Method for forming an integrated circuit

The method addresses the inefficiencies of existing 2.5D integration by forming a weakening zone in a donor substrate to transfer microchips at low temperatures, optimizing system-on-chip performance and connectivity.

FR3148319A1Pending Publication Date: 2024-11-01SOITEC SA
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
FR2023004355
Authority / Receiving Office
FR · FR
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-28
Publication Date
2024-11-01

AI Technical Summary

Technical Problem

The existing 2.5D integration process for systems on a chip is time-consuming and costly due to the need for low-speed grinding and low-temperature processing to avoid damaging electronic components, limiting the development of complex and high-performance systems.

Method used

A method involving the formation of a weakening zone in a donor substrate, placement of microchips or blocks on the weakened surface, bonding to a support substrate, detaching the donor substrate to transfer the microchips, and forming electrical interconnections, all at low temperatures to preserve component integrity.

Benefits of technology

Enables independent optimization of microchips with appropriate materials and processes, combining 2.5D and 3D integration to enhance system-on-chip performance and connectivity without damaging components.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
Patent Text Reader

Abstract

The invention relates to a method for forming an integrated circuit, comprising: - the formation of a weakened zone (21) in a donor substrate (2), said weakened zone defining a surface layer (22) of the donor substrate; - the placement of at least two microchips (24) and / or tiles (25) made of a semiconductor or piezoelectric material on the surface layer of the weakened donor substrate; - the coating of the semiconductor and / or piezoelectric microchips and / or tiles with at least one dielectric material; - the bonding of the donor substrate (2) to a support substrate (1) comprising at least one electronic circuit, the at least two microchips and / or tiles being at a bonding interface (I) with the support substrate; - the detachment of the donor substrate (2) along the embrittlement zone (21) so as to transfer the microchips (24) and / or the tiles (25) and the surface layer (22) onto the support substrate (1);- the formation of at least one electrical interconnection between the microchips and / or the pads and at least one electrical interconnection between the microchips and / or the pads and the electronic circuit. Figure for the abbreviation: [Fig 2E];
Need to check novelty before this filing date? Find Prior Art

Description

Title of the invention: Method of forming an integrated circuit Field of invention

[0001] The present invention relates to a method of forming an integrated circuit. Technical background

[0002] A system on a chip (SoC) is an integrated circuit integrating a plurality of components on a single chip. Such a system may include a central processing unit, memory, input / output interfaces, digital, analog, mixed signal and / or radio frequency (RF) signal processing functions and power management.

[0003] Such a system is particularly used in mobile computing systems such as tablets and smartphones, as well as in embedded systems.

[0004] Systems-on-chip are becoming increasingly complex and demanding in terms of high performance and functionality, especially for 5G / 6G connectivity.

[0005] 2.5D integration combines multiple integrated circuit chips (also known as microchips or "chiplets") in a single package with and without their stacking in a three-dimensional (3D) circuit with redistribution layers (RDLs) with and without through-hole vias (TSVs) to connect them.

[0006] Figures 1A to 1D illustrate a known method of 2.5D integration.

[0007] Referring to [Fig.lA], a support substrate 1' is processed to include the circuits electronics. Said support substrate may comprise several layers 10', 11', 12', 13' of different materials, electronic components 110' and metal interconnections 111' being arranged in and / or between said layers 10', 11', 12', 13'.

[0008] With reference to [Fig.lB], at least two blocks 24', 25' of a semiconductor or piezoelectric material are placed on an intermediate substrate 2' and the intermediate substrate with the blocks is bonded to the support substrate 1'.

[0009] With reference to [Fig. 1C], the intermediate substrate 2' is removed to expose the tiles 24', 25'. Said removal is generally carried out by grinding the intermediate substrate, and polishing the exposed surface of the tiles, for example using chemical mechanical polishing (CMP).

[0010] Next, additional devices are formed in the tiles to provide RF, filtering and / or power functions. After the formation of said additional devices, metallic interconnections with the underlying electronic circuit are formed.

[0011] Then, as shown in [Fig. 1D], an electrically insulating layer 26' is deposited on the support substrate 1' and the blocks 24', 25'.

[0012] A disadvantage of the above method is that the grinding must be carried out at low speed so as not to damage or move the paving stones. Therefore, the process is relatively time-consuming or involves increased cost.

