Adhesion prevention gel-forming agent set, and adhesion prevention gel-forming kit
The anti-adhesion gel forming agent set with controlled gelation time and viscosity improves sprayability and gel formation, addressing sprayability and gelation challenges of existing materials, enabling effective application in diverse surgical settings.
Patent Information
- Application Number
- JP2023098525
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-03-29
- Filing Date
- 2023-06-15
- Publication Date
- 2024-10-11
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing adhesion prevention materials face challenges in sprayability and gelation properties, making them difficult to apply effectively and adjust to specific treatment areas.
An anti-adhesion gel forming agent set comprising a first agent with two or more hydroxyl groups and a second agent with a phosphorylcholine and phenylboronic acid group, with controlled gelation time and viscosity within specific limits, allowing for improved spray application and gel formation.
The solution provides an anti-adhesion gel with enhanced sprayability and gelling properties, preventing nozzle clogging and ensuring uniform application, suitable for various surgical procedures including open, laparoscopic, and robot-assisted surgeries.
Smart Images

Figure 2024143960000001 
Figure 2024143960000002 
Figure 2024143960000003
Abstract
Description
[Technical field]
[0001] The present invention relates to an adhesion prevention gel forming agent set and an adhesion prevention gel forming kit. [Background technology]
[0002] Various adhesion prevention techniques have been developed so far. For example, the technique described in Patent Document 1 is known as this type of technique. Patent Document 1 describes a tissue adhesion and / or joint contracture prevention material that mainly contains a composition containing a compound having a polyvalent hydroxyl group and a polymer containing a phosphorylcholine group and a phenylboronic acid group (claim 1, etc. of Patent Document 1). In addition, Example 20 of the same document shows an example in which a three-dimensional crosslinked body (BV gel) prepared by mixing the above composition in an aqueous solvent is adhered to a rat Achilles tendon in order to examine tendon healing and adhesion in a rat Achilles tendon injury model. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] International Publication No. 2009 / 066746 Summary of the Invention [Problem to be solved by the invention]
[0004] However, as a result of investigations conducted by the present inventors, it was found that the joint contracture prevention material described in the above Patent Document 1 leaves room for improvement in terms of sprayability and gelling properties. [Means for solving the problem]
[0005] As a result of further investigation, the inventors found that in an adhesion prevention gel forming agent set comprising a first agent and a second agent, the gelling properties can be improved by setting the gelling time of a mixture of the first agent and the second agent to a predetermined value or less, and the sprayability can be improved by setting the viscosity of the first agent and the second agent to a predetermined value or less, thereby resulting in good spray application, and thus completed the present invention.
[0006] According to one aspect of the present invention, the following adhesion prevention gel forming agent set and adhesion prevention gel forming kit are provided. 1. An adhesion prevention gel forming agent set used for forming an adhesion prevention gel by spray application, the adhesion prevention gel forming agent set comprising a first agent and a second agent, The first agent contains a compound having two or more hydroxyl groups, the second agent comprises a polymer comprising a phosphorylcholine group and a phenylboronic acid group; the gelation time from immediately after mixing the first agent and the second agent to gelation, as measured according to the following procedure A, is 20 seconds or less; the viscosity of the first agent is 100.0 mPa s or less, and the viscosity of the second agent is 100.0 mPa s or less, as measured according to the following procedure B; Anti-adhesion gel forming agent set. (Step A) Using a dynamic viscoelasticity measuring device, the viscoelasticity of a mixture of the first agent and the second agent in a volume ratio of 1:1 is measured at room temperature of 25°C, a frequency of 1 Hz, and a strain oscillation angle of 1%. From the obtained viscoelasticity spectrum, the storage modulus (G') at 25°C and the loss modulus (G'') at 25°C are calculated, and the time (seconds) elapsed from the start of the measurement until G'' / G' becomes 1.0 or less is defined as the gelation time. (Step B) The viscosity of the first agent and the viscosity of the second agent are each measured using a cone-plate viscometer at room temperature of 25° C., a cone rotor angle of 1°34′, and a rotation speed of 50 rpm. 2. The adhesion prevention gel forming agent set according to 1., A set of adhesion prevention gel-forming agents, in which the viscosity of the first agent is 1.0 mPa·s or more, and the viscosity of the second agent is 1.0 mPa·s or more, as measured according to procedure B. 3. The adhesion prevention gel forming agent set according to 1. or 2. The adhesion prevention gel forming agent set is used in a spray device, The spray device comprises: a first container with a first nozzle containing the first part, and a second container with a second nozzle containing the second part; or An adhesion prevention gel forming agent set comprising a common container with a common nozzle for containing a mixed liquid including the first agent and the second agent. 