Roller shaft

The roller shaft design with a resin body and extending portions addresses manufacturing challenges by ensuring strong fixation and cost-effectiveness, enhancing sheet conveyance efficiency and reducing ink transfer.

JP2024133324AActive Publication Date: 2024-10-01SUNCALL CORP
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2024115671
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2024-07-19
Publication Date
2024-10-01
Estimated Expiration
2041-06-08

AI Technical Summary

Technical Problem

Existing roller shafts for sheet conveyance mechanisms in printers and facsimiles face challenges in efficient manufacturing due to the difficulty of press-fitting rubber rings, leading to high costs and unreliable fixation strength.

Method used

A roller shaft design featuring a resin body fixed to a long shaft body with extending portions, allowing for adhesive or welded attachment, which ensures strong fixation and reduces manufacturing complexity and costs.

Benefits of technology

The design achieves cost-effective manufacturing while maintaining robust adhesive strength, facilitating efficient sheet conveyance with reduced ink transfer.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024133324000001_ABST
    Figure 2024133324000001_ABST
Patent Text Reader

Abstract

To provide a roller shaft where a resin body is fixed to a long shaft body, which can achieve reduction of cost as much as possible while securing fixing strength to the shaft body of the resin body.SOLUTION: A roller shaft includes a long shaft body and a resin body fixed to a prescribed position in an axial direction having the same diameter as the shaft body, wherein the resin body integrally has a body part having prescribed thickness, and an extension part which is adjacent to the body part in the axial direction of the shaft body, and has a smaller diameter than the body part by being set to be thinner than the body part.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a roller shaft suitable for use in a sheet transport mechanism in a printer, a facsimile, or the like. [Background technology]

[0002] A structure in which a star wheel (spur) and a roller shaft are arranged opposite each other so as to sandwich the sheet of paper or other material to be transported, and the sheet is held and transported by the star wheel and the roller shaft, is used, for example, in the transport mechanisms of office equipment such as printers and facsimiles.

[0003] The roller shaft and the star wheel are arranged downstream in the sheet transport direction from a recording means such as an inkjet head, and it is necessary to transport the sheet while preventing as much as possible the transfer of ink printed on the sheet by the recording means.

[0004] In regard to this point, a stepped roller shaft has been proposed that includes a shaft body and a plurality of rubber rings press-fitted onto the shaft body (see Patent Document 1 below). Specifically, a plurality of star wheels are spaced apart along the width direction of the sheet body on one side in the thickness direction of the sheet body, while the stepped roller shaft is arranged on the other side in the thickness direction of the sheet body, and the plurality of rubber rings are press-fitted onto the shaft body so as to face the respective star wheels. With this configuration, the corresponding rubber rings and star wheels sandwich and transport the sheet body.

[0005] This stepped roller shaft is useful in that the area in contact with the sheet body can be essentially limited to just the rubber ring, thereby preventing as much as possible the transfer of ink printed on the sheet body to the roller shaft. However, there is a problem in that the rubber ring must be pressed into a predetermined position on the shaft body so that it faces the star wheel, making it difficult to manufacture the roller shaft efficiently and resulting in high manufacturing costs. Furthermore, since the rubber ring is fixed to the shaft by press fitting, there is also the problem that it is difficult to maintain the fixing strength of the rubber ring to the shaft. [Prior art documents] [Patent documents]

[0006] [Patent Document 1] JP 2002-316741 A Summary of the Invention [Problem to be solved by the invention]

[0007] The present invention has been made in consideration of the above-mentioned conventional technology, and aims to provide a roller shaft having a resin body fixed to the outer surface of a long shaft body, which can achieve the lowest possible cost while ensuring the fixing strength of the resin body to the shaft body. [Means for solving the problem]

[0008] In order to achieve the above object, the present invention provides a method for manufacturing a bearing comprising: The resin body provides a roller shaft having integrally therewith a main body portion of a predetermined thickness and an extension portion adjacent to the main body portion in the axial direction of the shaft body and having a smaller diameter than the main body portion by being thinner than the main body portion.

