Piezoelectric element and piezoelectric device

The piezoelectric element, with a dual-sided support and slit configuration, addresses detection accuracy issues by increasing resonance frequency and expanding sensitivity range, thereby improving detection precision.

JP2024133375AActive Publication Date: 2024-10-01DENSO CORP
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
JP2024117752
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2024-07-23
Publication Date
2024-10-01
Estimated Expiration
2041-02-03

AI Technical Summary

Technical Problem

Existing piezoelectric elements have limitations in detection accuracy due to their design, particularly when supported in a cantilevered manner, which affects the resonance frequency and sensitivity range.

Method used

A piezoelectric element with a vibrating part supported on both sides and featuring slits towards the center, allowing a gap between the support and the piezoelectric film, along with a base film and specific electrode configurations, enhances resonance frequency and detection accuracy.

Benefits of technology

The design increases resonance frequency, expands the frequency range for maintaining detection sensitivity, and improves overall detection accuracy by reducing noise and enhancing signal extraction.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024133375000001_ABST
    Figure 2024133375000001_ABST
Patent Text Reader

Abstract

To improve the detection accuracy.SOLUTION: A piezoelectric element includes a supporter 10, and a vibration part 20 disposed on the supporter 10 and including a piezoelectric film 50 and an electrode film 60 connected to the piezoelectric film 50 and extracting charges generated by deformation of the piezoelectric film 50, including a support region 21a supported by the supporter and a vibration region 22 connected to the support region 21a and floating from the supporter 10, and outputting a pressure detection signal based on the charges. The vibration region 22 has a plurality of slits formed from the support region 21a side toward a central part C in the vibration region 22, and is supported on both sides with respect to the support region 21a. A base film 70 is provided between the supporter 10 and the piezoelectric film 50.SELECTED DRAWING: Figure 1A
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a piezoelectric element and a piezoelectric device having a vibration region. [Background technology]

[0002] Conventionally, piezoelectric elements having a vibration region have been proposed (see, for example, Patent Document 1). Specifically, the vibration region of this piezoelectric element is configured to include a piezoelectric film and an electrode film connected to the piezoelectric film, and is supported in a cantilevered manner. In such a piezoelectric element, the vibration region vibrates due to acoustic pressure (hereinafter also simply referred to as sound pressure), etc., which causes the piezoelectric film to deform and generates an electric charge in the piezoelectric film. Therefore, the sound pressure applied to the vibration region can be detected by extracting the electric charge generated in the piezoelectric film via the electrode film. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Patent No. 5936154 Summary of the Invention [Problem to be solved by the invention]

[0004] However, there is a demand for improving the detection accuracy of the above-mentioned piezoelectric element.

[0005] In view of the above, an object of the present invention is to provide a piezoelectric element and a piezoelectric device that can improve detection accuracy. [Means for solving the problem]

[0006] Claim 1 for achieving the above object is a piezoelectric element having a vibration part (20) that outputs a pressure detection signal according to pressure, the vibration part having a support (10), a piezoelectric film (50) arranged on the support, and an electrode film (60) connected to the piezoelectric film and extracting electric charge generated by deformation of the piezoelectric film, the vibration part having a support region (21a) supported by the support, and a vibration region (22) connected to the support region and floating above the support, the vibration region having a plurality of slits (40-44) formed from the support region side toward a center (C) of the vibration region, and supported at both ends by the support region, and a base film (70) is provided between the support and the piezoelectric film.

[0007] This allows the resonance frequency to be increased compared to when the vibration region is cantilevered, thereby broadening the frequency range over which detection sensitivity can be maintained and improving detection accuracy.

[0008] Claim 3 is a piezoelectric device comprising a piezoelectric element having a vibration portion (20) that outputs a pressure detection signal according to pressure, comprising the piezoelectric element according to claim 1 or 2, a mounted member (101) on which the piezoelectric element is mounted, and a lid portion (102) fixed to the mounted member while accommodating the piezoelectric element, and a casing (100) having a through hole (101b) formed therein that communicates with the outside and through which pressure is introduced, and the slit is formed in a portion of the vibration area different from the portion facing the through hole.

[0009] According to this, since the piezoelectric element capable of increasing the resonance frequency is provided, the frequency range in which detection sensitivity can be maintained can be widened, and detection accuracy can be improved.

[0010] The reference symbols in parentheses attached to each component indicate an example of the correspondence between the component and specific components described in the embodiments described below. [Brief description of the drawings]

[0011] [Figure 1A] 1 is a cross-sectional view of a piezoelectric element according to a first embodiment. [Figure 1B] 1 is a cross-sectional view of a piezoelectric element according to a first embodiment. [Figure 1C] 1 is a cross-sectional view of a piezoelectric element according to a first embodiment. [Figure 2A] FIG. 2 is a plan view of a piezoelectric element according to the first embodiment. [Figure 2B] 4 is a plan view of an electrode film formed in a first region in the first embodiment. FIG. [Diagram 3] FIG. 2 is a schematic circuit diagram of a piezoelectric element in the first embodiment. [Figure 4A] 1C。 A method for manufacturing the piezoelectric element shown in FIG. [Figure 4B] This is a method for manufacturing a piezoelectric element following FIG. 4A. [Figure 4C] This is a method for manufacturing a piezoelectric element following FIG. 4B. [Diagram 5] 1 is a cross-sectional view of a piezoelectric device according to a first embodiment. [Figure 6] FIG. 13 is a diagram showing the relationship between the connection length and the resonance frequency of a piezoelectric element. [Figure 7] FIG. 13 is a diagram showing the relationship between the frequency applied to the vibration region and the output signal. [Figure 8] FIG. 13 is a diagram showing the relationship between connection length and generated stress ratio. [Figure 9] FIG. 4 is a diagram showing the relationship between sound pressure and output signal. [Figure 10A] FIG. 4 is a plan view of a piezoelectric element in a modified example of the first embodiment. [Figure 10B] FIG. 4 is a plan view of a piezoelectric element in a modified example of the first embodiment. [Figure 11A] FIG. 11 is a plan view of a vibration region in a modified example of the first embodiment. [Figure 11B] FIG. 11 is a plan view of a vibration region in a modified example of the first embodiment. [Figure 11C] FIG. 11 is a plan view of a vibration region in a modified example of the first embodiment. [Figure 11D] FIG. 11 is a plan view of a vibration region in a modified example of the first embodiment. [Figure 11E] FIG. 11 is a plan view of a vibration region in a modified example of the first embodiment. [Figure 11F] FIG. 11 is a plan view of a vibration region in a modified example of the first embodiment. [Figure 11G] FIG. 11 is a plan view of a vibration region in a modified example of the first embodiment. [Figure 12] 13 is a plan view of an electrode film formed in a first region in a modified example of the first embodiment. FIG. [Figure 13] 13 is a schematic circuit diagram of a piezoelectric element having the electrode film shown in FIG. 12. [Figure 14] FIG. 11 is a plan view of a piezoelectric element according to a second embodiment. [Figure 15] 13 is a schematic diagram of a vibration region described in a third embodiment. FIG. [Figure 16] FIG. 4 is a schematic diagram showing the magnitude of bending moment in a vibration region. [Figure 17] FIG. 13 is a diagram showing stress distribution in a vibration region. [Figure 18] FIG. 11 is a plan view of a piezoelectric element according to a third embodiment. [Figure 19] 19 is a schematic circuit diagram of the piezoelectric element shown in FIG. 18. [Figure 20] FIG. 13 is a cross-sectional view of a piezoelectric element according to a fourth embodiment. [Figure 21] FIG. 21 is a plan view of the piezoelectric element shown in FIG. [Figure 22] FIG. 13 is a cross-sectional view of a piezoelectric element according to a fifth embodiment. [Diagram 23] FIG. 23 is a plan view of the piezoelectric element shown in FIG. 22. [Figure 24A] FIG. 13 is a plan view of a piezoelectric element in a sixth embodiment. [Figure 24B] FIG. 13 is a plan view of an electrode film formed in a first region in the sixth embodiment. [Diagram 25] FIG. 13 is a schematic circuit diagram of a piezoelectric element in a sixth embodiment. [Figure 26] FIG. 13 is a cross-sectional view of a piezoelectric element according to a sixth embodiment. [Figure 27] FIG. 13 is a plan view of a piezoelectric element in a modified example of the sixth embodiment. [Figure 28] FIG. 23 is a plan view of an electrode film formed in a first region in a modified example of the sixth embodiment. [Figure 29] FIG. 13 is a schematic circuit diagram of a piezoelectric element in a modified example of the sixth embodiment. [Diagram 30] FIG. 13 is a plan view of a piezoelectric element in a seventh embodiment. [Diagram 31] FIG. 13 is a cross-sectional view of a piezoelectric device according to a seventh embodiment. [Diagram 32] FIG. 13 is a schematic cross-sectional view of a piezoelectric device according to an eighth embodiment. [Diagram 33] 11 is a diagram showing the relationship between the slit width, the slit length, and the acoustic resistance when the thickness of the vibration region is constant. FIG. [Diagram 34] 11 is a diagram showing the relationship between the thickness of the vibration region, the slit length, and the acoustic resistance when the slit width is constant. FIG. [Diagram 35] FIG. 13 is a diagram showing the relationship between a slit length and an acoustic resistance ratio. [Diagram 36] FIG. 13 is a cross-sectional view of a slit of a piezoelectric element in a ninth embodiment. [Figure 37] FIG. 13 is a diagram showing the relationship between the slit width on one surface side and acoustic resistance. [Figure 38A] FIG. 13 is a cross-sectional view of a slit of a piezoelectric element in a modified example of the ninth embodiment. [Figure 38B] FIG. 13 is a cross-sectional view of a slit of a piezoelectric element in a modified example of the ninth embodiment. [Figure 38C] FIG. 13 is a cross-sectional view of a slit of a piezoelectric element in a modified example of the ninth embodiment. [Figure 39] FIG. 23 is a plan view showing the positional relationship between a piezoelectric element and a bonding member in a tenth embodiment. [Figure 40A] FIG. 23 is a plan view showing the positional relationship between a piezoelectric element and a bonding member in a modified example of the tenth embodiment. [Figure 40B] FIG. 23 is a plan view showing the positional relationship between a piezoelectric element and a bonding member in a modified example of the tenth embodiment. [Figure 41A] FIG. 23 is a plan view showing the positional relationship between a piezoelectric element and a bonding member in a modified example of the tenth embodiment. [Figure 41B] FIG. 23 is a plan view showing the positional relationship between a piezoelectric element and a bonding member in a modified example of the tenth embodiment. [Figure 41C] FIG. 23 is a plan view showing the positional relationship between a piezoelectric element and a bonding member in a modified example of the tenth embodiment. [Diagram 42] FIG. 23 is a cross-sectional view of a piezoelectric device according to an eleventh embodiment. [Diagram 43] FIG. 23 is a cross-sectional view of a piezoelectric element according to a twelfth embodiment. [Figure 44A] 44A to 44C are cross-sectional views showing a manufacturing process of the piezoelectric element shown in FIG. [Figure 44B] 44B is a cross-sectional view showing a manufacturing process of the piezoelectric element subsequent to FIG. 44A. [Figure 44C] FIG. 44C is a cross-sectional view showing a manufacturing process of the piezoelectric element subsequent to FIG. 44B. [Diagram 45] FIG. 44D is a schematic diagram of a portion where a slit is formed in the manufacturing process of FIG. 44C. [Diagram 46] FIG. 13 is a diagram showing the relationship between frequency, sensitivity, and effective width. [Figure 47] 11 is a diagram showing the relationship between the film thickness of an etching mask material and the angle formed with respect to the film thickness of a piezoelectric film. [Figure 48] FIG. 11 is a cross-sectional view of a piezoelectric device according to another embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0012] Hereinafter, embodiments of the present invention will be described with reference to the drawings. In the following embodiments, parts that are the same or equivalent to each other will be denoted by the same reference numerals.

