1B, this type of bonding consists of bonding two substrates 10, 20 and more particularly two surfaces 11, 21 to each other, comprising metal pads 13 and an insulating material 12. Under each surface, the metal pads 13 are connected to the transistors. By assembling the substrates 10, 20, the metal areas come into contact and the transistors are connected on either side of the interface.
[0008] This type of bonding is particularly interesting because it makes it possible to achieve an interconnection pitch of the order of a micrometer and high interconnection densities.
[0009] However, it requires the use of vias 30 passing through the silicon (or TSV for “through-Silicon via”) because the electrical contacts are inaccessible after bonding (figures 1A and 1B).
[0010] However, the manufacture of TSVs requires numerous steps, which considerably increases the manufacturing costs and the number of process steps (implementation of the TSVs, treatment of the rear face, revelation of the TSVs, redistribution layer on the rear face (RDL for "redistribution layer"). Statement of the invention
[0011] An aim of the present invention is to propose a bonding method which overcomes the drawbacks of the prior art and makes it possible, in particular, to make the electrical contacts easily accessible.
[0012] For this, the present invention proposes a bonding method comprising the following steps:
[0013] - providing a first substrate comprising a first face and a second face, the first face of the first substrate comprising a first dielectric material and metal pads,
[0014] - providing a second substrate comprising a first face and a second face, the first face of the second substrate comprising a second dielectric material, metal pads, and a metal part,
[0015] - preferably, carrying out a treatment of the first face of the first substrate and of the second face of the second substrate (e.g., a polishing and / or plasma activation treatment),
[0016] - bringing the first face of the first substrate into contact with the first face of the second substrate,
[0017] - carry out a heat treatment to assemble the first substrate to the second substrate.
[0018] The metal pads of the first substrate, the metal pads of the second substrate and the metal part of the second substrate are arranged in such a way that, when the first face of the first substrate is brought into contact with the first face of the second substrate, two zones are formed:
[0019] - in a first zone the metal pads of the first substrate are arranged in look at the metal pads of the second substrate, and
[0020] - in a second zone the metal pads of the first substrate are arranged in facing the second dielectric material and the metal portion of the second substrate is arranged facing the first dielectric material.
[0021] Advantageously, the method further comprises a subsequent removal step during which the part of the second substrate arranged at the second zone is removed.
[0022] The invention is fundamentally distinguished from the prior art by the particular positioning of the metal pads of the two plates as well as of the metal part of the second substrate. Thus, at the level of the second zone, there are only metal / dielectric interfaces. There is no metal / metal interface or dielectric / dielectric interface.
[0023] In a conventional arrangement, the metal pads would be facing other metal pads (metal / metal bonding) and the dielectric material facing the dielectric material (dielectric / dielectric bonding).
[0024] While the dielectric / dielectric and metal / metal bonding forces are very strong, the dielectric material bonds poorly to the metal. For example, the bonding force between SiO2 and Cu is very weak or even negligible, pre- and post-annealing.
[0025] As an illustration, for example, in 'full plate' format, the metal / metal bonding forces are more than 3J / m2 for Cu-Cu, after annealing at 100°C, and the bonding forces for SiO2-SiO2 are approximately 2J / m2 after annealing at 400°C. For plates complementary materials comprising a SiO2 dielectric surface and Cu pads for hybrid bonding, bonding strengths can reach up to approximately 6.5J / m2 after annealing at 400°C.
[0026] With the arrangement according to the invention, it is possible to easily release a part of the upper substrate (i.e. the second substrate) after hybrid bonding and cutting to reveal the electrical pads.
[0027] Indeed, since the first zone has high bonding energies (on the one hand, metal / metal and, on the other hand, dielectric / dielectric) and since the second zone has negligible or even zero bonding energies (metal / dielectric), the separation of the part of the second substrate at the level of the second zone is relatively simple to implement.
