Heater unit and manufacturing method thereof
The heater unit with a mica heater sandwiched between metal plates, bonded via diffusion, addresses design limitations and insulation issues, enabling flexible design and uniform temperature distribution in semiconductor manufacturing.
Patent Information
- Application Number
- JP2023046005
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-22
- Publication Date
- 2024-10-04
AI Technical Summary
Conventional sheath heaters in semiconductor manufacturing apparatuses face limitations in design flexibility due to the difficulty in bending metal sheaths, while mica heaters suffer from insulation issues when brazing, leading to restricted shape, arrangement, and heater output.
A heater unit comprising a mica heater sandwiched between metal plates, bonded via diffusion at a temperature below the metal's melting point, ensuring free design and maintaining insulation properties.
The solution allows for flexible design and uniform temperature distribution without compromising insulation, reducing the risk of molten metal penetration and enhancing heater unit performance in semiconductor manufacturing.
Smart Images

Figure 2024135368000001_ABST
Abstract
Description
[Technical field]
[0001] SUMMARY OF THE DISCLOSURE The present invention relates to a heater unit and a method for manufacturing a heater unit. [Background technology]
[0002] Semiconductor devices mounted on electronic devices are manufactured by depositing a semiconductor film, an insulating film, a conductive film, etc. on a substrate and forming a pattern in a manufacturing process that includes removing a part of the deposited film. In order to stably form these patterns, it is important to quickly raise or lower the temperature of the substrate to the target temperature and to keep the temperature distribution of the substrate uniform.
[0003] An apparatus for manufacturing semiconductor devices is provided with a mounting stage on which a wafer is placed during processing. The temperature of the wafer is changed by controlling the temperature of the mounting stage. The mounting stage of the apparatus is provided with a heater for increasing the temperature of the wafer. The heater used in the semiconductor device manufacturing apparatus is preferably in close contact with the surface that contacts the wafer in order to achieve a uniform temperature distribution. For this reason, the shape, arrangement and heater output of the heater used in the semiconductor device manufacturing apparatus must be designed to match the structure, specifications, etc. of the semiconductor device manufacturing apparatus.
[0004] Conventionally, sheath heaters have been used as heaters in semiconductor device manufacturing equipment. Patent Document 1 discloses an example of a sheath heater used in a semiconductor device manufacturing equipment. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] JP 2019-142732 A Summary of the Invention [Problem to be solved by the invention]
[0006] The sheathed heater described in Patent Document 1 has a structure in which a tubular metal sheath that surrounds a heating element is bent. To avoid damaging the metal sheath, it is difficult to bend the metal sheath at a steep angle. For this reason, when using a sheathed heater in a semiconductor device manufacturing device, it is difficult to freely position the heating element, and there are strong restrictions on the design of the heater shape, position, and heater output.
[0007] On the other hand, when a mica heater having a structure in which a metal foil pattern is sandwiched between mica plates is used, since there is no metal sheath, the shape, arrangement and heater output of the heater can be designed relatively freely.
[0008] However, when attempting to bond the mica heater to the heater substrate by brazing, there is a problem in that the molten brazing metal seeps into the spaces between the mica layers in the mica heater due to capillary action, reducing the insulation properties of the heater.
[0009] In view of the above problems, an object of the present invention is to provide a heater unit and a manufacturing method thereof that allow relatively free design of the shape, arrangement, and heater output. [Means for solving the problem]
[0010] A heater unit according to one aspect of the present invention includes a mica heater having a heating element inside a mica plate, and a metal plate in which the mica heater is disposed in a space formed inside the metal plate.
[0011] The heater unit may be one in which both sides of a mica plate are in contact with metal plates.
[0012] The mica plate of the heater unit may include a first mica plate and a second mica plate, and the heating element may be sandwiched between the first mica plate and the second mica plate.
[0013] The metal plate of the heater unit includes a first metal plate and a second metal plate facing each other across the mica heater, and the first metal plate and the second metal plate may be in direct contact at least in part.
[0014] The metal plate of the heater unit includes a first metal plate and a second metal plate facing each other via a mica heater, and the first metal plate and the second metal plate may be in contact with each other via an insert material.
[0015] The mica plate of the heater unit does not need to contain the metal contained in the metal plate.
[0016] The metal plate of the heater unit may include a connection portion that passes through the first mica plate and the second mica plate.