[0009] Preferably, the extension portion may include first and second extension portions provided on one side and the other side of the main body portion, respectively, in the axial direction of the shaft. Effect of the Invention

[0010] According to the roller shaft of the present invention, it is possible to ensure the adhesive strength of the resin body to the shaft body while achieving the lowest possible cost. [Brief description of the drawings]

[0011] [Figure 1]FIG. 1 is a schematic diagram of a conveying mechanism to which a roller shaft according to an embodiment of the present invention is applied. [Diagram 2] FIG. 2(a) is a plan view of a roller shaft according to the first embodiment of the present invention, and FIG. 2(b) is a cross-sectional view taken along line IIb-IIb in FIG. 2(a). [Diagram 3] 3(a) is an enlarged view of part III in FIG. 2(b), and FIGS. 3(b) and 3(c) are cross-sectional views taken along lines IIIb-IIIb and IIIc-IIIc in FIG. 3(a), respectively. [Figure 4] FIG. 4 is a schematic plan view of an initial state of a manufacturing apparatus used in one manufacturing method (first manufacturing method) of the roller shaft according to the first embodiment. [Diagram 5] FIG. 5 is a schematic plan view of the manufacturing apparatus after the coating step in the first manufacturing method. [Figure 6] FIG. 6 is a schematic plan view of the manufacturing apparatus in a state where a molding step in the first manufacturing method is being performed. [Figure 7] FIG. 7 is an enlarged view of part VII in FIG. [Figure 8] 8(a) to (c) are cross-sectional views taken along lines VIIIa-VIIIa, VIIIb-VIIIb and VIIIc-VIIIc in FIG. 7, respectively. [Figure 9] FIG. 9 is a schematic plan view of a manufacturing apparatus used in another manufacturing method (second manufacturing method) of the roller shaft according to the first embodiment, showing a state after a coating step in the second manufacturing method. [Figure 10] FIG. 10 is a schematic plan view of the manufacturing apparatus in a state where a molding step in the second manufacturing method is being performed. [Figure 11] FIG. 11 is an enlarged view of a portion XI in FIG. [Figure 12] 12(a) to (c) are cross-sectional views taken along lines XIIa-XIIa, XIIb-XIIb and XIIc-XIIc in FIG. 11, respectively. [Figure 13]FIG. 13(a) is a plan view of a roller shaft according to the second embodiment of the present invention, and FIG. 13(b) is a cross-sectional view taken along line XIIIb-XIIIb in FIG. 13(a). [Figure 14] 14(a) is an enlarged view of part XVI in FIG. 13(b), and FIG. 14(b) is a cross-sectional view taken along line XIVb-XIVb in FIG. 14(a). [Figure 15] FIG. 15 is a schematic plan view of a manufacturing apparatus used in one manufacturing method (third manufacturing method) of the roller shaft according to the second embodiment, showing a state after a coating step in the third manufacturing method. [Figure 16] FIG. 16 is a schematic plan view of the manufacturing apparatus in a state where an intermediate molding step is being performed in the third manufacturing method. [Figure 17] FIG. 17 is an enlarged view of a portion XVII in FIG. [Figure 18] FIG. 18 is a schematic plan view of the manufacturing apparatus in a state where a final molding step is being performed in the third manufacturing method. [Figure 19] FIG. 19 is an enlarged view of a portion XIX in FIG. [Figure 20] 20(a) and (b) are cross-sectional views taken along lines XXa-XXa and XXb-XXb in FIG. 19, respectively. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0012] First embodiment DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS A preferred embodiment of a roller shaft according to the present invention will now be described with reference to the accompanying drawings. FIG. 1 is a schematic diagram showing an example of a conveying mechanism 1 for conveying a sheet such as paper to which a roller shaft 10 according to the present embodiment is applied.

[0013] The conveying mechanism 1 has one or more star wheels 3 arranged on one side of the thickness direction of the sheet body, and the roller shaft 10 arranged on the other side of the thickness direction of the sheet body so as to sandwich the sheet body and correspond to the star wheel 3, and the roller shaft 10 is configured to cooperate with the star wheel 3 to pinch and convey the sheet body.

[0014] In the conveying mechanism shown in FIG. 1, the roller shaft 10 is disposed downstream of the inkjet head 2 in the sheet conveying direction, and is used to eject the sheet after printing in cooperation with the star wheel 3. 1, reference numerals 4 and 5 respectively denote a paper feed roller and a separation roller, and reference numerals 6 and 7 respectively denote a pinch roller and a paper transport roller.

[0015] FIG. 2( a ) shows a plan view of the roller shaft 10 . FIG. 2(b) is a cross-sectional view taken along line IIb-IIb in FIG. 2(a). FIG. 3(a) is an enlarged view of part III in FIG. 2(b). Furthermore, FIGS. 3(b) and 3(c) are cross-sectional views taken along lines IIIb-IIIb and IIIc-IIIc in FIG. 3(a), respectively.

[0016] As shown in FIGS. 2 and 3, the roller shaft 10 has a rigid shaft body 20 and a resin body 30 fixed to the shaft body 20 at a predetermined position in the axial direction.

[0017] The shaft body 20 may be made of various materials as long as it has a predetermined rigidity, but is preferably made of a metal material such as steel. Additionally, the shaft 20 may be either solid or hollow.

