Vehicle pressurized gas tank
A polyurea-based protective coating with intumescent agents addresses the inadequacies of epoxy-based layers, enhancing the tank's resistance to impacts, chemicals, and thermal stresses, ensuring safety and durability in extreme conditions.
Patent Information
- Application Number
- FR2023004976
- Authority / Receiving Office
- FR · FR
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-19
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2043-05-19
AI Technical Summary
Existing pressurized gas tanks for vehicles face issues with inadequate protection against chemical, mechanical, and thermal stresses, particularly at extreme temperatures, leading to potential corrosion and failure due to post-impact cracking and the limitations of epoxy-based protective layers.
A protective coating based on polyurea with at least two layers, including a fire retardant intumescent agent, is applied to the composite reinforcement structure, providing enhanced resistance to impacts, chemicals, and thermal stresses over a wide temperature range.
The polyurea-based coating effectively protects the tank from -40°C to +85°C, withstands impacts, and maintains integrity against chemical and environmental agents, meeting safety standards for hydrogen-powered vehicles.
Abstract
Description
Title of the invention: Vehicle pressure tank
[0001] The invention relates to the field of vehicle pressure tanks, such as those for motor vehicles, trucks, buses, trains, or boats. More particularly, the invention relates to a vehicle pressure tank, a vehicle comprising such a pressure tank, and a method for preparing the gas.
[0002] Pressurized gas tanks are used to store and transport all types of gas under pressure. Pressurized gas tanks are generally classified according to one of the following five types: a type I pressurized gas tank having an all-metal construction; a type II pressurized gas tank having a metal construction including a fiber winding for the reinforcement of its cylindrical part; a type III pressurized gas tank having a metal liner with a composite reinforcement structure; a type IV pressurized gas tank including a plastic liner with a composite reinforcement structure; and a type V pressurized gas tank having a composite reinforcement structure and being without a liner.
[0003] Thus, in the prior art, a pressurized gas tank, for example, configured to store gas at a pressure of at least 350 bar or at least 700 bar, the gas being, for example, hydrogen, is already known. This pressurized gas tank is configured for use by a vehicle equipped with the pressurized gas tank for various functions, including as an energy source. This tank is usually made of composite material for reasons of weight reduction and safety.
[0004] Such a pressurized gas tank is conventionally composed of an inner casing called a liner, which provides a seal against the gas contained in the tank. The liner is made, for example, of a plastic material, in the case of a Type IV tank, chosen for its lightness and low manufacturing cost, or of a metal such as aluminum, or another material such as a metal alloy, in the case of a Type III tank. The "plastic" type liner includes at least one opening for filling and emptying the tank. It is manufactured by injection molding, rotational molding, or extrusion blow molding of a thermoplastic or thermosetting polymer material such as polyethylene, polyamide, polyphthalamide, polyurethane, silicone, or polyoxymethylene.Advantageously, in the context of a Type IV tank, the plastic chosen for the liner can be reinforced with fibers, particles of nanometric or micrometric size, or be composed of several layers. Reinforcing fibers are, for example, . Glass fibers, carbon fibers, basalt fibers, aramid fibers, polymer fibers, silica fibers, polyethylene fibers, natural fibers, metallic fibers, metal alloy fibers, or ceramic fibers can all be used to fill liners. The particles can be selected from various types of materials, such as ceramics, glass, metals, organic materials, or a combination thereof. These fillers increase the deformation resistance of the resulting material. In a polymer material filled with reinforcing fibers, the reinforcing fibers and the polymer are intertwined to form a single, solid material. In a multi-layered construction, the layers can be made from different materials, such as metals or organic materials. This multi-layered approach reduces the liner's gas permeability.The two approaches mentioned can be combined.
[0005] The liner is generally cylindrical in shape and has two domed ends. The liner has an opening, which is usually topped by a nozzle. The pressurized fluid exerts strong stresses on the internal surface of the liner, which can compromise the liner's integrity and cause dangerous leaks, particularly with combustible gases such as hydrogen.
[0006] To improve the mechanical properties of the pressurized gas tank, the liner is surrounded by a composite reinforcement structure, generally made by winding resin-impregnated fiber strips around the liner at various angles. The fibers used can be selected from ceramics, glasses, and organic materials. For example, carbon fibers, glass fibers, and aramid fibers are commonly used. The resins used can be thermosetting or thermoplastic. For example, epoxy or vinyl ester resins are used for thermosetting resins; and polyamide or PEEK resins for thermoplastic resins.The winding process can be carried out using a wet winding method, where the fibers are immersed in a resin bath before being wound, or a dry winding method, where the fibers are supplied as a strip of parallel fibers impregnated with resin, more commonly known as "tow preg." The resins used can be filled with nanometer and / or micrometer-sized particles to improve the properties of the composite reinforcement structure. These particles can be made from a material chosen from ceramics, glasses, metals, organic materials, or any combination thereof. For example, hollow glass beads can be used, allowing for weight reduction and a decrease in the risk of delamination of the composite reinforcement structure, while graphene or carbon nanotubes can lead to improved electrical properties of the composite reinforcement structure. or thermal, and to a reduction of the risk of delamination of the composite reinforcement structure, rubber beads allowing an increase in ductility, a reduction in the risk of delamination as well as a reduction of residual stresses within the composite reinforcement structure.
