Target substance detection reagent, target substance detection kit, and method for detecting target substance

Surface-modified latex particles with a phosphorylcholine group sensitizer improve dispersibility and sensitivity in target substance detection by preventing agglomeration and enhancing antigen-antibody reactions.

JP2024143336AInactive Publication Date: 2024-10-11SUMITOMO BAKELITE CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023055958
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-30
Publication Date
2024-10-11
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The dispersibility of latex particles in existing latex immunoagglutination reagents is inadequate, leading to potential agglomeration and reduced sensitivity in target substance detection.

Method used

Surface-treating latex particles with a surface-modified polymer containing a reactive functional group and using a sensitizer with a phosphorylcholine group to improve dispersibility and enhance antigen-antibody reactions.

Benefits of technology

Enhances the dispersibility of polymer-coated particles, preventing agglomeration and increasing sensitivity in target substance detection methods.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024143336000001_ABST
    Figure 2024143336000001_ABST
Patent Text Reader

Abstract

To provide a target substance detection reagent that excels in the dispersibility of a polymer-attached particle.SOLUTION: A target substance detection reagent according to the present invention includes a polymer-attached particle, a sensitizer, and a dispersant. The polymer-attached particle includes a core particle, and a surface-modified polymer formed on at least a portion of the surface of the core particle. The surface-modified polymer includes a structural unit A1 including a reactive functional group (A1) capable of binding to a ligand that has the ability to specifically bind to a target substance. The sensitizer includes a polymer having a phosphorylcholine group.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a target substance detection reagent, a target substance detection kit, and a method for detecting a target substance. [Background technology]

[0002] The latex immunoagglutination method is known as a method for measuring a target substance in a sample. The latex immunoagglutination method is a measurement method in which, for example, latex particles carrying antibodies against a target substance are used, and the degree of agglutination (turbidity) of the latex particles caused by binding between the target substance, an antigen, and the antibody-carrying latex particles is detected by optical means or the like. As an example of this type of technology, the technology described in Patent Document 1 is known. Patent Document 1 describes a reagent for measuring a target substance in a sample using a latex immunoagglutination method, which includes latex particles carrying an antibody that specifically recognizes the target substance in the sample (e.g., claim 7 of Patent Document 1). Patent Document 1 also describes that dipropylene glycol is contained in the reagent to increase the sensitivity in the agglutination method. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2021-162593 A Summary of the Invention [Problem to be solved by the invention]

[0004] However, as a result of investigations conducted by the present inventors, it was found that there is room for improvement in terms of dispersibility of the latex particles in the reagent containing the latex particles described in Patent Document 1 above. [Means for solving the problem]

[0005] After further investigation, the present inventors found that ligand binding ability can be imparted to the polymer-attached particles by surface-treating the surface of core particles such as latex particles with a surface-modifying polymer to form polymer-attached particles, and then introducing a reactive functional group (A1) having ligand binding ability into the surface-modifying polymer. Based on this finding, further intensive research led to the discovery that, in a reagent comprising such polymer-attached particles, a sensitizer and a dispersing medium, by using a polymer having a phosphorylcholine group as the sensitizer, the dispersibility of the polymer-attached particles in the dispersing medium before the ligand and target substance are bonded to each other can be increased, thereby completing the present invention.

[0006] According to one aspect of the present invention, there are provided the following target substance detection reagent, target substance detection kit, and target substance detection method. 1. A target substance detection reagent comprising a polymer-attached particle, a sensitizer, and a dispersion medium, The polymer-attached particle includes a core particle and a surface-modifying polymer formed on at least a portion of the surface of the core particle, The surface-modifying polymer comprises a structural unit A1 including a reactive functional group (A1) capable of binding to a ligand having specific binding ability to a target substance; The sensitizer is a target substance detection reagent that contains a polymer having a phosphorylcholine group. 2. The target substance detection reagent according to 1., A target substance detection reagent, wherein a ratio of structural units having a phosphorylcholine group contained in all structural units of the polymer having a phosphorylcholine group is 10 mol % or more and 100 mol % or less. 3. A target substance detection reagent according to 1. or 2., A target substance detection reagent, wherein the surface-modified polymer in the polymer-attached particle contains a structural unit A2 containing a salt formed between an acidic functional group (A2) and an organic base. 4. The target substance detection reagent according to 3., A target substance detection reagent, wherein the acidic functional group (A2) includes one or more groups selected from the group consisting of a carboxy group, a sulfo group, a phosphate group, and a hydroxyl group. 5. A target substance detection reagent according to any one of 1. to 4., A target substance detection reagent, wherein the reactive functional group (A1) includes one or more selected from the group consisting of a carboxy group, a phenolic hydroxy group, an amino group, a thiol group, an epoxy group, a maleimide group, an acryl group, a methacryl group, a (meth)acryl group, and an acid anhydride group. 6. A target substance detection reagent according to any one of 1. to 5., A target substance detection reagent, wherein the organic base comprises a nitrogen-containing base and / or a phosphorus-containing base. 7. The target substance detection reagent according to claim 3, A target substance detection reagent, wherein the surface-modifying polymer has a weight-average molecular weight of 1,000 or more and 10,000,000 or less. 8. A target substance detection reagent according to any one of 1. to 7., A target substance detection reagent, wherein the core particle is an organic particle or an inorganic particle. 9. A target substance detection reagent according to any one of 1. to 8., The surface-modifying polymer comprises the ligand bound to at least a portion of the reactive functional groups (A1). 10. A target substance detection reagent according to any one of 1. to 9., A target substance detection reagent, wherein the ligand is any one of an antibody, an antigen, a protein, and a nucleic acid. 11. A target substance detection reagent according to any one of 1. to 10., A target substance detection reagent used in agglutination methods. 12. A target substance detection kit comprising a reagent container containing a target substance detection reagent described in any one of 1. to 11. 13. A method for detecting a target substance, comprising a step of mixing a target substance with a target substance detection reagent described in any one of 1. to 11. Effect of the Invention

[0007] According to the present invention, there are provided a target substance detection reagent, a target substance detection kit, and a target substance detection method, which have excellent dispersibility of polymer-attached particles. [Brief description of the drawings]

[0008] [Figure 1] FIG. 2 is a cross-sectional view illustrating an example of the configuration of a polymer-attached particle according to the present embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0009] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. In all drawings, similar components are given similar reference numerals and their explanations will be omitted as appropriate. Also, the drawings are schematic diagrams and do not correspond to the actual dimensional ratios.

[0010] The target substance detection reagent of this embodiment will be outlined below.

[0011] The target substance detection reagent of this embodiment contains a polymer-attached particle, a sensitizer, and a dispersion medium. In the target substance detection reagent, the polymer-attached particle comprises a core particle and a surface-modified polymer formed on at least a portion of the surface of the core particle and comprising a structural unit A1 containing a reactive functional group (A1) capable of binding to a ligand having specific binding ability to the target substance, and the sensitizer comprises a polymer having a phosphorylcholine group.