[0017] The heating element of the heater unit may include a conductor patterned in a curved shape, and the second mica plate may have holes drilled therein exposing two different points of the conductor, and terminals connected to the two points and protruding from the positions of the holes may be disposed in a space provided in the metal plate.
[0018] The metal plate of the heater unit may be made of aluminum or an alloy containing aluminum.
[0019] A manufacturing method for a heater unit according to another aspect of the present invention includes placing a mica heater having a heating element inside a mica plate on a first metal plate, sandwiching the mica heater between a second metal plate and the first metal plate, and bonding the first metal plate and the second metal plate by diffusion bonding at a bonding temperature lower than the melting points of the first metal plate and the second metal plate.
[0020] In the method for manufacturing the heater unit, a first recess may be formed in the first metal plate, and the disposing step may include disposing the mica heater in the first recess.
[0021] In the method for manufacturing the heater unit, the depth of the first recess may be equal to or greater than the sum of the thickness of the mica plate and the thickness of the heating element.
[0022] In the method for manufacturing a heater unit, the depth of the first recess may be greater than 0 and less than the sum of the thickness of the mica plate and the thickness of the heating element.
[0023] In the method for manufacturing the heater unit, a second recess may be formed in the second metal plate, and the disposing step may include disposing the mica heater in a space formed by the first recess and the second recess.
[0024] In the method for manufacturing a heater unit, the sum of the depth of the first recess and the depth of the second recess may be equal to or greater than the sum of the thickness of the mica plate and the thickness of the heating element.
[0025] In the method for manufacturing a heater unit, the sum of the depth of the first recess and the depth of the second recess may be greater than 0 and less than the sum of the thickness of the mica plate and the thickness of the heating element.
[0026] In the method for manufacturing a heater unit, the first metal plate and the second metal plate may be made of aluminum or an alloy containing aluminum. [Brief description of the drawings]
[0027] [Figure 1] 1 is a perspective view of a heater unit produced by a manufacturing method for a heater unit according to an embodiment of the present invention; [Diagram 2] FIG. 2 is a plan view of the heater unit shown in FIG. [Diagram 3] 2 is a bottom view of the heater unit shown in FIG. 1. [Figure 4] 2 is a view taken along the line AA of the heater unit shown in FIG. 1. [Diagram 5] 2 is a partially enlarged cross-sectional view of a mica heater included in the heater unit shown in FIG. 1. [Figure 6] FIG. 2 is an explanatory diagram of a mica heater included in the heater unit shown in FIG. [Figure 7]4 is a flowchart illustrating a method for manufacturing the heater unit shown in FIG. [Figure 8] 2A to 2C are cross-sectional views for explaining a method for manufacturing the heater unit shown in FIG. [Figure 9] 13 is a flowchart illustrating another method for producing the heater unit shown in FIG. [Figure 10] 11A to 11C are diagrams showing experimental results of a manufacturing method for a heater unit according to one embodiment of the present invention. [Figure 11] 2A to 2C are diagrams illustrating an application example of the heater unit shown in FIG. 1. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0028] Hereinafter, each embodiment of the invention disclosed in this application will be described with reference to the drawings. However, the present invention can be embodied in various forms without departing from the gist of the invention, and the present invention should not be interpreted as being limited to the description of the embodiments exemplified below.
[0029] In the drawings, the width, thickness, shape, etc. of each part may be shown diagrammatically compared to the actual embodiment in order to clarify the explanation, but it is merely an example and does not limit the interpretation of the present invention. In addition, in this specification and each figure, elements having the same function as those explained in the previous figures may be given the same reference numerals and duplicate explanations may be omitted. For convenience of explanation, the words "upper" and "lower" are used in the explanation, but "upper" and "lower" respectively indicate the orientation when the heater unit is in use (when a substrate is placed).
[0030] In this specification and drawings, the same reference numeral is used to collectively represent multiple identical or similar components, and a lowercase alphabet is added to each of the multiple components to distinguish them from one another. The same reference numeral is used to distinguish multiple parts of a single component, and a hyphen and a natural number are used.
[0031] 1. Overview of the heater unit A description will now be given of a heater unit 10 according to a first embodiment. The heater unit 10 shown in Fig. 1 is a disk-shaped heater component that is installed on a stage of a semiconductor manufacturing device.
