Inkjet ink

The inkjet ink with a two-component organic solvent system addresses the issue of uneven layer thickness in electronic components by maintaining uniform dispersion and preventing solvent flow during drying, enhancing smoothness and reducing short circuit risks.

JP2024143557APending Publication Date: 2024-10-11NORITAKE MACHINE TECHNO CO LTD

Patent Information

Application Number
JP2023056295
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-30
Publication Date
2024-10-11

AI Technical Summary

Technical Problem

Inkjet printing methods struggle to achieve high smoothness in electrode and insulating layers of multilayer electronic components like MLCCs, leading to potential short circuits due to the coffee ring phenomenon during drying, which results in uneven thickness and poor layer uniformity.

Method used

The use of an inkjet ink comprising inorganic powder, binder resin, dispersant, and a two-component organic solvent system with specific vapor pressures and surface tensions to maintain uniform dispersion and prevent solvent flow during drying, ensuring smoothness of printed films.

Benefits of technology

The inkjet ink effectively suppresses the coffee ring phenomenon, resulting in improved smoothness and uniformity of printed films, enabling thinner layers and reducing the risk of short circuits in electronic components.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024143557000005
    Figure 2024143557000005
  • Figure 2024143557000006
    Figure 2024143557000006
  • Figure 2024143557000007
    Figure 2024143557000007
Patent Text Reader

Abstract

To provide technique for improving smoothness of a printed film.SOLUTION: Inkjet ink is used for manufacturing an electronic component. The inkjet ink includes inorganic powder, binder resin, a dispersion agent, and an organic solvent. The organic solvent includes a first organic solvent having a vapor pressure P1 at 20°C of 100 Pa or less and surface tension of 22 mN / m or more and 31 mN / m or less, and a second organic solvent having a vapor pressure P2 at 20°C which is smaller than the vapor pressure P1 and is 4 Pa or less. When the total organic solvent is 100 vol.%, a volume ratio of the second organic solvent is 30 vol.% or less. A ratio (Vs2 / Vp) of a volume ratio Vs2 of the second organic solvent when the total inkjet ink is 100 vol.% to a volume ratio Vp of the inorganic powder when the total inkjet ink is 100 vol.% is 1.5 or more.SELECTED DRAWING: None
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to ink-jet inks. [Background technology]

[0002] Inkjet printing has been used as one of the printing methods for drawing images such as patterns and characters on a printing target. Since inkjet printing can print highly accurate images at low cost and on demand, and causes little damage to the printing target, its application to various fields is being considered. In recent years, the use of inkjet printing has been considered for forming conductive circuit patterns (wiring, electrodes, etc.) in the manufacture of electronic components.

[0003] In the manufacture of such electronic components, for example, a conductive inkjet ink may be used in which inorganic powders containing metal particles or the like are added as a conductive material. As an example of such a conductive inkjet ink, Patent Document 1 discloses an ink containing nanometal powders such as silver or a silver-copper alloy. Patent Document 2 discloses an ink containing metal oxide particles such as silver oxide, copper oxide, palladium oxide, nickel oxide, lead oxide, and cobalt oxide. In general, in order to perform inkjet printing appropriately, it is required that the conductive ink has a low viscosity and that the concentration of inorganic powder is high. In the above-mentioned Patent Documents 1 and 2, techniques for obtaining these inkjet suitabilities are proposed.

[0004] Furthermore, in conductive inkjet inks, it is also required to stably disperse inorganic powders from the viewpoint of ensuring ejection properties during printing and conductivity after printing. For example, Patent Document 3 discloses a technique of adding a first dispersant having only either an acidic adsorption group or a basic adsorption group, and a second dispersant having both an acidic adsorption group and a basic adsorption group, in order to increase the dispersibility of solid fine particles (inorganic powder) having a mixture of acid sites and basic sites on the surface.

[0005] Patent Document 4 discloses a spacer particle dispersion liquid that contains spacer particles and a solvent mainly composed of an organic solvent and is used to arrange the spacer particles at any position on a substrate using an inkjet device. The spacer particle dispersion liquid is characterized by having a surface tension of 30 to 65 mN / m. The publication states that, with this configuration, it is possible to provide a spacer particle dispersion liquid that can selectively arrange spacer particles at any position on a substrate without the droplets of the spacer particle dispersion liquid discharged onto a substrate of a liquid crystal display device using an inkjet device spreading, and a liquid crystal display device using the spacer dispersion liquid. [Prior art documents] [Patent documents]

[0006] [Patent Document 1] Special Publication No. 2008-513565 [Patent Document 2] JP 2012-216425 A [Patent Document 3] JP 2015-62871 A [Patent Document 4] JP 2008-111985 A Summary of the Invention [Problem to be solved by the invention]

[0007] Incidentally, among electronic components, there are laminated products (e.g., multilayer ceramic capacitors (MLCCs) and the like) that require high smoothness in the electrode layer and insulating layer. In such laminated electronic components, ferroelectric ceramic materials such as barium titanate are used for the insulating layer, and metal materials such as palladium and nickel are used for the electrode layer. In the manufacturing process of the electrode layer and insulating layer, first, a ceramic layer is formed on a plastic film such as a PET film that has been treated to have a smooth surface, using a ceramic slurry by a doctor blade method, a screen printing method, or the like. A metal layer is formed on top of that by, for example, a screen printing method, using a metal slurry (paste). Next, all the printed matter is peeled off from the PET film and laminated, and then pressed and fired to form a laminated electronic component.

[0008] The inventors are considering forming laminated components by alternately inkjet printing the insulating layer patterns and electrode layer patterns of electronic components that require high smoothness using a ceramic inkjet ink mainly composed of barium titanate particles and a conductive inkjet ink mainly composed of nickel particles. The purpose is to make both the electrode layer and the insulating layer thinner, which has been difficult to achieve with the combination of green sheets and conductive pastes, as components become smaller and larger in capacity in MLCC manufacturing.

[0009] In order to achieve sufficient thinning using ceramic inkjet ink and conductive inkjet ink, it is essential to smooth the surface of each layer to prevent shorting between the upper and lower metal layers. This is required not only for conductive inkjet ink, but also for ceramic inkjet ink. By smoothing both the ceramic layer and the metal layer, it is possible to miniaturize to a level that was not possible with conventional screen printing methods, and to achieve high productivity by producing without peeling off the PET film.