[0007] However, these pressure vessels must withstand chemical and / or mechanical stresses to meet safety standards when used in a motor vehicle. In particular, they must meet the requirements laid down by Regulation No. 134 of the United Nations Economic Commission for Europe (UNECE) — Uniform provisions concerning the type-approval of motor vehicles and their components with regard to the safety requirements for hydrogen-powered vehicles [2019 / 795].
[0008] Under normal operating conditions, as defined by certification standards, high-pressure tanks for transport applications must be able to withstand various types of external stresses. These include chemical stresses related to exposure to high concentrations of strong acids and bases or to organic or inorganic solvents, mechanical stresses related to impacts such as gravel during transport, and environmental stresses such as salt spray, ozone exposure, and / or UV exposure.The temperature range over which the tank must retain its properties extends from -40°C to +85°C at 95% relative humidity according to Regulation No. 134 of the United Nations Economic Commission for Europe (UNECE) — Uniform provisions concerning the approval of motor vehicles and their components with regard to the safety requirements of hydrogen-powered vehicles [2019 / 795].
[0009] Conventionally, this resistance to chemical, mechanical, and / or thermal attack is provided by the presence of an additional protective layer on the exterior of the tank. This layer generally consists of either a layer of fiberglass impregnated with intumescent resin (applied by filament winding using a dry or wet process), an intumescent coating, generally based on a two-component (2K) epoxy, applied by spraying, direct application, or injection, or a combination of both. The epoxy-based protective layer contains intumescent agents which, after exposure to fire, expand and create an insulating barrier. The expansion and calcination of the resin by the intumescent reaction reduces and slows the heat transfer from the flames to the laminate, delaying the decomposition of the resin in the laminate.This phenomenon allows the rapid draining equipment installed on the bases to purge the tank and prevent its failure.
[0010] However, such protective layers do not guarantee a level of Adequate protection of the composite reinforcement structure is required at minimum thicknesses due to their inherent fragility. For example, post-impact cracking creates a pathway allowing chemicals to come into contact with the composite reinforcement structure and thus corrode it. This corrosion increases the risk of tank failure. This post-impact cracking phenomenon is exacerbated at sub-zero temperatures.
[0011] Furthermore, the epoxy-based system does not exhibit impact damping capacity at low temperatures. In addition, the epoxy-based system requires long curing times at room temperature, which necessitates the use of an oven to accelerate curing and thus increases costs. This curing delay, linked to the curing time, can also promote sagging of the composite reinforcement structure and the formation of air pockets, leading to weak points within it.
[0012] It is therefore desirable to have a protective layer capable of withstanding the chemical, mechanical, and thermal stresses imposed on the tank over a wide temperature range, and without these drawbacks. Furthermore, it is desirable that the protective layer possess these properties while being relatively lightweight.
[0013] Unexpectedly, the inventors found that these and other goals can be achieved with a polyurea-based protective coating, preferably applied in a predetermined manner.
[0014] Therefore, the present invention relates to a pressure vessel comprising at least one composite reinforcement structure, coated at least in part by a protective coating, in which the protective coating comprises at least two polyurea-based protective layers, at least one of the polyurea-based protective layers further comprising at least one fire retardant which is an intumescent agent, the polyurea(s) being reaction products of at least one hardener and at least one resin, for which (i) the resin is an aromatic or aliphatic polyamine compound, optionally substituted by at least one alcohol function, (ii) the hardener is an aromatic, cycloaliphatic, heterocyclic, alicyclic or aliphatic polyisocyanate compound,and their reaction products in the form of aliphatic or aromatic oligomers; at least one resin of a first polyurea-based protective layer being different from at least one resin of a second polyurea-based protective layer; the protective layer containing an intumescent agent being the outermost layer of the protective coating. Advantageously, the pressure vessel according to the invention comprises a liner and a composite reinforcement structure, and is coated at least partially by a protective coating, which comprises at least two layers of Polyurea-based protection as defined throughout this text. The liner is notably made of a plastic material.
[0015] The invention also relates to a method for preparing such a reservoir, comprising the following steps
[0016] a) obtaining a chuck,
[0017] b) winding a composite reinforcing structure around at least a portion of the mandrel to obtain a hollow body
[0018] c) formation on at least a portion of the surface of the composite reinforcement structure of a protective coating, said protective coating formation step comprising the steps of
[0019] cl) deposition on at least a portion of the surface of the composite reinforcing structure of a mixture (D) of at least one resin and at least one hardener, the stoichiometric ratio between the resin and the hardener being between 2:1 and 1:2, preferably from 1.3:1 to 1:1.3, in particular substantially equal to 1:1, and polymerization of the mixture (D) to obtain a first protective layer based on polyurea
[0020] c2) deposit on at least part of the surface of the hollow body coated with a layer of protection obtained at the end of step cl), of a mixture (I) of at least one resin, at least one hardener and at least one fire retardant, the stoichiometric ratio between the resin and the hardener being between 2:1 and 1:2, preferably from 1.3:1 to 1:1.3, in particular substantially equal to 1:1 and polymerization of the mixture (I) to obtain a second protective layer based on polyurea at least one resin of the mixture (D) being different from at least one resin of the mixture (I).