4. The adhesion prevention gel forming agent set according to any one of 1. to 3., An adhesion prevention gel forming agent set, in which a gel sample taken 30 minutes after mixing the first agent and the second agent has a storage modulus at 25°C of 10 Pa or more and 1000 Pa or less, measured according to procedure A. 5. An adhesion prevention gel forming agent set according to any one of 1. to 4., A set of adhesion prevention gel-forming agents, in which a gel sample taken 30 minutes after mixing the first agent and the second agent has a loss tangent calculated from G'' / G'' at 25°C, where G' is the storage modulus and G'' is the loss modulus, measured according to procedure A, of 0.01 or more and 0.1 or less. 6. An adhesion prevention gel forming agent set according to any one of 1. to 5., When the viscosity measured according to the procedure B immediately after preparation is defined as η1, the viscosity measured after storage at 80°C for one week is defined as η2, and the rate of change in viscosity is defined as (|η2-η1| / η1)×100, The adhesion prevention gel forming agent set, wherein the viscosity change rate of the first agent is 0% or more and 10% or less, and the viscosity change rate of the second agent is 0% or more and 10% or less. 7. An adhesion prevention gel forming agent set according to any one of 1. to 6., An adhesion prevention gel forming agent set, in which the compound having two or more hydroxyl groups in the first agent includes one or more selected from the group consisting of monosaccharides, polysaccharides, low molecular weight alcohols, and water-soluble polymer alcohols. 8. The adhesion prevention gel forming agent set according to any one of 1. to 7., An adhesion prevention gel-forming agent set, wherein the polymer in the second agent contains a (meth)acrylate group in the molecule. 9. The adhesion prevention gel forming agent set according to any one of 1. to 8., An adhesion prevention gel forming agent set, wherein the polymer in the second agent comprises a polymer having a skeleton represented by the following general formula (1): [ka] (In the above general formula (1), R1 represents a hydrogen atom, a methyl group, or an ethyl group, R2 represents an alkyl group having 2 to 12 carbon atoms or an oxyethylene group, R3 represents an alkyl group having 2 to 4 carbon atoms, X represents a single bond, a phenyl group which may have a substituent, or a group represented by -C(O)-, -C(O)O-, -O-, -C(O)NH-, or -S-, A represents a hydrogen atom, a halogen atom, or any organic substituent, n, m, and l represent, in the order of 0.01 to 0.99, 0.01 to 0.99, and 0 to 0.98, respectively (with the sum of n, m, and l being 1.00).) 10. The adhesion prevention gel forming agent set according to any one of 1. to 9., the weight average molecular weight of the compound having two or more hydroxyl groups in the first agent is 10,000 or more and 50,000 or less, and / or The weight average molecular weight of the polymer in the second agent is 10,000 or more and 32,000 or less. Anti-adhesion gel forming agent set. 11. An adhesion prevention gel forming kit comprising an adhesion prevention gel forming agent set described in any one of 1. to 10. and a spray device. Effect of the Invention
[0007] According to the present invention, there are provided an adhesion prevention gel forming agent set having excellent sprayability and gelling properties, and an adhesion prevention gel forming kit using the same. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0008] An outline of the adhesion prevention gel forming agent set of this embodiment will be described.
[0009] The adhesion preventing gel forming agent set of the present embodiment is used for forming an adhesion preventing gel by spray application.
[0010] The majority of current adhesion prevention techniques involve attaching a film-type adhesion prevention material to the treated tissue. Film-type adhesion prevention materials exert their adhesion due to the moisture present in the body, but they are known to be difficult to move after application and difficult to adjust the application site.
[0011] In contrast, the adhesion preventing gel forming agent set of the present embodiment is a spray composition set to be used as a spray-type adhesion preventing material. Since the application position of the spray-type adhesion preventing material is easily adjusted, it is easy to control the position where the adhesion preventing gel is formed around the treated tissue. In addition, the spray-type adhesion preventing material can be applied not only to open surgery but also to laparoscopic surgery and robot-assisted laparoscopic surgery, considering that it can be applied to tissues through a nozzle inserted into the body.
[0012] In the case of a spray-type adhesion preventing material, a layered application method in which one of the first agent and the second agent is applied around the treated tissue and then the other is applied on top of that, a batch application method in which a liquid solution of the first agent and the second agent mixed together is applied around the treated tissue before gelation, or a batch application method in which the spray-type first agent and the spray-type second agent are mixed and applied around the treated tissue while being mixed, etc., can be used. However, the application method is not limited to these.