[0010] However, in the case of inkjet inks mainly made of barium titanate and inkjet inks mainly made of nickel, accumulation on the outer periphery of the insulating layer and electrode layer (the so-called coffee ring phenomenon) is likely to occur when the organic solvent volatilizes due to heating and drying. If this causes the thickness of the outer periphery to become larger than the thickness of the inner periphery, the layer will not be sufficiently smoothed, and there is a possibility that a short circuit will occur in the metal layer.

[0011] When the doctor blade method or screen printing method is used, the viscosity of the ceramic slurry or metal paste can be increased, and the fluidity during heating and drying can be reduced in advance. This is thought to prevent the thickness from increasing at the periphery. In addition, in these film formation and printing methods, from the viewpoint of keeping the clearance (gap) between the substrate and the film formation surface constant, it is theoretically easy to obtain a smooth surface. However, when using a high-viscosity paste in the inkjet method, it is difficult to form a smooth inkjet ink printing layer because the inkjet method that can handle high viscosity is not common in industrial applications and the leveling ability between the ejected high-viscosity droplets is insufficient. Therefore, there have been no ceramic inkjet inks or metal inkjet inks that can prevent the thickness from increasing at the periphery and obtain a smooth printing film.

[0012] The present invention has been made in consideration of the circumstance that it is difficult to suppress accumulation on the outer periphery of a layer pattern when meeting the demand for achieving high smoothness in an inkjet method, and its main objective is to provide a technology for suppressing accumulation on the outer periphery of a layer pattern in an inkjet ink during heating and drying, thereby enhancing the smoothness of a printed film. [Means for solving the problem]

[0013] The inkjet ink disclosed herein is an inkjet ink used in the manufacture of electronic components. The inkjet ink contains an inorganic powder, a binder resin, a dispersant, and an organic solvent. The organic solvent has a vapor pressure P1 A first organic solvent having a vapor pressure P 2 is the vapor pressure P 1 and a second organic solvent having a viscosity smaller than 4 Pa ​​or less. When the total volume of the organic solvents is 100 volume %, the volume ratio of the second organic solvent is 30 volume % or less. The ratio (Vs2 / Vp) of the volume ratio Vs2 of the second organic solvent when the total volume of the inkjet ink is 100 volume % to the volume ratio Vp of the inorganic powder when the total volume of the inkjet ink is 100 volume % is 1.5 or more. With this configuration, it is possible to improve the smoothness of the printed film formed by inkjet printing.

[0014] In a preferred embodiment of the ink-jet ink, the inorganic powder has an average particle size of 20 nm to 200 nm, which can further increase the smoothness of the printed film.

[0015] In another preferred embodiment of the inkjet ink, the inorganic powder includes a ceramic powder or a metal powder. This configuration can improve the smoothness of the ceramic printed film or the metal printed film. Preferably, the inorganic powder includes a barium titanate powder or a nickel powder.

[0016] In another preferred embodiment of the inkjet ink, the first organic solvent is composed of at least one of ethers, esters, and alcohols. The second organic solvent is composed of at least one of ethers, esters, and hydrocarbon compounds. With this configuration, the effects of the technology disclosed herein are appropriately achieved.

[0017] In another preferred embodiment of the inkjet ink, the first organic solvent is composed of at least one of glycol ether, glycol ether acetate, and aliphatic alcohol, and the second organic solvent is composed of at least one of glycol ether, glycol ether acetate, aromatic ester, and linear alkane having 20 or less carbon atoms. With this configuration, the effects of the technology disclosed herein are appropriately achieved.

[0018] In another preferred embodiment of the inkjet ink, the ink contains at least 10% by volume of the second organic solvent relative to the total volume of the organic solvent, whereby the effects of the technology disclosed herein are appropriately achieved. [Brief description of the drawings]

[0019] [Figure 1] FIG. 1 is a cross-sectional view of an agitator / mill 100. [Diagram 2] FIG. 2 is an overall view of the inkjet device 1. As shown in FIG. [Diagram 3] FIG. 3 is a cross-sectional view of the ink-jet head 10. As shown in FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0020] Hereinafter, an embodiment of the technology disclosed herein will be described. Note that matters other than those specifically mentioned in this specification and necessary for implementing the technology disclosed herein can be understood as design matters for a person skilled in the art based on the conventional technology in the field. The technology disclosed herein can be implemented based on the contents disclosed in this specification and the technical common sense in the field. In this specification, the notation "P to Q" indicating a numerical range includes "P or more and Q or less", "more than P and less than Q", "more than P and Q or less", and "P or more and less than Q".

[0021] <Inkjet ink> The inkjet ink (hereinafter also simply referred to as "ink") disclosed herein may contain, for example, (A) an inorganic powder, (B) a binder resin, (C) a dispersant, and (D) an organic solvent. In the ink, for example, the inorganic powder is dispersed in an organic vehicle component (a mixture of a binder resin and an organic solvent). Each component contained in the ink disclosed herein will be described below.

[0022] (A) Inorganic powder The inorganic powder is a material that constitutes the printed film on the substrate. Here, the "printed film" is a film-like substance (dried film) obtained by applying an ink to a substrate and drying it, and is an unfired body. The inorganic powder is also a material that constitutes a fired body of the printed film (hereinafter also referred to as a "fired film") (for example, an electrode, etc.) obtained by firing such a printed film. In the ink disclosed here, the inorganic powder may contain a ceramic powder or a metal powder as a main component. Herein, "R contains S as a main component" means that, when the entire R (for example, the entire inorganic powder) is taken as 100 mass%, the content ratio of S (for example, ceramic powder or metal powder) is, for example, 50 mass% or more, preferably 70 mass% or more, more preferably 80 mass% or more, even more preferably 90 mass% or more, and particularly preferably 95 mass% or more (the closer to 100 mass%, the better).

[0023] The ceramic powder is composed of, for example, ceramic particles. The ceramic particles may contain, in addition to the ceramic that constitutes the ceramic particles, inevitable impurities that may be mixed in during the production process of the ceramic particles. The ceramic powder may be composed of one type of ceramic powder, or may be composed of two or more types of ceramic powder.