[0013] (First embodiment) The piezoelectric element 1 of the first embodiment will be described with reference to FIGS. 1A, 1B, 1C, 2A, and 2B. The piezoelectric element 1 of the present embodiment is preferably used as a microphone, for example. FIG. 1A corresponds to a cross-sectional view taken along line IA-IA in FIG. 2A, FIG. 1B corresponds to a cross-sectional view taken along line IB-IB in FIG. 2A, and FIG. 1C corresponds to a cross-sectional view taken along line IC-IC in FIG. 2A. In FIG. 2A, the first electrode portion 81 and the second electrode portion 82, which will be described later, are omitted. In each of the figures corresponding to FIG. 2A, which will be described later, the first electrode portion 81 and the second electrode portion 82, etc. are omitted as appropriate.

[0014] The piezoelectric element 1 of this embodiment includes a support 10 and a vibration part 20, and has a rectangular planar shape. The support 10 includes a support substrate 11 having one surface 11a and the other surface 11b, and an insulating film 12 formed on the one surface 11a of the support substrate 11. The support substrate 11 is made of, for example, a silicon substrate, and the insulating film 12 is made of, for example, an oxide film.

[0015] The vibration part 20 constitutes the sensing part 30 that outputs a pressure detection signal corresponding to sound pressure or the like as pressure, and is disposed on the support 10. The support 10 is formed with a recess 10a for floating the inner edge side of the vibration part 20. Therefore, the vibration part 20 has a support region 21a disposed on the support 10, and a floating region 21b that is connected to the support region 21a and floats on the recess 10a. Note that the recess 10a in this embodiment has an opening end on the vibration part 20 side (hereinafter, simply referred to as the opening end of the recess 10a) that is rectangular in plan view. Therefore, the entire floating region 21b is rectangular in plan view.

[0016] In addition, the floating region 21b is formed with slits 40 penetrating the floating region 21b in the thickness direction. In this embodiment, the floating region 21b is formed with first to fourth slits 41 to 44. The first to fourth slits 41 to 44 extend from each corner of the floating region 21b, which is rectangular in plan view, toward the center C of the floating region 21b. However, the first to fourth slits 41 to 44 are formed so as not to reach the center C. In other words, the first to fourth slits 41 to 44 are formed so as to terminate closer to the support region 21a than the center C. That is, the first to fourth slits 41 to 44 are formed so as not to divide the floating region 21b.

[0017] In this embodiment, the first to fourth slits 41 to 44 are formed so that the slit lengths L along the extension direction are equal to each other. Furthermore, the first to fourth slits 41 to 44 in this embodiment have a constant slit width g along the thickness direction of the vibrating region 22. The vibrating region 22 is configured by such floating region 21b, and the vibrating region 22 is supported at both ends by the supporting region 21a.

[0018] The slit width g of the first to fourth slits 41 to 44 is a length in a direction perpendicular to the extension direction of the first to fourth slits 41 to 44 and along the surface direction of the vibrating region 22. In other words, the slit width g of the first to fourth slits 41 to 44 is the distance between the side surfaces 22c of the vibrating region 22 exposed by the first slits 41 to 44.

[0019] Hereinafter, the surface of the vibrating region 22 opposite to the support 10 is referred to as one surface 22a of the vibrating region 22, and the surface of the vibrating region 22 on the support 10 side is referred to as the other surface 22b of the vibrating region 22. Similarly, the surface of the vibrating region 22 exposed from the first to fourth slits 41 to 44 is referred to as the side surface 22c of the vibrating region 22. In addition, in the normal direction to the one surface 22a of the vibrating region 22, the areas surrounded by one side forming the outline of the vibrating region 22 and the virtual lines K1 and K2 extending along the slits 41 to 44 are referred to as the first to fourth vibrating regions 221 to 224. In addition, in the following, the normal direction to the one surface 22a of the vibrating region 22 is also simply referred to as the normal direction. In other words, the normal direction to the one surface 22a of the vibrating region 22 can be referred to as when viewed from the normal direction to the one surface 22a of the vibrating region 22.

[0020] In this embodiment, a virtual line extending along the first slit 41 and the third slit 43 is defined as a virtual line K1, and a virtual line extending along the second slit 42 and the fourth slit 44 is defined as a virtual line K2. In the normal direction, a region of the vibration region 22 that includes the area between the first slit 41 and the second slit 42 and is surrounded by the virtual lines K1 and K2 is defined as a first vibration region 221. In the normal direction, a region of the vibration region 22 that includes the area between the second slit 42 and the second slit 43 and is surrounded by the virtual lines K1 and K2 is defined as a second vibration region 222. In the normal direction, a region of the vibration region 22 that includes the area between the third slit 43 and the fourth slit 44 and is surrounded by the virtual lines K1 and K2 is defined as a third vibration region 223. In the normal direction, a region of the vibration region 22 that includes a portion between the fourth slit 44 and the first slit 41 and is surrounded by the virtual lines K1 and K2 is defined as a fourth vibration region 224. The vibration region 22 of this embodiment is formed by integrating the first to fourth vibration regions 221 to 224.

[0021] The vibration section 20 has a configuration including a piezoelectric film 50 and an electrode film 60 connected to the piezoelectric film 50. Specifically, the piezoelectric film 50 has a lower layer piezoelectric film 51 and an upper layer piezoelectric film 52 laminated on the lower layer piezoelectric film 51. The electrode film 60 has a lower layer electrode film 61 arranged below the lower layer piezoelectric film 51, an intermediate electrode film 62 arranged between the lower layer piezoelectric film 51 and the upper layer piezoelectric film 52, and an upper layer electrode film 63 arranged on the upper layer piezoelectric film 52. In other words, the vibration section 20 has a bimorph structure in which the lower layer piezoelectric film 51 is sandwiched between the lower layer electrode film 61 and the intermediate electrode film 62, and the upper layer piezoelectric film 52 is sandwiched between the intermediate electrode film 62 and the upper layer electrode film 63.

[0022] The lower piezoelectric film 51 and the upper piezoelectric film 52 are made of lead-free piezoelectric ceramics such as scandium aluminum nitride (ScAlN) and aluminum nitride (AlN). The lower electrode film 61, the intermediate electrode film 62, and the upper electrode film 63 are made of molybdenum, copper, platinum, titanium, or the like.

[0023] Furthermore, the vibration section 20 of this embodiment has an undercoat film 70 on which the lower piezoelectric film 51 and the lower electrode film 61 are disposed. That is, the piezoelectric film 50 and the electrode film 60 are disposed on the support 10 via the undercoat film 70. The undercoat film 70 is not necessarily required, but is provided to facilitate crystal growth when forming the lower piezoelectric film 51 and the like. In this embodiment, the undercoat film 70 is made of aluminum nitride or the like. The piezoelectric film 50 has a thickness of about 1 μm, and the undercoat film 70 has a thickness of about several tens of nm. That is, the undercoat film 70 is made extremely thin compared to the piezoelectric film 50.

[0024] In addition, in each vibrating region 22 of this embodiment, the portion on the support region 21a side that becomes the fixed end when the vibrating region 22 vibrates is the first region R1, and the portion on the center C side is the second region R2. The lower electrode film 61, the intermediate electrode film 62, and the upper electrode film 63 are formed in the first region R1 and the second region R2, respectively. However, the lower electrode film 61, the intermediate electrode film 62, and the upper electrode film 63 formed in the first region R1 are separated from the lower electrode film 61, the intermediate electrode film 62, and the upper electrode film 63 formed in the second region R2, and are insulated. The lower electrode film 61, the intermediate electrode film 62, and the upper electrode film 63 formed in the first region R1 are appropriately extended to the support region 21a.

[0025] In this embodiment, the lower electrode film 61, the intermediate electrode film 62, and the upper electrode film 63 are formed so as not to reach the first to fourth slits 41 to 44. That is, the lower electrode film 61, the intermediate electrode film 62, and the upper electrode film 63 are formed so as to terminate on the inner side of the side surface 22c exposed from the first to fourth slits 41 to 44 of the vibration region 22. In other words, the lower electrode film 61, the intermediate electrode film 62, and the upper electrode film 63 are disposed on the inner side of the first to fourth slits 41 to 44 in the normal direction. Therefore, the side surface 22c of the vibration region 22 is composed of the lower piezoelectric film 51, the upper piezoelectric film 52, and the base film 70.

[0026] In the support region 21a of the vibration section 20, a first electrode section 81 electrically connected to the lower electrode film 61 and the upper electrode film 63 formed in the first region R1, and a second electrode section 82 electrically connected to the intermediate electrode film 62 formed in the first region R1 are formed. As described above, the first electrode section 81 and the second electrode section 82 are omitted in FIG. 2A.

[0027] The first electrode portion 81 has a through electrode 81b formed in a hole portion 81a penetrating the upper layer electrode film 63, the upper layer piezoelectric film 52, and the lower layer piezoelectric film 51, and electrically connected to the lower layer electrode film 61 and the upper layer electrode film 63. In this embodiment, the through electrode 81b is electrically connected to the lower layer electrode film 61 and the upper layer electrode film 63 formed in the first vibration region 221. In addition, the first electrode portion 81 has a pad portion 81c formed on the through electrode 81b and electrically connected to the through electrode 81b.

[0028] The second electrode portion 82 is formed in a hole portion 82a that penetrates the upper piezoelectric film 52 to expose the intermediate electrode film 62, and has a through electrode 82b electrically connected to the intermediate electrode film 62. In this embodiment, the through electrode 82b is electrically connected to the intermediate electrode film 62 formed in the fourth vibration region 224. In addition, the second electrode portion 82 has a pad portion 82c that is formed on the through electrode 82b and electrically connected to the through electrode 82b.

[0029] The first electrode portion 81 and the second electrode portion 82 are made of molybdenum, copper, platinum, titanium, aluminum, or the like, similarly to the electrode film 60. The lower electrode film 61, the intermediate electrode film 62, and the upper electrode film 63 formed in the second region R2 are not electrically connected to the respective electrode portions 81 and 82, and are in a floating state. For this reason, the lower electrode film 61, the intermediate electrode film 62, and the upper electrode film 63 formed in the second region R2 are not necessarily required, but in this embodiment, they are provided to protect the portions of the lower piezoelectric film 51 and the upper piezoelectric film 52 located in the second region R2.