[0012] Currently, sensitizers such as polyethylene glycol (PEG) that are commonly used for latex particles can increase sensitivity, but can also cause latex particles to aggregate. The sensitizer captures water contained in the dispersion medium, forms a hydrophobic field in the dispersion medium, and localizes the latex particles in the hydrophobic field, thereby increasing the probability of contact between the antibodies possessed by the latex particles and the antigens present in the dispersion medium, thereby increasing sensitivity. The hydrophobic field in the dispersion medium creates an environment in which latex particles attract each other and aggregate, which could reduce the dispersibility of the latex particles.

[0013] In contrast, the inventors have discovered that by using a polymer having a phosphorylcholine group as a sensitizer, the dispersibility of the polymer-attached particles in the dispersion medium before the ligand and target substance are bonded to each other can be increased. Although the detailed mechanism is unclear, it is presumed that by using a polymer having phosphorylcholine groups as a sensitizer, the phosphorylcholine groups become hydrated, thereby exhibiting an adsorption-inhibiting effect, thereby suppressing self-aggregation of the polymer-attached particles. It is also presumed that by increasing the ratio of structural units having phosphorylcholine groups in the polymer, a hydrophobic field is formed and polymer particles are delocalized, thereby promoting the antigen-antibody reaction.

[0014] The polymer having a phosphorylcholine group has at least one or two or more structural units M having a phosphorylcholine group in the side chain of the polymer. The phosphorylcholine group may be partially modified as long as it can be used as a phospholipid polar group, which is a component of biomembranes. The polymer having a phosphorylcholine group may be a homopolymer having only the structural unit M, or a copolymer having the structural unit M and another structural unit N. The structural unit N may be a structural unit having, for example, any one of a hydrophobic group, an anionic group, a cationic group, and a hydrogen-bonding group on a side chain of the polymer. The main chain of the polymer having a phosphorylcholine group has a structure in which the polymerizable groups in the raw material monomers are linked to each other.

[0015] The polymer having a phosphorylcholine group may be a polymer of raw material monomers containing at least 2-methacryloyloxyethyl phosphorylcholine (MPC), and specifically, may contain one or more types of MPC polymers represented by the following general formula (1).

[0016] [ka]

[0017] In the above general formula (1), R represents, for example, any one of a hydrophilic group, a hydrophobic group, an anionic group, a cationic group, and a hydrogen-bonding group. The hydrophobic group can be, for example, a hydrocarbon group having 1 to 20 carbon atoms, preferably a linear or cyclic hydrocarbon group having 1 to 20 carbon atoms, more preferably an alkyl group having 1 to 20 carbon atoms.

[0018] In the above general formula (1), m+n is 1.0. m is, for example, 0.1 to 1.0, preferably 0.2 to 1.0, and more preferably 0.3 to 1.0. n is, for example, 0 to 0.9, preferably 0 to 0.8, and more preferably 0 to 0.7.

[0019] The ratio of structural units having a phosphorylcholine group contained in all structural units of the polymer having a phosphorylcholine group is, for example, 10 mol% or more and 100 mol% or less, preferably 20 mol% or more and 100 mol% or less, and more preferably 30 mol% or more and 100 mol% or less. By adjusting the content of phosphorylcholine groups to the above lower limit or more, the sensitivity can be improved.

[0020] The ratio of structural units having phosphorylcholine groups can be determined from the peak area obtained by NMR measurement, the number of moles of each structural unit contained in the raw material, or the molecular weight of the monomer that is the base of each structural unit contained in the raw material.

[0021] The weight average molecular weight of the polymer having a phosphorylcholine group is, for example, 1,000 to 1,000,000, preferably 10,000 to 750,000, and more preferably 30,000 to 500,000. The weight average molecular weight can be measured by GPC (gel permeation chromatography).

[0022] The polymer having a phosphorylcholine group may be produced by polymerizing one or more monomers M containing a phosphorylcholine group and a polymerizable group. As the polymerizable group, for example, a methacryloyl group or the like may be used. Examples of the monomer M include 2-methacryloyloxyethyl phosphorylcholine, 2-acryloyloxyethyl phosphorylcholine, 4-methacryloyloxybutyl phosphorylcholine, 6-methacryloyloxyhexyl phosphorylcholine, 10-methacryloyloxydecyl phosphorylcholine, ω-methacryloyloxypoly(ethylene oxide)ethyl phosphorylcholine, 4-styryloxybutyl phosphorylcholine, etc. Among these, 2-methacryloyloxyethyl phosphorylcholine (MPC) is preferred from the viewpoints of polymerization characteristics and availability of raw material compounds.

[0023] A polymer bearing phosphorylcholine groups may be prepared by polymerizing a monomer M with another monomer N which is polymerizable with the polymerizable group of monomer M. Examples of the monomer N include methacrylic acid esters and methacrylamides. Examples of methacrylic acid esters include ethyl methacrylate, propyl methacrylate, n-butyl methacrylate, pentyl methacrylate, hexyl methacrylate, heptyl methacrylate, octyl methacrylate, tridecyl methacrylate, 2-ethoxyethyl methacrylate, 2-ethoxypropyl methacrylate, 2-phenoxyethyl methacrylate, 2-butoxyethyl methacrylate, etc. Among these, n-butyl methacrylate (n-butyl methacrylate, BMA) is particularly preferred.

[0024] The target substance detection reagent may be any one that contains a particle group of polymer-attached particles, which will be described later. The concentration of the polymer-attached particles in the dispersion medium can be appropriately set, and is, for example, 0.01 to 1.0% by weight, preferably 0.03 to 0.75% by weight, and more preferably 0.05 to 0.5% by weight.

[0025] As the dispersion medium, for example, an aqueous solvent described below is preferably used. The aqueous solvent may contain, within the scope of the invention, a third substance such as a buffer, a preservative (e.g., sodium azide), a blocking agent such as a protein (albumin), a sensitizer such as a water-soluble polymer (e.g., sugar, polyethylene glycol, dextran), a salt (e.g., sodium chloride, amino acid), a surfactant, etc. These may be used alone or in combination of two or more kinds. The polymer-attached particles in the reagent may be subjected to a blocking treatment using a blocking agent such as bovine serum albumin (BSA).

[0026] (particles with polymer) The configuration of the polymer-attached particles of this embodiment will be described in detail below.

[0027] FIG. 1 is a cross-sectional view that illustrates an example of the configuration of a polymer-attached particle 10 according to this embodiment. An example of the polymer-attached particle 10 has at least a core particle 1 and a surface-modifying polymer 2 formed on at least a part of the surface of the core particle 1 .

[0028] The polymer-attached particles 10 of this embodiment can be used as particles for an agglutination method used in detecting a target substance by an agglutination method. The polymer-attached particles 10 used in the aggregation method have ligands 3 chemically fixed to the surface.

[0029] The agglutination method is a method in which a sample containing a target substance (e.g., an antigen) is contacted in a dispersion medium with polymer-attached particles 10 carrying a ligand 3 (e.g., an antibody) that specifically recognizes (binds to) the target substance, causing the ligand 3 to bind to the target substance, forming a complex between the target substance, the ligand 3, and the polymer-attached particles 10, and selectively agglutinating the polymer-attached particles 10. The immunoagglutination method (also called immunoturbidimetry), which is one of the agglutination methods, utilizes an antigen-antibody reaction to react an antigen with an antibody present on the surface of the polymer-attached particles 10, thereby agglutinating the polymer-attached particles 10. In a method for detecting a target substance using an agglutination method, the degree of agglutination of the polymer-attached particles 10 can be characterized and quantified by optical measurement such as absorbance, scattered light intensity, or transmitted light intensity.