[0032] 2 and 3 are a plan view and a bottom view, respectively, of the heater unit 10. The heater unit 10 includes a heater body 11 and a pair of terminals 12. As described below, the pair of terminals 12 are disposed in holes 23 that do not penetrate the heater body 11. The heater unit 10 has a function of generating heat by passing a current through the pair of terminals 12. The surface of the heater body 11 on which an object to be heated is placed is formed flat.
[0033] FIG. 4 is a view taken along the line AA in FIG. 1. The heater body 11 is formed by joining a disk-shaped bottom plate 21 and a disk-shaped cover plate 22 by a method described later, and is formed into a single disk shape as a whole. The bottom plate 21 and the cover plate 22 are metal plates made of a material containing aluminum, for example. A mica heater 30 described later is disposed between the bottom plate 21 and the cover plate 22 of the heater body 11. The mica heater 30 is disposed in a space formed inside the metal plate. In FIG. 4, there is no gap between the mica heater 30, the bottom plate 21, and the cover plate 22. A hole 23 is formed in the bottom plate 21. A pair of terminals 12 is disposed in the hole 23. The pair of terminals 12 is provided in a direction perpendicular to the bottom plate 21 and the cover plate 22. Each terminal included in the pair of terminals 12 is for drawing out a lead wire described later, and is covered with an insulating sleeve, so that a heating element 32 described later is electrically insulated from the bottom plate 21 and the cover plate 22.
[0034] Figure 5 is an enlarged cross-sectional view of the mica heater 30 included in the heater unit 10 shown in Figure 1, cut along the same plane as Figure 4. The mica heater 30 has a structure in which a heating element 32 containing metal is sandwiched between an upper mica plate 34 and a lower mica plate 36. The upper mica plate 34 is disposed on the side closer to the cover plate 22, and the lower mica plate 36 is disposed on the side closer to the bottom plate 21.
[0035] The mica heater 30 shown in the plan view of Fig. 6(A) and the bottom view of Fig. 6(B) is formed in a disk shape with a smaller diameter than the bottom plate 21 and the cover plate 22 shown in Fig. 2 and Fig. 3. The lower mica plate 36 is provided with a terminal hole 38. The upper mica plate 34 and the lower mica plate 36 are provided with a through hole 37 for a post.
[0036] FIG. 6(C) is an enlarged view of the cross section of the mica heater 30 indicated by BB in the cross section of FIG. 5, particularly the schematic shape of the heating element 32. The heating element 32 is a conductor formed by chemically etching or laser processing a relatively thin metal foil into a pattern of a curved shape that is approximately zigzag in plan view. The material of the metal foil includes, but is not limited to, stainless steel, tungsten, nichrome, and molybdenum. In addition, other conductive materials, such as carbon, may be patterned instead of the metal foil. When a voltage is applied between the two ends 32P1 and 32P2 in the extension direction of the zigzag, a current flows through the heating element 32, and Joule heat is generated from the heating element 32. The two ends 32P1 and 32P2 of the heating element 32 are each connected to a pair of lead wires 33. The pattern of the heating element 32 is designed by computer simulation based on conditions such as the shape of the stage on which the heater unit 10 is placed, the electrical resistance value of the heating element 32, and the melting point. The pattern of the heating element 32 is formed so as to avoid the post hole 131. The pattern of the heating element 32 is formed so that the ends 32P1 and 32P2 of the heating element 32 are exposed from the terminal hole .
[0037] The mica heater 30 is formed, for example, by sandwiching the heating element 32 between an upper mica plate 34 and a lower mica plate 36, and then bonding the upper mica plate 34 and the lower mica plate 36 together by applying a binder, adhesive, or the like. A pair of lead wires 33 are attached to two ends 32P1 and 32P2 of the heating element 32 through terminal holes 38. The mica heater 30 does not have to have a structure in which the heating element 32 is sandwiched between two mica plates, i.e., the upper mica plate 34 and the lower mica plate 36. For example, the mica heater 30 may be one in which metal foil is embedded in a single mica plate. In addition, there may be a plurality of upper mica plates 34 and lower mica plates 36 that sandwich the heating element 32.