[0018] The resin body 30 is provided at a predetermined position in the axial direction of the shaft body 20 . For example, when the roller shaft 10 is used in the conveying device 1 so as to cooperate with the star wheel 3, the resin body 30 is provided at the same position as the star wheel 3 with respect to the axial position of the shaft body 20.

[0019] The roller shaft 10 has one or a desired number of the resin bodies 30 according to necessity or specifications. In FIG. 2, the roller shaft 10 has five of the resin bodies 30 .

[0020] As shown in Figure 3, the resin body 30 integrally has a main body portion 31 with an axial length L and a thickness T, and an extension portion 33 adjacent to the main body portion 31 in the axial direction of the shaft body 20 and having a thickness Ts thinner than the main body portion 31.

[0021] When the roller shaft 10 is used in a conveying device 1 together with the star wheel 3, the main body portion 31 of the resin body 30 cooperates with the corresponding star wheel 3 to convey a sheet body.

[0022] That is, the star wheel 3 is disposed so that its outer circumferential surface abuts against a first surface (eg, upper surface) on one side in the thickness direction of the sheet body, with its axis direction aligned with the width direction of the sheet body.

[0023] On the other hand, the roller shaft 10 is positioned so that the outer peripheral surface of the main body 31 abuts against a second surface (e.g., the lower surface) on the other side of the thickness direction of the sheet body, with the axial direction of the shaft body 20 aligned along the width direction of the sheet body.

[0024] As a result, the sheet body is conveyed in a state where it is sandwiched between the star wheel 3 and the main body portion 31 in response to the rotational drive of the star wheel 3 about its axis.

[0025] At this time, the roller shaft 10 is rotated about its axis by the frictional force between the sheet being conveyed and the outer circumferential surface of the main body portion 31 in contact with the sheet.

[0026] Therefore, in order to smoothly transport the sheet body, The main body 31 of the resin body 30 is firmly fixed to the shaft body 20 at a predetermined position in the axial direction. The body portion 31 has a predetermined axial length L and thickness T so that a desired frictional force is obtained between the sheet body and the body portion 31. becomes important.

[0027] In this regard, in this embodiment, as shown in Figures 3(a) to (c), etc., the resin body 30 has, in addition to the main body portion 31 of axial length L and thickness T that abuts the sheet body, the extension portion 33 is adjacent to the main body portion 31 in the axial direction of the shaft body 20 and has a thickness Ts that is thinner than the main body portion 31.

[0028] With the resin body 30 having such a configuration, the dimensions of the portion in contact with the sheet body (i.e., the main body portion 31) can be made the desired dimensions (i.e., axial length L and thickness T), while the contact area with the shaft body 20 can be increased, and the adhesive strength of the resin body 30 to the shaft body 20 can be increased.

[0029] In particular, in this embodiment, as shown in Figure 3(a), the extension portion 33 has first and second extension portions 33a, 33b respectively provided on one side and the other side of the main body portion 31 in the axial direction of the shaft body 20, making it possible to further increase the bonding strength of the resin body 30 to the shaft body 20.

[0030] The resin body 30 can be fixed to the shaft body by various means such as adhesives or welding, but in this embodiment, the resin body 30 is formed from a thermoplastic resin (hot melt resin) and is fixed to the shaft body 20 by welding.

[0031] An example of a method for manufacturing the roller shaft 10 according to the present embodiment (hereinafter referred to as a first manufacturing method) will be described below. FIG. 4 is a schematic plan view showing an initial state of a manufacturing apparatus used in the first manufacturing method.

[0032] The first manufacturing method includes a coating step in which, while rotating the shaft body 20 around its axis, hot melt resin 40 that has been heated and made molten is applied to a resin body forming region 25 (see Figure 4 and Figure 5 below) on the outer surface of the shaft body 20 where the resin body 30 is provided, so as to have an axial length La shorter than L and a thickness Ta thicker than T.

[0033] FIG. 5 is a schematic plan view of the manufacturing apparatus after the coating step. In the example shown in FIG. 5, the hot melt resin 40 is applied to five resin body forming regions 25. As shown in FIG.

[0034] The shaft 20 is rotated about its axis by a rotation drive mechanism (not shown), and the hot melt resin 40 is applied by a resin discharge mechanism (not shown).

[0035] The hot melt resin 40 has a viscosity such that when applied to the outer surface of the shaft body 20 in a heated and molten state, it does not come off from the shaft body 20 as it rotates around its axis. For example, polyolefin-based resins, polyurethane-based resins, etc. are preferably used.

[0036] The first manufacturing method includes a molding step of molding the hot melt resin 40 applied to the resin body forming region 25 using a molding roll 50.

