Manufacturing method of electronic device

The method addresses the issue of non-uniform sacrificial layer removal by using a laminated substrate structure with a supporting covering layer, ensuring efficient etching and accurate transfer of semiconductor layers.

JP2024139286AActive Publication Date: 2024-10-09OKI ELECTRIC INDUSTRY CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
JP2023050160
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-27
Publication Date
2024-10-09
Estimated Expiration
2043-03-27

AI Technical Summary

Technical Problem

The conventional method of removing a sacrificial layer in semiconductor layer transfer processes results in non-uniform removal due to sagging of the peripheral edge towards the substrate, leading to inefficiencies in etching and prolonged processing times.

Method used

A method involving a laminated substrate structure with a first and second sacrificial layer, where the semiconductor layer is supported by a covering layer, allowing for efficient removal of the first sacrificial layer by ensuring the etching solution spreads uniformly, and subsequent steps facilitate the transfer of the semiconductor layer to another substrate.

Benefits of technology

The method prevents sagging of the semiconductor layer during sacrificial layer removal, enhances etching efficiency, and improves the process by ensuring complete removal of the sacrificial layer and accurate transfer to a different substrate.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024139286000001_ABST
    Figure 2024139286000001_ABST
Patent Text Reader

Abstract

To efficiently remove a sacrificial layer when transferring a semiconductor layer.SOLUTION: A manufacturing method for an electronic device includes the steps of forming a covering layer from a substrate to a surface of a second sacrificial layer opposite a semiconductor layer by using a laminated substrate including a substrate, a first sacrificial layer provided on the substrate, a semiconductor layer formed on the first sacrificial layer, and a second sacrificial layer formed on the semiconductor layer from a material different from that of the first sacrificial layer, and includes removing the first sacrificial layer, removing the second sacrificial layer after removing the first sacrificial layer, peeling the semiconductor layer from the substrate, and transferring the semiconductor layer to a substrate other than the substrate.SELECTED DRAWING: Figure 7
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a method for manufacturing an electronic device. [Background technology]

[0002] There is known a technique in which a semiconductor layer is formed on a substrate via a sacrificial layer, the sacrificial layer is removed by etching, the semiconductor layer is peeled off from the substrate, and the semiconductor layer is transferred to another substrate (see, for example, Patent Document 1). [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2011-103466 A (see Abstract) Summary of the Invention [Problem to be solved by the invention]

[0004] In the above-mentioned conventional technique, when the sacrificial layer is removed, the peripheral portion of the semiconductor layer is likely to droop toward the substrate, which causes problems such as insufficient penetration of the etching solution between the semiconductor layer and the substrate, resulting in uneven removal of the sacrificial layer and a long time required for removal of the sacrificial layer.

[0005] The present disclosure aims to facilitate processes involving the transfer of semiconductor layers. [Means for solving the problem]

[0006] The method for manufacturing an electronic device disclosed herein uses a laminated substrate having a substrate, a first sacrificial layer provided on the substrate, a semiconductor layer formed on the first sacrificial layer, and a second sacrificial layer formed on the semiconductor layer from a material different from that of the first sacrificial layer, and includes the steps of forming a covering layer from the substrate to a surface of the second sacrificial layer opposite the semiconductor layer, removing the first sacrificial layer, removing the second sacrificial layer after removing the first sacrificial layer, peeling the semiconductor layer from the substrate, and transferring the semiconductor layer to a substrate other than the substrate. Effect of the Invention

[0007] According to the present disclosure, since the first sacrificial layer is removed while the semiconductor layer is supported by the covering layer, sagging of the semiconductor layer is suppressed and the etching solution can be sufficiently spread between the substrate and the semiconductor layer, which allows the first sacrificial layer to be efficiently removed and facilitates the process including the transfer of the semiconductor layer. [Brief description of the drawings]

[0008] [Figure 1] 3 is a flowchart showing a method for manufacturing the electronic device according to the first embodiment. [Diagram 2] 1A is a cross-sectional view showing a substrate, and FIG. 1B is a cross-sectional view showing a step of forming a semiconductor layer on the substrate, in the method for manufacturing the electronic device according to the first embodiment. [Diagram 3] 1A and 1B are a cross-sectional view and a plan view showing an entire structure substrate in which a semiconductor layer is formed on a substrate in a manufacturing method for an electronic device according to a first embodiment. [Figure 4] 4A and 4B are a cross-sectional view and a plan view showing a step of patterning a semiconductor layer in the method for manufacturing the electronic device according to the first embodiment. [Diagram 5] 1 is a plan view showing a semiconductor layer patterned on a substrate in a manufacturing method for an electronic device according to a first embodiment. [Figure 6] 5A and 5B are a cross-sectional view and a plan view showing a step of forming a second sacrificial layer in the method for manufacturing the electronic device according to the first embodiment. [Figure 7] 5A and 5B are a cross-sectional view and a plan view showing a step of patterning a second sacrificial body in the method for manufacturing the electronic device according to the first embodiment. [Figure 8] 4A and 4B are a cross-sectional view and a plan view showing a step of forming a support layer in the method for manufacturing the electronic device according to the first embodiment. [Figure 9]4A and 4B are a cross-sectional view and a plan view showing a step of removing a first sacrificial layer in the method for manufacturing the electronic device according to the first embodiment. [Figure 10] 5A and 5B are a cross-sectional view and a plan view showing a step of removing a second sacrificial layer in the method for manufacturing the electronic device according to the first embodiment. [Figure 11] 5A and 5B are cross-sectional views showing step by step the process of peeling a semiconductor layer from a substrate in the method for producing an electronic device according to the first embodiment. [Figure 12] 5A and 5B are cross-sectional views showing stepwise processes of transferring a semiconductor layer to a transfer substrate in the method for manufacturing the electronic device according to the first embodiment. [Figure 13] 1A and 1B are cross-sectional views showing a stepwise process of separating a pickup portion from a semiconductor layer in a manufacturing method for an electronic device according to the first embodiment, and FIG. 1C is a cross-sectional view showing a step of forming wiring or the like in the semiconductor layer. [Figure 14] 10 is a flowchart showing a method for manufacturing an electronic device according to a second embodiment. [Figure 15] 13A is a cross-sectional view showing a substrate, and FIG. 13B is a cross-sectional view showing a step of forming a first sacrificial layer and a semiconductor layer on the substrate, in a manufacturing method for an electronic device according to a second embodiment. [Figure 16] 13A and 13B are a cross-sectional view and a plan view showing a step of patterning a first sacrificial layer and a semiconductor layer in a manufacturing method for an electronic device according to a second embodiment. [Figure 17] 13A and 13B are a cross-sectional view and a plan view showing a step of forming a second sacrificial layer in a manufacturing method for an electronic device according to a second embodiment. [Figure 18] 13A and 13B are a cross-sectional view and a plan view showing a step of patterning a second sacrificial body in a manufacturing method for an electronic device according to a second embodiment. [Figure 19] 13A and 13B are a cross-sectional view and a plan view showing a step of forming a support layer in a method for manufacturing an electronic device according to a second embodiment. [Figure 20]13A and 13B are a cross-sectional view and a plan view showing a step of forming a stress-applying film in a manufacturing method for an electronic device according to a second embodiment. [Figure 21] 13A and 13B are a cross-sectional view and a plan view showing a step of removing a first sacrificial layer in a manufacturing method for an electronic device according to a second embodiment. [Figure 22] 13A and 13B are a cross-sectional view and a plan view showing a step of removing a second sacrificial layer in the method for manufacturing an electronic device according to the second embodiment. [Diagram 23] 13A and 13B are a cross-sectional view and a plan view showing a step of removing a stress-applying film in the method for manufacturing an electronic device according to the second embodiment. [Figure 24] 13A and 13B are cross-sectional views showing a step of peeling a semiconductor layer from a substrate in a method for producing an electronic device according to a second embodiment. [Diagram 25] 11A and 11B are cross-sectional views showing a step of transferring a semiconductor layer to a transfer substrate in a method for manufacturing an electronic device according to a second embodiment, and FIG. 11C is a cross-sectional view showing a step of forming wiring or the like on the semiconductor layer. [Figure 26] 13 is a flowchart showing a method for manufacturing an electronic device according to a third embodiment. [Figure 27] 13A is a cross-sectional view showing a substrate, and FIG. 13B is a cross-sectional view showing a step of forming a first sacrificial layer, a semiconductor layer, and a second sacrificial layer on the substrate in a manufacturing method for an electronic device according to a third embodiment. [Figure 28] 13A and 13B are a cross-sectional view and a plan view showing a step of patterning a first sacrificial layer, a semiconductor layer, and a second sacrificial layer in a manufacturing method for an electronic device according to a third embodiment. [Figure 29] 13A and 13B are a cross-sectional view and a plan view showing a step of forming a support layer in a manufacturing method for an electronic device according to a third embodiment, and FIG. 13C is a schematic diagram showing the shape of the support layer. [Diagram 30] 13A and 13B are a cross-sectional view and a plan view showing a step of forming a stress-applying film in a manufacturing method for an electronic device according to a third embodiment. [Diagram 31]13A and 13B are a cross-sectional view and a plan view showing a step of removing a first sacrificial layer in a manufacturing method for an electronic device according to a third embodiment. [Diagram 32] 13A and 13B are a cross-sectional view and a plan view showing a step of removing a second sacrificial layer in the method for manufacturing an electronic device according to the third embodiment. [Diagram 33] 13A and 13B are a cross-sectional view and a plan view showing a step of removing a stress-applying film in a manufacturing method for an electronic device according to a third embodiment. [Diagram 34] 13A and 13B are cross-sectional views showing a step of peeling a semiconductor layer from a substrate in a method for producing an electronic device according to a third embodiment. [Diagram 35] 13A and 13B are cross-sectional views showing stepwise processes for transferring a semiconductor layer to a transfer substrate in a manufacturing method for an electronic device according to a third embodiment. [Diagram 36] 13 is a flowchart showing a method for manufacturing an electronic device according to a fourth embodiment. [Figure 37] 13A is a cross-sectional view showing a substrate, FIG. 13B is a cross-sectional view showing a step of forming a first sacrificial layer and a semiconductor layer on the substrate, and FIG. 13C is a cross-sectional view showing a step of patterning the first sacrificial layer and the semiconductor layer in a manufacturing method for an electronic device of embodiment 4. [Figure 38] 13A and 13B are a cross-sectional view and a plan view showing a step of forming a second sacrificial layer in a manufacturing method for an electronic device according to a fourth embodiment. [Figure 39] 13A and 13B are a cross-sectional view and a plan view showing a step of patterning a second sacrificial layer in a method for manufacturing an electronic device according to a fourth embodiment. [Diagram 40] 13A and 13B are a cross-sectional view and a plan view showing a step of forming a support layer in a method for manufacturing an electronic device according to a fourth embodiment. [Diagram 41] 13A and 13B are a cross-sectional view and a plan view showing a state during removal of a first sacrificial layer in a manufacturing method for an electronic device according to a fourth embodiment. [Diagram 42]13A and 13B are a cross-sectional view and a plan view showing a state in which a first sacrificial layer has been completely removed in a manufacturing method for an electronic device according to a fourth embodiment. [Diagram 43] 13A and 13B are a cross-sectional view and a plan view showing a step of removing a second sacrificial layer in a manufacturing method for an electronic device according to a fourth embodiment. [Diagram 44] 13A and 13B are cross-sectional views showing a step of peeling a semiconductor layer from a substrate in a method for producing an electronic device according to a fourth embodiment. [Diagram 45] 13A and 13B are cross-sectional views showing stepwise processes for transferring a semiconductor layer to a transfer substrate in a manufacturing method for an electronic device according to a fourth embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0009] A method for manufacturing an electronic device according to an embodiment will be described below with reference to the drawings. The electronic device has a functional layer formed of a semiconductor and exhibiting a predetermined function. The electronic device is, for example, an optical device having a photoelectric conversion element (light emitting element, light receiving element) such as an LED (light emitting diode). The optical device is used in an LED display, an image sensor, etc. The electronic device may also be a diode, a transistor, a thyristor, etc. The electronic device may also be called a semiconductor device.