[0024] The type of ceramic powder is not particularly limited, as it may be appropriately set depending on the function to be imparted to the fired film formed using the ink disclosed herein. The ceramic powder may be, for example, a ceramic powder that functions as a dielectric. This allows a dielectric ceramic layer (for example, a dielectric layer of a multilayer ceramic capacitor (MLCC)) to be formed on the substrate. Examples of ceramics that constitute the ceramic powder include ABOs such as barium titanate, strontium titanate, calcium titanate, magnesium titanate, bismuth titanate, zirconium titanate, zinc titanate, barium magnesium niobate, calcium zirconate, and barium zirconate titanate. 3 Metal oxides having a perovskite structure represented by the formula: titanium dioxide (rutile), titanium pentoxide, hafnium oxide, zirconium oxide, aluminum oxide, forsterite, niobium oxide, barium neodymium titanate, rare earth element oxides, etc. Among them, as the ceramic, any of barium titanate, strontium titanate, calcium zirconate, and barium zirconate titanate can be preferably used.

[0025] The metal powder is composed of, for example, metal particles. In addition to the metal that constitutes the metal particles, the metal particles may contain inevitable impurities that may be mixed in during the production process of the metal particles. The metal powder may be composed of one type of metal powder, or may be composed of two or more types of metal powder.

[0026] Metal powders are materials used mainly to form conductors (including conductor films) with high electrical conductivity (hereinafter also simply referred to as "conductivity") such as electrodes, conductor wires, and conductive films in electronic elements, for example. For this reason, various metal powders having the desired electrical conductivity can be used without any particular limitation. Examples of metals constituting the metal powder include simple metals such as nickel (Ni), palladium (Pd), platinum (Pt), gold (Au), silver (Ag), copper (Cu), ruthenium (Ru), rhodium (Rh), osmium (Os), iridium (Ir), aluminum (Al), and tungsten (W); alloys containing these metals; and the like. Among these, nickel (Ni) can be preferably used as the metal from the viewpoints of chemical stability, safety, and the like.

[0027] The particle size of the inorganic powder in the ink is one of the factors that affect, for example, the ejection properties, the stability over time, and the smoothness of the printed film. For example, from the viewpoint of suppressing the decrease in the ejection properties of the inkjet device due to clogging of the ejection port of the inkjet device with the inorganic powder, the average particle size of the inorganic powder is, for example, 500 nm or less, preferably 450 nm or less, more preferably 400 nm or less, and even more preferably 350 nm or less. In addition, from the viewpoint of improving the smoothness of the printed film, the average particle size of the inorganic powder is preferably 320 nm or less, more preferably 300 nm or less, even more preferably 250 nm or less, and particularly preferably 200 nm or less. On the other hand, from the viewpoint of suppressing the aggregation of particles and suppressing the decrease in the stability over time of the ink, the average particle size of the inorganic powder is, for example, 5 nm or more, preferably 10 nm or more, and more preferably 20 nm or more. In this specification, the "average particle size" refers to the average particle size based on the dynamic light scattering (DLS) method. The average particle size based on the DLS method is measured in accordance with JIS Z 8828:2013.

[0028] The volume ratio of the inorganic powder in the ink is not particularly limited and can be appropriately set according to the printing purpose. For example, as the volume ratio of the inorganic powder in the ink increases, a printing layer of suitable thickness can be formed with fewer printing times. From this viewpoint, when the entire ink is taken as 100 volume%, the volume ratio of the inorganic powder is approximately 0.1 volume% or more, preferably 0.5 volume% or more, and more preferably 1 volume% or more. On the other hand, as the volume ratio of the inorganic powder decreases, the stability over time, ejection property, etc. tend to improve. From this viewpoint, when the entire ink is taken as 100 volume%, the content of the inorganic powder is approximately 20 volume% or less, preferably 15 volume% or less, and more preferably 10 volume% or less.

[0029] The content of the inorganic powder in the ink can be appropriately set according to, for example, the desired thickness of the printed film. Here, when the entire ink is taken as 100% by mass, the content of the inorganic powder is preferably about 1% by mass or more, preferably 3% by mass or more, more preferably 5% by mass or more, and particularly preferably 10% by mass or more. On the other hand, when the entire ink is taken as 100% by mass, the content of the inorganic powder is, for example, 50% by mass or less, preferably 40% by mass or less, more preferably 30% by mass or less, and particularly preferably 20% by mass or less. In one embodiment of the ink disclosed herein, when the entire ink is taken as 100% by mass, the content of the inorganic powder is preferably about 5% by mass to 30% by mass, and preferably 10% by mass to 20% by mass.

[0030] (B) Binder resin The binder resin is a component that fixes the inorganic powder on the substrate after the ink is inkjet printed on the substrate. The ink inkjet printed on the substrate is, for example, heated and dried on the substrate, and then baked. Therefore, it is preferable that the binder resin is one that completely disappears (burns out) during the baking process. For example, polyvinyl acetal resin, acrylic resin, etc. are preferably used as the binder resin.

[0031] The ink disclosed herein preferably contains a polyacetal resin as a binder resin. The polyvinyl acetal resin is, for example, a resin produced by acetalizing a polyvinyl alcohol resin with an aldehyde. In addition to the above-mentioned function of fixing an inorganic powder to a substrate, the polyvinyl acetal resin has a function of dispersing in an organic solvent and assisting the effect of the dispersant in suppressing the precipitation of the inorganic powder. Furthermore, in the polyvinyl acetal resin, for example, by adjusting the content of hydroxyl groups contained in the resin, a suitable configuration for suppressing the occurrence of sheet attack can be realized. For this reason, the polyacetal resin is suitable as a binder resin for the ink disclosed herein. Suitable examples of the polyvinyl acetal resin include, for example, polyvinyl butyral resin and polyvinyl formal resin.

[0032] The weight average molecular weight of the binder resin can be appropriately set as long as it does not impair the effects of the technology disclosed herein. For example, from the viewpoint of appropriately suppressing the precipitation of the inorganic powder, the weight average molecular weight of the binder resin is, for example, 0.5×10 4 It is better to use a value of 1.0×10 or more. 4 More than 1.5×10 is preferable. 4 More preferably, 2.0×10 4 On the other hand, from the viewpoint of maintaining the viscosity of the ink at an appropriate level and suppressing a decrease in the ejection performance, the weight average molecular weight of the binder resin is, for example, 10×10 4 It is better to use 7.5 x 10 or less. 4 Less than 5.0×10 is preferable. 4 Less than or equal to 4.5×10 is preferable. 4The above is more preferable. For example, the weight-average molecular weight of the binder resin and the dispersant is measured by gel permeation chromatography (GPC) and converted using a standard polystyrene calibration curve. For example, a GPC device (HLC-8320) manufactured by Tosoh Corporation may be used for such measurement. Alternatively, nominal values ​​of the resin binder and the dispersant manufacturers, or values ​​calculated based on the chemical formula may be used.