[0021] According to one embodiment of the invention, the mandrel is a fusible body. It will melt and disappear during the subsequent steps of the process.
[0022] According to another embodiment of the invention, the mandrel is a liner, in particular a liner made of plastic material.
[0023] The invention then relates to a method for preparing such a reservoir, comprising the following steps
[0024] a) obtaining a liner, preferably based on plastic material
[0025] b) winding a composite reinforcement structure around at least a portion of the liner to obtain a hollow body
[0026] c) formation on at least a portion of the surface of the composite reinforcement structure of a protective coating, said protective coating formation step comprising the steps of
[0027] cl) deposition on at least a part of the surface of the composite reinforcing structure of a mixture (D) of at least one resin and at least one hardener, the stoichiometric ratio between the resin and the hardener being between 2:1 and 1:2, preferably from 1.3:1 to 1:1.3, in particular substantially equal to 1:1, and polymerization of the mixture (D) to obtain a first protective layer based on polyurea
[0028] c2) deposition on at least part of the surface of the hollow body coated with a layer of protection obtained at the end of step cl), of a mixture (I) of at least one resin, at least one hardener and at least one fire retardant, the stoichiometric ratio between the resin and the hardener being between 2:1 and 1:2, preferably from 1.3:1 to 1:1.3, in particular substantially equal to 1:1 and polymerization of the mixture (I) to obtain a second protective layer based on polyurea at least one resin of the mixture (D) being different from at least one resin of the mixture (I).
[0029] The invention also relates to a motor vehicle comprising such a tank which is therefore covered at least in part by a protective coating.
[0030] In a known manner, a polyurea is a polymer comprising a plurality of urea bonds (-NH-CO-NH-) resulting from the reaction of a polyamine having at least two primary amine functions with a polyisocyanate, that is to say a compound bearing at least two isocyanate functions.
[0031] Other components may be involved in the manufacture of polyurea, including catalysts and additives.
[0032] US-A1-2013 / 0153458 describes a substrate coating system, in particular of a reservoir, comprising an inner layer and an outer layer made of polyurethane or polyurea, between which is an intermediate layer of viscous gel comprising surfactants and polybutadiene, which ensures their adhesion.
[0033] CN-A-114636095 describes a hydrogen storage container comprising a liner surrounded by several layers of fibers wound along different axes; a layer of polyurea is spread on the outer surface of the fiber layers.
[0034] These documents do not solve the problems underlying the present invention.
[0035] In the context of the present invention, resin means an aromatic or aliphatic polyamine compound, optionally substituted by at least one alcohol functional group. The amine functional groups may be primary, secondary, or tertiary; preferably, the compound comprises primary amine functional groups.
[0036] The resin may in particular be selected from the group consisting of the following compounds: polyoxypropylenediamine, diethylmethylbenzenediamine, glyceryl poly(oxypropylene)triamine, polyalkyl- or polyaryl-amines and polyetheramines, in particular from among ethylenediamine; 1,2-diaminopropane; 1,3-diaminopropane; 2,5-diamino-2,5-dimethylhexane; 1,11-diaminoundecane; 1,12-diaminododecane; 2,4-hexahydrotoluenediamine; 2,6-hexahydrotoluenediamine; 2,4'-Diamino-dicyclohexyl methane isophoronediamine; N-methyl-propylene-1,3-diamine; 1,6-hexamethylenediamine; 1,4-diaminocyclohexane; 1,3-diaminocyclohexane; N,N'-dimethylethylenediamine; 4,4 / -dicyclohexyl-methanediamine; 2,4-diaminotoluene; 2,6-diaminotoluene; 3,5-Diethyl-2,4-diaminotoluene; 3,5-diethyl-2,6-diaminotoluene; mono-, di-, tri-, or tetra-alkyl substituted 4,4'-diamino-diphenylmethanes; and amino alcohols such as ethanolamine, 1-aminopropanol, and 2-aminopropanol. Also noteworthy are the prepolymers of the Jeffamine® family, marketed, for example, by Huntsman, or Hycar®, marketed by Goodrich. A prepolymer is an oligomer or polymer with reactive groups that allow it to participate in subsequent polymerization. An oligomer is a molecule generally composed of fewer than ten identical or very similar components.
[0037] In the context of the invention, the term "hardener" refers to an aromatic, cycloaliphatic, heterocyclic, alicyclic, or aliphatic polyisocyanate compound, and their reaction products; it may be a monomer, polymer, or prepolymer. The polyisocyanate compound comprises at least two isocyanate functional groups and includes, in particular, diisocyanates, triisocyanates, tetraisocyanates, and mixtures thereof.
[0038] The polyisocyanate compound may in particular be selected from the group comprising toluene diisocyanate (TDI), methylene diphenyl diisocyanate (MDI), isophorone diisocyanate (IPDI), hexamethylene diisocyanate (HDI), pentamethylene diisocyanate (PDI) and their prepolymers. The prepolymers are preferably reacted with each other before being incorporated into the composition.
