Concentration method and concentration system for raw material liquid
By using a branched polymer inducing solute with specific molecular weight, the method addresses contamination issues in forward osmosis membrane concentration, achieving high flux and reduced solute mixing in organic solvent-rich raw material liquids.
Patent Information
- Application Number
- JP2024054112
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-12-22
- Filing Date
- 2024-03-28
- Publication Date
- 2024-10-11
AI Technical Summary
Conventional methods for concentrating organic solvent-rich raw material liquids using forward osmosis membranes face challenges in minimizing contamination of the inducing solute into the raw material solution, particularly when high flux is required.
The use of a specific inducing solute with a branched polymer structure and molecular weight between 30 and 100, which is easily blocked by the membrane, is employed to reduce contamination and enhance flux during concentration.
This approach effectively reduces the contamination of the inducing solute into the raw material liquid while maintaining high flux, allowing for efficient concentration of valuable substances.
Smart Images

Figure 2024144379000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method and a system for concentrating a raw material liquid. [Background technology]
[0002] In various industries, a raw material liquid rich in an organic solvent containing valuable substances is sometimes concentrated. When it is necessary to concentrate the valuable substances without deteriorating them, concentration using a forward osmosis membrane is particularly useful because it does not require the application of heat or pressure.
[0003] When a feed liquid rich in organic solvents containing valuable substances is concentrated using a forward osmosis membrane, the feed liquid may become contaminated with the inducer solute depending on the selection of the inducer solute. To minimize the inclusion of the inducer solute, it is necessary to select an inducer solute that is easily rejected by the membrane and can complete the concentration in a short time. To complete the concentration of the feed liquid in a short time, it is required that the flux during concentration is high, that is, the amount of liquid passing through per unit area of membrane is high. Also, polymeric inducers are often used in the hope that they will be easily rejected by the membrane. For example, Patent Document 1 discloses an example of concentrating methanol using a forward osmosis membrane with PEG-2000 as a leading solute, but does not disclose PEG-2000 mixed in the methanol. Furthermore, for example, Non-Patent Document 1 discloses an example in which levofloxacin is concentrated in acetone, which is a raw material liquid, using a forward osmosis membrane with PEG-400 as a leading solute. Furthermore, Non-Patent Document 1 discloses that PEG-400 was mixed into the raw material solution (reverse solute flux). [Prior art documents] [Patent documents]
[0004] [Patent Document 1] International Publication No. 2022 / 004738 [Non-patent literature]
[0005] [Non-Patent Document 1] Keng Siang Goh, Yunfeng Chen, Daniel Yee Fan Ng, Jia Wei Chew, Rong Wang,Journal of Membrane Science 642 (2022) 119965 Summary of the Invention [Problem to be solved by the invention]
[0006] However, according to the inventors' investigations, when concentrating a raw solution rich in organic solvent, it is difficult to keep the incorporation of the lead solute into the raw solution within a suitable range using conventional methods, and even the method described in Non-Patent Document 1 leaves room for improvement.
[0007] The present invention aims to solve the above problems and provide a raw material liquid concentrating method and a raw material liquid concentrating system that reduce the inclusion of a lead solute in a raw material liquid when a raw material liquid rich in an organic solvent is used. [Means for solving the problem]
[0008] The present invention includes the following aspects. [Item 1] A method for concentrating a raw material liquid, comprising the steps of: The method includes a concentration step of contacting a feed liquid with a derivative liquid through a forward osmosis membrane, The raw material liquid contains a valuable material and a solvent, the solvent comprises an organic solvent, the draw solution comprises a draw solute; The method for concentrating a raw material liquid, wherein the draw solute satisfies the following (1) and (2): (1) A polymer containing at least three repeating units with a molecular weight of 30 to 100. (2) The polymer has a branched structure in which atoms (atomic groups) other than hydrogen atoms and halogen atoms are bonded to the main chain. [Item 2] 2. The method for concentrating a raw material liquid according to item 1, wherein the concentration of the organic solvent in the solvent is 50% by mass or more. [Item 3] 2. The method for concentrating a raw material liquid according to item 1, wherein a concentration of the organic solvent in the solvent is 80% by mass or more. [Item 4] 4. The method for concentrating a raw material liquid according to any one of items 1 to 3, wherein the weight average molecular weight of the derivative solute is 300 Da or more and 2300 Da or less. [Item 5] 4. The method for concentrating a raw material liquid according to any one of items 1 to 3, wherein the weight average molecular weight of the derivative solute is 400 Da or more and 1000 Da or less. [Item 6] The solvent comprises an organic solvent and water; 6. The method for concentrating a raw material liquid according to any one of items 1 to 5, wherein the solubility of water in the draw solute is 2% by mass or more. [Item 7] The solvent comprises an organic solvent and water; 6. The method for concentrating a raw material liquid according to any one of items 1 to 5, wherein the solubility of the draw solute in water is 6% by mass or more. [Item 8] 8. The method for concentrating a raw material liquid according to any one of items 1 to 7, wherein the forward osmosis membrane is in the form of a hollow fiber. [Item 9] The forward osmosis membrane has a substrate layer and an active layer, 9. The method for concentrating a raw material solution according to any one of items 1 to 8, wherein the base layer comprises one or more polymers selected from the group consisting of polysulfone, polyethersulfone, polyvinylidene fluoride, polyacrylonitrile, polyethylene, polypropylene, a cellulose-based polymer, polyketone, polyamide, polyimide, polyetheretherketone, and polybenzimidazole. [Item 10] 10. The method for concentrating a raw material liquid according to item 9, wherein the active layer of the forward osmosis membrane comprises polyamide. [Item 11] Pure water was placed on the active layer side as a raw liquid, and a 3.5 mass% aqueous sodium chloride solution was placed on the base layer side as a deriving liquid. The base layer side was set to the positive side, and the raw liquid and the deriving liquid were passed through while being pressurized to 20 kPa. After 20 minutes, the forward osmosis membrane was evaluated. The RSF of the derived solute (g / (m 2 × hr) into the draw solution. 2 11. The method for concentrating a raw material liquid according to item 9 or 10, wherein RSF / water flux (salt selectivity) divided by RSF / hour (salt selectivity) is 0.05 g / kg or more and 1.00 g / kg or less. [Item 12] Item 12. The method for concentrating a raw material liquid according to item 11, wherein the salt selectivity is 0.10 g / kg or more and 0.90 g / kg or less. [Item 13] 13. The method for concentrating a raw material liquid according to any one of items 1 to 12, wherein the valuable material is a drug, an active pharmaceutical ingredient, a development pipeline (a candidate compound for a medical drug), or an intermediate or raw material thereof. [Item 14] 14. The method for concentrating a raw material liquid according to any one of items 1 to 13, wherein the valuable substance is a compound having a weight average molecular weight of 100 to 3,000,000. [Item 15] 15. The method for concentrating a raw material liquid according to any one of items 1 to 14, wherein the valuable product is a cosmetic product, a functional chemical product, or a raw material thereof. [Item 16] A raw material liquid concentrating system for concentrating a raw material liquid, comprising: the feed liquid concentration system includes a forward osmosis membrane module configured to receive the feed liquid and the derivative liquid and to allow the feed liquid and the derivative liquid to come into contact with each other via a forward osmosis membrane; The raw material liquid contains a valuable material and a solvent, the solvent comprises an organic solvent, The draw solution comprises a draw solute; A raw material liquid concentrating system, wherein the induced solute satisfies the following (1) and (2). (1) A polymer containing at least three repeating units with a molecular weight of 30 to 100. (2) The polymer has a branched structure in which atoms (atomic groups) other than hydrogen atoms and halogen atoms are bonded to the main chain. [Item 17] Item 17. The raw material liquid concentrating system according to item 16, wherein the concentration of the organic solvent in the solvent is 50% by mass or more. [Item 18] Item 17. The raw material liquid concentrating system according to item 16, wherein the concentration of the organic solvent in the solvent is 80% by mass or more. [Item 19] 19. The system for concentrating a raw material liquid according to any one of items 16 to 18, wherein the weight average molecular weight of the derived solute is 300 Da or more and 2300 Da or less. [Item 20] 19. The system for concentrating a raw material liquid according to any one of items 16 to 18, wherein the weight average molecular weight of the derived solute is 400 Da or more and 1000 Da or less. [Item 21] The solvent comprises an organic solvent and water; 21. The system for concentrating a raw material solution according to any one of items 16 to 20, wherein the solubility of water in the draw solute is 2% by mass or more. [Item 22] The solvent comprises an organic solvent and water; 21. The system for concentrating a raw material solution according to any one of items 16 to 20, wherein the solubility of water in the draw solute is 6% by mass or more. [Item 23] 23. The raw material liquid concentrating system according to any one of items 16 to 22, wherein the forward osmosis membrane is in the form of a hollow fiber. [Item 24] The forward osmosis membrane has a substrate layer and an active layer, 24. The raw material solution concentrating system according to any one of items 16 to 23, wherein the base layer comprises one or more polymers selected from the group consisting of polysulfone, polyethersulfone, polyvinylidene fluoride, polyacrylonitrile, polyethylene, polypropylene, cellulose-based polymers, polyketones, polyamides, polyimides, polyetheretherketones, and polybenzimidazoles. [Item 25] 25. The feedstock liquid concentrating system according to item 24, wherein the active layer of the forward osmosis membrane comprises polyamide. [Item 26] 26. The system for concentrating a raw material liquid according to any one of items 16 to 25, wherein the valuable substance is a compound having a weight-average molecular weight of 100 to 3,000,000. [Item 27] 27. The raw material liquid concentrating system according to any one of items 16 to 26, wherein the valuable material is a pharmaceutical product, a cosmetic product, or a functional chemical product, or a raw material thereof. [Item 28] 1. A method for removing organic solvents from a solution, comprising the steps of: The method includes contacting the solution with a draw solution through a forward osmosis membrane; the solution comprises an organic solvent; the draw solution comprises a draw solute; The method for removing an organic solvent, wherein the derived solute satisfies the following (1) and (2): (1) A polymer containing at least three repeating units with a molecular weight of 30 to 100. (2) The polymer has a branched structure in which atoms (atomic groups) other than hydrogen atoms and halogen atoms are bonded to the main chain. [Item 29] A derivative solute for removing organic solvents by forward osmosis, which satisfies the following (1) and (2): (1) A polymer containing at least three repeating units with a molecular weight of 30 to 100. (2) The polymer has a branched structure in which atoms (atomic groups) other than hydrogen atoms and halogen atoms are bonded to the main chain. Effect of the Invention
[0009] According to one aspect of the present invention, a raw material liquid concentrating method and a raw material liquid concentrating system can be provided that reduce the inclusion of a lead solute in a raw material liquid even when a raw material liquid rich in an organic solvent is used. [Brief description of the drawings]
[0010] [Figure 1] FIG. 1 is a schematic diagram showing the mechanism of solvent transport through a forward osmosis membrane. [Diagram 2] FIG. 1 is a schematic diagram for explaining an example of the structure of a forward osmosis membrane module used in a raw material liquid concentrating method and a raw material liquid concentrating system according to one embodiment of the present invention. [Diagram 3] FIG. 1 is a schematic diagram illustrating a raw material liquid concentrating system according to one embodiment of the present invention. [Figure 4] 1 shows various measured values of a polyketone hollow fiber used in the raw material liquid concentrating method of the present embodiment. [Diagram 5] Electron microscope images of polyketone hollow fibers used in the feedstock liquid concentrating method of the present embodiment: (a) an electron microscope image of the inner diameter surface of a polyketone hollow fiber, (b) an electron microscope image of the outer diameter surface of a polyketone hollow fiber, (c) an electron microscope image at low magnification of a cross section of a polyketone hollow fiber, (d) an electron microscope image of a cross section in the vicinity of the inner diameter surface of a polyketone hollow fiber, and (e) an electron microscope image at high magnification of a cross section of a polyketone hollow fiber in the vicinity of the inner diameter surface. [Figure 6] FIG. 1 is a flow diagram of a membrane under pressure test apparatus. [Figure 7] FIG. 1 is a schematic diagram of an interfacial polymerization apparatus and experimental procedure. [Figure 8] (a) X-ray photoelectron spectroscopy data on the inner surfaces of a polyketone hollow fiber and a forward osmosis membrane, respectively, and (b) ATR-FTIR data on the inner surfaces of a polyketone hollow fiber and a forward osmosis membrane, respectively. [Figure 9] Electron microscope images of the inner surface of a forward osmosis membrane. (a) Electron microscope image of the inner diameter surface of a forward osmosis membrane, (b) Electron microscope image at high magnification of the inner diameter surface of a forward osmosis membrane, (c) Electron microscope image of a cross section near the inner diameter surface of a forward osmosis membrane, and (d) Electron microscope image at high magnification of a cross section near the inner diameter surface of a forward osmosis membrane. [Figure 10] 1 is a graph showing the performance of a forward osmosis membrane module under pressure testing. [Figure 11] FIG. 1 is a schematic diagram of a laboratory-use forward osmosis membrane evaluation device used in Reference Examples 3, 4, 5, and 6. [Figure 12] 1 is a graph showing the relationship between sucrose octaacetate (SoA) concentration and MeOH Flux. [Figure 13]1 is a graph showing the concentration of each component (SoA and PEG-400) in the feed solution (FS) in a high concentration experiment. [Figure 14] Graphs showing the results of the high concentration experiment (2). (a) The graphs showing the feed amount over time (mL) and (b) MeOH flux (Lm-2h-1). [Figure 15] 1 is a graph showing the relationship between SoA concentration and MeOH Flux. [Figure 16] 1 is a graph showing the concentration of each component (SoA and PPG-400) in the feed solution (FS) in a high concentration experiment. [Figure 17] Graphs showing the results of the high concentration experiment (2). (a) The graphs showing the feed amount over time (mL) and (b) MeOH flux (Lm-2h-1). [Figure 18] FIG. 1 is a schematic diagram of an apparatus used in Reference Example 7 for measuring the vapor pressure of MeOH necessary for calculating the osmotic pressure. [Figure 19] 1 is a graph showing the calculation results of MeOH osmotic pressure of the draw solutions used in Reference Examples 3, 4, 5 and 6. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] <<Method and system for concentrating raw material liquid>> The present inventors have experimentally clarified that, when concentrating a raw material solution rich in an organic solvent, the draw solutes disclosed in the prior art are not suitable from the viewpoint of suppressing the contamination of the raw material solution by the draw solute, although the reason is unclear. The present inventors have found that a polymer having a specific molecular weight and branched structure is suitable for reducing contamination by the draw solute in the concentration using a forward osmosis membrane, and have completed the present invention. The present inventors conducted further studies and found that by using a specific inducer solute, a high flux can be achieved in concentrating a raw material solution rich in an organic solvent, thereby completing the present invention. The present inventors conducted further studies and found that in concentrating an organic solvent-rich raw liquid when the organic solvent contains water, the use of a specific inducer solute makes it possible to remove water (dehydrate) from the raw liquid at a high water flux, thereby obtaining a concentrated raw liquid, thereby completing the present invention. In this disclosure, removing water from the raw material liquid (dehydration) is described as part of concentration.