[0033] The glass transition temperature of the binder resin can be appropriately set as long as it does not impair the effect of the technology disclosed herein. For example, from the viewpoint of forming a dry film with excellent fixability, the glass transition temperature of the binder resin is preferably 40° C. or higher, more preferably 50° C. or higher, and even more preferably 60° C. or higher. The glass transition temperature is, for example, 100° C. or lower, preferably 90° C. or lower, and more preferably 80° C. or lower. In this specification, the term "glass transition point" refers to the glass transition temperature (Tg) based on differential scanning calorimetry (DSC). Alternatively, a nominal value of a manufacturer or the like may be adopted.

[0034] The volume percentage of the binder resin in the ink can be set as appropriate as long as it does not impair the effects of the technology disclosed herein. For example, when the total volume of the ink is 100%, the volume percentage of the binder resin is approximately 0.3 volume% to 3 volume%, and preferably 0.5 volume% to 1.5 volume%.

[0035] (C) Dispersant The dispersant is a component that uniformly disperses inorganic particles in the ink and suppresses aggregation and sedimentation of the inorganic particles. The ink disclosed herein preferably contains a cationic dispersant. The cationic dispersant is, for example, a dispersant having a cationic functional group. The cationic dispersant adheres to the surface of the metal particles via, for example, the cationic functional group, causing steric hindrance. For this reason, aggregation between inorganic particles can be suppressed, and the long-term stability of the ink can be improved.

[0036] As the cationic dispersant, a conventionally known cationic dispersant used for this type of application can be used without any particular limitation. As the cationic dispersant, for example, an amine dispersant, an imidazoline dispersant, a quaternary ammonium dispersant, etc. can be mentioned. As the amine dispersant, for example, an alkyl polyamine dispersant, a polyalkylene polyamine dispersant, a fatty acid amine dispersant, a polyester amine dispersant, etc. can be mentioned. As the imidazoline dispersant, for example, an alkyl imidazoline, etc. can be mentioned. In addition, the cationic dispersant may be used alone or in combination of two or more kinds.

[0037] As the cationic dispersant, an amine dispersant can be preferably used. The amine dispersant is, for example, an organic compound having an amine group in the molecule. Among them, a chain-like amine dispersant having an amine group at at least one end is preferably used. Suitable examples of such an amine dispersant include fatty acid amine dispersants and polyester amine dispersants. Although not particularly limited, the weight average molecular weight of the amine dispersant is, for example, 1×10 3 ~5×10 4 As a specific example of the cationic dispersant, S-ream AD series (registered trademark) AD-508E manufactured by NOF Corporation is preferably used.

[0038] The volume percentage of the cationic dispersant in the ink can be set as appropriate as long as it does not impair the effects of the technology disclosed herein. For example, when the total volume of the ink is taken as 100%, the volume percentage of the cationic dispersant is generally 0.5% to 5% by volume, and preferably 1% to 3% by volume.

[0039] In addition, the dispersant may contain a nonionic dispersant as necessary. A nonionic dispersant is a dispersant that does not have a group that ionizes when dissolved in water. A nonionic dispersant is less likely to adhere to the surface of inorganic particles than a cationic dispersant. However, for example, when a cationic dispersant having a cationic functional group (e.g., an amine group) at one end adheres to the surface of an inorganic particle, the nonionic dispersant may adhere to the other end of the cationic dispersant. In this case, the cationic dispersant generated on the surface of the inorganic particle can strengthen the steric hindrance. Therefore, the effect of the dispersant in inhibiting the aggregation of inorganic particles can be enhanced.

[0040] (D) Organic solvent The organic solvent disperses the inorganic powder and can impart fluidity and the like suitable for inkjet printing to the ink. In addition to having a surface tension suitable for improving the refillability of the inkjet ink, the organic solvent is required to be able to suppress the flow of the ink when the printed film is heated and dried after inkjet printing. The present inventor focused on the volatilization rate of the organic solvent. During heating and drying, the organic solvent volatilizes from the surface of the printed film that is in contact with the air. On the other hand, according to the inventor's study, it was found that at this time, the volatilization rate is particularly high at the outer periphery of the printed film due to the relationship with the vapor pressure of the surrounding organic solvent. From this, the present inventor considered that the organic solvent would flow within the film from the inner periphery to the outer periphery of the printed film. At a stage where the drying of the printed film has not progressed, this flow is completed inside the printed film, and the homogeneity of the solid content (here, the inorganic powder) in the printed film is maintained. However, if the drying progresses and the flow of the solid content at the outer periphery stops before the flow at the inner periphery, the solid content will accumulate at the outer periphery. This can impair the smoothness of the printed film.

[0041] In response to this, the present inventor came up with the idea of ​​using a two-component organic solvent. The present inventor decided to use an organic solvent with a relatively low volatility as the component with a relatively small volume ratio of the two components. Furthermore, the present inventor considered including this component in the ink at a predetermined volume ratio relative to the volume of the solid content, and conducted extensive research. According to this research, it was found that the presence of a relatively small amount of low-volatility component causes the entire printing film to lose fluidity at the same time, as if it were a high-viscosity paste that has already been printed smoothly, and the low-volatility solvent is uniformly diffused and supplied within the film, thereby suppressing the accumulation of solid content on the outer periphery. Note that the above-mentioned mechanism is based on the present inventor's speculation, and there is no intention to limit the mechanism by which the effects of the technology disclosed herein are obtained to this.

[0042] In the ink disclosed herein, the organic solvent includes a first organic solvent and a second organic solvent. The first organic solvent and the second organic solvent each have a vapor pressure at 20° C. within a predetermined range. The vapor pressure of the organic solvent at 20° C. may be a nominal value provided by a manufacturer or the like.

