Rubber material and method of making
A rubber material formulated with saturated polyolefins, curatives, and cross-linking agents addresses the stability and adhesion issues of EPDM and TPV materials, offering improved UV resistance and binder compatibility for outdoor flooring applications.
Patent Information
- Application Number
- GB2024004329
- Authority / Receiving Office
- GB · GB
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-03-30
- Filing Date
- 2024-03-26
- Publication Date
- 2024-11-13
AI Technical Summary
Rubber materials used for outdoor flooring, such as EPDM and TPV, face issues like degradation in extreme UV conditions, chalking, embrittlement, and poor adhesion with polyurethane binders due to incompatibility, leading to increased binder usage and UV degradation of polypropylene.
A rubber material composed of a saturated polyolefin, a curative, and a cross-linking agent, which includes a copolymer of ethene and another olefin, a radical forming compound, and a functional group-containing cross-linking agent, along with pigments and light stabilizers, is developed to enhance stability and adhesion.
The solution provides improved UV stability, reduced binder usage, and enhanced adhesion with polyurethane binders, preventing melting and coalescence, thus maintaining material integrity and appearance under outdoor conditions.
Abstract
Description
The present invention relates to rubber material and method of making, suitable for use in, though not exclusively, outdoor flooring. BACKGROUND Rubber materials have been used to make ground surfacing material by being bound by a binding agent, usually a polyurethane prepolymer. Previously used rubber particles have included Ethylene Propylene Diene Monomer (EPDM), and Thermoplastic elastomer Vulcanizate (TPV). EPDM is a polymeric material that has many applications including within the automotive industry, as well as in the building and construction industries. EPDM has also been used as a ground surfacing material, employed, for example, in playgrounds and running tracks. Problems with EPDM include degradation in extreme UV weather conditions, as well as chalking and embrittling of the material. EPDMs can also require significant amounts of binder when being used as flooring, due to the surface porosity of the material. TPV has also been used as a ground surfacing material. TPVs typically consist of two phases, a first rubber phase such as dynamically vulcanised EPDM, within a second thermoplastic polyolefin phase, which may be polypropylene, for example. The vulcanised EPDM is usually crosslinked with peroxide or sulphur within an extruder during production. The level of crosslinking is quite low and so the resulting TPV can soften quite readily and melt. This can cause permanent compression when used in hot climates, which is undesirable for applications such as playground flooring. For applications such as ground surfaces, polyurethane binders are used to bind the rubber granules. Because the rubber phase of a TPV is contained within the polyolefin phase, any polyurethane binder added tends to come into contact with the polyolefin, rather than the rubber phase. Commonly used polypropylene is known to have poor compatibility with polyurethanes. This means that the binder has poor adhesion to the TPV material, and more polyurethane is used to attempt to mitigate the incompatibility. Polypropylene is also degraded by UV light more easily than other polymers and over time, UV light weakens the material. Light stabilisers have previously been added to TPV materials to protect them, but this can be expensive and as a result, often fewer light stabilisers are added than are required for full protection. Embodiments of the present invention aim to provide a rubber material, wherein the aforementioned problems are at least addressed. According to one aspect of the present invention, a rubber material is obtainable by mixing - a saturated polyolefin; - a curative; and - a cross-linking agent. The saturated polyolefin may consist of a single-phase 2 polyolefin. The saturated polyolefin may comprise a copolymer of ethene and a further olefin, preferably not polypropylene. Preferably, the further olefin is a C4-C12 olefin, examples being butene, pentene, hexene, heptane, octene, nonene, decene, undecane, dodecane. More preferably, the saturated polyolefin comprises 90-95% by weight ethene, and 5-10% by weight of the further olefin. The ratio between ethene and the further polyolefin may be between 9:1 and 19:1. Preferably the rubber material comprises 10-20% saturated polyolefin by weight. Preferably, the rubber material comprises 5-30% saturated polyolefin by weight. More preferably, the rubber material comprises 10-25% saturated polyolefin by weight. Even more preferably, the rubber material comprises 15-20% saturated polyolefin by weight. The curative may comprise a radical forming compound. The radical forming compound may be any one of a peroxide, a halogen, or an azo compound. Where the radical forming compound is a peroxide, the peroxide may be an organic peroxide. The organic peroxide may be any one of: a hydroperoxide, a dialkyl peroxide, a peroxy ester, a diacyl peroxide, or a peroxycarboxylic acid. Preferably, the rubber material comprises 0.25-2% curative