[0012] One aspect of the present invention provides a method for concentrating a feedstock liquid, comprising the step of contacting the feedstock liquid with a derivative liquid via a forward osmosis membrane. Another aspect of the present invention provides a system for concentrating a feed liquid. In one aspect, the system includes a forward osmosis membrane module configured to receive a feed liquid and a draw liquid and to contact the feed liquid and the draw liquid through a forward osmosis membrane. In the method or system according to one aspect of the present invention, the raw material liquid includes a valuable substance and a solvent. In one aspect, the solvent includes an organic solvent. In one aspect, the solvent includes water. In one aspect, the solvent includes an organic solvent and water. The draw solution, in one embodiment, comprises a draw solute. The draw solution, in one embodiment, comprises a solvent for the draw solute. The draw solution, in one embodiment, comprises a draw solute and a solvent for the draw solute. The derivatizing solute is in one embodiment a polymer, and in one embodiment has a branched structure. According to the raw material liquid concentrating method and raw material liquid concentrating system of the present embodiment, a high flux is achieved when concentrating a raw material liquid rich in an organic solvent, so that contamination of the raw material liquid with the draw solute can be reduced.
[0013] <Raw material liquid> The raw material liquid to be concentrated by the raw material liquid concentrating method and raw material liquid concentrating system of this embodiment is a solution or dispersion containing at least a valuable substance and a solvent. Examples of the raw material liquid include food, pharmaceuticals, seawater, and produced water discharged from gas fields, oil fields, and the like. However, considering the advantage of this embodiment that concentration is possible without the need for heating, the raw material liquid concentration according to this embodiment is effectively applied to raw material liquids that contain substances that are likely to decompose when heated, particularly pharmaceuticals, cosmetics, functional chemicals, etc., or their raw materials, as valuable resources, and among these, raw material liquids that contain pharmaceuticals or their raw materials.
[0014] The temperature of the raw material liquid to be subjected to the raw material liquid concentration according to this embodiment is preferably adjusted to a range of 1°C or more and 50°C or less.
[0015] [Valuables] In this disclosure, valuables refer to tangible objects in general that have economic value. In one embodiment, valuables are pharmaceuticals, drug substances, development pipelines (medical drug candidate compounds), and intermediates thereof. In one embodiment, valuables are cosmetics and functional chemicals, as well as raw materials and intermediates thereof. Typically, the valuables are one or more selected from pharmaceuticals, active pharmaceutical ingredients, development pipelines (medical drug candidate compounds), cosmetics, functional chemicals, and raw materials and intermediates thereof.
[0016] In this disclosure, a drug substance refers to a substance (active ingredient) that has a pharmacological effect at the stage of the final product (e.g., drug product and formulation), and is used as a raw material for manufacturing drug products. In this disclosure, a development pipeline (e.g., a medical drug candidate compound) refers to a drug candidate compound that has passed from the research and development stage through clinical trials (clinical trials) to being sold as a drug, and is also called a new drug candidate. Compounds that have passed through the development phases (Phase I, Phase II, and Phase III) of clinical trials from the search for new compounds are sold as drugs after approval. The development pipeline in this disclosure may be a compound at any development stage (phase) before being approved as a drug. The company's drug substances and development pipeline include small molecule drugs, nucleic acid drugs, peptide drugs, and other medium molecule drugs; antibody drugs, protein drugs, and other polymer drugs; antibody drug conjugates (ADCs), which are small molecule drugs bound to antibodies; and derivatives of these. Drug substances and development pipelines are manufactured by processes such as chemical synthesis, fermentation, or extraction, or a combination of these processes.
[0017] In this disclosure, an intermediate refers to a substance produced in an intermediate step in the manufacture of a drug substance or a development pipeline, which becomes a drug substance or a development pipeline through further manufacturing steps. Examples of intermediates include a drug substance starting material that is incorporated as an important component in the structure of a drug substance, a key intermediate in which at least one essential molecular feature (a specific stereochemical structure or pharmacological activity) has been introduced into the molecular structure, and a final intermediate from which a drug substance is produced by carrying out one more reaction.
[0018] In this disclosure, raw materials refer to substances used in the manufacture of drug substances and development pipelines, and chemical species or mixtures containing chemical species not contained in the drug substances and development pipelines. Examples of raw materials include, but are not limited to, starting materials for the manufacture of drug substances and development pipelines, as well as one or more of catalysts, unrefined drug substances, and development pipelines.
[0019] In one aspect, the valuables include, for example, amino acids, peptides, proteins, sugars, vaccines, nucleic acids, antibiotics, vitamins, natural products, and synthetic raw materials and intermediates called "building blocks," as well as derivatives thereof.
[0020] Amino acids include essential amino acids, non-essential amino acids, and non-naturally occurring amino acids. Essential amino acids include, for example, tryptophan, lysine, methionine, phenylalanine, threonine, valine, leucine, isoleucine, etc. Non-essential amino acids include, for example, arginine, glycine, alanine, serine, tyrosine, cysteine, asparagine, glutamine, proline, aspartic acid, glutamic acid, etc.
[0021] In this disclosure, a non-natural amino acid refers to any artificial compound that does not occur in nature and has an amino acid backbone in the same molecule, and can be synthesized by attaching various labeling compounds to the amino acid backbone. In the present disclosure, the "amino acid backbone" includes the carboxyl group, the amino group in the amino acid, and the moiety connecting them. In this disclosure, "label compound" refers to dye compounds, fluorescent substances, chemi / bioluminescent substances, enzyme substrates, coenzymes, antigenic substances, and protein binding substances known to those skilled in the art. An example of an unnatural amino acid is a "labeled amino acid" that is an amino acid bound to a labeling compound. An example of a labeled amino acid is an amino acid having an amino acid skeleton containing an aromatic ring such as a benzene ring in the side chain, to which a labeling compound is bound. Examples of unnatural amino acids to which a specific function has been imparted include photoresponsive amino acids, photoswitch amino acids, fluorescent probe amino acids, and fluorescently labeled amino acids.
[0022] In the present disclosure, a peptide refers to a compound in which 2 or more and less than 70 amino acid residues are bound, and may be linear or cyclic, or may have a branched structure. Examples of peptides include L-alanyl-L-glutamine, β-alanyl-L-histidine cyclosporine, and glutathione.
[0023] In the present disclosure, a protein generally refers to a compound consisting of linked amino acid residues that has a longer chain length than a peptide. The protein is preferably one that is applied as a protein preparation, for example, interferon α, interferon β, interleukin 1 to 12, growth hormone, erythropoietin, insulin, granulocyte-colony stimulating factor (G-CSF), tissue plasminogen activator (TPA), natriuretic peptide, blood coagulation factor VIII, somatomedin, glucagon, growth hormone releasing factor, serum albumin, calcitonin, etc.
[0024] Examples of sugars include monosaccharides (e.g., glucose, fructose, galactose, mannose, ribose, deoxyribose, etc.), disaccharides (e.g., maltose, sucrose, lactose, etc.) and sugar chains (e.g., glucose, galactose, mannose, fucose, xylose, glucuronic acid, iduronic acid, etc.; sugar derivatives such as N-acetylglucosamine, N-acetylgalactosamine, N-acetylneuraminic acid, glucose 5-acetate, etc.).
[0025] Vaccines include, for example, Hepatitis A vaccine, Hepatitis B vaccine, Hepatitis C vaccine, and COVID-19 vaccine; Examples of nucleic acids include oligonucleotides, RNA, aptamers, and decoys; Antibiotics include, for example, streptomycin and vancomycin; Each of them can be mentioned.
[0026] Examples of vitamins include vitamin A, vitamin B, and vitamin C, including their derivatives and salts, etc. Examples of vitamin B include vitamin B6 and vitamin B12.
[0027] In one aspect, the cosmetic product or its raw material disclosed herein is a compound or a modified compound thereof listed in the List of Quasi-Drug Additives issued by the Ministry of Health, Labor and Welfare (more specifically, the partial amendment of the PSEHB / PDA Notification No. 0325-7 dated March 25, 2021, "Regarding the List of Quasi-Drug Additives"), and examples of such compounds include paraffin, sodium benzoate, oleic acid, and hydrolyzed collagen.
[0028] The functional chemical products or raw materials thereof in the present disclosure refer to various chemical species, or their modified products, precursors, raw materials, etc. Examples of functional chemical products or raw materials thereof include chemical species such as metal nanoparticles, semiconductor nanoparticles, metal colloids, nanodiamonds, porous nanoclays, metal organic frameworks (MOFs), carbon nanotubes, fullerenes, graphene, graphene oxide, carbon nanohorns, cellulose nanofibers, etc., as well as their modified products, precursors, raw materials, etc.
[0029] The weight average molecular weight of the valuable material is preferably 100 to 3,000,000, or 100 to 500,000, or 100 to 50,000, or 100 to 30,000. When the molecular weight of a valuable substance is relatively small (for example, when the molecular weight is 1500 or less), the weight average molecular weight can be determined by calculation from the chemical formula of the valuable substance. On the other hand, when the weight average molecular weight of the valuable material is relatively large (for example, when the molecular weight exceeds 1500), the weight average molecular weight can be determined as the weight average molecular weight converted into polyethylene glycol by GPC.
[0030] [Yield of valuable materials] According to the concentration of the raw material liquid according to the present embodiment, the yield of valuable substances can be, for example, 70% or more, 80% or more, 90% or more, 95% or more, or 99% or more. The yield of valuable substances is ideally 100%, but from the viewpoint of practical process efficiency, in one embodiment, it may be 99.99% or less, or 99.9% or less. In this disclosure, the yield of valuable materials refers to the value obtained by dividing the total mass of valuable materials obtained by the feedstock liquid concentration according to this embodiment by the total mass of valuable materials used in the feedstock liquid concentration (specifically, supplied to the forward osmosis membrane module), expressed as a percentage. The yield can be determined by mass measurement and component analysis of the valuables before and after concentration. The component analysis method is selected from known methods depending on the type of valuables, and in one embodiment, is selected from ICP-MS (inductively coupled plasma mass spectrometry), nuclear magnetic resonance spectroscopy (NMR), gas chromatography mass spectrometry (GC / MS), colorimetry, fluorescence, and high performance liquid chromatography (HPLC).