[0043] The first organic solvent has a vapor pressure P 1 The first organic solvent has a vapor pressure P of 100 Pa or less and a surface tension of 22 mN / m to 31 mN / m. The first organic solvent can, for example, increase the fluidity of the inorganic powder and contribute to making the printed film thinner. In addition, the first organic solvent can have a function of increasing the long-term stability of the ink. 1 is the vapor pressure P of the second organic solvent described below. 2 It is better if the vapor pressure P 1 is in the above range, and the vapor pressure P 2 There is no particular limitation as long as it is greater than 10 Pa. For example, it is greater than 4 Pa, may be 5 Pa or more, or may be 10 Pa. 1 The pressure may be 50 Pa or less, or 40 Pa or less.

[0044] The first organic solvent may be, for example, at least one of ethers, esters, and alcohols. The first organic solvent may be, for example, a compound classified as an ether, an ester, or an alcohol, which has a vapor pressure P of 100 Pa or less. 1 and at least one compound having a surface tension of 22 mN / m to 31 mN / m. In this specification, "ethers" refers to a group of compounds having at least one ether bond (-COC-) in the main chain (mother nucleus). In this specification, "esters" refers to a group of compounds having at least one ester bond (RC(=O)-O-R') in the main chain. In the following description, compounds having multiple functional groups in one molecule are classified according to the IUPAC nomenclature. However, compounds having an ether bond and a hydroxyl group in one molecule are classified as ethers.

[0045] Examples of the ethers used as the first organic solvent include glycol ethers. Examples of the esters used as the first organic solvent include glycol ether acetates. Examples of the alcohols used as the first organic solvent include aliphatic alcohols.

[0046] In this specification, "glycol ether" refers to an aliphatic or alicyclic compound in which two hydroxyl groups are bonded to two different carbon atoms, and the hydrogen atoms of one or both of the two hydroxyl groups are replaced with a hydrocarbon group or a hydrocarbon group containing an ether bond. Glycol ethers include, for example, glycol monoalkyl ethers in which only the hydrogen of one hydroxyl group is replaced, and glycol dialkyl ethers in which both hydrogen of two hydroxyl groups are replaced. As the glycol ether in the first organic solvent, for example, diethylene glycol dibutyl ether, diethylene glycol butyl methyl ether, etc. can be preferably used.

[0047] In this specification, the term "glycol ether acetate" refers to a compound obtained by esterifying the above-mentioned glycol ether. As the glycol ether acetate in the first organic solvent, for example, butyl monoglycol acetate (BMGAC), butyl diglycol acetate (BDGAC), etc. can be preferably used.

[0048] In this specification, the term "alcohols" refers to a group of compounds in which the hydrogen atom of a hydrocarbon is replaced with a hydroxyl group, and is represented by the general formula: R-OH. As the alcohol in the first organic solvent, for example, 1-octanol, tetrahydrolinalool, etc. can be preferably used.

[0049] The second organic solvent has a vapor pressure P 2 It is an organic solvent with a vapor pressure P 2 is the vapor pressure of the first organic solvent, P 1 The second organic solvent is an organic solvent having a higher boiling point than the first organic solvent, and is less likely to volatilize than the first organic solvent. The second organic solvent suppresses the flowability and dispersibility of the inorganic powder from being excessively increased by the first organic solvent, and can contribute to the inorganic powder being appropriately dispersed in the ink. Vapor pressure P 2 may be, for example, 3 Pa or less, or 2 Pa or less. On the other hand, the vapor pressure P 2 For example, the surface tension may be 0.5 Pa or more, or 1 Pa or more. Although not particularly limited, the surface tension of the second organic solvent is preferably 25 mN / m to 35 mN / m.

[0050] The second organic solvent may be, for example, at least one of ethers, esters, and hydrocarbon compounds. In this specification, the term "hydrocarbon compound" refers to a compound composed of carbon atoms and hydrogen atoms. The second organic solvent may be, for example, a compound classified as an ether, an ester, or a hydrocarbon compound, which has a vapor pressure P of 4 Pa ​​or less. 2 The compound may be constituted by at least one compound having the formula:

[0051] Examples of ethers used as the second organic solvent include glycol ethers. Examples of esters used as the second organic solvent include glycol ether acetates and aromatic esters. Examples of hydrocarbon compounds used as the second organic solvent include linear alkanes having 20 or less carbon atoms (preferably 10 to 16 carbon atoms).

[0052] As the glycol ether in the second organic solvent, for example, butyl carbitol (diethylene glycol monobutyl ether) can be preferably used. As the glycol ether acetate in the second organic solvent, for example, 2,2,4-trimethyl-1,3-pentanediol 1-monoisobutyrate can be preferably used. In addition, in this specification, "aromatic ester" refers to a compound group in which a hydrogen atom in an aromatic ring is substituted with an ester group. As the aromatic ester in the second organic solvent, for example, butyl benzoate can be preferably used. As the linear alkane in the second organic solvent, for example, tetradecane can be preferably used.

[0053] In the ink disclosed herein, for example, when the entire organic solvent is taken as 100% by volume, the volume ratio of the second organic solvent is 30% by volume or less. The second organic solvent has a lower vapor pressure than the first organic solvent, and therefore a higher boiling point, which tends to reduce the fluidity of the inorganic powder in the ink and inhibit dispersion. For this reason, by setting the volume ratio of the second organic solvent in the organic solvent within a predetermined range, the fluidity and dispersibility of the inorganic powder in the ink can be made appropriate, and the smoothness of the printed film can be improved. From this viewpoint, when the entire organic solvent is taken as 100%, the volume ratio of the second organic solvent is, for example, 3% by volume or more, preferably 5% by volume or more, more preferably 7% by volume or more, and even more preferably 10% by volume or more.

[0054] In the ink disclosed herein, for example, the ratio (Vs2 / Vp) between the volume ratio Vs2 of the second organic solvent when the entire ink is taken as 100 volume % and the volume ratio Vp of the inorganic powder when the entire ink is taken as 100 volume % is 1.5 or more. By including the second organic solvent in the ink at a volume 1.5 times or more the volume of the inorganic powder, the inorganic powder can be appropriately dispersed in the ink. In addition, in the process in which the ink is applied to the substrate and dried, the inorganic powder can be prevented from moving as the ink dries, and the smoothness of the printed film can be improved. From this viewpoint, the ratio (Vs2 / Vp) is preferably 2 or more, more preferably 2.3 or more. On the other hand, from the viewpoint of appropriately dispersing the inorganic powder in the ink, the ratio (Vs2 / Vp) is, for example, 20 or less, preferably 15 or less, and more preferably 10 or less. The ratio (Vs2 / Vp) is, for example, 1.5 to 20, preferably 2 to 10, and more preferably 2.3 to 9.8.