[0039] In particular, a polyisocyanate compound selected from alpha-hydro-omega-hydroxypoly[oxy(methyl-1,2-ethanediyl)] polymers is used with 1,1'-methylenebis[isocyanatobenzene], the reaction mass of 4,4'-methylenediphenyl diisocyanate (MDI) and o-(pisocyanatobenzyl)phenyl isocyanate, 4,4'-methylenediphenyl diisocyanate (MDI), oligomers of 4,4'-methylenediphenyl diisocyanate (MDI) and mixtures thereof.
[0040] The use of aliphatic polyisocyanates is preferred when seeking to prepare a product that does not yellow.
[0041] The stoichiometric ratio between the resin component(s) and the polyisocyanate compound(s) is generally between 2:1 and 1:2, in particular between 1.8:1 and 1:1.8, preferably between 1.5:1 and 1:1.5, even more preferably between 1.3:1 and 1:1.3. Good results are obtained for protective coatings in which the polyurea(s) is a reaction product of at least one resin and at least one polyisocyanate compound in ratios of 1:1.2 to 1.2:1, in particular for ratios of about 1:1 plus or minus 5% (1:1.05 to 0.95) or 1:1 plus or minus 3% (1:1.03-0.97).
[0042] By polyurea-based coating, we mean a coating comprising one or more polyureas, in particular a mixture of two, three or more polyureas; preferably at least 80% of the coating is composed of polyurea, in particular polyurea or the A polyurea mixture must constitute at least 90%, and in particular at least 95%, of the polyurea-based layer. These percentages are expressed by weight relative to the total weight of the polymers present in the polyurea layer. Fillers, additives, and / or intumescent agents are not included in this definition of a polyurea-based layer. Therefore, the polymers in the polyurea-based layer may be 100% polyurea.
[0043] According to the invention, at least one resin of a first protective layer based on polyurea is different from at least one resin of a second protective layer based on polyurea.
[0044] According to one embodiment, at least one polyisocyanate compound (or hardener) of a first polyurea-based protective layer is different from at least one polyisocyanate compound (or hardener) of a second polyurea-based protective layer.
[0045] These two embodiments can be combined, at least one resin and at least one polyisocyanate compound of a first protective layer based on polyurea are different from at least one resin and at least one polyisocyanate compound of a second protective layer based on polyurea.
[0046] It is understood that all or part of the polyurea(s) of said first polyurea-based layer is different from the polyurea(s) of said second polyurea-based layer of the protective coating.
[0047] The protective coating comprises at least two polyurea-based layers, it may thus comprise in particular two polyurea-based layers, in particular three polyurea-based layers, or even four or more polyurea-based layers.
[0048] Additives such as UV absorbers, hindered amine photostabilizers, antioxidants, dispersion and grinding aids, wetting agents, impact modifiers, antifoams, suspension stabilizers, biocides, etc., may be added to the binder to improve the manufacturability and overall durability of the coatings of the present invention.
[0049] Advantageously, at least one of the layers of the protective coating contains at least one additive selected from UV absorbers, light stabilizers, antioxidants, dispersing agents, wetting agents such as surfactants, plasticizers, defoamers, and impact attenuators, also known as impact modifiers. Advantageously, it includes an additive selected from surfactants that can function as both a wetting agent and a suspension stabilizer.
[0050] The number and thickness of the polyurea-based layers in the coating according to the invention will be adapted by those skilled in the art, depending on the properties required. In all cases, the total thickness of the protective coating is less than or equal to to 12 mm, in particular less than or equal to 8 mm, in particular less than or equal to 4 mm. It is understood that the total thickness of the protective coating is generally greater than or equal to approximately 1 mm, in particular greater than or equal to 2 mm. Protective coatings according to the invention have in particular a total thickness of 2 mm to 4 mm, in particular 2.5 mm to 4 mm.
[0051] Advantageously, the polyurea(s) is / are chosen such that the elastic deformation of each polyurea-based protective layer is greater than the maximum elastic deformation of the last layer of the laminate covering the liner, over the entire temperature and relative humidity range of tank operation. Normal operating conditions are defined in UNECE Regulation No. 134 (Uniform provisions for the approval of motor vehicles and their components with regard to the safety requirements for hydrogen-powered vehicles [2019 / 795]), published in the Official Journal of 17 / 05 / 2019.
[0052] Elastic deformation is measured by tensile tests according to ISO 527:2019, at temperatures from -45°C to 85°C at 95% humidity.
[0053] Indeed, it has now been shown that a protective coating according to the present invention meets the safety requirements of Regulation No. 134 cited above.
[0054] In particular, it protects the tank at temperatures from -40°C to +85°C, it can withstand impacts of 30 Joules at -40°C and provides resistance to chemical and environmental agents (UV, corrosion); it provides fire resistance by delaying fire through its intumescent properties.
[0055] Advantageously, at least one polyurea-based protective layer contains an intumescent agent selected from the group of halogenated compounds, phosphorus compounds, boron compounds, metal hydroxides and metal oxides, and mixtures of at least two of them. The concentration of the intumescent agent in the polyurea-based layer may be between 0.1% and 50% by weight, relative to the total weight of the polyurea-based layer, and in particular, may be from 10% to 24% by weight.