[0013] Another disadvantage of this method is that the additional devices must be formed by low temperature processes (e.g., processes not involving a temperature above 400°C) so as not to damage the electronic components or the metal interconnections of the supporting substrate.

[0014] Thus, the existing method has several limitations which hinder the development of 2.5D integration. Summary of the invention

[0015] An objective of the present invention is to overcome the above drawbacks in 2.5D integration in order to provide systems-on-chip with increased performance.

[0016] To this end, an object of the invention is a method of forming an integrated circuit, comprising:

[0017] - the formation of a weakening zone in a donor substrate, said weakening zone embrittlement defining a surface layer of the donor substrate;

[0018] - the placement of at least two microchips and / or blocks made of a material semiconductor or piezoelectric on the surface layer of the weakened donor substrate;

[0019] - the coating of microchips and / or semiconductor and / or piezo blocks electrical by at least one dielectric material;

[0020] - bonding the donor substrate to a support substrate comprising at least one electronic circuit, the at least two microchips and / or pads being at a bonding interface with the support substrate;

[0021] - detachment of the donor substrate along the weakening zone so as to transfer the microchips and / or the blocks and the surface layer onto the support substrate;

[0022] - the formation of at least one electrical interconnection between the microchips and / or the blocks and at least one electrical interconnection between the microchips and / or blocks and the electronic circuit.

[0023] With this method, each microchip can be independently optimized with appropriate materials and process technologies and known correct pads, before being transferred to the carrier substrate. In addition, 2.5D and 3D integrations are combined to optimize the form factor of the system-on-chip and to improve the connection or communication between microchips.

[0024] In this text, a microchip is an integrated circuit which contains a defined functionality and which is intended to be combined with other microchips on a single support substrate to form a system functionality package.

[0025] In the present text, a pad is a piece of semiconductor or piezoelectric material. Such a pad may be formed from a single semiconductor or piezoelectric material or from a stack of semiconductor and / or piezoelectric materials.

[0026] In some embodiments, forming the embrittlement zone comprises implanting atomic species, such as hydrogen and / or helium, into the donor substrate.

[0027] In some embodiments, the method comprises cutting the support substrate after forming said interconnections to form at least one system module or system in package ("System in package") comprising at least two tiles and / or microchips. Advantageously, the semiconductor or piezoelectric tiles may be smaller than the system module or system in package.

[0028] In some embodiments, at least one pad comprises a semiconductor material selected from the group consisting of: • III-V materials, in particular indium nitride (InN), indium phosphide (InP), gallium nitride (GaN), aluminum nitride (AIN), aluminum scandium nitride (AIScN), indium arsenide (InAs), gallium arsenide (GaAs), aluminum arsenide (AlAs), indium phosphide (InP), gallium phosphide (GaP) or aluminum phosphide (A1P), and • IV or IV-IV materials, in particular germanium or silicon carbide (SiC).

[0029] Alternatively or additionally, at least one pad may comprise a piezoelectric material selected from the group consisting of: lithium tantalate (LiTaO3), lithium niobate (LiNbO3), lanthanum aluminate (LaA103), potassium sodium niobate (K xNabx NbO3 or KNN), barium titanate (BaTiO3), quartz, lead zirconate titanate (PZT), lead magnesium niobate-lead titanate compounds (PMN-PT), and zinc oxide (ZnO).

[0030] In some embodiments, at least one pad comprises a semiconductor or piezoelectric material different from a semiconductor or piezoelectric material of at least one other pad.

[0031] In some embodiments, the donor substrate comprises silicon, silicon carbide, or a stack of layers of silicon and silicon carbide.

[0032] The detachment of the donor substrate along the weakening zone is advantageously carried out at a temperature below 900°C, preferably below 400°C.

[0033] In some embodiments, the method further comprises removing the surface layer of the donor substrate transferred to the support substrate. Removing the surface layer of the donor substrate may comprise chemical etching of said layer.

[0034] In some embodiments, the method further comprises forming at least one electronic component, such as a transistor, a capacitor, a diode and / or a metal interconnect in or on the surface layer of the donor substrate transferred to the support substrate.

[0035] Advantageously, the formation of said at least one electronic component in or on the surface layer is carried out at a temperature below 900°C, preferably below 400°C.

