Water-soluble composition with adhesive properties

A water-soluble composition with polyvinyl alcohol and CaCl2 maintains stickiness for long-term storage, addressing inefficiencies in existing methods by ensuring reliable particle collection and retention.

FR3148029A1Active Publication Date: 2024-10-25COMMISSARIAT A LENERGIE ATOMIQUE ET AUX ENERGIES ALTERNATIVES
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
FR2023004041
Authority / Receiving Office
FR · FR
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-21
Publication Date
2024-10-25
Estimated Expiration
2043-04-21

AI Technical Summary

Technical Problem

Existing particle collection methods, such as cotton swabs, brushes, vacuum cleaners, and sponges, are inefficient for low-level contamination and require cumbersome preparation or risk particle loss due to adhesion or spread, while existing water-soluble materials lose stickiness over time, making them unsuitable for long-term storage.

Method used

A water-soluble composition comprising polyvinyl alcohol or polyvinylpyrrolidone with CaCl2 or MgCl2 and optional glycerol maintains stickiness, allowing immediate use and efficient particle collection without prior humidification, even after storage.

Benefits of technology

The composition ensures consistent stickiness over time, enabling effective particle collection from large areas with ease of use and retention of collected particles in solution, maintaining efficiency up to 90% after 9 weeks of storage.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

The invention relates to a water-soluble composition, characterized in that it comprises: A solution of polyvinyl alcohol (PVA) or polyvinylpyrrolidone (PVP); 10 to 50% by mass of a compound selected from: A salt selected from CaCl2 and MgCl2; Silica beads; Figure to be published with the abbreviation: Figure 1 A
Need to check novelty before this filing date? Find Prior Art

Description

Title of the invention: Water-soluble composition with adhesive power Technical field of the invention

[0001] The present invention relates to a water-soluble composition, which can in particular be used for collecting particles. State of the art

[0002] The collection of particles present on a surface is useful for various applications, in particular for: - Check the effectiveness of decontamination after pollution, - Carry out analyses on the collected particles, - Check the contamination of containers and work surfaces used in the food industry...

[0003] In all these applications, it is useful to have a device that allows simple and rapid sampling of particles. By particles, we mean all types of biological compounds, such as bacteria, DNA molecules, spores, viruses, or any other type of particles, such as beads, dust, biofilm or pollen.

[0004] Particle collection devices are already known in the state of the art. The most common solutions use "cotton buds" or brushes that are applied to the surface to collect the particles present. The collected particles are then detached from the sampling tool by immersion in a specific buffer solution. Detection kits, generally strips, are then used to determine the nature of the contamination. These solutions are effective when there is significant contamination (suspect powder, stain, etc.). On the other hand, when the contamination is low, it is necessary to carry out a larger-scale collection to increase the number of particles collected.

[0005] For the collection of particles over a large surface, there is equipment in the form of a vacuum cleaner or collector. This type of equipment includes a compressor that sends sterile water under pressure into a shower head that removes contamination from the treated surface (fabric, fibrous surface, etc.). A second area of ​​the shower head also allows the water loaded with particles to be recovered by suction. The water and particles sucked up are collected in a tank and will then be analyzed in a laboratory. This device is focused on DNA recovery but could also be used for other contamination (particles, bacteria, spores, etc.). However, this solution is particularly bulky.

[0006] Another technique used in the food industry to ensure that a portion of a production line is contaminated by bacteria consists of using sterile sponges to collect the bacteria after moistening the collection area with a buffer solution. The sponge will collect the liquid deposited with the bacteria and then the liquid will be recovered and cultured for a few hours or days to check for the presence of bacteria. However, in this solution, bacteria can stick to the surface of the material constituting the sponge (polyurethane, polypropylene, etc.) and therefore not be present in the recovered liquid. Furthermore, these sponges are not suitable for collecting particles over large areas and can even spread the contamination from a soiled area A to an unsoiled area B. Finally, the sponge often needs to be moistened prior to collection.