[0030] According to the present embodiment, the dispersibility of the polymer-attached particles 10 in the dispersion medium can be increased. This makes it possible to suppress the polymer-attached particles 10 from aggregating with each other in the dispersion medium before reacting with the target substance, i.e., to suppress non-specific reactions.

[0031] Furthermore, according to this embodiment, the dispersibility of the polymer-attached particles 10 can be improved, so that the change in the degree of aggregation of the polymer-attached particles 10 before and after the reaction with the target substance can be increased. In other words, when comparing the presence and absence of the target substance, the difference in optical measurement values ​​such as absorbance in a dispersion medium containing the polymer-attached particles 10 becomes large, so that it is possible to improve the sensitivity of the polymer-attached particles 10, i.e., the detection sensitivity of the target substance.

[0032] The sample is not particularly limited as long as it may contain the target substance, and examples thereof include any one or more biological samples selected from the group consisting of whole blood, plasma, serum, urine, cerebrospinal fluid, saliva, amniotic fluid, urine, sweat, and pancreatic juice. The sample is preferably whole blood, plasma, serum, or urine. The sample may be an aqueous medium containing the target substance, for example the target substance diluted in phosphate buffered saline or the like.

[0033] The aqueous solvent is not particularly limited as long as it is an aqueous solvent that allows the aggregation method, and examples thereof include deionized water, distilled water, and buffer solutions, with buffer solutions being preferred. Examples of the buffering agent contained in the buffer solution include phosphate-based, acetate-based, Tris-based, borate-based, carbonate-based, glycine-based, and Gut-based buffer solutions. As the Good's buffer, for example, HEPES, PIPES, MOPS, etc. are preferably used. The buffering agent may be used alone or in combination of two or more kinds. In addition, acids that can be used to adjust the pH of a buffer solution containing a buffer component include ordinary hydrochloric acid, sulfuric acid, nitric acid, and organic acids such as acetic acid, and alkalis that can be used include sodium hydroxide, potassium hydroxide, lithium hydroxide, ammonium hydroxide, and the like.

[0034] The target substance is not particularly limited as long as it is a target substance that allows for the agglutination method, and examples thereof include CRP (C-reactive protein); prostate-specific antigen (PSA); ferritin; α2-macroglobulin; β2-microglobulin; myoglobin; fibrin; fibrinogen degradation products; D-dimer; thrombin-antithrombin III complex (TAT); soluble fibrin (SF); soluble interleukin-2 receptor (sIL-2R); and sodium diuretic peptides such as atrial natriuretic peptide (ANP), brain natriuretic peptide (BNP), and C-type natriuretic peptide (CNP). These include urinary peptides; N-terminal pro-brain natriuretic peptide (NT-proBNP); antistreptolysin O; rheumatoid factor; transferrin; haptoglobin; α1-antitrypsin; α1-acidoglycoprotein; hemopexin; antithrombin-III; α-fetoprotein; CEA (carcinoembrionic antigen); HBs-Ag (hepatitis B envelope antigen); Anti-HBs (anti-hepatitis B envelope antibody); HBe-Ag (hepatitis B e antigen); Anti-HBe (anti-hepatitis B e antibody); Anti-HBc (anti-hepatitis B core antibody); IgG; IgA; IgM, etc. The target substance is not particularly limited as long as it is in a form that allows binding to an antibody, and may be, for example, in a free form as a simple substance, or in a complexed form with another substance (such as a protein).

[0035] The ligand 3 is a compound that specifically binds to a receptor of a specific target substance. The site at which a ligand binds to a target substance is fixed, and the ligand has a high affinity selectively or specifically. Examples of ligands include, but are not limited to, antigens and antibodies, enzyme proteins and their substrates, signal substances such as hormones and neurotransmitters and their receptors, and nucleic acids. Examples of the ligand include antibodies such as full-length antibodies and antigen-binding fragments (e.g., antibody fragments such as Fab, F(ab')2, F(ab'), Fv, and scFv); antigens; nucleic acids such as naturally occurring nucleic acids and artificial nucleic acids; proteins such as aptamers, peptide aptamers, oligopeptides, enzymes, and coenzymes; etc. Commercially available antibodies can be used as the antibodies that specifically recognize the target substance.

[0036] The core particle 1 is a particle that becomes the nucleus of the polymer-attached particle 10, and may be composed of either an organic particle or an inorganic particle. According to this embodiment, it is possible to improve the dispersibility of the polymer-attached particle 10 while taking advantage of the core particle characteristics (e.g., particle characteristics such as specific gravity and particle distribution) derived from the organic particle / inorganic particle.

[0037] As the organic particles, particles made of an organic polymer can be used. Examples of organic polymers include synthetic resins such as polystyrene, polyvinyl chloride, polypropylene, (meth)acrylic resins, polymethyl methacrylate, and silicone rubber; cellulose derivatives such as nitrocellulose, cellulose, and methylcellulose; phenolic resins, polylactic acid, polyethylene, and melamine phenol; copolymers containing one of these as a main component (for example, copolymers containing styrene as a main component); and copolymers containing two or more of these. The organic polymer may be used alone or in combination of two or more. The organic polymer constituting the organic particles is not particularly limited as long as it is composed of a polymer different from the surface-modifying polymer 2.

[0038] As the organic particles, known latex particles can be used, for example, styrene-based latex particles such as polystyrene latex, acrylic acid-based latex particles, various modified latex particles (for example, carboxylic acid-modified latex particles in which a carboxyl group is introduced into the above-mentioned polystyrene), colored latex particles, fluorescent latex particles, and the like. The latex particles can be produced by a known method, or may be commercially available. Two or more kinds of the latex particles may be used in combination.

[0039] Examples of methods for producing organic particles (resin particles) include a method in which raw material monomers (styrene, methacrylic acid, etc.) are polymerized with a polymerization initiator (radical polymerization initiator, etc.) to form a granular organic polymer in a solvent (water, etc.). The method for forming the granular organic polymer can be a radical polymerization method such as emulsion polymerization, soap-free emulsion polymerization, or suspension polymerization, but is not limited to radical polymerization.

[0040] As the inorganic particles, particles made of an inorganic substance can be used. Examples of inorganic substances include inorganic materials such as metals, ceramics, and glass. Specific examples of inorganic substances include silica. These may be used alone or in combination of two or more. In addition, inorganic materials having magnetic properties may be used as inorganic substances. In this way, the inorganic particles may be non-magnetic particles or magnetic particles.

[0041] The shape of the core particle 1 is not particularly limited, but examples thereof include a spherical shape, an elliptical shape, and an irregular shape.