[0037] FIG. 6 is a schematic plan view of the manufacturing apparatus with the molding roll 50 positioned at the molding position. FIG. 7 shows an enlarged view of part VII in FIG. 8(a) to 8(c) are cross-sectional views taken along lines VIIIa-VIIIa, VIIIb-VIIIb, and VIIIc-VIIIc in FIG. 7, respectively.

[0038] In the first manufacturing method, one molding roll 50 is used for each of the resin body forming regions 25 . As described above, in the example shown in FIG. 5 and FIG. 6, five resin body forming regions 25 are provided, and therefore five molding rolls 50 corresponding to the five resin body forming regions 25 are used.

[0039] As shown in Figures 7 and 8(a) to (c), the molding roll 50 has a small diameter portion 51 having an axial length L and a cross-sectional shape that is a circle of a predetermined diameter, and a large diameter portion 53 having a cross-sectional shape that is a circle of a larger diameter than the small diameter portion 51, concentric with the small diameter portion 51, and adjacent to the small diameter portion 51 in the axial direction.

[0040] The small diameter portion 51 forms the main body portion 31 , and the large diameter portion 53 forms the extension portion 33 . As described above, in this embodiment, the extension portion 33 has the first and second extension portions 33a, 33b extending from the main body portion 31 to one side and the other side in the axial direction, respectively. Therefore, the forming roll 50 has, as the large diameter portion 53, first and second large diameter portions 53a, 53b extending from the small diameter portion 51 to one side and the other side in the axial direction, respectively.

[0041] The molding process is configured to move the molding roll 50 in a parallel position to the shaft body 20 in a direction approaching the shaft body 20, which is rotating around its axis, to the molding position, thereby molding the hot melt resin 40 applied to the resin body forming region 25 of the shaft body 20 into the final shape of the resin body 30.

[0042] The molding position is a position where the distance between the outer surface of the small diameter portion 51 and the outer surface of the shaft 20 is the thickness T of the main body 31. As shown in FIG. 7, by positioning the molding roll 50 at the molding position, a molding space 41 of thickness T and axial length L is formed between the outer surface of the small diameter portion 51 and the outer surface of the shaft 20, and further, a receiving space 43 of thickness Ts thinner than T and connected to the molding space 41 is formed between the outer surface of the large diameter portion 53 and the outer surface of the shaft 20.

[0043] The axial length La and thickness Ta (see FIG. 5) of the hot melt resin 40 applied in the application process are set to values ​​such that when the molding roll 50 is positioned at the molding position, the molding space 41 is filled with hot melt resin 40 and the excess resin overflowing from the molding space 41 flows into the receiving space 43.

[0044] According to the first manufacturing method having such a configuration, the roller shaft 10 can be efficiently manufactured in which the resin body 30 including the main body portion 31 and the extension portion 33 is fixed to a predetermined region of the shaft body 20 (the resin body forming region 25).

[0045] As shown in Figure 5 etc., in the first manufacturing method, the molding process is configured to be performed using a housing 60 that supports the molding roll 50 rotatably about its axis so that the small diameter portion 51 and the large diameter portion 53 are rotatable about their axes, and a molding reciprocating mechanism 70 that moves the housing 60 toward and away from the shaft body 20.

[0046] As shown in FIG. 7 and FIGS. 8(a) to (c), the forming roll 50 has a support shaft 55 that supports the small diameter portion 51 and the large diameter portion 53 on the central axis.

[0047] The housing 60 has a pair of side walls 61 that respectively support one end and the other end of the support shaft 55 in a position parallel to the shaft body 20, and is configured to allow access to the small diameter portion 51 and the large diameter portion 53 from the shaft body 20 side.

[0048] In the first manufacturing method, the housing 60 has, in addition to the pair of side walls 61, a base end wall 63 connecting the base ends of the pair of side walls 61, and is roughly U-shaped in plan view, with the free end side facing the shaft body 20, the upper side, and the lower side being open.

[0049] In this embodiment, the support shaft 55 rotates integrally around the axis together with the small diameter portion 51 and the large diameter portion 53, and the support shaft 55 is supported on the pair of side walls 61 so as to be rotatable around the axis, so that the small diameter portion 51 and the large diameter portion 53 are rotatable around the axis relative to the housing 60.

[0050] Alternatively, it is also possible to modify the support shaft 55 so that it supports the small diameter portion 51 and the large diameter portion 53 so as to be rotatable relative to one another, and so that the pair of side walls 61 support the support shaft 55 so as not to be rotatable around its axis.

[0051] The molding reciprocating mechanism 70 has a piston mechanism that moves the housing 60 toward and away from the shaft 20 so that the molding roll 50 can take a molding position (see Figure 6) and a retracted position (see Figure 5) spaced away from the shaft 20 from the molding position.