[0007] The patent application referenced FR2366554A1 (corresponding to US4144760) describes a sampling device using a water-soluble plastic which, after humidification, becomes sticky and allows the capture of biological particles on a surface by apposition. Once the capture is complete, the plastic film is partially or completely solubilized to collect the captured elements. This technique requires prior humidification of the plastic film to partially dissolve it and make it sticky. This step is very delicate because if the humidification is insufficient, the material is not sticky enough and if it is too great, the material dissolves and no longer performs its collection function.

[0008] Documents WO2017 / 209628A1, US2011 / 256531A1 and US4144760A1 also describe sampling devices.

[0009] Patent application EP3591372A1 describes a device for collecting particles present on a surface. The device is in the form of a foam roller impregnated with a water-soluble material, this material allowing the particles to be collected and easily put back into solution. The water-soluble material is in the form of a gel or film deposited on the surface of the roller. For example, the gel is a composition which comprises polyvinyl alcohol (PVA), water and glycerol.

[0010] After a certain storage period, this type of gel tends to lose its stickiness, which makes the device inoperative. The addition of an alcohol (such as glycerol) makes it possible to delay the drying of the film but does not allow the sticky characteristics of the film to be retained.

[0011] The aim of the invention is to propose a water-soluble composition capable of retaining its adhesive power over time, thus enabling a particle collection device using this composition to be used at all times, even after long-term storage. Statement of the invention

[0012] This goal is achieved by a water-soluble composition, which includes: A solution of polyvinyl alcohol (PVA) or Polyvinylpyrrolidone (PVP); 10 to 50% by mass of a compound chosen from: • A salt chosen from CaC12 and MgC12; • Silica beads;

[0013] According to a particular embodiment, the composition also comprises up to 50% by mass of glycerol.

[0014] Advantageously, the composition comprises: 10% to 20% of polyvinyl alcohol (PVA) or Polyvinylpyrrolidone (PVP) in an aqueous solution, to which are added 20% to 40% by mass of glycerol and 10% to 30% by mass of salt chosen from Cacl2 and MgC12.

[0015] Preferably, the composition comprises: 10% polyvinyl alcohol (PVA) or Polyvinylpyrrolidone (PVP) in water, then 30% by mass of glycerol, and 20% by mass of a Cacl2 salt.

[0016] The invention also relates to a particle collection device, comprising a support having a collection surface and a water-soluble material deposited on its collection surface, the water-soluble material having a water-soluble composition as defined above. Brief description of the figures

[0017] Other characteristics and advantages will appear in the detailed description which follows given with reference to the appended drawings in which: Figures 1A and 1B represent an exemplary embodiment of a particle collection device, for example produced in the form of a roller; [Fig.2] shows the different steps that are implemented for particle collection using the particle collection device shown in [Fig.1A]; [Fig.3] shows a diagram representing the collection efficiency as a function of the storage duration of a collection device;

[0018] Detailed description of at least one embodiment

[0019] A particle collection device 1, 10 as shown in [Fig.lA] and in [Fig.lB], comprises for example a support 2, 20 provided with a collection surface 30. In this embodiment, the support 2, 20 may be formed of a roller in the form of a cylinder of revolution having a lateral surface forming said collection surface 30. The roller may be rotatably mounted around a rod 4 forming an axis of rotation (X). The rod 4 may be connected to a gripping handle 5 of the device.

[0020] The device comprises a water-soluble material, at least partially covering its collection surface 30, advantageously the entire collection surface 30 of the support.

[0021] The water-soluble material is in the form of a gel 3 or a film. By gel is meant a material which has sufficient viscosity, in particular between 500 mPa s and 50000 mPa s.

[0022] The gel 3 is deposited on the collection surface 200 of the support 2, 20. In the case of a roll-shaped support, it is therefore deposited on the lateral surface of the roll.