[0028] Thus, during the removal step, the part of the second substrate at the first zone remains bonded to the first substrate and the part of the second substrate at the second zone detaches from the first substrate.
[0029] Implementing a method that removes (and thus "wastes") a significant surface area of substrate appears at first sight to be disadvantageous. However, in this method the added value of the bonded part justifies the sacrifice of the removed part and / or the discarded part may be inexpensive (for example, it may be a passive device).
[0030] With such a process, it is not systematically necessary to manufacture TSVs or RDLs.
[0031] Advantageously, the first dielectric material is an oxide or a nitride, preferably a silicon oxide and / or the second dielectric material is an oxide or a nitride, preferably a silicon oxide.
[0032] Advantageously, the metal pads of the first substrate, the metal pads of the second substrate and / or the metal part of the second substrate are made of copper.
[0033] Advantageously, the removal step is carried out according to the following sub-steps:
[0034] i) cutting the second substrate, for example with a saw, with a laser or by chemical etching, the cutting being carried out so as to be able to release the part of the second substrate arranged at the level of the second zone,
[0035] ii) removing the part of the second substrate disposed at the second zone.
[0036] Advantageously, sub-step ii) is carried out by gluing an adhesive element onto the second substrate.
[0037] According to a first advantageous variant, sub-step ii) is carried out by gluing an adhesive element onto the part of the second substrate arranged at the level of the second zone.
[0038] According to another advantageous variant, sub-step ii) is carried out by gluing an adhesive element onto the entire second substrate. The 'unglued' part (i.e. part of the second substrate arranged at the level of the second zone) will be removed with the adhesive element.
[0039] Advantageously, after the heat treatment, the method comprises a step during which the second substrate is thinned from the second face. This step is advantageously carried out before the removal step and / or before the cutting step.
[0040] Advantageously, the metal pads of the first substrate and / or the metal pads of the second substrate have a surface area, preferably square or rectangular, the largest dimension of the surface area being between 1 pm and 1 mm. The surface area of the metal pads is, for example, between 3 pm2 and 1 mm2.
[0041] The invention also relates to a device comprising a first substrate assembled with a second substrate:
[0042] - the first substrate comprising a first face and a second face, the first face of the first substrate comprising a first dielectric material and metal pads, preferably made of copper,
[0043] - the second substrate comprising a first face and a second face, the first face of the second substrate comprising a second dielectric material and metal pads, preferably copper, and a metal part, preferably copper,
[0044] the first face of the first substrate being arranged opposite the second face of the second substrate.
[0045] In a first zone, the metal pads of the first substrate are arranged opposite the metal pads of the second substrate. In a second zone, the metal pads of the first substrate are arranged opposite the second dielectric material and the metal part of the second substrate is arranged opposite the first dielectric material.
[0046] Advantageously, the first dielectric material is an oxide or a nitride, preferably a silicon oxide and / or the second dielectric material is an oxide or a nitride, preferably a silicon oxide.
[0047] Other characteristics and advantages of the invention will emerge from the additional description which follows.
[0048] It goes without saying that this additional description is given only as an illustration of the subject of the invention and must in no case be interpreted as a limitation of this subject. Brief description of the drawings
[0049] The present invention will be better understood on reading the description of exemplary embodiments given purely for informational purposes and in no way limiting, with reference to the appended drawings in which:
[0050] [Fig.lA]
[0051] [Fig.lB] previously described, schematically represent different stages of a bonding process according to the prior art.
[0052] [Fig.2A]
[0053] [Fig.2B]
[0054] [Fig.2C]
[0055] [Fig.2D]
[0056] [Fig.2E] schematically represent different stages of a bonding process according to a particular embodiment of the invention.
[0057] [Fig.3] schematically represents, in three dimensions, a step of a bonding process according to another particular embodiment of the invention.
[0058] The different parts represented in the figures are not necessarily on a uniform scale, in order to make the figures more readable.