[0055] Although there are no particular limitations, for example, from the viewpoint of improving the ejection properties of the ink, when the entire ink is taken as 100 volume %, the volume ratio of the organic solvent is, for example, 80 volume % or more, preferably 85 volume % or more, and more preferably 90 volume % or more.

[0056] (E) Other ingredients The ink disclosed herein may further contain known additives used in inkjet inks, to the extent that the effects of the technology disclosed herein are not impaired. The types and amounts of such additives can be appropriately changed based on conventionally known technical common sense, and do not characterize the technology disclosed herein. Therefore, a description thereof will be omitted here.

[0057] <Preparation of Inkjet Ink> Next, a procedure for preparing (manufacturing) the ink disclosed herein will be described. The ink disclosed herein is prepared by mixing the above-mentioned components and then crushing and dispersing the inorganic powder. FIG. 1 is a cross-sectional view of an agitator grinder 100. Note that the following description shows an example of a means for preparing the ink disclosed herein, and is not intended to limit the technology disclosed herein.

[0058] When manufacturing the ink disclosed herein, first, the above-mentioned components are weighed and mixed to prepare a slurry (including a paste and a suspension) which is a precursor of the ink. Then, the ink is prepared by stirring the slurry and crushing the inorganic powder using an agitation grinder 100 as shown in FIG. 1. For example, crushing beads (for example, zirconia beads having an average particle size of 10 μm to 150 μm) are added to the slurry, and the slurry is supplied from a supply port 110 into a stirring vessel 120. A shaft 134 having a plurality of stirring blades 132 is accommodated in the stirring vessel 120. One end of the shaft 134 is attached to a motor (not shown), and the motor is operated to rotate the shaft 134, thereby stirring the slurry while sending it downstream in the liquid sending direction D with the plurality of stirring blades 132. During this stirring, the inorganic powder is crushed by the crushing beads, and the fine inorganic powder is dispersed in the slurry.

[0059] Then, the slurry sent to the downstream side in the liquid sending direction D passes through the filter 140. As a result, the inorganic powder, disintegrating beads, etc. that have not been atomized are collected in the filter 140, and the ink in which the inorganic powder is sufficiently dispersed is discharged from the outlet 150. In this process, the average particle size, etc. of the inorganic powder can be adjusted to a desired range by appropriately adjusting the pore size of the filter 140, the average particle size of the disintegrating beads, etc.

[0060] <Inkjet ink applications> Next, applications of the ink disclosed herein will be described. The ink is used in the manufacture of electronic components. In this specification, "used in electronic components" includes not only an embodiment in which the ink is directly printed on the surface of an inorganic substrate, but also an embodiment in which the ink is indirectly attached to the surface of an inorganic substrate via an intermediate material such as transfer paper.

[0061] (1) Printing Fig. 2 is an overall view of the inkjet device 1. Fig. 3 is a cross-sectional view of the inkjet head 10. Ink is printed on the surface of a printing target by the inkjet device 1 as shown in Fig. 2. The material and shape of the inorganic substrate W to be printed are not particularly limited, and those used as substrates for general electronic components can be used without particular limitation.

[0062] As shown in Fig. 2, the inkjet device 1 includes an inkjet head 10 that stores ink. The inkjet head 10 is housed inside a print cartridge 40. The print cartridge 40 is inserted into a guide shaft 20 and configured to reciprocate along the axial direction X of the guide shaft 20. Although not shown, the inkjet device 1 also includes a moving means for moving the guide shaft 20 in the vertical direction Y. This allows the inkjet device 1 to eject ink at a desired position on the inorganic substrate W.

[0063] The inkjet head 10 may be, for example, a piezoelectric inkjet head as shown in Fig. 3. The piezoelectric inkjet head 10 is provided with a storage section 13 for storing ink in a case 12, and the storage section 13 is connected to a discharge section 16 via a liquid transfer path 15. The discharge section 16 is provided with a discharge port 17 that opens to the outside of the case 12, and a piezoelectric element 18 is arranged to face the discharge port 17. In the inkjet head 10, the piezoelectric element 18 is vibrated to discharge the ink in the discharge section 16 from the discharge port 17 toward the inorganic substrate W (green sheet) (see Fig. 2).

[0064] (2) Drying process Next, a drying process is performed in which the inorganic base material W (green sheet) to which the ink is attached is heated at a predetermined temperature. As a result, the organic solvent is removed from the ink to form a printed film (dried film) on the inorganic base material W. The ink disclosed herein contains a first organic solvent and a second organic solvent having predetermined characteristics at a predetermined volume ratio as organic solvents, so that the inorganic powder is in an appropriate dispersion state in the ink. In addition, during the drying process, in the ink attached to the inorganic base material, the first organic solvent having a relatively high vapor pressure (relatively low boiling point) evaporates first, and then the second organic solvent having a relatively low vapor pressure (relatively high boiling point) evaporates. Therefore, even during the drying process, the inorganic powder is kept in an appropriate dispersion state in the ink. As a result, a printed film with improved smoothness can be obtained after drying. The heating temperature in the drying process can be set to a temperature (for example, 50°C to 150°C) at which the organic solvent is removed and sintering of the inorganic powder does not occur.

[0065] (3) Firing This manufacturing method includes baking the inorganic base material W after the printing film is formed. As a result, organic components including the binder resin are burned away, and the inorganic powder is sintered and fixed to the surface of the inorganic base material W. As a result, an electronic component is manufactured having a baked film mainly composed of inorganic powder (e.g., ceramic powder or metal powder). The baking temperature can be appropriately set depending on, for example, the type of inorganic powder (e.g., ceramic powder or metal powder) contained in the ink. For example, the baking temperature is preferably set to 500°C to 2000°C.

[0066] Next, test examples related to the technology disclosed herein will be described. Note that the test examples shown below are not intended to limit the technology disclosed herein.