[0038] 2. Heater unit manufacturing method The heater unit 10 described above is manufactured, for example, by the following method. The manufacturing method of the heater unit 10 will be described with reference to the flowchart shown in FIG. 7 and the explanatory diagrams shown in FIGS. 8(A) to (F). As shown in FIGS. 8(D) and (E), the heater unit 10 is generally manufactured by sandwiching the mica heater 30 between a first aluminum plate 41a and a second aluminum plate 41b, and bonding the first aluminum plate 41a and the second aluminum plate 41b by diffusion bonding. The first aluminum plate 41a corresponds to the bottom plate 21 in FIG. 4, and the second aluminum plate 41b corresponds to the cover plate 22 in FIG. 4.
[0039] As shown in FIG. 8(A), a recess R1 having a depth D1 equal to the thickness T1 of the mica heater 30 is formed in the first aluminum plate 41a (S101). Here, the thickness T1 of the mica heater 30 is, for example, the sum of the thickness of the upper mica plate 34, the thickness of the heating element 32, and the thickness of the lower mica plate 36 shown in FIG. 5. The first aluminum plate 41a is cut using a milling machine, a machining center, or the like. A rotating tool is moved while being pressed against the first aluminum plate 41a to cut the portion where the mica heater 30 is to be placed, and the recess R1 is formed. A protrusion C1 is formed in the portion where the column hole 131 (FIG. 6) of the mica heater 30 is located. The protrusion C1 is formed, for example, by cutting while avoiding the protrusion C1 so as not to cut the first aluminum plate 41a when forming the recess R1.
[0040] 8(B), after forming the recess R1 or before forming the recess R1, the terminal hole H1 is formed in the first aluminum plate 41a. The terminal hole H1 is formed, for example, by pressing a rotating tool of a machining center against the first aluminum plate 41a.
[0041] The method of forming the recesses R1 with depth D1 in the first and second aluminum plates and the method of drilling holes in the first and second aluminum plates are not limited to the above. The recesses or holes may be formed by a chemical method. Note that the first aluminum plate 41a may be provided with a recess other than the recess R1 or a convex portion other than the convex portion C1, or a hole other than the terminal hole H1 may be drilled.
[0042] 8(C), the mica heater 30 is placed in the recess R1 formed in the first aluminum plate 41a (S102). The mica heater 30 is fitted into the recess R1 of the first aluminum plate 41a, and the protrusion C1 is inserted into the column hole 37 of the mica heater 30.
[0043] As shown in Fig. 8(D), the second aluminum plate 41b is placed on the first aluminum plate 41a (S103). The second aluminum plate 41b is placed on the upper side of the first aluminum plate 41a (the side on which the mica heater 30 is placed), and the mica heater 30 is sandwiched between the first aluminum plate 41a and the second aluminum plate 41b. In this way, the mica heater 30 is placed in the recess R1 shown in Figs. 8(A) and (B).
[0044] As shown in FIG. 8(E), the first aluminum plate 41a and the second aluminum plate 41b are bonded by diffusion bonding (S104). For example, when the first aluminum plate 41a and the second aluminum plate 41b are made of an Al-Mg-Si alloy aluminum material, a pressure of 1 MPa or more is applied to the bonding surface, and a temperature of less than 600°C is maintained for several hours. By keeping the temperature below the melting point of the material, the first aluminum plate 41a and the second aluminum plate 41b are diffusion bonded at the contacting portions, i.e., the outer periphery of the disk and the portion where the holes are formed, and the boundaries disappear. In addition, the alloy aluminum material of the material is softer than the mica heater 30 at the bonding temperature. The first aluminum plate 41a and the second aluminum plate 41b are deformed under the influence of temperature and pressure, so that the gap between the first aluminum plate 41a and the upper mica plate 34 and the second aluminum plate 41b and the lower mica plate 36 disappears, and they are easily bonded to each other. 8(A) and (B) is equal to the thickness T1 of the mica heater 30. Therefore, even if the first aluminum plate 41a and the second aluminum plate 41b are not significantly deformed, the first aluminum plate 41a and the upper mica plate 34, and the second aluminum plate 41b and the lower mica plate 36 can be easily attached to each other. If the depth D1 of the recess R1 shown in FIG. 8(A) and (B) is made larger than the thickness T1 of the mica heater 30, the parts of the first aluminum plate 41a and the second aluminum plate 41b that are in direct contact with each other can be more easily attached to each other. If the depth D1 of the recess R1 is made smaller than the thickness T1 of the mica heater 30, the first aluminum plate 41a and the upper mica plate 34, and the second aluminum plate 41b and the lower mica plate 36 can be easily attached to each other.