[0036] In some embodiments, the method further comprises depositing at least one metal redistribution layer on the surface layer.

[0037] The method may further comprise forming through-vias through the surface layer to electrically connect the microchips and / or the pads to the at least one redistribution layer.

[0038] In some embodiments, the method further comprises depositing at least one layer of amorphous and / or polycrystalline silicon and / or a dielectric layer on the surface layer.

[0039] In some embodiments, the method further comprises processing each tile to form an RF component, a filter, and / or a power amplifier.

[0040] Advantageously, said treatment of the paving stones is carried out at a temperature below 900°C, preferably below 400°C. Presentation of figures

[0041] Other features and advantages of the invention will be described in the following detailed description, on the basis of the appended drawings, in which:

[0042] - Figures 1A to 1D illustrate the steps of a known 2.5D integration method, wherein a support substrate is processed to form at least one electronic circuit ([Fig.lA]), at least two tiles of a semiconductor or piezoelectric material are placed on an intermediate substrate which is bonded to said support substrate ([Fig.lB]), the intermediate substrate is removed by grinding ([Fig.lC]), additional devices / circuits are formed in the tiles by low temperature processes and an electrically insulating layer is deposited on the support substrate and the tiles ([Fig.lD]);

[0043] - Figures 2A to 2H illustrate the steps of a 2.5D integration method according to the invention, wherein a support substrate comprising at least one electronic circuit is provided ([Fig.2A]), a weakening zone is formed in a donor substrate ([Fig.2B]), at least two microchips and / or blocks of semiconductor or piezoelectric material are placed on the donor substrate ([Fig.2C]), with the option of coating the donor with a low-temperature reflow dielectric or polymer, followed by CMP to planarize the oxide or polymer to meet bonding requirements or to stop on semiconductor or piezoelectric tiles ([Fig.2D]), the donor substrate is bonded to the carrier substrate ([Fig.2E]), the donor substrate is peeled off along the embrittlement zone ([Fig.2F]), the transferred layer from the donor substrate is removed ([Fig.2G]), or redistribution layers and / or TSVs are formed on the transferred layer ([Fig.2H]).

[0044] For reasons of readability of the drawings, the components or layers may not have been drawn to scale.

[0045] Elements designated by the same reference sign in different figures are identical or perform the same function and therefore may not be described in detail with reference to each figure. Detailed description of the embodiments

[0046] A method according to the invention is illustrated in Figures 2A to 2H.

[0047] As shown in [Fig.2A], a support substrate 1 is provided.

[0048] The support substrate 1 comprises a base layer 10 which forms a support mechanical, a device layer 11 and layers 12, 13. Said layers 10, 11, 12, 13 may be formed from one or more semiconductor materials, such as silicon or silicon carbide.

[0049] The device layer 11 comprises an electronic circuit comprising CMOS electronic components 110, such as transistors, and interconnects 111 providing an electrical connection between the components 110. This device layer may be formed by CMOS methods which are known to those skilled in the art and will not be described in detail in this text.

[0050] As shown in [Fig.2B], a donor substrate 2 is provided.

[0051] The donor substrate 2 comprises a semiconductor substrate 20 and a dielectric layer 23 extending over the semiconductor substrate 20.

[0052] The semiconductor substrate 20 may comprise silicon or silicon carbide (SiC).

[0053] A weakening zone 21 is formed by the implantation of ionic species such as hydrogen and / or helium into the semiconductor substrate 20 through the dielectric layer. The weakening zone 21 thus delimits a semiconductor layer 22 which extends between the weakening zone 21 and the dielectric layer 23.

[0054] As shown in [Fig.2C], after implantation, at least two microchips 24 and / or tiles 25 are placed on the donor substrate.

[0055] Each microchip is a piece of semiconductor material in which an integrated circuit having a defined functionality has been formed.

[0056] Each pad is a piece of semiconductor or piezoelectric material. Each tile may be formed from a single material or a stack of at least two different semiconductor or piezoelectric materials, respectively. The tiles may be cut from a wafer having a smaller area than the donor substrate.