[0052] As shown in Figure 8 (c), in this embodiment, the pair of side walls 61 have a vertical length H that is greater than the diameter D of the shaft body 20, and further, the tip surfaces of the pair of side walls 61 are provided with arc-shaped notches 62 that open toward the shaft body.

[0053] As shown in Figure 8 (c), when the molding roll 50 is positioned at the molding position, a portion of the shaft 20 is positioned within the arc-shaped notch 62 with a gap smaller than Ts between the outer surface of the arc-shaped notch 62 and the outer surface of the shaft 20.

[0054] According to this configuration, it is possible to effectively prevent or reduce the hot melt resin that flows from the molding space 41 into the receiving space 43 during the molding process from leaking outward in the axial direction from the receiving space 43.

[0055] Preferably, the molding process is configured such that, when the molding roll 50 is positioned at the molding position by the molding reciprocating mechanism 70, the non-resin body region 27 (see Figure 4) of the shaft 20 other than the resin body forming region 25 is pressed in the direction opposite to the pressing direction by the molding reciprocating mechanism 70 in the axial direction.

[0056] According to this configuration, it is possible to effectively prevent or reduce the “deflection” of the shaft body 20 that may occur when the molding reciprocating mechanism 70 presses the molding roll 50 against the shaft body 20 .

[0057] In this embodiment, as shown in Figure 6 etc., pressing of the non-resin region 27 in the direction opposite to the pressing direction by the molding reciprocating mechanism 70 is performed by a pressure-resistant reciprocating mechanism 75 configured to reciprocate a pressing rod 77, whose axial direction is parallel to the pressing direction of the molding reciprocating mechanism 70, along the axial direction.

[0058] The first manufacturing method can preferably include a cooling step of cooling the hot melt resin 40 on the shaft body 20 after the application step and before the molding step. The cooling process is configured to cool the hot melt resin 40 on the shaft body 20 to a degree that allows it to be completely hardened (i.e., to a degree that maintains a semi-hardened state that enables molding processing in the subsequent molding process).

[0059] The cooling step is performed, for example, by spraying water onto the hot melt resin 40 on the shaft body 20 . According to such a configuration, adhesion of the hot melt resin to the molding roll 50 during the molding step can be effectively prevented or reduced, and molding processability (outer diameter dimension and roundness) can be improved.

[0060] More preferably, the cooling step is configured to spray water onto the hot melt resin 40 using a sprayer. With this configuration, the adhesion of water to the outer surface of the hot melt resin 40 can be improved.

[0061] Preferably, a release material may be provided on the outer surfaces of the small diameter portion 51 and the large diameter portion 53 of the forming roll 50 . The release material is, for example, oil, silicone resin, or fluororesin. The oil or silicone is provided on the outer surface by, for example, applying it to the outer surfaces of the small diameter portion 51 and the large diameter portion 53 of the forming roll 50 before the forming step. The fluororesin is provided on the outer surfaces by, for example, applying a fluororesin to the outer surfaces of the small diameter portion 51 and the large diameter portion 53 during the production of the forming roll 50, and preferably baking the fluororesin.

[0062] Hereinafter, another example of the manufacturing method of the roller shaft 10 according to the present embodiment (hereinafter referred to as the second manufacturing method) will be described. FIG. 9 is a schematic plan view of a manufacturing apparatus used in the second manufacturing method.

[0063] The first manufacturing method is configured to mold the hot melt resin using one molding roll 50 for each of the resin body forming regions 25. In contrast, the second manufacturing method is configured to mold the hot melt resin 40 using a molding roll pair including a pair of first and second molding rolls 50-(1), 50-(2) for each resin body forming region 25.

[0064] Specifically, the second manufacturing method has the same coating step as in the first manufacturing method. FIG. 9 shows the state after the coating step.

[0065] The second manufacturing method includes a molding step of molding the hot melt resin 40 using the molding roll pairs provided for each of the resin body forming regions 25 after the application step.

[0066] In the example shown in FIG. 9, five resin body forming regions are provided, and therefore five molding roll pairs corresponding to the five resin body forming regions are used.

[0067] The first and second molding rolls 50-(1), 50-(2) of the pair of molding rolls have the same configuration as the molding roll 50 used in the first manufacturing method. That is, each of the first and second molding rolls 50-(1), 50-(2) has the small diameter portion 51 and the large diameter portion 53 (the first and second large diameter portions 53a, 53b in the illustrated example).

[0068] In the molding process of the second manufacturing method, the first molding roll 50-(1) is translated to a first molding position in a direction approaching the shaft body 20, which is rotated about its axis while being arranged parallel to the shaft body 20 on one side of a virtual vertical plane VP passing through the axis of the shaft body 20, and the second molding roll 50-(2), which is plane-symmetrical to the first molding roll 50-(1) with respect to the virtual vertical plane VP, is translated to a second molding position in a direction approaching the shaft body 20, which is rotated about its axis while being arranged parallel to the shaft body 20 on the other side of the virtual vertical plane VP, thereby molding the hot melt resin 40 applied to the resin body forming region 25.