[0067] [Preparing materials] (Inorganic powder) As inorganic powders, the following three types of ceramic powders and one type of metal powder were prepared. Ceramic powder PC1: Barium titanate powder (average particle size: 0.30 μm) Ceramic powder PC2: Barium titanate powder (average particle size: 0.10 μm) Ceramic powder PC3: Barium titanate powder (average particle size: 0.05 μm) ·Metal powder PM1: Nickel powder (average particle size: 0.06 μm)

[0068] (Organic solvent) The following 10 types of organic solvents were prepared. The physical properties of the following organic solvents are shown in Table 1. Among the physical properties shown in Table 1, the boiling point (boiling point under atmospheric pressure conditions) and vapor pressure at 20°C are the nominal values ​​of each manufacturer. The surface tension of each organic solvent shown in Table 1 is a measured value measured for each organic solvent using a static surface tensiometer (DYNEMASTER DY-300, manufactured by Kyowa Interface Science Co., Ltd.).

[0069] Organic solvent S1: Diethylene glycol butyl methyl ether (Hisorb BDM), manufactured by Toho Chemical Industry Co., Ltd., "7382-32-3" Organic solvent S2: Propylene glycol monomethyl ether acetate (PGMEA), manufactured by Tokyo Chemical Industry Co., Ltd., "108-65-6" Organic solvent S3: Tetrahydrolinalool, manufactured by Tokyo Chemical Industry Co., Ltd., "78-69-3" Organic solvent S4: Butyl monoglycol acetate (BMGAC), manufactured by Daicel Corporation, "112-07-2" Organic solvent S5: 1-Octanol, Fujifilm Wako Pure Chemical Corporation, "117-87-5" Organic solvent S6: Butyl diglycol acetate (BDGAC), manufactured by Daicel Corporation, "124-17-4" Organic solvent S7: 2,2,4-trimethyl-1,3-pentanediol 1-monoisobutyrate (NG-120), "25265-77-4" Organic solvent S8: Butyl benzoate, manufactured by Tokyo Chemical Industry Co., Ltd., "136-60-7" Organic solvent S9: Tetradecane, manufactured by Kanto Chemical Co., Ltd., "629-59-4" Organic solvent S10: Butyl carbitol, Fujifilm Wako Pure Chemical Industries, Ltd., "112-34-5"

[0070] [Table 1]

[0071] (binder resin) The following two types of binder resins were prepared. Binder resin B1: Polyvinyl acetal resin with 23 mol% hydroxyl groups and a weight average molecular weight of 23,000 (manufactured by Sekisui Chemical Co., Ltd., "BL-S") Binder resin B2: Polyvinyl acetal resin with 21 mol% hydroxyl groups and a weight average molecular weight of 39,000 (manufactured by Sekisui Chemical Co., Ltd., "BL-5Z")

[0072] (Dispersant) As the dispersant, a cationic dispersant C1 (manufactured by NOF Corporation, "AD-508E") was prepared.

[0073] [Ink preparation] 25 kinds of inks containing inorganic powder, binder resin, dispersant, and organic solvent were prepared. First, inorganic powder and organic vehicle (organic solvent, binder resin, and dispersant) were mixed to a predetermined mass ratio to prepare a slurry. The slurry was subjected to a crushing and dispersion process (rotation speed: 1500 rpm, mixing time: 4 hours) using crushing beads (zirconia beads with an average particle size of 100 μm), and the ink was obtained by filtering with pressure. The inorganic powder and organic solvent used in each example are as shown in the corresponding columns of Tables 2 to 4. The binder resin used in each example was composed of at least one of the above-mentioned binder resin B1 and binder resin B2. The dispersant used in each example was the above-mentioned cationic dispersant C1.

[0074] Regarding the evaluation of the inks of Examples 1 to 25 prepared in these test examples, the results of Examples 1 to 14 are shown in Table 2. The results of Examples 15 to 21 are shown in Table 3. The results of Examples 22 to 25 are shown in Table 4.

[0075] With regard to the inorganic powder and the organic solvent, the numerical values ​​shown in the "Ratio in ink (volume %)" column in Tables 2 to 4 are the volume ratios of each component when the entire ink is taken as 100 volume %. With regard to the organic solvent, the numerical values ​​shown in the "Content ratio Vs2 of second organic solvent in total organic solvent (volume %)" column in Tables 2 to 4 are the volume ratios of the second organic solvent when the entire organic solvent is taken as 100 volume %. With regard to the organic solvent, the numerical values ​​shown in the "Vs2 / Vp" column in Tables 2 to 4 are the ratios (Vs2 / Vp) of the volume ratio Vs2 of the second organic solvent when the entire ink is taken as 100 volume % to the volume ratio Vp of the inorganic powder when the entire inkjet ink is taken as 100 volume %.

[0076] [Table 2]

[0077] [Table 3]

[0078] [Table 4]

[0079] [Evaluation test] The following pattern printing test and ejection test were carried out using the ink of each example. Note that for Example 18, the inorganic powder aggregated during the preparation of the ink and did not become dispersed. For this reason, evaluation tests were not carried out for Example 18. The "-" in the "Smoothness of printed film" column in Tables 2 to 4 indicates that the test was not carried out.

[0080] -Pattern printing test- The pattern forming ability of the ink of each example was evaluated using an inkjet printer (Material Printer DMP-2831, manufactured by Fujifilm Corporation). In this test, the ejection frequency of the inkjet printer was set to 1 kHz, and four patterns of 2 mm x 2 mm were solidly printed together on the surface of an alumina substrate. The printed patterns were evaluated for the occurrence of the coffee ring phenomenon using a surface roughness meter ("SURFTEST SV-3100", manufactured by Mitutoyo Corporation). Specifically, the film thickness was measured at three points on the edge of each pattern, and the maximum value was obtained. In addition, the film thickness was measured at three points in the center of each pattern, and the average value was obtained. The calculated values ​​obtained were calculated using the following formula (A): Maximum edge thickness / average center thickness<2 (A) Examples that satisfied the above criteria were evaluated as "○ (no coffee ring phenomenon occurred)." On the other hand, examples that did not satisfy the above formula (A) were evaluated as "× (coffee ring phenomenon occurred)." The results are shown in the "Uniformity of printed film" column in Tables 2 to 4.