by weight. More preferably, the rubber material comprises 0.5-1.75% curative by weight. Even more preferably, the rubber material comprises 0.75-1.25% curative by weight. Curative may be present in a sufficient amount to substantially vulcanize the polyolefins. The cross-linking agent may comprise any of triallyl cyanurate, triallyl-isocyanurate, trimethylallyl isocyanurate, trimercapto-triazine, trimethylolpropane trimethacrylate, or an unsaturated polyolefin. Where the cross-linking agent is an unsaturated polyolefin, the unsaturated polyolefin may be any of polybutadiene, polypentadiene, or polyhexadiene. Preferably, the crosslinking agent contains at least one functional group. The functional group may be, for example, any of a carboxylic acid, an amine, a hydroxyl, a nitrile, a ketone, an ether, or an imine. Preferably, the cross-linking agent has a 1,2-vinyl moiety. Preferably, the rubber material comprises 0.5-2.5% cross-linking agent by weight. More preferably, the rubber material comprises 1-2% cross-linking agent by weight. Even more preferably, the rubber material comprises 1.5-1.75% cross-linking agent by weight. The rubber material may comprise at least one colorant. The colorant may be organic or inorganic. Preferably, the colorant is a pigment. The pigment may be in the form of a masterbatch, in which a proportion of a saturated polyolefin has been mixed with the pigment to provide an easily measurable source of pigment in the polymer. The pigment may be a powder. Alternatively, the pigment may be a liquid masterbatch and dispersed in oil. In embodiments of this invention the rubber material may contain a colorant which comprises a primary colour, or a black colorant, or a white colorant, or any mixture of said colorants . In embodiments of this invention the rubber material may comprise a primary colour, or a secondary colour, or a tertiary colour, or black, white or grey. In an embodiment of this invention the rubber material may comprise a red colorant, and the rubber material may be red or may have a red component. For example it may be red, pink, or orange, or red-orange, or red-brown. In an embodiment of this invention the rubber material may comprise a yellow colorant, and the rubber material may be yellow or have a yellow component. For example it may be yellow, or green, or orange. In an embodiment of this invention the rubber material may comprise a blue colorant and the rubber material may be blue or have a blue component. For example it may be blue, or green, or turquoise. In an embodiment of this invention the rubber material may comprise a green colorant and the rubber material may be green or have a green component. For example it may be green, or yellow-green, or turquoise. In an embodiment of this invention the rubber material may comprise a black colorant and the rubber material may be black or have a black component. For example it may be black, or grey, or brown. In an embodiment of this invention the rubber material may comprise a white colorant and the rubber material may be white or have a white component. For example it may be or white, or pink, or sky blue, or pale green, or pale yellow, or grey. In the context of this specification white includes colours that may often be considered as "off-white", and which may have various names, for example cream, eggshell, ivory, Navajo white, vanilla etc. A preferred colorant used in this invention is a pigment. A pigment is a particulate material used to change the visual appearance of an object or substrate. A pigment may be a powder in dry form, or may be in the form of a suspension in a liquid carrier, for example to form a masterbatch. A pigment can be formed by a dye carried by a particulate base, for example by adsorption. The colorant may be a red pigment or a red-containing pigment. Examples include cobalt phosphate, iron reds (including Indian red, haematite), quinacridone violet and vermilion. Red lakes are examples of red dyes carried by particulate bases, thereby forming pigments; examples of red dyes include madder, kermes, lac, carmine, brazil wood and alizarin, and these may be respectively fixed on particulate bases, for example comprising barytes, barium sulphate, barium carbonate, aluminium hydroxide, alum and chalk. The colorant may be a green pigment or a green-containing pigment. Examples include cobalt green (which may also be called Rinmann's green or zinc green, phthalocyanine green, emerald green, green verditer, malachite, copper resinate, dioptase, verdigris, opaque green oxide of chromium, terre verte and viridian. The colorant may be a yellow pigment or a yellow-containing pigment. Examples include aureolin, barium chromate, Indian yellow and iron yellows (which may also be called yellow ochre, or raw sienna or umber). Yellow lakes are examples of yellow dyes carried by particulate bases; examples of the red dyes include Auramine and Thioflavine T, and these may be respectively fixed on particulate bases, for example comprising barytes, barium sulphate, barium carbonate, aluminium hydroxide, alum and chalk. The colorant may be a blue pigment or a blue-containing pigment. Examples include phthalocyanine blue, Prussian blue, cobalt blue, ultramarine, Egyptian blue, indigo, aerinite, azurite, blue