[0057] The semiconductor tiles may comprise at least one of the following materials: • III-V materials, in particular indium nitride (InN), indium phosphide (InP), gallium nitride (GaN), aluminum nitride (AIN), aluminum scandium nitride (AIScN), indium arsenide (InAs), gallium arsenide (GaAs), aluminum arsenide (AlAs), indium phosphide (InP), gallium phosphide (GaP) or aluminum phosphide (AlP), and • IV or IV-IV materials, in particular germanium or silicon carbide (SiC).

[0058] The piezoelectric tiles may comprise at least one of the following materials: lithium tantalate (LiTaO3), lithium niobate (LiNbO3), lanthanum aluminate (LaA103), potassium sodium niobate (KxNaixNbO3 or KNN), barium titanate (BaTiO3), quartz, lead zirconate titanate (PZT), lead magnesium niobate-lead titanate compounds (PMN-PT), and zinc oxide (ZnO).

[0059] Preferably, the blocks and / or microchips may be of different types and / or materials so as to allow the combination of a plurality of functions on a module.

[0060] The blocks and microchips may have the same or different dimensions.

[0061] Chips and microchips are generally smaller than system modules or housing systems to be formed by the method according to the invention.

[0062] As shown in [Fig.2D], at least one dielectric or polymer material 26 is deposited on the donor substrate in order to fill the spaces between the microchips 24 and / or the pads 25. Said dielectric or polymer material may comprise a nitride, such as silicon nitride, an oxide, such as silicon oxide. Advantageously, said dielectric or polymer material is capable of reflow.

[0063] Advantageously, chemical-mechanical polishing (CMP) may be performed after said deposition of dielectric or polymer material in order to planarize the surface of the dielectric or polymer material and to adjust the thickness of the dielectric or polymer material to a desired thickness. In particular, said polishing may be carried out so as to expose the surface of the microchips or pads.

[0064] With reference to [Fig.2E], the donor substrate 2 is assembled to the support substrate 1. The bonding interface I comprises, on the one hand, the layer 13 and, on the other hand, the microchips 24 and / or the blocks 25 and the dielectric or polymer material 26. Preferably, the adhesion of the donor substrate to the support substrate is achieved by mo- bonding lecular.

[0065] With reference to [Fig.2F], the donor substrate is detached along the weakening zone 21. Consequently, the semiconductor layer 22, the dielectric layer 23, the microchips 24 and / or the tiles 25 are transferred onto the support substrate 1. The remainder of the donor substrate can be recycled for further use.

[0066] The detachment from the donor substrate can be initiated by a heat treatment. Said heat treatment is preferably carried out at a temperature below 900°C, preferably below 400°C, in order not to damage the interconnections and the devices / circuits formed in the support substrate.

[0067] In some embodiments (see [Fig.2G]), the semiconductor layer 22 and the dielectric layer 23 may be removed to expose the microchips and / or the pads. For this purpose, selective chemical etching may be implemented.

[0068] In other embodiments, the semiconductor layer 22 may be retained on the microchips and / or the pad in order to form additional components, such as transistors, capacitors, diodes, a metal interconnect (TSV) or a combination of these components in or on said layer 22. The formation of said electronic components is carried out at a temperature below 900°C, preferably below 500°C, in order not to damage the interconnects and / or the devices / circuits formed in the support substrate.

[0069] As shown in [Fig.2H], a metal redistribution layer (RDL) 27 may be deposited on the semiconductor layer 22. Optionally, through-vias (not shown) may be formed through the semiconductor layer to electrically connect the microchips and / or pads to the redistribution layer and thereby provide 3D integration.

[0070] Additionally or alternatively, at least one layer of amorphous and / or polycrystalline silicon may be deposited on the surface layer in order to thicken the surface layer and increase the stiffness of the assembly.

[0071] At least one electrical interconnection may be formed between the microchips and / or the tiles. Said interconnection may be made before or after the transfer of the tiles and the microchips onto the support substrate.

[0072] In addition, at least one electrical interconnection may be formed between the microchips and / or the pads and the electronic circuit formed in the support substrate.

[0073] The tiles may be processed to form radio frequency and / or power components. Examples of such components include an RF component, a filter and / or a power amplifier. Said processing of the tiles is carried out at a temperature below 900°C, preferably below 400°C, so as not to damage the interconnections and / or the devices / circuits formed in the support.

[0074] After the components and interconnections are finalized, the support substrate can be divided into system modules and / or system-in-packages comprising at least two blocks and / or microchips.