[0030] The lower electrode film 61, the intermediate electrode film 62, and the upper electrode film 63 formed in the first region R1 are divided by the first to fourth vibration regions 221 to 224. That is, the lower electrode film 61, the intermediate electrode film 62, and the upper electrode film 63 formed in the first region R1 are not formed so as to straddle the first to fourth vibration regions 221 to 224. The lower electrode film 61, the intermediate electrode film 62, and the upper electrode film 63 formed in the first region R1 of each of the vibration regions 221 to 224 are connected via a wiring film or the like (not shown).

[0031] In addition, as shown in FIG. 2B, the lower electrode film 61, the intermediate electrode film 62, and the upper electrode film 63 in this embodiment are formed so that the outer shape of the part formed in the first region R1 is approximately equal to the outer shape of the vibration region 22, and in this embodiment, they are formed in a planar rectangular shape. However, the lower electrode film 61, the intermediate electrode film 62, and the upper electrode film 63 are divided into the first to fourth vibration regions 221 to 224 as described above. Therefore, the outer shapes of the parts of the lower electrode film 61, the intermediate electrode film 62, and the upper electrode film 63 formed in the first region R1 here refer to shapes formed by the outer lines of the parts of the lower electrode film 61, the intermediate electrode film 62, and the upper electrode film 63 located in the first region R1 and the extension lines of the outer lines. In addition, although FIG. 2B is not a cross-sectional view, the electrode film 60 formed in the first region R1 is hatched to make it easier to understand. Furthermore, while FIG. 2B shows an electrode film 60, the lower electrode film 61, intermediate electrode film 62, and upper electrode film 63 that make up the electrode film 60 each have the same shape as the electrode film 60 in FIG. 2B in the first region R1.

[0032] The piezoelectric element 1 of this embodiment is configured to output the change in charge in the first to fourth vibration regions 221 to 224 as one pressure detection signal. Specifically, each vibration region 221 to 224 has a bimorph structure, and as shown in FIG. 3, the lower electrode film 61, the intermediate electrode film 62, and the upper electrode film 63 formed in each vibration region 22 are connected in parallel, while the vibration regions 22 are connected in series. The piezoelectric element 1 outputs the potential difference between the first electrode portion 81 and the second electrode portion 82 as a pressure detection signal. In this case, for example, the second electrode portion 82 is connected to the ground, and the piezoelectric element 1 outputs the potential difference between the ground and the first electrode portion 81 as a pressure detection signal.

[0033] Next, a method for manufacturing such a piezoelectric element 1 will be briefly described with reference to Figures 4A, 4B, and 4C. Figures 4A to 4C are cross-sectional views of a portion corresponding to Figure 1C.

[0034] First, as shown in FIG. 4A, a support 10 having a support substrate 11 and an insulating film 12 is prepared on which a base film 70, a piezoelectric film 50, an electrode film 60, a first electrode portion 81, a second electrode portion 82, and the like are formed. That is, a piezoelectric element 1 shown in FIG. 1C is prepared in which the recess 10a and the first to fourth slits 41 to 44 are not formed. The piezoelectric film 50 and the electrode film 60 formed in the process of FIG. A are parts that constitute the vibration portion 20. For this reason, in FIG. 4A, the same reference numerals are given to the one surface 22a and the other surface 22b of the vibration region 22. The first electrode portion 81 and the second electrode portion 82 are formed on a cross section different from that in FIG. 4A.

[0035] Here, the undercoat film 70, the piezoelectric film 50, the electrode film 60, etc. are formed by appropriately performing general sputtering, etching, etc. In this case, when the undercoat film 70 and the lower electrode film 61 as the electrode film 60 are formed on the support 10, the undercoat film 70 and the lower electrode film 61 are formed in a state in which tensile stress remains because the linear expansion coefficients of the undercoat film 70 and the lower electrode film 61 are greater than the linear expansion coefficient of the support 10. Therefore, if the piezoelectric film 50 is formed as it is, the piezoelectric film 50 is likely to be formed in a state in which tensile stress resulting from the tensile stress of the undercoat film 70 and the lower electrode film 61 remains. If tensile stress remains in the piezoelectric film 50, the characteristics of the piezoelectric element 1 are likely to fluctuate. Therefore, when forming the piezoelectric film 50, for example, it is preferable to do the following.

[0036] For example, when forming the upper piezoelectric film 52, it is preferable to apply a higher voltage during sputtering than when forming the lower piezoelectric film 51, so that compressive stress is generated in the upper piezoelectric film 52. This offsets the tensile stress of the lower piezoelectric film 51 and the compressive stress of the upper piezoelectric film 52, thereby reducing the stress remaining inside the piezoelectric film 50 as a whole. In this case, the upper piezoelectric film 52 may be formed by multiple sputtering operations. Then, the upper piezoelectric film 52 may be made to generate tensile stress in the portion of the upper piezoelectric film 52 on the lower piezoelectric film 51 side and compressive stress in the portion on the top layer side opposite the lower piezoelectric film 51, thereby reducing the stress remaining inside the piezoelectric film 50.

[0037] Next, as shown in FIG. 4B, anisotropic dry etching is performed using a mask (not shown) to form first to fourth slits 41 to 44 that penetrate the piezoelectric film 50 and reach the support 10. As a result, a vibration region component 220 that becomes the vibration region 22 by forming a recess 10a described later is formed. The second and third slits 43 and 44 are formed on a cross section different from that of FIG. 4B. The vibration region component 220 is a portion that becomes the vibration region 22 by forming the recess 10a. For this reason, in the drawing, the same reference numerals as the one surface 22a, the other surface 22b, and the side surface 22c of the vibration region 22 are assigned to one surface, the other surface, and the side surface of the vibration region component 220.

[0038] 4C, a mask (not shown) is used to etch from the other surface 11b of the support substrate 11 through the insulating film 12 to reach the base film 70, forming the recess 10a. In this embodiment, the support substrate 11 is removed by anisotropic dry etching, and then the insulating film 12 is removed by isotropic wet etching to form the recess 10a. As a result, the vibration region forming portion 220 is suspended from the support 10 to form the vibration region 22, and the piezoelectric element 1 shown in FIG. 1 is manufactured.

[0039] In this step, although not shown, a protective resist or the like may be disposed to cover the upper piezoelectric film 52 and the upper electrode film 63 to form the recess 10a. This can prevent the vibration region 22 from being destroyed when the recess 10a is formed. However, the protective resist is removed after the recess 10a is formed.

[0040] The above is the configuration of the piezoelectric element 1 in this embodiment. Next, a piezoelectric device S10 using such a piezoelectric element 1 will be described.

[0041] 5, the piezoelectric device of this embodiment is configured by housing a piezoelectric element 1 in a casing 100. The casing 100 has a printed circuit board 101 on which the piezoelectric element 1 and a circuit board 110 that performs predetermined signal processing and the like are mounted, and a lid 102 fixed to the printed circuit board 101 so as to house the piezoelectric element 1 and the circuit board 110. In this embodiment, the printed circuit board 101 corresponds to a mounted member.

[0042] Although not shown in particular, the printed circuit board 101 is configured to have wiring parts and through-hole electrodes appropriately formed, and also has electronic components such as capacitors (not shown) mounted as necessary. The piezoelectric element 1 is mounted on one surface 101a of the printed circuit board 101 via a bonding member 2 such as an adhesive on the other surface 11b of the support substrate 11. The circuit board 110 is mounted on one surface 101a of the printed circuit board 101 via a bonding member 111 made of a conductive material. The pad portion 81c of the piezoelectric element 1 and the circuit board 110 are electrically connected via a bonding wire 120. The pad portion 82c of the piezoelectric element 1 is electrically connected to the circuit board 110 via the bonding wire 120 in a cross section different from that of FIG. 5. The lid portion 102 is made of metal, plastic, resin, or the like, and is fixed to the printed circuit board 101 via a bonding member such as an adhesive (not shown) so as to accommodate the piezoelectric element 1 and the circuit board 110.

[0043] In this embodiment, a through hole 101b communicating with an external space is formed in a portion of the printed circuit board 101 facing the sensing unit 30. Specifically, the through hole 101b is substantially cylindrical, and is formed so that its central axis coincides with the center C of the vibration region 22 in the normal direction.

[0044] The above is the configuration of the piezoelectric device S10 in this embodiment. Hereinafter, the space between the part where the through hole 101b is formed and the vibration region 22 in the casing 100 is referred to as the pressure-receiving surface space S1. Also, the space including the space located on the opposite side of the vibration region 22 to the pressure-receiving surface space S1 and connected to the space without the slit 40 is referred to as the back space S2. Note that the back space S2 can be said to be a space different from the pressure-receiving surface space S1 in the space in the casing 100, and can also be said to be a space excluding the pressure-receiving surface space S1. In other words, the pressure-receiving surface space S1 can be said to be a space that affects the pressing of the surface on the side of the through hole 101b formed in the casing 100 in the vibration region 22 (i.e., the other surface 22b in this embodiment). The back space S2 can be said to be a space that affects the pressing of the surface on the opposite side of the through hole 101b formed in the casing 100 in the vibration region 22 (i.e., the one surface 22a in this embodiment).

[0045] Next, the operation and effects of the piezoelectric device S10 will be described.

[0046] In the piezoelectric device S10 of this embodiment, when sound pressure as pressure is introduced into the pressure-receiving surface space S1 and the sound pressure is applied to the vibration region 22 (i.e., the sensing portion 30), the vibration region 22 vibrates. Then, electric charges are generated in the lower-layer piezoelectric film 51 and the upper-layer piezoelectric film 52 based on stress according to the displacement of the vibration region 22. Therefore, in such a piezoelectric device S10, the sound pressure is detected by extracting the electric charges from the first electrode portion 81 and the second electrode portion 82.

[0047] At this time, the stress generated in the vibration region 22 (i.e., the piezoelectric film 50) is likely to be larger on the fixed end side where the vibration region 22 is supported than in the central portion C. For this reason, in the piezoelectric element 1 of this embodiment, the vibration region 22 is divided into a first region R1 where the stress is likely to be large and a second region R2 where the stress is likely to be small, as described above. In the piezoelectric element 1, the lower electrode film 61, the upper electrode film 63, and the intermediate electrode film 62 arranged in the first region R1 are connected to the first and second electrode portions 81 and 82, so that the electric charges generated in the lower piezoelectric film 51 and the upper piezoelectric film 52 located in the first region R1 can be extracted. This makes it possible to suppress the influence of noise from becoming too large.

[0048] Here, the resonant frequency f of the vibration region 22 in the piezoelectric element 1 (hereinafter also simply referred to as the resonant frequency f of the piezoelectric element 1) depends on the spring constant k of the vibration region 22 which serves as a beam and the mass m of the vibration region 22, and is expressed by the following formula 1.