[0031] [Solvent for raw material liquid] The raw material liquid contains a solvent (in one embodiment, an organic solvent). In the present disclosure, the solvent of the raw material liquid is a compound capable of dissolving or dispersing the valuable material and, if any, the minor component. Examples of the secondary components include inorganic salts such as lithium chloride, sodium chloride, potassium chloride, magnesium chloride, calcium chloride, sodium phosphate, potassium phosphate, sodium sulfate, magnesium sulfate, sodium thiosulfate, sodium sulfite, ammonium chloride, ammonium sulfate, and ammonium carbonate. Acids such as acetic acid, trifluoroacetic acid, hydrogen chloride, sulfuric acid, etc. Examples of bases include sodium hydroxide. In the present disclosure, an organic solvent is an organic compound having one or more carbon atoms, and in one embodiment, is a compound that exists in a liquid state at a temperature of −10° C. or higher and lower than 50° C. under normal pressure, and examples of the organic solvent include hydrophilic organic solvents and hydrophobic organic solvents. When the raw material liquid contains a hydrophilic organic solvent, it is advantageous in that a high flux can be easily achieved if the active layer of the forward osmosis membrane used is hydrophilic. In this disclosure, a hydrophilic organic solvent means an organic solvent that maintains a one-phase state when a sample containing 50 mL each of the solvent and water is stirred at 25°C for 24 hours using a φ8 mm × 25 mm stirrer tip and a magnetic stirrer.
[0032] Examples of the organic solvent include alcohols, carboxylic acids, esters, ethers, aprotic polar compounds, aromatic compounds, aliphatic compounds, chlorinated hydrocarbons, ketones, and aldehydes.
[0033] Specific examples of hydrophilic organic solvents include: Examples of alcohols include methanol, ethanol, 1-propanol, 2-propanol, normal butanol, sec-butanol, t-butanol, and hexafluoroisopropyl alcohol; Ethers, for example, tetrahydrofuran (THF), 2-methyltetrahydrofuran, 1,4-dioxane, diethylene glycol dimethyl ether, 1,2-dimethoxyethane, etc.; Aprotic polar compounds include, for example, acetonitrile, N,N-dimethylformamide, dimethylacetamide, N-methylpyrrolidone, dimethylsulfoxide, nitromethane, sulfolane, and the like; Aromatic compounds include, for example, pyridine; Ketones, for example, acetone, methyl ethyl ketone, etc.; Aldehydes include, for example, formaldehyde, acetaldehyde, propionaldehyde, butanal, acrolein, benzaldehyde, furfural, vanillin, etc.; Each of them can be mentioned.
[0034] The organic solvent may be one solvent or a combination of two or more solvents, and is preferably at least one selected from the group consisting of tetrahydrofuran, 2-methyltetrahydrofuran, 1,4-dioxane, methanol, ethanol, 1-propanol, 2-propanol, acetonitrile, N,N-dimethylformamide, dimethylacetamide, N-methylpyrrolidone, dimethylsulfoxide, sulfolane, chloroform, acetone, methylbutylketone, and pyridine. Examples of combinations of two or more organic solvents include a combination of tetrahydrofuran (THF) and methanol, a combination of tetrahydrofuran (THF) and ethanol, and the like. For example, the combination may be one in which the mass ratio of tetrahydrofuran (THF) and methanol is 1:1.
[0035] The raw material liquid may also contain a solvent that is not an organic solvent. For example, the raw material liquid may contain one or more organic solvents and water (in one embodiment, pure water) as a non-organic solvent. For example, the mass ratio of the organic solvent (the total when two or more kinds are used) to water may be 99:1 to 90:10, or 90:10 to 80:20, or 80:20 to 70:30, or 51:49. More typical examples include combinations in which the mass ratio of tetrahydrofuran (THF) to water is 95:5, or 88:12, or 80:20, or 51:49.
[0036] When the feed solution contains a hydrophobic organic solvent, it is advantageous in that a high flux can be easily achieved if the active layer of the forward osmosis membrane used is hydrophobic. In this disclosure, a hydrophobic organic solvent refers to an organic solvent that maintains a two-phase state when a sample containing 50 mL each of the solvent and water is stirred at 25°C for 24 hours using a φ8 mm × 25 mm stirrer tip and a magnetic stirrer.
[0037] Hydrophobic organic solvents include: Alcohols such as pentanol, hexanol, heptanol, etc.; Carboxylic acids include oleic acid, stearic acid, linoleic acid, palmitic acid, etc.; Aromatic hydrocarbons, such as toluene, xylene, ethylbenzene, cumene, isopropylbenzene, and triisopropylbenzene; Aliphatic hydrocarbons such as normal hexane, normal heptane, isooctane, cyclohexane, methylcyclohexane, and decahydronaphthalene; Ethers such as dimethyl ether, diethyl ether, diisopropyl ether, methyl tert-butyl ether, methyl cyclopentyl ether, etc.; Esters include methyl formate, ethyl formate, methyl acetate, ethyl acetate, isopropyl acetate, n-butyl acetate, t-butyl acetate, etc.; etc.
[0038] In one embodiment, the concentration of the organic solvent in the solvent of the raw material liquid is 50% by mass or more, preferably 60% by mass or more, 70% by mass or more, 80% by mass or more, or 90% by mass or more. The concentration may be, for example, 99.9% by mass or less, 99% by mass or less, or 98% by mass or less. In the present disclosure, a raw material liquid rich in an organic solvent means that the concentration of the organic solvent in the raw material liquid is 50% by mass or more.
[0039] <Inducing liquid> The draw solution used in the method of the present embodiment contains a draw solute. The draw solution used in the method of the present embodiment may contain a solvent for the draw solute. In one embodiment, the draw solution comprises a draw solute and a solvent for the draw solute.
[0040] [Induced solute] The inducer solute of the present embodiment satisfies the following requirements (1) and (2). Requirement (1): A polymer containing at least three repeating units with a molecular weight of 30 to 100. Requirement (2): The polymer satisfying requirement (1) has a branched structure in which atoms (atomic groups) other than hydrogen atoms and halogen atoms are bonded to the main chain. In one aspect, the inducer solute of the present embodiment satisfies the following requirements (1) and (2). Requirement (1): A polymer containing at least three repeating units with a molecular weight of 30 to 100. Requirement (2): The polymer satisfying requirement (1) has a branched structure in which atoms (substituents) other than hydrogen atoms and halogen atoms are bonded to the main chain.
[0041] In one embodiment, a "polymer" as used herein as a derivative solute comprises at least 3 to 100 repeat units, preferably 4 to 50, having a molecular weight of 30 to 100. In one embodiment, the "molecular weight of a polymer" used as a derivative solute in the present disclosure is preferably a weight average molecular weight of 200 Da or more and 5000 Da or less, more preferably a weight average molecular weight of 300 Da or more and 2300 Da or less, and even more preferably a weight average molecular weight of 400 Da or more and 1000 Da or less. The weight average molecular weight of the derivative solute of this embodiment is preferably 200 Da or more, or 300 Da or more, or 400 Da or more, or 500 Da or more, or 600 Da or more, or 700 Da or more, or 800 Da or more, or 900 Da or more, or 1000 Da or more, or 1100 Da or more, or 1200 Da or more, or 1300 Da or more, or 1400 Da or more, or 1500 Da or more, or 1600 Da or more, or 1700 Da or more, or 1800 Da or more, or 1900 Da or more, or 2000 Da or more. The weight average molecular weight of the derivative solute of this embodiment is preferably 5000 Da or less, or 4900 Da or less, or 4800 Da or less, or 4700 Da or less, or 4600 Da or less, or 4500 Da or less, or 4400 Da or less, or 4300 Da or less, or 4200 Da or less, or 4100 Da or less, or 4000 Da or less, or 3900 Da or less, or 3800 Da or less, or 3700 Da or less. Da or less, or 3600 Da or less, or 3500 Da or less, or 3400 Da or less, or 3300 Da or less, or 3200 Da or less, or 3100 Da or less, or 3000 Da or less, or 2900 Da or less, or 2800 Da or less, or 2700 Da or less, or 2600 Da or less, or 2500 Da or less, or 2400 Da or less, or 2300 Da or less, or 1000 Da or less. The weight average molecular weight of the derivatizing solute is preferably in the above range, from the viewpoints of handling problems due to high viscosity if the derivatizing solute is a liquid polymer, and of solubility problems if the derivatizing solute is a solid polymer.
[0042] In one embodiment, the term "polymer having a branched structure" used as a derivative solute in the present disclosure means a structure in which one or more atoms (atomic groups) other than hydrogen atoms and halogen atoms are bonded to the main chain of the polymer. In one embodiment, the atomic group may be a group attached to the main chain, for example, a group containing a hydroxyl group or a hydrocarbon group. The atomic group is preferably a hydroxyl group or a hydrocarbon group, and more preferably a hydrocarbon group.
[0043] Examples of the derivative solute, which is a "polymer having a specific branched structure" in this embodiment, include polypropylene glycol (PPG), polysorbate, polybutylene glycol, and polyvinyl alcohol. Among these, tripropylene glycol, PPG-400, PPG-700, PPG-1000, PPG-2000, PPG-3000, and PPG-4000 are preferably used as the inducer solute of this embodiment. By satisfying the requirements (1) and (2), the incorporation of the draw solute into the raw solution is suppressed, and a high flux is achieved in the concentration of the organic solvent-rich raw solution.
[0044] The concentration of the draw solute in the draw liquid may be appropriately set depending on the composition of the feed liquid, the type of the draw solute in the draw liquid, etc., so as to ensure the transfer of the organic solvent from the feed liquid to the draw liquid and to generate an osmotic pressure difference capable of generating a driving force within a range in which the composition of the feed liquid in the vicinity of the forward osmosis membrane does not change suddenly, but generally a higher concentration is desirable. The concentration is preferably 10% by mass or more, or 20% by mass or more, or 50% by mass or more, and in one preferred embodiment is 100% by mass, but in one embodiment may be 90% by mass or less, or 80% by mass or less. The deriving solution may contain, in addition to the deriving solutes exemplified above, an organic solvent, particularly a hydrophilic organic solvent, as a solvent for the deriving solute. The hydrophilic organic solvent may be the same as the hydrophilic organic solvents exemplified above in the raw material solution, and may be, for example, one or more selected from the group consisting of tetrahydrofuran, 2-methyltetrahydrofuran, ethanol, etc. In one embodiment, the organic solvent is desirably the same as the organic solvent that is the main component of the raw material liquid, from the viewpoint of maintaining the properties of the raw material liquid. In the present disclosure, the organic solvent that is the main component of the raw material liquid refers to an organic solvent whose concentration in the raw material liquid is 50% by mass or more. It is preferable that the draw solute is in a liquid state at room temperature, since the draw solute itself can be used as the draw liquid and the draw solute can be mixed quickly even when a high concentration draw liquid is prepared.
[0045] [Solubility of derivative solute in water] The raw liquid after concentration with the inducer is generally expected to be further refined by a process such as crystallization. From the viewpoint of facilitating the increase in the purity of valuable substances by washing with water during the refinement of the raw liquid, it is desirable for the solubility of the inducer solute in water to be as high as possible. In one aspect, the solubility of the derived solute in water is preferably 1% by weight or more, or 3% by weight or more, or 5% by weight or more, or 7% by weight or more, or 10% by weight or more, or 15% by weight or more, or 20% by weight or more, or 30% by weight or more, or 40% by weight or more, or 50% by weight or more, or 60% by weight or more, or 70% by weight or more, or 80% by weight or more, or 90% by weight or more. The solubility of the derivative solute in water is preferably 7% by mass or more, and more preferably 10% by mass or more. The solubility of the derived solute in water is measured by the method described in the Examples.
[0046] When a concentrated raw liquid is obtained by removing water from the raw liquid (with dehydration), the more hydrophilic the derived solute is, the higher the water flux at which the derived solute can remove water. The water flux refers to the amount of water that permeates the membrane (in one embodiment, the amount of water that permeates). The degree of hydrophilicity of the derived solute can be evaluated by the solubility of the derived solute in water.
[0047] [Water solubility for derivative solute] The solubility of water in a solute can be measured as the water content of the solute when pure water is dropped onto 100 g of the solute at 25°C and two phases are formed. The solubility of water in the derived solute is preferably 90% by mass or more, 80% by mass or more, 70% by mass or more, 60% by mass or more, 50% by mass or more, 40% by mass or more, 30% by mass or more, 25% by mass or more, 6% by mass or more, 2% by mass or more, or 1% by mass or more. The solubility of the derived solute in water is preferably 2% by mass or more, and more preferably 6% by mass or more. The solubility of water in the derived solute is measured by the method described in the Examples.
[0048] [Solvent for derivative solute] The draw solution used in the method of the present embodiment may contain a solvent for the draw solute. In the present disclosure, a solvent for a derivatizing solute is a compound that can dissolve or disperse the derivatizing solute. The solvent for the derivatizing solute can be one solvent or a combination of two or more solvents. The solvent for the derived solute may be the same as that contained in the raw material liquid, or may be the above-mentioned hydrophilic organic solvent or hydrophobic organic solvent. The solvent for the derived solute is preferably at least one selected from the group consisting of tetrahydrofuran (THF), ethyl acetate, toluene, methyl-tert-butyl ether, triisopropylbenzene, cyclohexane, methylcyclohexane, normal hexane, normal heptane, isooctane, and decahydronaphthalene. Examples of combinations of two or more solvents include a combination of methylcyclohexane and normal hexane, a combination of methylcyclohexane and isooctane, and the like. For example, the combination may be one in which the mass ratio of methylcyclohexane to normal hexane is 1:1.