[0010] First Embodiment <Manufacturing method> Fig. 1 is a flow chart showing a method for manufacturing an electronic device according to embodiment 1. Fig. 2(A) is a cross-sectional view showing a substrate 10. Fig. 2(B) is a cross-sectional view showing a step of forming a semiconductor layer 15 on the substrate 10.

[0011] The substrate 10 shown in Fig. 2(A) is a Si substrate. More specifically, the substrate 10 is a Si(111) substrate whose crystal orientation is the (111) direction. The substrate 10 is also referred to as a first substrate.

[0012] In step S101 (FIG. 1), a buffer layer 11 and a functional layer 12 are epitaxially grown on a substrate 10, as shown in FIG. 2(B).

[0013] The buffer layer 11 is, for example, an AlN layer. More specifically, the buffer layer 11 is an AlN layer in which the surface of a cubic crystal is a (0001) plane. The thickness of the buffer layer 11 is 20 nm to 2 μm, and is 0.05 μm here.

[0014] The functional layer 12 is, for example, a GaN layer. More specifically, the functional layer 12 is a GaN layer in which the surface of a cubic crystal is a (0001) plane. The thickness of the functional layer 12 is 1 to 100 μm, and here is 2 to 3 μm.

[0015] The functional layer 12 is not limited to GaN, but is preferably a GaN-based semiconductor, which is a III-V group nitride semiconductor such as GaN, AlGaN, or InGaN.

[0016] The a-axis lattice constant L of the Si(111) substrate constituting the substrate 10 10 The a-axis lattice constant L of the AlN constituting the buffer layer 11 is 3.89 Å. 11 The a-axis lattice constant L of the GaN that constitutes the functional layer 12 is 3.11 Å. 12 is 3.19 Å. These lattice constants are L 10 >L 12 >L 11 This is in a relationship.

[0017] The thermal expansion coefficient T of the Si(111) substrate constituting the substrate 10 at room temperature 10 is 2.4~4.4×10 -6 / K. The thermal expansion coefficient T 11 is 4.3~4.8×10 -6 / K. The thermal expansion coefficient T 12 is 3.72~5.45×10 -6 / K. These thermal expansion coefficients are T 12 >T 11 >T 10This is in a relationship.

[0018] The buffer layer 11 and the functional layer 12 are epitaxially grown under a tensile stress so that their lattice constants match the lattice constant of the substrate 10. That is, residual tensile stress is generated in the buffer layer 11 and the functional layer 12.

[0019] The buffer layer 11 and the functional layer 12 are collectively referred to as the semiconductor layer 15. The substrate 10 and the semiconductor layer 15 (the buffer layer 11 and the functional layer 12) are collectively referred to as the structural substrate.

[0020] 3A and 3B are a cross-sectional view and a plan view showing the entire structure substrate in which a semiconductor layer 15 is formed on a substrate 10. The above-mentioned epitaxial growth is performed at a temperature of 1000° C. or higher, but when the structure substrate is cooled to room temperature, the semiconductor layer 15 shrinks more than the substrate 10 due to the difference in thermal expansion coefficient between the semiconductor layer 15 and the substrate 10, and the structure substrate warps as shown by the arrow W in FIG. 3A.

[0021] 4(A) and 4(B) are a cross-sectional view and a plan view showing a step of patterning the semiconductor layer 15. Fig. 5 is a plan view showing a state in which the semiconductor layer 15 on the substrate 10 has been patterned.

[0022] In step S102 (FIG. 1), as shown in FIGS. 4A and 4B, the semiconductor layer 15 on the substrate 10, that is, the buffer layer 11 and the functional layer 12, are patterned. The patterning is performed by, for example, dry etching.

[0023] At this time, the upper layer of the substrate 10 is also patterned by making the etching depth deeper than the thickness of the semiconductor layer 15. The patterned upper layer of the substrate 10 becomes the first sacrificial layer 10a. The thickness t of the first sacrificial layer 10a, i.e., the amount of overetching, is 50 to 100 nm.

[0024] Although Fig. 4(A) shows a patterned portion of the semiconductor layer 15, the semiconductor layer 15 on the substrate 10 is divided into multiple parts as shown in Fig. 5. Specifically, the semiconductor layer 15 is separated into a grid shape by separation grooves G formed by the above-mentioned dry etching. The divided semiconductor layer 15 is arranged in rows and columns.

[0025] For ease of explanation, the row direction of the divided semiconductor layer 15 is defined as the X direction, and the column direction is defined as the Y direction. The planar shape of each divided semiconductor layer 15 is, for example, a rectangle having sides in the X direction and sides in the Y direction.

[0026] By dividing the semiconductor layer 15 into multiple parts in this way, the area of ​​each semiconductor layer 15 is reduced, so the residual tensile stress described above is reduced and the warping of the entire structural substrate is eliminated. However, residual tensile stress remains in each semiconductor layer 15 due to differences in thermal expansion coefficients and lattice constants.

[0027] 6(A) and 6(B) are a cross-sectional view and a plan view showing a step of forming the second sacrificial layer 13. As shown in FIG.

[0028] In step S103 (FIG. 1), a second sacrificial layer 13 is formed on the semiconductor layer 15. The second sacrificial layer 13 is formed so as to cover each side surface of the first sacrificial layer 10a and the semiconductor layer 15, as well as the surface of the semiconductor layer 15 (i.e., the surface opposite to the substrate 10). The second sacrificial layer 13 is, for example, a polyimide layer. The thickness of the second sacrificial layer 13 is, for example, 25 nm to 10 μm.