[0056] Halogenated intumescent agents are in particular selected from chlorinated and / or brominated compounds such as polybrominated diphenyl ethers (PBDEs), tetrabromo-bisphenol A, hexabromo-cyclododecanes, decabromo-diphenylethane, De-chlorane plus (polychlorinated flame retardant produced by OXYCHEM) and short-chain chlorinated paraffins (SCCPs).
[0057] Boron compounds are in particular polyborates.
[0058] Phosphorus compounds are in particular polyphosphates.
[0059] The metal hydroxides are in particular chosen from aluminium hydroxide and magnesium hydroxide.
[0060] Metal oxides are in particular selected from the group comprising the titanium dioxide, silica, aluminium oxide and antimony oxide.
[0061] The protective layer(s) may also include fillers. In particular, at least one of the polyurea-based protective layers contains at least one filler, in the form of particles or fibers, said filler being selected from ceramics, metals, metal oxides, plastics and mixtures thereof.
[0062] Preferably, at least one of the polyurea-based protective layers does not contain a fire retardant that is an intumescent agent. This protective layer(s) is / are located inside the protective layer containing at least one intumescent agent.
[0063] A protective layer not containing an intumescent agent in the coating according to the invention preferably has a glass transition temperature Tg, measured by DMA (dynamic mechanical analysis) which is less than or equal to -40°C, in particular less than or equal to -43°C, advantageously less than or equal to -45°C.
[0064] Advantageously, a protective layer based on polyurea containing an intumescent agent in the coating according to the invention preferably has a glass transition temperature Tg, measured by DMA (dynamic mechanical analysis) of less than -20°C.
[0065] Said protective layer containing an intumescent agent advantageously has a degree of expansion at 180°C less than 20 times its thickness, preferably less than 15 times its thickness.
[0066] Preferably, in the protective layer not containing an intumescent agent, the polyurea(s) are essentially aliphatic: they are preferably prepared from amines with long and branched polymeric chains with few aromatic amines.
[0067] Preferably, in the protective layer containing an intumescent agent, the polyurea(s) are essentially aromatic: they are preferably prepared from short-chain aliphatic or aromatic amines.
[0068] According to an advantageous embodiment, the hardeners used for the preparation of the polyureas of each of said first and second protective layers are identical or compatible.
[0069] By compatible, it is understood that at least one hardener comprises a mixture of polyisocyanate compounds, and that at least 60% of the composition of the polyisocyanate compounds of one hardener is identical to that of the polyisocyanate compounds of a second hardener, in particular at least 80%.
[0070] When the two polyurea-based layers of the protective coating are in contact, they exhibit very good adhesion to each other without the need to introduce a layer of glue between them or, generally speaking, without it being It is necessary to promote cohesion between these layers.
[0071] Polyurea-based coatings according to the invention can in particular be obtained from at least one hardener selected from alpha-hydro-omega-hydroxypoly [oxy(methyl-1,2-ethanediyl)] polymers with 1,1'-methylenebis[isocyanatobenzene], the reaction mass of 4,4'-methylenediphenyl diisocyanate (MDI) and o-(pisocyanatobenzyl) phenyl isocyanate, 4,4'-methylenediphenyl diisocyanate (MDI), oligomers of 4,4'-methylenediphenyl diisocyanate (MDI), and mixtures thereof.
[0072] Advantageously, at least one polyurea-based layer is obtained from a resin selected from the group consisting of polyoxypropylenediamine; diethylmethylbenzenediamine, glyceryl poly(oxypropylene)triamine; preferably, it is a layer not containing an intumescent agent, and which has the characteristics mentioned above.
[0073] Advantageously, at least one polyurea-based layer is obtained from a resin selected from the group consisting of diethylmethylbenzenediamine and oleylamine derivatives; preferably, this layer contains an intumescent agent. It preferably also contains at least one compound selected from diammonium decaborate, hexane 6-olide, and C18 unsaturated fatty acids.
[0074] Without being bound by any particular theory, the polyurea-based layer containing the intumescent agent provides the fire-resistant properties of the protective coating. The polyurea-based layer not containing the intumescent agent provides the impact resistance of the protective coating according to the invention. Both types of layers contribute to the corrosion and chemical attack resistance of the protective coating according to the invention.
[0075] Advantageously, when a liner is present, the liner comprises a cylindrical central portion. For example, the cross-section of the cylindrical central portion is a circle or an ellipse. The composite reinforcement structure surrounds at least a portion of the liner, for example, the cylindrical central portion. The tank thus comprises at least one cylindrical central portion and two dome-shaped ends, and the protective coating comprising the polyurea layers covers at least a portion of the cylindrical central portion of the tank; in particular, the protective coating covers at least 80% of the cylindrical central portion of the tank, and in particular at least 90%, for example, at least 95%. The protective coating according to the invention can cover the entire cylindrical central portion of the tank.
[0076] According to some embodiments of the invention, the protective coating does not cover the dome-shaped ends of the tank.