[0042] The average particle diameter (D50) of the core particles 1 may be, for example, 0.01 μm to 1.0 μm, 0.02 μm to 0.8 μm, or 0.03 μm to 0.6 μm. The particle size of the core particle 1 can be measured, for example, by a laser diffraction particle size distribution analyzer. The average particle size (D50) is defined as the particle size at which the integrated value from the small particle side in the volume-based particle size distribution is 50%.

[0043] The surface modifying polymer 2 may be formed on at least a part of the surface of the core particle 1, and may form a polymer coating layer that covers a part or the entire surface of the core particle 1.

[0044] The state in which the surface-modifying polymer 2 is formed on the surface of the core particle 1 means a state in which the surface-modifying polymer 2 is physically bonded to the surface of the core particle 1 and / or a state in which a polymer reactive group present on the surface of the core particle 1 is chemically bonded to a specified reactive group contained in the surface-modifying polymer 2.

[0045] The method of forming the surface-modifying polymer 2 on the surface of the core particle 1 uses, for example, a polymer introduction step in which the surface-modifying polymer 2 is introduced onto the surface of the core particle 1 by a chemical reaction. For the chemical reaction, an immobilization method using a carboxy group or an immobilization method using an amino group, which are known as methods for immobilizing antibodies, can be used. These chemical reactions may involve the use of condensing agents, if desired, such as carbodiimide-based crosslinkers and amine-reactive crosslinkers. Carboxy groups and amino groups can be reacted with each other by using a carbodiimide crosslinking agent such as EDC (1-ethyl-3-(3-dimethylaminopropyl)carbodiimide hydrochloride, also known as EDAC or WSC). Amine-reactive crosslinkers can also be used to react primary or secondary amino groups with synthetic chemical groups such as isothiocyanates, isocyanates, acyl azides, NHS esters, sulfonyl chlorides, aldehydes, glyoxals, epoxides, oxiranes, carbonates, aryl halides, imidoesters, carbodiimides, anhydrides, fluoroesters, and the like.

[0046] When the core particle 1 is an organic particle (resin particle), a method is used in which a polymer reactive group (such as a carboxy group or an amino group) contained in the raw material monomer of the organic particle is reacted with a predetermined reactive group contained in the surface-modifying polymer 2. For example, in the manufacturing process of the organic particle, it becomes possible to include a polymer reactive group in the organic polymer during polymerization of the raw material monomer. Note that, as the core particle 1, a commercially available polystyrene particle containing a carboxy group may be used. As a specific example, when a surface-modifying polymer 2 containing a carboxy group is fixed to a core particle 1 containing a carboxy group, a primary amino group (-NH2) may be introduced by amino treatment to some of the carboxy groups in the core particle 1 (amino treatment). Then, the primary amino group (polymer reactive group) in the core particle 1 after the amino treatment and a predetermined reactive group in the surface-modifying polymer 2 are chemically reacted with each other by adding the above-mentioned condensing agent if necessary. When the surface-modifying polymer 2 contains an acrylic group / methacrylic group, it is possible to react a primary amino group (polymer reactive group) with a carboxy group (predetermined reactive group) contained in the acrylic group / methacrylic group via the above-mentioned condensing agent. In another embodiment, when the surface modifying polymer 2 contains an anhydride group, it is possible to react a primary amino group (polymer reactive group) with an anhydride group (predetermined reactive group) such as a maleic anhydride group without using the above-mentioned condensing agent. On the other hand, when the core particle 1 is an inorganic particle, a method is used in which a polymer reactive group is introduced onto the surface of the inorganic particle, if necessary, using coupling or the like, and then the polymer reactive group is reacted with a specific reactive group contained in the surface-modifying polymer 2.

[0047] In addition, the reactive functional group (A1) such as a carboxy group remaining after the introduction step of the surface-modifying polymer 2 can be bonded by chemical reaction with a functional group such as an amino group possessed by the ligand 3 during sensitization. In addition, a functional group similar to the reactive functional group (A1) present in the surface-modifying polymer 2 can also chemically react with a functional group such as an amino group possessed by the ligand 3 during sensitization.

[0048] The surface modifying polymer 2 may be composed of a (meth)acrylic polymer, a maleic anhydride polymer, a methylene malonate polymer, a phenol resin, an epoxy resin, etc. These may be used alone or in combination of two or more kinds. According to this embodiment, by using the surface-modifying polymer 2 in addition to the core particle 1, a wide variety of molecular designs are possible for the surface-modifying polymer 2, and the degree of freedom in molecular design is increased.

[0049] Examples of the (meth)acrylic polymer include methacrylic polymers and acrylic polymers. Examples of maleic anhydride polymers include maleic anhydride-norbornene copolymers, styrene-maleic anhydride copolymers, maleic anhydride homopolymers, methyl vinyl ether-maleic anhydride copolymers, and olefin-maleic anhydride copolymers.

[0050] The surface-modifying polymer 2 may be any of a homopolymer, a random copolymer, an alternating copolymer, a block copolymer, and a periodic copolymer.

[0051] The weight average molecular weight of the surface modifying polymer 2 is, for example, 1,000 or more and 10,000,000 or less, preferably 2,000 or more and 5,000,000 or less, and more preferably 3,000 or more and 1,000,000 or less. The weight average molecular weight can be determined using a polystyrene equivalent value from a calibration curve of standard polystyrene (PS) obtained by gel permeation chromatography measurement.

[0052] The surface modifying polymer 2 comprises a structural unit A1 that includes a reactive functional group (A1) capable of binding with a ligand 3.

[0053] The polymer-attached particles 10 used in the aggregation method may contain a ligand 3 bonded to at least a portion of the reactive functional groups (A1). The polymer-attached particles 10 having the ligand 3 are called sensitized particles. A conventionally known method can be applied as a method of chemical reaction for chemically fixing the reactive functional group (A1) and the ligand 3. The above-mentioned carbodiimide-mediated reaction, NHS ester activation reaction, etc. can be used as a chemical reaction method, but are not limited thereto. If necessary, a condensing agent may be used. For example, in order to bind (support) the ligand 3 to the polymer-attached particle 10, the ligand 3 (antibody) and the polymer-attached particle 10 may be suspended in a buffer solution and reacted for a predetermined time at about 20 to 37°C, followed by a washing process and a blocking process. If necessary, other operational processes such as centrifugation, ultrasonication, and heating (aging) may be performed at an appropriate timing. Sensitized particles can be obtained by including one or more processes that are usually used in the technical field of sensitized particles, such as a sensitization process, a washing process, and a blocking process.

[0054] The reactive functional group (A1) may contain one or more selected from the group consisting of nucleophilic groups such as carboxyl groups, phenolic hydroxyl groups, amino groups, and thiol groups, and electrophilic groups such as epoxy groups, maleimide groups, acrylic groups, methacrylic groups, and acid anhydride groups. Examples of the acid anhydride groups include maleic anhydride groups and succinic anhydride groups. Among these, the reactive functional group (A1) may contain a carboxyl group.