[0029] 7(A) and (B) are a cross-sectional view and a plan view showing a step of forming an opening 13a in the second sacrificial layer 13. As shown in FIG.

[0030] In step S104 (FIG. 1), as shown in FIG. 7(A), an opening 13a is formed in the second sacrificial layer 13. The opening 13a is formed so as to expose the side surface of the first sacrificial layer 10a. The opening 13a is for allowing an etching solution to reach the first sacrificial layer 10a in a process of removing the first sacrificial layer 10a (step S106) described later.

[0031] The openings 13a are formed by patterning using oxygen plasma, but may also be formed by photolithography using photosensitive polyimide. As shown in Fig. 7(B), the openings 13a are formed, for example, on each of the four sides of the semiconductor layer 15. The arrangement of the openings 13a is not limited to this example, and may be any arrangement that exposes the side surfaces of the first sacrificial layer 10a.

[0032] The substrate 10 (including the first sacrificial layer 10a), the semiconductor layer 15, and the second sacrificial layer 13 are collectively referred to as a laminated substrate.

[0033] 8(A) and 8(B) are a cross-sectional view and a plan view showing a step of forming the retention layer 14.

[0034] In step S105 (FIG. 1), as shown in FIG. 8(A), a retention layer 14 is formed as a covering layer. The retention layer 14 is, for example, a nitride film. The retention layer 14 is formed so as to extend from the surface of the substrate 10 through the side surfaces of the first sacrificial layer 10a, the semiconductor layer 15, and the second sacrificial layer 13 to the surface of the second sacrificial layer 13 (i.e., the surface opposite to the substrate 10).

[0035] 8(B), the retaining layer 14 is formed at each of the four corners of the semiconductor layer 15. The arrangement of the retaining layer 14 is not limited to the four corners, and it is sufficient if the retaining layer 14 can support the semiconductor layer 15 at a position spaced apart from the substrate 10.

[0036] 9(A) and 9(B) are a cross-sectional view and a plan view showing the step of removing the first sacrificial layer 10a.

[0037] In step S106 (FIG. 1), as shown in FIGS. 9(A) and 9(B), the first sacrificial layer 10a is removed. The first sacrificial layer 10a is removed by wet etching using potassium hydroxide (KOH). The etching direction is the (100) direction of the substrate 10, which is a Si(111) substrate, that is, the direction parallel to the surface of the substrate 10.

[0038] When the first sacrificial layer 10a is removed, the semiconductor layer 15 tries to expand in the horizontal direction due to residual tensile stress. However, the semiconductor layer 15 cannot expand because the second sacrificial layer 13 is bonded to the semiconductor layer 15. Therefore, the semiconductor layer 15 warps so that the surface on the substrate 10 side (the lower surface in the figure) expands relative to the surface on the second sacrificial layer 13 side (the upper surface in the figure). In other words, the semiconductor layer 15 warps so as to be convex toward the substrate 10 side.

[0039] Therefore, the gap (indicated by the symbol A) between the semiconductor layer 15 and the substrate 10 is wider at the peripheral portion than at the center portion. This makes it easier for the etching liquid to enter the gap between the semiconductor layer 15 and the substrate 10. In addition, since the warping of the semiconductor layer 15 progresses as the etching progresses, the etching liquid becomes more likely to reach the center of the gap between the semiconductor layer 15 and the substrate 10 as the etching progresses.

[0040] In addition, since the semiconductor layer 15 is supported by the retaining layer 14 via the second sacrificial layer 13, sagging of the peripheral portion of the semiconductor layer 15 is suppressed through the process of removing the first sacrificial layer 10a. As a result, there is no etching residue and the etching speed is increased. In other words, the first sacrificial layer 10a can be removed efficiently.

[0041] 10(A) and 10(B) are a cross-sectional view and a plan view showing the step of removing the second sacrificial layer 13.

[0042] In step S107 (FIG. 1), as shown in FIG. 10(A), the second sacrificial layer 13 is removed. The second sacrificial layer 13 is removed by patterning using, for example, oxygen plasma or the like.

[0043] By removing the second sacrificial layer 13, the semiconductor layer 15 loses the hold by the holding layer 14, so that the semiconductor layer 15 falls onto the substrate 10 and is held on the substrate 10. Furthermore, by removing the second sacrificial layer 13, the warp of the semiconductor layer 15 is eliminated and the semiconductor layer 15 returns to a horizontal state.

[0044] As shown in FIG. 10(B), since the retention layer 14 is disposed around the semiconductor layer 15, the positional deviation of the semiconductor layer 15 during the step of removing the second sacrificial layer 13 is also prevented.

[0045] 11(A) and (B) are cross-sectional views showing a stepwise process of peeling off the semiconductor layer 15.

[0046] In step S108 (FIG. 1), the semiconductor layer 15 is peeled off from the substrate 10 using the pick-up unit 17. The pick-up unit 17 has a holder 18 and a support substrate 19 that supports the holder 18.

[0047] 11(A), the holder 18 is formed of an organic structure having adhesiveness (tackiness) and elasticity, such as PDMS (polydimethylsiloxane), acrylic resin, etc. The support substrate 19 is a substrate that supports the holder 18, and is formed of, for example, Si, glass, etc.

[0048] First, the pickup unit 17 is moved toward the substrate 10 as shown in FIG. 11(A), and the holder 18 is pressed against the surface of the functional layer 12 of the semiconductor layer 15.

[0049] 11(B), the pickup unit 17 is moved in a direction away from the substrate 10. Since the semiconductor layer 15 is held in a state of being placed on the substrate 10, the semiconductor layer 15 can be easily separated from the surface of the substrate 10.

[0050] As the semiconductor layer 15 is peeled off, a part of the retaining layer 14 (for example, a part located above the semiconductor layer 15) may break, or the retaining layer 14 may be elastically deformed.

[0051] 12(A), (B) and 13(A), (B) are cross-sectional views showing a stepwise process of transferring the semiconductor layer 15. FIG. 13(C) is a cross-sectional view showing a process of forming wiring and the like on the semiconductor layer 15.

[0052] In step S109 (FIG. 1), the pickup unit 17 is used to transfer the semiconductor layer 15 to a transfer substrate 50, which is separate from the substrate 10. The transfer substrate 50 has a smooth surface in the mounting area of ​​the semiconductor layer 15, and the surface roughness of the smooth surface is, for example, 10 nm or less. The transfer substrate 50 is also referred to as a second substrate.

[0053] First, the pickup unit 17 is moved toward the transfer substrate 50 as shown in Fig. 12(A), and the semiconductor layer 15 is pressed against the surface of the transfer substrate 50 as shown in Fig. 12(B). The bottom surface of the semiconductor layer 15 and the surface of the transfer substrate 50 are both smooth surfaces, and are bonded to each other by intermolecular forces due to the application of a predetermined pressure and heat.

[0054] 13(A), the pickup unit 17 is moved in a direction away from the transfer substrate 50. Since the semiconductor layer 15 is bonded to the transfer substrate 50 by intermolecular forces, the semiconductor layer 15 remains on the transfer substrate 50, and the holder 18 of the pickup unit 17 is moved away from the semiconductor layer 15.

[0055] As a result, the base substrate 5 in which the semiconductor layer 15 is bonded onto the transfer substrate 50 is obtained, as shown in FIG. 13(B).

[0056] In step S110 (FIG. 1), as shown in FIG. 13C, wiring and the like are formed in the semiconductor layer 15 on the transfer substrate 50. The semiconductor layer 15 is patterned to form a mesa structure, and by forming wiring and the like, it becomes, for example, an LED.

[0057] Furthermore, a wiring layer 53 that connects the anode layer 12a of the semiconductor layer 15 and the wiring 51 of the transfer substrate 50 is formed, and a wiring layer 54 that connects the cathode layer 12b of the semiconductor layer 15 and the wiring 52 of the transfer substrate 50 is formed.

[0058] This completes the electronic device 1. When a voltage is applied to the semiconductor layer 15 from a drive circuit (not shown) via the wirings 51, 52 and the wiring layers 53, 54, light is emitted from the semiconductor layer 15, which is an LED.

[0059] <effect> In general, when a semiconductor layer is formed on a substrate via a sacrificial layer and the sacrificial layer is removed by etching, the peripheral portion of the semiconductor layer may sag toward the substrate during removal of the sacrificial layer, which may prevent the infiltration of the etching solution. In this case, the etching solution may not sufficiently reach between the substrate and the semiconductor layer, resulting in etching residue and time-consuming etching. In particular, the larger the substrate size, the more likely the semiconductor layer to sag.

[0060] 9(A), the first sacrificial layer 10a is removed while the semiconductor layer 15 is held at a position separated from the substrate 10 by the holding layer 14. This prevents the semiconductor layer 15 from sagging, and allows the etching solution to sufficiently penetrate into the gap between the substrate 10 and the semiconductor layer 15.

