Electrochemical cell, current collector, and cell stack
The integration of a gas flow suppressor with a higher expansion coefficient than the electrode stack materials in electrochemical cells addresses gas bypass and leakage issues, ensuring efficient gas utilization and preventing deformation by thermal expansion-based sealing.
Patent Information
- Application Number
- JP2023043298
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-17
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2043-03-17
AI Technical Summary
Gas flow bypassing or leaking from the reaction region in electrochemical cells, leading to reduced gas utilization and potential deformation or damage due to internal stress and dimensional variations, especially in high-temperature solid oxide cells.
Incorporation of a gas flow suppressor made of a material with a higher linear expansion coefficient than the electrode stack, positioned to prevent gas flow between the electrode stack and its surrounding frame, and designed to thermally expand and seal the gap at operating temperatures.
Effectively suppresses gas flow and enhances sealing performance, preventing deformation and internal stress in the electrochemical cell while maintaining efficient gas utilization.
Smart Images

Figure 2024132507000001_ABST
Abstract
Description
[Technical field]
[0001] SUMMARY OF THE DISCLOSURE Embodiments of the present invention relate to electrochemical cells, current collectors, and cell stacks. [Background technology]
[0002] There are various types of electrochemical cells, such as solid polymer type and solid oxide type. Solid oxide electrochemical cells use solid oxide as an electrolyte, and therefore have a high operating temperature (for example, 600 to 1000°C). By operating at such a high operating temperature, solid oxide electrochemical cells can obtain a high reaction rate without using expensive precious metal catalysts.
[0003] By obtaining a high reaction rate as described above, when a solid oxide electrochemical cell is operated as a fuel cell (solid oxide fuel cell: SOFC), high power generation efficiency can be obtained. Furthermore, when a solid oxide electrochemical cell is operated as an electrolysis cell (solid oxide electrolysis cell: SOEC), for example, hydrogen can be produced highly efficiently at a low electrolysis voltage. For this reason, solid oxide electrochemical cells have attracted attention as a technology for realizing highly efficient fuel cells, electrolysis cells for hydrogen production, and power storage systems that combine these, and their development is underway.
[0004] An electrochemical cell includes a laminate (hereinafter sometimes referred to as an electrode laminate) including at least a cathode, an electrolyte, and an anode. The cathode, electrolyte, and anode are usually made of materials having different properties. The cathode and anode are electrical conductors, and are generally made of porous materials. Different gases are supplied to the cathode and anode, with the electrolyte as a boundary therebetween. On the other hand, the electrolyte is an ion conductor.
[0005] Electrochemical cells come in various shapes, such as flat plate type, cylindrical type, cylindrical flat plate type, etc. For example, in a flat plate type electrochemical cell, an air electrode, an electrolyte, a fuel electrode, etc. are laminated in a flat plate shape.
[0006] A structure in which multiple electrochemical cells are integrated to generate a large amount of electricity or hydrogen is generally called a cell stack. For example, in a cell stack including multiple flat electrochemical cells, the multiple electrochemical cells are stacked with their thickness directions aligned. A corresponding gas is supplied to the air electrode and fuel electrode of each electrochemical cell, and each electrochemical cell is electrically connected in series. The electrochemical cells that make up the cell stack usually include a separator. In the cell stack, an electrochemical cell is stacked with other electrochemical cells so that its separator is in contact with the other electrochemical cells. In such a configuration, the gas flow path of each electrochemical cell is separated by a separator. The separator is conductive and also plays a role in electrical conduction with other electrochemical cells.
[0007] The above-mentioned separator includes a separator that defines a gas flow path to either the air electrode or the fuel electrode by, for example, a plate-shaped base portion that contacts the electrode stack in the stacking direction (thickness direction) of the electrochemical cell, and a frame that surrounds the periphery of the electrode stack. In a separator configured in this manner, a gas supply path and an exhaust path may be formed in the frame. In this case, the gas that flows into the frame from the supply path is supplied to the air electrode or the fuel electrode in the electrochemical cell, and the gas that has passed through the air electrode or the fuel electrode is exhausted to the outside from the exhaust path.
[0008] One index for evaluating the performance of the above-mentioned cell stack is the gas utilization rate. For example, when operating in the electrolysis mode to generate hydrogen, the amount of hydrogen produced per unit of electricity is an important index. [Prior art documents] [Patent documents]
[0009] [Patent Document 1] Patent No. 5734823 [Patent Document 2] Patent No. 6172524 [Patent Document 3] Patent Publication No. 2022-24498 Summary of the Invention [Problem to be solved by the invention]
[0010] A part of the gas supplied to the electrochemical cell may be discharged without passing through the reaction region (air electrode and fuel electrode in the electrode stack) of the electrochemical cell. Specifically, for example, a gas flow that tries to bypass the reaction region or a gas flow that leaks out of the reaction region may occur.
[0011] However, gas flow that does not pass through the reaction area does not contribute to the reaction. Therefore, it is desirable to ensure gas sealing properties to prevent gas from bypassing the reaction area or leaking from the reaction area. It is also desirable to ensure suitable gas sealing properties so that gas can flow so that reactions at the air electrode and fuel electrode can be carried out efficiently.
[0012] In the configuration in which a frame is provided surrounding the electrode stack as described above, a gap may be formed between the electrode stack and the frame. In this case, a gas flow that tries to bypass the reaction region may occur in this gap. Here, if the electrode stack and the frame are brought into close contact with each other, the gas flow in the gap may be suppressed. However, due to variations in the dimensional processing accuracy of the electrode stack and the frame, it may be difficult to properly bring the electrode stack and the frame into close contact with each other. In addition, mutual interference may occur due to expansion of the electrode stack and the frame when the temperature rises, and pressure may be generated on the contact surface between the electrode stack and the frame during operation in a high-temperature state, which may cause undesirable internal stress or deformation in the electrochemical cell. If the pressure on the contact surface becomes excessively large, the electrochemical cell may be damaged, in which case the power generation or electrolysis performance may be significantly impaired.