[0049] The concentration of the solvent of the draw solute in the draw liquid may be appropriately set depending on the composition of the feed liquid, the type of the draw solute in the draw liquid, etc., so as to ensure the transfer of the organic solvent from the feed liquid to the draw liquid and to generate an osmotic pressure difference capable of generating a driving force within a range in which the composition of the feed liquid in the vicinity of the forward osmosis membrane does not change suddenly, but generally a low concentration is preferable. The concentration is preferably 10% by mass or less, or 20% by mass or less, or 50% by mass or less, and in one preferred embodiment is 0% by mass, but in one embodiment it may be 90% by mass or more, or 80% by mass or more.
[0050] <Forward osmosis membrane and forward osmosis membrane module> Next, a forward osmosis membrane and a forward osmosis membrane module that can be applied to the raw material liquid concentrating method or raw material liquid concentrating system of this embodiment will be described.
[0051] [Forward osmosis membrane] Fig. 1 is a schematic diagram showing the mechanism of solvent movement through a forward osmosis membrane. Referring to Fig. 1, a feed liquid (a) flows on one side of a forward osmosis membrane (120), and a draw liquid (d) having a higher osmotic pressure than the feed liquid (a) flows on the other side, and both liquids are in contact with each other through the forward osmosis membrane (120). At this time, the solvent (b) in the feed liquid (a) passes through the forward osmosis membrane (120) and moves into the draw liquid (d) using the osmotic pressure difference between the feed liquid (a) and the draw liquid (d) as a driving force.
[0052] 1, the forward osmosis membrane (120) has a base layer (121) and an active layer (122) formed on one side of the base layer (121). The active layer (122) has a very dense structure that allows small molecules to pass through but not valuable substances to pass through, and is formed on the surface of the base layer (121) that comes into contact with the raw material liquid (a).
[0053] In the forward osmosis method, the driving force for the movement of the solvent (b) from the feed liquid (a) to the draw liquid (d) is the osmotic pressure difference between the feed liquid (a) and the draw liquid (d). Therefore, it is necessary to refresh the liquid at the interface between the active layer (122) of the forward osmosis membrane (120) and the feed liquid (a) and at the interface between the base layer (121) of the forward osmosis membrane (120) and the draw liquid (d). Therefore, it is necessary to flow the feed liquid (a) and the draw liquid (d) at an appropriate flow rate on both sides of the forward osmosis membrane (120). The flow rate of the raw material liquid is preferably 0.1 cm / sec or more and 8 cm / sec or less in terms of linear velocity, and may be, for example, 0.3 cm / sec or more and 6 cm / sec or less. The flow rate of the guiding liquid is preferably 0.1 cm / sec or more and 8 cm / sec or less in terms of linear velocity, and may be, for example, 0.3 cm / sec or more and 6 cm / sec or less. In FIG. 1, the raw material liquid (a) and the derivative liquid (d) are flowed in countercurrent fashion, but the flows of the two liquids may be parallel.
[0054] In one aspect, the forward osmosis membrane and the forward osmosis membrane module that can be applied to the raw material liquid concentrating method or the raw material liquid concentrating system of the present embodiment have a base material layer and an active layer.
[0055] (base material layer) A porous membrane is generally used as the material for the base layer (121). The portion of the forward osmosis membrane (120) that is the base layer (121) made of a porous membrane is permeated with the draw liquid (d), and the raw liquid (a) and the draw liquid (d) are in contact with each other via the active layer (122). In this case, the solvent in the raw liquid (a) moves to the side of the draw liquid (d) that has a higher osmotic pressure, and concentration is performed.
[0056] The form of the forward osmosis membrane may be any of the following structures: hollow fiber membrane, tubular membrane, and flat membrane. A hollow fiber membrane is preferred because it can form a flow path through which the raw material liquid and the derivative liquid pass without using a spacer or the like, and can perform uniform concentration.
[0057] The material of the porous membrane constituting the base layer can be appropriately selected from known materials, but it is appropriate that the material is not one that dissolves or swells in the organic solvent contained in the raw material liquid and cannot maintain the pore shape of the membrane. Specific examples of the material of the porous membrane constituting the base layer include polymers such as polysulfone, polyethersulfone, polyvinylidene fluoride, polyacrylonitrile, polyethylene, polypropylene, cellulose-based polymers, polyketones, polyamides, polyimides, polyetheretherketones, and polybenzimidazoles. Moreover, the material of the porous membrane constituting the base layer preferably contains one or more polymers selected from the group consisting of these polymers, or preferably contains one selected from the group consisting of these polymers as the main component (i.e., the component that is present in the largest amount in the porous membrane constituting the base layer), and more preferably contains a polyketone. The above polymer also includes a crosslinked product. As the material of the porous membrane constituting the substrate layer of the forward osmosis membrane (particularly the hollow fiber membrane), from the viewpoint of solvent resistance, a material containing at least one selected from the group consisting of polysulfone, polyethersulfone, polyketone, polyamide, and polyimide, or a material having one selected from the group consisting of these as the main component, is preferred, and among these, polyketone is particularly preferred. Polyketones are copolymers of carbon monoxide and olefins (in one embodiment, ethylene, propylene, etc.), and two or more types of olefins may be copolymerized. The molecular weight of the polyketone is not particularly limited, but from the viewpoint of ease of molding into a porous hollow fiber membrane and mechanical strength, the intrinsic viscosity is preferably 0.5 dL / g or more and 5 dL / g or less. The intrinsic viscosity of the polyketone can be measured, for example, by the method described in JP 2015-203048 A.
[0058] (active layer) In the present disclosure, when the contact angle of water on the surface of the active layer where the active layer is not in contact with the base layer is less than 90°, the active layer is hydrophilic, and when the contact angle of water is 90° or more, the active layer is hydrophobic. The active layer in the forward osmosis membrane is preferably a layer mainly composed of at least one selected from the group consisting of polysulfone, polyethersulfone, polyvinylidene fluoride, polyacrylonitrile, polyethylene, polypropylene, polyamide, cellulose acetate, etc. More preferably, the active layer mainly composed of at least one selected from the group consisting of polysulfone, polyethersulfone, polyvinylidene fluoride, polyacrylonitrile, and polyamide, even more preferably, the active layer is a layer containing polyamide, and particularly preferably, the active layer is made of polyamide. As a material for the active layer, polyamide is advantageous in that it has high permeability and high solvent resistance to the source liquid containing a hydrophilic organic solvent.
[0059] The active layer made of polyamide can be formed by carrying out interfacial polymerization of a polyfunctional acid halide and / or a polyfunctional amine on a substrate layer. A polyfunctional acid halide is an acid halide compound having two or more acid halide groups in one molecule. Halide compounds of fatty acids such as oxalic acid, malonic acid, maleic acid, fumaric acid, glutaric acid, 1,3,5-cyclohexanetricarboxylic acid, 1,3-cyclohexanedicarboxylic acid, and 1,4-cyclohexanedicarboxylic acid; Acid halide compounds of aromatic acids such as phthalic acid, isophthalic acid, 1,3,5-benzenetricarboxylic acid (trimesic acid), 1,2,4-benzenetricarboxylic acid, 1,3-benzenedicarboxylic acid, and 1,4-benzenedicarboxylic acid; These acid halide compounds may be used alone or in combination of two or more. In the present embodiment, in terms of economy, availability, ease of handling, ease of reaction, and the like, trimesoyl chloride alone, a mixture of trimesoyl chloride and isophthaloyl chloride, or a mixture of trimesoyl chloride and terephthaloyl chloride is particularly preferably used.
[0060] The polyfunctional amine is an amino compound having two or more amino groups in one molecule, and examples of the polyfunctional amine include aromatic amino compounds and aliphatic amino compounds. Specific examples of the aromatic amino compound include m-phenylenediamine, p-phenylenediamine, 3,3'-diaminodiphenylmethane, 4,4'-diaminodiphenylamine, 4,4'-diaminodiphenyl ether, 3,4'-diaminodiphenyl ether, 3,3'-diaminodiphenylamine, 3,5-diaminobenzoic acid, 4,4'-diaminodiphenyl sulfone, 3,3'-diaminodiphenyl sulfone, 3,4'-diaminodiphenyl sulfone, 1,3,5-triaminobenzene, and 1,5-diaminonaphthalene. In the present embodiment, the aromatic amino compound is preferably at least one selected from m-phenylenediamine and p-phenylenediamine in terms of economy, availability, ease of handling, ease of reaction, and the like.
[0061] Specific examples of the aliphatic amino compound include piperazine, 2,5-dimethylpiperazine, 2-methylpiperazine, 2,6-dimethylpiperazine, 2,3,5-trimethylpiperazine, 2-ethylpiperazine, 2,5-diethylpiperazine, 2,3,5-triethylpiperazine, 2-n-propylpiperazine, 2,5-di-n-butylpiperazine, ethylenediamine, and bispiperidylpropane. In the present embodiment, piperazine is particularly preferably used as the aliphatic amino compound from the standpoints of economy, ease of availability, ease of handling, ease of reaction, and the like.
[0062] These polyfunctional amines may be used alone or in combination of two or more kinds. The interfacial polymerization of the polyfunctional acid halide and the polyfunctional amine can be carried out according to a conventional method.
[0063] As a material for the active layer, a silicone-based polymer is advantageous in that it has high permeability and high solvent resistance to a source liquid containing a hydrophobic organic solvent. Silicone-based polymers include, for example, polydimethylsiloxane, polydiethylsiloxane, polydi-iso-propylsiloxane, and polydiphenylsiloxane.
[0064] The active layer may be appropriately heat-treated. This heat treatment may be performed with hot water or with high-temperature, high-pressure steam in a pressure cooker such as an autoclave. By subjecting the active layer to heat treatment, it is expected that the back diffusion of the induced solute will be reduced, although the reason is unclear.
[0065] (Mold of hollow fiber membrane) When the forward osmosis membrane is a hollow fiber membrane, the outer diameter of the hollow fiber membrane is, for example, preferably 300 μm to 5,000 μm, more preferably 350 μm to 4,000 μm, and the inner diameter of the hollow fiber membrane is, for example, preferably 200 μm to 4,000 μm, more preferably 250 μm to 1,500 μm. When the inner diameter of the hollow fiber membrane is 200 μm or more, high back pressure is unlikely to occur when liquid flows through the space inside the hollow fiber, which is preferable. When the inner diameter of the hollow fiber membrane is 4,000 μm or less, the internal volume in the module per unit membrane area does not become excessively large, which is preferable, and effective concentration is possible. In addition, when the inner diameter of the hollow fiber membrane is 4,000 μm or less, valuable materials remaining in the module can be recovered with less cleaning liquid, which is preferable. For example, in a typical spiral module, the spacer thickness is 0.84 mm. In a spiral module, the spacer thickness is 0.01 m. 2 On the other hand, if the inner diameter of the hollow fiber membrane is 488 μm, the internal volume is 8.4 mL per 0.01 m 2 The internal volume per membrane area can be calculated to be 1.2 mL. This means that valuable materials can be recovered from the module with approximately seven times less cleaning solution than with a typical spiral module.
[0066] When the forward osmosis membrane is a hollow fiber membrane, the pore size of the hollow fiber membrane is, for example, preferably 0.1 nm or more and 1000 nm or less, more preferably 0.5 nm or more and 500 nm or less, from the viewpoint of diffusion of the draw solution. When the forward osmosis membrane is a hollow fiber membrane, the porosity of the hollow fiber membrane is, for example, preferably 50% or more and 99% or less, more preferably 60% or more and 98% or less, from the viewpoint of diffusion of the draw solution. The inner diameter, outer diameter, pore size and porosity of the hollow fiber membrane can be measured by the methods described in the Examples.
[0067] [Forward osmosis membrane module] Fig. 2 is a schematic diagram for explaining an example of the structure of a forward osmosis membrane module used in a raw material liquid concentrating method and raw material liquid concentrating system according to one embodiment of the present invention. In the forward osmosis membrane module (100) of Fig. 2, a plurality of hollow fiber forward osmosis membranes (120) are housed in a housing (110). Both ends of the forward osmosis membrane (120) are adhesively fixed to the housing (110) by an adhesive resin (130). Two housing side tubes are provided on the side of the housing (110). One of these housing side tubes is a draw liquid inlet (111), and the other is a draw liquid outlet (112). The inside of the housing (110) is divided into two spaces by the outer wall of the forward osmosis membrane (120) and the adhesive resin (130): a space through which the raw liquid (a) flows and a space through which the draw liquid (d) flows. The two spaces are fluidically isolated from each other except that the solvent can pass between them via the inner wall of the forward osmosis membrane (120).