[0061] In particular, as the first sacrificial layer 10a is removed, the semiconductor layer 15 warps convexly toward the substrate 10, causing the gap between the semiconductor layer 15 and the substrate 10 to widen particularly around the periphery, making it easier for the etching solution to penetrate into the gap.

[0062] Therefore, the etching residue of the first sacrificial layer 10a can be eliminated and the etching speed can be improved, that is, the first sacrificial layer 10a can be efficiently removed.

[0063] 10(A), the warping of the semiconductor layer 15 is eliminated by removing the second sacrificial layer 13, so that the semiconductor layer 15 can be held on the substrate 10 in a state where it is returned to a horizontal state. Therefore, the semiconductor layer 15 can be easily peeled off from the substrate 10 and transferred to the transfer substrate 50.

[0064] 9(A), since the retention layer 14 extends from the substrate 10 to the surface of the second sacrificial layer 13 (i.e., the surface opposite to the substrate 10), it is possible to suppress misalignment of the semiconductor layer 15 in the step of removing the second sacrificial layer 13. Therefore, it is possible to improve the positional accuracy of the semiconductor layer 15 on the substrate 10.

[0065] <Advantages of the First Embodiment> As described above, the manufacturing method of the electronic device 1 of embodiment 1 uses a laminated substrate having a substrate 10 (including a first sacrificial layer 10a), a semiconductor layer 15 formed on the first sacrificial layer 10a, and a second sacrificial layer 13 formed on the semiconductor layer 15 from a material different from that of the first sacrificial layer 10a, and includes the steps of forming a holding layer (covering layer) 14 that holds the semiconductor layer 15 at a position spaced apart from the substrate 10, from the substrate 10 to the surface of the second sacrificial layer 13 opposite the semiconductor layer 15, removing the first sacrificial layer 10a, removing the second sacrificial layer 13 after removing the first sacrificial layer 10a, peeling the semiconductor layer 15 from the substrate 10, and transferring the semiconductor layer 15 to a transfer substrate 50.

[0066] According to this manufacturing method, the first sacrificial layer 10a is removed while the semiconductor layer 15 is held at a position separated from the substrate 10 by the holding layer 14, so that sagging of the semiconductor layer 15 can be prevented. As a result, the etching solution can be sufficiently spread in the gap between the substrate 10 and the semiconductor layer 15. This allows the first sacrificial layer 10a to be efficiently removed. Furthermore, the removal of the second sacrificial layer 13 eliminates the warping of the semiconductor layer 15, so that the semiconductor layer 15 can be easily transferred to the transfer substrate 50. That is, the process including the transfer of the semiconductor layer 15 can be facilitated.

[0067] In particular, in the process of removing the first sacrificial layer 10a, the first sacrificial layer 10a is removed while the semiconductor layer 15 is warped so as to be convex toward the substrate 10. This makes it easier for the etching solution to penetrate into the gap between the substrate 10 and the semiconductor layer 15, and enables the first sacrificial layer 10a to be removed even more efficiently.

[0068] In addition, the substrate 10 and the semiconductor layer 15 (the buffer layer 11 and the functional layer 12) are 10 is the thermal expansion coefficient T 11 ,T 12Since a combination in which the thermal expansion coefficient is smaller than the thermal expansion coefficient is used, the semiconductor layer 15 can be warped so as to be convex toward the substrate 10 side by utilizing the difference in the thermal expansion coefficients.

[0069] In addition, since a Si substrate is used as the substrate 10 and a GaN-based semiconductor layer is formed as the functional layer 12 of the semiconductor layer 15, the semiconductor layer 15 can be warped so as to be convex toward the substrate 10 by utilizing the difference in thermal expansion coefficient and the difference in lattice constant.

[0070] Furthermore, since the process includes a step of forming an opening 13a in the second sacrificial layer 13 to expose the side surface of the first sacrificial layer 10a after the step of forming the second sacrificial layer 13 and before the step of forming the retention layer 14, the etching liquid can penetrate into the first sacrificial layer 10a in the step of removing the first sacrificial layer 10a.

[0071] Furthermore, since the first sacrificial layer 10a is a part of the substrate 10, the first sacrificial layer 10a can be formed by patterning the substrate 10, and the number of film formation steps can be reduced.

[0072] In the above example, the substrate 10 is a Si substrate, the buffer layer 11 is an AlN layer, and the functional layer 12 is a GaN layer, but other combinations are possible as long as the thermal expansion coefficient of the substrate 10 is smaller than the thermal expansion coefficient of each layer that constitutes the semiconductor layer 15.

[0073] Second Embodiment <Manufacturing method> Fig. 14 is a flowchart showing a method for manufacturing an electronic device according to embodiment 2. Fig. 15(A) is a cross-sectional view showing a substrate 20. Fig. 15(B) is a cross-sectional view showing a step of forming a first sacrificial layer 21 and a semiconductor layer 22 on the substrate 20.

[0074] The substrate 20 shown in FIG. 15A is, for example, a GaAs substrate. The thermal expansion coefficient T 20 is 5.7 x 10 -6 / K. The thickness of the substrate 20 is, for example, 600 μm.

[0075] In step S201 (FIG. 14), as shown in FIG. 15(B), a first sacrificial layer 21 is formed on a substrate 20 by epitaxial growth. The first sacrificial layer 21 is, for example, an AlAs layer. The thermal expansion coefficient T 21 is 5.0×10 -6 / K. The thickness of the first sacrificial layer 21 is, for example, 0.05 μm.

[0076] In step S202 (FIG. 14), a semiconductor layer 22 is formed by epitaxial growth on the first sacrificial layer 21. The semiconductor layer 22 is, for example, an AlGaAs layer. The thermal expansion coefficient T 22 is 5.4 x 10 -6 / K. The thickness of the semiconductor layer 22 is, for example, 1.2 μm.

[0077] 16(A) and 16(B) are a cross-sectional view and a plan view showing a step of patterning the first sacrificial layer 21 and the semiconductor layer 22. As shown in FIG.

[0078] In step S203 (FIG. 14), as shown in FIGS. 16(A) and 16(B), the first sacrificial layer 21 and the semiconductor layer 22 on the substrate 20 are patterned. The patterning is performed by, for example, dry etching. The first sacrificial layer 21 and the semiconductor layer 22 are divided into a grid shape similar to the semiconductor layer 15 (FIG. 5) of the first embodiment.

[0079] 17(A) and (B) are a cross-sectional view and a plan view showing the step of forming the second sacrificial layer 23. As shown in FIG.

[0080] 17(A) and (B), in step S204 (FIG. 14), a second sacrificial layer 23 is formed so as to cover the patterned first sacrificial layer 21 and semiconductor layer 22. The second sacrificial layer 23 is formed so as to cover the side surface of the first sacrificial layer 21, the side surface of the semiconductor layer 22, and the surface of the semiconductor layer 22 (i.e., the surface opposite to the substrate 20).

[0081] The second sacrificial layer 23 is, for example, Al2 O 3 The second sacrificial layer 23 is an Al layer, which is formed by sputtering or the like. 2 O 3 Thermal expansion coefficient T 23 is 5.9 x 10 -6 / K. The thickness of the second sacrificial layer 23 is, for example, 0.05 μm.

[0082] 18(A) and (B) are a cross-sectional view and a plan view showing a step of forming an opening 23a in the second sacrificial layer 23. As shown in FIG.

[0083] In step S205 (FIG. 14), as shown in FIG. 18(A), openings 23a are formed in the second sacrificial layer 23. The openings 23a are formed by, for example, dry etching. As shown in FIG. 18(B), the openings 23a are formed, for example, on each of the four sides of the semiconductor layer 22. The arrangement of the openings 23a is not limited to this example, and it is sufficient that the side surfaces of the first sacrificial layer 21 can be exposed.

[0084] The substrate 20, the first sacrificial layer 21, the semiconductor layer 22, and the second sacrificial layer 23 are collectively referred to as a laminated substrate.

[0085] 19(A) and 19(B) are a cross-sectional view and a plan view showing a step of forming the retention layer 24.

[0086] In step S206 (FIG. 14), as shown in FIG. 19(A), a retention layer 24 is formed as a coating layer. The retention layer 24 is, for example, an organic material, more specifically, a rubber-based resist. The thickness of the retention layer 24 is, for example, 3.5 μm.

[0087] The retention layer 24 is formed so as to extend from the surface of the substrate 20, through the side surface of the second sacrificial layer 23, to the surface (i.e., the surface opposite to the substrate 20). As shown in Fig. 19(B), the retention layer 24 is formed at each of the four corners of the semiconductor layer 22. The arrangement of the retention layer 24 is not limited to the four corners, and it is sufficient if it can support the semiconductor layer 22 at a position spaced apart from the substrate 20.

[0088] 20A and 20B are a cross-sectional view and a plan view showing a process of forming the stress-applying film 25.

