Resin composition and film using the resin composition
A resin composition combining polyolefin, polyester, ethylene-vinyl acetate copolymer, and styrenic block copolymer addresses the recycling challenge of multilayer plastics by reducing fish eyes and enhancing film appearance for diverse applications.
Patent Information
- Application Number
- JP2023049412
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-27
- Publication Date
- 2024-10-09
AI Technical Summary
Multilayer films and containers made of different types of plastics cannot be recycled due to poor compatibility, leading to the occurrence of fish eyes when formed into films, which affects their appearance and usability.
A resin composition is developed by blending thermoplastic resin containing polyolefin and polyester with an ethylene-vinyl acetate copolymer and a styrenic block copolymer, specifically in ratios that enhance compatibility and reduce fish eyes.
The resin composition results in films with fewer fish eyes and improved appearance, suitable for various applications including packaging containers.
Smart Images

Figure 2024138749000001
Abstract
Description
[Technical field]
[0001] The present invention relates to a resin composition containing a thermoplastic resin including a polyolefin and a polyester, an ethylene-vinyl acetate copolymer, and a styrene-based block copolymer. [Background technology]
[0002] In recent years, there has been growing interest in the problem of environmental pollution caused by plastics, and material recycling of plastic products has been promoted.
[0003] In the material recycling of plastics, when different types of plastics are mixed in the collected plastic waste, there is generally a problem that the physical properties of the recycled plastics are reduced due to their poor compatibility with each other.
[0004] Therefore, currently, collected plastic waste is sorted by material and then recycled into products.
[0005] However, in the case of multi-layer films and containers made of different types of plastics (hereinafter referred to as composite plastics), it is difficult to separate the materials, so they cannot be recycled and are currently landfilled or incinerated.
[0006] In this context, the addition of compatibilizers has been considered as a means of recycling composite plastics.
[0007] For example, Patent Document 1 shows that the physical properties of composite plastics such as polyethylene (PE) and polyethylene terephthalate (PET), or polypropylene (PP) and acrylonitrile-butadiene-styrene copolymer (ABS) can be improved by adding a compatibilizer.
[0008] However, while the present inventors were investigating the recycling of composite plastics, they found that when a resin containing polyester in polyolefin is formed into a film, a defect in appearance called fisheye occurs frequently. [Prior art documents] [Patent documents]
[0009] [Patent Document 1] JP 2001-220473 A Summary of the Invention [Problem to be solved by the invention]
[0010] The present invention aims to provide a resin composition which, when made into a film, produces a film with excellent appearance with few fisheyes, and a film using the resin composition, and further to provide a recycled film with good appearance made from waste materials containing multiple plastics. [Means for solving the problem]
[0011] Means for Solving the Problems The present inventors conducted intensive research to solve the above problems and discovered that a resin composition comprising a thermoplastic resin containing polyolefin and polyethylene terephthalate, blended with an ethylene-vinyl acetate copolymer and a styrene-based block copolymer, when made into a film, produces little fisheyes and has excellent film appearance, which led to the completion of the present invention.
[0012] That is, the respective aspects of the present invention are as follows [1] to
[13] . [1] A resin composition comprising 100 parts by mass of a thermoplastic resin (A) containing a polyolefin and a polyester, 1 part by mass or more and 15 parts by mass or less of an ethylene-vinyl acetate copolymer (B), and 1 part by mass or more and 15 parts by mass or less of a styrene-based block copolymer (C). [2] The resin composition according to the above [1], wherein the polyolefin is polyethylene or polypropylene. [3] The resin composition according to the above [1] or [2], wherein the ethylene-vinyl acetate copolymer (B) has a vinyl acetate content of 6% by mass or more and 90% by mass or less. [4] The resin composition according to any one of [1] to [3] above, wherein the styrene-based block copolymer (C) is a block copolymer containing at least one polymer block mainly composed of styrene monomer units and at least one polymer block mainly composed of conjugated diene compound monomer units, or a hydrogenated product thereof. [5] The resin composition according to any one of [1] to [4] above, wherein the styrene-based block copolymer (C) is a styrene-butadiene-styrene block copolymer (SBS), a styrene-isoprene-styrene block copolymer (SIS), or a hydrogenated product thereof. [6] The resin composition according to any one of the above [1] to [5], wherein the styrene-based block copolymer (C) is a styrene-ethylene-butylene-styrene block copolymer (SEBS). [7] The resin composition according to [5] above, wherein the styrene block ratio of the styrene-ethylene-butylene-styrene block copolymer is 10% by mass or more and 50% by mass or less. [8] The resin composition according to any one of [1] to [7] above, wherein the polyester is polyethylene terephthalate. [9] The resin composition according to any one of [1] to [8] above, wherein the resin contained in the thermoplastic resin (A) is a resin obtained by recovering plastic waste.