[0068] When the feed liquid (a) is introduced into one end of the forward osmosis membrane module (100), the feed liquid (a) flows inside the hollow fiber-shaped forward osmosis membrane (120) and flows out from the other end as concentrated feed liquid (c). Similarly, when the draw liquid (d) is introduced into the draw liquid inlet (111) of the side pipe of the housing (110), the draw liquid (d) flows through the outer space of the hollow fiber-shaped forward osmosis membrane (120) and flows out from the draw liquid outlet (112). As a result, the feed liquid (a) and the draw liquid (d) can come into contact with each other through the forward osmosis membrane (120). At this time, the components other than valuable materials move from the feed liquid (a) to the draw liquid (d) due to the difference in osmotic pressure between the two liquids. In the forward osmosis membrane method, concentration is performed by such a mechanism.
[0069] When the forward osmosis membrane (120) has a base layer and an active layer formed on one side of the base layer, the active layer is formed on the surface of the base layer that contacts the feed liquid, as described above. Therefore, in the forward osmosis membrane module (100) of Fig. 2 in which the feed liquid (a) flows inside the hollow fiber-shaped forward osmosis membrane, it is preferable that the active layer is formed on the inner surface of the hollow fiber-shaped base layer. When the flow rate of the feed liquid (a) and / or the flow rate of the derivative liquid (d) is high, the influence of the osmotic pressure difference on both sides of the forward osmosis membrane (120), particularly the active layer, becomes greater, and the amount of solvent permeating the forward osmosis membrane per membrane area becomes greater. In the forward osmosis membrane module (100) of Fig. 2, the feed liquid (a) and the derivative liquid (d) are flowed in countercurrent to each other, but the flow of the two liquids may be parallel.
[0070] The material of the housing (110) in the forward osmosis membrane module (100) in Fig. 2 is selected from the viewpoints of chemical resistance, pressure resistance, heat resistance, impact resistance, weather resistance, etc., so that the various performances are not deteriorated by the components contained in the feed liquid (a) and the derivative liquid (d). For example, resin, metal, etc. can be used as the material of the housing (110). From the above viewpoints, it is preferable to select the material from among resins such as polypropylene, polysulfone, polyethersulfone, polyvinylidene fluoride, polytetrafluoroethylene, perfluoroalkoxyalkane, ABS resin, fiber-reinforced plastic, and polyvinyl chloride resin; and metals such as stainless steel, brass, and titanium.
[0071] The adhesive resin (130) in the forward osmosis membrane module (100) in Fig. 2 is desirably one that has good mechanical strength. Examples of resins that can be used as the adhesive resin (130) include thermosetting epoxy resins, thermosetting urethane resins, ceramic-type adhesives, and sealing materials obtained by melting polyethylene or low-melting-point metals. From the viewpoint of heat resistance, epoxy resins are preferred, and from the viewpoint of handling, urethane resins are preferred. The forward osmosis membrane (120) may be fixed to the housing (110) by adhesive bonding according to known adhesive methods for producing hollow fiber membrane modules.
[0072] [Flux] In the concentration of the raw liquid in this embodiment, the flux, which is the amount of liquid passing through the membrane per unit area, is preferably 5 kg / m 2 / hr or more, or 10kg / m 2 / hr or more, or 12kg / m 2 / hr or more, or 15kg / m 2 / hr or more, or 18kg / m 2 / hr or more, or 20kg / m 2 / hr or more, or 25kg / m 2 / hr or more, or 30kg / m 2 / hr or more, or 35kg / m 2 / hr or more, or 40kg / m 2 / hr or more. In the present embodiment, the flux is preferably 300 kg / m 2 / hr or less, or 250kg / m 2 / hr or less, or 200kg / m 2 / hr or less, or 150kg / m 2 / hr or less, or 100kg / m 2 / hr or less. From the viewpoint of excellent efficiency in concentrating the raw material liquid, the flux is preferably 12 kg / m 2 / hr or more, more preferably 15 kg / m 2 / hr or more, more preferably 18 kg / m 2 / hr or more. The flux is preferably 12 kg / m 2 / hr or more 30kg / m 2 / hr or less, more preferably 15 kg / m 2 / hr or more 27kg / m 2 / hr or less. The flux can be calculated by the method described in the Examples.
[0073] [Reverse Solute Flux (RSF)] In the present disclosure, the RSF is an index that indicates the degree of contamination of the feed solution with the draw solute. The RSF can be calculated by the method described in the Examples.
[0074] [RSF / Flux] In the concentration of the raw material liquid in this embodiment, from the viewpoint of suppressing the contamination of the raw material liquid with the derived solute, RSF / Flux is preferably less than 100,000 g / kg, or less than 50,000 g / kg, or less than 40,000 g / kg, or less than 30,000 g / kg, or less than 10,000 g / kg, or less than 2,000 g / kg, or less than 1.000 g / kg, or less than 0.100 g / kg. Also, the RSF / Flux is preferably less than 2.000 g / kg, more preferably less than 1.000 g / kg. If the RSF / Flux is less than 100,000 g / kg, contamination of the raw liquid with a large amount of the lead solute during concentration is unlikely to occur, and the purity of the final valuable product after concentration can be increased, which is desirable. For example, when 1,000 g of a raw material liquid in which 100 g of valuable material is dissolved is concentrated to 200 g, if the concentration can be achieved with an RSF / Flux of less than 1.000 g / kg, the final raw material liquid after concentration will be a mixture of 100 g of valuable material, approximately 100 g of solvent, and less than 0.8 g of derived solute, and the concentration of the valuable material obtained after distilling off the solvent will be 99 mass% or more.
[0075] [Water Flux] In the concentration of the raw material liquid in this embodiment, the water flux, which is the amount of water removed per membrane area, is preferably 0.7 kg / m 2 / hr or more, or 1.0 kg / m 2 / hr or more, or 1.2kg / m 2 / hr or more, or 1.3kg / m 2 / hr or more, or 1.4kg / m 2 / hr or more, or 1.5kg / m 2 / hr or more, or 1.8kg / m 2 / hr or more. From the viewpoint of excellent efficiency in concentrating the raw material liquid, the water flux is preferably 1.2 kg / m 2 / hr or more, more preferably 1.4 kg / m 2 / hr or more, more preferably 1.8 kg / m 2 / hr or more. The water flux is preferably 1.2 kg / m 2 / hr or more 10kg / m 2 / hr or less, more preferably 1.4 kg / m 2 / hr or more 5kg / m 2 / hr or less, and even more preferably 1.8 kg / m 2 / hr or more 3kg / m 2 / hr or less. The water flux can be calculated by the method described in the Examples.
[0076] [RSF / Water Flux] In the concentration of the raw material liquid in this embodiment, from the viewpoint of suppressing the contamination of the raw material liquid with the derived solute, the RSF / water flux is preferably less than 100,000 g / kg, or less than 50,000 g / kg, or less than 40,000 g / kg, or less than 30,000 g / kg, or less than 10,000 g / kg, or less than 2,000 g / kg, or less than 1,500 g / kg, or less than 1,000 g / kg, or less than 0.100 g / kg, or less than 0.050 g / kg. Also, the RSF / water flux is preferably less than 2.000 g / kg, more preferably less than 1.000 g / kg, even more preferably less than 0.100 g / kg, and particularly preferably less than 0.050 g / kg.
[0077] The forward osmosis membrane according to the present embodiment is preferably one that does not allow valuable materials and draw solutes to pass through, but has high selectivity and allows a large amount of solvent to pass through. The selectivity of the forward osmosis membrane can be evaluated, for example, by salt selectivity, which can be calculated by the following method.
[0078] (Salt selectivity of forward osmosis membrane) Pure water (in one embodiment, pure water with an organic matter concentration (TOC) of 10 ppm or less and an electrical conductivity of 2 mS / cm or less) is passed as a raw material liquid at a linear speed of 4 cm / sec on the side of the forward osmosis membrane in contact with the active layer. In addition, a 3.5 mass % sodium chloride aqueous solution is placed as a guiding liquid on the substrate layer side opposite the active layer at a linear speed of 2.5 cm / sec. The base layer side is set as the positive side, and the raw material liquid and the derivative liquid are passed while being pressurized at 20 kPa. After 20 minutes, water moves to the derivative liquid side, while sodium chloride moves to the raw material liquid side. The former is the water flux (kg / m 2 / h), the latter is the RSF of the derived solute (g / (m 2 × hr), the RSF of the draw solute divided by the water flux into the draw solution, RSF / water flux (g / kg), is an index of the salt selectivity of the forward osmosis membrane. The salt selectivity of the forward osmosis membrane is preferably 0.05 g / kg or more and 1.00 g / kg or less, and more preferably 0.10 g / kg or more and 0.90 g / kg or less.
[0079] <Configuration of raw material liquid concentration system> Fig. 3 is a schematic diagram illustrating a feedstock liquid concentrating system according to one embodiment of the present invention. Referring to Fig. 3, the feedstock liquid concentrating system (1) includes a forward osmosis membrane module (100), a feedstock liquid tank (200), and a draw solution tank (300), and further includes a pipe for sending feedstock liquid (a) from the feedstock liquid tank (200) to the forward osmosis membrane module (100), and a pipe for sending draw solution (d) from the draw solution tank (300) to the forward osmosis membrane module (100). That is, the forward osmosis membrane module (100) is configured to receive the feed liquid (a) and the derivative liquid (d) and to bring the feed liquid (a) and the derivative liquid (d) into contact with each other via the forward osmosis membrane.
[0080] In the feed liquid concentration system (1), the feed liquid (a) is sent at an appropriate flow rate from the bottom of the feed liquid tank (200) filled with the feed liquid (a) to one space (e.g., the inner space of the hollow fiber membrane) of the forward osmosis membrane module (100) by a pump (P). At this time, the flow rate of the feed liquid (a) is manually or automatically adjusted by a flow meter or the like (not shown). On the other hand, the draw solution (d) is supplied from a draw solution tank (300) filled with the draw solution (d) to the other space (for example, the outer space of the hollow fiber membrane) of the forward osmosis membrane module (100) by a pump (P). Due to the difference in osmotic pressure between the feed liquid (a) and the draw liquid (d), the solvent moves from the feed liquid (a) to the draw liquid (d), concentrating the feed liquid (a). The concentrated feed liquid (a) leaves the forward osmosis membrane module (100) and returns to the feed liquid tank (200). The volume of the derivative liquid (d) increases due to the incorporation of the solvent from the raw liquid (a). For this reason, the derivative liquid tank (300) must have a sufficiently large capacity or must be provided with a means for discharging a portion of the derivative liquid out of the derivative liquid tank (300) by overflow or the like. In FIG. 3, a device for discharging the derivative liquid (d) out of the derivative liquid tank (300) is not shown. Providing a stirrer inside the raw liquid tank (200) is also effective for stable concentration.
[0081] From the viewpoint of improving the flux of the concentrated raw liquid, it is preferable that the raw liquid is continuously supplied to the forward osmosis membrane module (100), and it is also preferable that the concentrated raw liquid is continuously discharged from the forward osmosis membrane module (100). Such continuous supply and discharge can be achieved by appropriately controlling the above-mentioned pump (P).
[0082] The concentrated raw liquid (a) leaves the forward osmosis membrane module (100) and is returned to the raw liquid tank (200) for circulation. The return position is preferably a position far from the collection position of the raw liquid (a) to be supplied to the forward osmosis membrane module (100) and is located at the bottom of the raw liquid tank (200). Returning the raw liquid (a) to a position far from the collection position can prevent the concentration of the organic solvent in the raw liquid (a) from being excessively increased due to a short path. Returning the raw liquid (a) to the bottom of the raw liquid tank (200) can prevent valuable materials in the raw liquid (a) from precipitating on the wall surface of the raw liquid tank (200), which makes recovery difficult.
[0083] In the feedstock liquid concentration system (1), the specific gravity of the feedstock liquid (a) can be tracked by a specific gravity meter (not shown). This makes it possible to monitor the concentration of the organic solvent in the feedstock liquid (a). If necessary, the operating conditions of the forward osmosis membrane module can be changed to adjust the composition of the feedstock liquid (a) while concentrating it within a range in which valuable substances are not precipitated, coagulated, or denatured.
[0084] The degree of concentration of the raw material liquid (a) can be known by measuring the volume of the raw material liquid (a) using a liquid level gauge (LG). Finally, concentration can be completed when the target concentration rate is reached. In addition to the specific gravity measurement given above, the properties of the raw liquid (a) (e.g., the concentration of at least one of the components in the raw liquid) can be monitored by pH measurement, electrical conductivity measurement, optical rotation measurement, refractive index measurement, ultraviolet light analysis, visible light analysis, infrared light analysis, near-infrared light analysis, etc. Using one or more measurement results selected from these analyses, for example, the concentration of at least one of the components in the raw liquid can be determined. This result, the measured value of the liquid level gauge, the weight of the liquid, etc. can be simultaneously monitored, and the operating conditions of the forward osmosis membrane module can be changed as necessary to perform concentration while maintaining the concentration of the organic solvent in the raw liquid (a).