verditer, cerulean blue, manganese blue, maya blue, smalt, verdigris and vivianite. The colorant may be a white pigment or a white-containing pigment. Examples include barytes, barium sulphate, calcium carbonate, silica, diatomaceous earth, glass, gypsum, starch, titanium dioxide, witherite and zinc oxide, fluorite and smalt. The colorant may be a purple or violet pigment. Examples include cobalt phosphate, quinacridone violet and fluorite. The colorant may be black or brown pigment. Examples of black or brown pigments include charcoal, coal, galena, graphite, ivory and bone black, pyrolusite, smoke blacks, stibnite and umber. Typically a black or brown pigment is carbon-based. The rubber material of this invention may be used for outdoor flooring, for example to surface children's playgrounds. The rubber material may be supplied in bags (or other suitable containers) of different colours, ready to be applied to a surface in a pre-determined pattern. In accordance with a further aspect of the invention there is provided a plurality of containers (for example bags, or drums) of rubber material of the invention, in different colours. Suitably the containers provided are those needed for an intended surfacing operation. Typically the set may comprise rubber material of at least two colours, preferably of at least three colours, and in some embodiments of at least four colours; in each case preferably selected from black, blue, yellow, red and green. Preferably, the rubber material comprises 1-5% pigment by weight. More preferably, the rubber material comprises 2-4% pigment by weight. Even more preferably. The rubber material comprises 2.5-3.5% pigment by weight. The rubber material may comprise an antioxidant. Preferably the antioxidant is a phenolic antioxidant. The antioxidant may be any of a flavonoid, a phenolic acid, or a phenolic ester. Preferably, the rubber material comprises 0.01-0.1% antioxidant by weight. More preferably, the rubber material comprises 0.03-0.08% antioxidant by weight. Even more preferably, the rubber material comprises 0.05-0.07% antioxidant by weight. The rubber material may comprise a filler. Preferably the filler is a reinforcing filler. Preferably the rubber material comprises 50-80% filler by weight. More preferably, the rubber material comprises 55-75% filler by weight. Even more preferably, the rubber material comprises 60-65% filler by weight. Preferably, the filler is in powder form. The filler may comprise any of a clay, a silica, a silicate, talc, wollastonite, mica, kaolin, carbon black, dolomite, barium sulfate, Al(OH)3, Mg(OH)2, diatomaceous earth, magnetite / hematite, halloysite, zinc oxide, titanium dioxide, and calcium carbonate. The rubber material may comprise a light stabiliser. The light stabiliser may comprise hindered amine light stabilisers (HALS)or Ultraviolet light Absorbers (UVAs). Preferably, the rubber material comprises 0.3-0.6% light stabiliser by weight. More preferably, the rubber material may comprise 0.4-0.55% light stabiliser by weight. Even more preferably, the rubber material may comprise 0.45-0.5% light stabiliser by weight. The rubber material may comprise a lubricant. Preferably the lubricant is any of: paraffinic process oil, refined oil, hydrotreated oil, and mineral oil. Preferably, the rubber material comprises 10-20% by weight lubricant. More preferably, the rubber material comprises 12-18% lubricant by weight. Even more preferably, the rubber material comprises 14-16% lubricant by weight. The rubber material may be granular. The rubber material may be formed into a rubber surfacing material. This may be achieved by mixing the granular rubber material with a polyurethane binder. This may be promoted by treating the granular rubber material with an adhesion promoter. The adhesion promoter may promote adhesion of the polyurethane binder to the granular rubber material. The adhesion promoter may comprise a polyol. Preferably, the polyol may comprise at least one of: a polycarbonate, aliphatic polyester, aromatic polyester, polytetramethylene ether glycol, polytetrahydrofuran, 9 polycaprolactone, acrylic, and polyether. More preferable, the polyol comprises a modified polyether polyol. The modified polyether polyol may comprise polyharnstoff (polyurea) dispersion polyols, polyisocyanate polyaddition polyols, or styrene-acrylonitrile polyols. Addition of the adhesion promoter may occur during manufacture of the rubber material, or in situ during application. According to one aspect of the present invention, there is provided a method of preparing a rubber material, obtainable by compounding - a saturated polyolefin; - a curative; and - a cross-linking agent. Preferably, the saturated polyolefin is extruded with at least one of: -a cross-linking agent, -a filler, -pigment, -light stabiliser, -antioxidant, and -a lubricant. at between 130-160°C. Preferably, the mixture is continuously extruded. Preferably, the mixture is extruded in a twin screw extruder . The extruded material may chen be mixed with the curative at a temperature of between 140-150°C. The mixture may then be then heated at a temperature of 190-210°C and pressed. The resulting rubber material may then be cooled. The rubber material may be granulated in a granulating step . According to