[0055] The surface modifying polymer 2 also contains a structural unit A2 that includes a salt formed by an acidic functional group (A2) and an organic base. The acidic functional group (A2) constitutes a part of a side chain bonded to the main chain of the surface modification polymer 2. The acidic functional group (A2) may be bonded directly to the main chain of the surface modification polymer 2, or may be bonded, for example, without the intervention of a spacer having 5 or more carbon atoms. When bonded directly to the main chain without the intervention of the spacer, the ionic bond strength of the salt can be appropriately adjusted due to the steric hindrance of the surrounding side chains.

[0056] In the salt of the structural unit A2, the acidic functional group (A2) is H + (proton) is removed to form an anion (conjugate base), and the organic base is H +(proton) is accepted and the structure unit A2 is in a cationic (conjugate acid) state. It is presumed that the salt in the structural unit A2 is in an ionic bond between the anion of the acidic functional group (A2) and the cation of the organic base.

[0057] The acidic functional group (A2) includes, for example, one or more groups selected from the group consisting of a carboxy group, a sulfo group, a phosphate group, and a hydroxyl group. A part or all of the acidic functional group (A2) may be composed of the same group as the reactive functional group (A1), or may be composed of a group different from the reactive functional group (A1). For example, when the acidic functional group (A2) is a carboxyl group, the reactive functional group (A1) may be a carboxyl group, but may also be a different group selected from the above-mentioned groups other than the carboxyl group. When the acidic functional group (A2) and the reactive functional group (A1) contain the same group, at least a part of the other identical groups that do not form a chemical bond with an organic base among the multiple identical groups contained in the surface modification polymer 2 functions as the reactive functional group (A1). However, all of the other identical groups do not have to function as reactive functional groups (A1), and may be functional groups having other functions (functions other than ligand binding and salt formation) such as hydrophilic groups.

[0058] The organic base may include, for example, a nitrogen-containing base and / or a phosphorus-containing base, which may be used alone or in combination of two or more kinds. The nitrogen-containing base is not limited as long as it is a nitrogen-containing compound in which the nitrogen element easily accepts a proton to become a cation, and for example, an organic amine compound is used. Examples of the organic amine compound include aliphatic amines, aliphatic cyclic amines, aromatic amines, and heterocyclic amines. The aliphatic amines, aliphatic cyclic amines, and aromatic amines are preferably tertiary amines. In addition, a part of the group bonded to the nitrogen atom of the organic amine compound may be substituted with a substituent such as a hydroxyl group. The phosphorus-containing base is not limited as long as it is a phosphorus-containing compound in which the phosphorus element easily accepts a proton to become a cation, and for example, an organic phosphorus compound is used. The organic phosphorus may be, for example, a tertiary phosphine. The three groups bonded to the phosphorus atom in the tertiary phosphine are preferably either an aromatic group or a cyclic hydrocarbon group.

[0059] The organic base may include, for example, at least one of the nitrogen-containing bases and phosphorus-containing bases exemplified below. These may be used alone or in combination of two or more.

[0060] [ka]

[0061] Here, an example of a process for producing the polymer-attached particles 10 will be described. The above-mentioned production process includes a step of preparing the above-mentioned core particle 1, and a step of forming the above-mentioned surface-modifying polymer 2 on the surface of the core particle 1. The step of forming a surface modifying polymer 2 on the surface of a core particle 1 includes the steps of: a base introduction step of forming a salt between the acidic functional group (A2) of the surface-modifying polymer 2 and the organic base; It may also include the above-mentioned polymer introduction step of chemically reacting the above-mentioned polymer reactive group of the core particle 1 with a predetermined reactive group (functional group capable of reacting with the polymer reactive group) of the surface modifying polymer 2. Here, the order of the base introduction step and the polymer introduction step is not particularly limited, but the base introduction step may be performed after the polymer introduction step, or the base introduction step may be performed after the polymer introduction step. Note that one or more known treatments such as purification may be included between these steps.

[0062] When the base introduction step is performed after the polymer introduction step, the base introduction step is performed by mixing the above-mentioned nitrogen-containing compound and / or organic amine compound (organic base) with a surface-modified polymer precursor having an acidic functional group (A2) but no organic base to form a salt.

[0063] On the other hand, when the base introduction step is performed after the polymer introduction step, the base introduction step is performed by mixing the above-mentioned organic base with core particles 1 on whose surface a surface-modified polymer precursor having an acidic functional group (A2) but no organic base is formed, to form a salt-containing surface-modified polymer 2. The above-mentioned core particles 1 can be used in the form of a dispersion liquid in which they are dispersed in a dispersion medium such as water.

[0064] The above nitrogen-containing compound and / or organic amine compound (organic base) may be used in the form of a compound, or in the form of a solution containing the compound. The concentration of the organic base in the solution is, for example, 0.1 wt % to 90 wt %, preferably 0.2 wt % to 80 wt %, and more preferably 0.3 wt % to 70 wt %. The pH of the solution containing the organic base is, for example, 4 to 10, preferably 5 to 9, and more preferably 6 to 8. The solution containing an organic base preferably contains a solvent that does not dissolve the core particles 1 but dissolves the surface-modified polymer 2. From the viewpoint of such dissolution selectivity, it is preferable to use an alcohol solvent such as methanol, ethanol, isopropanol, etc. The solution may contain other additives such as a buffer, if necessary.

[0065] The manufacturing process of the polymer-attached particle 10 of this embodiment may, if necessary, include a step of reacting the reactive functional group (A1) of the surface-modifying polymer 2 with a ligand after the step of forming the surface-modifying polymer 2 on the surface of the core particle 1.

[0066] Here, an example of a method for synthesizing the surface modifying polymer 2 will be described. The method for synthesizing the surface-modified polymer 2 can include a polymer precursor production step of producing a surface-modified polymer precursor by polymerizing one or more raw material monomers, and an organic base introduction step of mixing the surface-modified polymer precursor with the above-mentioned organic base to form a salt.

[0067] The raw material monomers used in the polymer precursor production process can be one or more of raw material monomer A containing a diene compound and a diene parent compound, and raw material monomer B containing a functional group and an unsaturated group such as a double bond.

[0068] For the polymer of a diene compound and a parent diene compound, (i) if an anhydride group is contained, the anhydride group may be ring-opened to introduce a reactive functional group (A1), an acidic functional group (A2), or other functional groups (functional functional groups) into the side chain, (ii) if a carboxy group is contained, various functional groups may be introduced into the side chain by a condensation reaction or the like, and (iii) if an unsaturated group such as a double bond is contained, the above-mentioned various functional groups may be introduced into the side chain by an addition reaction or the like. Examples of the other functional groups mentioned above include known functional groups such as various reactive groups, hydrophobic groups, hydrophilic groups (water-soluble groups), and acidic groups. In addition, (i) when an anhydride group is included, the anhydride group may be ring-opened by water, alcohol, or the like, or the anhydride group may be ring-opened by the above-mentioned organic base. By ring-opening the anhydride group by an organic base, an organic base introduction step can be realized. In addition, the functional functional group described above may be introduced into the side chain of the polymer precursor by a condensation reaction or the like as in (ii) above for a functional group such as a carboxyl group formed by ring-opening the anhydride group.