[0013] For the above reasons, it may be necessary to provide a gap between the electrode stack and the frame in the electrochemical cell. In particular, when a solid oxide electrochemical cell is used, mutual interference during expansion is often a problem due to the high operating temperature, and the dimensional processing accuracy of the electrochemical cell (electrode stack and frame) may easily vary due to the forming material used. Therefore, in a solid oxide electrochemical cell, a gap is usually intentionally formed between the electrode stack and the frame. However, if the gap between the electrode stack and the frame is excessively large, the gas utilization rate decreases due to an increase in gas that does not pass through the oxygen electrode or the fuel electrode, which may result in a decrease in power generation or electrolysis performance. If the gas supplied to the reaction region is significantly insufficient from the desired supply amount, the electrochemical cell may be damaged.
[0014] In view of the above, the problem that the present invention aims to solve is to provide an electrochemical cell, a current collector, and a cell stack that can suppress undesirable internal stress and deformation in an electrochemical cell caused by contact between an electrode stack including an oxygen electrode, an electrolyte, and a fuel electrode and its surrounding members, while suppressing the flow of gas between the electrode stack and its surrounding members. [Means for solving the problem]
[0015] An electrochemical cell according to one embodiment comprises an electrode stack including an electrolyte having a first surface and a second surface opposite the first surface, an oxygen electrode in contact with the first surface, and a fuel electrode in contact with the second surface, and a gas flow suppression portion located at least partially adjacent to a side of the electrode stack located between the first surface and the second surface, and formed from a material different from the electrolyte, the oxygen electrode, and the fuel electrode. The current collector in one embodiment is a current collector that is arranged in a direction in which an electrolyte, an oxygen electrode, and a fuel electrode in an electrode stack of an electrochemical cell overlap with each other, and is disposed in contact with the oxygen electrode or the fuel electrode, and is provided with a gas flow suppression portion that is positioned at least partially adjacent to a side surface of the electrode stack. The cell stack according to one embodiment is a cell stack in which a plurality of the electrochemical cells described above are stacked. Effect of the Invention
[0016] According to the present invention, it is possible to suppress undesirable internal stress and deformation in an electrochemical cell caused by contact between an electrode stack including an oxygen electrode, an electrolyte, and a fuel electrode and its surrounding members, while suppressing gas flow between the electrode stack and its surrounding members. [Brief description of the drawings]
[0017] [Figure 1] 1 is a cross-sectional view in a stacking direction of a cell stack including an electrochemical cell according to a first embodiment. [Diagram 2] 2 is a cross-sectional view of the cell stack in the stacking direction corresponding to line II-II in FIG. 1. [Diagram 3] FIG. 3 is a schematic diagram of an electrochemical cell in the cell stack taken along line III-III in FIG. 2. [Figure 4] FIG. 4 is a diagram showing thermal expansion of the electrochemical cell shown in FIG. 3 during operation. [Diagram 5] FIG. 4 is a schematic diagram of an electrochemical cell according to a second embodiment. [Figure 6] FIG. 13 is a schematic diagram of an electrochemical cell according to a third embodiment. [Figure 7] 5(A) to 5(D) are diagrams illustrating an example of a method for manufacturing an electrochemical cell according to an embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0018] Hereinafter, each embodiment will be described with reference to the accompanying drawings. In the drawings accompanying this specification, the scale and dimensional ratio may be changed and exaggerated from those of the actual objects for the convenience of illustration and understanding.
[0019] <First embodiment> FIG. 1 is a cross-sectional view in the stacking direction of a cell stack S including an electrochemical cell 1 according to a first embodiment. FIG. 2 is a cross-sectional view in the stacking direction of the cell stack S corresponding to line II-II in FIG. 1. FIG. 3 is a schematic diagram of the electrochemical cell 1 as viewed from line III-III in FIG. 2. The electrochemical cell 1 is of a flat plate type. In the cell stack S, a plurality of electrochemical cells 1 are stacked on top of each other such that their thickness directions are aligned. Note that FIGS. 1 to 3 show the electrochemical cell 1 and the cell stack S when not in operation and at room temperature (25° C.).
[0020] The direction in which the electrochemical cells 1 are stacked in the cell stack S is hereinafter referred to as the stacking direction Z. Moreover, the direction perpendicular to the stacking direction Z, which extends left and right in Fig. 1, is referred to as the X direction. Moreover, the direction perpendicular to the stacking direction Z, which extends left and right in Fig. 2, is referred to as the Y direction. The X direction and the Y direction are perpendicular to each other in a plane perpendicular to the stacking direction Z.
[0021] In addition, a surface referred to as a side surface in a component of the electrochemical cell 1 or cell stack S described below means an outer surface of the component facing the X direction and / or Y direction. In addition, a plan view in the following means a view in a direction parallel to the stacking direction Z.
[0022] 1 and 2, the electrochemical cell 1 includes an electrode stack 10, a separator 12, a fuel electrode side current collector 14a, an oxygen electrode side current collector 14c, a sealing plate 16, and a sealant 18. The electrode stack 10 may also be simply called a "cell."
[0023] The electrode stack 10 includes an electrolyte 10e, an oxygen electrode 10c, an anode 10a, and an anode porous substrate 10g. The electrolyte 10e has a first surface 10e1 and a second surface 10e2 opposite to the first surface 10e1.
[0024] The oxygen electrode 10c is in contact with the first surface 10e1. The fuel electrode 10a is in contact with the second surface 10e2. The fuel electrode porous substrate 10g is in contact with the surface of the fuel electrode 10a opposite to the surface in contact with the electrolyte 10e. That is, in the electrode stack 10, the fuel electrode porous substrate 10g, the fuel electrode 10a, the electrolyte 10e, and the oxygen electrode 10c are stacked in this order.
[0025] Specifically, the electrochemical cell 1 is a flat plate type having a rectangular shape in a plan view. However, the shape of the flat plate type electrochemical cell 1 in a plan view is not particularly limited, and may be, for example, a circular shape.