[0045] In this embodiment, the first aluminum plate 41a and the second aluminum plate 41b are directly bonded by diffusion bonding, but the first aluminum plate 41a and the second aluminum plate 41b may be in contact with each other via another material. For example, the first aluminum plate 41a and the second aluminum plate 41b may be in contact with each other via an insert material that is a metal material that does not become liquid at the bonding temperature. There are no particular limitations on the insert material as long as it has good bonding properties with the first aluminum plate 41a and the second aluminum plate 41b.
[0046] 8(F), a pair of terminals 12 are connected to the mica heater 30 (S105). Since the metal foil (ends of the heating element 32) are exposed from the holes H1 (terminal holes 38) of the mica heater 30, the pair of lead wires 33 are connected to the exposed metal foil by soldering, welding, or other methods. An insulating sleeve is placed over the connected pair of lead wires 33 to form the pair of terminals 12.
[0047] By carrying out the above steps, the crystal grains at the joint between the first aluminum plate 41a and the second aluminum plate 41b penetrate beyond the boundary before the joint. Therefore, the mica heater 30 is covered by the first aluminum plate 41a and the second aluminum plate 41b integrated by diffusion bonding. The upper mica plate 34 and the lower mica plate 36 are in close contact with the first aluminum plate 41a and the second aluminum plate 41b, respectively. Since the diffusion bonding is performed at a temperature below the melting point, the first aluminum plate 41a and the second aluminum plate 41b do not melt, and do not soak into the upper mica plate 34 or the lower mica plate 36. In this way, the heater unit 10 is completed in which the mica heater 30 is disposed in the space formed inside the integrated aluminum plates.
[0048] 3. Experiment An experiment was carried out to examine whether a good bond could be obtained by changing the depth D1 of the recess formed in the first aluminum plate 41a.
[0049] 3-1. Preparation An experiment was carried out in which a mica heater 30 was sandwiched between coupon pieces (small pieces for the experiment) of aluminum plates conforming to the Japanese Industrial Standards (JIS) A6061 standard and diffusion bonded to each other. A commercially available mica heater with a diameter of 100 mm and a thickness of 0.95 mm was prepared as the mica heater. An aluminum plate containing A6061 aluminum, with a diameter of 160 mm and a thickness of 20 mm was prepared as the aluminum plate.
[0050] 3-2.Joining conditions For several hours, a temperature lower than the melting point of aluminum (approximately 660°C) and a pressure low enough to prevent the mica heater 30 from collapsing were maintained. Three cases were compared: a case where the recess was 0.2 mm shallower than the thickness of the mica heater 30 (P1), a case where the thickness of the mica heater 30 and the depth of the recess were the same (P2), and a case where the recess was 0.2 mm deeper than the thickness of the mica heater 30 (P3).
[0051] 3-3.Results 3-3-1.Zygosity Ultrasonic testing and leak testing were performed to confirm the bonding. The ultrasonic testing results showed that the aluminum bonding was good for P2 and P3. The He leak testing results showed that no leaks occurred for P2 and P3.
[0052] Figures 10(A) to (C) are cross sections of P1 to P3, respectively. The parts enclosed in ellipses in the figures are enlarged to the right. In Figures 10(B) and (C), no lines are visible in the parts enclosed by black ellipses. For this reason, it can be seen that the aluminum plates are sufficiently bonded at P2 and P3.
[0053] 3-3-2. Heating test The bonded coupon was heated to 200°C and the temperature was measured. The results showed that the maximum difference between the highest and lowest temperatures in each of the cases P1, P2, and P3 was 2.42°C, 2.68°C, and 3.65°C, respectively, and the temperature distribution was uniform in all cases.
[0054] 3-3-3.Cross section The contact surface between the aluminum plate and the mica plate was checked. Elemental analysis showed that potassium, which is not included in A6061 standard aluminum plates, was attached to the aluminum plate at the contact surface between the aluminum plate and the mica heater. The attached potassium element is thought to come from the mica of the mica heater. For this reason, it is thought that there is sufficient adhesion. Next, regarding the bonding between the aluminum plates, it was confirmed that the bonding of the aluminum plates was good in P2 and P3.