another aspect of the present invention, there is provided a method of making a rubber surfacing material onto a ground surface, wherein the rubber surfacing material comprises a rubber material comprising: - a saturated polyolefin; - a curative; and - a cross-linking agent, wherein the rubber material is mixed at room temperature with a polyurethane binder in situ. The method may further comprise the step of applying the rubber surfacing material to a surface. According to a further aspect of the present invention, there is a flooring comprising a rubber surfacing material, wherein the rubber surfacing material comprises - a saturated polyolefin; - a curative; and - a cross-linking agent, and any of: - a filler, -pigment, -Light stabilizer, -antioxidant, -lubricant, -polyurethane binder. The invention may include any combination of the features or limitations referred to herein, except such a combination of features as are mutually exclusive, or mutually inconsistent. The present invention is defined in the attached independent claims, to which reference should now be made. Further, preferred features may be found in the sub-claims appended thereto. The invention is further described in the following, nonlimiting examples. Example 1 An example composition of the rubber material is as follows : 15.66% Ethylene-octene copolymer (95% ethylene - 5% octene) 1.05% Di (tert-butylperoxyisopropyl) benzene, a curative 0.65% TAC-70 ™, a grade of triallyl cyanurate cross-linking agent 59.93% Calcium carbonate powder 2.73% Chrome Oxide pigment powder (green colour) 0.45% 2-hydroxy-4-methoxybenzophenone-5-sulfonic acid 0.09% Irganox 1010 ™, a grade of phenolic antioxidant 19.44% Paraffinic process oil The ethylene-octene copolymer is extruded with TAC-70 ™, catechin, paraffinic process oil, 2-hydroxy-4-methoxybenzophenone-5-sulfonic acid, calcium carbonate, and chrome oxide pigment in a twin extruder. Di(tert- butylperoxyisopropyl) benzene is then added to the extrudate at a temperature of 145°C . The mixture is then advanced through an oven at 210°C and is pressed. The resulting rubber material is cooled in a water bath, and then granulated. Example 2 A further example composition of the rubber material is as follows : 15.23% Ethylene-hexene copolymer (92% ethylene - 8% hexene) 0.86% 2,5-Dimethyl-2,5-di(tert-butylperoxy)hexane, a curative 1.05% Ricon ™, a polybutadiene cross-linking agent 58.35% Kaolin 5.16% Masterbatch pigment (2% ethylene-hexene copolymer-3.16% pigment) 0.56% 4-Amino-2,2,6,6-tertramethylpiperidine 0.94% benzenepropanoic acid, 3-5-bis (1,1-dimethyl-ethyl) - 4-hydroxy-.C7-C9 branched alkyl esters 17.85% Process oil The process of making is the same as in Example 1. Example 3 A further example composition of the rubber material is as follows : 16.38% Ethylene-butene copolymer (94% ethylene - 6% butene) 0.23% Dibenzoyl peroxide, a curative 0.55% Hydroxyl-terminated polybutadiene 67.42% Al(OH)3 2.18% Alizarin (pigmented, red colour) 0.42% Bis (2,2, 6, 6-tetramethyl-4-piperidyl) sebaceate 0.18% Glabridin 12.64% Mineral oil The process of making is the same as in Example 1. Table 1 Ex. 1 Ex. 2 Ex. 3 Cl C2 C3 % organic 39.33 39.95 31.78 40.56 32.8 56.61 % inorganic 60.67 60.05 68.22 59.44 67.2 43.39 Table 1 shows a comparison of percentage of organic and inorganic matter in each example and comparison materials, comparison 1 (Cl), comparison 2 (C2), and comparison 3 (C3), competitor EPDM samples. The colour change after exposure to UV light as according to grey scale test method: EN 20105-A02 was measured. The scale is from 1 to 5, wherein a measurement of 1 means most colour difference, and a measurement of 5 means no difference in colour. The colour fastness of from the rubber material of examples of the present invention consistently gave results of 5, whereas Cl, C2, and C3 gave results of 2, 1, and 4-5 respectively. However, there is no observable trend between the percentage of organic and inorganic components. The competitor EPDM samples are of known organic content, but full composition information is unknown. The rubber material according to one embodiment of the present invention comprises a single-phase polyolefin elastomer, that is substantially fully cross linked with peroxide. The material is fully vulcanized and so, is a thermoset rubber. This is advantageous because the rubber material both with and without the adhesion promoter and binder does not melt or coalesce. The material being a single phase means that there is very good adhesion to polyurethane binders, which are typically added when making a flooring. There is no polypropylene in the material and so, along with adhesion to binders, other issues associated with the use of polypropylene are also mitigated. The material has enhanced UV stability, which is advantageous for when the material is used as an outdoor surface. Further, the material has ample light stabilizer. Whilst endeavouring in the foregoing specification to draw attention to those features of the invention believed to be of particular importance, it should be understood that the applicant claims protection in respect of any patentable feature or combination of features referred to herein, and / or shown in she drawings, whether or not particular emphasis has been placed thereon.