[10] A molded article made of the resin composition according to any one of [1] to [9] above.
[11] A film made of the resin composition described in any one of [1] to [9] above.
[12] A packaging container made of the film described in
[11] above.
[13] A method for producing a film according to the above
[11] , comprising molding the resin composition according to any one of the above [1] to [9] at 190°C or higher and 250°C or lower. Effect of the Invention
[0013] A film made of the resin composition according to one embodiment of the present invention has few fisheyes and is excellent in appearance, and is useful for molded articles requiring these physical properties. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0014] The present invention will be described in detail below based on preferred embodiments thereof.
[0015] The resin composition according to one embodiment of the present invention comprises 80 to 98 parts by mass of a thermoplastic resin (A) containing a polyolefin and a polyester, 1 to 10 parts by mass of an ethylene-vinyl acetate copolymer (B), and 1 to 10 parts by mass of a styrene-based block copolymer (C).
[0016] The thermoplastic resin (A) containing polyolefin and polyester may contain polyolefin and polyester. In other words, the thermoplastic resin (A) may contain a thermoplastic resin other than polyolefin and polyester. Examples of the resin component other than polyolefin and polyester include polyamide, ethylene-vinyl alcohol copolymer, polystyrene, etc.
[0017] Examples of polyolefins include polyethylene, polypropylene, ethylene-propylene copolymers, ethylene-acrylic acid ester copolymers, and ethylene-methacrylic acid ester copolymers. Examples of polyethylenes include high-density polyethylene, low-density polyethylene, and linear low-density polyethylene.
[0018] Examples of polyester include polyethylene terephthalate, glycol-modified polyethylene terephthalate (PETG resin), polybutylene terephthalate, and polylactic acid.
[0019] Examples of polyamides include nylon 6, nylon 6,6, nylon 11, and nylon 12.
[0020] Among these, the polyolefin resin contained in the thermoplastic resin (A) is preferably polyethylene or polypropylene because of its excellent film formability, and polyethylene, particularly low-density polyethylene and linear low-density polyethylene, is more preferable. As the polyester, polyethylene terephthalate is preferable because of its excellent film appearance. As the resin other than polyolefin and polyester, polyamide or ethylene-vinyl alcohol copolymer is preferable.
[0021] The ratio of the resins constituting the thermoplastic resin (A) is preferably 70 parts by mass or more and 99 parts by mass or less of polyolefin, and 1 part by mass or more and 30 parts by mass or less of polyester, because the strength of the film is excellent, and more preferably 80 parts by mass or more and 99 parts by mass or less of polyolefin, and 1 part by mass or more and 20 parts by mass or less of polyester. When resins other than polyolefin and polyester are contained, the ratio of the resins constituting the thermoplastic resin (A) is preferably 70 parts by mass or more and 98 parts by mass or less of polyolefin, 1 part by mass or more and 29 parts by mass or less of polyester, and 1 part by mass or more and 29 parts by mass or less of resins other than polyolefin and polyester, and more preferably 80 parts by mass or more and 98 parts by mass or less of polyolefin, 1 part by mass or more and 19 parts by mass or less of polyester, and 1 part by mass or more and 19 parts by mass or less of resins other than polyolefin and polyester. The total of polyolefin and polyester is 100 parts by mass.