[0055] 3-4. Summary of experimental results It was confirmed that aluminum plates can be diffusion bonded together by embedding a mica heater in aluminum A6061 material. It was confirmed that the temperature distribution on the surface of the aluminum plate is relatively small. It was confirmed that aluminum plates and mica heaters can be diffusion bonded by adjusting the bonding conditions such as structure, pressure, and temperature.
[0056] When the first aluminum plate and the second aluminum plate are joined by brazing, the molten brazing metal permeates the mica plate included in the mica heater 30, and the insulation of the mica heater 30 is reduced. If brazing is performed only at a position away from the mica heater 30 to avoid the permeation of the molten brazing metal, the first aluminum plate and the second aluminum plate may not be joined sufficiently. If the first aluminum plate and the second aluminum plate are not joined sufficiently, a partial gap is generated between the mica heater 30 and the first aluminum plate or the second aluminum plate, and the temperature distribution of the heater unit 10 is likely to be biased. When joining is performed by raising the temperature to the melting point of the aluminum plate, part of the molten aluminum plate permeates the mica plate included in the mica heater 30, and the insulation of the mica heater 30 is reduced, as in the case of using the brazing method.
[0057] In contrast, according to the heater unit 10, since no brazing metal is used to bond the aluminum plates sandwiching the mica heater 30, the molten brazing metal does not seep into the mica plate included in the mica heater 30 due to capillary action, and the insulation of the mica heater 30 does not deteriorate. Since the aluminum plate does not melt at the temperature of diffusion bonding, a part of the molten aluminum plate does not seep into the mica plate of the mica heater 30. Therefore, aluminum is not contained in the mica heater 30, and the insulation of the mica heater 30 does not deteriorate. The diffusion bonding can bond all the contact parts of the first aluminum plate and the second aluminum plate. Therefore, heat is easily transferred compared to when the first aluminum plate and the second aluminum plate are bonded by welding, and the temperature distribution of the heater unit 10 can be made uniform. In addition, since both sides of the mica heater 30 are in contact with the first aluminum plate and the second aluminum plate and gaps are unlikely to occur, the temperature distribution of the heater unit 10 can be made uniform.
[0058] In the above description, the metal plate encasing the mica heater is an aluminum plate conforming to the A6061 standard, but the material of the metal plate is not limited to this. The metal plate encasing the mica heater may be an aluminum plate conforming to a standard other than the A6061 standard, for example, an aluminum material conforming to the JIS standard 1000 series, 3000 series, 5000 series, or 6000 series. The metal plate may be made of an alloy of pure aluminum and other types of metal. Furthermore, the metal plate may contain a substance other than a metal. The metal plate may be made of any material that can be diffusion bonded at a temperature of 700°C or less, preferably 600°C or less.
[0059] The heater unit 10 is manufactured by bonding a first aluminum plate and a second aluminum plate at a temperature lower than the melting point of aluminum. Because the bonded boundary is uniform, the heater unit 10 is less likely to crack or deform due to thermal stress even in an environment where the temperature fluctuates relatively greatly, unlike when the first aluminum plate and the second aluminum plate are welded together.
[0060] The heater unit 10 includes a pair of terminals 12, but the number of terminals is not limited to this. Each area may include a different heating element 32, and each heating element 32 may be provided with a pair of terminals 12. With such a heater unit 10, it is possible to adjust the temperature for each area.
[0061] 4. Variations The heater unit 10 has a recess formed in the first aluminum plate 41a with a depth D1 equal to the thickness T1 of the mica heater 30. In contrast, the heater unit 50 shown in Fig. 9 has a recess formed in the first aluminum plate 51a with a depth D2 shallower than the thickness T1 of the mica heater 30, and a recess formed in the second aluminum plate 41b with a depth D3 (=T1-D2) shallower than T1 and which, when combined with D2, equals the depth of T1.
[0062] A recess and a hole are formed in the first aluminum plate 51a (S201). Subsequently, recesses and holes are formed in the second aluminum plate 51b (S202). The subsequent steps S203 to S205 are similar to steps S103 to S105 of the heater unit 10, and therefore will be omitted.