[0069] FIG. 10 shows a schematic plan view of the manufacturing apparatus in a state where the first molding roll 50-(1) is positioned at the first molding position and the second molding roll 50-(2) is positioned at the second molding position. FIG. 11 shows an enlarged view of portion XI in FIG. 12(a) to (c) are cross-sectional views taken along lines XIIa-XIIa, XIIb-XIIb, and XIIc-XIIc in FIG. 11, respectively.

[0070] As shown in Figures 11 and 12(a) to (c), the first molding position is a position where the distance between the outer surface of the small diameter portion 51 of the first molding roll 50-(1) and the outer surface of the shaft body 20 is T.

[0071] By positioning the first molding roll 50-(1) at the first molding position, a first molding space 41-(1) having a thickness T and an axial length L is formed between the small diameter portion 51 of the first molding roll 50-(1) and the outer surface of the shaft body 20, and further, a first receiving space 43-(1) having a thickness Ts thinner than T and connected to the first molding space 41-(1) is formed between the outer surface of the large diameter portion 53 of the first molding roll 50-(1) and the outer surface of the shaft body 20.

[0072] The second molding position is a position where a distance T is provided between the outer surface of the small diameter portion 51 of the second molding roll 50-(2) and the outer surface of the shaft body 20.

[0073] By positioning the second molding roll 50-(2) at the second molding position, a second molding space 41-(2) having a thickness T and an axial length L is formed between the small diameter portion 51 of the second molding roll 50-(2) and the outer surface of the shaft body 20, and further, a second receiving space 41-(3) having a thickness Ts thinner than T and connected to the second molding space 41-(2) is formed between the outer surface of the large diameter portion 53 of the second molding roll 50-(2) and the outer surface of the shaft body 20.

[0074] As shown in Figure 9 etc., the second manufacturing method is configured to be performed using a first housing 60-(1) that supports the first molding roll 50-(1) so that the small diameter portion 51 and the large diameter portion 53 of the first molding roll 50-(1) are freely rotatable about their axis, a first molding reciprocating mechanism 70-(1) that moves the first housing 60-(1) toward and away from the shaft body 20, a second housing 60-(2) that supports the second molding roll 50-(2) so that the small diameter portion 51 and the large diameter portion 53 of the second molding roll 50-(2) are freely rotatable about their axis, and a second molding reciprocating mechanism 70-(2) that moves the second housing 60-(2) toward and away from the shaft body 20.

[0075] As shown in Figures 11 and 12(a) to (c), each of the first and second molding rolls 50-(1), 50-(2) has a support shaft 55 that supports the small diameter portion 51 and the large diameter portion 53 on the central axis.

[0076] The first and second housings 60-(1), 60-(2) have the same configuration as the housing 60.

[0077] The first and second molding reciprocating mechanisms 70-(1), 70-(2) have the same configuration as the molding reciprocating mechanism 70.

[0078] In the second manufacturing method, during the molding step, the shaft 20 is sandwiched and pressed between the first and second molding rolls 50-(1), 50-(2). Therefore, without providing the pressure-resistant reciprocating mechanism 75, the "deflection" of the shaft body 20 that occurs during the molding process can be effectively prevented or reduced.

[0079] In the second manufacturing method, as in the first manufacturing method, the cooling step can be provided after the application step and before the molding step, and the release material can be provided on the outer surfaces of the small diameter portion 51 and the large diameter portion 53 of the first and second molding rolls 50-(1), 50-(2).

[0080] Embodiment 2 Hereinafter, another preferred embodiment of a roller shaft according to the present invention will be described with reference to the accompanying drawings.

[0081] FIG. 13(a) shows a plan view of the roller shaft 110 according to this embodiment. FIG. 13(b) is a cross-sectional view taken along line XIIIb-XIIIb in FIG. 13(a). FIG. 14(a) is an enlarged view of portion XVI in FIG. 13(b). Furthermore, FIG. 14(b) shows a cross-sectional view taken along line XIVb-XIVb in FIG. 14(a). In the figure, the same members as those in the first embodiment are given the same reference numerals.

[0082] The roller shaft 110 has the shaft body 20 and a resin body 130 fixed to the shaft body 20 at a predetermined position in the axial direction.

[0083] As shown in FIGS. 13 and 14, a recess 133 is provided over the entire circumference of the outer surface of the resin body 130 at a midpoint in the axial direction of the shaft body 20 .

[0084] An example of a method for manufacturing the roller shaft 110 according to this embodiment (hereinafter referred to as a third manufacturing method) will be described below.