[0013] The adhesion prevention gel forming agent set of this embodiment comprises a first agent and a second agent, the first agent comprising a compound having two or more hydroxyl groups, and the second agent comprising a polymer comprising a phosphorylcholine group and a phenylboronic acid group. Such an adhesion prevention gel forming agent set includes: The gelation time from immediately after mixing the first and second parts to the time when the first and second parts start to gel, as measured according to the following procedure A, is 20 seconds or less; The viscosity of the first agent is 100.0 mPa·s or less, and the viscosity of the second agent is 100.0 mPa·s or less, as measured according to the following procedure B. (Step A) Using a dynamic viscoelasticity measuring device, the viscoelasticity of a mixture of the first agent and the second agent in a volume ratio of 1:1 is measured at room temperature of 25°C, a frequency of 1 Hz, and a strain oscillation angle of 1%. From the obtained viscoelasticity spectrum, the storage modulus (G') at 25°C and the loss modulus (G'') at 25°C are calculated, and the time (seconds) elapsed from the start of the measurement until G'' / G' becomes 1.0 or less is defined as the gelation time. (Step B) The viscosity of the first agent and the viscosity of the second agent are each measured using a cone-plate viscometer at room temperature of 25° C., a cone rotor angle of 1°34′, and a rotation speed of 50 rpm.
[0014] According to the findings of the present inventors, it has been found that by setting the viscosity of the first agent and the second agent contained in the adhesion prevention gel forming agent set to be equal to or less than the above upper limit value, it is possible to prevent nozzle clogging in the spray device and form a high-quality mist, thereby improving the uniformity of mixing of the first agent and the second agent at the spray destination. In addition, it was found that by setting the gelation time to not more than the above upper limit, the crosslinking reaction (gelation reaction) between the first and second components proceeds relatively quickly, making it possible to suppress dripping and the like at the point where the spray hits.
[0015] The upper limit of the gelation time is 20 seconds or less, preferably 18 seconds or less, and more preferably 15 seconds or less, which can suppress dripping after spraying. On the other hand, the lower limit of the gelation time is not particularly limited, but may be 3 seconds or more.
[0016] The upper limit of the viscosity of the first agent is 100.0 mPa·s or less, preferably 80 mPa·s or less, and more preferably 70 mPa·s or less, which results in finer droplets when sprayed and improves mixing efficiency. On the other hand, the lower limit of the viscosity of the first agent is not particularly limited, but may be 1.0 mPa·s or more.
[0017] The upper limit of the viscosity of the second agent is 100.0 mPa·s or less, preferably 60 mPa·s or less, and more preferably 50 mPa·s or less, which results in finer droplets when sprayed and improves mixing efficiency. On the other hand, the lower limit of the viscosity of the second part is not particularly limited, but may be 1.0 mPa·s or more.
[0018] The viscosity of the first agent or the second agent immediately after preparation, measured according to procedure B above, is defined as η1, the viscosity of the first agent or the second agent after storage at a temperature of 80°C for one week is defined as η2, and the rate of viscosity change is defined as (|η2-η1| / η1)×100. In this case, the upper limit of the viscosity change rate of the first agent is, for example, 10% or less, preferably 9% or less, and more preferably 8% or less, which can suppress the change in sprayability over time. On the other hand, the lower limit of the viscosity change rate of the first agent is not particularly limited, but may be 0% or more.
[0019] The upper limit of the rate of change in viscosity of the second agent is, for example, 10% or less, preferably 9% or less, and more preferably 8% or less, which can suppress changes in sprayability over time. On the other hand, the lower limit of the viscosity change rate of the second agent is not particularly limited, but may be 0% or more.
[0020] For the gel sample 30 minutes after mixing the first and second parts, the storage modulus (G') at 25°C and the loss modulus (G'') at 25°C are calculated according to procedure A above. In this case, the lower limit of the storage modulus of the gel sample after 30 minutes is, for example, 10 Pa or more, preferably 30 Pa or more, more preferably 50 Pa or more, and further preferably 100 Pa or more. On the other hand, the upper limit of the storage modulus of the gel sample after 30 minutes is, for example, 1000 Pa, preferably 800 Pa or less, and more preferably 500 Pa or less.
[0021] The loss tangent calculated from G'' / G' in the gel sample after 30 minutes is, for example, 0.01 to 0.15, preferably 0.03 to 0.13, and more preferably 0.04 to 0.10.
[0022] As used herein, the term "adhesion" refers to undesirable inter-organ or inter-tissue connection or fusion that occurs between one tissue and another tissue.
[0023] The adhesion prevention gel may be used in any living tissue, such as the abdominal cavity of an "animal." The animal may be either a mammal or a non-mammal, but is preferably a mammal, such as a primate, such as a human, a mouse, a guinea pig, a rat, a cow, a horse, a pig, a goat, a dog, a rabbit, etc.
[0024] The adhesion prevention gel forming kit may include an adhesion prevention gel forming agent set and a spray device. That is, the adhesion preventing gel forming agent set is used in the spray device.
[0025] The spray device may, for example, have a first configuration comprising a first container with a first nozzle containing a first agent, and a second container with a second nozzle containing a second agent, or may have a second configuration comprising a common container with a common nozzle containing a mixed liquid comprising the first agent and the second agent.