[0069] In synthesizing a polymer precursor of a maleic anhydride-based polymer, for example, a norbornene-based monomer such as norbornene can be used as the diene compound, and an unsaturated carboxylic acid anhydride having a cyclic structure in the molecule such as maleic anhydride can be used as the new diene compound.

[0070] On the other hand, the raw material monomer B may be a raw material monomer B1 having a reactive functional group (A1) and an acidic functional group (A2), or a combination of a raw material monomer B2 having a reactive functional group (A1) and a raw material monomer B2 having an acidic functional group (A2), etc. If necessary, in addition to these, a raw material monomer B3 having a functional group other than the reactive functional group (A1) and the acidic functional group (A2) may be used.

[0071] For the synthesis of the polymer precursor of the (meth)acrylic polymer, for example, (meth)acrylic acid such as acrylic acid, methacrylic acid, (meth)acrylic acid esters such as methyl (meth)acrylate, ethyl (meth)acrylate, propyl (meth)acrylate, butyl (meth)acrylate, isobutyl (meth)acrylate, hexyl (meth)acrylate, and ethylhexyl (meth)acrylate are used. One or more of these (meth)acrylic monomers can be used.

[0072] The polymerization may be, but is not limited to, addition polymerization and / or condensation polymerization. For example, addition polymerization may be carried out by radical polymerization. In addition, the reactive functional group (A1), the acidic functional group (A2), or other functional groups (functional functional groups) may be introduced into the side chains of the obtained polymer precursor by ring-opening reaction, condensation reaction, addition reaction, or the like. A specific example will be described. First, one or more raw material monomers and a polymerization initiator are dissolved in a solvent, and then the solution is polymerized by heating for a predetermined time. The heating temperature can be, for example, 50°C to 80°C. The heating time can be, for example, 1 hour to 20 hours. It is more preferable to remove dissolved oxygen in the solvent by nitrogen bubbling before carrying out the solution polymerization.

[0073] As the polymerization initiator, for example, an azo compound, an organic peroxide, etc. can be used. Specific examples of the azo compound include azobisisobutyronitrile (AIBN), dimethyl 2,2'-azobis(2-methylpropionate), and 1,1'-azobis(cyclohexanecarbonitrile) (ABCN). Examples of organic peroxides include hydrogen peroxide, di-tertiary butyl peroxide (DTBP), benzoyl peroxide (benzoyl peroxide, BPO), and methyl ethyl ketone peroxide (MEKP). As for the polymerization initiator, only one type may be used, or two or more types may be used in combination.

[0074] In addition, a molecular weight regulator or a chain transfer agent can be used as necessary. Examples of the chain transfer agent include thiol compounds such as dodecyl mercaptan, mercaptoethanol, and 4,4-bis(trifluoromethyl)-4-hydroxy-1-mercaptobutane. These chain transfer agents may be used alone or in combination of two or more.

[0075] As the solvent used in the polymerization reaction, for example, one or more of esters such as methyl ethyl ketone (MEK), propylene glycol monomethyl ether, diethyl ether, tetrahydrofuran (THF), toluene, ethyl acetate, and butyl acetate can be used. As the polymerization initiator, one or more of azo compounds and organic peroxides can be used. As the azo compound, for example, azobisisobutyronitrile (AIBN), dimethyl 2,2'-azobis(2-methylpropionate), and 1,1'-azobis(cyclohexanecarbonitrile) (ABCN) can be used. As the organic peroxide, for example, hydrogen peroxide, ditertiary butyl peroxide (DTBP), benzoyl peroxide (benzoyl peroxide (BPO)), and methyl ethyl ketone peroxide (MEKP) can be used.

[0076] The reaction liquid containing the (co)polymer thus obtained is added to an alcohol or ether such as hexane or methanol to precipitate the polymer. The polymer is then filtered, washed with an alcohol such as hexane or methanol, and then dried. In this manner, the polymer can be synthesized. This makes it possible to remove low molecular weight components such as residual monomers, oligomers, and polymerization initiators.

[0077] The target substance detection reagent of this embodiment contains a particle group of the polymer-attached particles 10 and a dispersion medium. The concentration (wt %) of the polymer-attached particles 10 in the dispersion medium can be appropriately set. As the dispersion medium, for example, the above-mentioned aqueous solvents are preferably used. The aqueous solvent may contain, within the scope of the invention, a third substance such as a buffer, a preservative (e.g., sodium azide), a blocking agent such as a protein (albumin), a sensitizer such as a water-soluble polymer (e.g., sugar, polyethylene glycol, dextran), a salt (e.g., sodium chloride, amino acid), a surfactant, etc. These may be used alone or in combination of two or more kinds. The polymer-attached particles 10 in the reagent may be subjected to a blocking treatment using a blocking agent such as bovine serum albumin (BSA).

[0078] (kit) The target substance detection reagent of this embodiment may be in the form of a kit from the viewpoints of storage, transportation, distribution, etc. The form of the kit is not particularly limited as long as it is a form that enables the measurement method of the present invention. The target substance detection kit of the present embodiment includes a reagent container containing the above-mentioned target substance detection reagent.

[0079] The kit can take various forms, such as the following: The kit of the first type includes a particle group of polymer-attached particles 10 and a first reagent container containing a dispersion medium. The kit of the second embodiment includes a second reagent container A containing a particle group of the polymer-attached particles 10, and a second reagent container B containing a dispersion medium. The first reagent container of the kit of the first embodiment and the second reagent container A and second reagent container B of the kit of the second embodiment may each contain at least one or more of the third substances exemplified above. Furthermore, each of the kits of the first and second embodiments may further include a third reagent container containing at least one of the third substances. In addition, each of the kits of the first and second forms may include, in addition to the above-mentioned reagent container, a fourth reagent container containing one or more of a positive control, a negative control, a diluent, a washing solution, instructions for use, etc. As the media for the positive and negative controls, serum, physiological saline, solvents, etc. that do not contain a measurable target substance are used.

[0080] (Method for detecting target substances) The method for detecting a target substance of the present embodiment includes a contacting step of mixing a target substance with a target substance detection reagent. In the contact step, a sample containing the target substance and the polymer-attached particles 10 having the ligand 3 are added to the same reaction vessel and allowed to coexist, allowing the ligand 3 bound to the polymer-attached particles 10 to come into contact with the target substance. The sample containing the standard substance and the target substance reagent containing the polymer-attached particles 10 may be added in any order. Furthermore, the target substance and the polymer-attached particles 10 may be mixed at a pH of about 3.0 or more and about 11.0 or less, and the temperature of the mixture may be about 20° C. or more and 50° C. or less.

[0081] The target substance is contacted with the ligand 3 and reacted with each other, so that the substance to be measured in the sample reacts with the antibody supported on the latex particles, forming a complex between the target substance, the ligand 3, and the polymer-attached particles 10, and causing aggregation of the polymer-attached particles 10 due to the formation of the complex.