[0077] According to other embodiments of the invention, at least one polyurea-based layer of the protective coating covers the ends of the tank.
[0078] The ends of the tank can be covered at least in part or in whole by a polyurea-based layer of the coating containing an intumescent agent as defined above.
[0079] According to one embodiment, the ends of the tank are covered at least partially or completely by a polyurea-based layer of the coating not containing an intumescent agent as defined above. The polyurea-based layer(s) containing an intumescent agent do not cover the ends of the tank.
[0080] According to another embodiment, the ends of the tank are covered at least partially by at least one polyurea-based layer not containing an intumescent agent and by at least one polyurea-based layer containing an intumescent agent. In particular, the protective coating as a whole covers at least partially the ends of the tank, specifically, it essentially covers all of the ends of the tank.
[0081] The protective coating can be applied or deposited on the tank according to methods known to those skilled in the art.
[0082] It can be applied in particular by pressure spraying, by immersion or by brush. Preferably, the coating is applied by spraying.
[0083] Advantageously, steps c1 and c2 are carried out successively. The time between steps c1) and c2) of applying the two coats is generally less than 1 hour. The polyurea-based protective layer obtained from mixture (I) is located on the outside of the protective coating; it is the outermost layer of the protective coating.
[0084] According to one variant of the process, at least one additional polyurea-based layer is deposited on the hollow body. The process then comprises at least one additional step of depositing a mixture of at least one resin and at least one hardener as defined herein. This step may be carried out between steps c1 and c2, or before step c1.
[0085] After the steps of depositing the mixtures of successive layers based on polyurea, the product obtained (comprising the hollow body covered with at least two layers based on polyurea) is placed under conditions allowing complete crosslinking and hardening of the polyureas.
[0086] The steps of depositing the polyurea-based coating layers are carried out at a temperature of 15°C to 75°C; they can be carried out at ambient temperature, this temperature having to be greater than or equal to the dew point + 3°C.
[0087] According to one embodiment of the invention, the polyurea-based coating deposition steps are carried out at room temperature; the hollow body obtained after removal from the oven is left to rest for a variable period until it cools. The time required to obtain a protective coating comprising the layers polyurea-based is less than or equal to 24 hours, in particular less than or equal to 7 hours, generally between 3 and 7 hours.
[0088] According to one embodiment of the invention, the polyurea-based coating deposition steps are carried out immediately after the hollow body is removed from the oven. "Immediately" means after a period of time of less than or equal to 1 hour after the hollow body is obtained, the temperature of which has not yet returned to ambient temperature. The surface temperature of the hollow body is approximately 70°C + / -5°C. The time required to obtain a protective coating comprising the polyurea-based layers is less than or equal to 3 hours.
[0089] The hollow body comprises a cylindrical central portion and two dome-shaped ends. The cylindrical central portion is generally covered, at least in part, by the composite reinforcing structure; the composite reinforcing structure does not cover the dome-shaped ends.
[0090] According to one embodiment, the deposition of mixtures D and I is carried out on at least 90% of the surface of the cylindrical part of the hollow body, in particular on the entire surface of the cylindrical part of the hollow body (covered by the composite reinforcement structure). The deposition may be carried out exclusively on the cylindrical part and / or on at least a portion of the dome-shaped ends of the hollow body.
[0091] According to one embodiment of the process, at least one of the mixtures D and I is further deposited on at least a portion of the dome-shaped ends of the hollow body. This may be solely mixture (D), solely mixture (I), or advantageously, mixture (D). According to another embodiment, mixtures (D) and (I) are deposited on the cylindrical portion of the hollow body and on its dome-shaped ends.
[0092] The process may include in particular the following steps, after the preparation, according to methods known to those skilled in the art, of the hollow body comprising the composite reinforcement structure and, where applicable, a liner.
[0093] A resin mixture as defined herein is prepared, preferably comprising long-chain, branched polymeric amines with few aromatic amines. A hardener as defined herein is also prepared, comprising a mixture of polyisocyanate compounds.
[0094] The resin mixture and the hardener are introduced into a mixing chamber of a spraying device in a stoichiometric ratio of 1:1 + / -5%. The reaction is almost immediate, and the polyurea is sprayed onto at least part of the hollow body to form the layer obtained from the mixture (D) (or layer (D)). The spraying conditions and the quantity of mixture are adjusted to obtain a layer (D) with a thickness greater than or equal to 1 mm and less than or equal to 3 mm, in particular less than or equal to 2 mm.
[0095] Advantageously, the temperature in the mixing chamber is 80°C + / - 10°C, and the pressure is 180 bars + / - 20 bars.
[0096] A resin mixture as defined herein is prepared, preferably comprising short-chain aliphatic or aromatic amines and containing an intumescent agent. A hardener as defined herein is also prepared, comprising a mixture of polyisocyanate compounds, identical or compatible with the hardener of the first polyurea layer.