[0022] The resin contained in the thermoplastic resin (A) may be an unused virgin resin or a resin obtained by recovering plastic waste. That is, the resin may be one or more types of resins that are all unused resins, at least one of the resins may be a used resin, or all of the resins may be a used resin.
[0023] The plastic waste is not particularly limited, and may be any of waste that cannot be used as a product, such as burrs or film trimming loss generated in plastic molding factories, non-standard products, and waste of used plastic products collected from the city or consumers. In an embodiment of the present invention, a recycled resin composition is produced as the resin composition by using plastic waste in the material resin composition. In addition, when using a resin obtained by collecting plastic waste, it may contain organic substances such as PVC resin, wax, adhesive, plasticizer, and antioxidant, or inorganic substances such as filler as impurities.
[0024] The ethylene-vinyl acetate copolymer (B) can be obtained by a known production method. Specifically, production methods such as high-pressure radical polymerization, solution polymerization, and emulsion polymerization can be mentioned, and such a resin can be conveniently selected from commercially available products, and ethylene-vinyl acetate copolymers are commercially available under the trade name Ultrathene from Tosoh Corporation and under the trade name Levaprene from Lanxess KK.
[0025] The vinyl acetate content of the ethylene-vinyl acetate copolymer (B) measured by JIS K6924-1 is preferably 6% by mass or more and 90% by mass or less, more preferably 15% by mass or more and 85% by mass or less. A vinyl acetate content of 6% by mass or more is excellent in compatibility with polyesters, and a vinyl acetate content of 90% by mass or less is excellent in compatibility with polyolefins, which is preferable.
[0026] The ethylene-vinyl acetate copolymer (B) may be an ethylene-vinyl acetate copolymer composition containing multiple ethylene-vinyl acetate copolymers with different vinyl acetate contents. In this case, the number of types of ethylene-vinyl acetate copolymers is preferably two or more, more preferably three or more, from the viewpoint of compatibility. The difference in the vinyl acetate content of each ethylene-vinyl acetate copolymer is preferably 40% by mass or less, and more preferably 5% by mass or more.
[0027] The styrene-based block copolymer (C) is a block copolymer containing at least one polymer block mainly composed of styrene monomer units and at least one polymer block mainly composed of conjugated diene compound monomer units, and may be a hydrogenated product of the copolymer.
[0028] Examples of the conjugated diene compound constituting the polymer block mainly composed of the conjugated diene compound monomer unit include 1,3-butadiene, isoprene, 1,3-pentadiene, 2,3-dimethyl-1,3-butadiene, 2-methyl-1,3-pentadiene, 1,3-hexadiene, phenylbutadiene, 4,5-diethyl-1,3-octadiene, and 3-butyl-1,3-octadiene. The polymer block mainly composed of the conjugated diene compound may be composed of one kind of these conjugated diene compounds alone or two or more kinds of them. In addition, the double bonds may be partially / fully saturated by subsequent hydrogenation.
[0029] Specific examples of the styrene-based block copolymer (C) include styrene-butadiene-styrene block copolymer (SBS), styrene-isoprene-styrene block copolymer (SIS), styrene-ethylene-butene-styrene block copolymer (SEBS) which is a hydrogenated product of SBS, and styrene-ethylene-propylene-styrene block copolymer (SEPS) which is a hydrogenated product of SIS, etc. Among these, styrene-ethylene-butene-styrene block copolymer (SEBS) is preferred in terms of compatibility with the thermoplastic resin (A).
[0030] The proportion of the polymer block mainly composed of styrene monomer units in the styrene-based block copolymer is preferably 10% by mass or more and 50% by mass or less, more preferably 10% by mass or more and 30% by mass or less. If it is 10% by mass or more, it is preferable because it has excellent compatibility with polyesters, and if it is 50% by mass or less, it is preferable because it has excellent compatibility with polyolefins.