[0082] The method for detecting a target substance may include, after the contact step, a detection step of optically measuring the agglutination of the polymer-attached particles 10. Examples of the method for optically measuring the agglutination include a method of measuring absorbance, scattered light intensity, or transmitted light intensity with an optical instrument. The wavelength for measuring absorbance is usually 340 nm to 1000 nm, and preferably 500 nm to 900 nm. The time for measuring the agglutination reaction can be measured based on the rate of change per unit time during which the agglutination reaction is occurring, or the amount of change per unit time. For example, when measuring absorbance, the time can be measured based on the rate of change in absorbance per unit time from 30 seconds to 5 minutes after the start of the agglutination reaction, or the amount of change in absorbance per unit time.

[0083] Although the embodiments of the present invention have been described above, these are merely examples of the present invention, and various configurations other than those described above can be adopted. Furthermore, the present invention is not limited to the above-described embodiments, and modifications and improvements within the scope of the present invention are included in the present invention. EXAMPLES

[0084] The present invention will be described in detail below with reference to examples, but the present invention is not limited to the descriptions of these examples. <Synthesis of surface-modifying polymer> (Maleic anhydride polymer) Norbornene and maleic anhydride were reacted by radical polymerization at a predetermined ratio using an azo compound (polymerization initiator), to obtain polymer precursor A. Subsequently, various functional monomers having the following functional groups 1 to 4 were subjected to a ring-opening reaction in the presence of an organic base (triethylamine) at a predetermined ratio, and introduced into the side chains (ring-opened maleic anhydride groups) of each polymer precursor A (organic base introduction treatment), followed by reprecipitation treatment with hexane or diethyl ether to obtain maleic anhydride-based polymers (polymers A1 to A10 shown in Table 1).

[0085] [Table 1]

[0086] [ka] [ka]

[0087] ((Meth)acrylic polymer) Butyl methacrylate and methacrylic acid were reacted by radical polymerization at a predetermined ratio using an azo compound (polymerization initiator). After polymerization, the reaction solution was reprecipitated with water or diethyl ether to obtain polymer precursor B. Next, each polymer precursor B and an organic base (triethylamine or diisopropylethylamine) were dissolved in ethanol and stirred at room temperature for 5 hours (organic base introduction treatment), and then reprecipitation treatment was carried out with hexane to obtain (meth)acrylic polymers (polymers B1 to B4 shown in Table 2). In addition, (meth)acrylic polymers (polymers B5 to B7 shown in Table 2) were obtained in the same manner as for polymer B1, except that the organic base introduction treatment was not carried out.

[0088] [Table 2]

[0089] [ka]

[0090] The weight average molecular weight (Mw) of each of the maleic anhydride polymers and (meth)acrylic polymers obtained above was calculated based on a calibration curve of a standard PEG sample using GPC (gel permeation chromatography) under the following measurement conditions. The results are shown in Table 1 or Table 2.

[0091] The maleic anhydride polymer obtained above was subjected to the following measurement conditions:13 The C-NMR spectrum was measured. The (meth)acrylic polymer obtained above was also measured under the following measurement conditions. 1 H-NMR spectrum was measured. Based on the obtained NMR spectrum results, the composition ratio (content of structural units having functional groups) in each polymer was calculated. The results are shown in Table 1 or Table 2. Table 1 also shows the ring-opening rate (%) of maleic anhydride groups. It was also found that the maleic anhydride polymer contains a structural unit having each functional group represented by the above general formula (A). R in the general formula (A) is represented by one or two of the functional groups 1 to 4 exemplified above. On the other hand, it has been found that the (meth)acrylic polymer contains structural units having each functional group represented by the above general formula (B).

[0092] The above polymer precursor A and the above polymers A1 to A10 were each measured under the following measurement conditions. 13 The C-NMR spectrum was measured. From the results of the NMR spectrum, a peak shift occurred between the polymer precursor A and the corresponding polymers A1 to A10, so it was confirmed that a salt was formed by an ionic bond between the carboxy group in the maleic anhydride polymer (surface-modified polymer) obtained above and an organic base. Similarly, for each of the polymer precursor B and the polymers B1 to B7, 1 As a result of measuring the H-NMR spectrum, a peak shift occurred between the polymer precursor B and the corresponding polymers B1 to B4, so it was confirmed that a salt was formed by an ionic bond between the carboxy group in the (meth)acrylic polymer (surface-modified polymer) obtained above and an organic base. Here, in the above general formula (A) and general formula (B), it is presumed that a carboxy group and / or two adjacent or nearby carboxy groups are ionic-bonded to an organic base.

[0093] (NMR measurement conditions) NMR measurements were performed using a JEOL ECA500 with deuterated dimethyl sulfoxide or deuterated ethanol as the solvent. (GPC measurement conditions) For the GPC measurement, one Tosoh TSKgel SuperAWM-H, one TSKgel SuperAW2500, and one TSKgel guardcolumn SuperAW-H were used, and the developing solvent was 70% methanol / 30% HO (with 10 mM LiBr added), with a column temperature of 40°C and a flow rate of 0.6 ml / min.

[0094] <Preparation of particles with polymer> [Examples 1 to 10] Diamine was mixed into the following latex liquid A, and the carboxyl groups of the polystyrene latex particles were reacted with the diamine to introduce primary amino groups, followed by purification (amino treatment). Next, the surface-modifying polymers (polymers A1 to A10) shown in Table 3 were mixed into a solution containing polystyrene latex particles having primary amino groups to react the primary amino groups with maleic anhydride groups, and the mixture was purified to obtain a dispersion containing core particles with the surface-modifying polymer introduced onto their surfaces (polymer introduction treatment).

[0095] [Examples 11 to 17] The surface-modifying polymers (polymers B1 to B7) shown in Table 3 were mixed, and the primary amino groups and carboxy groups were reacted using the condensation agent shown below. Except for this, amino treatment and polymer introduction treatment were carried out in the same manner as in Example 1, to obtain a dispersion containing core particles with a surface-modifying polymer introduced onto their surfaces.

[0096] [Comparative Examples 1 to 3] A dispersion liquid containing latex particles (latex liquid A below) was used.

[0097] Latex solution A: Carboxyl-modified polystyrene latex particles (manufactured by JSR, product name: IMMUNTEX, average particle size: 351 nm, solid content: 10%) Condensation agent: Carbodiimide crosslinking agent (EDC, 1-ethyl-3-(3-dimethylaminopropyl)carbodiimide hydrochloride, also known as WSC)

[0098] [Table 3]

[0099] In Tables 1 to 3, TEA stands for triethylamine, and DIEA stands for diisopropylethylamine.

[0100] The polymer-attached particles obtained above were evaluated for the following items.