[0097] The resin mixture and the hardener are introduced into a mixing chamber of a spraying device in a stoichiometric ratio of 1:1 + / -3%. The reaction is almost immediate; the polyurea is sprayed onto at least a portion of the hollow body coated with the first resin and hardener mixture, to form the layer obtained from mixture (I), (or layer (I)). The spraying conditions and the quantity of mixture are adjusted to obtain a layer (I) with a thickness greater than or equal to 1 mm and less than or equal to 3 mm, in particular less than or equal to 2 mm.
[0098] Advantageously, the temperature in the mixing chamber is 80°C + / - 10°C, and the pressure is 180 bars + / - 20 bars.
[0099] The resin and hardener mixtures are sprayed onto the hollow body by a spray gun, known to those skilled in the art. For example, an "airless" spray gun with a mechanical chamber and a flat spray pattern is used.
[0100] The polyurea layers are then allowed to harden for a period of between 3 and 7 hours, at room temperature or in an enclosure maintained at a temperature of approximately 70°C.
[0101] During the deposition of the resin and hardener mixture (optionally including at least one agent selected from additives, fillers and / or flame retardants such as intumescent agents), initial polymerization occurs. However, the layer does not fully harden upon deposition of the subsequent polyurea-based layer.
[0102] Polymerization is defined as a reaction comprising crosslinking. Polymerization is a chemical reaction between molecules, initiated, for example, by a catalyst or a reagent, with the action of heat or ambient humidity, by which a molecule of higher molar mass is formed. The initial molecules may be monomers or prepolymers. Crosslinking corresponds to the formation of chemical bonds along different spatial directions during this polymerization between the polymer chains and the crosslinking agents present in the product. The result is a three-dimensional molecular network that gives the product elasticity and prevents it from brittle.
[0103] The product that can be obtained by a process as described above is one of the objects of the invention.
[0104] According to an advantageous embodiment of the invention, the mixture of POLYRESYST® H 20020-70 RE resin and POLYRESYST® H20020-70 HA hardener marketed by Huntsman is used. This mixture is preferably prepared in a 2:1; 1:2 volume ratio.
[0105] According to another advantageous embodiment, the mixture of POLYRESYST H24505-90W HA hardener and POLYRESYST H24505-90W RE resin marketed by Huntsman is used. Said mixture is preferably made in a 2:1; l / 2 volume ratio.
[0106] In particular, in the process, the resin and hardener mixture used to prepare mixture (D) is obtained by mixing POLYRESYST® H 20020-70 RE and POLYRESYST® H20020-70 HA in a ratio of 1:1 + / -5% by volume. The reaction is almost immediate, and the polyurea is sprayed onto at least part of the hollow body to form the layer obtained from mixture (D) (or layer (D)). The resin mixture used to prepare mixture (I) is obtained by mixing POLYRESYST H24505-90W HA and POLYRESYST H24505-90W RE. The resin and hardener mixture is introduced into a mixing chamber of a spraying device in a ratio of 1:1 + / -3%. The reaction is almost immediate; the polyurea is sprayed onto at least part of the hollow body coated with the first mixture of resin and hardener, to constitute the layer obtained from mixture (I), (or layer (I)).
[0107] The tank incorporating the protective coating comprising two layers based on polyurea is subjected to the tests defined by Regulation No. 134 (UNECE). It meets the standards prescribed by this regulation.
Claims
Claims
1. Pressure vessel comprising - a composite reinforcement structure, coated at least in part with a protective coating, wherein the protective coating comprises at least two polyurea-based protective layers, - at least one of the protective layers based on one or more polyureas further comprising at least one fire retardant agent which is an intumescent agent, the polyurea(s) being one or more reaction products of at least one hardener and at least one resin, for which (i) the resin is an aromatic or aliphatic polyamine compound, optionally substituted by at least one alcohol function, (ii) the hardener is an aromatic, cycloaliphatic, heterocyclic, alicyclic or aliphatic polyisocyanate compound, and their reaction products in the form of oligomers, aliphatic or aromatic, at least one resin of a first protective layer based on polyurea being different from at least one resin of a second protective layer based on polyurea, the protective layer containing the intumescent agent being the outermost layer of the coating.
2. Pressure tank according to claim 1, characterized in that it comprises - a liner and - a composite reinforcement structure, coated at least in part with a protective coating, wherein the protective coating comprises at least two polyurea-based protective layers, - at least one of the protective layers based on one or more polyureas further comprising at least one fire retardant agent which is an intumescent agent, the polyurea(s) being one or more reaction products of at least one hardener and at least one resin, for which (i) the resin is an aromatic or aliphatic polyamine compound, optionally substituted by at least one alcohol function, (ii) the hardener is an aromatic, cycloaliphatic, heterocyclic, alicyclic or aliphatic polyisocyanate compound, and their products of reaction in the form of oligomers, aliphatic or aromatic, at least one resin of a first protective layer based on polyurea being different from at least one resin of a second protective layer based on polyurea, the protective layer containing the intumescent agent being the outermost layer of the coating.
3. Tank according to at least one of claims 1 or 2, characterized in that the total thickness of the protective coating is less than or equal to 12 mm, in particular less than or equal to 8 mm, in particular less than or equal to 4 mm, and in that the total thickness is greater than or equal to 1 mm.