[0085] Furthermore, it is more preferable to use known AI techniques such as regression analysis, classification, clustering, deep learning using neural networks, or an estimation model obtained by a combination of these techniques to estimate the concentration of the water-soluble organic solvent in the raw material liquid (a), since this allows for more accurate concentration estimation. By using such a method, the concentration of the water-soluble organic solvent in the raw material liquid (a) can be monitored with high accuracy, and the concentration of the water-soluble organic solvent can be maintained within a suitable range with higher accuracy by appropriately manipulating the operating conditions. In this case, the risk of precipitation, aggregation, or denaturation of valuable materials can be further reduced, which is preferable.
[0086] <Method for removing organic solvent> One aspect of the invention provides a method for removing an organic solvent, hi one aspect, the method comprises contacting a solution with a draw solution through a forward osmosis membrane. In one embodiment, the solution includes an organic solvent. In one embodiment, the draw solution includes a draw solute. In one embodiment, the draw solute satisfies the following (1) and (2). (1) A polymer containing at least three repeating units with a molecular weight of 30 to 100. (2) The polymer has a branched structure in which atoms (atomic groups) other than hydrogen atoms and halogen atoms are bonded to the main chain.
[0087] <Inducing solute for removing organic solvents> One aspect of the present invention provides a draw solute for removing an organic solvent. In one aspect, the draw solute satisfies the following (1) and (2): (1) A polymer containing at least three repeating units with a molecular weight of 30 to 100. (2) The polymer has a branched structure in which atoms (atomic groups) other than hydrogen atoms and halogen atoms are bonded to the main chain.
[0088] The lead solute of this embodiment, which satisfies the requirements (1) and (2), is prevented from being mixed into the solution, and when removing the organic solvent from a solution rich in organic solvent, the lead solute can remove the organic solvent with a high flux. EXAMPLES
[0089] EXAMPLES Hereinafter, examples will be given to more specifically illustrate the configuration and effects of the present invention, but the present invention is not limited to the following examples in any way.
[0090] The contact angle on the active layer surface was measured using DMo-602 manufactured by Kyowa Interface Science Co., Ltd. 2 μL of distilled water was dropped onto the active layer surface using an automatic dispenser, and the average of the dynamic contact angles measured at 100 msec intervals from 2000 msec to 3000 msec after the drop was taken as the contact angle.
[0091] The inner and outer diameters of the hollow fiber membrane were measured by observing slices of the hollow fiber membrane sample using an electron microscope.
[0092] The porosity of the hollow fiber membrane was calculated by the following formula (1).
number
[0093] The pore size of the hollow fiber membrane was calculated according to the method of JIS K 3832 using a perm porometer (CFP-1200AX; Porous Materials, Inc., USA) and Galwick liquid (surface tension 15.9 dynes / cm).
[0094] The water permeance of the hollow fiber was measured using the pressure membrane test device shown in FIG. 6 at a transmembrane pressure difference of 2 bar and a hollow side flow rate of 36 cc / min (linear velocity of 4 cm / sec).
[0095] <Preparation of forward osmosis membrane module 1> A polyketone having an intrinsic viscosity of 2.2 dL / g, which is a complete alternating copolymerization of ethylene and carbon monoxide, was added to a 65% by mass aqueous resorcinol solution so that the polymer concentration was 15% by mass, and the mixture was stirred and dissolved at 80° C. for 2 hours and degassed to obtain a uniform and transparent spinning dope. The spinning dope was filled into a wet hollow fiber spinning machine equipped with a double spinneret, and a 25% by mass aqueous methanol solution was extruded from the inside of the double spinneret, and the spinning dope was extruded from the outside into a coagulation tank filled with a 40% by mass aqueous methanol solution, respectively, to form a hollow fiber membrane by phase separation.
[0096] The obtained hollow fiber membrane was cut into a length of 70 cm, bundled, and washed with water. After washing with water, the hollow fiber membrane bundle was subjected to solvent replacement with acetone, and further to solvent replacement with hexane, and then dried at 50°C. The measured values of the polyketone hollow fiber (HF support) thus obtained are shown in FIG. FIG. 5 shows an electron microscope image of the polyketone hollow fiber.
[0097] A hollow fiber membrane bundle consisting of 80 of the above-mentioned polyketone hollow fiber membranes was stored in a cylindrical module housing (cylindrical case) having a diameter of 2 cm and a length of 10 cm. Both ends of the hollow fiber membrane bundle were then fixed with adhesive, and both ends of the adhesive fixing parts were cut to open holes in the hollow fiber membranes at both ends, thereby producing a polyketone hollow fiber supported membrane module with an effective length of 80 mm.
[0098] Using the obtained polyketone hollow fiber supported membrane module, interfacial polymerization was carried out on the inner surface (on the base layer) of each hollow fiber membrane as described below. In a 1 L container, 20.216 g of m-phenylenediamine and 1.52 g of sodium lauryl sulfate were placed, and 991 g of pure water was added to dissolve the mixture, to prepare a first solution for use in interfacial polymerization. In another 1 L container, 0.6 g of trimesoyl chloride was placed, and 300 g of n-hexane was added and dissolved to prepare a second solution for use in interfacial polymerization.
[0099] The formation of the active layer by interfacial polymerization was carried out using an interfacial polymerization apparatus shown in FIG. The core side (inside of the hollow fibers) of the hollow fiber support membrane module was filled with the first solution, and after leaving it to stand for 5 minutes, the first solution was removed from the inside of the hollow fibers. With the inside of the hollow fibers wetted with the first solution, the core side pressure was set to normal pressure, and the shell side (outside of the hollow fibers) pressure was set to a reduced pressure of 10 kPa absolute pressure (core side pressure > shell side pressure). After leaving it to stand for 2 minutes in this state, the second solution was pumped to the core side at a flow rate of 40 mL / min for 3 minutes while maintaining this pressure, and interfacial polymerization was performed. The polymerization temperature was 25°C.
[0100] Next, the hollow fiber support membrane module was removed from the device and left to stand in a thermostatic chamber set at 50° C. for 5 minutes to vaporize and remove n-hexane. Furthermore, both the shell side and the core side were washed with pure water. The above steps result in an effective membrane area of approximately 100 cm 2 Thus, a forward osmosis membrane module 1 was obtained. The obtained forward osmosis membrane module 1 has an active layer inside the hollow fibers. The contact angle with respect to the surface of the active layer was measured to be 40 degrees, and therefore, the active layer was hydrophilic.
[0101] The salt selectivity of the forward osmosis membrane module 1 was calculated by the following method. In the forward osmosis membrane module 1, pure water with an organic matter concentration (TOC) of 10 ppm or less and an electrical conductivity of 2 mS / cm or less was placed on the active layer side as the raw material liquid, and a 3.5 mass% aqueous sodium chloride solution was placed on the base layer side as the deriving liquid. The base layer side was set to the positive side, and the raw material liquid and the deriving liquid were passed while pressurizing to 20 kPa. After 20 minutes, the RSF of the deriving solute of the forward osmosis membrane module 1 and the water flux into the deriving solution were measured. The salt selectivity of the forward osmosis membrane module 1 was calculated by applying the RSF and water flux to the following formula. The RSF and water flux were measured by the method described below. RSF / water flux (salt selectivity) = RSF of derived solute (g / (m 2 × hr) ÷ Water flux into the draw solution (kg / m 2 / hr) As a result, the salt selectivity of the forward osmosis membrane module 1 was 0.15 g / kg.
[0102] The inner surfaces of the obtained forward osmosis membrane and the polyketone hollow fiber before interfacial polymerization were measured by X-ray photoelectron spectroscopy. The results are shown in Figure 8(a). Comparing the spectra of the forward osmosis membrane and the polyketone hollow fiber (HF), a nitrogen peak was confirmed, confirming that a polyamide active layer had indeed been formed on the inner surface. In addition, the inner surfaces of the obtained forward osmosis membrane and the polyketone hollow fiber before interfacial polymerization were measured by ATR-FTIR. The results are shown in Figure 8(b). The spectrum of the polyketone hollow fiber showed peaks at 1057, 1336, 1408 and 1693 cm. -1 Peaks were observed at wavelengths of 1000 to 1800 cm. -1 The IR peak at wavelengths of 300 nm was also seen in the spectrum of the forward osmosis membrane because the forward osmosis membrane and the polyketone hollow fiber have transparency above 300 nm. In addition to the peaks from the polyketone hollow fiber, the spectrum of the forward osmosis membrane showed three new peaks at 1541, 1610, and 1663 cm. -1These can be attributed to the amide II band, aromatic amide, and amide I band, respectively, according to the research of CY Tang et al. (Desalination 242 (2009) 149). From these peaks, it was confirmed that a polyamide layer was formed on the hollow side by interfacial polymerization.
[0103] The inner surface of the obtained forward osmosis membrane was observed using an electron microscope. An active layer was confirmed on the inner surface. The results are shown in Figure 9.
[0104] The obtained forward osmosis membrane module 1 was measured in the device shown in Figure 6 using a 0.1 mass% magnesium sulfate aqueous solution as the feed solution at a transmembrane pressure difference of 2 bar and a hollow side flow rate of 36 cc / min (linear velocity of 4 cm / sec), and the rejection rate of magnesium sulfate was approximately 100%. A similar test was performed using a 0.005 mass% MeOH solution of Brilliant Blue R, and the same rejection rate was observed. This confirmed that the active layer of the forward osmosis membrane module 1 was formed without defects and functioned both in water and in organic solvents. The above results are shown in Figure 10.
[0105] <Example 1> The forward osmosis membrane module 1 was set in the raw material liquid concentration system shown in FIG. 3, and a concentration test was carried out at room temperature (23° C.). As the raw material liquid, 350 g of a tetrahydrofuran (THF) solution containing 0.1 mass % of sucrose octaacetate (SoA) (weight average molecular weight 678, manufactured by Tokyo Chemical Industry Co., Ltd.), which is a valuable material, was used. The deriving liquid was 350 g of tripropylene glycol. The raw material liquid and the deriving liquid were circulated for 60 minutes in a parallel flow mode at 36 mm / min (linear velocity 4 cm / sec) and 50 mm / min (linear velocity 0.38 cm / sec), respectively.
[0106] (Flux measurement) The increase in the mass of the draw solution (kg) is calculated as the effective membrane area (m 2) and the circulation time (hr) to obtain the flux (kg / m 2 / hr) was calculated.
[0107] (Measurement of back diffusion of induced solute) The amount of the derived solute (g) contained in the raw liquid after the concentration test was measured by liquid chromatography, and the effective membrane area (m 2 ) and divided by the circulation time (hr), the reverse solute flux (RSF) (unit: g / m 2 / hr) was calculated as follows. Details are as follows.
[0108] (RSF / Flux measurement) As mentioned above, the calculated RSF (g / m 2 / hr) into the induction solution (kg / m 2 RSF / Flux (g / kg) was calculated by dividing the total flow rate by the total flow rate (hr).
[0109] (Measurement of the solubility of derivative solutes in water) The solubility of the derived solute in 100 g of water was measured as follows. The inducing solute was gradually added to 100 g of pure water at 25° C., and the mass just before the mixture became two phases was measured as the solubility (mass %) of the inducing solute in water.
[0110] (Measurement of water solubility for derivative solutes) The solubility of water in the derived solute per 100 g (water content of the derived solute) was measured as follows. Water was added little by little to 100 g of the induced solute at 25° C., and the mass just before the mixture became two phases was measured as the solubility (mass %) of water in the induced solute.
[0111] <Water flux measurement> Approximately 0.5 mL of the raw liquid was taken with a 1 mL syringe, and approximately 0.1 mL was injected into a Karl Fischer moisture content analyzer (Model CA-200, manufactured by Mitsubishi Chemical Analytech Co., Ltd.) to measure the moisture content in the raw liquid. The water flux into the draw solution was calculated from the moisture content in the raw liquid before and after the operation.
[0112] (RSF / water flux measurement) As mentioned above, the calculated RSF (g / m 2 / hr) into the induction solution is expressed as water flux (kg / m 2 The RSF / water flux (g / kg) was calculated by dividing the RSF by the water flux (g / hr).
[0113] (Hydrophilicity / hydrophobicity of the solvent in the raw material liquid) At 25°C, the solvent or derived solute was mixed with water in a volume ratio of 50:50 and stirred for 24 hours using a φ8 mm × 25 mm stirrer tip and a magnetic stirrer. If a one-phase state was maintained by visual observation, the solution was judged to be hydrophilic, and if a two-phase state was maintained, the solution was judged to be hydrophobic.
[0114] <Examples 2 to 7, Comparative Examples 1 and 3> A concentration test was carried out in the same manner as in Example 1, except that the valuable materials in the raw material solution, the solvent in the raw material solution, the derived solute in the derived solution, and the solvent in the derived solution were as shown in Table 1, and the flux and RSF were calculated.
[0115] <Reference example 1> A concentration test was carried out in the same manner as in Comparative Example 1, except that no valuable material was added to the raw material liquid and the solvent of the raw material liquid was changed to water, and the flux and RSF were calculated.