[0026] Each component of the adhesion preventing gel forming agent set of the present embodiment will be described in detail below.
[0027] The adhesion prevention gel-forming agent set includes a first agent and a second agent.
[0028] The first agent contains at least a compound having two or more hydroxyl groups. As the compound having two or more hydroxyl groups, one that dissolves in an aqueous medium can be used. The compound having two or more hydroxyl groups in the first agent may include one or more selected from the group consisting of monosaccharides, polysaccharides, low molecular weight alcohols, and water-soluble polymer alcohols.
[0029] Specifically, examples of monosaccharides include glucose and glucosamine. Examples of polysaccharides include maltose, lactose, amylose, amylopectin, chitin, hyaluronic acid, cellulose, pullulan, dextran, and derivatives thereof. Examples of low molecular weight alcohols include synthetic diols and triols. Examples of the water-soluble polymer alcohol include polyvinyl alcohol, poly(2-hydroxyethyl (meth)acrylate), poly(2,3-dihydroxyethyl (meth)acrylate), and poly((meth)acrylic acid glycoside). These may be used alone or in combination of two or more. The monosaccharides and polysaccharides may be either natural or artificial. Of these, polysaccharides and water-soluble polymer alcohols are preferred, and polyvinyl alcohol is more preferred.
[0030] The second agent includes at least a polymer that includes a phosphorylcholine group and a phenylboronic acid group. The polymer containing a phosphorylcholine group and a phenylboronic acid group can be produced, for example, by mixing a first monomer containing a phosphorylcholine group with a second monomer having a phenylboronic acid group, and carrying out a polymerization reaction such as a radical polymerization reaction in the presence of a radical generator. A third monomer may be added as appropriate to adjust the properties of the resulting polymer.
[0031] The first monomer having a phosphorylcholine group can be selected from compounds having a carbon-carbon double bond such as a vinyl group or an allyl group as a polymerizable group and having a phosphorylcholine group in the same molecule. Examples of the first monomer include 2-methacryloyloxyethyl phosphorylcholine, 2-(meth)acryloyloxyethyl-2'-(trimethylammonio)ethyl phosphate, 3-(meth)acryloyloxypropyl-2'-(trimethylammonio)ethyl phosphate, 4-(meth)acryloyloxybutyl-2'-(trimethylammonio)ethyl phosphate, and 5-(meth)acryloyloxypentyl-2'-(trimethylammonio)ethyl phosphate. phosphate, 6-(meth)acryloyloxyhexyl-2'-(trimethylammonio)ethyl phosphate, 2-(meth)acryloyloxypropyl-2'-(trimethylammonio)ethyl phosphate, 2-(meth)acryloyloxybutyl-2'-(trimethylammonio)ethyl phosphate, 2-(meth)acryloyloxypentyl-2'-(trimethylammonio)ethyl phosphate, 2-(meth)acryloyloxyhexyl-2'-(trimethylammonio)ethyl phosphate 2-(meth)acryloyloxyethyl-3'-(trimethylammonio)propyl phosphate, 3-(meth)acryloyloxypropyl-3'-(trimethylammonio)propyl phosphate, 4-(meth)acryloyloxybutyl-3'-(trimethylammonio)propyl phosphate, 5-(meth)acryloyloxypentyl-3'-(trimethylammonio)propyl phosphate, 6-(meth)acryloyloxyhexyl 3'-(trimethylammonio)propyl phosphate, 3-(meth)acryloyloxypropyl-4'-(trimethylammonio)butyl phosphate, 4-(meth)acryloyloxybutyl-4'-(trimethylammonio)butyl phosphate, 5-(meth)acryloyloxypentyl-4'-(trimethylammonio)butyl phosphate and 6-(meth)acryloyloxyhexyl-4'-(trimethylammonio)butyl phosphate. These may be used alone or in combination of two or more. Among these, 2-methacryloyloxyethyl phosphorylcholine (hereinafter abbreviated as MPC) may be used. In this specification, "(meth)acrylic" means methacryl and / or acrylic.
[0032] The second monomer having a phenylboronic acid group can be selected from compounds having a carbon-carbon double bond, such as a vinyl group or an allyl group, as a polymerizable group and having a phenylboronic acid group in the same molecule. Examples of the second monomer include p-vinylphenylboronic acid, m-vinylphenylboronic acid, p-(meth)acryloyloxyphenylboronic acid, m-(meth)acryloyloxyphenylboronic acid, p-(meth)acrylamidophenylboronic acid, m-(meth)acrylamidophenylboronic acid, p-vinyloxyphenylboronic acid, m-vinyloxyphenylboronic acid, vinylurethanephenylboronic acid, etc. These may be used alone or in combination of two or more. Among these, p-vinylphenylboronic acid or m-vinylphenylboronic acid is preferred in terms of availability of raw materials.