[0059] The different possibilities (variants and embodiments) must be understood as not being mutually exclusive and being able to be combined with each other.
[0060] Furthermore, in the following description, terms that depend on the orientation, such as "above", "below", etc. of a structure apply with the assumption that the structure is oriented as illustrated in the figures.
[0061] DETAILED DESCRIPTION OF PARTICULAR EMBODIMENTS
[0062] Although this is in no way limiting, the invention particularly finds applications in the field of microelectronics.
[0063] The bonding method comprises the following steps (Figures 2A to 2E and [Fig.3]):
[0064] a) providing a first substrate 100 comprising a first face 101 and a second face 102, the first face 101 of the first substrate 100 comprising a first dielectric material 110 and metal pads 120,
[0065] b) providing a second substrate 200 comprising a first face 201 and a second face 202, the first face 201 of the second substrate 200 comprising a second dielectric material 210, metal pads 220 and a metal part 230,
[0066] b') preferably, carry out a treatment of the two faces intended to be put in contact (for example by polishing and / or plasma activation) to make them directly bondable to each other ('bondable'), by Van der Waals forces,
[0067] c) bringing the first face 101 of the first substrate 100 into contact with the first face 201 of the second substrate 200; bringing the two substrates into contact leading to the formation of two zones:
[0068] - in a first zone Zl, the metal pads 120 of the first substrate 100 are arranged opposite the metal pads 220 of the second substrate 200,
[0069] - in a second zone Z2, the metal pads 120 of the first substrate 100 are arranged opposite the second dielectric material 210 and the metal part 230 of the second substrate 200 is arranged opposite the first dielectric material 110,
[0070] d) carrying out a heat treatment to assemble the first substrate 100 to the second substrate 200; the heat treatment making it possible to increase the adhesion forces between the surfaces and to reduce the resistivity between the metal pads by recrystallization,
[0071] e) preferably, removing a portion of the second substrate 200 to release at least a portion of the metal pads 120 of the first substrate 100.
[0072] The substrates 100, 200 provided in step a) and in step b) each comprise two main faces: a first face 101, 201 and a second face 102, 202. These faces are parallel or substantially parallel to each other.
[0073] The substrates 100, 200 are, for example, wafers.
[0074] The first face 101, 201 of each substrate 100, 200 is advantageously flat to increase the direct dielectric / dielectric and metal / metal bonds (Van der Waals forces).
[0075] The first face 101, 201 of each substrate 100, 200 comprises a dielectric material 110, 210 and metal pads 120, 220.
[0076] The metal pads 120, 220 may cover the dielectric material 110, 210. The metal pads 120, 220 may penetrate the dielectric material 110, 210. The metal pads 120, 220 may pass through the thickness of the dielectric material 110, 210.
[0077] The metal pads 120, 220 of the same substrate 100, 200 are electrically insulated from each other by the dielectric material 110, 210.
[0078] The metal studs 120, 220 can be regularly spaced.
[0079] The surface of the pads 120, 220 may be of any shape. It is preferably square or rectangular. The largest dimension of the surface of the pads 120, 220 is, for example, between 1 μm and 3 mm, preferably between 1 μm and 1 mm.
[0080] For example, for a square the largest dimension is the side. For a rectangle, the largest dimension is the length.
[0081] At the level of the first zone, the metal pads 120 of the first substrate 100 and the metal pads 220 of the second substrate 200 are identical and arranged in the same way on the substrates, so that, during assembly, they are opposite each other.
[0082] Concerning the first substrate 200, the pads of the first zone Z1 may be identical or different from the pads of the second zone Z2.
[0083] When the plots are different:
[0084] - the largest dimension of the surface of the pads 120 of the first zone ZI is, preferably, between 1 pm and 15 pm, even more preferably between 3 and 10 pm; these pads are so-called intersection pads between the chips,
[0085] - the largest dimension of the surface of the pads 120 of the second zone Z2 is, preferably between 20 pm and 3 mm, preferably between 50 pm and 1 mm; these pads are used to electrically connect the device to an element external to the device.