[0085] The third manufacturing method includes a coating step in which, while rotating the shaft body 20 around its axis, hot melt resin 40 that has been heated to a molten state is applied to a resin body forming region 25 on the outer surface of the shaft body 20 in which the resin body 130 is provided, so that the axial length Lc is shorter than L and the thickness Tc is thicker than T.

[0086] FIG. 15 is a schematic plan view of a manufacturing apparatus used in the third manufacturing method, showing the state after the coating step.

[0087] The third manufacturing method includes, after the application step, an intermediate molding step of performing intermediate molding on the hot melt resin 40 applied to the resin body forming region 25. The intermediate molding step is carried out using an intermediate molding roll 150 .

[0088] FIG. 16 is a schematic plan view of the manufacturing apparatus with the intermediate molding roll 150 positioned at the intermediate molding position. FIG. 17 shows an enlarged view of a portion XVII in FIG. In FIG. 17, the hot melt resin 40 after the application step and before the intermediate molding step is indicated by a two-dot chain line.

[0089] As shown in FIGS. 15 and 16, the intermediate molding roll 150 is provided for each of the resin body forming regions 25 . In the example shown in Figs. 15 and 16, five resin body forming regions 25 are provided, and therefore five intermediate molding rolls 150 corresponding to the five resin body forming regions 25 are used.

[0090] As shown in Figure 17 etc., the intermediate molding roll 150 has an intermediate cylindrical portion 151 whose cross-sectional shape is a circle of a predetermined diameter, and an intermediate support shaft 155 that supports the intermediate cylindrical portion 151 on its central axis, and the intermediate cylindrical portion 151 has a convex portion 153 that protrudes radially outward at a midpoint in the axial direction on its outer circumferential surface.

[0091] The intermediate molding process is configured to form a depression 43 by the convex portion 153 on the outer surface of the hot melt resin 40 applied to the resin body forming region 25 by moving the intermediate molding roll 150 in a direction approaching the shaft body 20, which is rotating around its axis in a parallel position to the shaft body 20, to an intermediate molding position where the distance Td between the outer surface of the intermediate cylindrical portion 151 and the outer surface of the shaft body 20 is smaller than Tc and larger than T.

[0092] In the third manufacturing method, the intermediate molding process is configured to be performed using an intermediate housing 160 that supports the intermediate molding roll 150 and the molding reciprocating mechanism 70 that moves the intermediate housing 160 toward and away from the shaft 20.

[0093] The intermediate housing 160 has a pair of intermediate side walls 161 that respectively support one end and the other end of the intermediate support shaft 155 when it is positioned parallel to the shaft body 20, and is configured to allow access to the intermediate cylindrical portion 151 from the shaft body 20 side.

[0094] In the third manufacturing method, the intermediate housing 160 has, in addition to the pair of intermediate side walls 161, an intermediate base end wall 163 connecting the base ends of the pair of intermediate side walls 161, and is roughly U-shaped in plan view, with the free end side facing the shaft body 20, the upper side, and the lower side being open.

[0095] The intermediate molding reciprocating mechanism 160 has a piston mechanism that moves the intermediate housing 160 toward and away from the shaft 20 so that the intermediate molding roll 150 can take an intermediate molding position (Figure 16) and a retracted position (Figure 15) spaced away from the shaft 20 from the intermediate molding position.

[0096] The third manufacturing method includes a final molding step of performing final molding on the hot melt resin 40 on the resin body forming region 25 after the intermediate molding step. The final forming step is performed using a final forming roll 170 .

[0097] FIG. 18 is a schematic plan view of the manufacturing apparatus with the final molding roll 170 positioned at the final molding position. FIG. 19 shows an enlarged view of portion XIX in FIG. In FIG. 19, the hot melt resin 40 after the intermediate molding step and before the final molding is indicated by a two-dot chain line. 19. Furthermore, FIGS. 20(a) and 20(b) are cross-sectional views taken along lines XXa-XXa and XXb-XXb in FIG. 19, respectively.

[0098] As shown in FIG. 18, the final molding roll 170 is provided for each of the resin body forming regions 25 . In the example shown in FIG. 18, five resin body forming regions 25 are provided, and therefore five final molding rolls 170 corresponding to the five resin body forming regions 25 are used.

[0099] As shown in FIG. 19 etc., the final molding roll 170 has a final cylindrical portion 171 whose cross-sectional shape is a circle with a predetermined diameter, and a final support shaft 175 that supports the final cylindrical portion 171 on its central axis. The final cylindrical portion 171 has the same length as the axial length L of the resin body 130 .