[0089] In step S207 (FIG. 14), as shown in FIGS. 20(A) and 20(B), a stress-applying film 25 is formed as an organic material layer on the second sacrificial layer 23. The stress-applying film 25 is attached to the surface of the second sacrificial layer 23 (i.e., the surface opposite to the substrate 10) in a heated state. The stress-applying film 25 also overlaps a part of the retention layer 24, i.e., the portion formed on the surface of the second sacrificial layer 23.

[0090] The stress-applying film 25 is, for example, a dry film resist. The thermal expansion coefficient T 25 is 70 x 10 -6 / K. This thermal expansion coefficient T 25 is the thermal expansion coefficient T of the substrate 20, the first sacrificial layer 21, the semiconductor layer 22, and the second sacrificial layer 23. 20 ,T 21 ,T 22 ,T 23 The thickness of the stress applying film 25 is, for example, 30 μm.

[0091] Since the stress-applying film 25, which has a large thermal expansion coefficient, is attached to the surface of the second sacrificial layer 23 in a heated state, when the temperature returns to room temperature, tensile stress remains in the stress-applying film 25 in a direction that causes a convex warp toward the substrate 20.

[0092] 21(A) and (B) are a cross-sectional view and a plan view showing the step of removing the first sacrificial layer 21.

[0093] In step S208 (FIG. 14), as shown in FIG. 21(A), the first sacrificial layer 21 is removed by wet etching using hydrochloric acid (Hcl) with a concentration of 4%.

[0094] When the first sacrificial layer 21 is removed, the semiconductor layer 22 and the second sacrificial layer 23 are warped so as to be convex toward the substrate 20 side due to the residual tensile stress of the stress-applying film 25. Due to this warping, the gap between the semiconductor layer 22 and the substrate 20 becomes wider at the periphery. Therefore, the etching solution can easily enter the gap between the semiconductor layer 22 and the substrate 20.

[0095] In addition, since the semiconductor layer 22 is supported by the retaining layer 24 via the second sacrificial layer 23, the peripheral portion of the semiconductor layer 22 is prevented from sagging toward the substrate 20. As a result, there is no etching residue and the etching rate is increased. In other words, the first sacrificial layer 21 can be removed efficiently.

[0096] 22(A) and (B) are a cross-sectional view and a plan view showing the step of removing the second sacrificial layer 23.

[0097] In step S209 (FIG. 14), as shown in FIGS. 22(A) and 22(B), the second sacrificial layer 23 is removed. The second sacrificial layer 23 is removed by, for example, etching using phosphoric acid. Since the stress-applying film 25 is held by the holding layer 24, a gap is formed between the stress-applying film 25 and the semiconductor layer 22, as shown by the symbol A.

[0098] Furthermore, by removing the second sacrificial layer 23, the semiconductor layer 22 loses the hold by the holding layer 24, and so falls onto the substrate 20 and is held on the substrate 20. Furthermore, by removing the second sacrificial layer 23, the warping of the semiconductor layer 22 is eliminated, and the semiconductor layer 22 returns to a horizontal state.

[0099] 23(A) and (B) are a cross-sectional view and a plan view showing a step of removing the stress-applying film 25.

[0100] In step S210 (FIG. 14), the stress-applying film 25 is removed. Since the stress-applying film 25 is formed of a dry film resist, the stress-applying film 25 can be peeled off from the retention layer 24 by pulling the stress-applying film 25 upward. This results in the semiconductor layer 22 surrounded by the retention layer 24 on the substrate 20, as shown in FIGS. 23(A) and (B).

[0101] 24(A) and (B) are cross-sectional views showing a stepwise process of peeling off the semiconductor layer 22 from the substrate 20.

[0102] In step S211 (FIG. 14), the semiconductor layer 22 is peeled off from the substrate 20 using the pickup unit 27. The pickup unit 27 has a holder 28 and a support substrate 29. The holder 28 and the support substrate 29 are configured similarly to the holder 18 and the support substrate 19 (FIG. 11(A)) of the pickup unit 17 of the first embodiment.

[0103] First, the pickup unit 27 is moved toward the substrate 20 as shown in FIG. 24(A), and the holder 28 is pressed against the surface of the semiconductor layer 22 (that is, the surface opposite to the substrate 20).

[0104] 24(B), the pickup unit 27 is moved in a direction away from the substrate 20. Since the semiconductor layer 22 is held in a state of being placed on the substrate 20, the semiconductor layer 22 can be easily separated from the surface of the substrate 20.

[0105] 25(A) and (B) are cross-sectional views showing a stepwise process of transferring the semiconductor layer 22 to a transfer substrate 60 which is different from the substrate 20. FIG. 25(C) is a cross-sectional view showing a process of forming wiring and the like on the semiconductor layer 22.

[0106] In step S212 (FIG. 14), the semiconductor layer 22 is transferred to a transfer substrate 60 separate from the substrate 20 using the pickup unit 27. The transfer substrate 60 has a structure similar to that of the transfer substrate 50 of the first embodiment (FIGS. 13(A) to (C)).

[0107] 25(A), the pickup unit 27 is moved toward the transfer substrate 60, and the semiconductor layer 22 is pressed against the surface of the transfer substrate 60. The bottom surface of the semiconductor layer 22 and the surface of the transfer substrate 60 are both smooth surfaces, and are bonded to each other by intermolecular forces due to the application of a predetermined pressure and heat.

[0108] Thereafter, the pick-up unit 27 is moved in a direction away from the transfer substrate 60. Since the semiconductor layer 22 is bonded to the transfer substrate 60 by intermolecular forces, the semiconductor layer 22 remains on the transfer substrate 60, and the holder 28 of the pick-up unit 27 moves away from the semiconductor layer 22. As a result, a base substrate 6 in which the semiconductor layer 22 is bonded onto the transfer substrate 60 is obtained, as shown in FIG. 25(B).

[0109] In step S213 (FIG. 14), as shown in FIG. 25(C), wiring and the like are formed in the semiconductor layer 22. The semiconductor layer 22 is patterned to form a mesa structure, and by forming wiring and the like, it becomes, for example, an LED.

[0110] Furthermore, a wiring layer 63 that connects the anode layer 22a of the semiconductor layer 22 and the wiring 61 of the transfer substrate 60 is formed, and a wiring layer 64 that connects the cathode layer 22b of the semiconductor layer 22 and the wiring 62 of the transfer substrate 60 is formed.

[0111] This completes the electronic device 2. When a voltage is applied to the semiconductor layer 22 from a drive circuit (not shown) via the wirings 61, 62 and the wiring layers 63, 64, the semiconductor layer 22, which is an LED, emits light.

[0112] <Advantages of the second embodiment> As described above, the method for manufacturing the electronic device 2 according to the second embodiment includes a step of forming the stress-applying film 25 as an organic material layer on the second sacrificial layer 23 after the step of forming the second sacrificial layer 23 on the semiconductor layer 22 and before the step of removing the first sacrificial layer 21. When the first sacrificial layer 21 is removed, the stress-applying film 25 acts to cause the semiconductor layer 22 to warp toward the substrate 20. Therefore, even in the semiconductor layer 22 in which warping is difficult to occur due to the difference in lattice constants (lattice mismatch), warping can be caused. This allows the etching solution to sufficiently spread in the gap between the substrate 20 and the semiconductor layer 22, and the first sacrificial layer 21 can be efficiently removed.

[0113] In particular, the thermal expansion coefficient T 25is the thermal expansion coefficient T 20 ,T 21 ,T 22 ,T 23 Since the stress-applying film 25 is larger than the stress-applying film 22, by attaching the stress-applying film 25 to the second sacrificial layer 23 in a heated state and then returning the stress-applying film 25 to room temperature, a residual tensile stress that warps the semiconductor layer 22 can be generated.

[0114] Furthermore, since the process includes a step of removing the stress-applying film 25 and at least a portion of the retention layer (covering layer) 24 prior to the step of peeling the semiconductor layer 22 from the substrate 20, warping of the semiconductor layer 22 is eliminated, and the semiconductor layer 22 can be easily peeled off from the substrate 20 and transferred to the transfer substrate 60.

[0115] In the above example, the substrate 20 is a GaA substrate, the stress-applying film 25 is a dry film resist, the first sacrificial layer 21 is an AlAs layer, the semiconductor layer 22 is an AlGaAs layer, and the second sacrificial layer 23 is an Al 2 O 3 However, other combinations are possible as long as the thermal expansion coefficient of the stress-applying film 25 is greater than the thermal expansion coefficients of the substrate 20, the sacrificial layers 21 and 23, and the semiconductor layer 22.

[0116] Third Embodiment <Manufacturing method> Fig. 26 is a flowchart showing a manufacturing method of an electronic device according to embodiment 3. Fig. 27(A) is a cross-sectional view showing a substrate 30. Fig. 27(B) is a cross-sectional view showing a step of forming a first sacrificial layer 31, a semiconductor layer 32, and a second sacrificial layer 33 on the substrate 30.