[0086] Preferably, the pads of the first zone ZI are identical to the pads of the second zone Z2. For example, the largest dimension of the surface of the pads 120 of the first zone ZI and the largest dimension of the surface of the pads of the second zone Z2 are between 1 μm and 3 mm, preferably between 1 μm and 1 mm, even more preferably between 1 μm and 15 μm, and even more preferably between 3 and 10 μm.
[0087] The metal pads 120 of the first substrate 100 and the metal pads 220 of the second substrate 200 may be made of the same material or different materials. The metal pads 120, 220 are, for example, made of W, Al, Ti, Ta, Ge, Ga or one of their alloys. Preferably, the metal pads 120, 220 are made of copper.
[0088] At the level of the second zone Z2, the second substrate 200 further comprises a metal part 230. The metal part 230 has a shape complementary to the metal pads 120 of the first substrate 100 arranged at the level of the second zone Z2. For example, it is a metal layer comprising openings having the shape of the pads 120 of the first substrate of the second zone Z2, and positioned such that, when the substrates 100, 200 are brought into contact, the openings are opposite these pads ([Fig. 3]).
[0089] The metal part 230 is, for example, made of W, Al, Ti, Ta, Ge, Ga or one of their alloys. Preferably, it is made of copper.
[0090] The first dielectric material 110 and the second dielectric material 210 may be the same or different.
[0091] Preferably, the first dielectric material 110 and the second dielectric material 210 are oxides. Preferably, it is silicon oxide. It could also be germanium dioxide or an oxide of SiGe, or even Ta2O5, Al2O3, ZrO2 or HfO2.
[0092] According to another preferred embodiment, the first dielectric material 110 and the second dielectric material 210 are nitrides. For example, it may be a SiNx nitride.
[0093] The dielectric material 110, 210 of each substrate 100, 200 is covered locally by metal pads 120, 220.
[0094] Between step b) and step c), a polishing step is advantageously carried out to obtain a first substrate 100 and / or a second substrate 200 having flat surfaces. For example, this step can be carried out by chemical mechanical polishing (or CMP for “Chemical Mechanical Polishing”).
[0095] The metal pads 120 of the first substrate 100, the metal pads 220 of the second substrate 200 and the metal part 230 of the second substrate are arranged in such a way that, during step c), two zones are formed.
[0096] In a first zone (denoted ZI in the figures), the metal pads 120 of the first substrate 100 are arranged opposite the metal pads 220 of the second substrate 200. The first dielectric material 110 is therefore arranged opposite the second dielectric material 120. In the zone Z1, there are two types of metal / metal bonding, on the one hand, and, on the other hand, dielectric / dielectric.
[0097] In a second zone (denoted Z2 in the figures), the metal pads 120 of the first substrate 100 are arranged opposite the second dielectric material 210 and the metal part 230 of the second substrate 200 is arranged opposite the first dielectric material 110. In zone Z2, there is only one type of bonding: metal / dielectric bonding.
[0098] At this second zone Z2, an overlap tolerance between the first dielectric material 110 and the metal part 230 of the second substrate 200 and / or between the second dielectric material 210 and the pads 120 of the first substrate 100 can be accepted. The tolerance is preferably less than 5%, even more preferably less than 2%, even more preferably less than 1%. By less than 5%, it is meant that less than 5% of the surface of each metal pad is covered by a dielectric material. For example, the offset can be between 2 and 20 nm. In other words, the first dielectric material 110 and the metal part 230 of the second substrate 200 and / or the second dielectric material 210 and the pads 120 of the first substrate 100 can overlap over an overlap length of between 2 nm and 20 nm.
[0099] The first zone Z1 and the second zone Z2 may each represent approximately 50% of the surface area of the substrates. The proportion of each zone may be adapted according to the desired final device. For example, Z1 may represent 80% of the surface area of the substrates and Z2 20% of the surface area of the substrates.