[0049]

number

[0050] 2A, the length between the first slit 41 and the center C of the vibrating region 22 is defined as a first length X, and the length between the second slit 42 and the center C of the vibrating region 22 is defined as a second length Y. In this embodiment, since the slit lengths L of the first to fourth slits 41 to 44 are equal as described above, the first length X and the second length Y are equal. If the sum of the first length X and the second length Y is defined as the connection length (i.e., X+Y), the relationship between the connection length and the resonant frequency f is shown in FIG.

[0051] Specifically, when the vibration region 22 is supported at both ends, the spring constant (i.e., rigidity) increases as the connection length increases, and therefore, it is confirmed that the resonance frequency f increases compared to when the vibration region 22 is supported at one end. Therefore, as shown in FIG. 7, by adjusting the connection length, the resonance frequency f can be made higher than 20,000 Hz (i.e., 20 kHz), which is an audible range. In other words, by adjusting the connection length, it becomes possible to make the resonance frequency f exist at a frequency higher than the frequency at which the output signal becomes +3 dB when the output signal is set to a reference (i.e., 0 dB) when the frequency is 1,000 Hz (i.e., 1 kHz). This makes it possible to widen the frequency range in which the detection sensitivity can be maintained. However, since the thickness of the piezoelectric film 50 of the vibration region 22 of this embodiment is set to about 1 μm, when the connection length becomes about 300 μm, the resonance frequency f is saturated at about 22.5 kHz. In addition, by allowing the low-frequency roll-off frequency to exist at frequencies where the output signal is smaller than -3 dB, the frequency range in which detection sensitivity can be maintained can be further expanded. This low-frequency roll-off frequency will be specifically described in the eighth embodiment described later.

[0052] On the other hand, as shown in FIG. 8, the longer the connection length, the larger the spring constant becomes, and the more difficult it is for the vibration region 22 to deform, so the stress ratio decreases. In other words, the longer the connection length, the lower the sensitivity becomes. In this case, as shown in FIG. 9, if the frequency of the input sound pressure is constant, the AOP (short for Acoustic Over Point) can be increased by lowering the sensitivity. Therefore, it is preferable that the connection length is adjusted according to the application. The stress ratio in FIG. 8 is based on the stress generated at the boundary between the vibration region 22 and the support region 21a when the vibration region 22 is supported at one end. The stress ratio indicates the ratio of the stress generated at the boundary between the vibration region 22 and the support region 21a when the vibration region 22 is supported at both ends to the reference stress.

[0053] According to the present embodiment described above, the vibration region 22 of the piezoelectric element 1 is supported at both ends. Therefore, compared to the case where the vibration region 22 is supported at one end, the resonance frequency f can be made larger. Therefore, the frequency range in which detection sensitivity can be maintained can be widened, and the detection accuracy can be improved.

[0054] (1) In this embodiment, the resonant frequency f of the piezoelectric element 1 can be set to 20 kHz or more. Therefore, in such a piezoelectric element 1, the resonant frequency f can be set outside the audible range, and the frequency range in which detection sensitivity can be maintained in the audible range can be expanded.

[0055] (Modification of the first embodiment) A modified example of the first embodiment will be described. As described above, it is preferable that the connection length is appropriately adjusted depending on the relationship between the application and the detection sensitivity. In this case, as shown in FIG. 10A, the first slit 41 and the third slit 43 and the second slit 42 and the fourth slit 44 may be formed so that their slit lengths L are different. The first length X and the second length Y may not be the same distance, and the first length X may be shorter than the second length Y. Although not particularly shown, the first length X and the second length Y may be longer than the second length Y.

[0056] 10B, the first to fourth slits 41 to 44 may be formed only in the first region R1 of the vibration region 22. Although not particularly shown, the first to fourth slits 41 to 44 may be formed to have different slit lengths L.

[0057] In this manner, in the piezoelectric element 1 of this embodiment, the slit length L of the first to fourth slits 41 to 44 can be changed as appropriate, and can be changed according to the product in which it is to be mounted. Therefore, in the piezoelectric element 1 of this embodiment, it is possible to improve the selectivity of the product in which it is to be mounted.

[0058] In addition, the planar shape of the vibration region 22 can be changed as appropriate. For example, as shown in Figs. 11A to 11G, the planar shape of the vibration region 22 may be a hexagon, an octagon, a decagon, a dodecagon, a tetragon, a hexagon, or a circle. Although not particularly shown, the vibration region 22 may be another polygonal shape. Note that, although the slits 40 formed in the vibration region 22 are omitted in Figs. 11A to 11G, the slits 40 are formed in each of the vibration regions 22. For example, when the planar shape of the vibration region 22 is a hexagon as shown in Fig. 11A, six slits 40 are formed from each corner of the outer shape of the vibration region 22 toward the center C. When the planar shape of the vibration region 22 is a circle as shown in Fig. 11G, a desired number of slits 40 are formed evenly in the circumferential direction.

[0059] Furthermore, as shown in FIG. 12, the electrode film 60 may be divided into a plurality of charge regions 60a in the first region R1. For example, the electrode film 60 may be divided into three charge regions 60a in the first region R1 of each of the vibration regions 221-224. The lower electrode film 61, the intermediate electrode film 62, and the upper electrode film 63 that constitute the electrode film 60 are each divided into charge regions 60a as shown in FIG. 12 in the first region R1. In this case, as shown in FIG. 13, the piezoelectric element 1 is in a state in which the capacitances formed by the divided charge regions 60a are connected in series. This makes it possible to reduce the capacitance in each of the vibration regions 221-224, thereby improving the output. In other words, it is possible to improve the detection sensitivity.

[0060] Second embodiment The second embodiment will be described. This embodiment is different from the first embodiment in that the shapes of the first to fourth slits 41 to 44 are changed. As the rest is the same as the first embodiment, the description will be omitted here.

[0061] In the piezoelectric element 1 of this embodiment, as shown in FIG. 14, the first to fourth slits 41 to 44 are tapered in the normal direction such that the slit width g narrows toward the center C.

[0062] According to the present embodiment described above, the vibration region 22 is supported at both ends. This makes it possible to increase the resonance frequency f of the piezoelectric element 1, thereby achieving the same effects as those of the first embodiment.

[0063] (1) In this embodiment, the first to fourth slits 41 to 44 are tapered such that the slit width g narrows toward the center C of the vibration region 22. Therefore, when sound pressure is applied to the vibration region 22 and the vibration region 22 is bent, the slit width g of the first to fourth slits 41 to 44 in the bent state is easily uniformed. In other words, when the vibration region 22 is bent, the slit width g of the first to fourth slits 41 to 44 is easily uniformed in the normal direction between the portion on the support region 21a side and the portion on the center C side. Therefore, differences in the ease with which local sound pressure escapes are less likely to occur within the first to fourth slits 41 to 44, and noise can be reduced. This can further improve the detection accuracy.

[0064] Third embodiment A third embodiment will be described. This embodiment is different from the first embodiment in that the method of dividing the first region R1 and the second region R2 is changed. As the rest is the same as the first embodiment, the description will be omitted here.

[0065] The piezoelectric element 1 of this embodiment has the same configuration as the first embodiment, and the vibration region 22 is supported at both ends. Here, as shown in FIG. 15, it is assumed that sound pressure is applied from the other surface 22b side of the vibration region 22. In this case, as shown in FIG. 16, the maximum bending moment Mmax occurs in the vibration region 22 on the support region 21a side, and a large bending moment also occurs in the center C. In addition, as shown in FIG. 17, opposite stresses are generated in the lower layer piezoelectric film 51 and the upper layer piezoelectric film 52 of the piezoelectric film 50. In addition, opposite stresses are generated in the outer edge part of the piezoelectric film 50 on the support region 21 side and the inner edge part on the center C side. In other words, opposite stresses are generated in the piezoelectric film 50 in the part located in the first region R1 and the part located on the center C side.

[0066] 18, in this embodiment, the central region 225 including the central portion C of the vibration region 22 and its peripheral portion is also defined as the first region R1, and the charge of the central region 225 is also extracted. Note that the central region 225 can also be said to be a region formed by the regions on the central portion C side of the first to fourth vibration regions 221 to 224.

[0067] Specifically, in this embodiment, as shown in FIG. 19, the charge in the central region 225 is combined with the charges in the first to fourth vibration regions 221 to 224 and output. More specifically, in addition to the first electrode portion 81 and the second electrode portion 82, the piezoelectric element 1 of this embodiment is formed with the third electrode portion 83 and the fourth electrode portion 84. In the central region 225, the lower electrode film 61 and the upper electrode film 63 are electrically connected to the third electrode portion 83, and the intermediate electrode film 62 is connected to the fourth electrode portion 84. The fourth electrode portion 82 connected to the intermediate electrode film 62 is connected to, for example, the ground, similar to the second electrode portion 82. In addition, opposite stresses are generated in the piezoelectric film 50 in a portion located in the first region R1 and a portion located in the central region 225. Therefore, the piezoelectric element 1 outputs the difference between the output based on the potential difference between the first electrode portion 81 and the second electrode portion 82 and the output based on the potential difference between the third electrode portion 83 and the fourth electrode portion 84 as an overall pressure detection signal.

[0068] According to the present embodiment described above, the vibration region 22 is supported at both ends. This makes it possible to increase the resonance frequency f of the piezoelectric element 1, thereby achieving the same effects as those of the first embodiment.

[0069] (1) In this embodiment, the charge is also extracted from the central region 225 of the vibration region 22. This makes it possible to improve the detection sensitivity.

[0070] (Fourth embodiment) A fourth embodiment will be described. This embodiment is different from the first embodiment in that the configuration of the vibration region 22 is changed. As the rest is the same as the first embodiment, the description will be omitted here.

[0071] In the piezoelectric element 1 of this embodiment, as shown in Fig. 20 and Fig. 21, the first to fourth slits 41 to 44 are extended to the center C of the vibration region 22. That is, the first to fourth slits 41 to 44 are formed so as to intersect at the center C. Therefore, the first to fourth vibration regions 221 to 224 are partitioned by the first to fourth slits 41 to 44. Note that Fig. 20 corresponds to a cross-sectional view taken along line XX-XX in Fig. 21. Also, although Fig. 21 is not a cross-sectional view, a connecting member 90, which will be described later, is hatched to facilitate understanding.

[0072] In this embodiment, a connecting member 90 is embedded in and near the center C of the first to fourth slits 41 to 44. In this embodiment, the first to fourth vibration regions 221 to 224 are integrated by this connecting member 90, and the vibration region 22 is supported at both ends by the support region 21a. The connecting member 90 in this embodiment is made of a material with lower rigidity than the piezoelectric film 50, and is made of, for example, a material in which an ionic liquid is mixed with a polyimide component and hardened by heat treatment at about 150°C. Note that the ionic liquid is a liquid salt compound composed of only ions (i.e., anions and cations).