[0026] The electrolyte 10e in this embodiment is a solid electrolyte, and is made of a solid oxide having oxygen ion conductivity. In this case, the electrolyte 10e is formed of, for example, dense stabilized zirconia, a compact of a ceria-based solid solution, a perovskite-type oxide, or the like. The electrolyte 10e is made of an oxide of at least one element selected from the group consisting of Y, Sc, Yb, Gd, Ca, Mg, and Ce (Y 2 O 3 ,Sc 2 O 3 ,Yb 2 O 3 ,Gd 2 O 3 ,CaO,MgO,CeO 2 The electrolyte 10e may be formed using zirconia stabilized with Sm, Gd, and Y. The electrolyte 10e may be formed using an oxide of at least one element selected from the group consisting of Sm, Gd, and Y (Sm 2 O 3 ,Gd 2 O 3 ,Y 2 O 3 ) may be formed using doped ceria.
[0027] The oxygen electrode 10c is a porous body and is made of, for example, a perovskite-type oxide, etc. In more detail, the oxygen electrode 10c may be made of, for example, LaSrMn oxide, LaSrCo oxide, LaSrCoFe oxide, LaSrFe oxide, etc.
[0028] The fuel electrode 10a is a porous body, and is formed of, for example, a mixed sintered body (cermet) of a metal and a solid oxide. In particular, the fuel electrode 10a may be formed of, for example, Ni-YSZ (yttria-stabilized zirconia), Ni-ScSZ (scandia-stabilized zirconia), etc. Here, the electrolyte 10e being "dense" as described above means that the electrolyte 10e has a lower porosity than at least the oxygen electrode 10c and the fuel electrode 10a, which are porous bodies.
[0029] The anode porous substrate 10g is also porous and formed in a sheet shape. In this embodiment, the anode porous substrate 10g, the anode 10a, the electrolyte 10e, and the cathode 10c are laminated in this order and integrated together. In this embodiment, the anode porous substrate 10g reinforces the electrode laminate 10 and functions as a support material that supports the electrode laminate 10.
[0030] The electrode stack 10 can be formed, for example, by sequentially depositing the fuel electrode 10a, the electrolyte 10e, and the oxygen electrode 10c on the fuel electrode porous substrate 10g. When the electrode stack 10 is formed by such a process, the fuel electrode porous substrate 10g, the fuel electrode 10a, the electrolyte 10e, and the oxygen electrode 10c are naturally integrated. However, the method of forming the electrode stack 10 is not particularly limited.
[0031] The fuel electrode porous substrate 10g may be formed of, for example, a sintered body containing metal particles and a metal oxide. The metal particles contained in the sintered body or dissolved in the oxide include, for example, one or more selected from the group consisting of nickel (Ni), cobalt (Co), iron (Fe), and copper (Cu), or an alloy containing them.
[0032] Since the electrochemical cell 1 according to the present embodiment is a solid oxide electrochemical cell, it may be made of the materials exemplified above. However, the type of the electrochemical cell 1 is not limited to the solid oxide type. For example, when the electrochemical cell 1 is configured as a solid polymer type or a molten carbonate type electrochemical cell, each part of the electrochemical cell may be made of a material corresponding to the type.
[0033] The separator 12 includes a base portion 121 that overlaps with the electrode stack 10 in the direction in which the electrolyte 10e, the oxygen electrode 10c, and the fuel electrode 10a overlap, that is, in the stacking direction Z, and a frame 122 that surrounds the side surface of the electrode stack 10. In this embodiment, a cell housing portion 12a is formed inside the frame 122. The electrode stack 10 is placed in the cell housing portion 12a. The electrode stack 10 is placed so that each side of the rectangular shape is aligned with one of the sides of the frame 122, and a gap is formed between the side surface of the electrode stack 10 and the frame 122. That is, the electrode stack 10 is surrounded by the frame 122 with a gap between the electrode stack 10 and the frame 122 without being in close contact with the inner surface of the frame 122.
[0034] As shown in Fig. 3, the base portion 121 has a rectangular shape in plan view. The frame 122 has a rectangular frame shape in plan view. As shown in Figs. 1 and 2, the base portion 121 contacts the fuel electrode side current collector 14a via the fuel electrode porous substrate 10g. The surface of the base portion 121 opposite to the surface on the fuel electrode porous substrate 10g side contacts the oxygen electrode side current collector 14c of another electrochemical cell 1.
[0035] The electrochemical cell 1 includes a plurality of flow paths for gas flow. Specifically, as shown in Fig. 1 to Fig. 3, the electrochemical cell 1 includes a shared fuel supply flow path 131, a shared fuel discharge flow path 132, a branched fuel supply flow path 133, a branched fuel discharge flow path 134, a shared oxygen supply flow path 135, a shared oxygen discharge flow path 136, a branched oxygen supply flow path 137, and a branched oxygen discharge flow path 138.
[0036] 3, a shared fuel supply channel 131 is formed on one of two opposing sides (two upper and lower sides in FIG. 3) of the frame 122, and a shared fuel discharge channel 132 is formed on the other of the two sides. A shared oxygen supply channel 135 is formed on one of the other two opposing sides (two left and right sides in FIG. 3) of the frame 122, and a shared oxygen discharge channel 136 is formed on the other of the two sides.
[0037] The shared fuel supply channel 131, the shared fuel exhaust channel 132, the shared oxygen supply channel 135, and the shared oxygen exhaust channel 136 each penetrate the frame 122 in the stacking direction. As shown in Figures 1 and 2, the shared fuel supply channel 131, the shared fuel exhaust channel 132, the shared oxygen supply channel 135, and the shared oxygen exhaust channel 136 are fluidly connected to the corresponding shared fuel supply channel 131, the shared fuel exhaust channel 132, the shared oxygen supply channel 135, and the shared oxygen exhaust channel 136 of another electrochemical cell 1, respectively.
[0038] 1 and 3, the fuel supply branch channel 133 is formed adjacent to the shared fuel supply channel 131 in the frame 122. More specifically, the fuel supply branch channel 133 is formed on the side of the frame 122 where the shared fuel supply channel 131 is formed, and fluidically connects the shared fuel supply channel 131 and the cell accommodating unit 12a. In addition, the fuel discharge branch channel 134 is formed adjacent to the shared fuel discharge channel 132 in the frame 122. More specifically, the fuel discharge branch channel 134 is formed on the side of the frame 122 where the shared fuel discharge channel 132 is formed, and fluidically connects the shared fuel discharge channel 132 and the cell accommodating unit 12a.