[0031] The content ratio of the thermoplastic resin (A), ethylene-vinyl acetate copolymer (B), and styrene-based block copolymer (C) constituting the above-mentioned resin composition is, per 100 parts by mass of the thermoplastic resin (A), 1 part by mass to 15 parts by mass of the ethylene-vinyl acetate copolymer (B) and 1 part by mass to 15 parts by mass of the styrene-based block copolymer (C), and more preferably, per 100 parts by mass of the thermoplastic resin (A), 1 part by mass to 10 parts by mass of the ethylene-vinyl acetate copolymer (B) and 1 part by mass to 10 parts by mass of the styrene-based block copolymer (C).
[0032] When the ethylene-vinyl acetate copolymer (B) is 1 part by mass or more, the film appearance is excellent, and when it is 15 parts by mass or less, the film formability is excellent, and when the styrene block copolymer (C) is 1 part by mass or more, the fisheye suppression effect is excellent, and when it is 15 parts by mass or less, the film appearance is not deteriorated, and it is preferable.
[0033] The MFR of the resin composition of the present invention is not particularly limited, but in order to provide excellent film formability, the melt mass flow rate (MFR) measured under conditions of 190°C and a load of 2.16 kg is preferably 0.5 g / 10 min or more and 30 g / 10 min or less, more preferably 0.8 g / 10 min or more and 20 g / 10 min or less, and most preferably 1 g / 10 min or more and 10 g / 10 min or less.
[0034] The method for producing the resin composition is not particularly limited as long as each component can be dispersed, and the resin composition can be produced by a commonly used resin kneading device. For example, kneading devices such as a single screw extruder, a twin screw extruder, a multi-screw extruder, a Banbury mixer, a pressure kneader, a rotating roll, and an internal mixer can be mentioned. Among these, a twin screw extruder is preferred because of its excellent dispersibility and continuous productivity.
[0035] When kneading with a twin-screw extruder, the screw rotation speed is not particularly limited, but kneading is preferably performed at 50 rpm to 3000 rpm, more preferably 150 rpm to 1000 rpm. A screw rotation speed of 50 rpm or more is preferable because the dispersibility of each mixed component is improved and the physical properties of the resulting resin are excellent, while a screw rotation speed of 3000 rpm or less is preferable because the resin does not deteriorate due to excessive shear heat generation, and the physical properties of the resulting resin are excellent.
[0036] The kneading temperature is preferably at least the melting point of the component with the lowest melting point among the resin composition containing the thermoplastic resin (A) including polyolefin and polyester, the ethylene-vinyl acetate copolymer (B) and the styrene-based block copolymer (C), and is preferably about 300°C or less.
[0037] The resin composition may further contain, within the scope of the effects of the present invention, an antistatic agent, a light stabilizer, an ultraviolet absorber, a nucleating agent, an antioxidant, an antiblocking agent, a flow improver, a release agent, a flame retardant, a colorant, an inorganic neutralizing agent, a hydrochloric acid absorber, a filler conductive agent, a chain extender, a hydrolysis inhibitor, or the like.
[0038] The resin composition may be used in any form, such as pellets or powder.
[0039] The molded article according to one embodiment of the present invention is made of the above-mentioned resin composition.
[0040] The method for molding the resin composition is not particularly limited, but examples include profile extrusion, film, sheet, blow, injection, foaming, extrusion coating, rotational molding, etc., of which film is preferred because of the excellent moldability of the resin composition of the present invention.
[0041] The film forming method is not particularly limited, and examples thereof include inflation molding, coextrusion inflation molding, T-die molding, coextrusion T-die molding, calendar molding, and compression molding. Among these, inflation molding, coextrusion inflation molding, T-die molding, and coextrusion T-die molding are preferred because of their excellent productivity. The film of the present invention may be laminated with other films, and the lamination method is also not particularly limited, and examples thereof include dry lamination, extrusion lamination, and sandwich lamination.
[0042] According to the resin composition of the present embodiment described above, the occurrence of fish eyes can be suppressed when the resin composition is formed into a film. Note that fish eyes are particulate aggregates resembling fish eyes that are caused by foreign matter (unmelted matter, etc.) occurring in the film.