[0101] <Production of Sensitized Particle Dispersion> (Sensitization treatment) 600 μL of the dispersion liquid (0.4% w / vol) of polymer-attached particles of Examples 1 to 17 containing the above-mentioned condensing agent or the dispersion liquid (0.4% w / vol) containing latex particles of Comparative Examples 1 to 3 described above was mixed with 600 μL of the antibody A solution (0.27 mg / mL) described below, and the mixture was shaken and stirred at 20°C for 180 minutes to obtain a mixture. Antibody A solution: Ferritin antibody (Mikuri Immuno Research Institute, Ferritin clone No. 14), 10 mM MES (pH 6.5)

[0102] (Cleaning process) The resulting mixture was centrifuged at 10,000 rpm for 15 minutes at 10° C. using a centrifuge (rotor: R15A (HI antibody ACH)). The supernatant was decanted, and 3.5 mL of the following HEPES buffer was added to the resulting sediment, which was then dispersed by sonication. Subsequently, the mixture was centrifuged at 10,000 rpm for 15 minutes at 10° C. using the above centrifuge. The supernatant was decanted, and 3.5 mL of the following HEPES buffer was added to the resulting sediment, which was then dispersed by sonication to obtain a suspension. HEPES buffer: 0.1% BSA, 10 mM HEPES (4-(2-hydroxyethyl)-1-piperazineethanesulfonic acid, pH 7.2), 0.1% Tween 20, 0.05% NaN3

[0103] (Blocking process) To the resulting suspension, 3.5 mL of the blocking solution described below was added, thoroughly dispersed, and then stirred for 1 hour at 37° C. Then, the mixture was centrifuged at 10,000 rpm and 10° C. for 15 minutes using the above centrifuge to obtain ligand-sensitized particles. Blocking solution: Bovine serum albumin (BSA) solution (1% BSA, 20 mM MES buffer (pH 6.0), 0.05% NaN3)

[0104] (Reagent processing) The following components were mixed in a given mixing ratio and uniformly dispersed by ultrasonic treatment (dispersion treatment) to prepare a reagent (sensitized particle dispersion) with a solid content of 0.1%. The ligand-sensitized particles obtained above · HEPES buffer containing 0.5% bovine serum albumin (BSA) 100mM NaCl ·0.09%NaN3 ·100mM HEPES buffer (pH7.0)

[0105] <Absorbance> Using an automatic analyzer TBA-120FR (manufactured by Canon Medical Systems Inc.), the absorbance at a wavelength of 700 nm was measured for each of the reagents of each Example and Comparative Example, the measurement reagents listed below, and the target substance (ferritin antigen solution) held at 10°C. Next, 20 μL of each of the reagents from each Example and Comparative Example was mixed with 80 μL of the measurement reagent described below and 4 μL of the target substance (antigen amount 0 ng / mL or 1,000 ng / mL), and the mixture was stirred uniformly and kept at 37°C. The absorbance at a wavelength of 700 nm was measured immediately after adding the measurement reagent and after 5 minutes had passed. The absorbance of each reagent when the antigen amount was 0 ng / mL and 1,000 ng / mL was calculated by subtracting the absorbance immediately after adding the measurement reagent from the absorbance after 5 minutes. As an index of sensitivity, the difference in absorbance (ΔAbs) between the presence and absence of added target substance was calculated by subtracting the absorbance at a wavelength of 700 nm when the antigen amount was 0 ng / mL from the absorbance at a wavelength of 700 nm when the antigen amount was 1,000 ng / mL.

[0106] (Measuring Reagents) The following components were mixed in a given ratio to prepare a measuring reagent. 0.1% Tween20 Sensitizers shown in Table 3 Polyethylene glycol (PEG) (5000~50000) MPC-containing polymer 1: A polymer having a phosphorylcholine group, in which the ratio of structural units having a phosphorylcholine group contained in all structural units (MPC content) is 37 mol%. MPC-containing polymer 2: A polymer having a phosphorylcholine group, in which the ratio of structural units having a phosphorylcholine group among all structural units (MPC content) is 100 mol %. However, the above MPC-containing polymers 1 and 2 were synthesized as follows. 2-Methacryloyloxyethyl phosphorylcholine (MPC) and polymethyl acrylate (PMA) were reacted by radical polymerization at a predetermined ratio using an azo compound (polymerization initiator). After polymerization, the reaction solution was reprecipitated with acetone to obtain the above MPC-containing polymers 1 and 2. ·1% bovine serum albumin (BSA) in HEPES buffer 150mM NaCl ·0.09%NaN3 ·100mM HEPES buffer (pH7.6)

[0107] The target substance detection reagents containing the polymer-attached particles of Examples 1 to 17 and the polymer having a phosphorylcholine group showed lower absorbance at a wavelength of 700 nm when the antigen amount was 0 ng / mL, i.e., the absorbance when no target substance (antigen) was added, compared to Comparative Examples 1 to 3, indicating that they have excellent dispersibility. It was found that such target substance detection reagents of Examples 1 to 17 can be suitably used as sensitized particle dispersions (reagents) for use in immune agglutination methods. [Explanation of symbols]

[0108] 1. Core Particle 2. Surface Modification Polymers 3. Ligand 10. Polymer-attached particles

Claims

1. A target substance detection reagent comprising a polymer-attached particle, a sensitizer, and a dispersion medium, The polymer-attached particle includes a core particle and a surface-modifying polymer formed on at least a portion of the surface of the core particle, The surface-modifying polymer includes a structural unit A1 including a reactive functional group (A1) capable of binding to a ligand having specific binding ability to a target substance, The sensitizer is a target substance detection reagent that contains a polymer having a phosphorylcholine group.

2. The target substance detection reagent according to claim 1 , A target substance detection reagent, wherein a ratio of structural units having a phosphorylcholine group contained in all structural units of the polymer having a phosphorylcholine group is 10 mol % or more and 100 mol % or less.

3. The target substance detection reagent according to claim 1 , A target substance detection reagent, wherein the surface-modified polymer in the polymer-attached particle contains a structural unit A2 containing a salt formed by an acidic functional group (A2) and an organic base.

4. The target substance detection reagent according to claim 3, A target substance detection reagent, wherein the acidic functional group (A2) includes one or more groups selected from the group consisting of a carboxy group, a sulfo group, a phosphate group, and a hydroxyl group.

5. The target substance detection reagent according to claim 1 , A target substance detection reagent, wherein the reactive functional group (A1) includes one or more selected from the group consisting of a carboxy group, a phenolic hydroxy group, an amino group, a thiol group, an epoxy group, a maleimide group, an acryl group, a methacryl group, a (meth)acryl group, and an acid anhydride group.

6. The target substance detection reagent according to claim 3, A target substance detection reagent, wherein the organic base comprises a nitrogen-containing base and / or a phosphorus-containing base.

7. The target substance detection reagent according to claim 1 , A target substance detection reagent, wherein the surface-modifying polymer has a weight-average molecular weight of 1,000 or more and 10,000,000 or less.

8. The target substance detection reagent according to claim 1 , A target substance detection reagent, wherein the core particle is an organic particle or an inorganic particle.

9. The target substance detection reagent according to claim 1 , The surface-modifying polymer comprises the ligand bound to at least a portion of the reactive functional groups (A1).

10. The target substance detection reagent according to claim 1 , A target substance detection reagent, wherein the ligand is any one of an antibody, an antigen, a protein, and a nucleic acid.

11. The target substance detection reagent according to claim 1 , A target substance detection reagent used in agglutination methods.

12. A target substance detection kit comprising a reagent container containing the target substance detection reagent according to any one of claims 1 to 11.

13. A method for detecting a target substance, comprising the step of mixing a target substance with the target substance detection reagent according to any one of claims 1 to 11.

Citation Information

Patent Citations

  • Measurement method using latex immunoagglutination method, reagent, and kit

    JP2021162593A