[0116] <Reference example 2> A concentration test was carried out in the same manner as in Example 2, except that no valuable material was added to the raw material liquid and the solvent of the raw material liquid was changed to water, and the flux and RSF were calculated.
[0117] <Example 8> As the raw material liquid, 150 g of a solution containing tetrahydrofuran (THF) and water in a ratio of 88:12 was used so as to contain 5 mass% of the valuable substance acetylglucopyranose (GpA) (weight average molecular weight 390 Da, manufactured by Tokyo Chemical Industry Co., Ltd.). As the deriving liquid, 150 g of polypropylene glycol (PPG-400) was used. The raw material liquid and the deriving liquid were circulated for 60 minutes in a parallel flow mode at 36 mm / min (linear velocity 4 cm / sec) and 50 mm / min (linear velocity 0.38 cm / sec), respectively.
[0118] <Example 9> A concentration test was carried out in the same manner as in Example 8, except that the solvent ratio in the raw liquid, the amount of the raw liquid, and the derived solute were as shown in Table 1, and the flux and RSF were calculated.
[0119] <Example 10> The forward osmosis membrane module 1 was set in the raw material liquid concentration system shown in FIG. 3, and a test for concentrating the raw material liquid by dehydration was carried out at room temperature (23° C.). As the raw material liquid, 150 g of a solution containing tetrahydrofuran (THF) and water in a ratio of 95:5 was used so as to contain 5 mass % of the valuable substance acetylglucopyranose (GpA) (weight average molecular weight 390 Da). As the deriving liquid, 150 g of polypropylene glycol (PPG-400) was used. The raw material liquid and the deriving liquid were circulated for 60 minutes in a parallel flow mode at 36 mm / min (linear velocity 4 cm / sec) and 50 mm / min (linear velocity 0.38 cm / sec), respectively. According to the above-mentioned methods, the solubility of the inducing solute in water, the solubility of water in the inducing solute, the water flux, the RSF, and the RSF / water flux of Example 10 were calculated.
[0120] <Examples 11 to 13, Comparative Example 2> A concentration test by dehydration was performed in the same manner as in Example 10, except that the induced solutes were as shown in Table 2, and the solubility of the induced solute in water, the solubility of water in the induced solute, water flux, RSF, and RSF / water flux were calculated.
[0121] <Comparative Example 4> A concentration test was carried out in the same manner as in Example 10, except that the valuable materials in the raw material solution, the solvent in the raw material solution, and the induced solute in the induced solution were as shown in Table 2, and the solubility of the induced solute in water, the solubility of water in the induced solute, water flux, RSF, and RSF / water flux were calculated.
[0122] <Reference example 3> The relationship between the SoA concentration in the feed solution and the flux was investigated using the forward osmosis membrane module 1 and a laboratory forward osmosis membrane evaluation device (Figure 11). As the feed solution, MeOH solutions containing 0 mass%, 20 mass%, 40 mass%, and 60 mass% SoA were prepared and passed through the inner surface side of the forward osmosis membrane module 1 at 36 cc / min (linear velocity 4 cm / sec). On the other hand, a 2M MeOH solution of PEG-400 was passed through the outer surface of the forward osmosis membrane module as a draw solution at 336cc / min (linear velocity 2.5cm / sec). The flux was measured from the weight change over a 20-minute period and the results are shown in Figure 12. From Fig. 12, it can be inferred that the flux of MeOH disappears when the SoA concentration in the raw solution is 71 mass%, and therefore it was confirmed that the use of this derivative liquid may enable the concentration of the SoA MeOH solution to be increased to 71 mass%.
[0123] <Reference example 4> An attempt was made to highly concentrate a 10% by mass SoA / MeOH solution using the same apparatus, flow rate, module, and deriving liquid as in Reference Example 3. The results are shown in Figures 13 and 14. As a result, the SoA was concentrated to 52% by mass. According to the inventors' research, the highest concentration achieved by forward osmosis of organic solvents to date was 16,000 ppm, as described in Non-Patent Document 1, and the results of this Reference Example confirmed the potential for advanced concentration by forward osmosis of organic solvents. According to a report by LG Peeva et al. (Effect of concentration polarisation and osmotic pressure on flux in organic solvent nanofiltration, J Memb Sci. 236 (2004) 121), the practical concentration range for concentrating pharmaceutical active ingredients is in the range of 5% by mass or more. Therefore, this reference example is the first case that shows the potential of organic solvent forward osmosis for concentrating pharmaceutical active ingredients. On the other hand, the final raw material solution contained 17% by mass of PEG-400, which is an induced solute. PEG-400 has a high boiling point and cannot be distilled off, so PEG-400 remains as an impurity in the drug substance. In order to put the technology of applying organic solvent forward osmosis to the concentration of pharmaceutical raw materials into practical use, it is necessary to improve the blocking property of the forward osmosis membrane or to develop an induced solute that is easily blocked. By using the induced solute of this embodiment, it is possible to significantly reduce contamination of the raw material solution during high concentration.
[0124] <Reference example 5> The same experiment as in Reference Example 3 was carried out using a MeOH solution of PPG-400 adjusted to 2M as the induced liquid, and the relationship between the SoA concentration in the raw liquid and the flux was investigated. From FIG. 15, it can be inferred that the flux of MeOH disappears when the SoA concentration in the raw liquid is 71 mass%. Therefore, it was confirmed that the use of this induced liquid may enable the concentration of the SoA MeOH solution to be up to 71 mass%.
[0125] <Reference example 6> An experiment similar to that in Reference Example 4 was carried out using a 2 M MeOH solution of PPG-400 as a draw solution to attempt high concentration of a 10 mass % SoA / MeOH solution. The results are shown in Figures 16 and 17. As a result, SoA was concentrated to nearly 50 mass % as in Reference Example 4. At this time, the final raw material solution contained only 0.04 mass % of the induced solute PPG-400. Experiments have shown that by using the induced solute of this embodiment, contamination of the raw material solution during high concentration can be significantly reduced.
[0126] <Reference example 7> The MeOH vapor pressure of a 2M PEG-400 MeOH solution and a 2M PPG-400 MeOH solution was measured using the vapor pressure measuring device shown in Figure 18. The osmotic pressure of each solution was calculated from the obtained vapor pressure data using the following formula.
number
[0127] The calculation results of the osmotic pressure of each solution are shown in Figure 19. It was found that the osmotic pressure of the MeOH solution of PPG-400 adjusted to 2M was higher than that of the MeOH solution of PEG-400 adjusted to 2M. When comparing Reference Example 3 and Reference Example 5, a higher flux was confirmed in Reference Example 5, and this result was not inconsistent with that.
[0128] The solvents of the deriving solutes and deriving solutions used in the examples are as follows: Tripropylene glycol: available from Tokyo Chemical Industry Co., Ltd. (molecular weight 30 to 100, repeating units: 3) Polypropylene glycol (equivalent to PPG-400): Available from Fujifilm Wako Pure Chemical Industries, Ltd. (molecular weight 30 to 100, repeating units: 5 to 12) Polypropylene glycol (equivalent to PPG-700): Available from Fujifilm Wako Pure Chemical Industries, Ltd. (molecular weight 30 to 100, repeating units: 8 to 18) Polypropylene glycol (equivalent to PPG-1000): Available from Fujifilm Wako Pure Chemical Industries, Ltd. (molecular weight 30 to 100, repeating units: 14 to 26) Polypropylene glycol (equivalent to PPG-2000): Available from Fujifilm Wako Pure Chemical Industries, Ltd. (molecular weight 30 to 100, repeating units: 28 to 46) Polyethylene glycol (equivalent to PEG-400): Available from Fujifilm Wako Pure Chemical Industries, Ltd. (molecular weight 30 to 100, repeating units: 5 to 13) Polyethylene glycol (equivalent to PEG-600): Available from Fujifilm Wako Pure Chemical Industries, Ltd. (molecular weight 30 to 100, repeating units: 8 to 18) Tetrahydrofuran (THF): available from Fujifilm Wako Pure Chemical Industries, Ltd.
[0129] [Evaluation method] (Flux ranking) In the concentration test of the draw solution in the Examples and Comparative Examples, the larger the flux value in the draw solution, the shorter the concentration time. The flux was ranked according to the following criteria. A: 20kg / m 2 / hr or more B: 16kg / m 2 / hr or more 20kg / m 2 Less than / hr C: 12kg / m 2 / hr or more 16kg / m 2 Less than / hr D: 10kg / m 2 / hr or more 12kg / m 2 Less than / hr E: 10kg / m 2 Less than / hr If the evaluation is A to D, the concentrating performance is high and the material can be suitably used as the draw solute according to this embodiment.
[0130] (RSF / Flux ranking) In the concentration tests of the induction liquids of the Examples and Comparative Examples, the smaller the RSF / Flux value of the induction solute, the less the induction solute is mixed into the raw material liquid. The RSF / Flux ranking was evaluated according to the following criteria. A: Less than 1g / kg B: 1g / kg or more and less than 2g / kg C: 2g / kg or more and less than 10g / kg D: 10g / kg or more but less than 100g / kg E:100g / kg or more If the evaluation is A to C, the concentration performance is high and the material can be suitably used as the draw solute according to this embodiment.
[0131] (Water Flux Ranking) In the concentration test of the draw solution in the Examples and Comparative Examples, a higher water flux value into the draw solution means higher dehydration performance (shorter concentration time), and the water flux was ranked according to the following criteria. A: 1.5kg / m 2 / hr or more B: 1.3kg / m 2 / hr or more 1.5kg / m 2 Less than / hr C: 1.0kg / m 2 / hr or more 1.3kg / m 2 Less than / hr D: 0.7kg / m 2 / hr or more 1.0kg / m 2 Less than / hr E: 0.7kg / m 2 Less than / hr If the evaluation is A to D, the concentrating performance is high and the material can be suitably used as the draw solute according to this embodiment.
[0132] (RSF / Water Flux Ranking) In the concentration tests of the draw solutions in the Examples and Comparative Examples, the smaller the RSF / water flux value of the draw solute, the less the draw solute is mixed into the raw solution. The RSF / water flux was ranked according to the following criteria. A: Less than 1g / kg B: 1g / kg or more and less than 2g / kg C: 2g / kg or more and less than 10g / kg D: 10g / kg or more but less than 100g / kg E:100g / kg or more If the evaluation is A to D, the concentrating performance is high and the material can be suitably used as the draw solute according to this embodiment.
[0133] [Table 1-1]
[0134] [Table 1-2]
[0135] [Table 2-1]
[0136] [Table 2-2]
[0137] The weight average molecular weight of the derived solute was determined by liquid chromatography-mass spectrometry. A liquid chromatograph (ACQUITY UPLC I-Class, manufactured by Nihon Waters K.K.) and a mass spectrometer (micrOTOF-QIII, manufactured by Bruker Japan K.K.) were used. For PEG, a column packed with octadecyl silica gel (ACQUITY UPLC BEH C18, inner diameter 2.1 mm, length 50 mm, particle size 1.7 μm, manufactured by Nihon Waters Co., Ltd.) was used. The column temperature was set to 40°C, and a combination of 0.1% formic acid aqueous solution and 0.1% acetonitrile solution was used as the mobile phase. The mobile phase was fed at 0.2 mL / min, and the concentration of 0.1% formic acid acetonitrile was gradient from 5% to 40% over 10 minutes. For PPG, a column packed with phenylhexylsilylated silica gel (ACQUITY UPLC BEH Phenyl, inner diameter 2.1 mm, length 100 mm, particle size 1.7 μm, manufactured by Nihon Waters, Inc.) was used. The column temperature was set to 50°C, and a combination of 10 mmol / L ammonium formate and acetonitrile was used as the mobile phase. The mobile phase was fed at 0.25 mL / min, and the acetonitrile concentration was increased from 40% to 99% over 6 minutes. The mass spectrometer was operated in the positive ion mode using electrospray ionization, and the data were analyzed using DataAnalysis software (Bruker Japan). The samples were adjusted in advance using a 50 v / v% 2-propanol solution by diluting appropriately. The m / z of each repeating structure n was calculated based on the proton-added molecule for PEG and the ammonium ion-added molecule for PPG, and the area values were obtained from the extracted ion chromatograms. Analysis was performed under the following assumptions. The weight abundance ratio was calculated from the area value of the repeating structure n of the derived solute under the assumption that the ionization rate of each repeating structure n is the same. The weight average molecular weight of the derived solute was calculated from the molecular weight and weight abundance ratio of each repeating structure n of the standard solution. As an example, the analysis results of PPG-1000 are shown below. The weight-average molecular weight Mw was calculated from the average molecular weight Mi and abundance ratio Ni of each repeating structure according to the following formula.
number
[0138] [Table 3]
[0139] [Table 4]
[0140] The amount of the derived solute mixed in the raw material solution was determined using data measured and analyzed in the same manner as in the calculation of the weight-average molecular weight. The data obtained was analyzed with the following assumptions: Since the distribution of repeating structure n in the polymer-derived solute and the polymer-derived solute in the sample sometimes differed, it was determined that it would be difficult to create a calibration curve using the area value of a specific repeating structure n and perform quantification. Therefore, the weight abundance ratio was calculated from the area value of repeating structure n in the standard solution under the assumption that the ionization rate of each repeating structure n is the same. The concentration of each repeating structure n was calculated by multiplying the standard solution concentration of each repeating structure n in the standard solution by the weight abundance ratio. The sum of the quantitative results of the detected repeating structure n was taken as the concentration of the polymer-derived solute in the sample.