[0043] The film according to one embodiment of the present invention can be obtained by forming the resin composition into a film (molding into a film). The film made of the resin composition may be a single layer or may be a multilayer film. The lamination structure of the multilayer film is not particularly limited, and may include, for example, not only the resin composition layer (I) of the present invention but also layers made of other components, such as a virgin resin layer (II), an adhesive layer (III) or a barrier layer (IV). Specific examples include layer (I) / layer (II), layer (II) / layer (I) / layer (II), layer (I) / layer (III) / layer (IV) / layer (III) / layer (I), layer (I) / layer (III) / layer (IV) / layer (III) / layer (II), and the like. The " / " between layers means that the layers are adjacent to each other. The thickness of the film made of the resin composition is not particularly limited, but is preferably 10 μm to 300 μm from the viewpoint of further suppressing the occurrence of fisheyes.
[0044] The film forming temperature is preferably in the range of 190° C. to 250° C., more preferably in the range of 200° C. to 250° C., and even more preferably in the range of 220° C. to 250° C. A forming temperature of 190° C. or higher reduces the occurrence of fish eyes, while a forming temperature of 250° C. or lower is preferable because of excellent film formability.
[0045] The above films are useful as packaging containers for food, daily necessities, industrial parts, medicines, office supplies, chemical supplies, etc., surface protection films, agricultural films such as silage wrap, shrink films, transport bags, etc. EXAMPLES
[0046] The present invention will be described below with reference to examples and comparative examples, but the present invention is not limited to these. (1) Melt mass flow rate (MFR) The MFR of the resin composition of the present invention, ethylene-vinyl acetate copolymer, was measured using a melt indexer (manufactured by Takara Kogyo Co., Ltd.) at 190° C. and a load of 2.16 kg. (2) Number of fish eyes 500cm of the film produced 2 The number of fish eyes per well was counted visually. (3) Total light transmittance As an index of film transparency, the total light transmittance was measured with a haze meter (manufactured by Nippon Denshoku Industries Co., Ltd., Model NDH7000). (4) Film surface smoothness The surface smoothness of the film was evaluated by visual inspection, with small surface roughness being rated as ◯ and large surface roughness being rated as ×. [Example 1] As the thermoplastic resin (A), 90 parts by mass of linear low-density polyethylene (manufactured by Tosoh, MFR 2.0 g / 10 min, product name Nipolon Z HF210K) and 10 parts by mass of polyethylene terephthalate (manufactured by Unitika, product name MA-2103) were dry-blended to 100 parts by mass of composite resin (A1). As the ethylene-vinyl acetate copolymer (B), 4 parts by mass of ethylene-vinyl acetate copolymer (B1) (manufactured by Tosoh, MFR 3.0 g / 10 min, vinyl acetate content 25% by mass, product name Ultrathene 640) were used, and as the styrene-based block copolymer (C), 1 part by mass of styrene-ethylene-butylene-styrene block copolymer (C1) (manufactured by KRATON, styrene content 13% by mass, product name G1657VS) was used. These were preliminarily blended in a tumbler mixer, and then extruded in a twin-screw extruder (manufactured by Technobel) with a screw diameter of 25 mm. Using a ULTnano25TW (trade name), the resin was melt-mixed at a resin temperature of 260°C (above the melting temperature of A1, B1, and C1) and a screw rotation speed of 300 rpm, and then cooled to room temperature to obtain resin composition pellets (molten mixture). The MFR of the resin composition was 3.0 g / 10 min.
[0047] A single layer film made of the above resin composition pellets was obtained using a microcast molding machine (manufactured by Labtech Engineering).
[0048] At this time, the molding temperature was 200° C., the take-up speed was 2 m / min, the film width was 50 mm, and the total film thickness was 50 μm.
[0049] The number of fish eyes generated in the obtained film, the total light transmittance, and the film surface smoothness were measured by the above-mentioned evaluation methods. The evaluation results are shown in Table 1. [Example 2] A single-layer film was obtained in the same manner as in Example 1, except that 1 part by mass of a styrene-ethylene-butylene-styrene block copolymer (C2) (manufactured by KRATON, styrene content 30% by mass, product name G1726MS) was used as the styrene-based block copolymer (C). The MFR of the resin composition was 3.0 g / 10 min.