[0081] As shown in Tables 2 to 4, the inkjet inks containing inorganic powder, organic solvent, binder resin, and dispersant in Examples 1 to 3, 15, 16, 22, and 23 have a vapor pressure P 1A first organic solvent having a vapor pressure P 2 is the vapor pressure P 1 and a second organic solvent having a pressure less than 4 Pa. When the total volume of the organic solvents was taken as 100 volume %, the content of the second organic solvent was 30 volume % or less. Furthermore, the ratio (Vs2 / Vp) of the volume fraction Vs2 of the second organic solvent when the total volume of the ink-jet ink was taken as 100 volume % to the volume fraction Vp of the inorganic powder when the total volume of the ink-jet ink was taken as 100 volume % was 1.5 or more. When the inks of Examples 1 to 3, 15, 16, 22, and 23 were used, the occurrence of the coffee ring phenomenon was not confirmed in the printed film, and it was found that the smoothness of the printed film was improved.

[0082] The technology disclosed herein has been described above, but these are merely examples and do not limit the scope of the claims. Various modifications can be made to the technology disclosed herein without departing from the spirit of the technology.

[0083] The techniques disclosed herein include the techniques described in the following sections. Section 1: 1. An inkjet ink for use in the manufacture of electronic components, comprising: Inorganic powder; A binder resin; A dispersant; An organic solvent; Including, Where: The organic solvent is Vapor pressure P at 20℃ 1 a first organic solvent having a viscosity of 100 Pa or less and a surface tension of 22 mN / m or more and 31 mN / m or less; Vapor pressure P at 20℃ 2 is the vapor pressure P 1 and a second organic solvent having a viscosity of 4 Pa ​​or less; Including, When the total volume of the organic solvent is 100%, the volume ratio of the second organic solvent is 30% or less; An ink-jet ink, wherein the ratio (Vs2 / Vp) of the volume fraction Vs2 of the second organic solvent when the entire ink-jet ink is taken as 100 volume % to the volume fraction Vp of the inorganic powder when the entire ink-jet ink is taken as 100 volume % is 1.5 or more. Section 2: Item 2. The ink-jet ink according to item 1, wherein the inorganic powder has an average particle size of 20 nm or more and 200 nm or less. Section 3: Item 3. The ink-jet ink according to item 1 or 2, wherein the inorganic powder comprises a ceramic powder or a metal powder. Section 4: 4. The ink-jet ink according to any one of items 1 to 3, wherein the inorganic powder includes barium titanate powder or nickel powder. Section 5: the first organic solvent is composed of at least one of ethers, esters, and alcohols; 5. The ink-jet ink according to any one of items 1 to 4, wherein the second organic solvent is composed of at least one of ethers, esters, and hydrocarbon compounds. Item 6: the first organic solvent is composed of at least one of glycol ether, glycol ether acetate, and aliphatic alcohol; 6. The ink-jet ink according to any one of items 1 to 5, wherein the second organic solvent is composed of at least one of glycol ether, glycol ether acetate, aromatic ester, and linear alkane having 20 or less carbon atoms. Section 7: 7. The ink-jet ink according to any one of items 1 to 6, wherein the second organic solvent is contained in an amount of at least 10% by volume when the total volume of the organic solvent is taken as 100% by volume. [Explanation of symbols]

[0084] 1 Inkjet device 10 Inkjet head 12 cases 13 Storage 15 Liquid delivery path 16 Discharge part 17 Outlet 18 Piezo element 20 Guide shaft 40 Print Cartridge 100 Stirring mill 110 Supply port 120 Mixing vessel 132 Stirring blade 134 Shaft 140 Filters 150 Outlet

Claims

1. 1. An inkjet ink for use in the manufacture of electronic components, comprising: Inorganic powder; A binder resin; A dispersant; An organic solvent; Including, Where: The organic solvent is Vapor pressure at 20°C P 1 a first organic solvent having a viscosity of 100 Pa or less and a surface tension of 22 mN / m or more and 31 mN / m or less; Vapor pressure at 20°C P 2 is the vapor pressure P 1 and a second organic solvent having a viscosity of 4 Pa ​​or less; Including, When the total volume of the organic solvent is 100%, the volume ratio of the second organic solvent is 30% by volume or less; an ink-jet ink, wherein a ratio (Vs2 / Vp) of a volume proportion Vs2 of the second organic solvent when the entire ink-jet ink is taken as 100 volume % to a volume proportion Vp of the inorganic powder when the entire ink-jet ink is taken as 100 volume % is 1.5 or more.

2. The ink-jet ink according to claim 1 , wherein the inorganic powder has an average particle size of 20 nm or more and 200 nm or less.

3. The ink-jet ink of claim 1 , wherein the inorganic powder comprises a ceramic powder or a metal powder.

4. The ink-jet ink of claim 1 , wherein the inorganic powder comprises barium titanate powder or nickel powder.

5. the first organic solvent is composed of at least one of ethers, esters, and alcohols; The ink-jet ink according to claim 1 , wherein the second organic solvent is composed of at least one of ethers, esters, and hydrocarbon compounds.

6. the first organic solvent is composed of at least one of glycol ether, glycol ether acetate, and aliphatic alcohol; 2. The ink-jet ink according to claim 1, wherein the second organic solvent is composed of at least one of glycol ether, glycol ether acetate, aromatic ester, and linear alkane having 20 or less carbon atoms.

7. The ink-jet ink according to any one of claims 1 to 6, wherein the second organic solvent is contained in an amount of at least 10% by volume when the total volume of the organic solvent is taken as 100% by volume.

Citation Information

Patent Citations

  • Spacer particle dispersion liquid and liquid crystal display device

    JP2008111985A

  • Inkjet printable composition

    JP2008513565A

  • Metal oxide fine particle dispersion element, conductive substrate and manufacturing method therefor

    JP2012216425A

  • Solid particle dispersion and device

    JP2015062871A

Cited By

  • Applied magnetic field synthesis and processing of iron nitride magnetic materials

    US12338536B2

  • Iron nitride permanent magnet and technique for forming iron nitride permanent magnet

    US12412686B2

  • Soft magnetic steel sheet, method for manufacturing the soft magnetic steel sheet, and core and dynamo-electric machine in which the soft magnetic steel sheet is used

    US12431269B2