Claims

Claims

1. A method of forming an integrated circuit, comprising: - forming a weakening zone (21) in a donor substrate (2), said weakening zone defining a surface layer (22) of the donor substrate; - placing at least two microchips (24) and / or tiles (25) made of a semiconductor or piezoelectric material on the surface layer of the weakened donor substrate; - coating the microchips and / or semiconductor and / or piezoelectric tiles with at least one dielectric material; - bonding the donor substrate (2) to a support substrate (1) comprising at least one electronic circuit, the at least two microchips and / or tiles being at a bonding interface (I) with the support substrate; - detaching the donor substrate (2) along the weakening zone (21) so as to transfer the microchips (24) and / or the blocks (25) and the surface layer (22) onto the support substrate (1);- the formation of at least one electrical interconnection between the microchips and / or the blocks and at least one electrical interconnection between the microchips and / or the blocks and the electronic circuit.;

2. The method of claim 1, wherein forming the embrittlement zone (21) comprises implanting atomic species, such as hydrogen and / or helium, into the donor substrate.

3. A method according to any one of claims 1 or 2, further comprising cutting the support substrate after forming said interconnections to form at least one system module or system-in-package comprising at least two tiles and / or microchips.

4. The method of claim 3, wherein the semiconductor or piezoelectric tiles are smaller than the system module or system-in-package.

5. Method according to any one of claims 1 to 4, in which at least one block comprises a semiconductor material selected from the group consisting of: • III-V materials, in particular indium nitride (InN), indium phosphide (InP), gallium nitride (GaN), aluminum nitride (AIN), aluminum scandium nitride (AIScN), indium arsenide (InAs), gallium arsenide (GaAs), aluminum arsenide (AlAs), indium phosphide (InP), gallium phosphide (GaP) or aluminum phosphide (A1P), and • IV or IV-IV materials, in particular germanium or silicon carbide (SiC).

6. The method of any one of claims 1 to 5, wherein at least one pad comprises a piezoelectric material selected from the group consisting of: lithium tantalate (LiTaO3), lithium niobate (LiNbO3), lanthanum aluminate (LaA103), potassium sodium niobate (KxNahxNbO3 or KNN), barium titanate (BaTiO3), quartz, lead zirconate titanate (PZT), lead magnesium niobate-lead titanate compounds (PMN-PT), and zinc oxide (ZnO).

7. A method according to claim 5 or claim 6, wherein at least one tile comprises a semiconductor or piezoelectric material different from a semiconductor or piezoelectric material of at least one other tile.

8. A method according to any one of claims 1 to 7, wherein the donor substrate comprises silicon, silicon carbide or a stack of layers of silicon and silicon carbide.

9. Method according to any one of claims 1 to 8, wherein the detachment of the donor substrate (2) along the weakening zone (21) is carried out at a temperature below 900°C, preferably below 400°C.

10. A method according to any one of claims 1 to 9, further comprising removing the surface layer (22) of the donor substrate transferred to the support substrate (1).

11. The method of claim 10, wherein removing the surface layer (22) from the donor substrate comprises chemically etching said layer.

12. A method according to any one of claims 1 to 9, further comprising forming at least one electronic component, such as a transistor, a capacitor, a diode and / or a metal interconnect in or on the surface layer (22) of the donor substrate transferred to the support substrate (1).

13. The method of claim 12, wherein the formation of said at least one electronic component in or on the surface layer is carried out at a temperature below 900°C, preferably below 400°C.

14. A method according to claim 12 or claim 13, further comprising depositing at least one metal redistribution layer (27) on the surface layer (22).

15. The method of any one of claims 12 to 14, further comprising forming through vias through the surface layer to electrically connect the microchips and / or pads to the at least one redistribution layer.

16. A method according to any one of claims 12 to 15, further comprising depositing at least one layer of amorphous and / or polycrystalline silicon and / or a dielectric layer on the surface layer (22).

17. A method according to any one of claims 1 to 16, further comprising processing each tile to form an RF component, a filter and / or a power amplifier.

18. A method according to claim 17, wherein said treatment of the paving stones is carried out at a temperature below 900°C, preferably below 400°C.

Citation Information

Patent Citations

  • Bonding process and layer transfer method

    EP2302671A1

  • Method and system for template assisted wafer bonding using pedestals

    US20160111407A1