[0039] As described above, by connecting the shared fuel supply channel 131, the shared fuel discharge channel 132, the branched fuel supply channel 133, and the branched fuel discharge channel 134, the fuel gas flowing through the shared fuel supply channel 131 can flow from the branched fuel supply channel 133 into the cell accommodating section 12a. This allows the fuel gas to be supplied to the fuel electrode 10a in the electrode stack 10. Then, the fuel gas that has passed through the electrode stack 10 can flow from the cell accommodating section 12a through the branched fuel discharge channel 134 to the shared fuel discharge channel 132. This allows the unreacted fuel gas to be discharged from the shared fuel discharge channel 132.
[0040] In this embodiment, the fuel supply branch channel 133 and the fuel discharge branch channel 134 are formed as grooves recessed from the top surface of the frame body 122 and extending in a direction intersecting the stacking direction. However, the fuel supply branch channel 133 and the fuel discharge branch channel 134 may be holes penetrating the frame body 122. The oxygen supply branch channel 137 and the oxygen discharge branch channel 138 are provided in the sealing plate 16. This will be described in detail later.
[0041] As described above, the separator 12 forms at least a part of the flow path of the fuel gas supplied to the fuel electrode 10a and the flow path of the oxygen supplied to the oxygen electrode 10c. The separator 12 is dense enough to prevent the permeation of the fuel gas and oxygen, and is made of a material having electrical conductivity. The separator 12 is made of, for example, metal, ceramics, etc. It is desirable that the linear expansion coefficient of the material of the separator 12 is close to the linear expansion coefficient of the electrode stack 10. Note that, as described above, the separator 12 being "dense" means that the separator 12 has a lower porosity than at least the oxygen electrode 10c and the fuel electrode 10a, which are porous bodies.
[0042] In the present embodiment, the frame 122 is a part of the separator 12, and the frame 122 stands up integrally with the outer circumferential side portion of the base portion 121. However, the frame 122 and the base portion 121 may be formed separately and connected to each other later.
[0043] The fuel electrode side current collector 14a is disposed in contact with the fuel electrode porous substrate 10g and the base portion 121 of the separator 12. The oxygen electrode side current collector 14c is disposed in contact with the oxygen electrode 10c and the separator 12 of the other electrochemical cell 1. The fuel electrode side current collector 14a may be bonded to the fuel electrode porous substrate 10g and the base portion 121 of the separator 12 via an adhesive. Similarly, the oxygen electrode side current collector 14c may be bonded to the oxygen electrode 10c and the separator 12 of the other electrochemical cell 1 via an adhesive.
[0044] The fuel electrode side current collector 14a and the oxygen electrode side current collector 14c are sheet-like members having electrical conductivity and are formed of an electrically conductive material. The fuel electrode side current collector 14a and the oxygen electrode side current collector 14c may be formed of, for example, stainless steel, iron, nickel, titanium, aluminum, Ag, Pt, Au, or an alloy material containing one or more of these. In particular, the fuel electrode side current collector 14a and the oxygen electrode side current collector 14c may be formed of a structure having gas diffusibility. More specifically, the fuel electrode side current collector 14a and the oxygen electrode side current collector 14c may be formed of a metal mesh, expanded metal, or metal foam that has gas diffusibility and is relatively easy to deform. The material of these meshes, expanded metals, and metal foams may be, as described above, for example, stainless steel, iron, nickel, titanium, aluminum, Ag, Pt, Au, or an alloy material containing one or more of these. Note that gas diffusibility is a property that allows the inflowing gas to diffuse and pass through.
[0045] As shown in Fig. 2, the fuel electrode side current collector 14a is provided with a fuel gas flow channel 24a. As shown in Fig. 1, the oxygen electrode side current collector 14c is provided with an oxygen flow channel 24c. In this example, the fuel gas flow channel 24a and the oxygen flow channel 24c extend in directions perpendicular to each other when viewed in the stacking direction Z. However, the patterns of the fuel gas flow channel 24a and the oxygen flow channel 24c are not particularly limited.
[0046] The fuel electrode side current collector 14a is formed in a corrugated shape with concave and convex portions alternately formed. The fuel gas flow passage 24a is formed between adjacent convex portions of the fuel electrode side current collector 14a that are convex upward in Fig. 2, and extends in the X direction. One end of the fuel gas flow passage 24a in the X direction is fluidly connected to the shared fuel supply flow passage 131 via the cell housing portion 12a and the fuel supply branch flow passage 133, as shown in Figs. 1 and 2. The other end of the fuel gas flow passage 24a in the X direction is fluidly connected to the shared fuel discharge flow passage 132 via the cell housing portion 12a and the fuel discharge branch flow passage 134.
[0047] The oxygen electrode side current collector 14c is also formed in a corrugated shape with concave and convex portions alternately formed. The oxygen flow paths 24c are formed between adjacent concave portions of the oxygen electrode side current collector 14c that is concave downward in Fig. 1, and extend in the Y direction. One end of the oxygen flow path 24c in the Y direction is fluidically connected to the oxygen supply shared flow path 135 via an oxygen supply branch flow path 137, as shown in Figs. 1 and 2. The other end of the oxygen flow path 24c in the Y direction is fluidically connected to the oxygen discharge shared flow path 136 via an oxygen discharge branch flow path 138.
[0048] The fuel electrode side current collector 14a and the oxygen electrode side current collector 14c do not necessarily have to be provided with the fuel gas flow passage 24a and the oxygen flow passage 24c as described above. In this case, for example, the fuel electrode side current collector 14a and the oxygen electrode side current collector 14c may be formed of a porous body, and groove-shaped flow passages such as the fuel gas flow passage 24a and the oxygen flow passage 24c may be formed in the separator 12.
[0049] In this embodiment, the size of the oxygen electrode 10c in a plan view is smaller than that of the electrolyte 10e, and the outer peripheral portion of the electrolyte 10e is not covered by the oxygen electrode 10c. Here, the sealing plate 16 is installed so as to straddle the surface of the electrolyte 10e where the oxygen electrode 10c is not located and the top surface of the frame 122. The sealing plate 16 is a rectangular frame-shaped plate, and surrounds the oxygen electrode 10c and the oxygen electrode-side current collector 14c. Oxygen supplied to the oxygen electrode 10c flows into the inside of the sealing plate 16, but the sealing plate 16 separates the space inside the sealing plate 16 from the gas atmosphere of the cell housing portion 12a.