[0073] Such a piezoelectric element 1 is manufactured, for example, as follows. That is, when the first to fourth slits 41 to 44 are formed in the step of FIG. 4B, the first to fourth slits 41 to 44 are made to intersect at the center C of the vibration region 22. Then, photoresist or the like is arranged so as to cover the upper electrode film 63 and the like, and the photoresist is patterned so as to form an opening in the portion where the connecting member 90 is to be arranged. Next, the connecting member 90 is embedded in the first to fourth slits 41 to 44 by a spin coating method or the like, and is hardened by performing a heat treatment. Then, lift-off is performed to remove the photoresist, so that the connecting member 90 is arranged in the first to fourth slits 41 to 44. Then, the step of FIG. 4C is performed to manufacture the piezoelectric element 1 shown in FIG. 20 and FIG. 21.

[0074] According to the present embodiment described above, the vibration region 22 is supported at both ends. This makes it possible to increase the resonance frequency f of the piezoelectric element 1, thereby achieving the same effects as those of the first embodiment.

[0075] (1) As in this embodiment, the vibrating region 22 may be supported at both ends by the connecting members 90.

[0076] (2) In this embodiment, the connecting member 90 is made of a material having a lower rigidity than the piezoelectric film 50. For this reason, the connecting member 90 can be prevented from affecting the detection sensitivity of the piezoelectric element 1.

[0077] Fifth embodiment A fifth embodiment will be described. This embodiment is different from the fourth embodiment in that the configuration of the vibration region 22 is changed. As the rest is the same as the fourth embodiment, a description thereof will be omitted here.

[0078] In the piezoelectric element 1 of this embodiment, as shown in Fig. 22 and Fig. 23, no connecting member 90 is disposed in the first to fourth slits 41 to 44, and a connecting member 91 is disposed on one surface 22a of the vibration region 22. Fig. 22 corresponds to a cross-sectional view taken along line XXII-XXII in Fig. 23. Although Fig. 23 is not a cross-sectional view, a connecting member 91, which will be described later, is hatched to facilitate understanding.

[0079] Specifically, the connecting member 91 is disposed on one surface 22a of the vibrating region 22 so as to cover (i.e., straddle) the center C and the surrounding area of ​​the first to fourth slits 41 to 44. In this embodiment, the first to fourth vibrating regions 221 to 224 are integrated in this manner, and the vibrating region 22 is supported at both ends by the support region 21a. The connecting member 91 is made of a material having a lower rigidity than the piezoelectric film 50, such as polyimide. More specifically, the connecting member 90 is made of polydimethylsiloxane (i.e., PDMS) or the like.

[0080] Such a piezoelectric element 1 is manufactured, for example, as follows. That is, after the first to fourth slits 41 to 44 are formed so as to intersect at the center C of the vibration region 22, the connecting member 91 is arranged by a spin coating method or the like. In this embodiment, the viscosity of the connecting member 91 is adjusted so that the connecting member 91 does not enter the first to fourth slits 41 to 44 when the spin coating method is performed. Next, the connecting member 91 is patterned using a photoresist. Thereafter, the step of FIG. 4C is performed to manufacture the piezoelectric element 1 shown in FIG. 22 and FIG. 23.

[0081] According to the present embodiment described above, the vibration region 22 is supported at both ends. This makes it possible to increase the resonance frequency f of the piezoelectric element 1, thereby achieving the same effects as those of the first embodiment.

[0082] (1) As in this embodiment, the vibrating region 22 may be supported at both ends by the connecting members 91.

[0083] (2) In this embodiment, since the connecting member 91 is made of a material having a lower rigidity than the piezoelectric film 50, the same effects as those of the fourth embodiment can be obtained.

[0084] Sixth embodiment In this embodiment, compared to the first embodiment, the shapes of the vibration region 22 and the intermediate electrode film 62 are adjusted. As the rest is similar to the first embodiment, a description thereof will be omitted here.

[0085] The piezoelectric element 1 of this embodiment will be described with reference to Fig. 24A and Fig. 24B. In Fig. 22, the slits 40 are omitted. However, the slits 40 actually extend from each corner of the planar shape of the vibration region 22 toward the center C, similarly to the first embodiment.

[0086] As shown in FIG. 24A, the vibrating region 22 has a regular octagonal outer shape in the normal direction. That is, the recess 10a of the support 10 has an opening shaped like a regular octagon. The reason why the vibrating region 22 has a regular octagonal shape will be described below. As described above, in this embodiment, the support substrate 11 is made of silicon. Therefore, by making the opening of the recess 10a (i.e., the outer shape of the vibrating region 22) a regular octagon, it is possible to suppress strain concentration at a local location at the opening end of the recess 10a in the support substrate 11 (i.e., the outer end of the vibrating region 22). Therefore, it is possible to suppress strain concentration at a local location at the boundary between the vibrating region 22 and the support region 21a.

[0087] In addition, as shown in FIG. 24B, the electrode film 60 of this embodiment has a regular octagonal outer shape in the normal direction in the portion formed in the first region R1. That is, the electrode film 60 is formed in the first region so that the outer edge portion substantially coincides with the opening end of the recess 10a. The electrode film 60 is separated by the electrode film slits 60b, which are different from the slits 40, in the portion formed in the first region R1. Specifically, six electrode film slits 60b are formed, and a virtual shape (hereinafter, simply referred to as a virtual shape) KS formed by connecting predetermined points in each electrode film slit 60b is formed to be a hexagon. More specifically, the electrode film slits 60b are formed so that a virtual shape KS formed by connecting the portions where each electrode film slit 60b and the outer shape of the electrode film 60 intersect is formed to be a hexagon.

[0088] In this case, the outline of the portion of the electrode film 60 located in the first region R1 refers to a shape formed by the outline of the portion of the electrode film 60 located in the first region R1 and an extension of the outline, as described above.

[0089] The reason why the virtual shape KS of the electrode film 60 is hexagonal will be described below. As described above, the electrode film 60 and the piezoelectric film 50 are stacked and arranged in the order of the lower electrode film 61, the lower piezoelectric film 51, the intermediate electrode film 62, the upper piezoelectric film 52, and the upper electrode film 63. When forming the lower electrode film 61, the intermediate electrode film 62, and the upper electrode film 63, a metal film is formed and then patterned into a desired shape by dry etching using a mask. At this time, although a mask is used, the lower piezoelectric film 51 and the upper piezoelectric film 52, which are the base, may be etched. In this case, when the piezoelectric film 50 is made of ScAlN, AlN, or the like, it has a hexagonal crystal structure, so that by making the virtual shape KS of the electrode film 60 hexagonal, it is possible to suppress the crystallinity of the piezoelectric film 50 from collapsing when the surface of the piezoelectric film 50 is etched. In other words, by matching the part where the electrode film slit 60b is formed to the crystal structure of the piezoelectric film 50, it is possible to suppress the characteristics of the piezoelectric film 50 from fluctuating.

[0090] 25, in the piezoelectric element 1 of this embodiment, the capacitances between the electrode films 61 to 63 are connected. In this embodiment, as described above, the electrode film 60 is divided into six by the electrode film slits 60b separate from the slits 40. Therefore, the piezoelectric element 1 of this embodiment has six divided regions 226, and outputs a pressure detection signal based on the capacitance of each region 226.

[0091] In addition, the electrode film 60 of this embodiment is separated by the electrode film slits 60b as described above, and is not separated by the slits 40. Therefore, as shown in FIG. 26, the electrode film 60 is connected at the portion where the slits 40 are formed. Such a piezoelectric element 1 is manufactured, for example, by forming the slits 40 or the electrode film slits 60b each time each film is formed when performing the steps of FIG. 4A and FIG. 4B. For example, after forming the base film 70, a metal film is formed on the base film 70. Then, when the metal film is patterned to form the lower electrode film 61, the electrode film slits 60b are formed. Thereafter, the lower layer piezoelectric film 51 is formed on the lower layer electrode film 61, and before forming the intermediate electrode film 62, the slits 40 that penetrate only the lower layer piezoelectric film 51 are formed in the lower layer piezoelectric film 51. Thereafter, the intermediate electrode film 62, the upper layer piezoelectric film 52, and the upper layer electrode film 63 are also formed in the same manner, thereby manufacturing the piezoelectric element 1 of this embodiment.

[0092] In addition, in the electrode film 60 of this embodiment, the outer edge portion opposite the center portion C is actually formed to the outside of the first region R1, and the inner edge portion is formed to the inside of the second region R2. Therefore, when forming a metal film and then patterning the metal film into a desired shape to form the intermediate electrode film 62 and the upper electrode film 63, even if the piezoelectric film 50 is removed in the portion other than the electrode film slit 60b, the piezoelectric film 50 outside the first region R1 is removed. Therefore, by forming the virtual shape KS into a hexagonal shape, it is possible to suppress a decrease in detection accuracy.

[0093] Moreover, the virtual shapes KS of the vibrating region 22 and the electrode film 60 are arranged so as to be point-symmetrical with respect to the center C. In this embodiment, in the normal direction, the virtual shape KS of the electrode film 60 is hexagonal, and the outer shape of the vibrating region 22 is regular octagonal. The vibrating region 22 and the electrode film 60 are arranged so that two opposing vertices in the virtual shape KS of the electrode film 60 coincide with two opposing vertices in the outer shape of the vibrating region 22. In other words, the two opposing vertices in the virtual shape KS of the electrode film 60 are arranged on a virtual line K3 connecting the two opposing vertices in the vibrating region 22.

[0094] Furthermore, the piezoelectric element 1 (i.e., the vibration part 20) of this embodiment is formed in a planar rectangular shape as described above. The imaginary shape KS of the vibration region 22 and the electrode film 60 is formed so that each corner is located at a position different from the imaginary line K4 connecting the opposing corners in the outer shape of the piezoelectric element 1.

[0095] According to the present embodiment described above, the vibration region 22 is supported at both ends. This makes it possible to increase the resonance frequency f of the piezoelectric element 1, thereby achieving the same effects as those of the first embodiment.

[0096] (1) In this embodiment, in the normal direction, the vibration region 22 and the electrode film 60 are arranged so as to be point symmetrical with respect to the center C. Therefore, when sound pressure is applied to the vibration region 22, it is easy to extract electric charge uniformly from the electrode film 60. Therefore, it is possible to suppress a decrease in detection sensitivity and a decrease in detection accuracy.

[0097] (2) In this embodiment, the virtual shape KS of the vibration region 22 and the electrode film 60 is formed so that each corner is located at a part different from the virtual line K4 connecting the opposing corners in the outer shape of the piezoelectric element 1. Therefore, it is possible to suppress a decrease in detection accuracy. That is, in the piezoelectric element 1, the part on the virtual line K4 connecting the opposing corners is easily distorted by thermal stress or the like. In this case, if the corner of the vibration region 22 or the corner of the virtual shape KS of the electrode film 60 is located on the virtual line K4, a large thermal stress is easily applied to the corner that is easily deformed, and noise is likely to increase. Therefore, as in this embodiment, by making the corners of the vibration region 22 and the electrode film 60 to be located at a part different from the virtual line K4, it is possible to suppress a decrease in detection accuracy.