[0023] The support 2 may be made entirely of a non-deformable material, for example a hard plastic, or of an elastically deformable material, such as a deformable foam, such as for example a polymer foam, for example of the polyurethane (PU), polyvinyl chloride (PVC), polyethylene (PE), or silicone type.

[0024] The principle of particle collection is illustrated by [Fig.2].

[0025] With reference to [Fig.2], the different stages of the collection process implemented at using a collection device 1 as described above, are as follows:

[0026] El: The device 1 is ready for use and does not require any preparation. The gel 3 is in fact already present on the collection surface 30 of the roller and the device is always ready for use.

[0027] E2: the roller is placed on the surface SI to be sampled (flat surface here in this example) so as to bring the gel 3 present on the roller into contact with the surface SI to be sampled. Passing the roller over the surface SI to be sampled allows the roller to rotate around its axis (X). When the roller is applied, the particles P present on the surface SI to be sampled are detached from the surface to be sampled and stick to the gel 3. Several passes may be necessary.

[0028] E3: The particles P are collected on the collection surface 30 of the device. To be recovered, the collection surface is immersed at least partially or even completely in an aqueous solution 60, for example an aqueous buffer (e.g.: saline phosphate - PBS), present in a collection tank 6. To facilitate immersion, the entire support 2 can be separated from the rest of the device.

[0029] E4: During immersion of the collection surface, the gel 3 dissolves in the aqueous solution 60, thus releasing the collected P particles into the solution. An analysis of the aqueous solution 60 will then make it possible to identify the P particles that have been collected.

[0030] According to the invention, the gel is composed of: - A solution of polyvinyl alcohol (PVA) or Polyvinylpyrrolidone (PVP) present in a proportion of between 5% and 30% in an aqueous solution; - 10 to 50% by mass of a compound chosen from: • a salt such as CaC12 or MgC12, • silica beads;

[0031]

[0032]

[0033]

[0034]

[0035]

[0036]

[0037]

[0038]

[0039]

[0040]

[0041]

[0042]

[0043]

[0044]

[0045]

[0046]

[0047] - 0 to 50% by mass of glycerol; It should be noted that the presence of glycerol is optional. The PVP solution is obtained, for example, by dissolving 13g of polypyrrolidone in 150ml of distilled water. After complete dissolution, 30% by mass of glycerol is added, for example, followed by 20% by mass of CaCl2. Advantageously, a composition according to the invention is as follows: - 10% to 20% PVA or PVP in water, then - 20% to 40% glycerol, and - 10% to 30% by mass of MgC12 or CaC12 in the solution. A preferred composition is for example the following: - 10% PVP or PVA in the water, then - 30% glycerol, and - 20% by mass of CaCl2 in the solution. According to a particular aspect of the invention, by adding a salt such as CaCl2 or MgCl2, the drying of the gel is delayed and the sticky characteristics of the material are preserved over time. The salt chosen is advantageously that composed of CaCl2. According to a particular feature, the gel can therefore be deposited on the collection surface of the roller in order to obtain complete coverage of its surface. The coated surface of the roll is then oven-baked to dry the gel on the roll surface. The roll is then ready for use. Upon removal from the oven, the roll is wrapped in a non-stick film to protect the sticky gel. The roll can be stored at atmospheric pressure or placed in a bag and vacuum sealed. Of course, the gel could be deposited on the collection surface of a collection device with another architecture (cotton swab, brush, sponge, sphere, balls, etc.). It should be noted that the composition described above could be used for applications other than particle collection, such as as a hydrogel in ECG or EEG measurements, or as a glue that does not dry or dries very slowly. The adhesive power of the composition was tested in two trials. It was first tested for the collection of polystyrene beads of 5 pm to 10 pm diameter, distributed over an area of ​​1 m2. For the polystyrene beads, the protocol was as follows: Step 1: Deposit the beads contained in an aqueous solution on the surface to be treated. The deposition is done by distributing drops of liquid on the surface or using a spray which distributes the drops containing the balls on the surface. Step 2: Wait for the drops containing the beads to dry completely on the surface - 4 hours at room temperature.