[0117] The substrate 30 shown in FIG. 27A is, for example, a GaAs substrate. The thermal expansion coefficient T 30 is 5.7 x 10 -6 / K. The thickness of the substrate 30 is, for example, 600 μm.

[0118] In step S301 (FIG. 26), as shown in FIG. 27(B), a first sacrificial layer 31 is formed on a substrate 30 by epitaxial growth. The first sacrificial layer 31 is, for example, an AlAs layer. The thermal expansion coefficient T 31 is 5.0 x 10 -6 / K. The first sacrificial layer 31 has a thickness of, for example, 0.05 μm.

[0119] In step S302 (FIG. 26), a semiconductor layer 32 is formed by epitaxial growth on the first sacrificial layer 31. The semiconductor layer 32 is, for example, an AlGaAs layer. The thermal expansion coefficient T 32 is 5.4 x 10 ―6 / K. The thickness of the semiconductor layer 32 is, for example, 1.2 μm.

[0120] In step S303 (FIG. 26), a second sacrificial layer 33 is formed on the semiconductor layer 32. The second sacrificial layer 33 is made of, for example, Si 3 N 4 The second sacrificial layer 33 is formed by, for example, plasma CVD (chemical vapor deposition). 3 N 4 Thermal expansion coefficient T 33 is 3.0 to 3.5 × 10 -6 / K. The second sacrificial layer 33 has a thickness of, for example, 0.3 μm.

[0121] 28(A) and (B) are a cross-sectional view and a plan view showing the steps of patterning the first sacrificial layer 31, the semiconductor layer 32 and the second sacrificial layer 33. As shown in FIG.

[0122] In step S304 (FIG. 26), as shown in FIGS. 28(A) and (B), the first sacrificial layer 31, the semiconductor layer 32, and the second sacrificial layer 33 on the substrate 30 are patterned. The patterning is performed by, for example, dry etching. The first sacrificial layer 31, the semiconductor layer 32, and the second sacrificial layer 33 are divided into a grid shape similar to the semiconductor layer 15 (FIG. 5) of the first embodiment.

[0123] The substrate 30, the first sacrificial layer 31, the semiconductor layer 32, and the second sacrificial layer 33 are collectively referred to as a laminated substrate.

[0124] 29(A) and (B) are a cross-sectional view and a plan view showing a step of forming the support layer 34. FIG. 29(C) is a schematic view for explaining the shape of the support layer 34.

[0125] In step S305 (FIG. 26), as shown in FIG. 29(A), a retention layer 34 is formed as a coating layer. The retention layer 34 is, for example, an organic material, more specifically, a rubber-based resist. The thickness of the retention layer 34 is, for example, 3.5 μm.

[0126] The retention layer 34 is formed to extend from the surface of the substrate 30, through the side of the first sacrificial layer 31, the side of the semiconductor layer 32, and the side of the second sacrificial layer 33, to the surface of the second sacrificial layer 33 (i.e., the side opposite the substrate 30).

[0127] 29(B), the retention layer 34 is formed at each of the four corners of the semiconductor layer 32. The arrangement of the retention layer 34 is not limited to the four corners as long as it can support the semiconductor layer 32 at a position spaced apart from the substrate 30.

[0128] In addition, while the shape of the retention layer 34 is simplified in Figure 29(A), as shown in Figure 29(C), the retention layer 34 has a base 34a formed on the substrate 30, a top 34b formed on the surface of the second sacrificial layer 33, and a column portion 34c extending between them.

[0129] The base 34a of the retaining layer 34 is formed so as to maximize the contact area with the substrate 30, thereby increasing the bonding strength between the retaining layer 34 and the substrate 30. The pillar portions 34c of the retaining layer 34 are bonded to the side surfaces of the first sacrificial layer 31, the semiconductor layer 32 and the second sacrificial layer 33.

[0130] 30(A) and (B) are a cross-sectional view and a plan view showing a process of forming the stress-applying film 35.

[0131] In step S306 (FIG. 26), as shown in FIG. 30(A), the stress-applying film 35 is formed on the second sacrificial layer 33. The stress-applying film 35 is attached to the surface of the second sacrificial layer 33 (i.e., the surface opposite to the substrate 10) in a heated state.

[0132] The stress-applying film 35 is, for example, a dry film resist. The thermal expansion coefficient T 35 is 70 x 10 -6 / K. This thermal expansion coefficient T 35 is the thermal expansion coefficient T of the substrate 30, the first sacrificial layer 31, and the second sacrificial layer 33. 30 ,T 31 ,T 32 ,T 33 The thickness of the stress applying film 35 is, for example, 30 μm.

[0133] Since the stress-applying film 35, which has a large thermal expansion coefficient, is attached to the surface of the second sacrificial layer 33 in a heated state, when the temperature returns to room temperature, tensile stress remains in the stress-applying film 35 in a direction that causes a convex warp toward the substrate 30.

[0134] In addition, the second sacrificial layer 33 (Si 3 N 4 ) has the smallest thermal expansion coefficient and is also relatively thick, so that when the stress-applying film 35 is attached to the surface of the second sacrificial layer 33, a tensile stress remains in the second sacrificial layer 33 in a direction that causes the second sacrificial layer 33 to warp convexly toward the substrate 30.

[0135] 31(A) and (B) are a cross-sectional view and a plan view showing the step of removing the first sacrificial layer 31.

[0136] In step S307 (FIG. 26), as shown in FIGS. 31(A) and 31(B), the first sacrificial layer 31 is removed by wet etching using hydrochloric acid with a concentration of 4%.

[0137] When the first sacrificial layer 31 is removed, the semiconductor layer 32 and the second sacrificial layer 33 are warped so as to be convex toward the substrate 30 side due to the residual tensile stress of the stress-applying film 35 and the second sacrificial layer 33. Due to this warping, the gap between the semiconductor layer 32 and the substrate 30 becomes wider at the periphery. Therefore, the etching solution can easily enter the gap between the semiconductor layer 32 and the substrate 30.

[0138] The second sacrificial layer 33 has a thickness of 0.3 μm, which is thicker than the second sacrificial layer 23 of the second embodiment. In addition, the side surface of the semiconductor layer 32 is bonded to the retaining layer 34. Therefore, the second sacrificial layer 33 and the retaining layer 34 can support the semiconductor layer 32 and the stress-applying film 35.

[0139] 32(A) and 32(B) are a cross-sectional view and a plan view showing the step of removing the second sacrificial layer 33.

[0140] In step S308 (FIG. 26), as shown in FIGS. 32(A) and 32(B), the second sacrificial layer 33 is removed. The second sacrificial layer 33 is removed by, for example, etching using phosphoric acid. Since the stress-applying film 35 is held by the holding layer 34, a gap is formed between the stress-applying film 35 and the semiconductor layer 32.

[0141] Unlike the first and second embodiments, in the third embodiment, the side surface of the semiconductor layer 32 is bonded to the retention layer 34. Therefore, the semiconductor layer 32 is supported by the retention layer 34 while being spaced apart from both the substrate 30 and the stress-applying film 35.

[0142] 33(A) and (B) are a cross-sectional view and a plan view showing a step of removing the stress-applying film 35.

[0143] In step S309 (FIG. 26), the stress-applying film 35 is removed as shown in FIGS. 33(A) and 33(B). The stress-applying film 35 can be peeled off from the retaining layer 34 by pulling it upward. At this time, a part of the retaining layer 34 (e.g., the top portion 34b) may be broken and attached to the stress-applying film 35, and may be removed together with the stress-applying film 35.

[0144] As a result, the semiconductor layer 32 supported by the support layer 34 on the substrate 30 is obtained, as shown in FIGS. 33(A) and (B).

[0145] 34(A) and (B) are cross-sectional views showing a stepwise process of peeling off the semiconductor layer 32 from the substrate 30.

[0146] In step S310 (FIG. 26), the semiconductor layer 32 is peeled off from the substrate 30 using the pickup unit 37. The pickup unit 37 has a holder 38 and a support substrate 39. The holder 38 and the support substrate 39 are configured similarly to the holder 18 and the support substrate 19 (FIG. 11(A)) of the pickup unit 17 of the first embodiment.

[0147] 34(A), the pickup unit 37 is moved toward the substrate 30, and the holder 38 is pressed against the surface of the semiconductor layer 32. Although the semiconductor layer 32 is held by the holding layer 34, it may be dropped onto the substrate 30 by the pressing force of the pickup unit 37.

[0148] 34(B), the pickup unit 37 is moved in a direction away from the substrate 30. By appropriately adjusting the adhesive force of the holder 38 of the pickup unit 37, the semiconductor layer 32 can be separated from the holder layer 34 or the substrate 30.

[0149] 35(A) and (B) are cross-sectional views showing stepwise the process of transferring the semiconductor layer 32 to a transfer substrate 60 which is different from the substrate 30. FIG.