[0033] Examples of the third monomer that can be added include hydrophilic monomers such as (meth)acrylic acid, sodium (meth)acrylate, 2-hydroxyethyl (meth)acrylate, glycerol (meth)acrylate, N-vinylpyrrolidone, acrylonitrile, (meth)acrylamide, polyethylene glycol mono(meth)acrylate, vinylbenzenesulfonic acid, and sodium vinylbenzenesulfonate, methyl (meth)acrylate, ethyl (meth)acrylate, butyl (meth)acrylate, lauryl (meth)acrylate, dodecyl (meth)acrylate, stearyl (meth)acrylate, 2-ethylhexyl (meth)acrylate, styrene, Examples of the monomer include hydrophobic monomers such as vinyl acetate, monomers having alkyloxysilane groups such as (3-methacryloyloxypropyl)trimethoxysilane, (3-methacryloyloxypropyl)triethoxysilane, (3-methacryloyloxypropyl)methyldimethoxysilane, and trimethoxyvinylsilane, monomers having siloxane groups, monomers having glycyl groups such as glycidyl methacrylate, monomers having amino groups such as allylamine, aminoethyl (meth)acrylate, and 2-methylallylamine, and monomers having groups such as carboxyl, hydroxyl, aldehyde, thiol, halogen, methoxy, epoxy, succinimide, and maleimide. These may be used alone or in combination of two or more. Among these, butyl (meth)acrylate may be used.
[0034] The solvent used in the polymerization reaction may be any solvent capable of dissolving the first and second monomers. More preferably, the solvent may also be capable of dissolving the polymer produced by polymerization. The solvent may be a single solvent or a mixed solvent of two or more kinds.
[0035] The radical generator can be used without limitation as long as it dissolves in the solvent used in the polymerization reaction and decomposes at a reaction temperature in the range of, for example, 30° C. to 90° C. to generate radicals. From the viewpoint of safety and stability, aliphatic azo compounds such as azobisisobutyronitrile and 4,4'-azobis(4-cyanopentanoic acid), and peroxides such as benzoyl peroxide and succinic acid peroxide are preferred. Furthermore, the molecular structure and molecular weight can be controlled by utilizing an initiator that generates radicals upon irradiation with light, an atom transfer living radical polymerization reaction, a reversible addition-fragmentation chain transfer polymerization method, or the like.
[0036] The polymer containing a phosphorylcholine group and a phenylboronic acid group may contain a (meth)acrylate group in the molecule.
[0037] Furthermore, the polymer containing a phosphorylcholine group and a phenylboronic acid group may include a polymer having a skeleton represented by the following general formula (1).
[0038] [ka]
[0039] In the above general formula (1), R1 represents a hydrogen atom, a methyl group, or an ethyl group, R2 represents an alkyl group having 2 to 12 carbon atoms or an oxyethylene group, R3 represents an alkyl group having 2 to 4 carbon atoms, X represents a single bond, a phenyl group which may have a substituent, or a group represented by -C(O)-, -C(O)O-, -O-, -C(O)NH-, or -S-, A represents a hydrogen atom, a halogen atom, or any organic substituent, n, m, and l represent, in order, 0.01 to 0.99, 0.01 to 0.99, and 0 to 0.98, respectively (with the sum of n, m, and l being 1.00).
[0040] The weight average molecular weight (Mw) of the compound having two or more hydroxyl groups in the first agent is, for example, 10,000 or more and 50,000 or less, preferably 12,500 or more and 40,000 or less, and more preferably 15,000 or more and 30,000 or less. The number average molecular weight (Mn) of the compound having two or more hydroxyl groups in the first agent is, for example, 5,000 or more and 20,000 or less, preferably 6,000 or more and 19,000 or less, and more preferably 7,000 or more and 18,000 or less.
[0041] On the other hand, the weight average molecular weight (Mw) of the polymer in the second agent is, for example, 10,000 or more and 32,000 or less, preferably 12,000 or more and 31,000 or less, and more preferably 14,000 or more and 30,000 or less. The number average molecular weight (Mn) of the polymer in the second agent is, for example, 5,000 or more and 15,000 or less, preferably 6,000 or more and 14,000 or less, and more preferably 7,000 or more and 13,000 or less.
[0042] In this embodiment, the weight average molecular weight and the number average molecular weight can be calculated based on a calibration curve of a standard PEG sample using GPC.
[0043] The first agent and the second agent may each further contain additives such as a viscosity modifier, a wetting agent, an emulsifier, a lubricant, a colorant, a release agent, a preservative, an antioxidant, a pH buffer, etc. These may be used alone or in combination of two or more kinds.