[0100] The final molding process is configured to mold the hot melt resin 40 after the intermediate molding process into the resin body 130 having an axial length L and a thickness T by moving the final molding roll 170 in a direction approaching the shaft body 20, which is rotating around its axis in a parallel position to the shaft body 20, to a final molding position where the distance between the outer surface of the final cylindrical portion 171 and the outer surface of the shaft body 20 is T.

[0101] In the third manufacturing method, the axial length Lc and thickness Tc of the hot melt resin 40 applied in the application process are set to values ​​such that when the final molding roll 170 is positioned at the final molding position, a molding space of axial length L and thickness T defined between the outer surface of the final cylindrical portion 171 and the outer surface of the shaft body 20 is filled with the hot melt resin 40.

[0102] Any error in the amount of hot melt resin applied during the application process is effectively absorbed by the recess 43. That is, if the amount of hot melt resin applied in the application step exceeds the amount that fills the molding space (molding space filling amount), the recess 43 will be filled with the excess amount. Therefore, as the amount of excess hot melt resin in the coating step increases with respect to the amount of filling of the molding space, the recess 133 becomes smaller than the recess 43 .

[0103] As shown in Figure 19 etc., in the third manufacturing method, the final molding process is performed using a final housing 180 that supports the final molding roll 170 so that the final cylindrical portion 171 is freely rotatable around its axis.

[0104] The final housing 180 has a pair of final side walls 181 that support one side and the other side of the final support shaft 175, respectively, while being adjacent to one end side and the other end side of the final cylindrical portion 171 in the axial direction, and is configured to allow access to the final cylindrical portion 171 from the shaft body 20 side.

[0105] In the third manufacturing method, the final housing 180 has, in addition to the pair of final side walls 181, a final base end wall 183 connecting the base ends of the pair of final side walls 181, and is roughly U-shaped in plan view, with the free end side facing the shaft body 20, the upper side, and the lower side being open.

[0106] In the third manufacturing method, as shown in FIGS. 16 and 18, the intermediate molding step and the final molding step are performed using the molding reciprocating mechanism 70.

[0107] Furthermore, in the third manufacturing method, the intermediate molding process and the final molding process are configured so that when the intermediate molding roll 150 and the final molding roll 170 are positioned at the intermediate molding position and the final molding position, respectively, by the molding reciprocating mechanism 70, the non-resin body region 27 of the shaft 20 other than the resin body forming region 25 in the axial direction is pressed in the direction opposite to the pressing direction by the molding reciprocating mechanism 70.

[0108] As shown in FIGS. 16 and 18, the pressing of the non-resin region 27 in the direction opposite to the pressing direction by the molding reciprocating mechanism 70 is performed by the pressure-resistant reciprocating mechanism 75.

[0109] In addition, during the intermediate molding process and the final molding process, instead of pressing the non-resin body region 27 of the shaft body 20 in the direction opposite to the pressing direction by the molding reciprocating mechanism 70, it is also possible to provide a pair of intermediate molding rolls 150 and a pair of final molding rolls 170 that face each other across the shaft body 20 for each resin body forming region 25.

[0110] In other words, the hot melt resin 40 applied to the resin body forming region 25 is compressed between a pair of the intermediate molding rolls 150 to perform intermediate molding, and the hot melt resin 40 after intermediate molding is compressed between a pair of the final molding rolls 170 to perform final molding, thereby effectively preventing or reducing "deflection" of the shaft body 20 during the intermediate molding process and the final molding process.

[0111] The third manufacturing method may preferably include a cooling step that is the same as the cooling step in the first and second manufacturing methods after the coating step and before the intermediate molding step, and / or after the intermediate molding step and before the final step. In addition, the release material may be provided on the outer surface of the intermediate cylindrical portion 151 and / or the final cylindrical portion 171 . [Explanation of symbols]

[0112] 10 Roller shaft 20 Axial body 25 Resin body forming area 27 Non-resin area 30 Resin body 31 Main body 33a, 33b 1st and 2nd extension part

Claims

1. A long shaft body and a resin body fixed to a predetermined position in the axial direction of the shaft body and having the same diameter as the shaft body, The roller shaft is characterized in that the resin body integrally has a main body portion of a predetermined thickness and an extension portion that is adjacent to the main body portion in the axial direction of the shaft body and has a smaller diameter than the main body portion by being thinner than the main body portion.

2. 2. The roller shaft according to claim 1, wherein the extension portion includes first and second extension portions provided on one and the other sides of the main body portion in the axial direction of the shaft body.

Citation Information

Patent Citations

  • Thermal printer

    JP2000118023A

  • Stepped paper discharge roller and method of manufacturing the same

    JP2013188949A

  • Roller shaft

    JP2024109995A

  • Shaft rod with roller for paper feeding and discharging, conveying and the like

    JP2002316741A