[0063] The mica heater 30 of the heater unit 50 manufactured by the above procedure is sandwiched between the first aluminum plate 51a in which a recess of depth D2 is formed and the second aluminum plate 51b in which a recess of depth D3 is formed. The mica heater 30 of the heater unit 50 is disposed in a recess of thickness D1 (D2+D3). Therefore, like the mica heater 30 of the heater unit 10, the first aluminum plate 51a and the second aluminum plate 51b are integrated by diffusion bonding. If the sum of the depth D2 of the recess of the first aluminum plate 51a and the depth D3 of the recess of the second aluminum plate 51b is made larger than the thickness T1 of the mica heater 30, the portions of the first aluminum plate 51a and the second aluminum plate 51b that are in direct contact with each other are more likely to adhere to each other. If the sum of the depth D2 of the recess in the first aluminum plate 51a and the depth D3 of the recess in the second aluminum plate 51b is made smaller than the thickness T1 of the mica heater 30, the first aluminum plate 51a and the upper mica plate 34, and the second aluminum plate 51b and the lower mica plate 36 will be easily adhered to each other.
[0064] Therefore, the heater unit 50 achieves all of the effects achieved by the heater unit 10. According to the heater unit 50, the depth of the recess formed in the first aluminum plate 51a can be made shallower than the depth of the recess formed in the first aluminum plate 41a of the heater unit 10. Therefore, according to the heater unit 50, compared to the heater unit 10, it is possible to reduce distortion of the first aluminum plate 51a that occurs when forming the recess.
[0065] In the above-described example, a recess is formed in at least one of the first aluminum plate and the second aluminum plate before diffusion bonding. However, it is not necessary that a recess is formed in either the first aluminum plate or the second aluminum plate before diffusion bonding. Also, the depth of the recess may be greater than 0 and less than the thickness of the mica heater 30. Mica is softer than aluminum. Therefore, even if there is no recess in the aluminum plate, the mica heater can be sandwiched between the aluminum plate, the temperature is increased, and pressure is applied, so that the mica heater deforms the aluminum plate and the mica heater can be embedded inside the aluminum plate. In this way, both sides of the mica heater are more firmly attached to the inner surface of the aluminum plate.
[0066] 5. Application Examples The heater unit 10 is disposed on a stage of a semiconductor manufacturing device and is used to increase the temperature of the stage.
[0067] 11 shows a cross section of an etching apparatus 200 in which a heater unit 10 is arranged on a stage 201. The etching apparatus 200 is an apparatus that performs dry etching on a film by bringing ion plasma into contact with a wafer placed on a stage 201 in a chamber 202.
[0068] The pressure inside the chamber 202 is reduced by an exhaust device 204 connected to the chamber 202. A reaction gas is introduced into the chamber 202 via an introduction pipe 206.
[0069] A microwave source 212 is connected to the top of the chamber 202 via a waveguide 210. Microwaves generated by the microwave source 212 are introduced into the chamber 202 through the waveguide 210 and a window 214 that separates the waveguide 210 from the chamber 202. Magnets 216, 218, and 220 are arranged around the chamber 202. A high-frequency power supply 224 is connected to the stage 201. The electromagnetic waves turn the reactive gas into plasma, and the film on the wafer placed on the stage 201 is etched by the electrons, ions, and radicals contained in the plasma.
[0070] Since the temperature distribution of the heater unit 10 is highly uniform, the etching progress does not vary depending on the location on the wafer even in the etching apparatus 200 that performs etching in a highly reactive plasma environment. Therefore, the etching apparatus 200 can etch the film on the wafer uniformly.
[0071] According to the heater unit 10, since no brazing metal is used to bond the aluminum plates sandwiching the mica heater 30, no particles resulting from molten brazing metal are generated when used in the etching device 200. Therefore, the cleanliness inside the chamber 202 can be kept higher than when a heater unit using brazing metal is used.
[0072] The heater unit 10 can be formed thinner than a typical sheathed heater. In addition, since the pattern of the metal foil of the heating element 32 can be formed by etching, the heating elements 32 can be arranged at a narrower pitch, i.e., at a higher density, than in a typical sheathed heater. Furthermore, the pattern of the metal foil of the mica heater 30 can be designed more freely than when it is formed by bending the metal sheath of the sheathed heater. Therefore, the layout of the components of the etching device 200 can be designed more flexibly by making the space inside the chamber 202 of the etching device 200 larger or forming the heater unit 10 into a shape other than a disk.