[0050] As described above, the sealing plate 16 is formed with the oxygen supply branch channel 137 and the oxygen exhaust branch channel 138. For more details, see FIG. 2. The oxygen supply branch channel 137 is formed so as to fluidically connect the shared oxygen supply channel 135 and the space inside the sealing plate 16. The oxygen exhaust branch channel 138 is formed so as to fluidically connect the shared oxygen exhaust channel 136 and the space inside the sealing plate 16. The sealing plate 16 is made of a dense material, and may be made of, for example, metal, ceramics, or the like, or may be made of the same material as the separator 12.
[0051] The sealant 18 is provided between the sealing plate 16 and the separator 12 of the other electrochemical cell 1, and provides an air-tight and liquid-tight seal between the sealing plate 16 and the separator 12 of the other electrochemical cell 1. The sealant 18 may be made of a compressible material that is deformed by the application of pressure.
[0052] In the electrochemical cell 1 according to the present embodiment, the above-described electrode stack 10, separator 12, fuel electrode side current collector 14a, oxygen electrode side current collector 14c, sealing plate 16, and sealant 18 constitute a unitary unit, or so-called single cell. An arbitrary number of such electrochemical cells 1 are stacked up to form a cell stack S. In the cell stack S, end plates (not shown) or the like are disposed at both ends in the stacking direction Z. A pair of end plates or other members are then fastened and fixed by fastening means, for example, a plurality of bolts and nuts (not shown).
[0053] 1 to 3, the electrochemical cell 1 includes a gas flow suppression section 20. The gas flow suppression section 20 is located so as to be adjacent to at least a portion of the side surface of the electrode stack 10. More specifically, the gas flow suppression section 20 in this embodiment is located so as to be adjacent to a portion or all of the side surface of the electrode stack 10 from the surface on the fuel electrode side (the lower surface in the figure) to the electrolyte 10e, and is not adjacent to the oxygen electrode 10c.
[0054] As described above, a gap is formed between the side surface of the electrode stack 10 and the frame 122. The gas flow suppression unit 20 is located in the gap between the side surface of the electrode stack 10 and the frame 122, and thereby functions to block the flow of fuel gas that attempts to pass through the gap between the side surface of the electrode stack 10 and the frame 122.
[0055] The gas flow suppression unit 20 is formed of a material different from the electrolyte 10e, the oxygen electrode 10c, and the fuel electrode 10a. More specifically, the gas flow suppression unit 20 is formed of a material having a linear expansion coefficient larger than that of the electrolyte 10e, the oxygen electrode 10c, and the fuel electrode 10a. As described above, in this embodiment, the electrolyte 10e, the oxygen electrode 10c, and the fuel electrode 10a are mainly formed of ceramics. In contrast, the gas flow suppression unit 20 may be formed of, for example, stainless steel, iron, nickel, titanium, aluminum, Ag, Pt, Au, or an alloy material containing at least one of these. As a result, the linear expansion coefficient of the gas flow suppression unit 20 can be larger than that of the electrolyte 10e, the oxygen electrode 10c, and the fuel electrode 10a.
[0056] Specifically, in this embodiment, the gas flow suppression portion 20 is integrally formed with the fuel electrode side current collector 14a made of metal. That is, the fuel electrode side current collector 14a is provided with the gas flow suppression portion 20 located so as to be at least partially adjacent to the side surface of the electrode stack 10. In addition, in this embodiment, since the fuel electrode side current collector 14a is integrated with the electrode stack 10, the gas flow suppression portion 20 is integrated with the electrode stack 10. Note that the gas flow suppression portion 20 does not have to be integrated with the fuel electrode side current collector 14a, and may be integrated with, for example, the fuel electrode porous substrate 10g. In this embodiment, the gas flow suppression portion 20 is formed from the same material as the fuel electrode side current collector 14a. Therefore, the gas flow suppression portion 20 may be formed from a structure having gas diffusibility. More specifically, the gas flow suppression portion 20 may be formed from a metal mesh, expanded metal, or metal foam that has gas diffusibility and is relatively easy to deform.
[0057] As shown in FIG. 2 and FIG. 3, the gas flow suppression unit 20 is located away from the frame 122 when the electrochemical cell 1 is not operating, for example, at room temperature (25° C.). Here, if the linear expansion coefficient of the gas flow suppression unit 20 is larger than the linear expansion coefficients of the electrolyte 10e, the oxygen electrode 10c, and the fuel electrode 10a, the gas flow suppression unit 20 is likely to expand toward the frame 122 so as to narrow the distance between the gas flow suppression unit 20 and the frame 122 during operation of the electrochemical cell 1. This makes it easier to block the flow of fuel gas passing through the gap between the electrode stack 10 and the frame 122. In addition, as described above, when a member such as the gas flow suppression unit 20 that blocks the flow of fuel gas is appropriately formed with high processing accuracy from the same material as the electrode stack 10, which is mainly made of ceramics, it may take a lot of time. Therefore, forming the gas flow suppression unit 20 from a material different from the electrolyte 10e, the oxygen electrode 10c, and the fuel electrode 10a may be advantageous in terms of processing the gas flow suppression unit 20.
[0058] More specifically, the gas flow suppression portion 20 in this embodiment has a convex shape protruding from the electrode stack 10 toward the frame 122 as shown in Fig. 4. As an example, the gas flow suppression portion 20 is a rectangular plate with a constant thickness, and the plate surface is formed along the stacking direction Z. In this embodiment, a plurality of gas flow suppression portions 20 are provided at intervals along a direction going around the side surface of the electrode stack 10. More specifically, a plurality of gas flow suppression portions 20 are provided at intervals along a portion of the side surface of the electrode stack 10 that is parallel to the fuel gas flow path 24a of the fuel electrode side current collector 14a.
[0059] It is desirable that adjacent gas flow suppression units 20 are spaced apart to a certain extent so that fuel gas flows between them, causing a switch from abrupt contraction to abrupt expansion and resulting in pressure loss. It is also desirable that the gas flow suppression units 20 are configured so that a vortex is generated when fuel gas flows between adjacent gas flow suppression units 20.