[0098] (3) In this embodiment, the imaginary shape KS of the electrode film 60 is a hexagon. This makes it possible to prevent the crystallinity of the piezoelectric film 50 from being destroyed when the electrode film 60 is patterned. This makes it possible to prevent the characteristics of the piezoelectric element 1 from fluctuating.

[0099] (4) In this embodiment, the outer shape of the vibration region 22 is a regular octagon. This can prevent distortion from concentrating in a local area of ​​the vibration region 22.

[0100] (Modification of the sixth embodiment) A modified example of the sixth embodiment will be described. In the sixth embodiment, if the vibration region 22 and the electrode film 60 are arranged so as to be point symmetric with respect to the center C, it is possible to easily extract electric charges uniformly from the electrode film 60, as in the sixth embodiment. For this reason, for example, as shown in FIG. 27, the vibration region 22 and the electrode film 60 may be arranged so that a pair of vertices in the virtual shape KS of the electrode film 60 are located on a virtual line K3 connecting the centers of a pair of opposing sides of the vibration region 22 and the center C. Even in such a configuration, it is preferable that the vibration region 22 and the electrode film 60 are formed so that each corner is located at a part different from the virtual line K4. Also, in FIG. 27, the slits 40 are omitted, as in FIG. 24A.

[0101] Furthermore, in the sixth embodiment, similarly to the modified example of the first embodiment, the electrode film 60 may be divided into a plurality of charge regions 60a in the first region R1 as shown in Fig. 28. Then, each divided charge region 60a may be connected in series as shown in Fig. 29. When the electrode film 60 is configured in this way, the electrode film 60 may be formed by slits 40 formed in the piezoelectric film 50.

[0102] Seventh embodiment A seventh embodiment will be described. In this embodiment, the through hole 101b of the piezoelectric device S10 is formed at a specific location in comparison with the first embodiment. As the rest is the same as the first embodiment, a description thereof will be omitted here.

[0103] 30 and 31, in the piezoelectric device S10 of this embodiment, the first to fourth slits 41 to 44 are formed in a portion different from a portion facing the through hole 101b formed in the printed circuit board 101. In other words, the through hole 101b is formed in a portion different from a portion facing the first to fourth slits 41 to 44 in the printed circuit board 101. In FIG. 30, the portion facing the through hole 101b is indicated by a dashed line.

[0104] According to the present embodiment described above, the vibration region 22 is supported at both ends. This makes it possible to increase the resonance frequency f of the piezoelectric element 1, thereby achieving the same effects as those of the first embodiment.

[0105] (1) In this embodiment, the first to fourth slits 41-44 are formed in a portion different from the portion facing the through hole 101b formed in the printed circuit board 101. This makes it possible to prevent sound pressure from flowing directly into the back space S2 through the first to fourth slits 41-44. This makes it possible to reduce noise caused by Brownian motion in the first to fourth slits 41-44. In addition, it is possible to prevent foreign matter such as dust from accumulating in the first to fourth slits 41-44.

[0106] Eighth embodiment An eighth embodiment will be described. In this embodiment, the slit length L and the like are specified in comparison with the first embodiment. As the rest is the same as the first embodiment, the description will be omitted here.

[0107] The piezoelectric device S10 of this embodiment is basically the same as that of the first embodiment, and is configured as shown in Fig. 32. The piezoelectric element 1 in Fig. 32 corresponds to the piezoelectric element 1 in Fig. 1C. Fig. 32 also shows a schematic diagram of acoustic resistance Rg, which will be described later. In this case, the sensitivity of the piezoelectric device S10 is expressed as 1 / {(1 / Cm)+(1 / Cb)}, where Cm is the acoustic compliance of the piezoelectric element 1 and Cb is the acoustic compliance of the back space S2. The acoustic compliance Cb is expressed by the following formula 2.

[0108]

number

[0109] In the first embodiment, the frequency range over which sensitivity can be maintained is broadened by increasing the resonant frequency of the piezoelectric element 1. In this case, the frequency range over which sensitivity can be maintained can also be broadened by decreasing the low-frequency roll-off frequency. For this reason, in this embodiment, the low-frequency roll-off frequency is decreased.

[0110] First, the low-frequency roll-off frequency fr is expressed by the following formula 3, where Rg is the acoustic resistance (that is, the air resistance) due to the slits 40 (that is, the first to fourth slits 41 to 44).

[0111]

number

[0112]

number

[0113] In order to set the low-frequency roll-off frequency fr to 20 Hz or less, which is outside the audible range, the following formula 5 should be satisfied.

[0114]

number

[0115]

number

[0116]

number

[0117] Here, for example, when the thickness h of the vibration region 22 is 1 μm, it is confirmed that the acoustic resistance Rg decreases as the slit width g increases and also decreases as the slit length L increases, as shown in Fig. 33. Also, when the slit width g is 1 μm, it is confirmed that the acoustic resistance Rg decreases as the thickness h of the vibration region 22 increases and also decreases as the slit length L increases, as shown in Fig. 34. And, as shown in Fig. 35, for example, when the slit length L at which the acoustic resistance is about 100 Hz is set as a reference, it is confirmed that if the slit length L is about 150 μm, the acoustic resistance can be 20 Hz or less.

[0118] In FIG. 35, the slit length L is set to 700 μm as a reference, so the acoustic resistance ratio when the slit length L is 700 μm is 1. Also, FIG. 35 shows the volume of the back space S2 that affects the acoustic compliance Cb of the back space S2 as 4×10 -9 m 3 It states that:

[0119] According to the present embodiment described above, the vibration region 22 is supported at both ends. This makes it possible to increase the resonance frequency f of the piezoelectric element 1, thereby achieving the same effects as those of the first embodiment.

[0120] (1) In this embodiment, the slit length L, the slit width g, the thickness h of the vibration region 22, and the acoustic compliance Cb of the back space S2 are formed to satisfy the above formula 7. Therefore, the low-frequency roll-off frequency fr can be set to 20 Hz or less, and the range in which the sensitivity can be maintained can be widened.

[0121] Ninth embodiment A ninth embodiment will be described. This embodiment is different from the eighth embodiment in that the shape of the slit 40 is changed. As the rest is the same as the eighth embodiment, a description thereof will be omitted here.

[0122] In the above eighth embodiment, a configuration has been described in which the slit width g is constant along the thickness direction of the vibrating region 22. However, the slit 40 may be configured so that the slit width g varies along the thickness direction of the vibrating region 22, and may be configured so that the slit width g varies in three stages, for example, as shown in Fig. 36. Specifically, in this embodiment, the slit 40 (i.e., the first to fourth slits 41 to 44) are formed so that the slit width g becomes wider in the order of g1, g2, and g3 from the other surface 22b side toward the one surface 22a side of the vibrating region 22.

[0123] In this case, the slit length L is expressed by the following formula 8. In the following formula 8, the thickness of the portion of the vibration region 22 where the slit width is g1 is the thickness h1 of the vibration region 22, the thickness of the portion of the vibration region 22 where the slit width is g2 is the thickness h2 of the vibration region 22, and the thickness of the portion of the vibration region 22 where the slit width is g3 is the thickness h3 of the vibration region 22.

[0124]

number

[0125] According to the present embodiment described above, the vibration region 22 is supported at both ends. This makes it possible to increase the resonance frequency f of the piezoelectric element 1, thereby achieving the same effects as those of the first embodiment.

[0126] (1) As in this embodiment, the slit 40 does not need to have a constant slit width g along the thickness direction of the vibration region 22.

[0127] (Modification of the tenth embodiment) A modified example of the tenth embodiment will be described. In the tenth embodiment, the shape of the slit 40 (i.e., the first to fourth slits 41 to 44) can be appropriately changed. For example, as shown in FIG. 38A, the first to fourth slits 41 to 44 may be tapered such that the slit width g on the other surface 22b side is constant and the slit width g on the one surface 22a side gradually becomes wider. Also, as shown in FIG. 38B, the first to fourth slits 41 to 44 may be configured such that the slit width g is narrowest at the center in the thickness direction of the vibrating region 22. And, as shown in FIG. 38C, the first to fourth slits 41 to 44 may be formed such that narrow and wide portions of the slit width g of the vibrating region 22 are alternately formed in the thickness direction of the vibrating region 22.

[0128] Tenth embodiment A tenth embodiment will be described. In this embodiment, the shape of the joining member 2 is specified in comparison with the first embodiment. As the rest is similar to the first embodiment, the description will be omitted here.

[0129] In the piezoelectric device S10 of this embodiment, as shown in FIG. 39, the bonding member 2 has a rectangular shape with corners in the normal direction. The bonding member 2 is bonded to the other surface 11b of the support substrate 11 of the piezoelectric element 1 at a portion different from the corner of the piezoelectric element 1. In this embodiment, the bonding member 2 is arranged such that the corners of the bonding member 2 protrude from the opposing sides of the piezoelectric element 1 in the normal direction. The bonding member 2 is arranged such that the corners of the bonding member 2 are located at a portion different from the virtual line K4 connecting the opposing corners in the outer shape of the piezoelectric element 1. The bonding member 2 of this embodiment is formed using a bonding sheet whose outer shape is specified in advance.

[0130] In addition, in the present embodiment, the electrode film 60 and the vibration region 22 are hexagonal and regular octagonal, respectively, as in the sixth embodiment. The electrode film 60 and the vibration region 22 are arranged to be point symmetrical with respect to the center C. In addition, the slits 40 are omitted in FIG. 39.

[0131] According to the present embodiment described above, the vibration region 22 is supported at both ends. This makes it possible to increase the resonance frequency f of the piezoelectric element 1, thereby achieving the same effects as those of the first embodiment.

[0132] (1) In this embodiment, the bonding member 2 is disposed in a portion different from the corners of the outer shape of the piezoelectric element 1. This makes it possible to suppress the propagation of thermal stress from the printed circuit board 101 to the corners of the piezoelectric element 1 where deformation is likely to be large. As a result, the piezoelectric element 1 is less likely to deform due to the propagated thermal stress, and the vibration region 22 is less likely to deform. This makes it possible to suppress a decrease in detection sensitivity and improve detection accuracy.

[0133] (2) In this embodiment, the bonding member 2 has a rectangular shape having corners. The bonding member 2 is disposed such that the corners are located in a portion different from the virtual line K4 in the normal direction. This can prevent stress from concentrating on the corners of the bonding member 2 due to deformation of the piezoelectric element 1, and can prevent defects such as peeling of the bonding member 2 from occurring.

[0134] (Modification of the tenth embodiment) A modified example of the tenth embodiment will be described. The bonding member 2 may be an equilateral triangular shape in the normal direction as shown in Fig. 40A, or may be a regular octagonal shape in the normal direction as shown in Fig. 40B. Although not shown, the bonding member 2 may be a regular hexagon or a regular decagon in the normal direction. The bonding member 2 may be disposed so as to protrude from the piezoelectric element 1 in the normal direction, or may be disposed only inside the piezoelectric element 1.