[0044] One method for producing an adhesion prevention gel is to use an adhesion prevention gel forming agent set containing a first agent and a second agent, for example by mixing a compound having two or more hydroxyl groups contained in the first agent with a polymer containing a phosphorylcholine group and a phenylboronic acid group contained in the second agent to form an adhesion prevention gel composed of a three-dimensional crosslinked body.
[0045] The temperature for obtaining a three-dimensional crosslinked body is, for example, 4 to 90°C, unless otherwise limited by the application, and is preferably 10 to 40°C from the viewpoint of preventing structural changes and activity reduction during immobilization of biological components, and is preferably around room temperature, i.e., 20 to 37°C, from the viewpoint of operation.
[0046] The first agent and / or the second agent may contain a solvent. The solvent may be an aqueous solvent, specifically, pure water, a buffer solution, a cell culture solution, an aqueous solution containing 30% or less of an organic solvent, or the like.
[0047] Although the embodiments of the present invention have been described above, these are merely examples of the present invention, and various configurations other than those described above can be adopted. Furthermore, the present invention is not limited to the above-described embodiments, and modifications and improvements within the scope of the present invention are included in the present invention. EXAMPLES
[0048] The present invention will be described in detail below with reference to examples, but the present invention is not limited to the descriptions of these examples.
[0049] <Production of adhesion prevention gel forming agent set> (Synthesis of PMBV) 30 mL of reaction solvent, raw material monomer, and reaction initiator were introduced into a glass reaction vessel according to the concentration ratio shown in Table 1, and the mixture was bubbled with nitrogen gas for 15 minutes. After that, the mixture was reacted for about 18 hours at a reaction temperature shown in Table 1 of 60 to 70°C to obtain a reaction liquid. Ethanol (special grade reagent) was used as the reaction solvent. As the raw material monomers, 2-methacryloyloxyethyl phosphorylcholine (MPC, reagent, special grade), butyl methacrylate (BMA), and p-vinylphenylboronic acid (VPBA, reagent, special grade) were used according to the charging ratios shown in Table 1. The reaction initiator used was 2,2'-azobis(isobutyronitrile) (AIBN, reagent, special grade). Subsequently, the obtained reaction liquid was dropped into a reprecipitation solvent to precipitate a polymer, which was then subjected to suction filtration and drying under reduced pressure to obtain a white powdery polymer. The reprecipitation solvent used here was one or a suitable mixture of two or more solvents selected from the group consisting of hexane, acetone, diethyl ether, and chloroform. The resulting polymer powder was dissolved in pure water and sealed in a dialysis membrane with a molecular weight cutoff of 3500. The polymer was then purified by dialysis in a glass container filled with pure water for three days, with the pure water being replaced once a day. After three days, the aqueous solution in the dialysis membrane was freeze-dried to obtain white powdery polymers (PMBV1-3) with a yield of approximately 5 g.
[0050] [Table 1]
[0051] (Preparation of the first agent) A polyhydric hydroxyl group-containing compound was dissolved in pure water so as to give a viscosity value shown in Table 2, and a colorant was added thereto so as to give a concentration of 0.01 weight percent, thereby preparing a first agent shown in Table 2. As the polyhydroxyl group-containing compound, polyvinyl alcohol (PVA, reagent, special grade) having the molecular weight shown in Table 2 was used. Brilliant Blue FCF (special grade reagent) was used as the colorant. However, the first agent in Comparative Example 1 further contained a specified amount of polyethylene glycol 20000. The concentration of PVA3 in the first agent in Comparative Example 3 was 0.5 times the concentration (wt%) of PVA1 in the first agent in Example 1. When used in animal experiments, the first agent was sterilized by filtration using a filter.
[0052] (Preparation of the second agent) A polymer containing a phosphorylcholine group and a phenylboronic acid group was dissolved in pure water so that the viscosity became the value shown in Table 2, to prepare a second agent shown in Table 2. As the polymer containing a phosphorylcholine group and a phenylboronic acid group, any one of PMBV1 to 3 synthesized above was used. However, the second agent in Comparative Example 2 further contained a specified amount of polyethylene glycol 20000. The second agent in Comparative Example 3 had a PMBV3 concentration (wt%) 0.33 times that of the second agent in Example 3. When used in animal experiments, the second agent was sterilized by filtration using a filter.
[0053] (Molecular weight analysis) The weight average molecular weight and number average molecular weight of PMBV1-3 (powdered polymers after dialysis purification) synthesized in Table 1 and PVA1-2 used in Table 2 were calculated using GPC (gel permeation chromatography) based on a calibration curve using a standard PEG sample. The results are shown in Table 2. For the GPC measurement, one Tosoh TSKgel SuperAWM-H, one TSKgel SuperAW2500, and one TSKgel guardcolumn SuperAW-H were used, and the developing solvent was 70% methanol / 30% HO (with 10 mM LiBr added), with a column temperature of 40°C and a flow rate of 0.6 ml / min.