[0060] Furthermore, this embodiment is intended to cause the gas flow suppression part 20 to expand toward the frame 122 so as to narrow the distance between the gas flow suppression part 20 and the frame 122 during operation of the electrochemical cell 1. In other words, the gas flow suppression part 20 is configured to come into contact with or approach the frame 122 due to thermal expansion when the gas flow suppression part 20 reaches or exceeds a predetermined temperature.
[0061] Specifically, the gas flow suppression unit 20 is located in the gap between the electrode stack 10 and the frame 122 so as to be separated from the frame 122 when the electrochemical cell 1 is not operating at room temperature (25° C.), in other words, during assembly. As described above, the linear expansion coefficient of the gas flow suppression unit 20 is set to be larger than the linear expansion coefficients of the electrolyte 10e, the oxygen electrode 10c, and the fuel electrode 10a, and is also set to be larger than the linear expansion coefficient of the frame 122. In detail, as an example, the linear expansion coefficients of the gas flow suppression unit 20 and the frame 122 are set so that the difference between the dimension in which the gas flow suppression unit 20 expands at a predetermined temperature and the dimension in which the frame 122 expands at a predetermined temperature is equal to or larger than the distance between the gas flow suppression unit 20 and the frame 122 at room temperature. As a result, as shown in FIG. 4, the gas flow suppression unit 20 may come into contact with the frame 122 due to thermal expansion when the temperature reaches or exceeds a predetermined temperature.
[0062] Explaining in detail with reference to FIG. 3, the reference character L1 in FIG. 3 indicates the distance between the inner faces of the mutually opposing frames 122. The reference character L2 indicates the distance between the tips of the gas flow suppressing parts 20 provided on the mutually opposing edges of the fuel electrode side current collector 14a. Here, the distance between the gas flow suppressing parts 20 and the frame 122 at room temperature is calculated by ((L1-L2) / 2). In this embodiment, the linear expansion coefficients of the gas flow suppressing parts 20 and the frame 122 are set so that the relationship ((L1-L2) / 2)-(c1×L1-c2×L2)×(Td-Ts)≧0 holds, where c1 is the linear expansion coefficient of the frame 122, c2 is the linear expansion coefficient of the gas flow suppressing parts 20, Td is the predetermined temperature, and Ts is the room temperature.
[0063] When the gas flow suppression portion 20 is thermally expanded to contact the frame 122 as described above, it is preferable that the gas flow suppression portion 20 is structured such that deformation is permitted or buckling can easily occur even when the gas flow suppression portion 20 contacts the frame 122 under high-temperature operating conditions, and that the gas flow suppression portion 20 does not restrict deformation of the electrode stack 10 or transmit a load to the electrode stack 10. From this perspective, the gas flow suppression portion 20 is a structure having gas diffusibility and is preferably formed from a metallic mesh, expanded metal, or metallic foam that is relatively easily deformed, and nickel foam is particularly preferable, for example.
[0064] In addition, the gas flow suppression unit 20 is separated from the frame 122 when the electrochemical cell 1 is not operating, for example, at room temperature (25° C.), in other words, during assembly, so that it does not hinder the assembly of the frame 122 and the electrode stack 10. In addition, in this embodiment, as shown in FIG. 1 and FIG. 2, the top surface of the gas flow suppression unit 20 (the surface facing the sealing plate 16) is also located so as to be separated from the sealing plate 16 when the electrochemical cell 1 is not operating, for example, at room temperature (25° C.). It is desirable that the top surface of the gas flow suppression unit 20 is also formed so as to be separated from the sealing plate 16, in other words, not to exceed the electrolyte 10e, in order to avoid any influence on proper assembly. On the other hand, even when the top surface of the gas flow suppression unit 20 is separated from the sealing plate 16 in this way, the gas flow suppression unit 20 may approach the sealing plate 16 due to thermal expansion at high temperatures. Therefore, the flow of the fuel gas can be suitably suppressed.
[0065] Next, the operation of the electrochemical cell 1 according to this embodiment will be described.
[0066] When the cell stack S is operated as an SOEC (Solid Oxide Electrolysis Cell), a fuel gas is introduced from the outside into the shared fuel supply channel 131. When the cell stack S is operated as an SOEC, for example, a gas containing at least water vapor or carbon dioxide can be used. This fuel gas flows into the cell housing portion 12a from the fuel supply branch channel 133. The fuel gas then passes through the fuel gas channel 24a of the fuel electrode side current collector 14a, where it is diffused in the fuel electrode porous substrate 10g and supplied to the fuel electrode 10a in the electrode stack 10. As a result, the fuel gas is used as a reactant for the electrolysis reaction in the electrode stack 10. The fuel gas that is not used as a reactant for the electrolysis reaction is discharged to the outside via the fuel supply branch channel 133 and the fuel discharge branch channel 134.
[0067] In this embodiment, a gap is formed between the electrode stack 10 and the frame 122, and the fuel gas tries to pass through this gap. By providing the gas flow suppression unit 20 here, the flow of the fuel gas through the gap is suppressed. Particularly in this embodiment, during operation of the electrochemical cell 1, the gas flow suppression unit 20 thermally expands toward the frame 122 and comes into contact with or close to the frame 122 so that the gap between the gas flow suppression unit 20 and the frame 122 narrows. This can improve the sealing performance.
[0068] In this embodiment, since the electrolyte 10e is a solid oxide, it is difficult to bring the electrode stack 10 and the frame 122 into close contact with each other, and therefore a gap is formed between the electrode stack 10 and the frame 122. Here, in this embodiment, a gas flow suppressing unit 20 made of a material different from that of the electrode stack 10 is provided, so that a desired sealing function can be easily imparted. In detail, by making the gas flow suppressing unit 20 from a material different from that of the electrode stack 10, for example, a metal with excellent workability, a gas flow suppressing unit 20 of a size or dimension that does not come into contact with the frame 122, or a mode that does not cause undesired deformation or internal stress in the electrode stack 10 even if it comes into contact with the frame 122, can be easily made. Therefore, it is possible to effectively impart sealing performance.
[0069] Incidentally, even when the cell stack S is operated as an SOEC (solid oxide electrolysis cell), the gas flow suppression portion 20 can effectively impart sealing performance in the same manner as described above.