4. Tank according to at least one of claims 1 to 3, characterized in that the intumescent agent is chosen from the group of halogenated compounds, phosphorus compounds, boron compounds, metal hydroxides and metal oxides and the mixture of at least two of them.
5. Tank according to at least one of claims 1 to 4, characterized in that at least one of the polyurea-based protective layers contains at least one filler, in the form of particles or fibers, said filler being chosen from ceramics, metals, metal oxides, plastics and their mixtures.
6. Tank according to at least one of the preceding claims, characterized in that at least one of the polyurea-based protective layers does not contain a fire retardant agent which is an intumescent agent.
7. Tank according to at least one of the preceding claims, characterized in that at least one of the polyurea-based protective layers contains at least one additive chosen from UV absorbers, light stabilizers, antioxidants, dispersing agents, wetting agents such as surfactants, plasticizing agents, anti-foams and impact attenuators.
8. Tank according to at least one of the preceding claims, characterized in that it comprises at least one cylindrical central portion and two dome-shaped ends, and in that the protective coating covers the cylindrical central portion of the tank.
9. Tank according to at least one of the preceding claims, comprising at least one cylindrical central portion and two dome-shaped ends, characterized in that at least one layer at polyurea base protective coating covers the ends of the tank.
10. Tank according to at least one of the preceding claims, characterized in that the hardeners for each of the polyurea-based layers are compatible or identical.
11. Tank according to at least one of the preceding claims, characterized in that at least one hardener is chosen from polymers of alpha-hydro-omega-hydroxypoly [oxy(methyl-1,2-ethanediyl)] with 1,1'-methylenebis[isocyanatobenzene], the reaction mass of 4,4'-methylenediphenyl diisocyanate (MDI) and o-(isocyanatobenzyl) phenyl isocyanate, 4,4'-methylenediphenyl diisocyanate (MDI) and oligomers of 4,4'-methylenediphenyl diisocyanate (MDI).
12. Tank according to at least one of the preceding claims, characterized in that at least one polyurea-based layer is obtained from a resin chosen from the group consisting of polyoxypropylenediamine, diethylmethylbenzenediamine, glyceryl poly(oxypropylene)triamine, polyalkylamine, polyarylamine and that at least one polyurea-based layer is obtained from a resin chosen from the group consisting of diethylmethylbenzenediamine and oleylamine derivatives.
13. A method of preparing a tank according to any one of the preceding claims, comprising the following steps: a) obtaining a mandrel b) winding a composite reinforcing structure around at least a portion of the mandrel to obtain a hollow body c) forming on at least a portion of the surface of the composite reinforcing structure a protective coating comprising the steps of cl) depositing on at least a portion of the composite reinforcing structure a mixture (D) of at least one resin and at least one hardener as defined in one of the preceding claims, the stoichiometric ratio between the resin and the hardener being between 2:1 and 1:2, and polymerizing the mixture (D) to obtain a first protective layer based on polyurea c2) depositing on at least a portion of the surface of the hollow body coated with a protective layer obtained at the end of step cl),of a mixture (I) of at least one resin, at least one hardener and at least one, fire retardant agent as defined in one of the preceding claims, the stoichiometric ratio between the resin and the hardener being between 2:1 and 1:2, preferably 1:1 and polymerization of the mixture (I) to obtain a second protective layer based on polyurea at least one resin of the mixture (D) being different from at least one resin of the mixture (I).
14. A method of preparing a tank according to claim 13, characterized in that it comprises the following steps a) obtaining a mandrel which is a liner b) winding a composite reinforcing structure around at least a portion of said liner to obtain a hollow body c) forming on at least a portion of the surface of the composite reinforcing structure a protective coating comprising the steps of cl) depositing on at least a portion of the composite reinforcing structure a mixture (D) of at least one resin and at least one hardener as defined in one of the preceding claims, the stoichiometric ratio between the resin and the hardener being between 2:1 and 1:2, and polymerizing the mixture (D) to obtain a first protective layer based on polyurea c2) depositing on at least a portion of the surface of the hollow body coated with a protective layer obtained at the end of step cl),of a mixture (I) of at least one resin, at least one hardener and at least one fire retardant as defined in one of the preceding claims, the stoichiometric ratio between the resin and the hardener being between 2:1 and 1:2, preferably 1:1 and polymerization of the mixture (I) to obtain a second protective layer based on polyurea, at least one resin of the mixture (D) being different from at least one resin of the mixture (I).,
15. Method for preparing a tank according to at least one of claims 13 or 14, characterized in that steps c1 and c2 are carried out successively, and in that the polyurea-based protective layer obtained from the mixture (I) is located outside the coating.
16. Method for preparing a reservoir according to at least one of claims 13 to 15, characterized in that at least one additional step- method of depositing a mixture of at least one resin and at least one hardener is carried out between steps cl) and c2).
17. Vehicle comprising a tank according to at least one of claims 1 to 12.
Citation Information
Patent Citations
Self Healing Coating System for Use With Fuel Tanks
US20130153458A1
Plastic inner container hydrogen storage bottle wound by fibers and provided with polyurea coating
CN114636095A
Coating compositions comprising polyurea and graphite
US20110313084A1
Container for pressurized gas
US20170307139A1