[0050] The number of fish eyes generated in the obtained film, the total light transmittance, and the film surface smoothness were measured by the above-mentioned evaluation methods. The evaluation results are shown in Table 1. [Example 3] A monolayer film was obtained in the same manner as in Example 1, except that the ethylene-vinyl acetate copolymer (B) was an ethylene-vinyl acetate copolymer composition (B2) having the following composition. The MFR of the resin composition was 3.0 g / 10 min.
[0051] 50% by mass of an ethylene-vinyl acetate copolymer (Ultrathene 640, manufactured by Tosoh Corporation) with a vinyl acetate content of 25% by mass and a melt mass flow rate of 3.0 g / 10 min 25% by mass of an ethylene-vinyl acetate copolymer (manufactured by LANXESS AG, product name: Levaprene 500) with a vinyl acetate content of 50% by mass and a melt mass flow rate of 3.0 g / 10 min 25% by mass of an ethylene-vinyl acetate copolymer (manufactured by LANXESS AG, product name: REVAPREN 800) with a vinyl acetate content of 80% by mass and a melt mass flow rate of 5.0 g / 10 min The number of fish eyes generated in the obtained film, the total light transmittance, and the film surface smoothness were measured by the above-mentioned evaluation methods. The evaluation results are shown in Table 1. [Example 4] A monolayer film was obtained in the same manner as in Example 3, except that 1 part by mass of a styrene-ethylene-butylene-styrene block copolymer (C2) (manufactured by KRATON, styrene content 30% by mass, product name G1726MS) was used as the styrene-based block copolymer (C). The MFR of the resin composition was 3.0 g / 10 min.
[0052] The number of fish eyes generated in the obtained film, the total light transmittance, and the film surface smoothness were measured by the above-mentioned evaluation methods. The evaluation results are shown in Table 1. [Example 5] A monolayer film was obtained in the same manner as in Example 4, except that 3 parts by mass of the ethylene-vinyl acetate copolymer composition (B2) was used as the ethylene-vinyl acetate copolymer (B) and 2 parts by mass of the styrene-ethylene-butylene-styrene block copolymer (C2) was used as the styrene-based block copolymer (C). The MFR of the resin composition was 3.0 g / 10 min.
[0053] The number of fish eyes generated in the obtained film, the total light transmittance, and the film surface smoothness were measured by the above-mentioned evaluation methods. The evaluation results are shown in Table 1. [Comparative Example 1] A monolayer film was obtained in the same manner as in Example 1, except that 100 parts by mass of a composite resin (A1) prepared by dry blending 90 parts by mass of linear low-density polyethylene (manufactured by Tosoh, MFR 2.0 g / 10 min, product name Nipolon Z HF210K) and 10 parts by mass of polyethylene terephthalate (manufactured by Unitika, product name MA-2103) was used as the thermoplastic resin (A). The MFR of the resin composition was 3.0 g / 10 min.
[0054] The number of fish eyes generated in the obtained film, the total light transmittance, and the film surface smoothness were measured by the above-mentioned evaluation methods. The evaluation results are shown in Table 1. [Comparative Example 2] A monolayer film was obtained in the same manner as in Example 1, except that 5 parts by mass of ethylene-vinyl acetate copolymer (B1) was used as the ethylene-vinyl acetate copolymer (B) for 100 parts by mass of composite resin (A1) prepared by dry blending 90 parts by mass of linear low-density polyethylene (manufactured by Tosoh, MFR 2.0 g / 10 min, product name Nipolon Z HF210K) and 10 parts by mass of polyethylene terephthalate (manufactured by Unitika, product name MA-2103) as the thermoplastic resin (A). The MFR of the resin composition was 3.0 g / 10 min.
[0055] The number of fish eyes generated in the obtained film, the total light transmittance, and the film surface smoothness were measured by the above-mentioned evaluation methods. The evaluation results are shown in Table 1. [Comparative Example 3] A monolayer film was obtained in the same manner as in Comparative Example 1, except that 5 parts by mass of the ethylene-vinyl acetate copolymer composition (B2) was used as the ethylene-vinyl acetate copolymer (B). The MFR of the resin composition was 3.0 g / 10 min.