[0048] Step 3: Rolling the surface.

[0049] Step 4: Introduction of the roller into a tank containing 10ml of aqueous solution.

[0050] Step 5: Stir (30 seconds) the tank so that the water contained in it is in contact with the surface of the roller and dissolves the sticky film.

[0051] Step 6: Recovery of a calibrated volume of solution (20pl) and deposit on a counting slide.

[0052] Step 7: Counting the number of beads recovered in the 20pl sample and comparing it with the quantity of beads initially deposited on the surface.

[0053] The collection principle is also validated on spores of Bacillus thuringiensis.

[0054] Protocol used for Bacillius Thiuringensis spores

[0055] Step 1: Preparation of the spore solution with counting of the spores in the initial solution.

[0056] Step 2: The deposit is done by distributing a defined volume (1ml) of drops of liquid on the surface or using a spray which distributes the drops containing the spores on the surface.

[0057] Step 2: Wait for the drops containing the spores to dry completely on the surface - 4 hours at room temperature.

[0058] Step 3: Rolling the surface.

[0059] Step 4: Introduction of the roller into a tank containing 10ml of aqueous solution.

[0060] Step 5: Stir (30 seconds) the tank so that the water contained in it is in contact with the surface of the roller and dissolves the sticky film.

[0061] Step 6: Deposit 100pl of solution on a suitable culture dish.

[0062] Step 7: Place in an incubator at 36°C overnight.

[0063] Counting the number of colonies on the culture dishes and comparing them with the number of spores deposited on the surface.

[0064] In both cases, in connection with [Fig. 3], no loss of collection efficiency was observed, regardless of the storage duration of the roll. This means that the roll, impregnated with the composition of the invention, retained its stickiness over time. On the spores, for example, the roll made it possible to collect 90% of the spores distributed over a surface area of ​​2m2, even after a storage period of 9 weeks.

[0065] The invention has numerous advantages, including: - The guarantee of conservation of the adhesive power of the composition over time, even after a long storage period; - Ease of manufacturing the composition; Ease of use of the composition; Get a ready-to-use tool; The possibility of recovering all the particles collected by the roller in the gel dissolution solution;

Claims

Claims

1. Water-soluble composition, characterized in that it comprises: - A solution of polyvinyl alcohol (PVA) or Polyvinylpyrrolidone (PVP); - 10 to 50% by mass of a compound chosen from: • A salt chosen from CaCl2 and MgCl2; • Silica beads;

2. Water-soluble composition according to claim 1, characterized in that it also comprises up to 50% by mass of glycerol.

3. Water-soluble composition according to claim 1 or 2, characterized in that it comprises: 10% to 20% of polyvinyl alcohol (PVA) or Polyvinylpyrrolidone (PVP) in an aqueous solution, to which are added 20% to 40% by mass of glycerol and 10% to 30% by mass of salt chosen from Cacl2 and MgC12.

4. Water-soluble composition according to claim 1 or 2, characterized in that it comprises: - 10% of polyvinyl alcohol (PVA) or Polyvinylpyrrolidone (PVP) in water, then - 30% by mass of glycerol, and - 20% by mass of a Cacl2 salt.

5. Particle collection device, comprising a support having a collection surface (30) and a water-soluble material deposited on its collection surface, characterized in that the water-soluble material has a water-soluble composition as defined in one of the preceding claims.

Citation Information

Patent Citations

  • Method and implement to take and collect sample material, especially for scientific or diagnostic examination

    FR2366554A1

  • Method and implement to take and collect sample material, especially for scientific or diagnostic examination

    US4144760A

  • Cold resistant agent for Chinese chestnut growth

    CN1163145C

  • Device for collecting particles

    EP3591372A1

  • Fishing Lure Formulations

    US20090196849A1