[0150] In step S311 (FIG. 26), the semiconductor layer 32 is transferred to a transfer substrate 60 separate from the substrate 30 using the pickup unit 37. The transfer substrate 60 has a structure similar to that of the transfer substrate 50 of the first embodiment (FIGS. 13(A) to (C)).

[0151] 35(A), the pickup unit 37 is moved toward the transfer substrate 60, and the semiconductor layer 32 is pressed against the surface of the transfer substrate 60. The bottom surface of the semiconductor layer 32 and the surface of the transfer substrate 60 are both smooth surfaces, and are bonded to each other by intermolecular forces due to the application of a predetermined pressure and heat.

[0152] Thereafter, the pick-up unit 37 is moved in a direction away from the transfer substrate 60. Since the semiconductor layer 32 is bonded to the transfer substrate 60 by intermolecular forces, the semiconductor layer 32 remains on the transfer substrate 60, and the holder 18 of the pick-up unit 37 moves away from the semiconductor layer 32. As a result, a base substrate 6 in which the semiconductor layer 32 is bonded onto the transfer substrate 60 is obtained, as shown in Fig. 35(B).

[0153] In step S312 (FIG. 26), as described in the second embodiment with reference to FIG. 25(C), wiring and the like are formed in the semiconductor layer 32. This completes the electronic device.

[0154] <Advantages of the Third Embodiment> As described above, in the method for manufacturing an electronic device according to the third embodiment, tensile stress in a direction that causes warping remains in both the stress-applying film 35 and the second sacrificial layer 33. Therefore, it is possible to cause warping in the semiconductor layer 32 more effectively than in the second embodiment, and to efficiently remove the first sacrificial layer 31.

[0155] Furthermore, since the retention layer 34 is formed so as to contact the side surface of the semiconductor layer 32, the semiconductor layer 32 can be retained by the retention layer 34 in the step of removing the sacrificial layers 31 and 33. Since no gap is generated between the semiconductor layer 32 and the retention layer 34, the positional accuracy of the semiconductor layer 32 in the step of removing the second sacrificial layer 33 can be improved.

[0156] Fourth Embodiment <Manufacturing method> Fig. 36 is a flowchart showing a manufacturing method of the electronic device of the fourth embodiment. Fig. 37(A) is a cross-sectional view showing a substrate 40. Fig. 37(B) is a cross-sectional view showing a step of forming a first sacrificial layer 41 and a semiconductor layer 42 on the substrate 40. Fig. 37(C) is a cross-sectional view showing a step of patterning the first sacrificial layer 41 and the semiconductor layer 42.

[0157] 37A is a GaAs substrate, for example. The thickness of the substrate 40 is, for example, 600 μm.

[0158] In step S401 (FIG. 36), as shown in FIG. 37(B), a first sacrificial layer 41 is formed by epitaxial growth on a substrate 40. The first sacrificial layer 41 is, for example, an AlAs layer. The thickness of the first sacrificial layer 41 is, for example, 0.05 μm.

[0159] In step S402 (FIG. 36), the semiconductor layer 42 is formed by epitaxial growth on the first sacrificial layer 41. The semiconductor layer 42 is, for example, an AlGaAs layer. The thickness of the semiconductor layer 42 is, for example, 1.2 μm.

[0160] In step S403 (FIG. 36), as shown in FIG. 37(C), the first sacrificial layer 41 and the semiconductor layer 42 are patterned. The patterning is performed by, for example, dry etching. The first sacrificial layer 41 and the semiconductor layer 42 are divided into a grid shape similar to the semiconductor layer 15 (FIG. 5) of the first embodiment.

[0161] 38(A) and (B) are a cross-sectional view and a plan view showing a step of forming a second sacrificial layer 43.

[0162] In step S404 (FIG. 36), as shown in FIGS. 38(A) and (B), a second sacrificial layer 43 is formed so as to cover the patterned first sacrificial layer 41 and semiconductor layer 42. The second sacrificial layer 43 is formed so as to cover the side surface of the first sacrificial layer 41, the side surface of the semiconductor layer 42, and the surface of the semiconductor layer 42 (i.e., the surface opposite to the substrate 40).

[0163] The second sacrificial layer 43 is, for example, Al 2 O 3 The second sacrificial layer 43 is a layer formed by sputtering, etc. The thickness of the second sacrificial layer 43 is, for example, 0.05 μm.

[0164] 39(A) and (B) are a cross-sectional view and a plan view showing a step of forming an opening in the second sacrificial layer 43. As shown in FIG.

[0165] In step S405 (FIG. 36), as shown in FIG. 39(A), openings 43a are formed in the second sacrificial layer 43. The openings 43a are formed by, for example, dry etching. As shown in FIG. 39(B), the openings 43a are formed on, for example, each of the four sides of the semiconductor layer 42. The arrangement of the openings 43a is not limited to this example, and it is sufficient that the side surfaces of the first sacrificial layer 41 can be exposed.

[0166] The substrate 40, the first sacrificial layer 41, the semiconductor layer 42, and the second sacrificial layer 43 are collectively referred to as a laminated substrate.

[0167] 40(A) and (B) are a cross-sectional view and a plan view showing a step of forming the retention layer 44.

[0168] In step S406 (FIG. 36), as shown in FIG. 40(A), a retention layer 44 is formed as a coating layer. The retention layer 44 is, for example, an organic material, more specifically, a rubber-based resist. The thickness of the retention layer 44 is, for example, 3.5 μm.

[0169] The retention layer 44 is formed so as to extend from the surface of the substrate 40, through the side surface of the second sacrificial layer 43, to the surface of the second sacrificial layer 43 (i.e., the surface opposite to the substrate 40). As shown in FIG. 40(B), the retention layer 44 is formed at each of the four corners of the semiconductor layer 42. Note that the arrangement of the retention layer 44 is not limited to the four corners, and it is sufficient if it can support the semiconductor layer 42 at a position spaced apart from the substrate 40. For example, two or more retention layers 44 may be formed so as to intersect in a lattice pattern.

[0170] 41(A) and (B) are a cross-sectional view and a plan view showing a state in the middle of removing the first sacrificial layer 41.

[0171] In step S407 (FIG. 36), as shown in FIG. 41(A), the first sacrificial layer 41 is removed by wet etching using hydrochloric acid with a concentration of 4%.

[0172] Etching of the first sacrificial layer 41 progresses from the periphery to the center. If the periphery of the semiconductor layer 42 sags downward (i.e., toward the substrate 40), the infiltration of the etching liquid into the gap between the semiconductor layer 42 and the substrate 40 may be hindered.

[0173] However, since the second sacrificial layer 43 supports the semiconductor layer 42 from above (i.e., the side opposite to the substrate 40), the peripheral portion of the semiconductor layer 42 is prevented from drooping toward the substrate 40. Therefore, the etching liquid easily enters the gap between the semiconductor layer 42 and the substrate 40.

[0174] 42(A) and (B) are a cross-sectional view and a plan view showing a state in which the first sacrificial layer 41 has been completely removed. As shown in Fig. 42(A) and (B), until the first sacrificial layer 41 is completely removed, the semiconductor layer 42 is supported from above by the holding layer 44 via the second sacrificial layer 43, so that the semiconductor layer 42 is prevented from sagging. This allows the etching solution to spread throughout the entire gap between the semiconductor layer 42 and the substrate 40, eliminating etching residue and allowing the first sacrificial layer 41 to be removed efficiently.

[0175] 43(A) and (B) are a cross-sectional view and a plan view showing a step of removing the second sacrificial layer 43.

[0176] In step S408 (FIG. 36), as shown in FIGS. 43(A) and (B), the second sacrificial layer 43 is removed. The second sacrificial layer 43 is removed by etching using phosphoric acid, for example. By removing the second sacrificial layer 43, the semiconductor layer 42 falls onto the substrate 40 and is held in a state on the substrate 40.

[0177] 44(A) and (B) are cross-sectional views showing a stepwise process of peeling off the semiconductor layer 42 from the substrate 40.

[0178] In step S409 (FIG. 36), the semiconductor layer 42 is peeled off from the substrate 40 using the pickup unit 47. The pickup unit 47 has a holder 48 and a support substrate 49 that supports the holder 48. The holder 48 and the support substrate 49 are configured similarly to the holder 18 and the support substrate 19 of the pickup unit 17 of the first embodiment.

[0179] First, the pickup unit 47 is moved toward the substrate 40 as shown in FIG. 44(A), and the holder 28 is pressed against the surface of the semiconductor layer 42 (that is, the surface opposite to the substrate 40).

[0180] 44(B), the pickup unit 27 is moved in a direction away from the substrate 40. Since the semiconductor layer 42 is held in a state of being placed on the substrate 40, it can be easily separated from the surface of the substrate 40.

[0181] 45(A) and (B) are cross-sectional views showing stepwise the process of transferring the semiconductor layer 42 to a transfer substrate 60 which is different from the substrate 40. FIG.