[0056] The number of fish eyes generated in the obtained film, the total light transmittance, and the film surface smoothness were measured by the above-mentioned evaluation methods. The evaluation results are shown in Table 1. [Comparative Example 4] A monolayer film was obtained in the same manner as in Comparative Example 1, except that 5 parts by mass of styrene-ethylene-butylene-styrene block copolymer (C1) was used as the styrene-based block copolymer (C) for 100 parts by mass of composite resin (A1) prepared by dry blending 90 parts by mass of linear low-density polyethylene (manufactured by Tosoh, MFR 2.0 g / 10 min, product name Nipolon Z HF210K) and 10 parts by mass of polyethylene terephthalate (manufactured by Unitika, product name MA-2103) as thermoplastic resin (A) containing at least polyolefin and polyester. The MFR of the resin composition was 3.0 g / 10 min.
[0057] The number of fish eyes generated in the obtained film, the total light transmittance, and the film surface smoothness were measured by the above-mentioned evaluation methods. The evaluation results are shown in Table 1. [Comparative Example 5] A single layer film was obtained in the same manner as in Comparative Example 4, except that 5 parts by mass of styrene-ethylene-butylene-styrene block copolymer (C2) was used as the styrene-based block copolymer (C). The MFR of the resin composition was 3.0 g / 10 min.
[0058] The number of fish eyes generated in the obtained film, the total light transmittance, and the film surface smoothness were measured by the above-mentioned evaluation methods. The evaluation results are shown in Table 1.
[0059] [Table 1] [Industrial Applicability]
[0060] Films made of the resin composition of the present invention are useful as packaging containers for food, daily necessities, industrial parts, medicines, office supplies, chemical products, etc., surface protection films, agricultural films such as silage wrap, shrink films, transport bags, etc.
Claims
1. The resin composition contains 1 part by mass or more and 15 parts by mass or less of an ethylene-vinyl acetate copolymer (B) and 1 part by mass or more and 15 parts by mass or less of a styrene-based block copolymer (C) relative to 100 parts by mass of a thermoplastic resin (A) containing a polyolefin and a polyester.
2. 2. The resin composition according to claim 1, wherein the polyolefin is polyethylene or polypropylene.
3. The resin composition according to claim 1, wherein the ethylene-vinyl acetate copolymer (B) has a vinyl acetate content of 6% by mass or more and 90% by mass or less.
4. The resin composition according to claim 1, wherein the styrene-based block copolymer (C) is a block copolymer containing at least one polymer block mainly composed of styrene monomer units and at least one polymer block mainly composed of conjugated diene compound monomer units, or a hydrogenated product thereof.
5. The resin composition according to claim 1, wherein the styrene-based block copolymer (C) is a styrene-butadiene-styrene block copolymer (SBS), a styrene-isoprene-styrene block copolymer (SIS), or a hydrogenated product thereof.
6. 2. The resin composition according to claim 1, wherein the styrene-based block copolymer (C) is a styrene-ethylene-butylene-styrene block copolymer (SEBS).
7. The resin composition according to claim 6, wherein the styrene block ratio of the styrene-ethylene-butylene-styrene block copolymer is 10% by mass or more and 50% by mass or less.
8. 2. The resin composition according to claim 1, wherein the polyester is polyethylene terephthalate.
9. The resin composition according to claim 1, wherein the thermoplastic resin (A) is a resin obtained by recovering plastic waste.
10. A molded article made of the resin composition according to claim 1 .
11. A film comprising the resin composition according to any one of claims 1 to 9.
12. A packaging container comprising the film according to claim 11.
13. The method for producing a film according to claim 11, wherein the resin composition according to any one of claims 1 to 9 is molded at 190°C or higher and 250°C or lower.
Citation Information
Patent Citations
Resin composition and molded article made thereof
JP2008038142A
Highly-processable polymer material
JP2008115295A
Resin composition
JP2016190967A
Resin composition and molding using the resin composition
JP2021080428A
Compatibilizing agent, modifier for plastic recycling use, recycling plastic material and molded form therefrom