[0141] The concentration of SoA leaked into the induction solution was measured by high performance liquid chromatography mass spectrometry. The measurements were performed using liquid chromatography (product name: ACQUITY UPLC I-Class, manufactured by Nihon Waters), a mass spectrometer (product name: micrOTOF-QIII, manufactured by Bruker Japan), and a column (ACQUITY UPLC BEH C18 2.1 mm ID × 50 mm, 1.7 μm, manufactured by Nihon Waters). The measurement conditions were as follows: a photodiode array detector (scan range 195 nm to 600 nm) and a mass spectrometer were used as the detector, a column packed with octadecyl silica gel (inner diameter 2.1 mm, length 50 mm, particle size 1.7 μm, manufactured by Nihon Waters Co., Ltd.) was used as the column, the column temperature was constant at around 40°C, 10 mmol / L ammonium formate solution and ethanol (99.5%) were used as the mobile phase, and the mobile phase was delivered at 0.2 mL / min, with the mixture ratio of the 10 mmol / L ammonium formate solution from 80% to 10%, and the ethanol (99.5%) concentration from 20% to 90%, with a gradient over 14 minutes. The mass spectrometer used electrospray ionization, and measurements were performed in positive ion mode. DataAlysis software (manufactured by Bruker Japan Co., Ltd.) was used for analysis. The samples were adjusted in advance by diluting them appropriately with ethanol (99.5). The data obtained was analyzed with the following assumptions: For SoA, the area value of the peak in the extracted ion chromatogram of the m / z (696.2296, [M+NH4]+) of the ammonium salt adduct molecule was obtained, and the sample concentration was calculated using a calibration curve of the standard solution obtained in advance. A similar analysis was performed for GpA. In all of the Examples, Comparative Examples, and Reference Examples, no valuable substances were detected leaking into the deriving solution, suggesting that the yield of valuable substances was 99% or more.
[0142] From Reference Examples 1 and 2, Example 1, and Comparative Example 2, the RSF of the organic solvent system is larger than that of the aqueous system. This is considered to be because the active layer made of a polymer swells in the solvent. In other words, in the organic solvent forward osmosis, it is more difficult to block the inducer solute than in the aqueous system. Although it is not clear why the RSF becomes smaller by using a polymer with a branched structure as a lead solute, the inventors speculate as follows. In aqueous systems, the polymer-derived solute has low affinity with the solvent (water), so it is believed to form a fully entangled coil. In this case, it is believed that the branched polymer, which has a limited conformation, has a larger radius of gyration per molecular weight, and therefore a lower RSF. According to a reference example, the RSF / Flux when PEG is used is about 8 times higher than when PPG is used. On the other hand, in organic solvent systems, the polymer-derived solute has a high affinity with the organic solvent, so it is thought that it is less entangled and forms a relatively elongated coil. In such a situation, the inventors speculate that the movement of the polymer-derived solute through the membrane is influenced by the cross-sectional area of the conformation in which the polymer is elongated in the main chain direction, rather than the radius of gyration. In the conformation in which the polymer is stretched in the main chain direction, the cross-sectional area of the plane perpendicular to the main chain direction is larger for the branched polymer than for the linear polymer PEG. Therefore, it is considered that the branched polymer is sufficiently blocked by the membrane, and the RSF in the organic solvent system is small. According to Example 1 and Comparative Example 1, the RSF / Flux when PEG is used is more than 230 times higher than that when PPG is used. The inventors consider the reason why the flux of Comparative Example 1 is lower than that of Example 1 as follows. When a linear polymer is used as the induced solute in organic solvent forward osmosis, it is difficult to block the induced solute, and it is thought that the induced solute leaks into the feed solution. The inventors believe that this causes a decrease in the concentration difference (≒ osmotic pressure difference) of the induced solute near the membrane, a decrease in the driving force for membrane permeation, and a decrease in flux. For the same reason, the inventors believe that in Comparative Example 2, although PEG-400 has a high affinity for water, no osmotic pressure difference occurs between the membranes, resulting in a low driving force for water permeation and a low water flux.
[0143] From the above perspective, pharmaceutical excipients can be screened as shown in Table 5 below. Table 5 lists pharmaceutical excipients with molecular weights between 400 and 2000 Da. Since osmotic pressure depends on the molar concentration of the inducer solute in the inducer solution, solubility in the solvent is also one of the physical properties required of the inducer solute. Table 5 also shows the solubility in methanol. In addition, considering the ease of handling in plants, it is desirable for the excipient to be liquid at room temperature and have low viscosity. Both the state and viscosity of the pharmaceutical excipients at room temperature are shown in Table 5. From these results, it can be seen that PPG has uniformly desirable physical properties as a pharmaceutical excipient. PEG-400 also has desirable properties, but the comparative examples show that it has a large reverse diffusion factor (RSF). Similarly, polysorbate 20 has almost the desired properties, but has the drawback of being somewhat high in viscosity.
[0144] [Table 5] [Explanation of symbols]
[0145] 1. Raw material liquid concentration system 100 Forward osmosis membrane module 110 Housing 111 Induction fluid inlet 112 Inductive liquid outlet 120 Forward Osmosis Membrane 130 Adhesive resin 121 Base material layer 122 Active layer 200 Raw material tank 300 Induction liquid tank a Raw material liquid b. Solvent c Concentrated raw material liquid d Inducing solution LG liquid level gauge P-Pump
Claims
1. A method for concentrating a raw material liquid, comprising the steps of: The method includes a concentration step of contacting a feed liquid with a derivative liquid through a forward osmosis membrane, The raw material liquid contains a valuable material and a solvent, the solvent comprises an organic solvent, the draw solution comprises a draw solute; The method for concentrating a raw material liquid, wherein the draw solute satisfies the following (1) and (2): (1) A polymer containing at least three repeating units having a molecular weight of 30 to 100. (2) The polymer has a branched structure in which an atom (atomic group) other than a hydrogen atom or a halogen atom is bonded to the main chain.
2. 2. The method for concentrating a raw material liquid according to claim 1, wherein a concentration of the organic solvent in the solvent is 50% by mass or more.
3. 2. The method for concentrating a raw material liquid according to claim 1, wherein a concentration of the organic solvent in the solvent is 80% by mass or more.
4. 3. The method for concentrating a raw material liquid according to claim 1, wherein the weight average molecular weight of the derivative solute is 300 Da or more and 2,300 Da or less.
5. 3. The method for concentrating a raw material liquid according to claim 1, wherein the weight average molecular weight of the derivative solute is 400 Da or more and 1000 Da or less.
6. The solvent comprises an organic solvent and water; 3. The method for concentrating a raw material liquid according to claim 1, wherein the solubility of the lead solute in water is 2% by mass or more.
7. The solvent comprises an organic solvent and water; 3. The method for concentrating a raw material liquid according to claim 1, wherein the solubility of the lead solute in water is 6% by mass or more.
8. 3. The method for concentrating a raw material liquid according to claim 1, wherein the forward osmosis membrane is in the form of a hollow fiber.
9. The forward osmosis membrane has a substrate layer and an active layer, 3. The method for concentrating a raw material liquid according to claim 1 or 2, wherein the base layer comprises one or more polymers selected from the group consisting of polysulfone, polyethersulfone, polyvinylidene fluoride, polyacrylonitrile, polyethylene, polypropylene, cellulose-based polymers, polyketones, polyamides, polyimides, polyetheretherketones, and polybenzimidazoles.
10. 10. The method for concentrating a raw material liquid according to claim 9, wherein an active layer of the forward osmosis membrane comprises a polyamide.
11. Pure water was placed as a raw material liquid on the active layer side, and a 3.5% by mass aqueous solution of sodium chloride was placed as a deriving liquid on the base layer side. The base layer side was set as the positive side, and the raw material liquid and the deriving liquid were passed through the base layer side while being pressurized to 20 kPa. After 20 minutes, the forward osmosis membrane was evaluated. The RSF of the derived solute (g / (m 2 × hr) into the draw solution. 2 11. The method for concentrating a raw material liquid according to claim 9 or 10, wherein RSF / water flux (salt selectivity) divided by RSF / water flux (salt selectivity) is 0.05 g / kg or more and 1.00 g / kg or less.
12. The method for concentrating a raw material liquid according to claim 11, wherein the salt selectivity is 0.10 g / kg or more and 0.90 g / kg or less.
13. 3. The method for concentrating a raw material liquid according to claim 1 or 2, wherein the valuable materials are pharmaceuticals, drug substances, and development pipelines (medical drug candidate compounds), as well as intermediates and raw materials thereof.
14. 3. The method for concentrating a raw material liquid according to claim 1 or 2, wherein the valuable substance is a compound having a weight average molecular weight of 100 to 3,000,000.
15. 3. The method for concentrating a raw material liquid according to claim 1 or 2, wherein the valuable material is a cosmetic product, a functional chemical product, or a raw material thereof.
16. A raw material liquid concentrating system for concentrating a raw material liquid, comprising: the feed liquid concentration system includes a forward osmosis membrane module configured to receive the feed liquid and the derivative liquid and to allow the feed liquid and the derivative liquid to come into contact with each other via a forward osmosis membrane; The raw material liquid contains a valuable material and a solvent, the solvent comprises an organic solvent, the draw solution comprises a draw solute; A raw material liquid concentrating system, wherein the induced solute satisfies the following (1) and (2). (1) A polymer containing at least three repeating units having a molecular weight of 30 to 100. (2) The polymer has a branched structure in which an atom (atomic group) other than a hydrogen atom or a halogen atom is bonded to the main chain.
17. 17. The system for concentrating a raw material liquid according to claim 16, wherein a concentration of the organic solvent in the solvent is 50% by mass or more.
18. 17. The system for concentrating a raw material liquid according to claim 16, wherein a concentration of the organic solvent in the solvent is 80% by mass or more.
19. 18. The raw material liquid concentrating system according to claim 16 or 17, wherein the weight average molecular weight of the derivative solute is 300 Da or more and 2300 Da or less.
20. 18. The raw material liquid concentrating system according to claim 16 or 17, wherein the weight average molecular weight of the derived solute is 400 Da or more and 1000 Da or less.
21. The solvent comprises an organic solvent and water; 18. The raw material liquid concentrating system according to claim 16, wherein the solubility of water in the guiding solute is 2% by mass or more.
22. The solvent comprises an organic solvent and water; 18. The raw material liquid concentrating system according to claim 16, wherein the solubility of the lead solute in water is 6% by mass or more.
23. The raw material liquid concentrating system according to claim 16 or 17, wherein the forward osmosis membrane is in the form of a hollow fiber.
24. The forward osmosis membrane has a substrate layer and an active layer, 18. The raw material liquid concentrating system according to claim 16 or 17, wherein the base layer comprises one or more polymers selected from the group consisting of polysulfone, polyethersulfone, polyvinylidene fluoride, polyacrylonitrile, polyethylene, polypropylene, cellulose-based polymers, polyketones, polyamides, polyimides, polyetheretherketones, and polybenzimidazoles.
25. 25. The feedstock liquid concentrating system of claim 24, wherein the active layer of the forward osmosis membrane comprises polyamide.
26. The raw material liquid concentrating system according to claim 16 or 17, wherein the valuable substance is a compound having a weight average molecular weight of 100 to 3,000,000.
27. 18. The raw material liquid concentrating system according to claim 16 or 17, wherein the valuable material is a pharmaceutical product, a cosmetic product, or a functional chemical product, or a raw material thereof.
28. 1. A method for removing organic solvents from a solution, comprising the steps of: The method includes contacting the solution with a draw solution through a forward osmosis membrane; the solution comprises an organic solvent; the draw solution comprises a draw solute; The method for removing an organic solvent, wherein the derived solute satisfies the following (1) and (2): (1) A polymer containing at least three repeating units having a molecular weight of 30 to 100. (2) The polymer has a branched structure in which atoms (atomic groups) other than hydrogen atoms and halogen atoms are bonded to the main chain.
29. A derivative solute for removing organic solvents by forward osmosis, which satisfies the following (1) and (2): (1) A polymer containing at least three repeating units having a molecular weight of 30 to 100. (2) The polymer has a branched structure in which an atom (atomic group) other than a hydrogen atom or a halogen atom is bonded to the main chain.
Citation Information
Patent Citations
Composite hollow fiber membrane module and method for producing same
WO2022004738A1
Cited By
Method for dehydrating raw-material liquid stream and system for dehydrating raw-material liquid stream
WO2026186895A1