[0100] During step d), the heat treatment is, for example, carried out at a temperature between 200°C and 400°C. This step increases the adhesion energies at the level of the first zone ZL
[0101] Even after step d), the adhesion energies at the level of the second zone Z2 remain low or even negligible.
[0102] The difference in adhesion energy between the first zone Z1 and the second Z2 is greater after annealing than before annealing.
[0103] At the end of step d), the part of the substrates 100, 200 at the level of the second zone Z2 (so-called non-bonded zone) is mechanically held by the part of the substrates 100, 200 at the level of the first zone Z1 (so-called bonded zone).
[0104] Advantageously, after step d), the method further comprises a step e) during which the part of the second substrate 200 arranged at the level of the second zone Z2 is removed.
[0105] The removal step is carried out according to the following sub-steps:
[0106] i) cutting the second substrate 200, for example, with a saw, with a laser or by chemical etching, the cutting being carried out in such a way as to be able to release the part of the second substrate 200 at the level of the second zone Z2,
[0107] ii) removing the part of the second substrate 200 at the level of the second zone Z2.
[0108] During step i), a division is carried out at the border of the first zone ZI and the second zone Z2 to separate the second substrate 200 into two parts.
[0109] Step i) may be carried out by a conventional sawing technique. A saw 300 is, for example, shown in [Fig.2C]. Step i) may be carried out by other techniques, for example by a laser etching step and / or by chemical etching. Sub-step ii) advantageously leads to the formation of a trench going from the first face 201 to the second face 202 of the second substrate 200.
[0110] Sub-step ii) can be carried out by gluing an adhesive element onto the part of the second substrate 200 positioned at the level of the second zone Z2.
[0111] Alternatively, sub-step ii) can be carried out by gluing an adhesive element onto the entire second substrate 200. When the adhesive element is removed, the unglued areas will leave with the adhesive element, the glued areas will not move.
[0112] It could also be possible to remove the unbonded portion of the second substrate 200 by hydraulic means (water and / or air blasting), by chemical removal (acids), by thermal expansion (including local thermal expansion applied by laser), by thermal contraction (cold treatment), or by a combination of these possibilities.
[0113] Between step d) and step e), the method may comprise a step during which the second substrate 200 is thinned from the second face 202.
[0114] Thinning can be achieved by conventional grinding, chemical etching, reactive ions, or a combination of these techniques.
[0115] Thus, at the end of step d), a device is obtained comprising a first substrate 100 assembled with a second substrate 200:
[0116] - the first substrate 100 comprising a first face 101 and a second face 102, the first face 101 of the first substrate 100 comprising a first dielectric material 110 and metal pads 120, preferably made of copper,
[0117] - the second substrate 200 comprising a first face 201 and a second face 202, the first face 201 of the second substrate 200 comprising a second dielectric material 210, metal pads 220, preferably made of copper, and a metal part 230, preferably made of copper.
[0118] The first face 101 of the first substrate 100 is arranged opposite the first face 201 of the second substrate 200.
[0119] In a first zone Zl, the metal pads 120 of the first substrate 100 are arranged opposite the metal pads 220 of the second substrate 200.
[0120] In a second zone Z2, the metal pads 120 of the first substrate 100 are arranged opposite the second dielectric material 210 and the metal part 230 of the second substrate 200 is arranged opposite the first dielectric material 110.
[0121] At the end of step e), a device is obtained comprising the first substrate 100 (called the base substrate) covered locally by the second substrate 200 at the level of the first zone Z1. At the level of the second zone Z2, the metal pads 120 of the first substrate 100 are exposed and therefore accessible to make a contact recovery.
[0122] The method may further comprise one or more of the following steps: cleaning the pads (if necessary), cutting and packaging.