[0070] As described above, the electrochemical cell 1 of this embodiment comprises an electrode stack 10 including an electrolyte 10e having a first surface 10e1 and a second surface 10e2 located opposite the first surface 10e1, an oxygen electrode 10c in contact with the first surface 10e1, and a fuel electrode 10a in contact with the second surface 10e2, and a gas flow suppression unit 20 located at least partially adjacent to a side surface of the electrode stack 10 and formed from a material different from the electrolyte 10e, the oxygen electrode 10c, and the fuel electrode 10a.
[0071] With the above configuration, even when the electrode stack 10 is surrounded by the frame 122 such that a gap is formed between the electrode stack 10 and the frame 122, the gas flow suppression unit 20 can suppress the fuel gas flowing through the gap. The gas flow suppression unit 20 is made of a material different from the electrode stack 10, for example, a metal with excellent workability. This makes it easy to manufacture a gas flow suppression unit 20 that is of a size and dimensions that does not contact the frame 122, or that does not cause undesired deformation or internal stress in the electrode stack 10 even if it contacts the frame 122. Therefore, according to the electrochemical cell 1 according to the present embodiment, it is possible to suppress the flow of gas between the electrode stack 10 and the frame 122, which is a member surrounding the electrode stack 10, while suppressing undesired internal stress and deformation in the electrochemical cell 1 caused by contact between the electrode stack 10 and the frame 122, which is a member surrounding the electrode stack 10.
[0072] <Second embodiment> Next, an electrochemical cell 2 according to a second embodiment will be described with reference to Fig. 5. The same components of the second embodiment as those of the first embodiment are denoted by the same reference numerals, and duplicated descriptions will be omitted.
[0073] 5, the frame 122 in this embodiment has a plurality of protrusions 30 that protrude toward the electrode stack 10. The protrusions 30 protrude toward the portion of the side surface of the electrode stack 10 to which the gas flow suppression portion 20 is adjacent. However, the protrusions 30 are formed so that their tips are away from the side surface of the electrode stack 10. In this embodiment, as an example, the protrusions 30 are in the form of a rectangular plate with a constant thickness, and are formed so that the plate surface is aligned with the stacking direction Z.
[0074] In this embodiment, the gas flow suppression units 20 and the protruding units 30 are arranged in a staggered manner. The protruding units 30 are positioned so as to block the fuel gas passing between the tip of the gas flow suppression unit 20 and the frame 122. That is, the protruding units 30 have a function of preventing blow-through. By arranging the gas flow suppression units 20 and the protruding units 30 in a staggered manner, the fuel gas passing between the tip of the gas flow suppression unit 20 and the frame 122 may then repeatedly suddenly contract and expand in the space between the adjacent gas flow suppression units 20 and the protruding units 30, causing a pressure loss. This effectively suppresses the flow of fuel gas through the gap between the gas flow suppression unit 20 and the frame 122. Here, the space between the adjacent gas flow suppression units 20 and the protruding units 30 is preferably configured so that a vortex may be generated when the fuel gas flows in.
[0075] In this embodiment, as in the first embodiment, the gas flow suppression section 20, which is located away from the frame 122 at room temperature, is configured to come into contact with or approach the frame 122 due to thermal expansion when the temperature reaches a predetermined level or higher. In this embodiment, even if the gas flow suppression section 20 does not come into contact with the frame 122 when the temperature rises, the flow of fuel gas is blocked by the protrusions 30. This improves sealing performance.
[0076] <Third embodiment> Next, an electrochemical cell 3 according to a third embodiment will be described with reference to Fig. 6. The same components of the third embodiment as those of the first and second embodiments are denoted by the same reference numerals, and duplicated descriptions will be omitted.
[0077] 6, in the electrochemical cell 1 of the present embodiment, the gas flow suppression section 20 covers a wide area of the side surface of the electrode stack 10. That is, the gas flow suppression section 20 is formed in a wall shape extending in a direction circumferentially around the side surface of the electrode stack 10. In detail, the gas flow suppression section 20 is formed so as to partially or entirely cover a portion of the side surface of the electrode stack 10 that extends in a direction from the shared fuel supply channel 131 toward the shared fuel discharge channel 132.
[0078] In this embodiment, when the electrochemical cell 3 is not in operation, for example at room temperature (25° C.), the gas flow suppression unit 20 is positioned away from the frame 122, and the gas flow suppression unit 20 and the frame 122 are maintained apart even when the electrochemical cell 3 is in operation. As in the first embodiment, the gas flow suppression unit 20 in this embodiment may also be configured to come into contact with or approach the frame 122 due to thermal expansion when the temperature reaches or exceeds a predetermined temperature.
[0079] In this embodiment as well, the flow of fuel gas through the gap between the electrode stack 10 and the frame 122 can be suppressed.
[0080] <Electrochemical cell manufacturing method> An example of the manufacturing method will be described below with reference to Fig. 7. Fig. 7 shows a manufacturing procedure for the electrochemical cell 1 according to the first embodiment, but the electrochemical cells according to the second and third embodiments can also be manufactured by the same procedure.
[0081] In the example described here, an assembly jig 40 is used so as to form a desired gap between the electrode stack 10, particularly the gas flow suppression portion 20, and the frame 122. The assembly jig 40 may be, for example, a rectangular block formed to have dimensions slightly smaller than the desired gap between the electrode stack 10 and the frame 122.
[0082] As shown in Fig. 7(A), first, the separator 12 is prepared, and then, as shown in Fig. 7(B), an assembly jig 40 is placed on the base portion 121 of the separator 12. At this time, at least two assembly jigs 40 are arranged so as to be close to each of two opposing sides of the frame body 122. The two sides of the frame body 122 are the sides that will face the gas flow suppressing portion 20 after assembly.
[0083] Next, the fuel electrode side current collector 14a is placed on the base portion 121 so as not to come into contact with the assembly jig 40. In this state, the fuel electrode side current collector 14a is adhered to the base portion 121 with an adhesive or the like. As a result, the fuel electrode side current collector 14a is fixed at a desired position, and the distance between the gas flow suppression portion 20 integrated with the fuel electrode side current collector 14a and the frame 122 becomes a desired state.