[0073] In the above description, the mica heater 30 is used as the heater, but the heater is not limited to the mica heater 30. A heater having a heating element sandwiched between laminar insulating plates other than mica may also be used.
[0074] The present invention allows various embodiments and modifications without departing from the broad spirit and scope of the present invention. The above-described embodiments are for the purpose of explaining the present invention and do not limit the scope of the present invention. That is, the scope of the present invention is indicated by the claims, not the embodiments. Various modifications made within the scope of the claims and the scope of the invention equivalent thereto are considered to be within the scope of the present invention. [Explanation of symbols]
[0075] 10, 50: Heater unit 11: Heater body 12: A pair of terminals 21: Bottom plate 22: Lid plate 23: Hole 30: Mica heater 32: Heating element 32P1, 32P2: End 33: A pair of leads 34: Upper mica plate 36: Lower mica plate 37: Pillar hole 38: Terminal hole 41a, 51a: First aluminum plate 41b, 51b: Second aluminum plate 200: Etching equipment 201: Stage 202: Chamber 204: Exhaust system 206:Introduction tube 210: Waveguide 212: Microwave source 214: Window 216, 218, 220: Magnets C1: Convex part R1: Recess H1: hole
Claims
1. a mica heater having a heating element inside a mica plate; a metal plate having a space formed therein and the mica heater disposed therein; Heater unit.
2. Both sides of the mica plate are in contact with the metal plate; The heater unit according to claim 1 .
3. The mica plate includes a first mica plate and a second mica plate, The heating element is sandwiched between the first mica plate and the second mica plate. The heater unit according to claim 1 .
4. The metal plate includes a first metal plate and a second metal plate facing the first metal plate with the mica heater interposed therebetween, The first metal plate and the second metal plate are in direct contact with each other at least in part. The heater unit according to claim 1 .
5. The metal plate includes a first metal plate and a second metal plate facing the first metal plate with the mica heater interposed therebetween, The first metal plate and the second metal plate are in contact with each other via an insert material. The heater unit according to claim 1 .
6. The mica plate does not contain the metal contained in the metal plate. The heater unit according to claim 1 .
7. The metal plate includes a connection portion penetrating the first mica plate and the second mica plate. The heater unit according to claim 3 .
8. The heating element includes a conductor patterned in a curved shape, The second mica plate is provided with holes through which two different points of the conductor are exposed, A terminal connected to the two points and protruding from the hole is disposed in a space provided in the metal plate. The heater unit according to claim 3 .
9. The metal plate is formed of aluminum or an alloy containing aluminum. The heater unit according to claim 1 .
10. disposing a mica heater having a heating element inside the mica plate on a first metal plate; sandwiching the mica heater between a second metal plate and the first metal plate, and bonding the first metal plate and the second metal plate by diffusion bonding at a bonding temperature lower than the melting points of the first metal plate and the second metal plate. A manufacturing method of a heater unit.
11. The first metal plate has a first recess formed therein, the disposing step includes disposing the mica heater in the first recess; The method for manufacturing the heater unit according to claim 10 .
12. The depth of the first recess is equal to or greater than the sum of the thickness of the mica plate and the thickness of the heating element. The method for manufacturing the heater unit according to claim 11 .
13. The depth of the first recess is greater than 0 and less than the sum of the thickness of the mica plate and the thickness of the heating element. The method for manufacturing the heater unit according to claim 11 .
14. The second metal plate has a second recess formed therein. The placing step includes placing the mica heater in a space defined by the first recess and the second recess. The method for manufacturing the heater unit according to claim 12 .
15. The sum of the depth of the first recess and the depth of the second recess is equal to or greater than the sum of the thickness of the mica plate and the thickness of the heating element. A method for manufacturing the heater unit according to claim 14.
16. The sum of the depth of the first recess and the depth of the second recess is greater than 0 and less than the sum of the thickness of the mica plate and the thickness of the heating element. A method for manufacturing the heater unit according to claim 14.
17. The first metal plate and the second metal plate are formed of aluminum or an alloy containing aluminum. The method for manufacturing the heater unit according to claim 10 .
Citation Information
Patent Citations
Electric rice cooker
JP1991066313A
mica heater
JP1994058593U
Heating element and manufacturing method of the same
JP2003217800A
Heater unit and its manufacturing method
JP2008047500A
Planar heating element and manufacturing method therefor
JP2008293870A