[0054] (composition analysis) Regarding PMBV1 to 3 synthesized in Table 1, 1 The ratio of each monomer introduced was calculated from the H-NMR spectrum, and the results are shown in Table 2. NMR measurements were performed using a JNM-ECA500 manufactured by JEOL Ltd., with a deuterated ethanol solvent and 32 accumulations.
[0055] (viscosity) The viscosity of the first and second parts in Table 2 was measured using a cone-plate viscometer (Toki Sangyo Co., Ltd., TV-100EH) at room temperature of 25°C, a cone rotor angle of 1°34', and a rotation speed of 50 rpm. The viscosity of the first and second agents was measured immediately after preparation and after storage at 80°C for one week. The viscosity immediately after preparation was taken as η1 and the viscosity after storage as η2, and the viscosity change rate (%) was calculated based on (|η2-η1| / η1)×100.
[0056] (storage modulus, loss modulus) Using the dynamic viscoelasticity (DMA) measurement method, a dynamic viscoelasticity measuring device (manufactured by Anton Paar, product name: MCR301) was used to measure the viscoelasticity (gelation process) of a mixture of the first and second agents in a volume ratio of 1:1 at room temperature of 25°C, a frequency of 1 Hz, and a strain oscillation angle of 1%. The storage modulus (G') at 25°C and the loss modulus (G'') at 25°C were determined from the viscoelasticity spectrum, and the loss tangent (G'' / G') was calculated using these values. The gelation time was defined as the time (seconds) elapsed from the start of measurement until G'' / G' became 1.0 or less after G' gradually decreased and then increased.
[0057] [Table 2]
[0058] The adhesion prevention gel forming agent set containing the first agent and the second agent obtained above was used to evaluate the following items.
[0059] <Sprayability> When the first and second agents obtained above were sprayed using a two-liquid mixing type spray nozzle (nozzle inner hole diameter: Φ0.60 mm), the case where the spray particles were observed to become a mist and diffuse in a cone shape was judged to be "good", and the case where the nozzle was clogged, the droplets dripped, or a continuous body of droplets was released in a straight line was judged to be "poor".
[0060] <Gelling properties> When the first and second agents obtained above were sprayed onto paper placed on a 30° inclined surface using a two-liquid mixing spray nozzle, if a gel was formed at the desired position, it was rated as "good," and if droplets dripped and it was difficult to form a gel at the desired position, it was rated as "poor."
[0061] <Evaluation of the effect of preventing adhesion in the abdominal cavity of animals> When using the adhesion prevention gel forming agent set, the first agent and the second agent were each connected to a two-liquid mixing type sprayer, and the first agent and the second agent were mixed in a volume ratio of 1:1 and sprayed.
[0062] From the above results, it was found that the adhesion prevention gel forming agent sets of Examples 1 to 3 were superior in sprayability compared to Comparative Examples 1 and 2, and superior in gelling properties compared to Comparative Example 3.
[0063] The following animal experiments were conducted with the approval of the ethical committee for animal experiments at the study site. Male SD rats (8 weeks old at the time of receipt), a strain commonly used in general animal experiments, were used. Anesthesia was administered using isoflurane, and the abdomen was opened through a midline incision. The omentum and fat pad surrounding the cecum were removed, the cecum was exposed to the outside of the wound, and a 1x2cm area of the cecum wall facing the abdominal wall was scraped until pinpoint bleeding occurred. Depending on the location of the cecum, a 1x2cm area of the abdominal wall, either left or right, was removed at least 1cm away from the incision. The first and second agents obtained above were sprayed onto the scraped area of the cecum and the entire abdominal cavity in a total amount of 1 mL to create a gel film. The peritoneum and muscle layer at the incision site were sutured with absorbable sutures, and the skin was sutured with non-absorbable sutures, and the abdomen was closed.
[0064] (Autopsy Observation and Evaluation) Seven days after the treatment, the animals were euthanized by isoflurane inhalation anesthesia (mixed with carbon dioxide). The abdomen was opened, taking care to avoid the treatment site, and the treatment site was exposed, and adhesions that had developed at the treatment site were evaluated. The incidence rate of adhesions (%) was calculated based on (number of animals in which adhesions were observed between at least one of the treated areas of the cecum and the treated area of the abdominal wall) / (number of experimental animals) × 100. The number of experimental animals was 6.
[0065] By using the adhesion prevention gel forming agent sets of Examples 1 to 3 to form an adhesion prevention gel that prevents adhesions within the abdominal cavity, the incidence of adhesions was reduced compared to when the adhesion prevention gel forming agent set was not used, demonstrating excellent adhesion prevention ability.