Claims
A rubber material obtainable by mixing:a saturated polyolefin;a curative; anda cross-linking agent.A rubber material according to Claim 1, whereinthe saturated polyolefin comprises at least one of a copolymer of ethene and a C4-C12 alkene, preferably one of butene or octene.A rubber material according to any precedingclaim, wherein the rubber material comprises 5-30% saturated polyolefin by weight.A rubber material according to any precedingclaim, wherein the curative comprises any of a peroxide, a halogen, or an azo compound.A rubber material according to any precedingclaim, wherein the rubber material comprises 0.25-2% curative by weight.A rubber material according to any precedingclaim, wherein the cross-linking agent is any of polybutadiene, polypentadiene, or polyhexadiene, and preferably contains at least one functional of a carboxylic acid, an amine, a hydroxyl, a nitrile, aketone, an ether, or an imine.A rubber material according to any precedingclaim, wherein the rubber material comprises 0.5-2.5% cross-linking agent by weight.A rubber material according to any precedingclaim, wherein the rubber material comprises at least one pigment.A rubber material according to claim 8, whereinthe pigment is selected from a red pigment, a blue pigment, a yellow pigment and a green pigment.
10. A rubber material according to Claim 8 or 9, wherein the rubber macerial comprises 1-5% pigment by weight.
11. A rubber material according to any preceding claim, wherein the rubber material comprises antioxidant.12 . A rubber material according to Claim 11, wherein the rubber material comprises 0.01-0.1% antioxidant by weight.
13. A rubber material according to any precedingclaim, wherein the rubber material comprises afiller .
14. A rubber material according to Claim 13,wherein the rubber material comprises 50-80% fillerby weight.
15. A rubber material according to any preceding claim, wherein the rubber material comprises a light stabilizer, wherein the rubber material preferably comprises 0.3-0.6% light stabiliser by weight.
16. A rubber material according to any preceding claim, wherein the rubber material comprises a lubricant, wherein the rubber material preferably comprises 10-20% lubricant by weight.
17. A rubber material according to any precedingclaim, wherein the rubber material is a granularmaterial.
18. A rubber material according to Claim 17,wherein the granular material is mixed with anadhesion promoter.
19. A rubber material comprising a rubber materialaccording to claim 18, wherein the adhesion promoteris a polyol.2 0 . A plurality of packaged rubber materials each of which is as claimed in any preceding claim, andwhich are of different colours.2 1 . A consolidated material comprising a rubber material according to any preceding claim and a polyurethane binder.2 2 . A method of producing a rubber material, the rubber material obtainable by mixing:- a saturated polyolefin- a curative; and- a cross-linking agentwherein the method comprises the steps of continuously extruding the saturated polyolefin with at least one of:- a cross-linking agent, a filler, pigment, light stabiliser, antioxidant, and a lubricant, extruding the resulting material, then heating the resulting material with the curative to form the rubber material.2 3 . A method of producing a rubber material according to Claim 22, wherein the rubber material is granulated in a granulating step.2 4. A method employing a rubber material onto a playground surface, wherein the rubber material comprises :a saturated polyolefin;a curative; anda cross-linking agent,the method comprising the step of adding at least one of:- a polyether polymer polyol, and- polyurethane binderto the rubber material to form a consolidated material.2 5 . A method as claimed in claim 24, wherein a plurality of containers of rubber material is supplied to a site co be surfaced, wherein the containers of rubber material are provided in a plurality of different colours.
Citation Information
Patent Citations
Vulcanized POE waterproofing coil material and production method thereof
CN108546358A
Functionally graded materials, preparation methods of sole substrates and shoes
CN109111636B
Antibacterial and anti-aging denture soft lining material
CN109646313A
Thermoelastic composition of ethylene-1-olefin copolymer and rubber
US4978717A
Fluid and heat resistant chlorinated polyethylenes (CPE)
US7754816B2