[0135] The bonding member 2 may be disposed as shown in Fig. 41A to Fig. 41C with reference to the through hole 101b formed in the printed circuit board 101. Fig. 41A to Fig. 41C are plan views of the piezoelectric element 1 and the bonding member 2 as viewed from the other surface 11b side of the support substrate 11. In Fig. 41A to Fig. 41C, the vibrating region 22 is omitted, and the portion facing the through hole 101b is indicated by a dashed line. In Fig. 41A to Fig. 41C, the recess 10a formed in the support substrate 11 has a shape that coincides with the through hole 101b in the normal direction.

[0136] For example, as shown in FIG. 41A, the bonding member 2 may be annular in the normal direction surrounding the through hole 101b. As shown in FIG. 41B, the bonding member 2 may be cross-shaped in the normal direction, with a portion extending in one direction and a portion extending perpendicular to the one direction. As shown in FIG. 41C, the bonding member 2 may be rhombus in the normal direction. In FIG. 41B, the corners of the bonding member 2 are located on the virtual line K4. However, even with such a configuration, the bonding member 2 is bonded only to a portion other than the corners of the piezoelectric element 1, so that thermal stress is less likely to propagate to the corners of the piezoelectric element 1, and the same effect as the tenth embodiment can be obtained.

[0137] Eleventh embodiment An eleventh embodiment will be described. In this embodiment, in contrast to the first embodiment, a protrusion is formed on the printed circuit board 101. As the rest is similar to the first embodiment, a description thereof will be omitted here.

[0138] In the piezoelectric device S10 of this embodiment, as shown in Fig. 42, a protrusion 101c is formed on the printed circuit board 101. Specifically, the protrusion 101c is shaped to match the outer shape of the joining member 2 and is configured as a part of the printed circuit board 101. For example, the protrusion 101c of this embodiment is formed in a portion of the printed circuit board 101 that faces the piezoelectric element 1 and is different from the portion that faces the corner of the piezoelectric element 1.

[0139] According to the present embodiment described above, the vibration region 22 is supported at both ends. This makes it possible to increase the resonance frequency f of the piezoelectric element 1, thereby achieving the same effects as those of the first embodiment.

[0140] (1) In this embodiment, the printed circuit board 101 has a protrusion 101c. Therefore, when applying and arranging the liquid bonding member 2, the outer shape of the bonding member 2 to be bonded to the piezoelectric element 1 can be easily adjusted by applying the bonding member 2 onto the protrusion 101c. Therefore, a liquid bonding member can be used as the bonding member 2, and the selectivity of the bonding member 2 can be improved. In particular, when adjusting the shape of the bonding member 2 as in the above tenth embodiment, the outer shape of the bonding member 2 can be easily adjusted.

[0141] (Modification of the eleventh embodiment) A modification of the eleventh embodiment will be described below. In the eleventh embodiment, the protruding portion 101c may be formed of a separate member from the printed circuit board 101.

[0142] Twelfth embodiment A twelfth embodiment will be described. This embodiment is different from the first embodiment in that the shape of the slit 40 is changed. As the rest is similar to the first embodiment, a description thereof will be omitted here.

[0143] In the piezoelectric element 1 of this embodiment, the piezoelectric film 50 is made of ScAlN. As shown in FIG. 43, the first slit 41 and the fourth slit 44 are formed to have a tapered portion 45 that narrows from the one surface 22a side toward the other surface 22b side. In other words, the first slit 41 and the fourth slit 44 are formed so that the side surface 22c becomes the tapered portion 45. In addition, the first slit 41 and the fourth slit 44 of this embodiment are formed so that the width continuously narrows from the one surface 22a side toward the other surface 22b side. In other words, the first slit 41 is formed so that the side surface 22c of the vibration region 22 is substantially flat.

[0144] The first slit 41 and the fourth slit 44 are formed so that the angle θ1 between the other surface 22b and the side surface 22c of the vibrating region 22 (hereinafter simply referred to as the angle of the vibrating region 22) is 39 to 81°.

[0145] The angle θ1 can be said to be the taper angle of the slit 40. The second slit 42 and the third slit 43 have the same shape as the first slit 41 and the fourth slit 44 in a cross section different from that of FIG. 43. FIG. 43 corresponds to a cross section taken along line IC-IC in FIG. 1. The vibration region 22 has one surface 22a and another surface 22b parallel to each other. In this embodiment, the other surface 22b corresponds to a surface parallel to the one surface 22a.

[0146] Next, a method for manufacturing the piezoelectric element 1 will be described with reference to Figures 44A to 44C, 45, and 46. Figures 44A to 44C correspond to cross-sectional views taken along line IC-IC in Figure 1. Although Figures 44A to 44C show cross-sectional views of the first slit 41 and the fourth slit 44, the same is true for the second and third slits 42 and 43.

[0147] First, a process similar to that shown in FIG. 4A is carried out to prepare a substrate in which the first to fourth slits 41 to 44 are not formed.

[0148] 44A, an etching mask material 200 made of photoresist or the like is disposed so as to cover the upper electrode film 63, etc., and an opening 201 is formed in the etching mask material 200, where the first to fourth slits 41 to 44 are to be formed. The second and third slits 42 and 43 are formed in a cross section different from that in FIG. 44A. In the following, the surface of the etching mask material 200 that covers the upper electrode film 63 and the upper piezoelectric film 52 is referred to as the other surface 200b, the surface of the etching mask material 200 opposite to the other surface 200b is referred to as the first surface 200a, and the side of the opening 201 is referred to as the side surface 200c.

[0149] Next, as shown in FIG. 44B, a heat treatment is performed to adjust the shape of the opening 201 of the etching mask material 200. Specifically, the etching mask material 200 is arranged so as to cover the upper electrode film 63 and the upper piezoelectric film 52, and the part on the other surface 200b side fixed thereto and the part on the one surface 200a side thermally shrink in different ways. More specifically, when a heat treatment is performed, the part on the other surface 200b side of the etching mask material 200 is less likely to thermally shrink, and the part on the one surface 200a side is more likely to thermally shrink. For this reason, the heat treatment is performed to adjust the angle θ2 between the other surface 200b and the side surface 200c of the etching mask material 200 (hereinafter, simply referred to as the angle θ2 of the etching mask material 200) to the angle θ1 of the desired vibration region 22. In this case, since the piezoelectric film 50 and the etching mask material 200 are made of different materials, the etching rates are usually different when anisotropic dry etching, which will be described later, is performed. Therefore, based on the etching rate, etc., the angle θ2 of the etching mask material 200 is adjusted so that the angle θ1 of the vibration region 22 becomes a desired value. Note that, since the angle θ2 of the etching mask material 200 here is adjusted as described above, it may match the angle θ1 of the vibration region 22, but it may not match the angle θ1 of the vibration region 22.

[0150] 44C, anisotropic dry etching is performed using the etching mask material 200 as a mask to form first to fourth slits 41 to 44 that penetrate the piezoelectric film 50 and reach the support 10. In this embodiment, the first to fourth slits 41 to 44 are formed so as to form a vibration region constituent part 220 having a side surface 22c that becomes a tapered part 45.

[0151] At this time, as described above, the angle θ2 of the etching mask material 200 is adjusted according to the angle θ1 of the vibration region 22, and the angle θ1 of the vibration region component 220 is set to 39 to 81°. The vibration region component 220 is a portion that becomes the vibration region 22 by forming the recess 10a. Therefore, the angle θ1 of the vibration region component 220 is the same as the angle θ1 of the vibration region 22. In the drawing, the same reference numerals are given to one surface, the other surface, and the side surface of the vibration region component 220 as the one surface 22a, the other surface 22b, and the side surface 22c of the vibration region 22. The shapes of the lower electrode film 61, the intermediate electrode film 62, and the upper electrode film 63 are adjusted so as not to reach the first to fourth slits 41 to 44. Therefore, in this process, the piezoelectric film 50 and the base film 70 are anisotropically dry etched.

[0152] 4C, etching is performed from the other surface 11b of the support substrate 11 through the insulating film 12 to reach the base film 70, forming the recess 10a. This causes the vibrating region forming portion 220 to float above the support 10, forming the vibrating region 22, and thus producing the piezoelectric element 1 shown in FIG.

[0153] Next, the angle θ1 formed by the vibrating region component 220 (that is, the vibrating region 22) in the manufacturing process of this embodiment will be described.

[0154] First, according to the study by the present inventors, when the piezoelectric film 50 of ScAlN or the like is anisotropically dry etched, the following phenomenon was confirmed when the angle θ1 is 81° or more. That is, when the angle θ1 is 81° or more, it was confirmed that the machinability tends to decrease due to the effect of redeposition, in which the etched atoms are redeposited on the side surface 22c of the first to fourth slits 41 to 44. Furthermore, according to the study by the present inventors, when the piezoelectric film 50 of ScAlN or the like is anisotropically dry etched, the following phenomenon was confirmed when the angle θ1 is 63° or more. That is, when the angle θ1 is 63° or more, it was confirmed that the machinability tends to decrease due to the effect of fences formed by redepositing the etched atoms in the vicinity of the openings on the one surface 22a side of the first to fourth slits 41 to 44. For this reason, when the first to fourth slits 41 to 44 are formed, it is preferable that the angle θ1 is 63° or less. This makes it possible to suppress the machinability from being decreased due to the fences or the like.

[0155] Moreover, ScAlN constituting the piezoelectric film 50 is a material that is difficult to etch. According to the study by the present inventors, when the first to fourth slits 41 to 44 penetrating the piezoelectric film 50 are formed, in order to leave the etching mask material 200 on the piezoelectric film 50, it is preferable to set the thickness of the etching mask material 200 to 1 to 5 times the thickness of the piezoelectric film 50. In other words, when the first to fourth slits 41 to 44 penetrating the piezoelectric film 50 are formed, in order to prevent the piezoelectric film 50 covered with the etching mask material 200 from being removed by anisotropic dry etching, it is preferable to set the thickness of the etching mask material 200 to 1 to 5 times the thickness of the piezoelectric film 50. That is, as shown in FIG. 45, when the thickness of the piezoelectric film 50 is A1, the thickness A2 of the etching mask material 200 is preferably A1 to 5A1. Note that the base film 70 of this embodiment is formed extremely thin with respect to the piezoelectric film 50 as described above. For this reason, the influence of the base film 70 is ignored. In other words, the film thickness A1 of the piezoelectric film 50 corresponds to the thickness h of the vibration region 22 described above.

[0156] In addition, when the first to fourth slits 41 to 44 are formed, they are also affected by the exposure constraints of the processing equipment. According to the study by the present inventors, in a current general processing equipment, as shown in Fig. 45, when the width of the first to fourth slits 41 to 44 on the one surface 22a side is defined as the slit width g, it has been confirmed that the resolution of the slit width g relative to the film thickness A2 of the etching mask material 200 is limited to 1 / 2 to 1 / 3 of the film thickness A2 of the etching mask material 200. Therefore, since the film thickness A2 of the etching mask material 200 is represented by A1 to 5A1, the slit width g is limited to a range of A1 / 3 to 5A1 / 2.