Claims
Claims
1. A bonding method comprising the following steps: - providing a first substrate (100) comprising a first face (101) and a second face (102), the first face (101) of the first substrate (100) comprising a first dielectric material (110) and metal pads (120), - providing a second substrate (200) comprising a first face (201) and a second face (202), the first face (201) of the second substrate (200) comprising a second dielectric material (210), metal pads (220) and a metal part (230), - bringing the first face (101) of the first substrate (100) into contact with the first face (201) of the second substrate (200), - carrying out a heat treatment to assemble the first substrate (100) to the second substrate (200), characterized in that the metal pads (120) of the first substrate (100), the metal pads (220) and the metal part (230) of the second substrate (200) are arranged such that,when the first face (101) of the first substrate (100) is brought into contact with the first face (201) of the second substrate (200), in a first zone (Zl) the metal pads (120) of the first substrate (100) are arranged opposite the metal pads (220) of the second substrate (200) and in a second zone (Z2) the metal pads (120) of the first substrate (100) are arranged opposite the second dielectric material (210) and the metal part (230) of the second substrate (200) is arranged opposite the first dielectric material (110).,
2. Method according to claim 1, characterized in that the first dielectric material (110) is an oxide or a nitride, preferably a silicon oxide and / or in that the second dielectric material (120) is an oxide or a nitride, preferably a silicon oxide.
3. Method according to any one of the preceding claims, characterized in that the metal pads (120) of the first substrate (100), the metal pads (220) and / or the metal part (230) of the second substrate (200) are made of copper.
4. Method according to one of claims 1 to 3, characterized in that the method further comprises a subsequent removal step during which the part of the second substrate (200), arranged at the level of the second zone (Z2), is removed.
5. Method according to the preceding claim, characterized in that the removal step is carried out according to the following sub-steps: i) cutting the second substrate (200) for example with a saw, with a laser or by chemical etching, the cutting being carried out in such a way as to be able to release the part of the second substrate (200) arranged at the level of the second zone (Z2), ii) removing the part of the second substrate (200) at the level of the second zone (Z2).
6. Method according to claim 5, characterized in that sub-step ii) is carried out by gluing an adhesive element onto the second substrate (200).
7. Method according to any one of the preceding claims, characterized in that, after the heat treatment, the method comprises a step during which the second substrate (200) is thinned from the second face (202).
8. Method according to any one of the preceding claims, characterized in that the metal pads (120) of the first substrate (100) and / or the metal pads (220) of the second substrate (200) have a surface, preferably square or rectangular, the largest dimension of the surface being between 1 μm and 1 mm.
9. Device comprising a first substrate (100) assembled with a second substrate (200): - the first substrate (100) comprising a first face (101) and a second face (102), the first face (101) of the first substrate (100) comprising a first dielectric material (110) and metal pads (120), preferably made of copper, - the second substrate (200) comprising a first face (201) and a second face (202), the first face (201) of the second substrate (200) comprising a second dielectric material (210), metal pads (220), preferably made of copper, and a metal part (230), preferably made of copper, The first face (101) of the first substrate (100) being arranged opposite the first face (201) of the second substrate (200), Characterized in that, in a first zone (Zl), the metal pads (120) of the first substrate (100) are arranged opposite the metal pads (220) of the second substrate (200) and,in a second zone (Z2), the metal pads (120) of the first substrate (100) are arranged opposite the second dielectric material (210) and the metal part (230) of the second substrate (200) is arranged in, regard to the first dielectric material (110).
10. Device according to the preceding claim, characterized in that the first dielectric material (110) is an oxide or a nitride, preferably a silicon oxide and / or in that the second dielectric material (210) is an oxide or a nitride, preferably a silicon oxide.
Citation Information
Patent Citations
Semiconductor Interconnect Structure and Method
US20200006266A1
Selective alteration of interconnect pads for direct bonding
US20210242152A1
Bonded structure with interconnect structure
US20220077063A1
Semiconductor device and electronic system including the same
US20220139855A1