Claims
1. An adhesion prevention gel forming agent set used for forming an adhesion prevention gel by spray application, the adhesion prevention gel including a first agent and a second agent, The first agent contains a compound having two or more hydroxyl groups, the second agent comprises a polymer comprising a phosphorylcholine group and a phenylboronic acid group; the gelation time from immediately after mixing the first agent and the second agent to gelation, as measured according to the following procedure A, is 20 seconds or less; The viscosity of the first agent is 100.0 mPa s or less, and the viscosity of the second agent is 100.0 mPa s or less, as measured according to the following procedure B. Anti-adhesion gel forming agent set. (Procedure A) Using a dynamic viscoelasticity measuring device, the viscoelasticity of a mixture obtained by mixing the first agent and the second agent in a volume ratio of 1:1 is measured under conditions of room temperature of 25° C., a frequency of 1 Hz, and a strain oscillation angle of 1%. From the obtained viscoelasticity spectrum, the storage modulus (G') at 25° C. and the loss modulus (G'') at 25° C. are obtained, and the time (seconds) elapsed from the start of the measurement until G'' / G' becomes 1.0 or less is defined as the gelation time. (Procedure B) The viscosity of the first agent and the viscosity of the second agent are each measured using a cone-plate viscometer at room temperature of 25° C., a cone rotor angle of 1°34′, and a rotation speed of 50 rpm.
2. The adhesion prevention gel forming agent set according to claim 1, A set of adhesion prevention gel-forming agents, in which the viscosity of the first agent is 1.0 mPa·s or more, and the viscosity of the second agent is 1.0 mPa·s or more, as measured according to procedure B.
3. The adhesion prevention gel forming agent set according to claim 1 or 2, The adhesion prevention gel forming agent set is used in a spray device, The spray device comprises: a first container with a first nozzle containing the first part, and a second container with a second nozzle containing the second part; or An adhesion prevention gel forming agent set comprising a common container with a common nozzle for containing a mixed liquid including the first agent and the second agent.
4. The adhesion prevention gel forming agent set according to claim 1 or 2, An adhesion prevention gel forming agent set, in which a storage modulus at 25°C, measured according to procedure A for a gel sample 30 minutes after mixing the first agent and the second agent, is 10 Pa or more and 1,000 Pa or less.
5. The adhesion prevention gel forming agent set according to claim 1 or 2, A set of adhesion prevention gel-forming agents, in which a gel sample taken 30 minutes after mixing the first agent and the second agent has a loss tangent calculated from G'' / G'' at 25°C, where G' is the storage modulus and G'' is the loss modulus, measured according to procedure A, of 0.01 or more and 0.1 or less.
6. The adhesion prevention gel forming agent set according to claim 1 or 2, When the viscosity measured according to the procedure B immediately after preparation is defined as η1, the viscosity measured after storage at 80° C. for one week is defined as η2, and the viscosity change rate is defined as (|η2−η1| / η1)×100, The adhesion prevention gel forming agent set, wherein the viscosity change rate of the first agent is 0% or more and 10% or less, and the viscosity change rate of the second agent is 0% or more and 10% or less.
7. The adhesion prevention gel forming agent set according to claim 1 or 2, An adhesion prevention gel forming agent set, wherein the compound having two or more hydroxyl groups in the first agent includes one or more selected from the group consisting of monosaccharides, polysaccharides, low molecular weight alcohols, and water-soluble polymer alcohols.
8. The adhesion prevention gel forming agent set according to claim 1 or 2, The adhesion preventing gel forming agent set, wherein the polymer in the second agent contains a (meth)acrylate group in the molecule.
9. The adhesion prevention gel forming agent set according to claim 1 or 2, The adhesion preventing gel forming agent set, wherein the polymer in the second agent comprises a polymer having a skeleton represented by the following general formula (1): 【Chemistry 1】 (In the above general formula (1), R 1 represents a hydrogen atom, a methyl group, or an ethyl group; R 2 represents an alkyl group having 2 to 12 carbon atoms or an oxyethylene group; R 3 represents an alkyl group having 2 to 4 carbon atoms, X represents a single bond, a phenyl group which may have a substituent, or a group represented by -C(O)-, -C(O)O-, -O-, -C(O)NH- or -S-, A represents a hydrogen atom, a halogen atom or any organic substituent, and n, m and l represent, respectively, 0.01 to 0.99, 0.01 to 0.99 and 0 to 0.98 (with the proviso that the sum of n, m and l is 1.00).
10. The adhesion prevention gel forming agent set according to claim 1 or 2, the weight average molecular weight of the compound having two or more hydroxyl groups in the first agent is 10,000 or more and 50,000 or less, and / or The weight average molecular weight of the polymer in the second agent is 10,000 or more and 32,000 or less. Anti-adhesion gel forming agent set.
11. An adhesion prevention gel-forming kit comprising the adhesion prevention gel forming agent set according to claim 1 or 2 and a spray device.
Citation Information
Patent Citations
Material for preventing tissue adhesion and material for preventing joint contracture
WO2009066746A1