[0084] Thereafter, the electrode stack 10 is placed on the fuel electrode side current collector 14a so as not to come into contact with the assembly jig 40 and the gas flow suppression unit 20. In this state, the electrode stack 10 is adhered to the fuel electrode side current collector 14a with an adhesive or the like. This fixes the electrode stack 10 in a desired position, and the gap between the electrode stack 10 and the frame 122 has a desired dimension. This allows the gas flow suppression unit 20 to function properly. Thereafter, the assembly jig 40 is removed by being pulled out.
[0085] Although each embodiment has been described above, the above-mentioned embodiments are presented as examples and are not intended to limit the scope of the invention. This new embodiment can be implemented in various other forms, and various omissions, substitutions, and modifications can be made without departing from the gist of the invention. The above-mentioned embodiments and other modifications are included in the scope and gist of the invention, and are included in the scope of the invention and its equivalents described in the claims.
[0086] For example, while the gas flow suppression portion 20 in the first and second embodiments described above is a plate-like portion with a constant thickness, the gas flow suppression portion 20 may be tapered toward the frame 122. In addition, the gas flow suppression portion 20 may be in a block shape.
[0087] In the first to third embodiments described above, the gas flow suppressing portion 20 is configured to suppress the flow of fuel gas, but the gas flow suppressing portion 20 may be applied to suppress the flow of oxygen. In this case, the gas flow suppressing portion 20 is disposed between the oxygen electrode 10c and the sealing plate 16. In this case, the gas flow suppressing portion 20 may be integrated with the oxygen electrode side current collector 14c. [Explanation of symbols]
[0088] Reference Signs List 1, 2, 3...electrochemical cell, 10...electrode laminate, 10e...electrolyte, 10e1...first surface, 10e2...second surface, 10c...oxygen electrode, 10a...fuel electrode, 10g...fuel electrode porous substrate, 12...separator, 12a...cell housing, 121...base, 122...frame, 131...fuel supply common flow path, 132...fuel discharge common flow path, 133...fuel supply branch flow path, 134...fuel discharge branch flow path, 135...oxygen supply common flow path, 136...oxygen discharge common flow path, 137...oxygen supply branch flow path, 138...oxygen discharge branch flow path, 14a...fuel electrode side current collector, 14c...oxygen electrode side current collector, 16...sealing plate, 18...sealing material, 20...gas flow suppressing portion, 30...projection, 40...assembly jig, S...cell stack
Claims
1. an electrolyte having a first surface and a second surface opposite to the first surface, an electrode stack including an oxygen electrode in contact with the first surface, and a fuel electrode in contact with the second surface; a gas flow suppression portion located so as to be at least partially adjacent to a side of the electrode stack located between the first surface and the second surface, the gas flow suppression portion being formed from a material different from the electrolyte, the oxygen electrode, and the fuel electrode.
2. 10. The electrochemical cell of claim 1, wherein the gas flow control is integral with the electrode stack.
3. 2. The electrochemical cell of claim 1, wherein the gas flow control portion is formed from a material having a linear expansion coefficient greater than linear expansion coefficients of the electrolyte, the oxygen electrode, and the fuel electrode.
4. The electrochemical cell according to claim 1 , wherein the gas flow suppressing portion is made of a metal having gas diffusibility.
5. The electrochemical cell includes a plurality of the gas flow suppression portions, The electrochemical cell according to claim 1 , wherein the gas flow suppressing portions are provided at intervals along a direction going around the side surface of the electrode stack.
6. The electrochemical cell according to claim 1 , wherein the gas flow suppressing portion is formed in a wall shape extending in a direction surrounding a side surface of the electrode stack.
7. a sheet-like member in contact with the oxygen electrode or the fuel electrode in a direction in which the electrolyte, the oxygen electrode, and the fuel electrode overlap each other; The electrochemical cell according to claim 1 , wherein the sheet-like member and the gas flow suppressing portion are integrated together.
8. The electrochemical cell according to claim 7 , wherein the sheet-like member and the gas flow suppressing portion are made of a metal having gas diffusibility.
9. 9. The electrochemical cell according to claim 7, wherein the sheet-like member is electrically conductive and functions as a current collector.
10. a separator including a base portion overlapping the electrode stack in a direction in which the electrolyte, the oxygen electrode, and the fuel electrode overlap; A frame body surrounding a side surface of the electrode stack, A gap is formed between the side surface of the electrode stack and the frame, The electrochemical cell according to claim 1 , wherein the gas flow suppressing portion is located in the gap so as to be at least partially adjacent to a side surface of the electrode stack and spaced apart from the frame.
11. The electrochemical cell according to claim 10 , wherein the gas flow suppressing portion comes into contact with or close to the frame due to thermal expansion when the gas flow suppressing portion reaches or is at or above a predetermined temperature.
12. 11. The electrochemical cell of claim 10, wherein the gas flow restrictor has a linear expansion coefficient greater than a linear expansion coefficient of the frame.
13. The frame body includes a plurality of protrusions protruding toward the electrode stack, The electrochemical cell according to claim 10 , wherein the gas flow suppression portions and the protrusions are arranged in a staggered manner.
14. The electrochemical cell according to claim 10 , wherein the frame is a part of the separator and is integrated with an outer peripheral portion of the base.
15. 10. The electrochemical cell of claim 1, wherein the electrolyte is a solid electrolyte.
16. A current collector arranged in a direction in which an electrolyte, an oxygen electrode, and a fuel electrode overlap each other in an electrode stack of an electrochemical cell, the current collector being in contact with the oxygen electrode or the fuel electrode, A current collector comprising a gas flow restrictor positioned at least partially adjacent a side surface of the electrode stack.
17. A cell stack comprising a plurality of electrochemical cells according to claim 1 stacked together.
Citation Information
Patent Citations
Stack sealing method
JP1988211570A
Water electrolysis reactors (SOECs) or fuel cells (SOFCs) with increased steam or fuel usage, respectively
JP2019530802A
Solid oxide fuel cell and method for producing solid oxide fuel cell
JP2023023652A
Electrochemical reaction unit and electrochemical reaction cell stack
WO2018155112A1
Endoscope apparatus with adaptor
JP1982034823A