[0157] In the piezoelectric element 1 as described above, sound pressure escapes from the first to fourth slits 41 to 44. In this case, as shown in FIG. 46, the longer the effective width of the first to fourth slits 41 to 44, the lower the sensitivity at low frequencies. For this reason, it is preferable that the first to fourth slits 41 to 44 are formed so that their effective widths are narrower. The effective width of the first to fourth slits 41 to 44 refers to the average width of the first to fourth slits 41 to 44. For example, in the case where the first to fourth slits 41 to 44 are tapered such that the slit width g is continuously narrowed from the one surface 22a toward the other surface 22b as in this embodiment, the effective width is the average of the width on the one surface 22a side and the width on the other surface 22b side.

[0158] In addition, since the first to fourth slits 41 to 44 of this embodiment are formed by anisotropic dry etching, the side surface 22c becomes substantially flat. Therefore, in order to suppress the decrease in sensitivity, the width of the first to fourth slits 41 to 44 on the other surface 22b side is assumed to be substantially 0, the film thickness of the piezoelectric film 50 is A1, and the slit width on the one surface 22a side is g, then tan θ1=A1 / (g / 2). Note that g / 2 can also be called the effective slit width. Therefore, since the slit width g is A1 / 3 to 5A1 / 2 as described above, tan θ1=6 to 0.8, and θ1=39 to 81° is preferable. In other words, when forming the first to fourth slits 41 to 44, it is preferable that the angle θ1 formed by the vibration region component 220 is 39 to 81°. This makes it possible to suppress the decrease in the workability of the first to fourth slits 41 to 44 due to the film thickness A2 of the etching mask material 200.

[0159] 47 shows the relationship between the ratio of the thickness A2 of the etching mask material 200 to the thickness A1 of the piezoelectric film 50 (hereinafter also referred to as the thickness ratio) and the formed angle. As described above, the resolution of the slit width g relative to the thickness A2 of the etching mask material 200 is limited to 1 / 2 to 1 / 3 of the thickness A2 of the etching mask material 200. For this reason, the lower limit of the formed angle θ1, 39°, occurs when the resolution is 1 / 2 times that of the etching mask material 200, and the upper limit occurs when the resolution is 1 / 3 times that of the etching mask material.

[0160] Here, the piezoelectric element 1 of the comparative example is one in which the piezoelectric film 50 is made of an easily etchable material such as AlN, and the side surface 22c of the vibration region 22 is approximately perpendicular to the other surface 22b. The effective width of the slit 40 in the piezoelectric element 1 of the comparative example is g. In this case, if the effective width in the piezoelectric element 1 of the present embodiment is g or more, the slit width g of the first to fourth slits 41 to 44 becomes too wide, and the sensitivity may be lower than that of the piezoelectric element 1 of the comparative example.

[0161] Therefore, it is preferable that the slit 40 is formed so that its effective width is equal to or smaller than the effective width of the slit 40 in the piezoelectric element 1 of the comparative example. In other words, it is preferable that the slit 40 is configured so that tan θ1 is 1 or greater. For this reason, it is preferable that θ1 is 45° or greater. This can also prevent the sensitivity from decreasing. In this case, by setting θ1 to 63° or less, it can also prevent the workability of the slit 40 from decreasing due to a fence or the like.

[0162] According to the present embodiment described above, the vibration region 22 is supported at both ends. This makes it possible to increase the resonance frequency f of the piezoelectric element 1, thereby achieving the same effects as those of the first embodiment.

[0163] (1) In this embodiment, the angle θ1 of the vibration region 22 is set to 39 to 81°. This makes it possible to suppress a decrease in the processability of the slit 40 due to the film thickness A2 of the etching mask material 200, and the slit 40 can be suitably formed. In addition, since the angle θ1 is 81° or less, it is possible to reduce the effect of redeposition and suppress a decrease in the processability.

[0164] (2) In this embodiment, the angle θ of the vibration region 22 is set to 63° or less, so that the deterioration of workability due to the influence of the fence can be suppressed.

[0165] (3) In this embodiment, the angle θ1 of the vibration region 22 is set to 45° or more, which can further prevent the detection sensitivity from decreasing.

[0166] This embodiment can also be applied to the case where the slits 40 are formed stepwise along the thickness direction of the vibration region 22, as in the above-mentioned ninth embodiment. In this case, as shown in Fig. 36, the angle θ1 is defined as the angle between the line connecting the opening end of the slit 40 on the other surface 22b side and the opening end of the slit 40 on the one surface 22a side and the other surface 22b.

[0167] Furthermore, when forming the electrode film slits 60b in the electrode film 60 as in the sixth embodiment, the slits 40 are formed each time each of the piezoelectric films 51, 52 is formed. For this reason, in this configuration, the angle θ1 is set as the angle between the portion of each of the piezoelectric films 51, 52 on the other surface 20b side and the side surface 20c.

[0168] (Modification of the twelfth embodiment) A modified example of the twelfth embodiment will be described. In the twelfth embodiment, when the first slits 41 to 44 are formed, dry etching may be performed after wet etching. According to this, since the etching mask material 200 is not removed when wet etching is performed, the film thickness A2 of the etching mask material 200, which is determined based on the film thickness A1 of the piezoelectric film 50, can be thinned, and the slit width g, which is determined by the film thickness A2 of the etching mask material 200, can be narrowed. Therefore, the effective width g / 2 can be narrowed, and the sensitivity can be improved.

[0169] (Other embodiments) Although the present disclosure has been described based on the embodiment, it is understood that the present disclosure is not limited to the embodiment or structure. The present disclosure also encompasses various modifications and modifications within the equivalent range. In addition, various combinations and forms, as well as other combinations and forms including only one element, more than one element, or less than one element, are also within the scope and concept of the present disclosure.

[0170] For example, in each of the above embodiments, the vibration section 20 may be configured to have at least one layer of piezoelectric film 50 and one layer of electrode film 60. Furthermore, the planar shape of the piezoelectric element 1 need not be rectangular, but may be polygonal, such as pentagonal or hexagonal.

[0171] In each of the above embodiments, the piezoelectric device S10 may be configured such that a through hole 102a is formed in the lid portion 102 as shown in Fig. 48. In this case, as shown in Fig. 48, the pressure-receiving surface space S1 is the space on the one surface 22a side of the vibration region 22 of the casing 100, and the back space S2 is the space on the other surface 22b side of the vibration region 22 of the casing 100.

[0172] In each of the above embodiments, the piezoelectric element 1 in which the detection accuracy is improved by supporting the vibration region 22 at both ends has been described. However, for example, in the above second embodiment, the detection accuracy can be improved by forming the slit 40 in a tapered shape. In the above sixth embodiment, the detection accuracy can be improved by the shapes of the piezoelectric film 50 and the electrode film 60. In the above seventh embodiment, the detection accuracy can be improved by the positional relationship between the slit 40 and the through hole 101b. In the above eighth embodiment, the detection accuracy of the piezoelectric element 1 can be improved by reducing the low-frequency roll-off frequency. In the tenth embodiment, the detection accuracy can be improved by the positional relationship between the piezoelectric element 1 and the bonding member 2. Therefore, in these piezoelectric elements 1 or piezoelectric devices S10, the vibration region 22 may be supported at one end. That is, for example, when the outer shape of the vibration region 22 is a rectangular shape in plan view and the first to fourth slits 41 to 44 are formed in the vibration region 22, the first to fourth slits 41 to 44 may be formed to intersect at the center C of the vibration region 22. The manufacturing method in the twelfth embodiment relates to the shape of the slits 40, and is therefore also applicable to a manufacturing method of a piezoelectric element 1 in which the vibrating region 22 is supported in a cantilevered manner.

[0173] The above-mentioned embodiments may be appropriately combined. For example, the second embodiment may be combined with the third to twelfth embodiments, and the slit 40 may be tapered so that the width narrows toward the center C. The third embodiment may be combined with the fourth to twelfth embodiments, and the charge may be taken out from the central region 225 of the vibration region 22 as well. The fourth or fifth embodiment may be combined with the sixth to twelfth embodiments, and the vibration region 22 may be supported at both ends by the connecting member 90 or the connecting member 91. The sixth embodiment may be combined with the seventh to twelfth embodiments, and the shape and arrangement of the vibration region 22 and the electrode film 60 may be defined. The seventh embodiment may be combined with the eighth to twelfth embodiments, and the slit 40 may be formed in a portion different from the portion facing the through hole 101b. The eighth embodiment may be combined with the ninth to twelfth embodiments, and the slit length L may be defined. The ninth embodiment may be combined with any of the tenth to twelfth embodiments so that the slit width g of the slit 40 varies along the thickness direction of the vibration region 22. The tenth embodiment may be combined with any of the eleventh and twelfth embodiments so that the location of the joining member 2 is specified. The eleventh embodiment may be combined with the twelfth embodiment so that the protrusion 101c is formed on the printed circuit board 101. Furthermore, combinations of the above embodiments may be further combined with each other. [Explanation of symbols]

[0174] 10 Support 20 Vibration section 21a Support area 22 Vibration area 50 Piezoelectric film 60 Electrode membrane C center

Claims

1. A piezoelectric element having a vibration part (20) that outputs a pressure detection signal according to pressure, A support (10); the vibration section is disposed on the support, and includes a piezoelectric film (50) and an electrode film (60) connected to the piezoelectric film and extracting electric charges generated by deformation of the piezoelectric film, the vibration section having a support region (21a) supported by the support, and a vibration region (22) connected to the support region and floating above the support, and outputs the pressure detection signal based on the electric charges; The vibration region has a plurality of slits (40 to 44) formed from the support region toward a center (C) of the vibration region, and is supported at both ends by the support region. A piezoelectric element, comprising an undercoat film (70) provided between the support and the piezoelectric film.

2. The piezoelectric element according to claim 1 , wherein the undercoat film is thinner than the piezoelectric film.

3. A piezoelectric device including a piezoelectric element having a vibration portion (20) that outputs a pressure detection signal according to pressure, The piezoelectric element according to claim 1 or 2, The piezoelectric element is mounted on a support member (101) and a cover portion (102) is fixed to the support member in a state in which the piezoelectric element is housed therein. A casing (100) is provided with a through hole (101b) that communicates with the outside and through which the pressure is introduced. The slit is formed in a portion of the vibration region different from a portion facing the through hole.

Citation Information

Patent Citations

  • Electroacoustic transducer

    JP1983100000U

  • Manufacturing method of shape-changeable mirror and optical disk information input / Output device

    JP2003207729A

  • Bulk elastic wave resonator, filter using the bulk elastic wave resonator, high-frequency module using the same, and oscillator using the bulk elastic wave resonator

    JP2006333276A

  • Piezoelectric element

    JP2018137297A

  • Piezoelectric element

    JP2019161030A