[0182] In step S410 (FIG. 36), the semiconductor layer 42 is transferred to a transfer substrate 60 separate from the substrate 40 using the pickup unit 47. The transfer substrate 60 has a structure similar to that of the transfer substrate 50 of the first embodiment (FIGS. 13(A) to (C)).

[0183] First, the pickup unit 47 is moved toward the transfer substrate 60 as shown in Fig. 45(A) to press the semiconductor layer 42 against the surface of the transfer substrate 60. The bottom surface of the semiconductor layer 42 and the surface of the transfer substrate 60 are both smooth surfaces, and are bonded to each other by intermolecular forces due to the application of a predetermined pressure and heat.

[0184] Thereafter, the pick-up unit 47 is moved in a direction away from the transfer substrate 60. Since the semiconductor layer 42 is bonded to the transfer substrate 60 by intermolecular forces, the semiconductor layer 42 remains on the transfer substrate 60, and the holder 28 of the pick-up unit 47 moves away from the semiconductor layer 42. As a result, a base substrate 6 in which the semiconductor layer 42 is bonded onto the transfer substrate 60 is obtained, as shown in Fig. 45(B).

[0185] In step S411 (FIG. 36), as described in the second embodiment with reference to FIG. 25(C), wiring and the like are formed in the semiconductor layer 42. This completes the electronic device.

[0186] <Advantages of the Fourth Embodiment> As described above, in the method for manufacturing an electronic device according to the fourth embodiment, the first sacrificial layer 41 is removed while the semiconductor layer 42 is supported by the retaining layer 44 via the second sacrificial layer 43. Therefore, sagging of the peripheral portion of the semiconductor layer 42 can be suppressed during the removal of the first sacrificial layer 41. This allows the etching solution to sufficiently spread in the gap between the substrate 40 and the semiconductor layer 42, and the first sacrificial layer 41 can be efficiently removed.

[0187] It should be noted that the first to fourth embodiments can be combined as appropriate, and each embodiment can be improved or modified in various ways.

[0188] Various aspects of the present disclosure are summarized below as appendices. (Appendix 1) A step of forming a coating layer from the substrate to a surface of the second sacrificial layer opposite to the semiconductor layer, using a laminate substrate having a substrate, a first sacrificial layer provided on the substrate, a semiconductor layer formed on the first sacrificial layer, and a second sacrificial layer formed on the semiconductor layer from a material different from that of the first sacrificial layer; removing the first sacrificial layer; removing the second sacrificial layer after removing the first sacrificial layer; peeling the semiconductor layer from the substrate; transferring the semiconductor layer to a substrate other than the substrate; A method for manufacturing an electronic device comprising the steps of: (Appendix 2) Before the step of forming the coating layer, forming the semiconductor layer on the first sacrificial layer provided on the substrate; forming a second sacrificial layer on the semiconductor layer, the second sacrificial layer being of a different material than the first sacrificial layer. 2. A method for producing an electronic device according to claim 1, (Appendix 3) The substrate and the semiconductor layer include A combination is used in which the thermal expansion coefficient of the substrate is smaller than the thermal expansion coefficient of the semiconductor layer. 3. A method for producing an electronic device according to claim 1 or 2. (Appendix 4) A Si substrate is used as the substrate, A GaN-based semiconductor layer is formed as the semiconductor layer. 4. A method for producing an electronic device according to claim 1, (Appendix 5) In the step of removing the first sacrificial layer, The first sacrificial layer is removed in a state in which the semiconductor layer is warped so as to be convex toward the substrate. 5. A method for producing an electronic device according to claim 1, (Appendix 6) The method further includes forming an organic material layer on the second sacrificial layer before removing the first sacrificial layer; The organic material layer has a thermal expansion coefficient greater than the thermal expansion coefficients of the substrate, the semiconductor layer, the first sacrificial layer, and the second sacrificial layer. 6. A method for producing an electronic device according to any one of claims 1 to 5. (Appendix 7) In the step of removing the first sacrificial layer, the first sacrificial layer is removed in a state in which the semiconductor layer is warped so as to be convex toward the substrate side due to the deformation of the organic material layer. 7. A method for producing an electronic device according to claim 6, (Appendix 8) Prior to the step of peeling the semiconductor layer from the substrate, removing at least a portion of the organic material layer and the covering layer; 8. The method for producing an electronic device according to claim 6 or 7, further comprising: (Appendix 9) Before the step of forming the coating layer, patterning the first sacrificial layer, the semiconductor layer, and the second sacrificial layer; In the step of forming the covering layer, the covering layer is formed so as to be in contact with a side surface of the semiconductor layer. 9. A method for producing an electronic device according to any one of claims 1 to 8. (Appendix 10) Before the step of forming the coating layer, forming an opening in the second sacrificial layer to expose a side surface of the first sacrificial layer; 10. A method for producing an electronic device according to any one of claims 1 to 9. (Appendix 11) The first sacrificial layer is part of the substrate. 11. A method for producing an electronic device according to any one of claims 1 to 10. (Appendix 12) The first sacrificial layer is formed on the substrate. 11. A method for producing an electronic device according to any one of claims 1 to 10. [Explanation of symbols]

[0189] 1,2 electronic device; 5,6 base substrate; 10,20,30,40 substrate; 10a,21,31,41 first sacrificial layer; 11 buffer layer; 12 functional layer; 13,23,33,43 second sacrificial layer; 13a,23a,43a opening; 14,24,34,44 holding layer (covering layer); 15,22,32,42 semiconductor layer; 17,27,37,47 pick-up portion; 18,28,38,48 holding body; 19,29,39,49 support substrate; 25,35 stress-applying film; 50,60 transfer substrate.

Claims

1. A step of forming a coating layer from the substrate to a surface of the second sacrificial layer opposite to the semiconductor layer, using a laminate substrate having a substrate, a first sacrificial layer provided on the substrate, a semiconductor layer formed on the first sacrificial layer, and a second sacrificial layer formed on the semiconductor layer from a material different from that of the first sacrificial layer; removing the first sacrificial layer; removing the second sacrificial layer after removing the first sacrificial layer; peeling the semiconductor layer from the substrate; transferring the semiconductor layer to a substrate other than the substrate; A method for manufacturing an electronic device comprising the steps of:

2. Before the step of forming the coating layer, forming the semiconductor layer on the first sacrificial layer provided on the substrate; forming a second sacrificial layer on the semiconductor layer, the second sacrificial layer being of a different material than the first sacrificial layer. The method for manufacturing an electronic device according to claim 1 .

3. The substrate and the semiconductor layer include A combination is used in which the thermal expansion coefficient of the substrate is smaller than the thermal expansion coefficient of the semiconductor layer.

3. The method for manufacturing an electronic device according to claim 1 or 2.

4. A Si substrate is used as the substrate, A GaN-based semiconductor layer is formed as the semiconductor layer.

3. The method for manufacturing an electronic device according to claim 1 or 2.

5. In the step of removing the first sacrificial layer, The first sacrificial layer is removed in a state in which the semiconductor layer is warped so as to be convex toward the substrate.

3. The method for manufacturing an electronic device according to claim 1 or 2.

6. The method further includes forming an organic material layer on the second sacrificial layer before removing the first sacrificial layer; The organic material layer has a thermal expansion coefficient greater than the thermal expansion coefficients of the substrate, the semiconductor layer, the first sacrificial layer, and the second sacrificial layer.

3. The method for manufacturing an electronic device according to claim 1 or 2.

7. In the step of removing the first sacrificial layer, the first sacrificial layer is removed in a state in which the semiconductor layer is warped so as to be convex toward the substrate side due to the deformation of the organic material layer. The method for manufacturing an electronic device according to claim 6 .

8. Prior to the step of peeling the semiconductor layer from the substrate, removing at least a portion of the organic material layer and the covering layer; The method for producing an electronic device according to claim 6 , further comprising:

9. Before the step of forming the coating layer, patterning the first sacrificial layer, the semiconductor layer and the second sacrificial layer; In the step of forming the covering layer, the covering layer is formed so as to be in contact with a side surface of the semiconductor layer.

3. The method for manufacturing an electronic device according to claim 1 or 2.

10. Before the step of forming the coating layer, forming an opening in the second sacrificial layer to expose a side surface of the first sacrificial layer; 3. The method for manufacturing an electronic device according to claim 1 or 2.

11. The first sacrificial layer is part of the substrate.

3. The method for manufacturing an electronic device according to claim 1 or 2.

12. The first sacrificial layer is formed on the substrate.

3. The method for manufacturing an electronic device according to claim 1 or 2.

Citation Information

Patent Citations

  • Method of manufacturing semiconductor thin-film element and semiconductor wafer, and the semiconductor thin-film element

    JP2010258352A

  • Semiconductor wafer, and method of manufacturing semiconductor device using the same

    JP2011103466A